Forming history monitoring device, manufacturing system for molded object, and forming history monitoring method

The molding history monitoring device and method address the challenge of defect estimation in additive manufacturing by analyzing weld bead profiles and characteristics, enabling reliable detection and repair of defects in weld bead formations.

JP7572256B2Active Publication Date: 2024-10-23KOBE STEEL LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021013390
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-01-29
Publication Date
2024-10-23
Estimated Expiration
2041-01-29

AI Technical Summary

Technical Problem

Existing techniques for determining welding quality, such as those in Patent Documents 1 and 2, are not applicable to additive manufacturing where weld beads are repeatedly formed on an existing base without side walls, making it difficult to estimate defects reliably.

Method used

A molding history monitoring device and method that estimate defects by acquiring shape profiles and welding information from existing and adjacent weld beads, determining angular features and welding characteristics, and extracting defect candidates based on threshold values.

Benefits of technology

Enables highly reliable estimation of defects in repeatedly formed weld beads, allowing for quick identification and repair of defective parts in the manufacturing process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007572256000001
    Figure 0007572256000001
  • Figure 0007572256000002
    Figure 0007572256000002
  • Figure 0007572256000003
    Figure 0007572256000003
Patent Text Reader

Abstract

To provide a molding history monitoring device that can estimate a defect of a molding having weld beads repeatedly formed, with high reliability, a molding manufacturing system, and a molding history monitoring method.SOLUTION: A molding history monitoring device comprises a shape sensor 25 that obtains a profile of a shape disposed along an extending direction of an existing weld bead 29A. A control part 21 has: welding-information obtaining means that obtains welding-information during formation of an adjacent weld bead 29B, when forming the adjacent weld bead 29B at a position adjacent to the existing weld bead 29A; and defect-candidate extracting means that determines an angle characterizing portion Rc having a an angle θ of a root which is equal to or more than a threshold in the existing weld bead 29A, on the basis of the profile of a shape, determines weld characterizing portion Wc of the welding-information, on the basis of the welding-information, and extracts the weld characterizing portion Wc corresponding to the angle characterizing portion Rc as a defect candidate F, associating the weld characterizing portion with the angle characterizing portion Rc.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a molding history monitoring device, a manufacturing system for a molded object, and a molding history monitoring method. [Background technology]

[0002] Patent Document 1 discloses a technology for performing welding operations in which a number of visual sensors are used to obtain multiple pieces of information relating to the extension length of the welding wire, the shape of the molten pool, and the behavior of the welder, and the quality of the welding operations is judged based on this information.

[0003] Furthermore, Patent Document 2 discloses a technology for determining the quality of butt welding from the shape of the weld bead generated when butt welding metal plate materials using high energy density welding, based on the cross-sectional shape acquired by a cross-section reading sensor that acquires the two-dimensional cross-sectional shape of the weld bead formed in the groove. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2008-110388 A [Patent Document 2] JP 2008-212944 A Summary of the Invention [Problem to be solved by the invention]

[0005] Incidentally, in additive manufacturing, in which a heat source such as a laser or an arc is used to melt metal powder or metal wire to form a weld bead to form a shaped object, the weld bead is repeatedly layered, and the shaped object accumulates heat. In additive manufacturing, an existing weld bead is used as the base, rather than a regular base with walls supporting the bead from both sides, as in a groove, and the next weld bead is formed along the existing weld bead. Therefore, it is difficult to apply the techniques of Patent Documents 1 and 2, which judge the quality of welding to a regular base with walls supporting the bead from both sides, as in a groove, to additive manufacturing.

[0006] Therefore, an object of the present invention is to provide a molding history monitoring device, a manufacturing system for a molded object, and a molding history monitoring method that are capable of reliably estimating defects in a molded object in which weld beads are repeatedly formed. [Means for solving the problem]

[0007] The present invention comprises the following configurations. (1) A manufacturing history monitoring device that estimates defects from history information when a plurality of weld beads are formed by melting and solidifying a filler metal by a torch to manufacture a molded object, comprising: A shape profile acquisition means for acquiring a shape profile along an extension direction of an existing weld bead; a welding information acquisition means for acquiring welding information during the formation of an adjacent weld bead when the adjacent weld bead is formed at a position adjacent to the existing weld bead; a defect candidate extraction means for identifying an angle feature having a root angle equal to or greater than a threshold in the existing weld bead based on the shape profile, and for identifying a welding feature of the welding information based on the welding information, and for associating the welding feature corresponding to the angle feature with the angle feature and extracting it as a defect candidate; having Modeling history monitoring device. (2) A system for manufacturing objects that manufactures objects by moving a torch and forming a weld bead by melting and solidifying a filler metal with the torch, the system being equipped with the manufacturing history monitoring device described in (1) above. (3) A manufacturing history monitoring method for estimating defects from history information when a plurality of weld beads are formed by melting and solidifying a filler metal by a torch to manufacture a molded object, comprising the steps of: A shape profile acquisition process for acquiring a shape profile along an extension direction of an existing weld bead; a welding information acquisition process for acquiring welding information during the formation of an adjacent weld bead when forming an adjacent weld bead at a position adjacent to the existing weld bead; a defect candidate extraction process for identifying an angle feature having a root angle equal to or greater than a threshold in the existing weld bead based on the shape profile, identifying a welding feature of the welding information based on the welding information, and associating the welding feature corresponding to the angle feature with the angle feature and extracting it as a defect candidate; Including, A method for monitoring build history. Effect of the Invention

[0008] The present invention can estimate with high reliability defects in a molded object in which welding beads are repeatedly formed. [Brief description of the drawings]

[0009] [Figure 1] 1 is a schematic diagram illustrating a manufacturing system according to an embodiment of the present invention. [Diagram 2] FIG. 1 shows a weld bead formed by overlapping, where (A) is a schematic cross-sectional view showing a case where the root angle of the existing weld bead is small, and (B) is a schematic cross-sectional view showing a case where the root angle of the existing weld bead is large. [Diagram 3] FIG. 13 is a perspective view showing the formation of an adjacent weld bead along an existing weld bead. [Figure 4]FIG. 2 is an explanatory diagram illustrating a root angle of an existing weld bead and a welding voltage profile of an adjacent weld bead; [Diagram 5] FIG. 11 is a perspective view showing a state in which a weld bead is formed along an existing weld bead. [Figure 6] FIG. 2 is a perspective view illustrating a molten pool formed in a weld bead. [Figure 7] 1A and 1B are diagrams for explaining the change in the shape of a molten pool, in which (A) is a perspective view of a state in which a bulge is formed, and (B) is a perspective view of a state in which a depression is formed. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. FIG. 1 is a schematic diagram showing the configuration of a system 100 for manufacturing a molded object that includes a molding history monitoring device according to the present invention. The manufacturing system 100 for a molded object having this configuration includes a welding robot 11, a robot controller 13, a filler metal supply unit 15, a welding power source 19, and a control unit 21.

[0011] The welding robot 11 is an articulated robot, and a torch 23 is supported on the tip shaft. The position and posture of the torch 23 can be set arbitrarily in three dimensions within the range of the degrees of freedom of the robot arm. The torch 23 holds the filler material (welding wire) M, which is continuously supplied from a filler material supply unit 15, in a state where it protrudes from the tip of the torch. The tip shaft of the welding robot 11 is provided with the torch 23 and a shape sensor 25.

[0012] The torch 23 has a shield nozzle (not shown) through which a shield gas is supplied to the welded portion. The arc welding method may be either a consumable electrode type such as shielded metal arc welding or carbon dioxide gas arc welding, or a non-consumable electrode type such as TIG welding or plasma arc welding, and is appropriately selected depending on the object to be produced.

[0013] For example, in the case of a consumable electrode type, a contact tip is disposed inside the shield nozzle, and a filler material M to which a melting current is supplied is held by the contact tip. The torch 23 holds the filler material M and generates an arc from the tip of the filler material M in a shielding gas atmosphere. The filler material M is fed to the torch 23 by a feeding mechanism (not shown) attached to a robot arm or the like. Then, as the torch 23 moves, the continuously fed filler material M is melted and solidified, and a weld bead 29, which is a molten and solidified body of the filler material M, is formed on the base plate 27.

[0014] The base plate 27 is made of a metal plate such as a steel plate, and is basically larger than the bottom surface (the surface of the lowest layer) of the model W. The base plate 27 is not limited to a plate shape, and may be a base of other shapes such as a block or a rod.

[0015] The heat source for melting the filler metal M is not limited to the above-mentioned arc. For example, other types of heat sources may be used, such as a heating method using both an arc and a laser, a heating method using plasma, or a heating method using an electron beam or a laser. When heating with an electron beam or a laser, the amount of heat can be controlled more precisely, and the state of the weld bead can be more appropriately maintained, which contributes to further improving the quality of the molded product.

[0016] Any commercially available welding wire can be used as the filler metal M. For example, wires specified in MAG and MIG welding solid wires for mild steel, high tensile steel and low temperature steel (JIS Z 3312), arc welding flux-cored wires for mild steel, high tensile steel and low temperature steel (JIS Z 3313), etc. can be used.

[0017] An active metal such as titanium can be used as the filler metal M. In that case, it is necessary to place the weld in a shielding gas atmosphere to prevent oxidation and nitridation due to reaction with the atmosphere during welding.

[0018] Shape sensor 25 is provided alongside torch 23 and moves together with torch 23. This shape sensor 25 is a sensor that measures the shape of a base portion when forming weld bead 29. As shape sensor 25, for example, a laser sensor that acquires reflected light of irradiated laser light as height data is used. Note that as shape sensor 25, a three-dimensional shape measuring camera may also be used.

[0019] The robot controller 13 receives instructions from the control unit 21 to drive each part of the welding robot 11 and controls the output of the welding power source 19 as necessary.

[0020] The control unit 21 is configured with a computer device equipped with a CPU, memory, storage, etc., and executes a drive program prepared in advance or a drive program created under desired conditions to drive each part such as the welding robot 11. As a result, the torch 23 is moved according to the drive program, and multiple layers of weld beads 29 are stacked on a base plate 27 based on the created stacking plan, thereby forming a multi-layered object W. A database 17 is also connected to the control unit 21. This database 17 stores and accumulates history information including defect candidates extracted by the control unit 21, which will be described later.

[0021] Incidentally, the width and height of the weld bead 29 formed when forming the object W varies depending on the fluidity of the material, the melting conditions, etc. As a result, when forming the weld bead 29 adjacent to an existing weld bead 29 in forming the object W, there is a risk of defects occurring in the overlapping portion between the adjacent weld beads 29.

[0022] Figure 2 shows a weld bead formed by overlapping, where (A) is a schematic cross-sectional view showing a case where the root angle θ of the existing weld bead 29A is small, and (B) is a schematic cross-sectional view showing a case where the root angle θ of the existing weld bead 29A is large.

[0023] As shown in Fig. 2A, when the root angle θ of the existing weld bead 29A is small, when an adjacent weld bead 29B is formed by overlapping the existing weld bead 29A, the occurrence rate of defects between these weld beads 29A and 29B is low. In contrast, as shown in Fig. 2B, when the root angle θ of the existing weld bead 29A is large, when an adjacent weld bead 29B is formed by overlapping the existing weld bead 29A, the molten metal does not flow sufficiently to the root of the existing weld bead 29A, and the occurrence rate of defects between these weld beads 29A and 29B increases. For example, when the root angle θ of the existing weld bead 29A is 40° or more, the occurrence rate of defects due to insufficient fusion between the weld beads 29A and 29B increases.

[0024] In addition, the occurrence rate of defects in the overlapping portion between adjacent weld beads 29 varies depending on the root angle θ of the existing weld bead 29A, as well as the welding conditions when forming the weld bead 29, such as the welding voltage, welding current, feed speed of the filler metal M, feed resistance of the filler metal M, shielding gas flow rate, and flow conditions of the molten pool.

[0025] For this reason, the manufacturing system 100 according to this embodiment includes a modeling history monitoring device that estimates defects in the adjacent weld beads 29A and 29B as described above.

[0026] This molding history monitoring device extracts defect candidates based on the measurement results from a shape sensor (shape profile acquisition means) 25 arranged in parallel with the torch 23, and welding information, which is information on the welding state such as the welding voltage, welding current, the feed rate of the filler metal M, and the flow state of the molten pool when forming the weld bead 29. The control unit 21 includes a welding information acquisition means and a defect candidate extraction means, and the welding information acquisition means acquires the welding information and the defect candidate extraction means extracts the defect candidates. Then, the control unit 21 stores the history information including the defect candidates in the database 17.

[0027] Next, extraction of defect candidates by the molding history monitoring device will be described. Here, a case will be described in which the welding voltage when forming a weld bead 29B adjacent to an existing weld bead 29A is used as welding information.

[0028] (Shape profile acquisition process) FIG. 3 is a perspective view showing how an adjacent weld bead 29B is formed along an existing weld bead 29A. 3, a weld bead 29B is formed adjacent to an existing weld bead 29A while moving the torch 23. At this time, the shape of the existing weld bead 29A is measured by a shape sensor 25 in front of the torch 23, and a shape profile along the extension direction of the weld bead 29A is obtained.

[0029] (Welding information acquisition process) When forming weld bead 29B adjacent to existing weld bead 29A, the welding voltage during the formation of weld bead 29B is acquired as welding information by the welding information acquisition means of control unit 21. Note that the welding information acquisition means of control unit 21 acquires the welding information by, for example, monitoring the output of welding power source 19.

[0030] (Defect candidate extraction process) The defect candidate extraction means of the control unit 21 extracts defect candidates. Specifically, first, the root angle θ of the open side of the existing weld bead 29A is determined based on the shape profile of the existing weld bead 29A acquired by the shape sensor 25, and a portion where the root angle θ is equal to or greater than a preset threshold is determined as the angle characteristic portion Rc. The threshold value of the root angle θ is, for example, 40°, at which defects are likely to occur.

[0031] Next, based on the welding information including the welding voltage acquired during the formation of the weld bead 29B at the adjacent position, the welding characteristic portion Wc of the welding information is determined. The welding characteristic portion Wc is a portion where the welding voltage has greatly fluctuated. For example, if an abnormal disturbance occurs in the waveform of the welding voltage, the arc may be disturbed or interrupted, which may have an undesirable effect on the fluidity of the molten metal. Therefore, by setting a threshold value for the instantaneous fluctuation value or the slope of the fluctuation based on the past abnormal waveform, a state where a defect is likely to occur is extracted as the welding characteristic portion Wc.

[0032] Then, the determined angle feature Rc is compared with the weld feature Wc, and the weld feature Wc corresponding to the angle feature Rc is associated with the angle feature Rc and extracted as a defect candidate F.

[0033] The historical information to be acquired in order to extract defect candidate F is, for example, information recorded over time (for each position) when the weld bead 29B is formed, with the coordinates X, Y, Z, root angle θ, and welding voltage V corresponding to each other.

[0034] FIG. 4 is an explanatory diagram that shows a schematic view of the root angle θ of an existing weld bead 29A and the profile of the welding voltage for an adjacent weld bead 29B. 4, the defect candidate extraction means of the control unit 21 determines an angle characteristic portion Rc when the root angle θ of the existing weld bead 29A is equal to or greater than a threshold value, and determines a welding characteristic portion Wc when the welding voltage of the adjacent weld bead 29B varies from a steady state. Then, the portion where the welding characteristic portion Wc occurs in the angle characteristic portion Rc is extracted as a defect candidate F, and history information including this defect candidate F (information for each position in which the coordinates X, Y, Z, the root angle θ, and the welding voltage V are associated with each other) is stored in the database 17.

[0035] As described above, according to the molding history monitoring device and molding history monitoring method of this embodiment, when there is a characteristic in the welding information of the adjacent weld bead 29B at a position corresponding to the angle characteristic portion Rc where the root angle θ of the existing weld bead 29A is equal to or greater than a threshold value, it is possible to extract a highly reliable defect candidate F by determining that the welding information of the adjacent weld bead 29B is characteristic.

[0036] Furthermore, according to the manufacturing system 100 for a molded object equipped with the molding history monitoring device, it is possible to easily grasp defective parts that may occur in the molded object W when molding the molded object W. As a result, it is possible to quickly repair defective parts of the molded object W after the molded object W is molded.

[0037] In addition, the defect candidate extraction means of the control unit 21 preferably performs an occurrence frequency calculation process for calculating the occurrence frequency of the defect candidate F in the defect candidate extraction process. By calculating the occurrence frequency of the defect candidate F in this way, it is possible to estimate the locations in the molded object W that should be precisely inspected based on the occurrence frequency of the defect candidate F. The occurrence frequency of the defect candidate F can be calculated using the number of times the defect candidate F appears during the formation of one weld bead 29 or the duration of the appearance of the defect candidate as an index. In addition, the defect candidate F may be divided into groups for forming a wall portion, filling the inside of a wall portion, forming an overhang portion, etc., with reference to information on the trajectory plan, and the occurrence frequency of the defect candidate F may be calculated for each group.

[0038] Furthermore, in the defect candidate extraction process, the defect candidate extraction means of the control unit 21 preferably estimates the defect size in the shaped object W from the appearance time of the defect candidate F and the moving speed of the torch 23 based on the appearance frequency of the defect candidate F. By estimating the defect size in the shaped object W in this manner, it is possible to easily grasp the defect that has occurred in the shaped object W without performing a complicated inspection such as a destructive inspection or an ultrasonic inspection. Furthermore, if the appearance frequency of the defect candidate F continues for a certain length, it can be estimated that a long and thin defect has appeared, and if it is very short, it can be estimated that the defect candidate is a minute defect or has appeared due to the influence of noise. Therefore, if the length of the appearance frequency of the defect candidate F is equal to or greater than a preset threshold, history information including the defect candidate F may be stored as defect information.

[0039] In the above embodiment, the welding voltage is used as the welding information for determining the welding characteristic portion Wc, but the welding information is not limited to the welding voltage. As the welding information, at least one of the welding voltage, welding current, feed speed of the filler metal M, feed resistance of the filler metal M, shield gas flow rate, and flow state of the molten pool may be used, and the welding voltage, welding current, feed speed of the filler metal M, and flow state of the molten pool may be used in combination.

[0040] Here, a case where the flow state of the molten pool is used as the welding information will be described. FIG. 5 is a perspective view showing how a weld bead 29B is formed along an existing weld bead 29A.

[0041] As shown in FIG. 5, when the flow state of the molten pool is used as welding information, a camera 26 for photographing the molten pool P is provided in parallel with a shape sensor 25 on the torch 23 .

[0042] When forming a weld bead 29B adjacent to an existing weld bead 29A, the shape of the existing weld bead 29A is measured by the shape sensor 25, and the molten pool P of the weld bead 29B is photographed by the camera 26, and the photographed data is acquired as welding information. Based on the welding information consisting of the photographed data, for example, a portion where the shape of the molten pool P has changed significantly is identified as the welding characteristic portion Wc. Note that the photographed data may be a digitalized version of the area of ​​the molten pool P.

[0043] Fig. 6 is a perspective view illustrating the molten pool P formed in the weld bead 29B. Fig. 7 is a diagram illustrating the variation in the shape of the molten pool P, in which (A) is a perspective view of a state in which a bulge Pb has been formed, and (B) is a perspective view of a state in which a depression Pk has been formed.

[0044] Fig. 6 shows a molten pool P with a normal shape. The molten pool P may vary significantly from the normal shape shown in Fig. 6. For example, the molten pool P may expand partially to form a bulging portion Pb as shown in Fig. 7(A), or may be recessed partially to form a depression portion Pk as shown in Fig. 7(B). The welding information acquisition means of the control unit 21 then identifies the portion of the weld bead 29B where the shape of the molten pool P has changed to form a bulging portion Pb or a depression portion Pk as a weld characteristic portion Wc.

[0045] Furthermore, the defect candidate extraction means of the control unit 21 compares the angle characteristic part Rc determined based on the shape profile of the existing weld bead 29A acquired by the shape sensor 25 with the welding characteristic part Wc determined based on the welding information consisting of the photographing data of the camera 26, and associates the welding characteristic part Wc corresponding to the angle characteristic part Rc with the angle characteristic part Rc and extracts it as a defect candidate F.

[0046] In this way, even when the flow condition of the molten pool P is used as the welding information, highly reliable defect candidates can be extracted by associating the welding feature portion Wc in the acquired welding information of the flow condition of the molten pool P with the angle feature portion Rc to obtain defect candidates F.

[0047] In addition, the flow condition of the molten pool P may be the temperature, brightness, etc., in which case a temperature sensor for detecting the temperature of the molten pool P and a brightness sensor for detecting the brightness of the molten pool P are arranged in parallel to the torch 23.

[0048] As such, the present invention is not limited to the above-described embodiments, and the present invention also contemplates mutual combinations of the various components of the embodiments, as well as modifications and applications by those skilled in the art based on the descriptions in the specification and well-known technologies, and these are included in the scope of protection sought.

[0049] As described above, the present specification discloses the following: (1) A manufacturing history monitoring device that estimates defects from history information when a plurality of weld beads are formed by melting and solidifying a filler metal by a torch to manufacture a molded object, comprising: A shape profile acquisition means for acquiring a shape profile along an extension direction of an existing weld bead; a welding information acquisition means for acquiring welding information during the formation of an adjacent weld bead when the adjacent weld bead is formed at a position adjacent to the existing weld bead; a defect candidate extraction means for identifying an angle feature having a root angle equal to or greater than a threshold in the existing weld bead based on the shape profile, and for identifying a welding feature of the welding information based on the welding information, and for associating the welding feature corresponding to the angle feature with the angle feature and extracting it as a defect candidate; The molding history monitoring device has the following features. According to this molding history monitoring device, a welding feature corresponding to an angle feature where the root angle of an existing weld bead is equal to or greater than a threshold is associated and extracted as a defect candidate. When forming an adjacent weld bead adjacent to an existing weld bead, if the root angle of the existing weld bead is large, there is a high risk of a defect occurring due to insufficient fluidity. Therefore, by determining as a defect candidate a case where there is a feature in the welding information of an adjacent weld bead at a position corresponding to an angle feature where the root angle of the existing weld bead is equal to or greater than a threshold, a highly reliable defect candidate can be extracted.

[0050] (2) The forming history monitoring device according to (1), wherein the welding information acquisition means acquires at least one of the welding voltage, welding current, filler metal feed speed, filler metal feed resistance, shielding gas flow rate, and flow condition of the molten pool as the welding information. According to this manufacturing history monitoring device, highly reliable defect candidates can be extracted by associating welding features in at least one of the acquired welding information, i.e., welding voltage, welding current, filler metal feed rate, and molten pool flow condition, with angle features to extract defect candidates.

[0051] (3) The molding history monitoring device according to (1) or (2), wherein the defect candidate extraction means performs an occurrence frequency calculation process for calculating an occurrence frequency of the defect candidates. According to this molding history monitoring device, by calculating the appearance frequency of defect candidates, it is possible to estimate locations in the molded object that should be precisely inspected based on the appearance frequency.

[0052] (4) The molding history monitoring device according to (3), wherein the defect candidate extracting means estimates a defect size in the object based on an appearance frequency of the defect candidate. According to this molding history monitoring device, defects that have occurred in a molded object can be easily identified based on the defect size estimated from the appearance frequency of the defect candidate, without performing cumbersome inspections such as destructive inspection, ultrasonic inspection, etc. Also, when the appearance frequency of the defect candidate continues for a certain length, it can be estimated that a long and thin defect has appeared, and when it is very short, it can be estimated that the defect candidate is a very small defect or has appeared due to the influence of noise.

[0053] (5) A system for manufacturing objects that manufactures objects by moving a torch and forming a weld bead by melting and solidifying a filler metal with the torch, the system comprising a manufacturing history monitoring device described in any one of (1) to (4). According to this system for manufacturing a molded object, it is possible to easily grasp any defects that may occur in the molded object when the object is being molded, and therefore it is possible to quickly repair the defects in the molded object after the object has been molded.

[0054] (6) A method for monitoring a manufacturing history, which estimates defects from history information when a plurality of weld beads are formed by melting and solidifying a filler metal by a torch to manufacture a structure, comprising: A shape profile acquisition process for acquiring a shape profile along an extension direction of an existing weld bead; a welding information acquisition process for acquiring welding information during the formation of an adjacent weld bead when forming an adjacent weld bead at a position adjacent to the existing weld bead; a defect candidate extraction process for identifying an angle feature having a root angle equal to or greater than a threshold in the existing weld bead based on the shape profile, identifying a welding feature of the welding information based on the welding information, and associating the welding feature corresponding to the angle feature with the angle feature and extracting it as a defect candidate; A method for monitoring a build history, comprising: According to this molding history monitoring method, a welding feature corresponding to an angle feature where the root angle of an existing weld bead is equal to or greater than a threshold is associated and extracted as a defect candidate. When forming an adjacent weld bead adjacent to an existing weld bead, if the root angle of the existing weld bead is large, there is a high risk of a defect occurring due to insufficient fluidity. Therefore, by determining as a defect candidate a case where there is a feature in the welding information of an adjacent weld bead at a position corresponding to an angle feature where the root angle of the existing weld bead is equal to or greater than a threshold, a highly reliable defect candidate can be extracted.

[0055] (7) The method for monitoring a molding history according to (6), wherein in the welding information acquisition process, at least one of a welding voltage, a welding current, a filler metal feed speed, a filler metal feed resistance, a shielding gas flow rate, and a flow condition of a molten pool is acquired as the welding information. According to this method for monitoring the manufacturing history, highly reliable defect candidates can be extracted by associating welding features in at least one of the acquired welding information, i.e., welding voltage, welding current, filler metal feed speed, filler metal feed resistance, shielding gas flow rate, and molten pool flow condition, with angle features to extract defect candidates.

[0056] (8) The molding history monitoring method according to (6) or (7), wherein the defect candidate extraction process includes an occurrence frequency calculation process for calculating an occurrence frequency of the defect candidates. According to this molding history monitoring method, by calculating the appearance frequency of defect candidates, it is possible to estimate locations in the molded object that should be precisely inspected based on the appearance frequency.

[0057] (9) The molding history monitoring method according to (8), wherein in the defect candidate extraction process, a defect size in the object is estimated based on an appearance frequency of the defect candidates. According to this molding history monitoring method, defects that have occurred in a molded object can be easily identified based on the defect size estimated from the appearance frequency of the defect candidate, without performing cumbersome inspections such as destructive inspection, ultrasonic inspection, etc. Also, when the appearance frequency of the defect candidate continues for a certain length, it can be estimated that a long and thin defect has appeared, and when it is very short, it can be estimated that the defect candidate is a very small defect or has appeared due to the influence of noise. [Explanation of symbols]

[0058] 21 Control unit (welding information acquisition means, defect candidate extraction means) 23. Torch 25 Shape sensor (shape profile acquisition means) 29, 29A, 29B Weld bead 100 Manufacturing system (modeling history monitoring device) M filler metal F Defect candidate P Molten pool W sculpture Rc Angle Feature Wc Weld feature θ Base angle

Claims

1. A molding history monitoring device that estimates defects from history information when a molded object is molded by forming a plurality of weld beads by melting and solidifying a filler metal with a torch, comprising: A shape profile acquisition means for acquiring a shape profile along an extension direction of an existing weld bead; a welding information acquisition means for acquiring welding information during the formation of an adjacent weld bead when the adjacent weld bead is formed at a position adjacent to the existing weld bead; a defect candidate extraction means for identifying an angle feature having a root angle equal to or greater than a threshold in the existing weld bead based on the shape profile, and for identifying a welding feature of the welding information based on the welding information, and for associating the welding feature corresponding to the angle feature with the angle feature and extracting it as a defect candidate; having Modeling history monitoring device.

2. The welding information acquisition means acquires at least one of a welding voltage, a welding current, a filler metal feed speed, a filler metal feed resistance, a shielding gas flow rate, and a flow state of a molten pool as the welding information. The molding history monitoring apparatus according to claim 1 .

3. the defect candidate extraction means performs an occurrence frequency calculation process for calculating an occurrence frequency of the defect candidates; The molding history monitoring device according to claim 1 or 2.

4. the defect candidate extraction means estimates a defect size in the object based on an appearance frequency of the defect candidate. The molding history monitoring apparatus according to claim 3 .

5. A manufacturing system for a molded object, which molds a molded object by forming a weld bead by melting and solidifying a filler metal by a torch while moving the torch, comprising: A molding history monitoring device according to any one of claims 1 to 4, A manufacturing system for objects.

6. A molding history monitoring method for estimating defects from history information when a molded object is molded by forming a plurality of weld beads by melting and solidifying a filler metal by a torch, comprising: A shape profile acquisition process for acquiring a shape profile along an extension direction of an existing weld bead; a welding information acquisition process for acquiring welding information during the formation of an adjacent weld bead when forming an adjacent weld bead at a position adjacent to the existing weld bead; a defect candidate extraction process for identifying an angle feature having a root angle equal to or greater than a threshold in the existing weld bead based on the shape profile, identifying a welding feature of the welding information based on the welding information, and associating the welding feature corresponding to the angle feature with the angle feature and extracting it as a defect candidate; Including, A method for monitoring build history.

7. In the welding information acquisition process, at least one of a welding voltage, a welding current, a filler metal feed speed, a filler metal feed resistance, a shielding gas flow rate, and a flow state of a molten pool is acquired as the welding information. The method for monitoring a molding history according to claim 6 .

8. In the defect candidate extraction process, an occurrence frequency calculation process is performed to calculate an occurrence frequency of the defect candidates. The method for monitoring a molding history according to claim 6 or 7.

9. In the defect candidate extraction process, a defect size in the object is estimated based on an appearance frequency of the defect candidates. The method for monitoring a molding history according to claim 8 .

Citation Information

Patent Citations

  • Automatic welding, defect repair method and automatic welding equipment

    JP2000167666A

  • Method and apparatus for measuring welding operation information

    JP2008110388A

  • Method and equipment for deciding good / defective condition of butt welding

    JP2008212944A

  • Manufacturing method of laminated molding and manufacturing apparatus

    JP2019089100A

  • Structure manufacturing system and manufacturing method

    JP2020189324A