Vehicle window glass

A vehicle window glass with a rigid layer and non-rigid peripheral layer addresses the rigidity issues of thin glass plates by preventing water absorption and interfacial peeling, ensuring structural integrity and safety.

JP7566768B2Active Publication Date: 2024-10-15CENTRAL GLASS PRODUCTS CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2021554907
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-01-30
Filing Date
2020-10-28
Publication Date
2024-10-15
Estimated Expiration
2040-10-28

AI Technical Summary

Technical Problem

Thinner glass plates in laminated vehicle window glasses result in reduced rigidity, leading to visible elastic deformation and increased risk of interfacial peeling between the interlayer film and glass plate, especially at the edges where water absorption is higher, compromising safety and structural integrity.

Method used

A vehicle window glass design featuring a rigid layer with controlled water content and a non-rigid peripheral layer to prevent water absorption, ensuring the interlayer film and glass plate remain bonded, even when edges are exposed.

Benefits of technology

The design effectively reduces the risk of interfacial delamination and maintains structural integrity by minimizing water absorption at the edges, enhancing safety and durability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007566768000003
    Figure 0007566768000003
  • Figure 0007566768000004
    Figure 0007566768000004
  • Figure 0007566768000005
    Figure 0007566768000005
Patent Text Reader

Abstract

The vehicle window glass (10) includes a first glass plate (1), a second glass plate (2), and a middle film (3) sandwiched between a second surface (S2) and a third surface (S3) thereof. For the purpose of weight reduction, at least one of the glass plates (1, 2) has a thickness of 2.0 mm or thinner. The middle film (3) includes a main portion (4) having a rigid layer and a peripheral portion (5) comprising a non-rigid layer. The peripheral portion (5) is disposed along an upper edge, which is exposed to the atmosphere, of the vehicle window glass (10). Contact between water and the rigid layer of the main portion (4) is prevented by the peripheral portion (5) comprising the non-rigid layer. The water content of the rigid layer measured using a near-infrared spectrum is limited to 0.5% or lower.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to laminated glass vehicle glazing. [Background technology]

[0002] In response to the recent demand for lighter vehicles, lighter laminated glass is also required for use in vehicle window glass. The glass sheets used in laminated glass are thinned to reduce the weight of the laminated glass. There is a correlation between the thickness and rigidity of the glass sheet, and the thinner the glass sheet, the lower the rigidity of the laminated glass. Therefore, the stress load on the vehicle window glass that may occur in the daily environment may cause elastic deformation of the vehicle window glass that is visible to the naked eye, increasing the risk that the vehicle window glass will be difficult to maintain in a specified shape. In order to compensate for the loss in rigidity of laminated glass that occurs when the glass sheets are made thinner, Patent Document 1 discloses laminated glass that includes an interlayer film with high rigidity. Patent Document 2 discloses an interlayer film for laminated glass that contains a polyvinyl acetal resin and a plasticizer and that has excellent adhesive performance and does not lose its penetration resistance and glass shatter resistance, particularly when used over a long period of time in an environment with a lot of moisture or humidity. The interlayer film has a pummel value of 3 to 8, which represents the adhesiveness between the interlayer film and the glass plates, at a moisture content of 1 to 2% by weight, and is sandwiched between two glass plates.

[0003] In laminated glass, good adhesion between the glass sheets and the interlayer film is advantageous in terms of safety inside the vehicle when the laminated glass is subjected to an impact. A pummel test is a method for examining the adhesion between the glass sheets and the interlayer film in laminated glass. In this test, the laminated glass is struck with a hammer to shatter, and the degree of exposure of the film after the glass is partially peeled off is determined. It is disclosed that the laminated glass with the interlayer film described in Patent Document 2 passes the pummel test when a glass sheet with a thickness of 2.5 mm is used, as no glass pieces peel off even when it is shattered with a hammer.

[0004] However, when the inventors performed a pummel test on laminated glass equipped with an interlayer film made of several high-rigidity polyvinyl butyral (PVB), they found some that did not pass the test. When the inventors investigated the cause of this, they found that, while the high-rigidity interlayer film was attached to the glass, for an unknown reason, there was a large tendency for the water absorption over time to vary to the extent that the results in the pummel test were divided into pass and fail, resulting in poor yield, and that there was no correlation with the moisture content of the high-rigidity interlayer film measured while it was attached to the glass. On the other hand, when the inventors investigated the water absorption of interlayer films made of several polyvinyl butyral (PVB) films with different rigidity as single films, they found that the higher the rigidity of the interlayer film, the higher the water absorption tends to be. This suggests that the pummel test of an interlayer film made of high rigidity PVB is difficult to predict, unlike that of an interlayer film made of conventional PVB, because the water absorption in the single film state is different from the water absorption after it is bonded to the glass by the lamination process.

[0005] In recent vehicles, the design of windshields that expose the edges of the window glass is increasing (see Figure 8). When laminated glass formed with a high-rigidity interlayer so that the edges are exposed is used for the window glass of an automobile, the interlayer film has more opportunities to absorb water as it approaches the edges of the window glass. In particular, the upper edge of the vehicle window glass has more opportunities for water to come into contact with the interlayer film. Therefore, under conditions that reproduce the pummel test, the risk of interfacial peeling between the interlayer film and the glass sheet increases as it approaches the edges of the window glass.

[0006] One object of the present disclosure is to provide a window glass for vehicles that can reduce the risk of interfacial peeling between the interlayer film and the glass sheet on the edge side of the window glass, even if the edge face is exposed, when a high-rigidity interlayer film is used to supplement the rigidity of the laminated glass in response to the trend toward thinner glass sheets used in the laminated glass. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Patent No. 6466917 [Patent Document 2] JP 2000-302490 A Summary of the Invention

[0008] The vehicle window glass of the present disclosure is A first glass plate having a first surface facing an exterior of a vehicle and a second surface opposite to the first surface; a second glass plate having a fourth surface facing the interior of the vehicle and a third surface opposite to the fourth surface; an interlayer film disposed between the first glass plate and the second glass plate and facing the second surface and the third surface; A vehicle window glass comprising: The intermediate film is At least one end surface is arranged to be exposed to the atmosphere; A main portion having at least one rigid layer, and a peripheral portion made of a non-rigid layer adjacent to the main portion and disposed along at least one side of the vehicle window glass, The rigid layer has a moisture content of 0.5% or less as measured using a near-infrared spectroscopic spectrum, At least one of the first glass plate and the second glass plate has a thickness of 2.0 mm or less.

[0009] According to the present disclosure, there is provided a vehicle window glass which can reduce the risk of interfacial peeling between the interlayer film and the glass sheet on the edge side of the window glass when a high-rigidity interlayer film is used to compensate for the rigidity of the laminated glass in response to the thinning of the glass sheets used in the laminated glass. [Brief description of the drawings]

[0010] [Figure 1] 1 is a schematic cross-sectional view of an example of a vehicle window glass. [Diagram 2] 1 is a schematic cross-sectional view of an example of a vehicle window glass. [Diagram 3] 1 is a schematic cross-sectional view of an example of a vehicle window glass. [Figure 4] 1 is a schematic cross-sectional view of an example of a vehicle window glass. [Diagram 5] 1 is a schematic cross-sectional view of an example of a vehicle window glass. [Figure 6] FIG. 2 is a schematic diagram of an example of an interlayer film. [Figure 7] FIG. 2 is a schematic diagram of an example of an interlayer film. [Figure 8] 1 is a schematic diagram of an example of a vehicle equipped with a vehicle window glass. [Figure 9] 1 is a graph showing the relationship between the stiffness and moisture content of an interlayer film. [Figure 10] 1 is a graph showing the relationship between the moisture content and the pummel value of an interlayer film. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] The vehicle window glass of the present disclosure is A first glass plate having a first surface facing an exterior of a vehicle and a second surface opposite to the first surface; a second glass plate having a fourth surface facing the interior of the vehicle and a third surface opposite to the fourth surface; an interlayer film disposed between the first glass plate and the second glass plate and facing the second surface and the third surface; A vehicle window glass comprising: The intermediate film is At least one end surface is arranged to be exposed to the atmosphere; A main portion having at least one rigid layer, and a peripheral portion made of a non-rigid layer adjacent to the main portion and disposed along at least one side of the vehicle window glass, The rigid layer has a moisture content of 0.5% or less as measured using a near-infrared spectroscopic spectrum, At least one of the first glass plate and the second glass plate has a thickness of 2.0 mm or less.

[0012] FIG. 1 shows a schematic cross-sectional view of an example of a vehicle window glass according to the present disclosure. The vehicle window glass 10 in Fig. 1 has a first glass plate 1, a second glass plate 2, and an interlayer film 3. The first glass plate 1 has a first surface S1 facing the outside of the vehicle and a second surface S2 opposite the first surface S1. The second glass plate 2 has a fourth surface S4 facing the interior of the vehicle and a third surface S3 opposite the fourth surface S4. The interlayer film 3 is disposed between the first glass plate 1 and the second glass plate 2 so as to face the second surface S2 and the third surface S3.

[0013] [Interlayer] The interlayer film comprises a main portion having at least one rigid layer, and a peripheral portion adjacent to the main portion and comprising a non-rigid layer disposed along at least one edge of the vehicle glazing. In the vehicle window glass 10 of Fig. 1, the interlayer film 3 includes a main portion 4 having a rigid layer and a peripheral portion 5 consisting of a non-rigid layer. The main portion 4 and the peripheral portion 5 are adjacent to each other. The peripheral portion 5 is disposed along at least one side of the vehicle window glass 10.

[0014] The main portion of the intermediate film comprises at least one stiff layer. The rigid layer is a film having a Young's modulus at 23°C of 2.5 MPa to 200 MPa. In order to compensate for the loss of rigidity of the lightweight laminated glass, the Young's modulus of the main part is preferably 2.5 MPa to 200 MPa at 23°C. The stiffness layer may be constructed, for example, from relatively stiff PVB, SentryGlas® (Dupon), polycarbonate, ionomer, polyethylene terephthalate (PET), or other suitable polymeric or thermoplastic materials, and is preferably a thermoplastic film.

[0015] In the vehicle window glass of the present disclosure, if the moisture-resistant non-rigid layer prevents contact between the rigid layer and water, interfacial peeling between the interlayer film and the glass sheet can be further suppressed. Therefore, the main part has at least one rigid layer whose moisture content measured using a near-infrared spectrum is suppressed to 0.5% or less, and may have two or more rigid layers. In addition, as long as the main part has at least one rigid layer, it may further have a layer other than the rigid layer (e.g., a non-rigid layer). 2 to 5 each show a schematic cross-sectional view of another example of the vehicle window glass of the present disclosure. FIG. 2 differs from FIG. 1 in that the intermediate film 3 has a two-layer structure of a rigid layer HR provided on the third surface S3 side and a non-rigid layer LR provided on the second surface S2 side. FIG. 3 differs from FIG. 1 in that the intermediate film 3 has a two-layer structure including a rigid layer HR provided on the second surface S2 side and a non-rigid layer LR provided on the third surface S3 side. FIG. 4 differs from FIG. 1 in that the intermediate film 3 has a three-layer structure consisting of a rigid layer HR, a non-rigid layer LR, and a rigid layer HR. FIG. 5 differs from FIG. 1 in that the intermediate film 3 has a three-layer structure of a non-rigid layer LR, a rigid layer HR, and a non-rigid layer LR.

[0016] The peripheral portion of the interlayer is made of a non-rigid layer. The non-rigid layer is a film having a Young's modulus at 23° C. of 0.1 MPa to 2.0 MPa (preferably a film made of a thermoplastic resin). In order to prevent the main portion from absorbing moisture or water from the outside of the laminated glass for vehicles, the Young's modulus of the peripheral portion is preferably 0.1 MPa to 2.0 MPa at 23°C. The non-rigid layers may be constructed, for example, from relatively soft PVB, acoustic PVB, ethylene vinyl acetate (EVA), thermoplastic polyurethane (TPU), or other suitable polymeric or thermoplastic materials.

[0017] Fig. 6 is a schematic diagram of an example of an interlayer film provided in the vehicle window glass of the present disclosure (schematic diagram of the interlayer film viewed from the film thickness direction). The interlayer film 3 in Fig. 6 is provided with a band-shaped peripheral portion 5 having a width W along one side of the vehicle window glass. The width of the peripheral portion of the interlayer film (the length of the peripheral portion in a direction perpendicular to the direction along one side of the vehicle window glass on which the peripheral portion is provided, the length W in FIG. 6) is not particularly limited and will vary depending on the design and size of the vehicle window glass, but for example, it is preferable that W is 50 mm to 300 mm. Note that while the interlayer film shown in FIG. 6 is rectangular, the shapes of the interlayer film, the first glass plate, the second glass plate, and the vehicle window glass including these in the present disclosure are not particularly limited. For example, they may have a shape that is at least partially curved (for example, a side of the vehicle window glass on which the peripheral portion is provided is not a straight line but a curved line). The thickness of the intermediate film is not particularly limited, but is preferably, for example, 0.5 mm to 3.0 mm.

[0018] In the interlayer film of the present disclosure, at least one end surface is arranged so as to be exposed to the atmosphere. The interlayer film has at least one rigid layer, and the moisture content of the rigid layer is suppressed to 0.5% or less as measured using a near-infrared spectroscopic spectrum. The peripheral portion of the interlayer film may be arranged along at least one side of the vehicle window glass, but is preferably arranged along the side that will be the upper side when the vehicle window glass is mounted on the vehicle. The upper side of the vehicle window glass mounted on the vehicle is particularly likely to come into contact with water, so by providing a peripheral portion made of a non-rigid layer at least on the side that will be the upper side, the risk of interfacial peeling between the interlayer film and the glass sheet on the end side of the window glass can be reduced. In the interlayer film of the present disclosure, the peripheral portion may be disposed along all sides of the vehicle window glass. A schematic diagram of an example of the interlayer film of this embodiment (a schematic diagram of the interlayer film viewed from the film thickness direction) is shown in Figure 7. By disposing the peripheral portion along all sides of the vehicle window glass, it is possible to suppress contact between the rigid layer of the main portion and water, and it is possible to further suppress interfacial peeling between the interlayer film and the glass sheet.

[0019] The method for producing the interlayer film unit in the present disclosure is not particularly limited, and any known method can be used. For example, the method for forming the interlayer film raw material resin into a film includes, but is not limited to, the usual die extrusion method or calendar roll method.

[0020] Ordinary laminated glass is produced by sandwiching one continuous interlayer film between two glass plates, but the manufacturing method for laminated glass for vehicles disclosed herein is produced by sandwiching a laminated interlayer film including at least one rigid layer and an interlayer film made of a non-rigid layer, which are arranged side by side, between two glass plates. In this case, a seam will occur between the two interlayer films, but when the films are heated and pressurized in the autoclave, the seam will become inconspicuous as they are fused together, so the passengers' visibility will not be obstructed.

[0021] The vehicle window glass of the present disclosure is characterized by being lighter than conventional general laminated glass. Therefore, it is preferable that at least one of the first glass sheet and the second glass sheet in the vehicle window glass of the present disclosure is 2.0 mm or less in thickness, more preferably that the second glass sheet is 2.0 mm or less in thickness, and further preferably that both the first glass sheet and the second glass sheet are 2.0 mm or less in thickness.

[0022] [First glass plate] The first glass plate in the vehicle window glass of the present disclosure is not particularly limited, and any glass plate known as a glass plate used in vehicle window glasses can be used. The thickness of the first glass plate is preferably 1.4 mm to 2.2 mm. The composition of the first glass plate is not particularly limited. Chemically strengthened glass may be used as the first glass plate. Preferable compositions of the chemically strengthened glass include the following compositions (1) and (2). (1) By mass%, SiO2: 65-75%, Al2O3: 0-5%, Na2O+K2O: 5-20%, MgO: 0-10%, CaO: 2-15% (2) By mass%, SiO2: 55-65%, B2O3: 0-10%, Al2O3: 10-25%, Na2O+K2O: 10-20%, MgO: 0-10%, CaO: 0-5%

[0023] [Second glass pane] The second glass plate in the vehicle window glass of the present disclosure is not particularly limited, and any glass plate known as a glass plate used in vehicle window glass can be used. The thickness of the second glass plate is preferably 0.7 mm to 1.8 mm. The composition of the second glass plate is not particularly limited. Chemically strengthened glass may be used as the second glass plate. The preferred composition of the chemically strengthened glass is the same as the composition (1) or (2) above.

[0024] The manufacturing method of the vehicle window glass (laminated glass) of the present disclosure is not particularly limited, and a known method can be used. For example, an intermediate film is sandwiched between a first glass plate and a second glass plate, and the plate is passed through a pressing roll or placed in a rubber bag and suctioned under reduced pressure to remove air remaining between the members, and then pre-bonded to obtain a laminate, which is then placed in an autoclave or pressed to bond (may be bonded while appropriately heated), to obtain a laminated glass, but the method is not limited to these.

[0025] FIG. 8 is a schematic diagram of an example of a vehicle 11 equipped with a vehicle window glass 10 according to the present disclosure, but the present invention is not limited to this.

[0026] <Experiment 1: Relationship between interlayer film stiffness and moisture content> As the interlayer film, the following interlayer film samples 1 to 4 were prepared. The Young's modulus of interlayer film samples 1 to 4 was all measured in an environment with a temperature of 23° C. and a humidity of 50 to 60%. The method for measuring the Young's modulus of interlayer film samples 1 to 4 is shown below in detail. The Young's modulus of interlayer film samples 1 to 4 was measured in accordance with JIS K 7161-1. The purpose of this method is to determine the tensile modulus of elasticity (Young's modulus) of a test specimen by measuring the force and elongation applied to the test specimen when the specimen is pulled at a constant rate along the main axis (length direction) until the stress or strain (elongation) reaches a predetermined value. The test machine used was a Tensilon universal testing machine (RTC-2410) manufactured by A&D Co., Ltd., which complies with JIS K 7161-1. Test specimens were prepared by machining interlayer film samples 1 to 4 into a "tensile No. 5 dumbbell shape" conforming to JIS K 6251 by cutting.

[0027] The thickness of interlayer film sample 1 was 0.80 mm. The thickness of interlayer film sample 2 was 0.85 mm. The thickness of interlayer film sample 3 was 0.78 mm. The thickness of interlayer film sample 4 was 0.80 mm. The gauge length of the test piece was 33 mm. The number of test pieces was one for each interlayer film sample. The prepared test pieces were stored for 4 hours or more in an environment with a temperature of 23°C and a humidity of 50 to 60%. The tensile tests were performed in an environment with a temperature of 23°C and a humidity of 50 to 60%, the same as when the samples were stored. During the tensile test, a preliminary force (load: 20 mN, hold time: 10 sec) was applied only to interlayer film sample 3. The other interlayer film samples 1, 2, and 4 were subjected to tensile tests without applying a preload. The test speed during the tensile test was 0.33 mm / min, which is a speed that gives a strain of 1% of the gauge length per minute. The stress σ [MPa] applied to the test piece was calculated by dividing the force F [N] applied during measurement by the initial cross-sectional area A [mm2] of the test piece. The strain ε [-] generated in the test piece was calculated by dividing the increase in the gauge length of the test piece, ΔL0 [mm], by the gauge length of the test piece, L0 [mm]. The Young's modulus E [MPa] of the test specimen was calculated by dividing the difference between the stress σ2 [MPa] at the strain ε2 (0.25%) of the test specimen and the stress σ1 [MPa] at the strain ε1 (0.05%) of the test specimen by the difference between the strain ε2 of the test specimen and the strain ε1 of the test specimen. The stress, Young's modulus, and strain in this test were reported to two significant figures.

[0028] Interlayer film sample 1: Saflex (registered trademark, hereinafter the same) RF41 (manufactured by Eastman Chemical Company) Single layer low elasticity PVB film Young's modulus E: 1.1 MPa Interlayer film sample 2: Saflex QF51 (manufactured by Eastman Chemical Company) 3-layer low-elasticity PVB film Young's modulus E: 1.3 MPa Interlayer film sample 3: Saflex DG41 (manufactured by Eastman Chemical Company) Single-layer highly elastic PVB film Young's modulus E: 49 MPa Interlayer film sample 4: S-LEC clear film HIRZN-10 (manufactured by Sekisui Chemical Co., Ltd.) Single-layer low-elasticity PVB film Young's modulus E: 0.94 MPa

[0029] The changes in moisture content over time of interlayer film samples 1 to 4 were examined using the following procedure. (1) Each of the interlayer film samples 1 to 4 was cut into a 4 cm square and the weight was measured. (2) Each cut interlayer film sample was stored in a desiccator for several days to remove the initial moisture (this was continued until there was no change in the weight of each cut interlayer film sample). The weight of each interlayer film sample after the initial moisture had been removed was measured (this weight is also referred to as the "weight of the interlayer film sample before testing"). (3) Each interlayer film sample, from which the initial moisture had been removed, was placed in a thermostatic chamber (23°C, relative humidity 60%) and the weight and moisture content were examined over time. The weight of each interlayer film sample at each time point is also referred to as the "weight of the interlayer film sample after the test." The moisture content was calculated according to the following formula (A).

[0030] Moisture content (%) = 100 × {weight of interlayer film sample after test (g) - weight of interlayer film sample before test (g)} / weight of interlayer film sample after test (g) Formula (A)

[0031] The results are shown in Figure 9. From the results shown in Figure 9, it was found that interlayer film sample 3 containing a high elasticity PVB film had a higher moisture content over time than interlayer film samples 1, 2, and 4 made of low elasticity PVB film. This means that interlayer films with high rigidity tend to absorb water more easily than interlayer films with low rigidity.

[0032] <Experiment 2: Relationship between moisture content of interlayer film and pummel value> (1) Creating laminated glass samples The glass plates were a glass plate B1 having a thickness of 1.8 mm or 2.1 mm and a glass plate B2 having a thickness of 0.70 mm or 1.1 mm, and four combinations were made. As the interlayer film, the above-mentioned interlayer film sample 2 or sample 3 from which the initial moisture had been removed was used. Each interlayer film sample was sandwiched between glass plate B1 and glass plate B2, placed in a rubber bag and suctioned under reduced pressure to remove any air remaining between the components, after which preliminary bonding was performed to obtain a laminate, which was then placed in an autoclave and laminated under the conditions shown in Table 1. After preliminary bonding, the samples were removed from the rubber bag, and final bonding was performed using the same autoclave under the conditions shown in Table 1. The laminated glass samples prepared are as follows: Laminated glass sample C1 ··· Glass plate B1 / Interlayer film sample 2 / Glass plate B2 Laminated glass sample C2 ··· Glass plate B1 / Interlayer film sample 3 / Glass plate B2

[0033] [Table 1]

[0034] (2) Pummel test The laminated glass samples C1 and C2 (300 mm x 300 mm in size) were stored for about 17 hours in a constant temperature and humidity chamber cooled to -18°C. Each sample was placed with a glass stand to ensure a gap of about 1 cm. The laminated glass samples C1 and C2 were taken out of the constant temperature and humidity chamber and immediately struck with a hammer. A 13 mm thick iron plate was used as the striking table, tilted at 45 degrees. The hammer used had a head of approximately 500 g and a diameter of 30 mm. The angle between the sample and the striking table was approximately 5 degrees. The hammer head was swung down so that the entire surface hit the glass surface. A 100 mm x 100 mm area of ​​the corner of the sample was struck starting from the corner on the B1 side of the glass plate, and after the first row of strikes, the striker pulled back and then struck the second row so that about half of the first row overlapped. This process was repeated until it was confirmed that the struck surface of the glass was completely shattered. After the test on the first sheet was completed, the second sheet was removed from the temperature and humidity chamber and subjected to the same test. After the test was completed, the samples were left at room temperature for approximately 1 hour to allow any condensation to dry out. The exposed area of ​​the interlayer of each sample was compared with the pummel value judgment sample (pummel value 2 to 8) to determine the pummel value and evaluate the adhesion of the striking surface. The relationship between the pummel value and the adhesion of the striking surface is as shown in Table 2 below. Table 2 shows that the lower the pummel value, the higher the degree of exposure of the interlayer film, and the easier it is for the glass plate and the interlayer film to peel off.

[0035] [Table 2]

[0036] (3) Moisture content The near-infrared spectrum of the laminated glass sample was measured, the ratio of the absorption due to PVB (methylene group) to the absorption due to water was calculated, and the water content was calculated using a formula derived from the calibration curve. The measurement point was 5 to 10 cm from the edge of the glass toward the center. The measurement was performed using a spectrophotometer (U-4000) manufactured by Hitachi High-Technologies Corporation, and the water content was calculated using the absorption band of water at 1925 nm and the absorption band of a methylene group at 1705 nm.

[0037] Figure 10 shows the relationship between the moisture content and pummel value of the interlayer film when it is adhered to the glass plate. In Figure 10, "Saflex QF51" represents laminated glass sample C1 that was beaten from the glass plate B1 side, and "Saflex DG41" represents laminated glass sample C2 that was beaten from the glass plate B1 side. From the results shown in FIG. 10, it was found that the moisture content of the laminated glass sample C1 including the interlayer film sample 2 made of a low-elasticity PVB film was 0.5% or less for all four pieces, and that the moisture content of the interlayer film was small when the non-rigid interlayer film was attached to the glass. And, it was found that the moisture content of the laminated glass sample C2 including the interlayer film sample 3 made of a high-elasticity PVB film was more than 0.5% for three out of four pieces, and that the moisture content of the interlayer film was large when the high-rigidity interlayer film was attached to the glass. It was found that when the moisture content was lower than 0.5%, it showed a good pummel value like the laminated glass including the conventional interlayer film, but when the moisture content was higher than 0.5% due to water absorption, the pummel value deteriorated and the glass plate was easily peeled off. From this, it can be said that when the high-rigidity interlayer film was attached to the glass, the moisture content of the high-rigidity interlayer film could be suppressed to 0.5% or less by using the non-rigid interlayer film to prevent water absorption from the interlayer film edge after the laminated glass was manufactured, and the deterioration of the pummel value could be avoided.

[0038] The results of Experiments 1 and 2 above show that a high-rigidity interlayer film tends to absorb water easily while adhered to a glass sheet, and when it absorbs more than 0.5% moisture, it becomes easily peeled off from the glass sheet. Based on this, the present inventors have found that by covering a high-rigidity interlayer film with an interlayer film with low rigidity, a film configuration is created in which the high-rigidity interlayer film cannot absorb water from the outside of the edge face of the laminated glass, and it is possible to provide a vehicle window glass that is less likely to peel off due to water absorption on the edge side of the window glass and has high rigidity.

[0039] For example, the above-mentioned interlayer film sample 3 can be used as the main portion 4 having a relatively high rigidity in the vehicle window glass of the present disclosure, and the interlayer film samples 1, 2, and 4 can be used as the peripheral portion 5 having a relatively low rigidity. [Industrial Applicability]

[0040] The vehicle window glass of the present disclosure is not only used as a windshield or side glass in which the end faces of the laminated glass and the interlayer film are exposed to the atmosphere, but also can suppress peeling of the glass sheets at the end of the window glass due to water absorption by the interlayer film even when stored or transported in a humid environment, and is therefore suitable for transportation, for example, by land or sea freight that is not humidity-controlled.

Claims

1. a first glass sheet having a first surface facing an exterior of the vehicle and a second surface opposite the first surface; a second glass plate having a fourth surface facing the interior of the vehicle and a third surface opposite to the fourth surface; an interlayer film disposed between the first glass plate and the second glass plate and facing the second surface and the third surface; A vehicle window glass comprising: The intermediate film is At least one end surface is arranged to be exposed to the atmosphere; A main portion having at least one rigid layer, and a peripheral portion made of a non-rigid layer adjacent to the main portion and disposed along at least one side of the vehicle window glass, the rigid layer has a moisture content of 0.5% or less as measured using a near-infrared spectroscopic spectrum; At least one of the first glass plate and the second glass plate has a thickness of 2.0 mm or less. Vehicle window glass.

2. 2. The vehicle window glass according to claim 1, wherein the interlayer film constituting the main portion has a Young's modulus of 2.5 MPa to 200 MPa.

3. 3. The vehicle window glass according to claim 1, wherein the Young's modulus of the intermediate film constituting the peripheral portion is 0.1 MPa to 2.0 MPa.

4. The vehicle window glass according to any one of claims 1 to 3, wherein the width of the peripheral portion is 50 mm to 300 mm.

5. 5. A vehicle glazing as claimed in any one of the preceding claims, wherein the peripheral portion is disposed along all edges of the vehicle glazing.

6. The vehicle window glass according to any one of claims 1 to 5, wherein the first glass plate has a thickness of 1.4 mm to 2.2 mm.

7. The vehicle window glass according to any one of claims 1 to 6, wherein the second glass plate has a thickness of 0.5 mm to 1.8 mm.

8. The vehicle window glass according to claim 1 , wherein the non-rigid layer has a moisture content of 0.5% or less as measured using a near-infrared spectroscopic spectrum.

9. 9. The vehicle window glass according to claim 1, wherein a Young's modulus of an interlayer film constituting the peripheral portion is lower than a Young's modulus of an interlayer film constituting the main portion.

Citation Information

Patent Citations

  • Manufacture of laminated ceramic capacitor

    JP1989066917A

  • Laminated glass and window structure for car

    JP1999060293A

  • Glass laminate structure with improved edge strength

    JP2016539890A

  • JP302490A