Plastic alloy earplug core
The push-on earplug with a polyamide-polypropylene core and foamable outer layer addresses manufacturing challenges and hygiene issues, enabling direct insertion and efficient sound attenuation.
Patent Information
- Application Number
- JP2022518637
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-09-24
- Filing Date
- 2020-09-15
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2040-09-15
AI Technical Summary
Push-in earplugs are costly and pose manufacturing challenges due to difficult assembly and hygiene issues from compressing the sound-attenuating portion before insertion.
A push-on earplug design featuring an elongated core made of a polyamide and polypropylene blend, coated with a foamable outer layer that thermally bonds during activation, allowing direct insertion of the sound-attenuating portion without compression.
The design enables efficient manufacturing, improves hygiene by eliminating the need for rolling, and provides effective sound attenuation with a rigid core for comfortable insertion.
Smart Images

Figure 0007573604000002 
Figure 0007573604000003 
Figure 0007573604000004
Abstract
Description
[Background technology]
[0001] The use of hearing protection and noise attenuation devices is well known, and various types of devices have been considered, including earplugs and semi-aural devices constructed partially or completely from foam or rubber materials that are inserted into or placed over a user's ear canal to physically block the passage of sound waves to the inner ear.
[0002] Compressible or "roll-up" type earplugs generally have a compressible, resilient body portion and may be made of a suitable slow recovery foam material. The earplug can be inserted into a user's ear canal by first rolling it between the fingers to compress the body portion, then forcing the body portion into the ear canal, and then allowing the body portion to expand to fill the ear canal.
[0003] Push-in earplugs are also contemplated and may include a compressible dampening portion and a rigid portion extending from the dampening portion. To insert a push-in earplug, a user grasps the rigid portion and pushes the dampening portion into the ear canal with an appropriate level of force. The dampening portion compresses once seated in the ear canal. Push-in earplugs can allow for quick and easy insertion of the earplug into the ear canal and can improve hygiene by minimizing contact with the dampening portion of the earplug prior to insertion.
[0004] While push-in earplugs exhibit desirable properties in a variety of applications, they can be expensive and pose difficult manufacturing challenges. Summary of the Invention
[0005] A push-in earplug is provided. The push-in earplug comprises an elongated core comprising a first material and a second material. The push-in earplug also comprises an outer layer comprising a foamable material, the outer layer covering at least a portion of an outer surface of the elongated core. The second material is configured to thermally bond to the outer layer during activation of the foamable material. [Brief description of the drawings]
[0006] [Figure 1] 1 is a cross-sectional view of a push-in earplug according to the present disclosure.
[0007] [Diagram 2] 1 is a micrograph of a push-in earplug core showing the blended polymer core of an earplug in one embodiment of the present invention.
[0008] [Figure 3A] 1A-1D are cross-sectional views of exemplary push-in earplugs according to the present invention, with sound-attenuating portions having various exemplary shapes. [Figure 3B] 1A-1D are cross-sectional views of exemplary push-in earplugs according to the present invention, with sound-attenuating portions having various exemplary shapes. [Figure 3C] 1A-1D are cross-sectional views of exemplary push-in earplugs according to the present invention, with sound-attenuating portions having various exemplary shapes. [Figure 3D] 1A-1D are cross-sectional views of exemplary push-in earplugs according to the present invention, with sound-attenuating portions having various exemplary shapes.
[0009] [Figure 4] 1A-1C are perspective views of a preform including an elongated core and an outer layer at intermediate stages in an exemplary method of making an earplug.
[0010] [Diagram 5] 1 is a schematic representation of an exemplary manufacturing process according to the present invention.
[0011] [Figure 6A] FIG. 2 is a cross-sectional view of an example of a mold used in an exemplary embodiment of the present invention. [Figure 6B] FIG. 2 is a cross-sectional view of an example of a mold used in an exemplary embodiment of the present invention.
[0012] [Figure 7A] FIG. 2 is a cross-sectional view of an example of a mold used in an exemplary embodiment of the present invention. [Figure 7B] FIG. 2 is a cross-sectional view of an example of a mold used in an exemplary embodiment of the present invention.
[0013] [Figure 8] 1 is a schematic representation of an exemplary manufacturing process according to the present invention.
[0014] [Figure 9] 1 is a method of making a push-in earplug in an exemplary embodiment of the present invention.
[0015] [Figure 10A] FIG. 1 shows an earplug and a preform as discussed in the examples. [Figure 10B] FIG. 1 shows an earplug and a preform as discussed in the examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] By "mold" is meant a hollow form that may or may not impart a shape to a component placed within the hollow form.
[0017] "Thermally bonded" means that the molecules of two materials or surfaces, when in the molten phase, have diffused into the other material or surface such that a bond is formed. No chemical bond exists or provides the primary source of bonding between the thermally bonded materials or surfaces.
[0018] "Thermoplastic" means a polymer that can be repeatedly heated and remolded and retains its shape upon cooling.
[0019] "Thermoset" means a polymer that can be irreversibly cured.
[0020] "Unactivated," when referring to a blowing agent, means that the blowing agent can be further activated to promote the formation of gas or bubbles in the material.
[0021] Unless otherwise indicated, all compositions are presented as weight percent.
[0022] Earplugs that provide hearing protection to a user, and methods of manufacturing the earplugs, are provided in the following description. The earplugs described herein include a relatively rigid elongated core that is covered, directly or indirectly, by a relatively soft outer layer. The outer layer includes a compressible, acoustically attenuating portion that may be inserted into a user's ear canal, and a stem portion that the user may grasp to handle the earplug. Such earplugs can be inserted into the ear canal without first requiring the acoustically attenuating portion to be compressed or "rolled."
[0023] 1 is a cross-sectional view of a push-in earplug according to the present disclosure. Earplug 100 is a push-in earplug comprising an elongated core 110 having a first end 111 and a second end 112 and an outer major surface 113. Earplug 100 further comprises an outer layer 120 bonded directly or indirectly to at least a portion of outer major surface 113 of elongated core 110. Outer layer 120 includes, for example, an acoustically attenuating portion 121 for at least partial insertion into a user's ear canal and a stem portion 122 having a smaller diameter and a greater average density than acoustically attenuating portion 121.
[0024] During insertion of the earplug 100, the stem portion 122 and elongated core 110 function as a handle that a user may grasp. The earplug 100, specifically the sound attenuating portion 121, is brought close to the user's ear and inserted into the ear canal. The sound attenuating portion 121 is compressed when positioned, and the elongated core 110 provides sufficient rigidity to facilitate insertion. In use, the sound attenuating portion 121 is positioned substantially within the ear canal to block the passage of sound, and the stem portion 122 extends outwardly from the ear canal to provide a handle for removing the earplug.
[0025] In one embodiment, the elongated core 110 has a substantially uniform circular cross-section anywhere between the first end 111 and the second end 112, and the elongated core 110 exhibits a generally cylindrical shape. The circular cross-section can minimize edges that may cause discomfort by contacting a portion of the user's ear. In various other exemplary embodiments, the elongated core may have a triangular cross-section, a square cross-section, or other suitable cross-section, or may have a cross-section that varies along the length of the earplug 100. The outer major surface 113 may have a knurled, grooved, or otherwise textured surface. Such a surface can increase the surface area that contacts the outer layer 120 or an intermediate layer so that a robust bond is created. In some embodiments, the elongated core 110 includes multiple concentric layers, such as layers to provide a desired stiffness, as well as layers that promote a robust bond with the outer layer or provide other desired properties.
[0026] The earplug 100 further includes an outer layer 120 that substantially covers, directly or indirectly, the elongated core 110. In one embodiment, the outer layer 120 includes both the acoustically attenuating portion 121 and the stem portion 122. In one embodiment, the outer layer 120 substantially surrounds the outer major surface 113 of the elongated core 110 and extends from the first end 111 to the second end 112 of the elongated core 110. In some embodiments, the outer layer 120 is a continuous layer such that a portion of the acoustically attenuating portion 121 contacts a portion of the stem portion 122. The first end 111 and the second end 112 of the elongated core 110 may be at least partially exposed, and the elongated core 110 may be a color similar to that of the outer layer 120 to hide the presence of the elongated core 110, or a color different from that of the outer layer 120 to indicate the presence of the elongated core 110. Acoustic attenuating portion 121 is disposed near first end 111 of elongated core 110 and is shaped to be received in a user's ear canal. In one embodiment, acoustic attenuating portion 121 has a bell shape and has a diameter at its widest point that is greater than the diameter of stem portion 122. In various other embodiments shown in Figures 3A-3D, for example, acoustic attenuating portions 125, 126, 127, 128 may each be bullet-shaped, hemispherical, conical, mushroom-shaped, or otherwise shaped to provide a desired fit or suit a particular application.
[0027] As described in more detail below, outer layer 120 is formed of a material that is configured to expand when heated to fill a mold, allowing for the creation of a variety of shapes for sound-attenuating portion 121. The material of outer layer 120 may be selected to control the brittleness of outer layer 120 so that it does not easily break or crumble during use. The brittleness of the earplug may be controlled in part by selecting a material having an appropriate molecular weight, with higher molecular weights generally resulting in less brittle earplugs.
[0028] The density of the outer layer 120 can be controlled during manufacturing to provide a particular density as desired for a particular application. The outer layer 120 can exhibit a density that varies through thickness, such as, for example, the outer layer 120 having an integral outer skin that is denser than the remainder of the outer layer 120. Such a skin can be present in one or both of the acoustically attenuating portion 121 and the stem portion 122. Alternatively, the acoustically attenuating portion 121 or the stem portion 122 can have a substantially uniform density. In some embodiments, the outer layer 110 is an expandable thermoplastic elastomer. The thermoplastic elastomer can be styrene-ethylene-butadiene-styrene (SEBS), styrene-isoprene rubber (SIS), or a combination thereof.
[0029] The elongated core 110 provides a substrate that the outer layer 120 may directly or indirectly cover to facilitate insertion of the earplug 100 into the user's ear canal. The elongated core 110 must have a greater stiffness or rigidity than the outer layer 120, but be soft enough to be comfortable and safe for the user. The elongated core 110 must provide sufficient stiffness that the earplug 100 may be placed at least partially in the user's ear for use by forcing the sound attenuating portion 121 into the ear canal with adequate force. A sufficiently stiff elongated core 110 in combination with an appropriate outer layer 120 allows the earplug 100 to be placed at least partially in the user's ear without first having to compress or "roll" the sound attenuating portion 121. Direct insertion without first having to compress or "roll" the sound attenuating portion 121 improves hygiene, for example by limiting contact with the sound attenuating portion 121 prior to placement in the ear. The elongate core 110 must also exhibit an appropriate level of flexibility so that it can deform slightly to the contours of the ear canal when placed for use.
[0030] Therefore, one important aspect of earplug design and construction is the selection of materials for the elongated core 110 and outer layer 120. During the manufacturing process, the foamed outer layer 120 is exposed to high temperatures and expands to fit the shape of a mold. At the same time, the foamed layer 120 is also thermally bonded to the core 110. This requires at least some compatibility with the thermoplastic elastomer.
[0031] The core material should not melt or deform at the temperatures required for expansion of the foamable overcoating layer 120. However, the elongated core 110 is desirably made of a material that will thermally bond with the outer layer 120. Although the elongated core 110 will undergo some blending with the outer layer 120 during manufacture, the core should also maintain its own structural integrity. Additionally, the core material desirably has an adjustable stiffness so that the earplug is stiff enough to be inserted into a user's ear, yet still comfortable during use.
[0032] Several different materials were investigated as possible materials for the preferred elongated core 110. Polyolefins are miscible with many suitable thermoplastic elastomers. Miscibility is important because the separate core 110 and outer layer 120 do not experience chain entanglement, and surface forces (van der Waals forces) are not sufficient to bond the layers together. Polypropylene was chosen for its higher heat resistance. A polypropylene core deformed too much and did not provide enough support during the molding process. Filling the polypropylene core with a mineral-based filler material provided additional support, but resulted in a core that was too stiff. Other polymer bases were also investigated, including acrylic, acrylonitrile butadiene styrene (ABS), polyurethane, and the like.
[0033] A third layer to be added to the structure has also been investigated, but this would add an additional step to the manufacturing process, increasing cost and complexity.
[0034] 2 is a micrograph of a push-in earplug core showing the blended polymer core of an earplug in one embodiment of the present invention. The blended core 150 has a polyamide matrix 170 supporting multiple polypropylene regions 160.
[0035] It has been found that a blend of polypropylene and polyamide provides sufficient structure during the manufacturing process while also allowing for thermal bonding between the core and the foamable overcoat layer. The polyamide forms a lattice structure 170 with a high melting point support scaffold having a melting temperature of about 220° C. The polypropylene regions 160 facilitate bonding between the outer layer 120 and the core 110. The polyamide has a high enough melting temperature to remain solid during the foaming process, allowing for thermal bonding between the polypropylene regions 220 and the outer layer 120.
[0036] In some embodiments, the core 110 comprises at least about 50%, or at least about 55%, or at least about 60% of the polyamide blend. In some embodiments, the core 110 comprises about 65% of the polyamide blend and about 35% of polypropylene. The polyamide blend comprises an impact modifier. The impact modifier is at least 10%, or at least 15%, or at least 20%, or at least 25% of the polyamide blend. In one embodiment, the impact modifier is maleated styrene-ethylene-butylene-styrene (SEBS). The inclusion of the impact modifier improved flexibility but surprisingly did not result in a significant reduction in the stability of the core. The inclusion of the impact modifier would have been expected to result in lower heat deflection temperatures and greater deformation when heated in a mold. However, the embodiments described herein have similar bond quality to a pure polypropylene core without deformation during manufacturing. Also, the cord-to-core tensile strength improved from 2 lbs to 6 lbs with the addition of the impact modifier. The cord bond strength must be higher than a minimum to prevent unwanted / accidental cord dislodgment. The cord-to-core tensile strength is measured with a tensile testing machine such as the Model 5967 Universal Testing System available from Instron, Inc. (Norwood, MA, USA). The cord is secured in one clamp with the plug secured in the opposite clamp. The clamps are moved apart at a given rate and the tensile force is measured with a load cell. When the force drops sharply the test is stopped. The peak force is recorded.
[0037] 3A-3D are cross-sectional views of exemplary push-in earplugs according to the present invention having sound-attenuating portions with various exemplary shapes. While FIG. 1 shows one exemplary shape of the sound-attenuating portion of a push-in earplug, other embodiments have different shapes. For example, any of the shapes of sound-attenuating portions 125, 126, 127, or 128 may be possible. Other suitable shapes are also envisioned.
[0038] 4 is a perspective view of a preform including an elongated core and an outer layer in an intermediate state of one method of manufacturing an earplug. Earplug 100 may be formed in a multiple step process. In one embodiment, earplug 100 is formed in a process that includes an intermediate state in which outer layer 120 is wrapped directly or indirectly around elongated core 110 to provide a preformed hearing protection device, such as preform 130, but does not yet include acoustic attenuating portion 121.
[0039] In the intermediate state shown in FIG. 4, the outer layer 120 of the preform 130 includes an unactivated blowing agent. In one embodiment, the unactivated blowing agent includes an expandable sphere blowing agent including thermoplastic spheres including a shell enclosing, for example, a hydrocarbon or other suitable gas that expands upon exposure to heat or other activation source. The expansion of the thermoplastic shell results in an increase in volume and a decrease in density of the material of the outer layer 120. The unactivated blowing agent may also be a chemical blowing agent including an expandable material that is incorporated or otherwise not contained in an expandable sphere. Activation of such a blowing agent causes the expandable material to expand to create voids or gaps in the material of the outer layer. In one embodiment, the outer layer 120 of the preform 130 includes an unactivated expandable sphere blowing agent and an unactivated chemical blowing agent. Activation of the blowing agent present in the outer layer 120 and the associated expansion of the outer layer 120 can be controlled to provide an earplug 100 having an acoustically attenuating portion 121 and a stem portion 122 that exhibit a desired shape, density, hardness, and other desired properties.
[0040] The presence of both the expanding spherical blowing agent and the chemical blowing agent can help provide sufficient structure and expansion so that the outer layer 120 can be properly formed during activation while reducing the hardness of the outer layer 120 from levels that would otherwise result if only the expanding spherical blowing agent were used. Some or all of the gas generated by the chemical blowing agent can escape during activation such that some or all of the gas is not present within the outer layer after activation. Some or all of the expanding spherical blowing agent can remain within the outer layer of the final earplug such that the final earplug may include thermoplastic spheres. In one embodiment, the outer layer 120 of the earplug 100 includes between 1% and 5% by weight of the blowing agent or residual of the blowing agent, and may include approximately 3% by weight of the blowing agent or residual of the blowing agent.
[0041] In the intermediate state shown in FIG. 4, the preform 130 may be cut to the desired length of an earplug 100, cut to an extended length sufficient to subsequently form multiple earplugs, or may remain uncut so that activation of the outer layer 120 occurs prior to cutting as described below with reference to FIG. 8. The preform 130 having an extended length may facilitate handling for subsequent processing and activation of the blowing agent. In one embodiment, the preform 130 is cut to an extended length that may then be cut and activated to obtain a desired quantity of earplugs 100. The extended preform 130 may be coiled or otherwise shaped for ease of transportation or handling.
[0042] 5 is a schematic representation of one manufacturing process according to the present invention. The present disclosure further provides a method of manufacturing an earplug. The method may include coating a substrate, such as an elongated core of blended polymers, with an outer layer containing an unactivated blowing agent, and activating the blowing agent to expand at least a portion of the outer layer to a desired shape.
[0043] The present invention provides a method of manufacturing a personal protective device, such as the earplug 100 described with respect to Figure 1. One method includes coating a substrate with an outer layer and applying heat to at least a portion of the outer layer to expand at least a portion of the outer layer. The expansion of the outer layer occurs due to activation of a blowing agent present in the material of the outer layer and can be controlled by placing at least a portion of the outer layer in a mold prior to expansion. The portion of the outer layer may be restricted by the shape of the mold as the outer layer expands or is shielded from the heat to limit activation of the blowing agent.
[0044] The methods described herein are suitable not only for making earplugs, but also for making components for other types of hearing protection devices and other personal protective equipment, as well as other molded or formed parts suitable for other uses. For example, the methods provide a process for producing seals for face pieces of respiratory protective equipment that can be foamed to provide a desired shape and density. Other exemplary uses include the manufacture of earmuffs, respirators, eyewear, other personal protective equipment, components of such personal protective equipment, and other applications.
[0045] One method of making a push-in earplug according to the present invention includes directly or indirectly coating a blended elongate core with an outer layer comprising an unactivated foaming agent, and activating the foaming agent in at least a portion of the outer layer to form an acoustically attenuating portion and a stem portion bonded directly or indirectly to the blended elongate core.
[0046] In one embodiment, the blended elongate core comprises a polyolefin. In one embodiment, the blended elongate core comprises an impact modifier. In one embodiment, the blended elongate core comprises at least about 50% polyamide, or at least about 60% polyamide, or at least about 65% polyamide. In one embodiment, the blended core comprises at least 10% binding component, or at least about 15% binding component, or at least about 20% binding component, or at least about 25% binding component, or at least about 25% binding component, or at least about 30% binding component, or at least about 35% binding component. In one embodiment, the binding component is polypropylene.
[0047] In one embodiment, the polyamide blend comprises at least 10% impact modifier, or at least 15% impact modifier, or at least 20% impact modifier, or at least 25% impact modifier. In one embodiment, the impact modifier is SEBS.
[0048] FIG. 5 shows a schematic of one embodiment of a method for manufacturing an earplug 200 according to the present disclosure. The elongated blended elongated core 210 is formed by extruding a first material through a first die 240 and stretching the first material to an appropriate diameter. The blended elongated core may be solid or may include longitudinal channels that extend through all or a portion of the elongated core 210 and may include one or more concentric layers with different properties. After extrusion, the blended elongated core may be cooled so that it remains stable in subsequent steps of the manufacturing process. The magnitude of the temperature change may depend on the materials used and the desired properties of the final product. In one embodiment, the elongated core 210 is cooled as needed to exhibit a temperature lower than the activation or curing temperature of the outer layer 220 at a point before being coated by the second die 250. Before being coated, the blended elongated core 210 has an elongated length and has not yet been cut to the desired length of the earplug.
[0049] In the embodiment shown in FIG. 5, the blended elongated core 210 is directly or indirectly coated with an outer layer 220 comprising a foamable material by a second die 250. The second die 250 may be a coextrusion die or other suitable die known in the art. In one embodiment, the foamable comprises a thermoplastic material and one or more unactivated blowing agents. The outer layer 220 is applied to the blended elongated core 210 while remaining at a temperature below the activation temperature of the unactivated blowing agent. In one embodiment, the outer layer comprises SEBS and a blowing agent having an activation temperature of 100° C. to 205° C., 120° C. to 190° C., or about 170° C. Other suitable materials include plasticized polyvinyl chloride, ethylene propylene diene monomer (EPDM) rubber, styrene butadiene rubber (SBR), butyl rubber, natural rubber, other thermoplastics, thermoset polymers, and other suitable materials known in the art. In embodiments where outer layer 220 includes a second material having a rubber or thermoset polymer, outer layer 220 may be applied at a temperature below the vulcanization or curing temperature of the rubber or thermoset polymer. In such embodiments, outer layer 220 may include an unactivated blowing agent and an uncured or partially cured rubber or thermoset polymer, which can then be activated and cured, respectively, using heat or other suitable activation or curing processes.
[0050] When initially applied to the blended elongated core 210, the weight percentage of the blowing agent in the outer layer 220 may be selected based on the type of thermoplastic or other material used and the desired final shape, density, hardness, or other properties of the acoustic attenuating portion 221. In one embodiment, the outer layer 220 has an initial composition of 90%-99.5% SEBS and 10%-0.5% of a suitable unactivated blowing agent, or alternatively, about 93% SEBS and 7% unactivated expandable spherical blowing agent, such as EXPANCEL 930 DU 120, EXPANCEL 920 DU 120, both available from Eka Chemicals AB, Sundsvall, Sweden.
[0051] In another embodiment, the outer layer 220 has an initial composition that includes an unactivated chemical blowing agent, such as oxybisbenzenesulfonylhydrazide (OBSH), available from Biddle Sawyer Corp. (New York, N.Y.). The presence of a chemical blowing agent, such as an OBSH blowing agent, can result in an acoustic damping portion having a lower hardness value than an acoustic damping portion formed from an outer layer that includes an expandable spherical blowing agent, such as EXPANCEL, as the only blowing agent.
[0052] In one embodiment, the outer layer 220 includes a non-activated expandable spherical blowing agent and a non-activated chemical blowing agent. The presence of both the expandable spherical blowing agent and the chemical blowing agent may help provide sufficient structure so that the outer layer is properly formed and may not be present with only the chemical blowing agent, while at the same time reducing the hardness of the outer layer from a level that would otherwise result if only the expandable spherical blowing agent were used. Thus, the combination of the chemical blowing agent and the expandable spherical blowing agent may result in an outer layer having a hardness level suitable for a desired application, such as insertion into the ear canal. In one embodiment, the outer layer 220, when initially applied, may include about 0.5% to 3% by weight of the non-activated chemical blowing agent, or about 2% by weight of the non-activated chemical blowing agent, and about 0.5% to 9.5% by weight of the non-activated expandable spherical blowing agent, or about 2% by weight of the non-activated expandable spherical blowing agent. Outer layer 220 may also include other suitable blowing agents or various combinations of EXPANCEL blowing agents, OBSH blowing agents, and other suitable blowing agents. Outer layer 220 may further include pigments to impart desired color, antioxidants, UV stabilizers, and oils or waxes to aid in extrusion and demolding, as known in the art.
[0053] In some exemplary embodiments, the outer layer 220 is in a molten state when coated over the blended elongated core 210. As a result, it is believed that the molecules of the outer layer 220 and the elongated core 210, or the molecules of one or more intermediate layers, diffuse into each other's materials or surfaces and a thermal bond is formed. When the materials or surfaces cool and solidify, the outer layer 220 remains thermally bonded directly or indirectly to the elongated core 210. In one embodiment, there is no significant chemical bond and the primary source of bonding between the elongated core 210 and the outer layer 220 is thermal bonding. In other exemplary embodiments, the outer layer 220 contacts the elongated core 210 or one or more intermediate layers when coated over the elongated core 210, but no significant bond is formed between the outer layer 220 and the elongated core 210 or between the one or more intermediate layers. Upon activation and / or curing of the outer layer 220, a thermal bond can be formed directly or indirectly between the outer layer 220 and the elongated core 210.
[0054] In other exemplary embodiments, the elongated core 210 may be coated with the outer layer 220 or one or more intermediate layers by lamination, molding, spraying, dipping, or other suitable process known in the art, instead of or in addition to the second die 250. Such steps may occur before or after the elongated core 210 is cut to the desired length. Regardless of the process used, the temperature of the outer layer 220 should remain below the activation temperature of the blowing agent so that the blowing agent remains unactivated during the coating process. If an uncured or partially cured material, such as EPDM rubber or a thermoset polymer, is included in the outer layer 220, the temperature of the outer layer 220 must remain below the cure temperature of the material.
[0055] In one embodiment, the blended core 210 coated with the outer layer 220 is cut to the desired earplug length with a cutter 260. The result is a preform 230 having the blended elongated core 210 and the outer layer 220, which includes an unactivated foaming agent that can then be activated to produce an earplug having an acoustically attenuating portion 221 and a stem portion 222.
[0056] The cutter 260 may cut the preform 230 into a desired length of earplug 200 or into an extended length sufficient to subsequently form multiple earplugs. In one embodiment, the preform 230 is cut into extended lengths that can then be cut and activated, or activated and cut, to obtain a desired quantity of earplugs 200. The extended preform 230 may be coiled or otherwise shaped for ease of handling or transportation.
[0057] In one embodiment, the unactivated blowing agent present in the outer layer 220 comprises thermoplastic spheres encapsulating a hydrocarbon or other expandable material. The application of an appropriate amount of heat causes the thermoplastic shell and the hydrocarbon to expand. In another exemplary embodiment, the blowing agent comprises an expandable material that produces gas when exposed to heat or other activation source, either alone or in combination with the expandable sphere blowing agent, embedded or otherwise unencapsulated. If left unchecked, activation of the blowing agent produces gas bubbles in the outer layer 220, ultimately increasing the volume and decreasing the density of the outer layer 220. The expansion of the outer layer 220 can be controlled by the thickness and composition of the outer layer 220, by selectively applying heat, catalyst, or other activation source, and / or by placing at least a portion of the preform 230 in a mold to limit the expansion of the outer layer 220 when the blowing agent is activated.
[0058] In the exemplary method shown in Figures 6A and 6B, a mold 270 is used to control the expansion of the outer layer 220. The mold 270 includes a first cavity 271 in the form of a stem portion that receives a portion of the preform 230. The preform 230 may be cut to the desired earplug 200 length before being placed into the mold 270. Alternatively, the preform 230 may be an extended length and cut to length after insertion into the mold 270. Cutting the preform 230 after insertion into the mold 270 may allow for easier handling and insertion. Heat is applied to the exposed portion of the preform 230 to raise the temperature of the outer layer 220 to at least the activation temperature of the blowing agent present in the outer layer 220, causing the outer layer 220 to expand as shown in Figure 6B. The portion of the earplug 200 disposed in the first cavity 271 may be effectively shielded from the heat such that activation of the blowing agent is limited. Alternatively, or in addition, the first cavity 271 restrains the outer layer 220, substantially restricting the expansion caused by the activation of the blowing agent that would otherwise result in a larger volume and lower density outer layer. The blended elongated core 210 and outer layer 220 are then cooled and ejected from the mold 270. The finished earplug 200 includes an acoustically attenuating portion 221 formed by the exposed outer layer, which is free to expand, and a stem portion 222 that was partially restrained within the mold 270 during the activation of the blowing agent. Due to the mold restraint and / or limited activation of the blowing agent, the stem portion 222 may have a higher average density than the acoustically attenuating portion 221 and / or a higher hardness than the acoustically attenuating portion 221.
[0059] In the exemplary embodiment of Figures 7A and 7B, a mold 370 is used to control the expansion of the outer layer 320 of the preform 330. The mold 370 includes a first cavity 371 in the form of a stem portion that receives a portion of the preform 330. The mold 370 further includes a second cavity 372 in the form of an acoustically attenuating portion. When the preform 330 is initially placed in the mold 370, a gap 375 exists between the preform 330 and the outer periphery of the second cavity 372. In some embodiments, a small gap 376 may exist between the preform 330 and the outer periphery of the first cavity 371. Upon application of heat or other suitable activation source, a portion of the outer layer 320 expands to fill the gap 375 and substantially conform to the shape of the second cavity 372. The portion of the earplug 300 disposed in the first cavity 371 may be effectively shielded from heat such that activation of the blowing agent is limited. Alternatively, or in addition, expansion of outer layer 220 that would otherwise occur during activation of the blowing agent is restrained by first cavity 371. Furthermore, when heat is applied to soften outer layer 320 and the blowing agent is activated, outer layer 320 can expand to fill first cavity 371, initially allowing the portion of outer layer 320 in first cavity 371 to flow into second cavity 372 to fill gap 375. In one embodiment, mold 370 includes small vent holes to allow excess gas to escape while preventing the passage of any molten material.
[0060] In one embodiment, the mold 370 is oriented such that the first cavity 371 is directed above the second cavity 372 during part or all of the activation process. Such an orientation may allow material to flow from the first cavity 371 to the second cavity 372 during activation. Additionally, an orientation in which the first cavity 371 is directed above the second cavity 372 may promote the formation of an integral skin over the acoustic attenuating portion 321, as any bubbles or voids formed during activation of the blowing agent may tend to migrate upwardly and away from the underside of the cavity 372.
[0061] Earplug 300 is then cooled and ejected from mold 370. The finished earplug 300 includes an acoustically attenuating portion 321 having the shape of second cavity 372 of mold 370 and a stem portion 322 having the shape of first cavity 371 of mold 370. Due to the constraints of first cavity 371 and / or the limited activation of the blowing agent in the area of first cavity 371, stem portion 322 may have a higher average density and / or hardness than acoustically attenuating portion 321.
[0062] 7A and 7B, earplug 300 is formed from a preform 330 having a total length l in the longitudinal direction of about 15 mm to 40 mm, or about 25.5 mm. Outer layer 320 has an outer diameter d1 of about 2.5 mm to 6.5 mm, or about 4.5 mm, and elongated core 310 has an outer diameter d3 of about 1.5 mm to 3.5 mm, or about 2.5 mm. After activation of the outer layer 320 as described above, the final earplug 300 has an overall length L in the longitudinal direction of about 15 mm to 40 mm, or about 25.5 mm, the acoustic attenuating portion 321 has an outer diameter D1 at its widest point of about 8 mm to 16 mm, or about 12.5 mm, the stem portion 322 has a diameter D2 of about 3 mm to 10 mm, or about 6.5 mm, and the elongated core 310 has an outer diameter D3 of about 1.5 mm to 3.5 mm, or about 2.5 mm, as shown in FIG. 7B. Based on the materials of the outer layer 320 and the elongated core 310, and as needed, the dimensions of the preform 330 and the finished earplug 300 can be varied to form a final earplug 300 with desired characteristics for a particular application. Although not shown in FIGS. 7A and 7B, it is also expressly contemplated that in some embodiments, there may be a channel extending partially or completely from a first end of the earplug to a second end of the earplug.
[0063] 8 is a schematic representation of an exemplary manufacturing process according to the present invention. Components of schematic 400 are not necessarily drawn to scale.
[0064] The first material 402 is provided to a first extruder 410 which outputs an extruded elongated core 415. The elongated core 415 is provided along with a second material 422 to a second extruder 422 which outputs a preform 425. The preform 425 includes an elongated core with an overlayer formed from the second material. The second material 422 may include a foamable material.
[0065] The preform 425 is provided to a mold cavity 452 within a mold 450. Heat 454 or another activation mechanism is applied, causing the foamable overlayer to expand within the mold cavity 452 and conform to the shape of the mold cavity 452. Once the activation process is complete, the push-in earplug 460 is removed from the mold 450.
[0066] Extruders 410 and 420 may be configured to stretch material 402, 422 to an appropriate diameter. Either of extruders 410 and 420 may also include a cutting mechanism configured to cut the extruded material to the desired length of the in-ear plug. However, in another embodiment, the cutting mechanism (not shown) is a separate operation that occurs prior to providing preform 425 to mold 450.
[0067] Although an extruder is shown as a mechanism for forming the core 415 and preform 425, it is also envisioned that the core 415 can be coated with an outer layer using lamination, molding, spraying, dipping, or any other suitable process known in the art.
[0068] The blended elongated core 415 and coated core may be cooled during the extrusion and / or cutting operations. FIG. 8 illustrates an embodiment in which the entire preform 425 is placed in the mold cavity 452. However, in some embodiments, only a portion of the preform 425, for example the acoustically attenuating portion, is placed in the mold. In one embodiment, a blowing agent is activated by heat or other activation source to expand the outer layer of the preform 425. In some embodiments in which the outer layer comprises an uncured or partially cured material, application of heat or other activation source also hardens the outer layer. In one embodiment, the mold cavity 452 includes a first cavity in the form of a stem portion and a second cavity in the form of an acoustically attenuating portion. Upon application of heat or other suitable activation source, a portion of the outer layer expands to fill the second cavity and substantially conforms to the shape of the second cavity, while the portion disposed within the first cavity is effectively shielded from the heat such that activation of the blowing agent is limited. Alternatively, or in addition, the expansion of the outer layer that would otherwise occur during activation of the blowing agent is substantially constrained by the shape of the first cavity. In one embodiment, the mold 450 includes small vent holes to allow excess gas to escape while preventing the passage of any molten material.
[0069] In another exemplary embodiment, only a portion of the preform 425 is placed into the mold cavity. The mold cavity can be in the form of a stem to substantially restrain the expansion of a portion of the preform 425 to form the stem, while the remainder of the preform is free to expand to form the acoustically attenuating portion. Alternatively, the mold cavity can be in the form of an acoustically attenuating portion to restrain the expansion of a portion of the preform and selectively activate to form the acoustically attenuating portion, while the remainder of the preform 425 is activated or only partially activated to form the stem.
[0070] 9 is a method of manufacturing a push-in earplug in an exemplary embodiment of the invention. Method 500 may be useful for forming any of the in-ear earplugs described herein. Method 500 may be performed using a system similar to that generally described with respect to FIG. 8, or using another suitable system.
[0071] In step 510, the core is extruded. In some embodiments, the core 510 comprises at least about 50%, or at least about 55%, or at least about 60% of the polyamide blend. In some embodiments, the core 110 comprises about 65% of the polyamide blend and about 35% of the polyamide blend. The polyamide blend includes an impact modifier. The impact modifier is at least 10%, or at least 15%, or at least 20%, or at least 25% of the polyamide blend. In step 520, an overcoat layer is extruded onto the core. In one embodiment, the overcoat layer substantially covers the elongated core. The overcoat layer is formed of a material that is configured to expand when heated to fill the mold cavity. The material may be selected to control the brittleness of the outer layer so that it does not easily break or crumble during use. The brittleness of the earplug may be controlled in part by selecting a material with an appropriate molecular weight, with higher molecular weights generally resulting in a less brittle earplug. In some embodiments, the overcoat layer is an expandable thermoplastic elastomer. The thermoplastic elastomer can be styrene-ethylene-butadiene-styrene (SEBS), styrene-isoprene rubber (SIS), or a combination thereof.
[0072] At step 530, an acoustically attenuating portion is formed. This may include cutting the coated core to size, as shown in block 532. The acoustically attenuating portion may be formed by placing at least a portion of the coated core into a mold, as shown in block 534. The mold may include a cavity having the desired shape of the acoustically attenuating portion, such as the shapes shown in Figures 3A-3D, as well as other suitable shapes. Forming the acoustically attenuating portion may include activating the overcoat layer with heat, as shown in block 536. Other processing steps may be applied, as shown in block 538. For example, the outer layer may be somewhat cured.
[0073] The earplugs and methods of manufacturing earplugs described herein provide several advantages. The earplugs described herein can be comfortably positioned in the user's ear canal to provide a desired level of hearing protection, and the presence of a more rigid elongated core can improve hygiene by eliminating the need to roll the acoustically attenuating portion prior to insertion. The methods described herein allow for efficient manufacturing of earplugs. The earplugs described herein having an outer layer bonded directly or indirectly to an elongated core eliminate the cost and complexity of the additional step of joining a rigid component to the required acoustically attenuating components of many conventional push-in earplugs. The elongated core and outer layer can be thermally bonded without the need for additional adhesive or assembly steps.
[0074] The present invention has been described with reference to several embodiments thereof. The above detailed description and examples are given only for clarity of understanding. No unnecessary limitations are to be made thereby. It will be apparent to those skilled in the art that many changes can be made in the described embodiments without departing from the scope of the present invention. Therefore, the scope of the present invention should not be limited to the exact details and structures described herein, but rather by the structures described in the language of the claims and the equivalents of these structures. Any feature or characteristic described with respect to any of the above embodiments can be incorporated individually or in combination with any other feature or characteristic, and are presented in the above order and combinations merely for clarity. Embodiment
[0075] Embodiment 1 is a push-in earplug. The push-in earplug has an elongated core having a first material and a second material. The push-in earplug also has an outer layer including a foamable material, the outer layer covering at least a portion of the outer surface of the elongated core. The second material is configured to thermally bond to the outer layer during activation of the foamable material.
[0076] Embodiment 2 includes the features of embodiment 1, except that the expandable material includes a blowing agent that increases the volume of the outer layer when activated.
[0077] Embodiment 3 includes the features of embodiment 2, except that the blowing agent includes a non-activated expandable spherical blowing agent.
[0078] Embodiment 4 includes the features described in embodiment 2, except that the blowing agent includes a non-activated chemical blowing agent.
[0079] Embodiment 5 includes the features described in any one of embodiments 2-4, except that the blowing agent is heat activated.
[0080] Embodiment 6 includes the features of embodiment 5, except that the blowing agent is heat activated at a temperature that allows for thermal bonding with the second material.
[0081] Embodiment 7 includes the features of embodiment 6, except that the temperature is lower than the melting temperature of the first material.
[0082] Example 8 includes the features of any one of Examples 1-7, except that the elongate core has a first stiffness and the outer layer has a second stiffness, the first stiffness being greater than the second stiffness.
[0083] Example 9 includes the features of any one of Examples 1-8, except that the first material is a polyamide.
[0084] A tenth embodiment includes the features of any one of the first to ninth embodiments, except that the second material is polypropylene.
[0085] An eleventh embodiment includes the features of any one of the first to tenth embodiments, except that the first material is at least about 50% by weight of the elongate core.
[0086] Example 12 includes the features described in example 11, except that the first material is at least about 60% by weight of the elongate core.
[0087] Example 13 includes the features of example 12, except that the first material is at least 65% by weight of the elongate core.
[0088] Example 14 includes the features of any one of Examples 9-13, except that the first material also includes an impact modifier.
[0089] Embodiment 15 includes the features described in embodiment 14, except that the impact modifier is at least about 10% of the first material.
[0090] Embodiment 16 includes the features described in embodiment 15, except that the impact modifier comprises at least about 15% of the first material.
[0091] Embodiment 17 includes the features described in embodiment 16, except that the impact modifier is at least about 20% of the first material.
[0092] Embodiment 18 includes the features described in embodiment 17, except that the impact modifier is at least about 25% of the first material.
[0093] Embodiment 19 includes the features of any one of embodiments 14-18, except that the impact modifier includes styrene-ethylene-butylene-styrene.
[0094] Example 20 includes the features of any one of Examples 1-19, except that the first material and the second material are co-extruded.
[0095] Embodiment 21 includes the features of any one of embodiments 1-20, except that the outer layer is extruded onto an elongate core.
[0096] Embodiment 22 is an article. The article has a substrate. The substrate comprises an extruded mixture of a first material and a second material. The article also comprises an outer layer comprising a third material. The outer layer at least partially covers an outer surface of the substrate. The third material comprises an activatable blowing agent. The activatable blowing agent thermally bonds with the second material during activation.
[0097] Example 23 includes the features of example 22, except that the article is an earplug.
[0098] Embodiment 24 includes the features of either embodiment 22 or 23, except that the blowing agent is configured to expand upon activation.
[0099] Embodiment 25 includes the features described in embodiment 24, except that the blowing agent is configured to expand upon activation to assume the shape of the mold.
[0100] Example 26 includes the features of any one of Examples 22-25, except that the first material includes a polyamide and the second material includes a polyolefin.
[0101] Embodiment 27 includes the features of embodiment 26, except that the polyolefin is polypropylene.
[0102] Example 28 includes the features of any one of Examples 22-27, except that the first material is at least about 50% of the extruded mixture.
[0103] Example 29 includes the features of any one of Examples 22-28, except that the first material is at least about 60% of the extruded mixture.
[0104] Example 30 includes the features of any one of Examples 22-29, except that the first material is at least about 65% of the extruded mixture.
[0105] Embodiment 31 includes the features of any one of embodiments 22-30, except that the first material also includes an impact modifier.
[0106] Embodiment 32 includes the features described in embodiment 31, except that the impact modifier is at least about 10% of the first material.
[0107] Embodiment 33 includes the features of embodiment 31, except that the impact modifier is at least about 15% of the first material.
[0108] Embodiment 34 includes the features described in embodiment 31, except that the impact modifier is at least about 20% of the first material.
[0109] Embodiment 35 includes the features described in embodiment 31, except that the impact modifier is at least about 25% of the first material.
[0110] Embodiment 36 includes the features of any one of embodiments 31-35, except that the impact modifier is styrene-ethylene-butylene-styrene.
[0111] Example 37 includes the features of any one of Examples 22-36, except that the third material is extruded onto the substrate.
[0112] Example 38 includes the features of any one of Examples 22-37, except that the outer layer forms a portion of the hearing protective device.
[0113] Example 39 includes the features of any one of Examples 22-38, except that the outer layer forms part of the seal of the facepiece.
[0114] Embodiment 40 includes the features of any one of embodiments 22-39, except that the outer layer forms part of the respiratory protection device.
[0115] Example 41 includes the features of any one of examples 22-40, except that the outer layer forms a portion of the earmuff.
[0116] Example 42 includes the features of any one of Examples 22-41, except that the outer layer forms a portion of an eyewear article.
[0117] Embodiment 43 is a method of making an article. The method includes forming a preform having a first end portion and a second end portion opposite the first end portion by coating a substrate with an outer layer. The substrate includes a first material coextruded with a second material. The outer layer includes a third material, the third material extending at least partially from the first end portion to the second end portion. The method also includes disposing the first end portion in a first mold cavity and disposing the second end portion in a second mold cavity, the first mold cavity having a diameter at its widest point less than a diameter of the second mold cavity. The method also includes applying heat to at least a portion of the outer layer at the second end portion such that at least a portion of the outer layer expands and conforms to a shape of the second mold cavity, the outer layer thermally bonds to the substrate, the first end portion forms the stem, and the second end portion forms the acoustic damping portion.
[0118] Embodiment 44 includes the features of embodiment 43, except that the third material includes a non-activated expandable spherical blowing agent.
[0119] Example 45 includes the features of example 43 or 44, except that applying heat includes subjecting a portion of the outer layer to a temperature between 100°C and 205°C.
[0120] An embodiment 46 includes the features of any one of claims 43 to 45, however, the thermal bonding comprises bonding of a second material to a third material.
[0121] Embodiment 47 includes the features of any one of claims 43 to 46, except that the third material includes a non-activated chemical blowing agent.
[0122] An embodiment 48 includes the features of any one of claims 43 to 47, except that the first material comprises polyamide.
[0123] Embodiment 49 includes the features of any one of claims 43 to 48, except that the first material includes an impact modifier.
[0124] An embodiment 50 includes the features of any one of claims 43 to 49, however, the second material comprises polypropylene.
[0125] Example 51 includes the features of any one of Examples 43-50, except that the first material includes a scaffold structure within the substrate and the second material includes at least some distinct regions within the scaffold structure.
[0126] Embodiment 52 includes the features of any one of embodiments 43-50, except that the first material is at least 50% of the substrate.
[0127] Example 53 includes the features of any one of Examples 43-52, except that the first material is at least 60% of the substrate.
[0128] Example 54 includes the features of any one of Examples 43-53, except that the first material is at least about 65% of the substrate.
[0129] Embodiment 55 includes the features of any one of embodiments 49-54, except that the impact modifier is at least about 10% of the first material.
[0130] Embodiment 56 includes the features of any one of embodiments 49-54, except that the impact modifier is at least about 15% of the first material.
[0131] Embodiment 57 includes the features of any one of embodiments 49-54, except that the impact modifier is at least about 20% of the first material.
[0132] Embodiment 58 includes the features of any one of embodiments 49-54, except that the impact modifier is at least about 25% of the first material.
[0133] Example 59 includes the features of any one of Examples 43-58, except that the outer layer forms a portion of the hearing protective device.
[0134] Embodiment 60 includes the features of any one of embodiments 43-58, except that the outer layer forms part of the seal of the facepiece.
[0135] Embodiment 61 includes the features of any one of embodiments 43-58, except that the outer layer forms part of a respiratory protection device.
[0136] Example 62 includes the features of any one of examples 43-58, except that the outer layer forms a portion of the earmuff.
[0137] Embodiment 63 includes the features of any one of embodiments 43-58, except that the outer layer forms a portion of an eyewear article.
[0138] Embodiment 64 is a method of making an article. The method includes coating a substrate with an outer layer to prepare a preform having a first end portion and a second end portion. The substrate includes a first material and a second material, and the outer layer includes a third material, the third material including a blowing agent having an activation temperature. The third material has a temperature less than the activation temperature. The method also includes placing the first end portion of the preform in a first cavity of a mold and placing the second end portion in a second cavity of a mold, the first mold cavity having a diameter at its widest point less than a diameter of the second mold cavity. The method also includes raising the temperature of the second end portion to at least an activation temperature of the blowing agent to activate the blowing agent in the second end portion and form the second end portion into an acoustically attenuating portion.
[0139] Embodiment 65 includes the features of embodiment 64, except that the first material is a polyamide.
[0140] Embodiment 66 includes the features of any of embodiments 64 or 65, except that the first material includes an impact modifier.
[0141] Embodiment 67 includes the features described in embodiment 66, except that the impact modifier is at least about 10% of the first material.
[0142] Embodiment 68 includes the features described in embodiment 66, except that the impact modifier is at least about 15% of the first material.
[0143] Embodiment 69 includes the features of embodiment 66, except that the impact modifier is at least about 20% of the first material.
[0144] Embodiment 70 includes the features described in embodiment 66, except that the impact modifier is at least about 25% of the first material.
[0145] Example 71 includes the features of any one of Examples 64-70, except that the first material and the second material are co-extruded.
[0146] Example 72 includes the features of any one of Examples 64-71, except that the first material is at least about 50% of the substrate.
[0147] Example 73 includes the features of any one of Examples 64-72, except that the first material is at least about 60% of the substrate.
[0148] Example 74 includes the features of any one of Examples 64-73, except that the first material is at least about 65% of the substrate.
[0149] Example 75 includes the features of any one of Examples 64-74, except that coating the substrate includes extruding a third material onto the substrate.
[0150] Example 76 includes the features of any one of Examples 64-75, except that the second material is a polyolefin.
[0151] Example 77 includes the features of any one of Examples 64-75, except that the second material is polypropylene.
[0152] Example 78 includes the features of any one of examples 64-77, except that activating the blowing agent causes the second end portion to expand and conform to the shape of the second cavity.
[0153] Example 79 includes the features of any one of Examples 64-78, except that the activation temperature is lower than the melting point of the first material.
[0154] Example 80 includes the features of any one of Examples 64-79, except that the activation temperature is high enough for thermal bonding between the second material and the third material.
[0155] Embodiment 81 includes the features of any one of embodiments 64-80, except that the activation temperature is between 100°C and 205°C.
[0156] Example 82 includes the features of any one of Examples 64-81, but also includes positioning the first cavity above the second cavity during activation of the blowing agent. EXAMPLES
[0157] Core Test Method Core Binding Test The bond between the outer foam material and the core is visually assessed from the appearance of the core after the foam molding process. Specifically, the foam should be physically attached to the core after molding. The image on the right of 10A shows good foam bonding. In this image, some of the foam remains adhered to the core when the outer foam material is pulled away from the core. This indicates that the failure mode is cohesive failure of the foam. The image on the left shows a similarly shaped core after molding. In this case, the bond between the foam and the core is not maintained when the foam is pulled away. This is considered an unacceptable failure. Core Mechanical Stability Test
[0158] The mechanical stability of the core is also assessed somewhat qualitatively. Measurements of the core diameter and length are taken before molding. Failure occurs when the overall length or diameter of the core changes by more than 5% after molding, as assessed using calipers. Core Flexibility Test
[0159] Flexibility is related to the flexural modulus of the material used in the core and is believed to be unaffected by the molding process, however, highly stiff materials may not be comfortable for the end user and therefore may be rejected for this application. Working Example
[0160] The one inch cylindrical preforms shown on the left side of FIG. 10B were made by extruding a foamable material onto a polypropylene core and then cutting the resulting overcoat extrudate to one inch lengths. To evaluate different core materials, the polypropylene was extruded from the middle of the preform and replaced with a similarly sized piece of alternative core material. Alternative core materials were obtained from commercial sources as rod stock and then cut to length, or obtained in pellet form and then extruded and cut to length. Compression molding of approximately one inch long preforms resulted in a polypropylene core containing very long glass fibers.
[0161] With the alternative core material in place, the preform was placed in the mold for 5 minutes at 375F and then cooled to yield an earplug (example shown on the right side of Figure 2). The foam was then pulled away from the core material and the bond and deformation of the core was evaluated as described above. The results for the various materials tested are shown in Table 1. [Table 1]
Claims
1. an elongate core comprising a first material and a second material; an outer layer comprising an expandable material, the outer layer covering at least a portion of an outer surface of the elongate core; Equipped with the first material comprises polyamide and the second material comprises polypropylene; the second material is configured to thermally bond to the outer layer during activation of the expandable material; Push-in earplugs.
2. The push-in earplug of claim 1 , wherein the foamable material includes a foaming agent that increases the volume of the outer layer when activated.
3. The push-in earplug of claim 2 , wherein the foaming agent comprises a non-activated expandable sphere foaming agent.
4. The push-in earplug of claim 2 , wherein the foaming agent comprises a non-activated chemical foaming agent.
5. A push-in earplug according to any one of claims 2 to 4, wherein the foaming agent is heat activated at a temperature that allows thermal bonding with the second material, the temperature being lower than the melting temperature of the first material.
6. A push-in earplug according to any one of claims 1 to 5, wherein the first material also comprises an impact modifier.
7. The push-in earplug according to any one of claims 1 to 6, wherein the first material and the second material are co-extruded.
8. A push-in earplug according to any one of claims 1 to 7, wherein the outer layer is extruded onto the elongate core.
9. a substrate comprising an extruded mixture of a first material and a second material; an outer layer comprising a third material, the outer layer at least partially covering an outer surface of the substrate; and Equipped with the first material comprises polyamide and the second material comprises polypropylene; the third material includes an activatable foaming agent, the activatable foaming agent thermally bonding with the second material upon activation; Goods.
10. The article of claim 9 , wherein the blowing agent is configured to expand to the shape of a mold upon activation.
Citation Information
Patent Citations
Polypropylene composition
JP1992096956A
Earplug
JP1998314213A
Foam containing surface-modified nanoparticles
JP2004518793A
How to make earplugs
JP2015529483A
Ear-insertion member
JP2019125922A