Multi-use drinking straws and their manufacture

A glass drinking straw with a hydrophobic coating addresses cleaning difficulties by ensuring easy liquid drainage and hygiene, enabling multiple uses and dishwasher safety.

JP7568649B2Active Publication Date: 2024-10-16HILGENBERG GMBH
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2021568164
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-05-14
Filing Date
2020-05-05
Publication Date
2024-10-16
Estimated Expiration
2040-05-05

AI Technical Summary

Technical Problem

Traditional drinking straws are difficult to clean due to their cylindrical shape, especially when used multiple times, and often require additional tools like pipe cleaners, which can be kinked and fail to meet hygiene standards.

Method used

A glass-based drinking straw with a hydrophobic coating, preferably made of silanes, silicone oils, or inorganic-organic hybrid polymers, applied through a process involving hydrophobization and heat treatment, ensuring easy drainage of liquids and reducing dirt accumulation.

Benefits of technology

The hydrophobic coating allows for efficient cleaning without residue, prevents dripping, and maintains hygiene, making the straw suitable for multiple uses and dishwasher safety.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007568649000001
    Figure 0007568649000001
  • Figure 0007568649000002
    Figure 0007568649000002
  • Figure 0007568649000003
    Figure 0007568649000003
Patent Text Reader

Abstract

The present invention relates to a tube (1) comprising a tube base body (2) made of glass, at least the interior of which is at least partially covered with a hydrophobic coating (3). The use of such a tube (1) as a drinking straw results in a multi-use, environmentally friendly drinking straw that meets hygiene requirements and has good washability. The present invention also relates to a process for producing such a tube.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This application relates to a drinking straw made of glass for multiple use and its manufacture. The multiple use straw of the present invention can be used multiple times, has improved washability, and is even dishwasher safe. The manufacturing method allows for the manufacture of said drinking straw with low cost and high durability. [Background technology]

[0002] Conventional drinking straws are made of hard plastic, allowing for very thin walls and very smooth surfaces. Drinking straws usually have a kink point that allows a portion of the drinking straw to bend in a certain direction.

[0003] However, recent European regulations prohibit drinking straws from being made from single-use materials such as plastics in order to avoid plastic waste in the future, so other materials must be found for making drinking straws and to meet the environmental protection requirements of the European Union.

[0004] Patent document DE 10 2007 045935 A1 discloses a productivity test on a carrier body, optionally a filter layer with reduced pore size, optionally consisting of at least two strips, one of which is a reagent layer.

[0005] Patent document US2018 / 112083A1 discloses a tube and a coating for the inner wall of the tube.

[0006] Patent document US2006 / 029808A1 discloses a superhydrophobic coating having a water contact angle of more than 150°. The coating can maintain its superhydrophobicity even after being immersed in water for one week.

[0007] Patent document US 5 112 658 A1 discloses coated glass containers having a surface-hardened composition which is the reaction product of at least one ethylenically unsaturated monoene, a polyene and a curing initiator. The coating is bonded to the exterior or interior surface of the glass container to increase its hardness and strength.

[0008] Patent document US2004 / 082699A1 discloses a durable, weather-resistant and scratch-resistant coating provided by a composition comprising a fluorinated component and an adhesion-promoting compound. The adhesion-promoting compound may include an alkoxy group, a furfuryl-containing ring structure, and a reactive group.

[0009] Patent document TWM572182 discloses a drinking straw made from the hollow stem of a plant, such as reed, wheat or bamboo, the inner surface of which may be covered with a grease such as linseed oil or sticky rice water to make the inner surface of the drinking straw smoother and more durable.

[0010] Furthermore, patent document AU2018102071A4 discloses an environmentally friendly drinking straw made from wheat stalks. Summary of the Invention [Problem to be solved by the invention]

[0011] However, drinking straws that are used multiple times must be regularly cleaned after each use, which is difficult due to the long cylindrical shape of the drinking straw. Especially in the field of gastronomy, efficient and fast cleaning of the drinking straws must be guaranteed.

[0012] Besides washing the drinking straw with water and cleaning liquid, the use of small brushes, such as pipe cleaners, may also be required to remove stuck off or drink residues, such as fruit particles that may be contained in fruit milkshakes or smoothies. However, said pipe cleaners easily get kinked and have to be washed again themselves, which often does not meet hygiene requirements.

[0013] Thus, a typical problem with prior art ecological drinking straws is that they are very difficult to clean, which may contribute to user dislike, and furthermore, fast and efficient cleaning, e.g. for gastronomic purposes, cannot be guaranteed.

[0014] Therefore, the technical problem targeted by this application is to provide a multiple-use, environmentally friendly drinking straw that is easily washable.Furthermore, the technical problem targeted by this application is to provide a process for the manufacture of such a drinking straw. [Means for solving the problem]

[0015] This objective technical problem is solved by the use of a glass tube with a hydrophobic coating for a tube according to claim 1, a process for producing such a tube according to claim 8 and a drinking straw according to claim 13. Further advantages and preferred embodiments are defined in the dependent claims.

[0016] The present invention provides the following aspects, subjects and preferred embodiments, taken individually or in combination, which further contribute to solving the technical problem for which the present invention is directed.

[0017] 1. A tube comprising a tube base body made of or consisting of glass, at least the interior of the tube base body being at least partially covered with a hydrophobic coating.

[0018] 2. A tube according to item 1, wherein the tube body is made of soda-lime glass, borosilicate glass or quartz glass.

[0019] 3. A tube according to one of the preceding items, wherein the coating comprises a hydrophobic polymeric material. 4. The tube according to item 3, wherein the polymeric material is selected from the group consisting of silanes, silicone oils, halogenated hydrocarbons and inorganic-organic hybrid polymers.

[0020] 5. A tube according to one of items 3 or 4, wherein the coating further comprises an antibacterial agent. 6. The tube according to item 5, wherein the antibacterial agent is selected from the group consisting of silver and copper and compounds thereof.

[0021] 7. The tube according to item 6, wherein the antibacterial agent is silver, either elemental or colloidal. 8. The tube according to item 6, wherein the antibacterial agent is silver nitrate.

[0022] 9. A tube according to any one of the preceding items, wherein said tube has an inner diameter between 3 and 10 mm, preferably between 5 and 8 mm.

[0023] 10. A tube according to one of the preceding items, wherein the tube has a wall thickness between 0.8 and 3 mm, preferably between 1 and 2 mm.

[0024] 11. A tube according to one of the preceding items, wherein the coating has a thickness between 0.1 μm and 1000 μm, preferably between 1 μm and 500 μm, more preferably between 10 μm and 100 μm.

[0025] 12. A tube according to one of the preceding items, wherein said tube has a length between 100 and 350 mm, preferably between 120 mm and 300 mm.

[0026] 13. A tube according to one of the preceding items, wherein the tube body has a straight cylindrical shape or an angled cylindrical shape or a twisted cylindrical shape.

[0027] 14. A tube according to one of the preceding items, wherein at least the interior of the tube base body is entirely coated with a hydrophobic coating.

[0028] 15. A tube according to one of the preceding items, wherein the tube base body is entirely covered with a hydrophobic coating.

[0029] 16. A tube according to one of the preceding claims, in which the glass tube body is hydrophobized, preferably silanized, at least in the part that is covered by the hydrophobic coating.

[0030] Therefore, to further improve adhesion of the hydrophobic polymer coating to the glass, the glass itself undergoes a hydrophobic treatment before the coating is applied.

[0031] 17. A process for producing a coated glass tube, comprising: a) providing a glass tube base body; b) providing a solution or suspension comprising a hydrophobic polymeric material; c) contacting the tubular body with the solution or suspension provided in step b) at least on the inner surface of the tubular body; d) optionally drying the tubular body obtained in step c); e) heat treating the tube obtained in step c).

[0032] 18. The process according to item 18, wherein the solution provided in step b) is a solution containing 0.5-10 wt. %, preferably 1.0-2.0 wt. % of hydrophobic polymeric material, and the solvent is preferably water.

[0033] 19. The process according to item 17 or 18, wherein the hydrophobic polymeric material is selected from the group consisting of silanes, silicone oils, halogenated hydrocarbons and inorganic-organic hybrid polymers.

[0034] 20. The process according to any one of items 17 to 19, wherein the solution of step b) further comprises an antibacterial agent.

[0035] 21. The process according to item 20, wherein the antibacterial agent is selected from the group consisting of silver and copper and compounds thereof.

[0036] 22. The process according to item 21, wherein the antibacterial agent is silver, elemental or colloidal. 23. The process according to item 21, wherein the antibacterial agent is silver nitrate.

[0037] 24. The process according to one of the preceding items, wherein in step d) a temperature of at least 100°C, preferably at least 200°C, more preferably at least 250°C is used.

[0038] 25. The process according to one of the preceding items, wherein the heat treatment of step d) is carried out for at least 5 minutes, preferably at least 15 minutes, more preferably at least 30 minutes, even more preferably at least 60 minutes.

[0039] 26. The process according to any one of the preceding items, wherein step c) comprises immersing the tube in the solution provided in step b). This is therefore dip coating.

[0040] 27. The process according to one of the preceding items, wherein step c) includes vaporizing the tube with the solution provided in step b).

[0041] 28. A process according to one of the preceding items, wherein step c) comprises surface diffusion. 29. A process according to one of the preceding items in which the entire tube is coated.

[0042] This means that both the inner and outer surfaces of the tube are coated. 30. Use of a hydrophobic coating for drinking straws made of glass.

[0043] 31. The use according to item 30, wherein the hydrophobic coating is selected from the group consisting of silanes, silicone oils and halogenated hydrocarbons.

[0044] A principal aspect of the present invention is a tube comprising a tube base body constructed from glass, at least the interior of the tube base body having a hydrophobic coating.

[0045] The hydrophobic coating provides water repellent properties to the glass base body, and furthermore, it allows efficient droplet generation, so that for the relevant parts, i.e. at least the interior of the base body, the liquid does not spread on the surface of the coating, but is present in droplet form, preferably in the form of small droplets.

[0046] Suitable hydrophobicity of the coating can be achieved by selecting an appropriate organic or hybrid organic coating material, and optionally confirmed or defined by an appropriate measurement or parameter, such as by exhibiting a contact angle of the coating with a water drop of at least 90°, preferably at least 120°, more preferably at least 160°, as measurable by a drop shape analyzer such as a goniometer.

[0047] The hydrophobic coating is preferably made of a hydrophobic polymer. Said hydrophobic polymer coating ensures that the cleaning liquid entering inside the tube can be easily drained from the tube without leaving any cleaning liquid inside the tube, resulting in the fact that the tube is more easily cleanable, so that capillary forces and the so-called bottleneck effect can be avoided. Furthermore, dirt is less likely to accumulate and adhere to the inner surface of the base body. The hydrophobic polymer coating can ensure sufficient bonding and adhesion of the coating to the main glass tube body, especially when it undergoes heat treatment when in contact with the glass tube body during preparation, and especially when selected from suitable polymer materials. This prevents leakage and therefore problems that are critical for health.

[0048] The hydrophobic behavior of the coating, and the resulting avoidance of the bottleneck effect, may also prevent the tube used as a drinking straw from dripping or shedding droplets when removed from a glass of liquid, thus avoiding possible staining of the user's clothes. The bond strength between the tube base body and the hydrophobic polymer coating can preferably be further increased by prior hydrophobization or water repellent treatment of the tube base body surface, preferably by silanization at least in the parts that will be covered with the hydrophobic coating. Therefore, in order to further improve the adhesion of the hydrophobic polymer coating to the glass, the glass itself is subjected to a hydrophobization treatment before the coating is applied.

[0049] Additionally, the hydrophobic coating may provide additional durability, making cleaning of the tube even possible in a regular dishwasher.

[0050] Additionally, the hydrophobic coating provides a glossy effect to the glass, improving user acceptance of such glass tubes as drinking straws.

[0051] Preferably, in order to fully achieve the above-mentioned advantageous effects, the inside of the tube base body is entirely covered with a hydrophobic coating.

[0052] More preferably, the inner and outer surfaces of the tube base body are entirely covered with a hydrophobic coating, which further improves the feel of the glass to the touch, as well as the acceptability of a drinking straw that uses the coated glass tube body.

[0053] The tube base body is made of or consists of glass, preferably soda-lime glass, borosilicate glass or even quartz glass, as such materials are environmentally friendly and suitable for multiple uses.

[0054] According to a further preferred embodiment, the coating for the tube base body comprises a polymeric material selected from the group of silanes, silicone oils, halogenated hydrocarbons such as Teflon®, and inorganic-organic hybrid polymers. A preferred example of an inorganic-organic hybrid polymer is the material known by the trademark Ormocer® (https: / / www.ormocere.de). Such materials generally exhibit excellent heat resistance and thermal shape stability, excellent adhesion to multiple materials, as well as many other advantageous properties (see US Patent US7687654B2).

[0055] The described materials are easy to handle and are furthermore suitable for use on glass. When a coating of, for example, silane or silicone oil on glass is tempered at high temperature, a bond is formed between the coating and the glass, so that such coating is very durable and suitable for multiple cleanings. Inorganic-organic hybrid polymers such as Ormocer® also have excellent durability when coated on glass. Such inorganic-organic hybrid polymers such as Ormocer® furthermore have excellent abrasion resistance and dishwasher resistance when coated on glass.

[0056] Further suitable materials for hydrophobic polymer coatings are manganese oxide polystyrene composites (e.g. in nanocomposite form), zinc oxide polystyrene composites (also e.g. in nanocomposite form), precipitated calcium carbonate in combination with fatty acids and / or triglycerides, carbon nanotube structures, silica nanocoatings, and fluorinated silanes.

[0057] Moreover, said coating further comprises at least one antimicrobial agent, more preferably an antimicrobial agent selected from the group consisting of silver and copper and their compounds. For example, silver can be present in its elemental or colloidal form, or it can be silver nitrate. Titanium dioxide is also a suitable biocide, which decomposes organic compounds under the influence of UV light. The application of UV light for cleaning purposes is also easily achievable. Such additional antimicrobial properties further improve the hygiene requirements of gastronomy despite multiple uses.

[0058] The glass tube preferably has a thickness between 0.8 mm and 3 mm, a length between 100 mm and 350 mm, more preferably between 120 and 300 mm, and the tube body preferably has a straight cylindrical shape or an angled cylindrical shape. Preferably, the tube has an inner diameter between 3 and 10 mm, more preferably between 5 and 8 mm. Preferably, the tube has a wall thickness between 0.8 and 3 mm, preferably between 1 and 2 mm. Preferably, the coating has a thickness between 0.1 μm and 1000 μm, more preferably between 1 μm and 500 μm, most preferably between 10 μm and 100 μm.

[0059] Such tubes are therefore easy to manufacture and, furthermore, due to the simple shape of the tube, the hydrophobic coating can be applied evenly and continuously without risk of accumulation and / or thickening or bulging of the coating liquid.

[0060] The invention further provides a process for manufacturing a coated glass tube, comprising the steps of providing a glass tube body, providing a solution or suspension comprising a hydrophobic polymeric material, contacting the tubular body at least on its inner surface in the solution or suspension provided in the previous step, optionally drying the tubular body, and heating the tube.

[0061] Such a heat treatment is so-called tempering. Coating substances such as the above mentioned polymeric materials are able to form a bond with the glass, and in particular with the glass surface, leading to the fact that the resulting coated glass is very durable, without the risk of the coating being removed, decomposing or even scratching the glass.

[0062] The aqueous solution or suspension for coating contains 0.5-10% by weight, preferably 1.0-2.0% by weight, of the hydrophobic polymeric material. The solvent is preferably water.

[0063] The specifically selected concentration of the hydrophobic polymer is particularly preferred because the suitable viscosity range can be adjusted in a good manner for the coating step, so that the tube base body is homogeneously contacted and wetted, and the solution or suspension containing the hydrophobic polymer drips onto the tube base body without forming bulges or residues.

[0064] Preferably, the hydrophobic polymeric material is selected from the group consisting of silanes, silicone oils, halogenated hydrocarbons and inorganic-organic hybrid polymers.

[0065] Preferably, the solution comprising the hydrophobic polymeric material further comprises an antimicrobial agent. Preferably, the antimicrobial agent is selected from the group consisting of silver and copper and compounds thereof. More preferably, the antimicrobial agent is silver, either elemental or colloidal. Most preferably, the antimicrobial agent is silver nitrate.

[0066] Preferably, a temperature of at least 100° C., more preferably at least 200° C., most preferably at least 250° C. is used in the heating step.

[0067] Preferably, the heating step is carried out for at least 5 minutes, more preferably at least 15 minutes, even more preferably at least 30 minutes, and most preferably at least 60 minutes.

[0068] The invention also relates to the use of a hydrophobic coating for a drinking straw made of glass. Preferably, the hydrophobic coating is selected from the group consisting of silanes, silicone oils and halogenated hydrocarbons.

[0069] The present invention is described in detail in the following disclosure of preferred but non-limiting embodiments by making reference to the accompanying drawings. [Brief description of the drawings]

[0070] [Figure 1] 1 is a cross-sectional view of a first embodiment of a glass tube according to the present invention. [Diagram 2] FIG. 2 is a cross-sectional view of a second embodiment of a glass tube according to the present invention. [Diagram 3] FIG. 4 is a cross-sectional view of a third embodiment of a glass tube according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0071] 1 shows a cross-sectional view of a tube 1 according to a first embodiment of the present invention, comprising a tube base body 2 and a hydrophobic coating 3. Here, the hydrophobic coating 3 is shown applied to the inner surface of the tube base body 2, where the hydrophobic coating may be composed of silanes, silicone oils, halogenated hydrocarbons or inorganic-organic hybrid polymers as disclosed herein.

[0072] For example, silicone oils from the company Wacker can be used, which have a very efficient cost-performance ratio, allow easy handling and allow good hydrophobization of the surface to be achieved.

[0073] Additionally, different types of Dynasilan® manufactured by Evonik Industries are available which offer excellent hydrophobic properties.

[0074] Additionally, different types of Baysilon® M100 are available.

[0075] Additionally, chlorinated or chlorinated hydrocarbons, such as Teflon, may function as coatings.

[0076] Another specific embodiment exemplified for hydrophobic coatings are different types of inorganic-organic hybrid polymers, such as Ormocer®. Such hybrid polymer materials can be synthesized by sol-gel methods, by monomers or pre-condensed components (generally silanes, optionally organo-modified, in combination with partially additional metal alkoxy compounds and / or other compounds) undergoing hydrolysis and condensation of appropriate groups (see US Patent US7687654B2).

[0077] For example, the inorganic network is mainly constructed via targeted hydrolysis and condensation of organically modified Si-alkoxides. Furthermore, co-condensation with other metal alkoxides, such as Ti, Zr or Al-alkoxides, is also possible. In a subsequent step, the polymerizable groups fixed to the inorganic network are crosslinked with each other. Furthermore, organically modified Si-alkoxides can be used, which do not participate in organic polymerization reactions and therefore contribute to the organic functionalization of the inorganic network. Such polymers can be greatly used for surface functionalization.

[0078] 2 shows a second embodiment of the invention, in which an antimicrobial agent 4 is incorporated into the coating 3. The antimicrobial agent may be provided as particles of a material selected from the group including silver, copper and their respective compounds, and titanium dioxide. For example, elemental or colloidal silver may be incorporated into the coating 3. The antimicrobial agent may also be silver nitrate, which may be dissolved and homogeneously dispersed in the coating 3.

[0079] 3 shows a further embodiment of the present application, showing coating layers 3 on the inside and outside of the tube base body. In this case, the entire drinking straw may be protected with a hydrophobic coating 3.

[0080] In the following, a process for the manufacture of a coated glass tube according to one of the three above-described embodiments is further presented.

[0081] The process provides a step of providing a glass tube body 2 and a solution or suspension comprising a hydrophobic polymeric material, the hydrophobic polymeric material being as defined above. The tubular body is then contacted with the solution or suspension, at least the inner surface of the tubular body being contacted. As for the third embodiment, the entire glass tube body is contacted with the solution or suspension comprising the hydrophobic polymeric material.

[0082] The tubular body is then optionally dried. Finally, the tubular body is heat treated, typically at a relatively high temperature that is still tolerable for the coating material, for example at a temperature of at least 200°C, more preferably at least 250°C, even more preferably at least 300°C, in order to fix the coating to the glass surface. The heat treatment time is typically at least 5 minutes, preferably at least 15 minutes, more preferably at least 30 minutes, even more preferably at least 60 minutes. To obtain an advantageous viscosity for the coating process, the aqueous solution comprises 0.5 to 10% by weight, preferably 1.0 to 2.0% by weight, of hydrophobic polymeric material. The solvent is preferably water. However, other solvents, in particular organic solvents, are also possible.

[0083] Preferably, contacting the glass tube body with the solution or suspension involves immersing the tube 2 in the solution. This dip coating is very easy and cheap, and furthermore allows the entire surface of the drinking straw to be in contact with the hydrophobic polymer solution or suspension.

[0084] In another embodiment, a solution or suspension containing a hydrophobic polymer is vaporized and sprayed onto the glass tube. If only the inner surface is to be contacted, the spray nozzle would be inserted into the body of the glass tube and moved along the body of the glass tube to ensure a uniform coating.

[0085] In another alternative embodiment, the glass tube base body is contacted with the hydrophobic polymer by a surface diffusion process.

[0086] The invention is not limited to the embodiments described above: the tubes may have a triangular, square or rectangular cross section, or even a polygonal or oval cross section, depending on the corresponding shape of the tube base body.

[0087] It is also possible to apply the hydrophobic coating to only a portion of the inside of the tube, so that for example an area, say 0.5 cm at the top and bottom, is left uncoated.

[0088] The tube according to the invention can be very advantageously used as a drinking straw.

Claims

1. A tube (1) adapted to be used as a drinking straw, comprising a tube base body (2) made of or consisting of glass, at least the inside of said tube base body (2) being at least partially covered with a hydrophobic coating (3), said glass tube body (2) being hydrophobized, preferably silanized, at least in the part covered by said hydrophobic coating (3), said coating (3) further comprising an antimicrobial agent (4).

2. 2. The tube (1) according to claim 1, wherein the inside of the tube base body (2) is entirely covered with a hydrophobic coating (3).

3. 3. The tube (1) according to claim 1 or 2, wherein the tube body (2) is made of soda-lime glass, borosilicate glass or quartz glass.

4. The tube (1) according to one of claims 1 to 3, wherein the coating (3) comprises a hydrophobic polymeric material, preferably selected from the group consisting of silanes, silicone oils, halogenated hydrocarbons and hydrophobic inorganic-organic hybrid polymers.

5. Tube (1) according to one of the claims 1 to 4, wherein the antimicrobial agent is selected from the group consisting of silver, preferably elemental or colloidal silver, a compound of silver, preferably silver nitrate, and copper and its compounds.

6. Tube (1) according to one of the claims 1 to 5, wherein the tube (1) has an internal diameter between 3 and 10 mm, preferably between 5 and 8 mm, and / or a wall thickness between 0.8 and 3 mm, preferably between 1 and 2 mm, and / or a length between 100 and 350 mm, preferably between 120 and 300 mm, and / or the coating (3) has a thickness between 0.1 μm and 1000 μm, preferably between 1 μm and 500 μm, more preferably between 10 μm and 100 μm.

7. Tube (1) according to one of the claims 1 to 6, wherein the tube body (2) has a straight cylindrical shape or an angled cylindrical shape or a twisted cylindrical shape.

8. 1. A process for producing coated drinking straws, comprising: a) providing a glass tube base body (2), said glass tube base body (2) being hydrophobized, preferably silanized, at least in the part that is covered by the hydrophobic coating (3); b) providing a solution or suspension comprising a hydrophobic polymeric material; c) contacting the tubular body (2) with the solution or suspension provided in step b) at least on the inner surface of the tubular body (2) by immersing the tubular body (2) in the solution or suspension; d) optionally drying said tubular body (2) obtained in step c); e) heat treating the tubular body (2) obtained in step c), process.

9. 9. The process according to claim 8, wherein the solution provided in step b) is a solution comprising 0.5-10 wt. %, preferably 1.0-2.0 wt. % of a hydrophobic polymeric material, and / or the hydrophobic polymeric material is selected from the group consisting of silanes, silicone oils, halogenated hydrocarbons and inorganic-organic hybrid polymers.

10. The process of claim 9 , wherein the solvent for the solution is water.

11. The process according to any one of claims 8 to 10, wherein the solution of step b) further comprises an antimicrobial agent, preferably selected from the group consisting of silver, copper and compounds thereof, preferably elemental or colloidal silver or silver nitrate.

12. The process according to one of claims 8 to 11, wherein in step e) a temperature of at least 200°C, preferably at least 250°C, more preferably at least 300°C is used and / or said heat treatment in step e) is carried out for a period of at least 5 minutes, preferably at least 15 minutes, more preferably at least 30 minutes, even more preferably at least 60 minutes.

13. The process according to one of claims 8 to 12, wherein step c) comprises immersing the tube in the solution provided in step b) or evaporating the tube with the solution provided in step b) or by surface diffusion.

Citation Information

Patent Citations

  • fertility test

    DE102007045935A1

  • JP1977166688U

  • Paper tube

    JP1994133840A

  • Kit for food, drink and cooking

    JP1995275137A

  • Glass vessel and its manufacturing method

    JP2003286047A