Charging device and method for producing raw materials for blast furnace
The charging device with a cylindrical chute, diffusion section, and chute extension portion addresses uneven distribution in vertical carbonization furnaces, enhancing the uniformity of carbon-containing materials and improving ferro coke strength and quality.
Patent Information
- Application Number
- JP2022172846
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-02-22
- Filing Date
- 2022-10-28
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2042-10-28
AI Technical Summary
Existing vertical carbonization furnaces face challenges in uniformly distributing carbon-containing materials, leading to uneven gas flow and segregation of powders, which affects the carbonization process and results in non-uniform ferro coke production.
A charging device with a cylindrical chute, diffusion section, and chute extension portion that diffuses materials in both the transportation and perpendicular directions, combined with a stepped portion and comb-like chute extension to improve distribution within the furnace.
The solution enhances the uniform distribution of carbon-containing materials, improving the strength and quality of ferro coke production by reducing segregation and ensuring consistent gas flow.
Smart Images

Figure 0007571778000002 
Figure 0007571778000003 
Figure 0007571778000004
Abstract
Description
[Technical field]
[0001] The present invention relates to a charging device for charging a carbon-containing material into a vertical carbonization furnace for producing coke, and a method for producing raw material for a blast furnace using the charging device. [Background technology]
[0002] In recent years, the steel industry has been required to reduce CO2 gas emissions in light of global warming. For this reason, there is an urgent need to reduce the use of fossil fuels. In the steel industry, molten iron is produced in blast furnaces by reducing iron ore with carbon (coke produced by carbonizing coal in a coke oven). In order to reduce the coke consumption, technology is being developed to use ferro-coke as a raw material for blast furnaces. Ferro-coke is produced by mixing a certain amount of iron ore with coal, agglomerating it, and then carbonizing it to disperse fine metallic iron particles in the coke. The catalytic action of the metallic iron increases the reactivity of the coke.
[0003] A method using a vertical carbonization furnace has been proposed as a method for carbonizing ferro-coke. Patent Document 1 discloses a vertical carbonization furnace having a carbonization zone at the top and a cooling zone at the bottom. The method for producing ferro-coke in a vertical carbonization furnace includes a charging step of charging molded materials made of a carbon-containing material and an iron-containing material into the vertical carbonization furnace using a charging chute or the like, a carbonization step of producing ferro-coke by blowing in a heated gas in the carbonization zone and carbonizing the molded materials, a cooling step of cooling the ferro-coke by blowing in a cooling gas provided in the cooling zone, an in-furnace gas discharge step of discharging in-furnace gas from a discharge port at the top of the vertical carbonization furnace, and a ferro-coke discharge step of discharging the ferro-coke from the bottom of the cooling zone.
[0004] In the carbonization process, low-temperature gas is blown in through a low-temperature gas blowing nozzle in the middle of the vertical carbonization furnace, and high-temperature gas is blown in through a high-temperature gas blowing nozzle in the lower part.
[0005] Here, the low-temperature gas and the high-temperature gas are blown in the depth direction of the vertical carbonization furnace so that the carbon-containing material is effectively heated and cooled, since the carbon-containing material is charged into the vertical carbonization furnace from the charging chute in the direction almost the same as the depth direction of the vertical carbonization furnace. In addition, in order to allow the low-temperature gas and the high-temperature gas to penetrate to the center of the vertical carbonization furnace, it is necessary to suppress the dimension of the vertical carbonization furnace in the depth direction. In order to increase the production amount of ferro-coke, it is necessary to increase the volume of the vertical carbonization furnace, so that the structure of the vertical carbonization furnace needs to have a larger dimension in the furnace width direction perpendicular to the depth direction than in the depth direction.
[0006] Considering the structural constraints of this vertical carbonization furnace, if the furnace width direction is made larger than the depth direction, the carbon-containing material supplied from the charging chute needs to be dispersed evenly in the furnace width direction. Regarding a conveying device for conveying bulk materials such as minerals, Patent Document 2 discloses a conveying device that is provided with a material dispersion guide section from the center of the conveying direction toward the outlet side and disperses the material radially. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] JP 2011-057970 A [Patent Document 2] JP 2011-162271 A Summary of the Invention [Problem to be solved by the invention]
[0008] However, in a vertical carbonization furnace having a structure in which the size in the furnace width direction is larger than that in the depth direction, it is difficult to arrange a large number of charging chutes to correspond to all positions in the furnace width direction in order to uniformly distribute the carbon-containing material corresponding to the size in the furnace width direction. Even if a limited number of charging chutes are arranged in the furnace width direction, the carbon-containing material discharged from the charging chutes is distributed at the bottom of the vertical carbonization furnace according to the angle of repose of the charged material (carbon-containing material), and does not have a uniform charging shape. For this reason, when the molded material (carbon-containing material) is charged into the furnace, there are places where there are many molded materials (carbon-containing material) in the furnace width direction and places where there are few molded materials (carbon-containing material), which causes the gas flow in the furnace to become uneven, which affects the carbonization of the molded material (carbon-containing material).
[0009] In addition, the powder generated by the collision between the molded products and the wall of the charging chute or between the molded products themselves tends to segregate and accumulate on the charging device side at the bottom of the vertical carbonization furnace. This is because most of the powder in the charge slips through the molded products and settles, causing the charge to separate into two layers, a molded product layer (upper layer) and a powder layer (lower layer), before reaching the carbonization furnace. When one ton of molded products is charged, the thickness of the charge when it enters the carbonization furnace is about 150 mm at maximum, but since the molded products are charged from a position higher than the powder present below them, they tend to fly to a position far from the charging inlet, while the powder in the lower layer falls near the charging inlet. The molded products form mountains according to their angle of repose, resulting in a relatively uniform distribution, but the powder is fixed in position by slipping between the molded products, so if the powder falls at one point, significant segregation will occur. The problem caused by powder segregation is that the gas flow in the furnace becomes uneven, which affects the carbonization of the molded product. If the carbon-containing material cannot be uniformly charged in the furnace width direction, the powder pressure will be locally high in the furnace, and the resulting local weight will cause the molded product (carbon-containing material) to crack.
[0010] Furthermore, Patent Document 2 discloses a method for uniformly charging (transporting) materials by providing a dispersion guide section with an inclined surface that slopes radially downward from the center of the width of the transport path toward the outlet side, thereby dispersing the materials radially. However, the presence or absence of a dispersion guide section does not affect the flying distance of the powder, and the installation of a dispersion guide section cannot eliminate powder segregation at the charging inlet side.
[0011] The present invention has been made in consideration of the above circumstances, and aims to provide a charging device and a method for producing raw materials for a blast furnace that can charge carbon-containing materials while improving the distribution of the materials inside a vertical carbonization furnace. [Means for solving the problem]
[0012] The gist and configuration of the present invention to solve the above problems are as follows. [1] A charging device for charging a carbon-containing material into a vertical carbonization furnace, the charging device having a cylindrical charging chute through which the carbon-containing material passes, a diffusion section that diffuses the carbon-containing material that has passed through the charging chute in a direction in which the carbon-containing material passes and in a diffusion direction perpendicular to the direction of passage, and a chute extension section that charges the carbon-containing material after being diffused in the diffusion section into the vertical carbonization furnace and protrudes into the furnace. [2] The charging device described in [1], further comprising a step section downstream of the diffusion section, which provides a drop in the feeding direction toward the chute extension section for the carbon-containing material diffused in the diffusion section. [3] The charging device described in [2], wherein the drop of the step portion is 30 mm or more and 60 mm or less. [4] The charging device described in [2] or [3], wherein the length w of the chute extension portion in the feeding direction satisfies the relationship of 0.27≦w / W<0.47, where W is the depth dimension of the vertical carbonization furnace. [5] The charging device described in [1], wherein the chute extension section extends in a comb-tooth shape in the depth direction of the vertical carbonization furnace. [6] The charging device described in [5], wherein the width of each comb blade and the distance between adjacent comb blades of the chute extension portion are 50 mm or more and 200 mm or less. [7] The charging device described in [5] or [6], wherein the length x of the depth direction of the chute extension portion satisfies the relationship of 0.20≦x / W≦0.50, where W is the depth dimension of the vertical carbonization furnace. [8] A method for producing raw materials for a blast furnace, comprising the steps of: producing raw materials for a blast furnace using the charging device according to any one of [1] to [7] and the vertical carbonization furnace. Effect of the Invention
[0013] According to the present invention, it is possible to charge carbon-containing materials while improving the distribution of the carbon-containing materials inside a vertical carbonization furnace. [Brief description of the drawings]
[0014] [Figure 1] FIG. 2 is a schematic perspective view showing an example of a charging device and a vertical carbonization furnace in the first embodiment. [Diagram 2] FIG. 2 is a side schematic view showing an example of a charging device and a vertical carbonization furnace in the first embodiment. [Diagram 3] FIG. 11 is a schematic perspective view showing an example of a charging device and a vertical carbonization furnace in a second embodiment. [Figure 4] FIG. 11 is a side schematic view showing an example of a charging device and a vertical carbonization furnace in a second embodiment. [Diagram 5] FIG. 1 is a side schematic view showing an example of a charging device and a vertical carbonization furnace that are not provided with a step portion and a chute extension portion. [Figure 6] FIG. 13 is a diagram showing the results of measuring the distribution of carbon-containing materials using a charging device that does not have a step portion and a chute extension portion. [Figure 7] FIG. 13 is a diagram showing the results of measuring the distribution of carbon-containing materials using a charging device having a step portion and a chute extension portion. [Figure 8] 1 is a diagram showing the relationship between the drop of a step and the deviation of the average value of the fine particle distribution of carbon-containing materials in a vertical carbonization furnace. FIG. [Figure 9] 1 is a diagram showing the relationship between the drop of a step and the deviation of the average value of the distribution of molded products of a carbon-containing material in a vertical carbonization furnace. FIG. [Figure 10] FIG. 11 is a diagram showing the measurement results of the strength of ferro coke in the second embodiment. [Figure 11] FIG. 11 is a top schematic view showing an example of a modified charging device in the second embodiment. [Figure 12] FIG. 13 is a schematic perspective view showing an example of a charging device and a vertical carbonization furnace in a third embodiment. [Figure 13] FIG. 11 is a top schematic view showing an example of a charging device and a vertical carbonization furnace in a third embodiment. [Figure 14] FIG. 13 is a diagram showing the relationship between the width of a single comb blade of a chute extension and the maximum powder ratio in the third embodiment. [Figure 15] FIG. 13 is a diagram showing the relationship between the distance between the comb blades of the chute extension and the maximum powder rate in the third embodiment. [Figure 16] FIG. 11 is a diagram showing the relationship between the ratio of the horizontal length of the chute extension part to the depth dimension of the vertical carbonization furnace and the maximum powder rate in the third embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] The present invention will be described below through embodiments of the present invention, taking as an example the case of producing ferro-coke, which is a type of molded coke. Here, the drawings are schematic and may differ from the actual ones. Furthermore, the following embodiments are merely examples of devices and methods for embodying the technical idea of the present invention, and are not intended to limit the configuration to those described below. In other words, the technical idea of the present invention can be modified in various ways within the technical scope described in the claims.
[0016] First Embodiment The configuration of a charging device 9 according to a first embodiment of the present invention will be described with reference to Fig. 1 and Fig. 2. Fig. 1 shows a schematic perspective view of the charging device 9 and a vertical carbonization furnace 20. Fig. 2 shows a schematic side view of the charging device 9 and the vertical carbonization furnace 20.
[0017] The charging device 9 charges the briquetted carbon-containing material into the vertical carbonization furnace 20. The vertical carbonization furnace 20 carbonizes the carbon-containing material charged from the charging device 9 to produce coke. The charging device 9 may charge the vertical carbonization furnace 20 with briquettes containing a carbon-containing material (coal, etc.) and an iron-containing material (iron ore, etc.) that are raw materials for ferro coke, in order to produce ferro coke in the vertical carbonization furnace 20.
[0018] The charging device 9 has a charging chute 1, a diffusion section 2, and a chute extension section 3. The charging chute 1 has a cylindrical shape that allows the carbon-containing material to pass through inside. The charging chute 1 has an opening / closing section 1a such as an openable / closable gate at the outlet. The diffusion section 2 has a shape of a square pyramid. The diffusion section 2 is arranged so that the top of the square pyramid is located below the outlet of the charging chute 1. The diffusion section 2 diffuses the carbon-containing material that has passed through the charging chute 1 in the passing direction M and the diffusion direction N perpendicular to the passing direction M. In the diffusion section 2, the dimension of the bottom of the square pyramid in the diffusion direction N is larger than the dimension of the cylinder diameter of the charging chute 1. As shown in FIG. 1, the diffusion direction N corresponds to the furnace width direction of the vertical carbonization furnace 20. As shown in FIG. 2, the chute extension section 3 is provided so as to extend and protrude into the furnace of the vertical carbonization furnace 20. The chute extension section 3 charges the carbon-containing material after diffusion in the diffusion section 2 into the vertical carbonization furnace 20 .
[0019] In the first embodiment, a charging chute 1, a diffusion section 2, a chute extension section 3, and a vertical carbonization furnace 20 are provided in this order from upstream to downstream along a feeding direction M of a carbon-containing material shown in Fig. 2. As shown in Fig. 2, the charging chute 1, the diffusion section 2, and the chute extension section 3 of the charging device 9 are inclined at an inclination angle θ with respect to a depth direction P. Therefore, the carbon-containing material passing through the charging chute 1 flows down along the charging chute 1, the diffusion section 2, and the chute extension section 3 due to the inclination having the inclination angle θ, and is finally charged into the vertical carbonization furnace 20.
[0020] The opening / closing section 1a provided on the charging chute 1 is shown in a closed state in FIG. 2. By closing the charging chute 1 with the opening / closing section 1a, the carbon-containing material that has passed through the inside of the charging chute 1 can be temporarily stored upstream of the opening / closing section 1a. By closing the charging chute 1 with the opening / closing section 1a, for example, one batch of carbon-containing material can be stored upstream of the opening / closing section 1a. By changing the charging chute 1 from the closed state to the open state by the opening / closing section 1a, the carbon-containing material stored inside the charging chute 1 is released toward the diffusion section 2.
[0021] The configuration shown as the first embodiment, i.e., the configuration in which the charging chute 1, the diffusion section 2, and the chute extension section 3 are provided in this order, makes it possible to improve the distribution of the carbon-containing material in the vertical carbonization furnace when the carbon-containing material is fed through the charging chute 1 by providing the chute extension section 3. As a result of the improved distribution of the carbon-containing material in the furnace, the strength of the ferro-coke after carbonization can be improved.
[0022] <Second embodiment> Next, the configuration of the charging device 10 according to the second embodiment of the present invention will be described with reference to Figs. 3 and 4. The same components as those shown in the first embodiment are given the same numbers in the drawings and will not be described. Fig. 3 shows a schematic perspective view of the charging device 10 and the vertical carbonization furnace 20. Fig. 4 shows a schematic side view of the charging device 10 and the vertical carbonization furnace 20. As shown in Figs. 3 and 4, the charging device 10 in the second embodiment is configured by providing a step portion 5 to the charging device 9 in the first embodiment.
[0023] The step section 5 is provided between the diffusion section 2 and the chute extension section 3. The step section 5, downstream of the diffusion section 2, provides a drop in the feeding direction M toward the chute extension section 3 to the carbon-containing material diffused in the diffusion section 2. The drop is the distance between the top side of the step section 5 and the bottom side on the downstream side in the feeding direction M.
[0024] In the second embodiment, the charging chute 1, the diffusion section 2, the step section 5, the chute extension section 3, and the vertical carbonization furnace 20 are provided in this order from upstream to downstream along the direction M of the carbon-containing material flow shown in FIG. 3. The direction M of the carbon-containing material flow is inclined at an inclination angle θ with respect to the depth direction P in the horizontal direction of the vertical carbonization furnace 20. As shown in FIG. 4, the charging chute 1, the diffusion section 2, the step section 5, and the chute extension section 3 of the charging device 10 are inclined at an inclination angle θ with respect to the depth direction P. For this reason, the carbon-containing material passing through the charging chute 1 flows down along the charging chute 1, the diffusion section 2, the step section 5, and the chute extension section 3 due to the inclination having the inclination angle θ, and is finally charged into the vertical carbonization furnace 20.
[0025] Using the configuration shown in FIG. 4 which is the present embodiment and the configuration shown in FIG. 5 which does not include the step portion 5 and the chute extension portion 3, the molded carbon-containing material was charged into the vertical carbonization furnace 20, and the distribution of the carbon-containing material in the depth direction P of the furnace was measured. The chute extension portion 3 had a length w of 500 mm, and the step portion 5 had a drop of 40 mm. The charging device 10 used was the same as that used in the actual machine. The measurement was performed by installing a recovery box likened to the vertical carbonization furnace 20 at the outlet side of the charging chute 1.
[0026] The measurement was performed by first measuring the weight of the carbon-containing material at each position in the depth direction P at the bottom of the vertical carbonization furnace 20 when the carbon-containing material was charged from the charging chute 1 for a certain period of time. Then, the distribution of fine particles was measured from the measured weight. The weight was measured by dividing the depth direction P at the bottom of the vertical carbonization furnace 20 into eight regions and measuring the weight of the carbon-containing material for each divided region. The measurement of the distribution of the carbon-containing material in the depth direction P at the bottom of the furnace was performed when the weight (charge amount) of the carbon-containing material charged from the charging chute 1 per batch was set to 250 kg and 500 kg, respectively.
[0027] FIG. 6 shows the results of measuring the distribution of carbon-containing materials in the depth direction P of the furnace using a configuration (see FIG. 5) without the step portion 5 and the chute extension portion 3. FIG. 6(a) shows the weight ratio of the carbon-containing material for eight regions in the depth direction P of the furnace bottom of the vertical carbonization furnace 20. FIG. 6(b) shows the weight ratio of fine particles of the carbon-containing material for eight regions in the depth direction P of the furnace bottom of the vertical carbonization furnace 20. In FIG. 6(a), the vertical axis shows the weight ratio (%) of the carbon-containing material, and the horizontal axis shows the eight regions in the depth direction P from the charging device 10 side "1" to the opposite side of the charging device 10 "8". In FIG. 6(b), the vertical axis shows the weight ratio (%) of fine particles of the carbon-containing material, and the horizontal axis shows the eight regions in the depth direction P from the charging device 10 side "1" to the opposite side of the charging device 10 "8".
[0028] The weight ratio (%) of fine particles of the carbon-containing material was calculated by recovering the carbon-containing material from each of eight regions in the depth direction P, sieving the recovered carbon-containing material, and classifying the material with sieve openings of 20 mm or more as molded products and the material with sieve openings of less than 20 mm as fine particles.
[0029] As shown in Fig. 6(a), when the step section 5 and the chute extension section 3 were not provided downstream of the diffusion section 2, it was confirmed that the carbon-containing material was unevenly dispersed in the depth direction P. Also, as shown in Fig. 6(b), when the step section 5 and the chute extension section 3 were not provided downstream of the diffusion section 2, it was confirmed that the fine particles were unevenly distributed on the charging device 10 side.
[0030] FIG. 7 shows the results of measuring the distribution of carbon-containing materials in the depth direction P of the furnace using the configuration (see FIG. 4) in which the step portion 5 and the chute extension portion 3 are provided according to this embodiment. FIG. 7(a) shows the weight ratio of the carbon-containing material for eight regions in the depth direction P of the furnace bottom of the vertical carbonization furnace 20. FIG. 7(b) shows the weight ratio of fine particles of the carbon-containing material for eight regions in the depth direction P of the furnace bottom of the vertical carbonization furnace 20. In FIG. 7(a), the vertical axis shows the weight ratio (%) of the carbon-containing material, and the horizontal axis shows eight regions in the depth direction P from the charging device 10 side "1" to the opposite side of the charging device 10 "8". In FIG. 7(b), the vertical axis shows the weight ratio (%) of fine particles of the carbon-containing material, and the horizontal axis shows eight regions in the depth direction P from the charging device 10 side "1" to the opposite side of the charging device 10 "8".
[0031] As shown in Figure 7(a), when the step section 5 and the chute extension section 3 were provided downstream of the diffusion section 2, it was confirmed that the carbon-containing material was efficiently and almost uniformly dispersed in the depth direction P. Also, as shown in Figure 7(b), when the step section 5 and the chute extension section 3 were provided downstream of the diffusion section 2, it was confirmed that the fine particles were efficiently and almost uniformly dispersed without being unevenly concentrated in a specific position.
[0032] Next, in the present embodiment shown in FIG. 4, the distribution of carbon-containing materials at the bottom of the vertical carbonization furnace 20 was confirmed when the drop of the step portion 5 was changed. Regarding the distribution, first, the weight ratio (%) of fine particles was calculated for each of eight regions in the depth direction P of the bottom of the vertical carbonization furnace 20 for each drop of the step portion 5. Then, an average value was calculated, which was the average of the weight ratio (%) of fine particles for each of the eight regions. After that, a total average value of all the average values for each calculated drop was calculated, and the maximum deviation of the average value for each drop from the total average value was calculated (hereinafter, referred to as "deviation (%) of carbon-containing materials" in FIG. 8).
[0033] FIG. 8 shows the relationship between the drop of the step portion 5 and the deviation of the carbon-containing material. In FIG. 8, the vertical axis represents the deviation of the carbon-containing material (%), and the horizontal axis represents the drop of the step portion 5 (mm). As shown in FIG. 8, considering that the allowable range of the deviation of the carbon-containing material is 5% or less, it was confirmed that the deviation of the carbon-containing material becomes large when the drop of the step portion 5 is less than 30 mm or when the drop exceeds 60 mm. In other words, it was confirmed that the distribution of fine particles of the carbon-containing material in the furnace can be more efficiently made almost uniform by setting the drop of the step portion 5 to be 30 mm or more and 60 mm or less.
[0034] Next, in the present embodiment shown in Fig. 4, the distribution of carbon-containing materials at the bottom of the vertical carbonization furnace 20 was confirmed when the length of the chute extension portion 3 was changed. Specifically, the length of the chute extension portion 3 in the feed direction M was set to w, and the depth dimension of the vertical carbonization furnace 20 in the depth direction P was set to W. The distribution of carbon-containing materials at the bottom of the vertical carbonization furnace 20 was confirmed when the length w of the chute extension portion 3 was changed.
[0035] Regarding the distribution, first, for each length w of the chute extension 3, the value obtained by dividing the length w of the chute extension 3 by the depth dimension W of the vertical carbonization furnace 20 (w / W: hereinafter referred to as "w / W") was calculated. Then, for each w / W, the average value of the weight ratio (%) of the molded product for each of the eight regions in the depth direction P of the bottom of the vertical carbonization furnace 20 was calculated. Then, the overall average value, which is the average of all the average values for each of the eight regions, was calculated. After that, the total average value of all the calculated overall average values for each w / W was calculated, and the maximum deviation of the overall average value for each w / W from the total average value (hereinafter referred to as "deviation of weight ratio (%)" in the following description and in FIG. 7) was calculated.
[0036] Figure 9 shows the relationship between w / W and the deviation in weight ratio. In Figure 9, the vertical axis shows the deviation in weight ratio (%), and the horizontal axis shows w / W (-(dimensionless number)). As Figure 9 shows, considering that the allowable range for deviation in weight ratio is 5% or less, it was confirmed that the deviation in weight ratio becomes large when w / W is less than 0.27 or when w / W is 0.47 or more. In other words, it was confirmed that by setting w / W at least 0.27 and less than 0.47 (0.27≦w / W<0.47), it is possible to more efficiently and approximately evenly distribute the molded carbon-containing material in the furnace.
[0037] Next, using the configuration shown in Fig. 4 which is the present embodiment and the configuration shown in Fig. 5 which does not have the step portion 5 and the chute extension portion 3, the molded carbon-containing material was charged into a vertical carbonization furnace 20, and the strength of each ferro-coke produced by carbonization in the vertical carbonization furnace 20 was measured. The measurement was performed according to the rotational strength test method described in JIS K2151, and the strength of the ferro-coke was measured using the DI 150 15 (hereinafter referred to as "DI") was measured.
[0038] The measurement results of the strength of ferro-coke are shown in Fig. 10. As shown in Fig. 10, it was confirmed that by charging a carbon-containing material into a vertical carbonization furnace 20 and producing ferro-coke in a configuration in which the step portion 5 and the chute extension portion 3 are provided in the charging device 10 ("present invention" in Fig. 10), the strength of the ferro-coke was efficiently improved compared to a configuration in which the step portion 5 and the chute extension portion 3 are not provided ("conventional" in Fig. 10).
[0039] Here, in this embodiment, as shown in Figures 3 and 4, a configuration in which multiple rows of the charging devices 10 are arranged on one side in the depth direction P of the vertical carbonization furnace 20 is shown as an example of the charging device 10, but the present invention is not limited to this configuration. In other words, as shown in Figure 11, a configuration in which the charging devices 10 are arranged on both sides of the vertical carbonization furnace 20 in the depth direction P of the vertical carbonization furnace 20 may be used.
[0040] <Third embodiment> Next, the configuration of the charging device 30 according to the third embodiment of the present invention will be described with reference to Figs. 12 and 13. The same components as those shown in the first and second embodiments are given the same numbers in the drawings, and the description will be omitted. Fig. 12 shows a schematic perspective view of the charging device 30 and the vertical carbonization furnace 20. Fig. 13 shows a schematic top view of the charging device 30 and the vertical carbonization furnace 20. As shown in Figs. 12 and 13, the charging device 30 according to the third embodiment is configured such that the step portion 5 is not provided, compared to the charging device 10 according to the second embodiment.
[0041] In the third embodiment, as shown in Fig. 12, a charging chute 1, a diffusion section 2, a chute extension section 3, and a vertical carbonization furnace 20 are provided in this order from upstream to downstream in the direction in which the carbon-containing material flows down. Only the charging chute 1 is inclined at an inclination angle θ with respect to the depth direction P in the horizontal direction of the vertical carbonization furnace 20. In other words, only the direction in which the carbon-containing material flows down inside the charging chute 1 corresponds to the feeding direction M. Also, as shown in Fig. 12, the diffusion section 2 is provided on a horizontal surface, and the chute extension section 3 is arranged to extend in the depth direction P in the horizontal direction.
[0042] 12 and 13, in the third embodiment, the chute extension 3 has a comb-tooth shape extending in the depth direction P. In order to more efficiently improve the effect of uniformly dispersing the carbon-containing material in the vertical carbonization furnace 20, the width L of each comb blade and the distance D between adjacent comb blades are desirably 50 mm or more and 200 mm or less. If the width L of each comb blade is less than 50 mm, the carbon-containing material passing over the comb blade is likely to fall near the base of the comb blade (near the inlet of the vertical carbonization furnace 20), and uniform dispersion of the carbon-containing material at the bottom of the vertical carbonization furnace 20 cannot be performed more efficiently. On the other hand, if the width L of the comb blade alone exceeds 200 mm, the powder contained in the carbon-containing material that has passed over the comb blade will be more likely to fly to a position away from the loading device 30 in the furnace space of the vertical carbonization furnace 20, making it difficult to efficiently distribute the carbon-containing material evenly at the bottom of the furnace.
[0043] Regarding the distance D between adjacent comb blades, if it is less than 50 mm, it becomes difficult for the carbon-containing material to be supplied to the vicinity of the base of the comb blade, and it becomes difficult to efficiently distribute the carbon-containing material evenly at the bottom of the vertical carbonization furnace 20. On the other hand, if the distance D between adjacent comb blades exceeds 200 mm, it becomes easy for the carbon-containing material passing over the comb blade to fall near the base of the comb blade, and it becomes difficult to efficiently distribute the carbon-containing material evenly at the bottom of the vertical carbonization furnace 20.
[0044] In the third embodiment, the value obtained by dividing the length x of the chute extension 3 in the depth direction P by the depth dimension W of the vertical carbonization furnace 20 (x / W: hereinafter referred to as "x / W") preferably satisfies the relationship of 0.20≦x / W≦0.50. This is because, if x / W is less than 0.20, the length x of the chute extension 3 in the depth direction P becomes short, and the carbon-containing material cannot be uniformly dispersed in the vertical carbonization furnace 20 more efficiently. On the other hand, if x / W exceeds 0.50, even if the length x of the chute extension 3 in the depth direction P is increased, an effect exceeding that in the state of x / W=0.50 cannot be obtained. This is because most of the carbon-containing material passing over the comb blade falls into the vertical carbonization furnace 20 before reaching the tip of the chute extension 3 in the state of x / W=0.50.
[0045] In order to increase the probability that the carbon-containing material passing over the comb blade reaches the tip of the chute extension 3, the cross-sectional shape of the chute extension 3 may be multi-stage (for example, if there are two stages, a convex shape is preferable) or trapezoidal. However, even in this case, it is preferable that the width L of the comb blade itself is 50 mm or more and 200 mm or less.
[0046] As described above, the first to third embodiments of the charging device according to the present invention have been described. In these embodiments, the case of producing ferro coke as a raw material for a blast furnace has been described as an example, but the raw material for a blast furnace is not limited to ferro coke. In other words, the charging device and vertical carbonization furnace according to the present invention may be used to produce raw materials for a blast furnace as a method for producing various cokes. EXAMPLES
[0047] Hereinafter, examples carried out using the charging device according to this embodiment will be described.
[0048] <Example 1> Using the charging device 9 (see FIG. 1) shown as the first embodiment and the charging device 10 (see FIG. 3) shown as the second embodiment, the strength of ferro-coke was measured when the charging weight (kg) to the vertical carbonization furnace 20 was changed. In the comparative example, a configuration without the step portion 5 or the chute extension portion 3 was used, and the strength of ferro-coke was measured when the charging weight to the vertical carbonization furnace 20 was changed.
[0049] The measurement was carried out by carbonizing the carbon-containing material in the vertical carbonization furnace 20, and then sampling ferro-coke at 10 locations in the furnace width direction Q of the vertical carbonization furnace 20 to measure the strength of the ferro-coke and confirm the maximum and minimum values of the strength. The strength was measured according to the rotational strength test method described in JIS K2151, and the DI 150 15 (hereinafter referred to as "DI") was measured.
[0050] [Table 1]
[0051] Table 1 shows the results (invention examples 1 to 4) of measuring the strength of ferro coke produced using the charging device 9 in the first embodiment. Also shown are the results (invention examples 5 to 12) of measuring the strength of ferro coke produced using the charging device 10 in the second embodiment. As shown in Table 1, in invention examples 1 to 4 having the chute extension 3, the strength (maximum and minimum) of the ferro coke was 72 or more under all conditions. In other words, it was confirmed that the distribution of carbon-containing substances in the vertical carbonization furnace 20 can be improved, and the strength of the ferro coke after carbonization can be improved. In addition, in invention examples 5 to 12 having the step portion 5 and the chute extension 3, the strength (maximum and minimum) of the ferro coke was 77 or more under all conditions. In invention examples 5 to 12, the variation in the maximum and minimum values was small, and it was confirmed that high-quality ferro coke can be produced. That is, it was confirmed that the distribution of carbon-containing substances in the vertical carbonization furnace 20 can be efficiently improved, and the strength of the ferro-coke after carbonization can be efficiently improved.
[0052] On the other hand, it was confirmed that in Comparative Examples 1 to 4 in which the chute extension 3 was not provided, the strength of the ferro-coke was lower than those in Invention Examples 1 to 12, and the variation in the strength (maximum and minimum values) of the ferro-coke was also large.
[0053] <Example 2> Next, a test device simulating a charging device 30 (see FIG. 12) having a charging chute 1, a diffusion section 2, and a comb-tooth-shaped chute extension section 3 shown as the third embodiment was used to investigate the distribution of the charging material in the depth direction P of the bottom of the vertical carbonization furnace 20 when a molded carbon-containing material was charged. The charging device 30 in this embodiment had the same shape as that installed in the actual machine. In addition, as the vertical carbonization furnace 20 in this embodiment, a recovery box was installed on the outlet side of the charging device 30 to resemble a carbonization furnace.
[0054] In the investigation, a certain amount of carbon-containing material was charged from the charging chute 1, and then the distribution of the carbon-containing material present in the bottom of the recovery box, which was divided into 4 equal parts in the depth direction and 5 equal parts in the width direction (total of 20 equal parts), was investigated. Specifically, the carbon-containing material was collected from each of the 20 equal parts, and the collected carbon-containing material was sieved with a 20 mm mesh, and the over-sieve (diameter 20 mm or more) was classified as a molded product, and the under-sieve (diameter less than 20 mm) was classified as a powder. Then, the weights of the molded product and the powder were measured, and the "powder ratio" (weight ratio (%) of the powder in the contents of each region) was calculated. Although the powder ratio was obtained for each of the 20 equal parts, in Figs. 14 to 16 described later, the "maximum powder ratio (%)" is shown as an index of powder segregation. The maximum powder ratio is the maximum value of the powder ratio obtained by comparing the powder ratios of the 20 equal parts.
[0055] FIG. 14 shows the results of investigating the relationship between the width L of the individual comb blades of the chute extension 3 and the maximum powder ratio. In FIG. 14, the vertical axis indicates the maximum powder ratio (%), and the horizontal axis indicates the width L (mm) of the individual comb blades of the chute extension 3. The weight of the carbon-containing material charged into the charging chute 1 was 250 kg, the length x of the individual comb blades of the chute extension 3 in the depth direction P was 500 mm (x / W: 0.33), and the distance D between the comb blades was 100 mm. As shown in FIG. 14, it was confirmed that in order to improve the dispersibility of the powder more efficiently and to achieve the maximum allowable powder ratio (40% or less), it is preferable to set the width L of the individual comb blades of the chute extension 3 to 50 mm or more and 200 mm or less.
[0056] Next, the results of investigating the relationship between the distance D between the comb blades of the chute extension 3 and the maximum powder ratio are shown in FIG. 15. In FIG. 15, the vertical axis indicates the maximum powder ratio (%), and the horizontal axis indicates the distance D (mm) between the comb blades of the chute extension 3. As in the case shown in FIG. 14, the weight of the carbon-containing material charged into the charging chute 1 was 250 kg, the length x of the comb blades of the chute extension 3 in the depth direction P was 500 mm (x / W: 0.33), and the distance D between the comb blades was 100 mm. As shown in FIG. 15, it was confirmed that in order to improve the dispersion of the powder more efficiently and to achieve the maximum allowable powder ratio (40% or less), it is preferable to set the distance D between the comb blades of the chute extension 3 to 50 mm or more and 200 mm or less, the same as the width L of the comb blades.
[0057] FIG. 16 shows the results of an investigation into the relationship between the ratio (x / W) of the length x in the depth direction P of the chute extension 3 to the depth dimension W of the vertical carbonization furnace 20 and the maximum powder ratio. The weight of the carbon-containing material charged into the charging chute 1 was 250 kg, and the width L of each comb blade of the chute extension 3 and the distance D between the comb blades were both 100 mm. As shown in FIG. 16, it was confirmed that in order to improve the dispersion of the powder more efficiently and to achieve the maximum allowable powder ratio (40% or less), it is preferable that the ratio (x / W) of the length x in the depth direction P of the chute extension 3 to the depth dimension W of the vertical carbonization furnace 20 be 0.20 or more and 0.50 or less. Furthermore, it was confirmed that even if the length x in the depth direction P of the chute extension portion 3 is further extended and the ratio (x / W) of the length x in the depth direction P of the chute extension portion 3 to the depth dimension W of the vertical dry distillation furnace 20 exceeds 0.50, the effect obtained when x / W is 0.50 cannot be improved more efficiently. [Explanation of symbols]
[0058] 1 Charging chute 1a Opening and closing section 2 Diffusion section 3. Chute extension 5 Step 9, 10, 30 charging device 20 Vertical carbonization furnace D Distance between teeth L Width of the comb blade alone M Feeding direction N Diffusion direction P Depth direction Q Furnace width direction θ Tilt angle
Claims
1. A charging device for charging a carbon-containing material into a vertical carbonization furnace, comprising: A cylindrical charging chute through which the carbon-containing material passes; a diffusion section that diffuses the carbon-containing material that has passed through the charging chute in a direction in which the carbon-containing material passes and in a diffusion direction perpendicular to the direction in which the carbon-containing material passes; a chute extension portion for charging the carbon-containing material after diffusion in the diffusion portion into the vertical carbonization furnace and projecting into the furnace; a step portion downstream of the diffusion portion that provides a drop in the feeding direction toward the chute extension portion to the carbon-containing material diffused in the diffusion portion, A charging device, wherein the length w of the chute extension portion in the feeding direction satisfies the relationship 0.27≦w / W<0.47, where W is the depth dimension of the vertical carbonization furnace.
2. The charging device according to claim 1, wherein the drop of the step portion is 30 mm or more and 60 mm or less.
3. The charging device according to claim 1 , wherein the chute extension portion extends in a comb-tooth shape in a depth direction of the vertical carbonization furnace.
4. The charging device according to claim 3, wherein the width of each comb blade and the distance between adjacent comb blades in the chute extension portion are 50 mm to 200 mm.
5. The charging device according to claim 3, wherein the length x of the chute extension in the depth direction satisfies a relationship of 0.20≦x / W≦0.50, where W is a depth dimension of the vertical carbonization furnace.
6. The charging device according to claim 4, wherein the length x of the chute extension in the depth direction satisfies a relationship of 0.20≦x / W≦0.50, where W is a depth dimension of the vertical carbonization furnace.
7. A method for producing raw materials for a blast furnace, comprising the steps of: producing raw materials for a blast furnace using the charging device according to any one of claims 1 to 6 and the vertical carbonization furnace.
Citation Information
Patent Citations
U - an oven charging device
JP1983056048U
Powder dispersing device
JP1994191615A
Method and apparatus for producing ferrocoke
JP2011057970A
Bulk material carrying device
JP2011162271A
Reduction furnace and iron smelting apparatus including the same
JP2011508074A