Edge trimming method and edge trimming device for bonded wafers
The edge trimming method for bonded wafers addresses misalignment issues by using the base wafer's center as the processing center and a two-stage grinding process, ensuring accurate and damage-free trimming, thus maintaining yield in semiconductor manufacturing.
Patent Information
- Application Number
- JP2023123284
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-07-28
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2038-12-14
AI Technical Summary
In bonded wafers formed by laminating two wafers of substantially the same shape, misalignment during bonding leads to uneven trimming, risking damage and reduced yield in semiconductor manufacturing due to improper edge trimming based on incorrect center detection.
An edge trimming method and device that processes the bonded wafer's peripheral edge using the center of the base wafer as the processing center, involving two-stage grinding to ensure accurate trimming without damaging the wafer, utilizing optical contour detection and precise alignment to determine the base wafer's center, and adjusting the grindstone position accordingly.
Ensures reliable edge trimming of bonded wafers close to the target processing amount, preventing cracks and damage, thereby maintaining yield in semiconductor manufacturing by accurately aligning and processing the entire outer periphery of the upper bond wafer.
Smart Images

Figure 0007572518000001 
Figure 0007572518000002 
Figure 0007572518000003
Abstract
Description
[Technical field]
[0001] The present invention relates to an edge trimming method for a bonded wafer formed by bonding two wafers together, and more particularly to an edge trimming method for a bonded wafer that is suitable for bonding two wafers having substantially the same shape. [Background technology]
[0002] Advances in LSI technology have led to greater integration of semiconductor chips, but further integration requires even smaller elements. However, there is a limit to how small elements can be, and two-dimensional circuit layouts are approaching that limit. For this reason, attempts are being made to achieve higher integration by making the circuit layout three-dimensional instead of miniaturizing elements. One example is the wafer-on-wafer (WOW) method, in which two wafers are laminated and bonded together.
[0003] In the case of bonded wafers, two wafers of substantially the same shape are bonded together either directly or via an adhesive, etc. In the process of bonding two wafers together, there is a possibility of relative movement between the two wafers due to positional errors during bonding or for some reason between the time when the bonding surfaces of the wafers come into contact and are fixed, so a certain positional deviation of, for example, 0.5 mm is allowed.
[0004] This misalignment between the wafers is eliminated in the subsequent edge trimming process: the center position of the two bonded wafers is found, and the bonded wafer is rotated around the found center and the edges are trimmed using a grindstone to obtain a perfectly circular bonded wafer.
[0005] Patent Document 1 discloses an outer periphery grinding device that grinds the outer periphery of a bonded substrate formed by stacking and bonding two wafers, a bond wafer placed on the upper side and a base wafer placed on the lower side. In this publication, in order to improve the tolerance of the terrace processing width when grinding the outer periphery of the bonded substrate, an alignment means that aligns the bonded substrate and a grinding means that grinds the outer periphery of the bond wafer of the bonded substrate aligned by the alignment means are provided. The alignment means aligns the bonded substrate with the base wafer as a reference.
[0006] Patent Document 2 also discloses a processing method for accurately detecting the outer circumferential position of a bonded wafer. In this publication, a cutting blade is used to cut a position at a predetermined distance from the outer circumferential edge of a bonded wafer, which is attached to a support plate, toward the center of the wafer. Then, an irradiation means irradiates light onto the outer circumferential edge of the bonded wafer, and an imaging means facing the irradiation means across the bonded wafer captures an image of the outer circumferential edge of the bonded wafer to form an image, and the outer circumferential edge of the bonded wafer is detected based on the image. Furthermore, based on the detected outer circumferential edge position, a rotating cutting blade is cut into the bonded wafer at a position at a predetermined distance from the outer circumferential edge toward the center, and the chuck table is rotated to cut the wafer.
[0007] Non-Patent Document 1 describes measuring the misalignment of the centers of two wafers in a bonded wafer made by bonding two wafers together. In this document, a shape sensor that performs laser scanning and an edge sensor consisting of an LED light source and a CCD sensor are disposed on the side of the bonded wafer, and the center position of each wafer in the bonded wafer is obtained based on the output from the edge sensor. Then, the misalignment of the two bonded wafers is calculated from the difference between these two center positions. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] JP 2006-253387 A [Patent Document 2] Special Publication No. 2017-188599 [Non-patent literature]
[0009] [Non-Patent Document 1] Furuta et al., "Measuring Method for Misalignment of Bonded Wafers," Kobe Steel Techniques, Vol. 64, No. 2, pp. 115-118, October 2014. Summary of the Invention [Problem to be solved by the invention]
[0010] In a bonded wafer formed by bonding two wafers of substantially the same shape together, a center misalignment is allowed within a certain range during bonding, as described above. Therefore, the center positions of the two bonded wafers do not necessarily match, and in some cases, a part of the upper bond wafer protrudes from the lower base wafer, resulting in a portion not supported by the base wafer when the wafer is bonded. If the bonded wafer in this state is positioned using a laser sensor or the like that detects only the wafer contour, the overlapping shape of the upper and lower wafers is detected as the wafer shape, so that the center position of the bonded wafer, in which the centers of the upper and lower wafers are misaligned, is different from the center position of the lower base wafer.
[0011] In conventional edge trimming, the bonded wafer is rotated around the center position based on the detected contour of the bonded wafer, and the grinding wheel is brought into contact with the outer circumference. Therefore, the wafer is processed around a point different from the center of the base wafer, and the grinding wheel may cut into a position different from the initial target position, which may cause an abnormality in the trimming width. In the worst case, this may cause damage to the wafer and reduce the yield in semiconductor manufacturing.
[0012] In the above-mentioned Patent Document 1, a holder and a plurality of pins are provided, and the pins are arranged around the holder so that their positions can be adjusted. A bonded wafer, which is a base wafer and a bond wafer bonded together, is placed on the holder with the bond wafer facing up. The heights of the plurality of position-adjustable pins are adjusted so that they do not come into contact with the bond wafer but only with the outer periphery of the base wafer. After that, the center position of the base wafer is obtained from the positions of the adjustable pins, making it possible to process the outer periphery of the bonded substrate based on the base wafer.
[0013] By the way, the bonded wafer of the WOW method is made by bonding two wafers of substantially the same shape, so its total thickness is about the sum of the thicknesses of each wafer. Therefore, if the pin height is adjusted within the range of the base wafer thickness, for example, for a 100 μm thick wafer, the pin height adjustment range will be less than 100 μm, and a large number of adjustment steps will be required. In addition, as the number of steps for adjusting the pin height increases, the chances of contact between the pin and the wafer increase, and the risk of damaging the wafer due to contact between the solid pin and the wafer during adjustment also increases.
[0014] In addition, in the bonded wafer processing method described in Patent Document 2, an image obtained by optical means is binarized to detect the contour of the bonded wafer. In the wafer processing method described in this publication, the case where the center positions of two stacked wafers are misaligned when they are bonded together is not fully considered. Therefore, if the upper and lower wafers are misaligned, the wafer may be cut with the center being the midpoint between the misaligned centers of the upper and lower wafers. As a result, there is a risk that the outer peripheral unbonded portion of the upper bond wafer may not be processed or may be cut too far toward the center.
[0015] Non-Patent Document 1 describes a method of detecting the contour of a bonded wafer, which is made by stacking two wafers of substantially the same shape one above the other and bonding them together, using a laser optical system. However, although the method of measuring the deviation of a bonded wafer described in this document can measure the amount and position of deviation between the two wafers, it does not disclose how to edge trim the wafer based on the amount of deviation.
[0016] The present invention has been made in consideration of the above-mentioned problems of the conventional technology, and its object is to make it possible to reliably trim the edge of the outer periphery of a wafer by an appropriate amount close to the target processing amount, without affecting the chip formation parts of the bond wafer and the base wafer, in a bonded wafer formed by bonding two wafers of substantially the same shape. Another object of the present invention is to prevent a decrease in yield caused by the occurrence of cracks or damage in the wafer parts that do not contribute to semiconductor manufacturing, by performing processing based on the lower base wafer and processing the entire outer periphery of the upper bond wafer in edge trimming of a bonded wafer by the WOW method. [Means for solving the problem]
[0017] The features of the present invention that achieve the above object are as follows.
[0018] [1] An edge trimming method for processing a peripheral portion of a bonded wafer formed by bonding a base wafer and a bond wafer, comprising: grinding the peripheral portion of the bonded wafer using the center of the base wafer as a processing center. [2] The edge trimming processing method for a bonded wafer according to [1], characterized in that, when the bond wafer protrudes from the contour of the base wafer, the peripheral portion of the bonded wafer is ground using the center of the base wafer as a processing center. [3] A method for edge trimming a bonded wafer according to [1] or [2], characterized in that a peripheral portion of the bonded wafer is ground around a processing center set based on a trimming width determined based on a maximum and minimum outer diameter of the bonded wafer and a center position of the bond wafer as a rotation center. [4] An edge trimming processing apparatus for processing a peripheral portion of a bonded wafer formed by bonding a base wafer and a bond wafer, comprising: a processing unit that grinds the peripheral portion of the bonded wafer using the center of the base wafer as a processing center. [5] The edge trimming processing apparatus described in [4], characterized in that when the bond wafer protrudes from the contour of the base wafer, the processing unit grinds the peripheral portion of the bonded wafer, using the center of the base wafer as the processing center. [6] The edge trimming processing apparatus according to [4] or [5], characterized in that the processing unit grinds the peripheral portion of the bonded wafer using the processing center, which is set based on a trimming width determined based on the maximum and minimum outer diameters of the bonded wafer and the center position of the bond wafer, as a rotation center.
[0019] Other configurations of the present invention are as follows.
[0020] [1] An edge trimming method for processing a peripheral portion of a bonded wafer formed by bonding a base wafer and a bond wafer, comprising: a protruding region of the bond wafer protruding from a contour of the base wafer is ground, and a peripheral portion of the bond wafer and a peripheral portion of the base wafer are simultaneously ground with the center of the base wafer as a rotation center. [2] The edge trimming processing method for a bonded wafer according to [1], characterized in that the protruding region is ground around a processing center set based on a trimming width determined based on maximum and minimum outer diameters of the bonded wafer and a center position of the bond wafer as a rotation center. [3] An edge trimming processing apparatus for processing a peripheral portion of a bonded wafer formed by bonding a base wafer and a bond wafer, comprising: a measuring device for grinding an area of the bond wafer that protrudes beyond the contour of the base wafer; and a processing unit for simultaneously grinding the peripheral portion of the bond wafer and the peripheral portion of the base wafer, with the center of the base wafer as the center of rotation. [4] The edge trimming processing apparatus described in [3], characterized in that the measuring device grinds the protruding region using a processing center set based on a trimming width determined based on the maximum and minimum outer diameters of the bonded wafer and a center position of the bond wafer as a rotation center.
[0021] Another feature of the present invention for achieving the above-mentioned object is that, in an edge trimming method for processing a peripheral portion of a bonded wafer formed by bonding a base wafer and a bond wafer, the method includes a first stage grinding process for detecting an overhanging area of the bond wafer constituting the bonded wafer from the base wafer and grinding only the peripheral portion of the bond wafer including the detected overhanging area, and a second stage grinding process for simultaneously grinding the peripheral portions of the bond wafer and the base wafer.
[0022] In this feature, it is preferable that in the first stage grinding process and the second stage grinding process, a Y-axis cut is used to bring the bonded wafer closer to a rotating grindstone from a substantially horizontal direction, and that the detection of the protruding region of the bond wafer is performed using a light source and a line sensor arranged opposite to the outer periphery of the bonded wafer.
[0023] In the above-mentioned feature, in the first stage grinding process, it is preferable that the minimum diameter of the bonded wafer obtained when detecting the protrusion region of the bond wafer is subtracted from the maximum diameter, and the grinding process is performed with a position offset from the rotation center of the base wafer by half of the difference as the rotation center, and that in the maximum protrusion region of the bond wafer, the bond wafer is ground to a substantially planar position with the base wafer after processing, and in the maximum protrusion region of the base wafer, the bond wafer is not substantially ground after processing.
[0024] In addition, in the second grinding step, it is preferable to process the bonded wafer that has been subjected to the first grinding step to a predetermined cutting depth around the center position of the base wafer. Furthermore, the bonded wafer may be two silicon wafers having substantially the same shape. Effect of the Invention
[0025] According to the present invention, the center of each wafer of a bonded wafer formed by bonding two wafers one above the other can be detected by using an optical contour detection means, so that edge trimming based on the center position of the lower base wafer becomes possible, and the outer periphery of the wafer can be edge trimmed by an appropriate amount close to the target processing amount with certainty. Also, in edge trimming of a bonded wafer by the WOW method, processing can be performed based on the lower base wafer, so that the outer periphery of the upper bond wafer can be processed over the entire circumference, and a decrease in yield due to cracks or damages in the wafer parts that do not contribute to semiconductor manufacturing can be prevented. [Brief description of the drawings]
[0026] [Figure 1] 1 is a top view of an embodiment of a wafer processing apparatus according to the present invention; [Diagram 2] 2 is a front view of a grinding unit provided in the wafer processing apparatus of FIG. 1. [Diagram 3] FIG. 1 is a perspective view of a wafer outer diameter measuring device equipped with a laser sensor. [Figure 4] FIG. 4 is a diagram showing an example of the output of FIG. 3. [Diagram 5] 11A and 11B are diagrams for explaining a method for determining the center of edge trimming processing. [Figure 6] 1A to 1C are diagrams illustrating a method for edge trimming a bonded wafer. [Figure 7] 1 is a flowchart illustrating an edge trimming method for a bonded wafer. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0027] An embodiment of a wafer edge trimming apparatus according to the present invention will be described below with reference to the drawings. Fig. 1 is a schematic top view of an embodiment of an edge trimming apparatus 10, and Fig. 2 is a front view of a grinding device 16 provided in the edge trimming apparatus 10 shown in Fig. 1. The edge trimming apparatus 10 of this embodiment is provided with two sets of the same grinding devices 16.
[0028] The edge trimming processing apparatus 10 includes a supply / recovery section 14, a measurement / alignment section 22, two grinding devices 16, a cleaning / drying section 20, and a transport means 24. Although not shown, the apparatus also includes an operation panel and a control device for controlling these sections 14, 22, 16, 20, and the transport means 24.
[0029] The supplying and collecting section 14 supplies the bonded wafers W to be edge-trimmed from the wafer cassette 30 to the measurement and alignment section 22 and the processing section 19, and also collects the edge-trimmed bonded wafers W from the processing section 19 to the wafer cassettes 30, 31. The supplying and collecting section 14 in this embodiment includes three wafer cassettes 30, a measurement and transport section 12 equipped with one wafer supplying and collecting robot 34, and one reject wafer cassette 31.
[0030] The measurement and transport unit 12 takes out the bonded wafers W one by one from each wafer cassette 30 set on the cassette table and supplies them to the measurement and alignment unit 22. At the same time, the bonded wafers W that have been subjected to edge trimming processing are stored from the measurement and alignment unit 22 into the wafer cassettes 30 and 31. At this time, the bonded wafers W that do not meet the specifications in the measurement and alignment unit 22 are stored in the reject wafer cassette 31, and the bonded wafers W that meet the specifications are stored in the wafer cassette 30. The supply and recovery robot 34 is, for example, a three-axis rotating transport arm, and holds the bonded wafer W by vacuum adsorbing the surface of the bonded wafer W with an adsorption pad. The measurement and transport unit 12 has a structure in which the base can move in a circle, for example, and the base moves around the outer periphery of the circle, so that the bonded wafers W can be supplied to and recovered from each wafer cassette 30 and 31 and the measurement and alignment unit 22. On the other hand, each of the wafer cassettes 30, 31 and the measurement and alignment section 22 opens toward the measurement and transport section 12 side, making it possible to receive and remove the bonded wafer W.
[0031] The measurement and alignment unit 22 measures the thickness of the bonded wafer W to be edge trimmed and the center position of the bonded wafer W, which will be described in detail below. The measurement and alignment unit 22 includes a measurement table 50, a thickness sensor 52, an outer diameter measuring device 54, and optionally an edge shape detection sensor. The measurement table 50 rotates the bonded wafer W around its central axis. The edge shape detection sensor 56 (not shown) is a laser sensor, and detects the outer peripheral edge shape of the bonded wafer W and the notch, if one is formed.
[0032] The two grinding devices 16 are arranged in parallel on the front portion of the edge trimming processing apparatus 10, and each performs two-stage peripheral edge trimming processing of the bonded wafer W. The two grinding devices 16 have the same configuration, and each comprises a grinding table 60 and a spindle 62 for positioning the bonded wafer W at a predetermined position.
[0033] The cleaning / drying unit 20 cleans the bonded wafer W after the edge trimming process, and then dries the bonded wafer W. The cleaning / drying unit 20 includes, for example, a spin cleaning device that sprays a cleaning liquid onto the surface of the bonded wafer W while rotating the bonded wafer W held on the cleaning table 82, thereby peeling off and removing dirt adhering to the surface of the bonded wafer W. The cleaning / drying unit 20 also includes a drying means (not shown) for removing the cleaning liquid.
[0034] The transport means 24 transports and collects the bonded wafer W that has finished processing in the grinding device 16 to the cleaning and drying section 20. The collected bonded wafer W is returned to the grinding device 16 for reprocessing, or is transported to the measurement and alignment section 22 for a final shape check and a product check for cracks, chips, etc. When a shape check or product check is performed in the measurement and alignment section 22, the transport means 24 transports the bonded wafer W after grinding to the measurement and alignment section 22 through the back space 66 of the grinding device 16.
[0035] Next, the configuration of the grinding device 16, which is a characteristic part of the present invention shown in part A of Fig. 1, will be described with reference to Fig. 2. Since the configuration of the two grinding devices 16 is the same, only part A of Fig. 1 will be described, but the other grinding device 16 is also similar.
[0036] The grinding device 16A includes a grinding table 60 on which the bonded wafer W is placed, and a spindle 62 on which a grinding wheel 152 is mounted. In this embodiment, the grinding table 60 is movable within the XY plane, and the position of the spindle 62 is fixed within the XY plane. Therefore, when edge trimming, which is the outer periphery processing of the bonded wafer W, is performed, the bonded wafer W is moved together with the grinding table 60 to approach the grinding wheel 152 on the spindle 62.
[0037] 2 by X-axis driving means 125 consisting of a ball screw and a servo motor, and constitutes an X-axis driving mechanism 220. Two Y-axis guide rails 126 are placed on the X-table 124, and together with four Y-axis linear guides 127, Y-axis driving means consisting of a ball screw and a servo motor (not shown), and a Y-table 128 moved in the Y direction perpendicular to the X direction by the Y-axis driving means, constitute a Y-axis driving mechanism 230.
[0038] A Z table 131 is mounted on the upper portion of the Y table 128. The Z table 131 is guided by two Z-axis guide rails 129 and four Z-axis linear guides (not shown) and moved in the Z direction in FIG. 2 by Z-axis driving means 130. The Z table 131 is moved in the Z direction in FIG. 2 by Z-axis driving means 130 including a ball screw and a stepping motor. The Z-axis driving means 130 and the like constitute a Z-axis driving mechanism 240. A θ-axis motor 132 and a θ-spindle 133 are mounted on the Z table 131. A wafer table 134 on which a bonded wafer W is placed by suction is attached to one end side of the θ-spindle 133.
[0039] The wafer table 134 rotates in the θ direction in FIG. 2 around the center of rotation Og (see FIG. 6). The transport means 24 shown in FIG. 1 can be disposed on the upper surface of the wafer table 134, and a suction pad is attached to the tip of the transport means 24 facing downward. The suction pad communicates with a vacuum source, and the bonded wafer W to be edge-trimmed is placed on and fixed by suction. The grinding table 60 rotates the bonded wafer W in the θ direction in FIG. 2 and moves it to a predetermined position in the X, Y, and Z directions. In the spindle 62, an AC servo motor 151 is fixedly accommodated in a base 150, and rotates at a rotation speed of, for example, 500 rpm (approximately 8.3 Hz) by a direct drive method.
[0040] Incidentally, the bonded wafer W used in this embodiment is formed by bonding two silicon wafers W0 of substantially the same shape in a previous process. Each silicon wafer W0 is, for example, a 12-inch wafer W with a diameter of 300 mm and a thickness of about 0.6 to 1.0 mm, and is bonded together by an adhesive means such as an adhesive. In a specific bonding process, the two wafers W0 are stacked, and an adhesive means is applied between the two stacked wafers W0, W0. At this time, due to a positional deviation in the stacking of the two wafers W0 and a positional deviation caused by local non-uniformity in the adhesive force when the adhesive means solidifies, the central positions O1 and O2 of the substantially identical wafers W0 are different from each other microscopically.
[0041] When bonding wafers W, two wafers W ba , W bo For example, an error of 0.5 mm is allowed between the center positions Oba and Obo. If cutting into chips is performed in a later process without considering the position error between the center positions, the effective chip area will change, which may cause problems such as poor insulation, and some kind of action will be required.
[0042] Therefore, in order to prevent the misalignment during bonding from affecting the cutting into chips, after the bonding process is completed, an edge trimming process is performed to remove unnecessary parts such as incomplete adhesion formed on the periphery of the bonded wafer W and to compensate for the misalignment. For example, in the edge trimming process, the base wafer W located on the lower side of the bonded wafer W is trimmed. ba Based on this, the bond wafer W located on the outer periphery at a radial length of about 1 to 7 mm and on the upper side in the height direction is bo Total height of base wafer W ba It is required to perform edge trimming to a thickness of about 100 μm, including the thickness from the bonding surface.
[0043] Next, a method for measuring the outer diameter of a bonded wafer W, which is performed in the measurement and alignment unit 22 of Fig. 1 before edge trimming processing, and a method for determining the processing center position of the bonded wafer W based on the measurement results will be described with reference to Fig. 3 to Fig. 6. Fig. 3 is a schematic diagram of an outer diameter measuring device 54 disposed in the measurement and alignment unit 22, Fig. 3(a) is a perspective view thereof, and Fig. 3(b) is a side view thereof.
[0044] A measurement table 50 is provided in the measurement and alignment section 22, and a bonded wafer W transferred by the wafer supply and recovery robot 34 is placed on the measurement table 50. In this state, the bonded wafer W is placed almost at the center of the measurement table 50, but is not positioned at the exact processing center. As described above, the base wafer W ba and bond wafer W bo Since the positions are not exactly the same, the edge trimming process may result in unintended wafer areas, especially bond wafers. bo In order to prevent grinding of the chip formation surface of the base wafer W ba The exact machining center O bo Request.
[0045] A bonded wafer W is made of two silicon wafers W sliced by wire cutting or other methods. bo , W ba Since it is formed by bonding two wafers together, its surface quality is close to a mirror surface, and it does not transmit light like a glass substrate. Therefore, the outer diameter of the bonded wafer W is calculated by comparing the area where light transmits (or passes) optically with the area where it is reflected. bo The base wafer W ba It is not possible to determine whether the light was reflected from the upper surface of the object, but it is possible to determine from which surface the light was reflected by a shape observation means or a visible camera (not shown).
[0046] The outer diameter measuring device 54 for the bonded wafer W is disposed on the outer periphery of the measuring table 50. The outer diameter measuring device 54 includes two holding members 324, 326 that are held at a distance from each other in the longitudinal middle of a support 322 erected on a base 328. The two holding members 324, 326 are disposed so as to substantially coincide with the radial direction of the measuring table 50. On the side where one holding member 324 faces the other holding member 326, one or more light sources 310 are disposed so as to coincide with the radial direction of the measuring table 50. On the side where the other holding member 326 faces the one holding member 324, a line sensor 312 having a plurality of sensors corresponding to the light source 310 is disposed. The line sensor 312 is also disposed so as to substantially coincide with the radial direction of the measuring table 50. The light source 310 and the line sensor 312 are connected to a control unit 350, and the .... The light source 310 and the line sensor 312 are connected to a control unit 350. The control unit 350 detects the light intensity of the base wafer W constituting the bonded wafer W from the detection light detected by the line sensor 312. ba The distribution of the center and outer diameter φD is calculated.
[0047] The light source 310 emits parallel light downward toward the line sensor 312, and the bond wafer W bo and base wafer W ba The radiation light 304 is interrupted by at least one of the upper surfaces of the measuring table 50 and the radiation light 302 reaches the line sensor 312 without being interrupted. The measuring table 50 is continuously rotated around the central axis 50a, and the boundary between the two types of radiation light 304 and 302 is continuously detected, thereby detecting the contour of the bonded wafer W. Based on the detected contour, the position of the base wafer W relative to the current rotation center (the rotation center of the measuring table 50) O is calculated. ba Position O ba , and the outer diameter (distance to the contour) of the bonded wafer W corresponding to the current rotation center O is obtained for the rotation angle α of the measuring table 50.
[0048] An example of the output of the line sensor 312 is shown in Fig. 4(a), and the trajectory of the outer diameter (contour) of the bonded wafer W relative to the current center of rotation O, which is determined based on this example output, is shown in Fig. 4(b). In Fig. 4(a), the horizontal axis is the rotation angle α (°) of the measurement table 50. The vertical axis is the overall output (V) of the line sensor 312 consisting of multiple sensors, and indicates how much of the light emitted from the light source 310 reaches the line sensor 312, or conversely, how much is blocked by the bonded wafer W. The output (V) of the line sensor is configured in advance with respect to the radial position of the measurement table 50, and a lower output (V) indicates a larger outer diameter of the bonded wafer W, and a higher output (V) indicates a smaller outer diameter of the bonded wafer W.
[0049] Two silicon wafers W ba and W bo When the positions of the two silicon wafers W are perfectly aligned to form the bonded wafer W, and the center of the measurement table 50 and the center of the bonded wafer W are perfectly aligned, the output is constant with respect to the rotation angle α of the measurement table 50. ba and W bo Even if the two silicon wafers W are bonded together in perfect agreement, if they are placed displaced relative to the measurement table 50, an output shape having one maximum portion and one minimum portion will be obtained during one rotation of the measurement table 50. ba and W bo The positions of the two maxima and two minima do not coincide perfectly, and if the position is not adjusted, it is difficult to align the center of the bonded wafer W with the center of the measurement table 50. As a result, as shown in FIG. 4(a), an output shape having two maxima and two minima is obtained during one rotation of the measurement table 50.
[0050] Based on the output shown in Fig. 4(a), the outer diameter (contour) of the bonded wafer W is plotted in polar coordinates in Fig. 4(b). In order to clarify the central position deviation, for example, a nominal diameter (φ300 for a 12-inch wafer) is taken as the reference outer diameter φRef, and the deviation Δρ from this reference outer diameter φRef is plotted on a diagram with one scale, for example 50 μm, against the angle α from the starting position. Here, the reference outer diameter φRef in Fig. 4(b) corresponds to V0 in Fig. 4(a). From Fig. 4(a), a gourd-shaped combination of two circular arcs can be obtained.
[0051] Next, from the polar coordinate diagram thus obtained, the base wafer W constituting the bonded wafer is ba and bond wafer W bo Center position of O ba , O bo The calculation method for obtaining the above will be described with reference to FIG. 5. FIG. 5 is a diagram corresponding to FIG. 4(b). In this calculation, the base wafer W ba and bond wafer W bo The positional relationship between the deviations is assumed to be known by other methods. For example, in FIG. 5, the arc-shaped portion on the left side is the base wafer W detected by the outer diameter measuring device 54. ba The right-hand arc is the bond wafer W bo This is the outline of the
[0052] Three or more points are selected on the left-hand arc-shaped portion, and the contour line is approximated by a circular arc from the three or more points to obtain a circular arc of radius ρ and its center position. The obtained center position is the base wafer W ba The center position Oba of the bond wafer W is bo The center position Obo of each wafer W is also calculated. bo , W ba The positional deviation vectors A and B from the center positions Oba and Obo of the bonded wafer W are calculated. Therefore, if the position of the bonded wafer W is moved by the amount of the positional deviation vector A, the base wafer W ba The center position Oba of the base wafer W can be aligned with the rotation center O of the measurement table 50. baThe bonded wafer W can be rotated around the center Oba of the outer diameter measuring device 54 (see FIG. 6(c)). These relationships are stored in the control unit 350 included in the outer diameter measuring device 54.
[0053] Details of edge trimming of the bonded wafer W based on the obtained rotation center Oba of the base wafer Wba will be described with reference to Fig. 6. For comparison, Fig. 6 also shows a conventional edge trimming method for the bonded wafer W (Figs. 6(d) and 6(e)). Note that in Fig. 6, grindstones 152 are shown by dashed lines at two locations in the circumferential direction of the bonded wafer W, but as is clear from Fig. 2, only one grindstone 152 is used for processing. In order to show the difference in processing due to the difference in the circumferential position of the bonded wafer W, the relative positional relationship is also shown for reference.
[0054] As shown in FIG. 6(a), the bonded wafer W transported from the wafer cassette 30 to the measurement and alignment section 22 by the supply and collection robot 34 is placed on the measurement table 50 with a position offset from the rotation center O of the measurement table 50. In this state, the contour of the bonded wafer W is measured by the outer diameter measuring device 54 according to the method described in FIGS. ba The center position Oba of the base wafer W is then determined. Then, the supply / recovery robot 34 is used to place the base wafer W on the wafer table 134. ba The center position Oba of the grinding table and the rotation center Og of the grinding table are aligned using the measurement and calculation results of the measurement and alignment unit 22.
[0055] In the bonded wafer W, which is bonded together by applying an adhesive, the amount of adhesive is reduced near the edge in order to prevent the adhesive applied to the outer periphery from spilling out of the gap at the edge and contaminating the surfaces other than the bonded surface of the wafer. As a result, a bonded surface without adhesive may be formed at the outer periphery of each wafer. Since the wafers are not bonded to each other in the part without adhesive and chips cannot be formed, edge trimming is performed in advance in anticipation of the occurrence of such an area where chips cannot be formed. As described above, the outer periphery of the bonded wafer W is ground by anticipating 1 to 7 mm in the radial direction from the outer periphery of each wafer as the area where chips cannot be formed. In this embodiment, the incomplete overlapping part of the two upper and lower wafers constituting the bonded wafer W, i.e., the non-overlapping part, of the wafers is processed in the range expected as the area where the bonding is incomplete, thereby preventing the occurrence of grinding with an excessive cutting depth during edge trimming.
[0056] Therefore, in the present invention, the grinding process is performed in two stages. The first stage is the processing state shown in FIG. 6(b), and the second stage is the processing state shown in FIG. 6(c). In the first stage processing state, the diameter of the bond wafer W detected by the outer diameter measuring device 54 is bo The protruding portion of the bonded wafer W is ground. The bonded wafer W is transported to the measurement and alignment section 22, and aligned so that the processing center O1 of the bonded wafer W, which will be described in detail later, coincides with the rotation center Og of the wafer table 134. The aligned bonded wafer W is moved to the processing section 19. Thereafter, Y-axis cutting is performed to bring the grinding table 60 closer to the spindle 62 shown in FIG. 2. The grindstone 152 attached to the spindle 62 is, for example, a metal grindstone of No. 800 having a diameter of 200 mm.
[0057] Before performing the Y-axis cutting, the height of the grindstone 152 is adjusted by using the Z-axis driving mechanism 240 provided on the grinding table 60. Specifically, the bond wafer W constituting the bonded wafer W bo and base wafer W baThe bottom surface of the grindstone 152 is aligned with the bonding interface of the bonded wafer W. Then, in the Y-axis cutting, the grinding table 60 is moved horizontally from the outer periphery to the center of the bonded wafer W. The cutting amount at this time and the processing center O1 of the bonded wafer W will be described in detail below.
[0058] In the first stage grinding process, the bond wafer W is ground to a degree that does not exceed the target shape required after the edge trimming process of the bonded wafer W. bo is the base wafer W ba The protruding portion is removed. At this time, the trimming width (length in the radial direction of the bonded wafer W) is determined using the maximum and minimum values of the outer diameter of the bonded wafer W detected when the bonded wafer W is measured by the measurement and alignment unit 22. The maximum value of the outer diameter of the bonded wafer W is the sum of the outer diameter of the base wafer Wba and the length of the protruding portion of the bond wafer Wbo. The minimum value is the sum of the outer diameter of each wafer W constituting the bonded wafer W. ba , W bo The minimum outer diameter of the bonded wafer W is subtracted from this maximum value to obtain the difference, and edge trimming is performed by the width (trimming width) between the target value (initial setting value) and the average value.
[0059] Now that the edge trimming width has been determined, the bond wafer W bo The processing center position O1 is offset from the center position Obo of the bond wafer W toward the maximum outer diameter by 1 / 2 the trimming width. bo The maximum protruding part of the base wafer W ba The surface position is along the contour of the base wafer W ba There are only bond wafers bo In the maximum overlapping portion where the bond wafer W is not bonded, bo Therefore, the shape of the bonded wafer W after the first edge trimming process is a perfect circle of the base wafer W when viewed from above. ba Niko base wafer W ba Slightly smaller bond wafer Wbo The overall wafer is made up of the base wafer W ba The contour of the circle is shown along the outer diameter of the figure.
[0060] Next, as shown in FIG. 6(c), a second-stage grinding process is performed. Before the second-stage grinding process is performed, the bonded wafer W that has been subjected to the first-stage grinding process is transported again to the measurement and alignment unit 22. Then, the rotation center Og of the wafer table 134 and the base wafer W that constitutes the bonded wafer W are aligned. ba After the alignment is completed, the bonded wafer W is moved to the processing section 19 side, and then the grinding table 60 is moved closer to the spindle 62 side shown in FIG.
[0061] In the second stage grinding process, the cutting depth of the grindstone 152 is ba This is the predetermined cutting depth required for edge trimming, including a part of the Y-axis cutting depth. In the second stage grinding process, Y-axis cutting is performed to bring the bonded wafer W closer to the grindstone 152 from a substantially horizontal direction. That is, the bottom surface of the grindstone 152 is brought closer to the bond wafer W. bo The grinding table 60 is moved in the Y-axis direction to the bond wafer W bo and base wafer W ba and processed simultaneously.
[0062] After the second grinding process, the bond wafer W bo The center position Obo of the base wafer W ba A difference occurs between the maximum processing width Δl1 and the minimum processing width Δl2 by the amount of positional deviation from the center position Oba of the base wafer W. ba The edge trimming is performed by rotating the bonded wafer W around the rotation center Oba. baConversely, the outer periphery of the bonded wafer W can be edge-trimmed so that the designed processing diameter φDdes or the maximum allowable range closest thereto remains without affecting the chip formation range of the base wafer Wba.
[0063] On the other hand, the conventional edge trimming method is the same as the present invention in that the bonded wafer W is transported from the wafer cassette 30 to the measurement and alignment unit 22 by the supply / recovery robot 34. In this case, as shown in Fig. 6(a), the bonded wafer W is placed on the measurement table 50 at a position displaced from the center O of the measurement table 50, which is also the same as the present invention.
[0064] However, in the conventional edge trimming method, as shown in FIG. 6(d), the measurement and alignment unit 22 detects the contour of the bonded wafer W, and then determines the position of the maximum diameter from the detected contour, and aligns the midpoint of the diameter with the rotation center Og of the wafer table 134. ba Center of Oba and bond wafer W bo The center O of the bonded wafer W is the midpoint of the center Obo of the bonded wafer W, which is aligned with the rotation center Og of the wafer table 134. The bonded wafer W is rotated around this position. At this time, the cutting depth of the grindstone 152 is set to the designed cutting depth t, and the radial cutting amount is set to the amount that the designed processing diameter φDdes remains. After that, the bonded wafer W bo and the total thickness of the base wafer W ba The grinding process is carried out in one go from the bonding surface to a certain height.
[0065] After the grinding process is completed, as shown in FIG. 6(e), the designed processing diameter φDdes is obtained with the maximum processing width Δl1 and the minimum processing width Δl2. However, in the maximum processing width Δl1 part, the base wafer W ba On the other hand, there was a risk that the edge trimming process would be performed beyond the removal range of 1 to 7 mm of the unnecessary part including the bonded part, which is set for each type of bonded wafer W. In other words,ba In the edge trimming method according to the present invention, the base wafer W is ground away from the surface of the base wafer W, and the edge trimming method according to the present invention is performed by grinding the base wafer W to a desired area. ba The second stage grinding process is performed based on the base wafer W. ba There is no risk of grinding beyond the tolerance range.
[0066] Next, the procedure for the edge trimming method of the bonded wafer W is shown in a flow chart in FIG. 7. Also refer to FIG. 1. In step S710, the bonded wafer W accommodated in the wafer cassette 30 of the supply / recovery section 14 is transported to the measurement / alignment section 22 by the measurement / transport section 12. In the measurement / alignment section 22, the outline of the bonded wafer W is detected by using the outer diameter measuring device 54 or the like, and then the edge of each wafer W constituting the bonded wafer W is measured. ba , W bo In order to perform the first stage grinding process on the bonded wafer W, the calculated center positions Oba, Obo and the bond wafer W are calculated. bo Based on the protrusion position and protrusion amount, the rotation center position O1 of the bonded wafer W is obtained and aligned (step S720). The aligned rotation center position O1 of the bonded wafer W is matched with the center position of the grinding table 60, and the bonded wafer W is held by vacuum suction (step S730).
[0067] The X- and Z-axis drive mechanisms 220 and 240 of the grinding table 60 are driven to match the grinding direction and height with the grindstone 152 attached to the spindle 62, and the Y-axis drive mechanism 230 of the grinding table 60 is used to perform the first stage of grinding processing with a predetermined cutting depth at the Y-axis cutting (step S740). As described above, in this first stage of grinding processing, the bond wafer W bo After the first stage of grinding is completed, the bonded wafer W is transported to the cleaning and drying section 20 by the transport means 24, where it is cleaned and dried (step S750).
[0068] Thereafter, the bonded wafer W is transported to the measurement and alignment section 22 using the transport means 24. In the measurement and alignment section 22, the base wafer W of the bonded wafer W is ground to perform the second stage grinding process, i.e., the final edge trimming process. ba The center position Oba of the bonded wafer W is aligned to coincide with the rotation center Og of the wafer table 134 (step S760). The aligned bonded wafer W is aligned and placed on the grinding table 60 by the supply / recovery robot 34 of the measurement / transport unit 12, and is held by vacuum suction (step S770).
[0069] The X- and Z-axis drive mechanisms 220 and 240 of the grinding table 60 are driven to match the grindstone 152 attached to the spindle 62 with the processing direction and processing height, and the Y-axis drive mechanism 230 of the grinding table 60 is used to perform the second stage grinding process by a predetermined cutting depth with the Y-axis cutting (step S780). bo Not only that, but also the base wafer W ba Also, a part of the outer periphery in the height direction is ground.
[0070] When the second stage grinding process is completed, the edge trimming process is also completed, so that the bonded wafer W after grinding is transported again to the cleaning / drying section 20 using the transport means 24, where it is cleaned and dried (step S790).
[0071] After the cleaning and drying are completed, the bonded wafer W is stored in the wafer cassette 30 of the supply / recovery section 14 using the transport means 24 (step S800). Before storing in the wafer cassette 30, the bonded wafer W may be checked for chipping, cracks, etc. by the measurement / alignment section 22, and any defective wafers may be stored in a reject wafer cassette 31.
[0072] In the above embodiment, a bonded wafer formed by bonding two silicon wafers together has been described, but it goes without saying that the present invention can be applied to other types of bonded wafers as long as the bonded wafer is formed by bonding two wafers made of opaque materials together. Also, in the above embodiment, the diameters of the two silicon wafers are the same, but the base wafer W ba Compared to bonded wafers, bo The present invention can also be applied to a bonded wafer W having a slightly smaller diameter than that of the first wafer W, or vice versa. [Explanation of symbols]
[0073] 10...edge trimming processing device, 12...measurement and transport section, 14...supply and recovery section, 16...grinding device, 19...processing side, 20...cleaning and drying section, 22...measurement and alignment section, 24...transport means, 30...wafer cassette, 31...reject wafer cassette, 34...supply and recovery robot, 50...measurement table, 50a...center axis, 52...thickness sensor, 54...outer diameter measuring device, 60...grinding table, 62...spindle, 66...rear space, 82...cleaning table, 121...X-axis base, 122...X-axis guide rail, 123...X-axis linear guide, 124...X-table, 125...X-axis Driving means, 126... Y-axis guide rail, 127... Y-axis linear guide, 128... Y table, 129... Z-axis guide rail, 130... Z-axis driving means, 131... Z table, 132... θ-axis motor, 133... θ spindle, 134... wafer table, 141... base, 150... base, 151... AC servo motor, 152... grindstone, 220... X-axis driving mechanism, 230... Y-axis driving mechanism, 240... Z-axis driving mechanism, 302, 304... synchrotron radiation, 310... light source, 312... line sensor, 322... pillar, 324, 326... holding material, 328... base, 350... control unit, W... wafer, W ba …base wafer, Wbo…bond wafer, O…rotation center of wafer, O1…rotation center of wafer during first grinding process, Oba…rotation center of base wafer, Obo…rotation center of bond wafer, Og…rotation center of wafer table
Claims
1. An edge trimming method for processing a peripheral portion of a bonded wafer formed by bonding a base wafer and a bond wafer, comprising: a center of the base wafer being set as a processing center, which is a rotation center when processing the peripheral portion of the bonded wafer, and grinding the peripheral portions of the base wafer and the bond wafer.
2. 2. The edge trimming processing method for a bonded wafer according to claim 1, characterized in that, when the bond wafer protrudes from a contour of the base wafer, the center of the base wafer is set as the processing center, and peripheral portions of the base wafer and the bond wafer are ground.
3. 3. The edge trimming processing method for a bonded wafer according to claim 1, characterized in that peripheral portions of the base wafer and the bond wafer are ground with the processing center set based on a trimming width determined based on a maximum value and a minimum value of an outer diameter of the bonded wafer and a center position of the bond wafer as a rotation center.
4. An edge trimming processing apparatus for processing a peripheral portion of a bonded wafer formed by bonding a base wafer and a bond wafer, comprising: a processing unit that grinds the peripheral portions of the base wafer and the bond wafer using the center of the base wafer as a processing center that is a rotation center when processing the peripheral portion of the bonded wafer.
5. 5. The edge trimming processing apparatus according to claim 4, wherein when the bond wafer protrudes from a contour of the base wafer, the processing unit grinds peripheral portions of the base wafer and the bond wafer with a center of the base wafer as the processing center.
6. 6. The edge trimming processing apparatus according to claim 4, wherein the processing unit grinds peripheral portions of the base wafer and the bond wafer around the processing center set based on a trimming width determined based on a maximum value and a minimum value of an outer diameter of the bonded wafer and a center position of the bond wafer as a rotation center.
Citation Information
Patent Citations
Manufacture of laminated wafer
JP1993226305A
Periphery grinding apparatus and grinding method of bonded substrate
JP2006253387A
Positional shift detector for laminated substrate and semiconductor manufacturing device using the same, and positional shift detection method for laminated substrate
JP2012007898A
Wafer detection method
JP2015102389A
Processing method
JP2017188599A