Forming device

The molding apparatus addresses the challenge of thermal shock resistance by using inert materials and cushioning to manage thermal expansion, enabling efficient temperature changes and improved production efficiency.

JP7574751B2Active Publication Date: 2024-10-29AGC INC
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2021104796
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-06-24
Publication Date
2024-10-29
Estimated Expiration
2041-06-24

AI Technical Summary

Technical Problem

Conventional molding devices for glass sheet manufacturing are limited in their ability to rapidly change temperatures due to materials with thermal shock resistance having high reactivity with glass, leading to difficulties in increasing production efficiency.

Method used

A molding apparatus with a main body and plate members made of materials inert to molten glass, featuring a cushioning material between the inner side wall and plate members to manage thermal expansion differences.

Benefits of technology

Enables rapid temperature changes, reducing the risk of damage and enhancing production efficiency by using materials resistant to thermal shock.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007574751000001
    Figure 0007574751000001
  • Figure 0007574751000002
    Figure 0007574751000002
  • Figure 0007574751000003
    Figure 0007574751000003
Patent Text Reader

Abstract

To provide a molding device for glass plate manufacturing facility capable of quickly increasing and decreasing a temperature.SOLUTION: A molding device for forming a glass ribbon by molding molten glass housed in a housing part has a main body, and a plate member provided at a portion contacting the molten glass of the main body. Each plate member has thickness in a range between 0.5 mm to 100 mm, and is made of an inactive material to the molten glass. The housing part has an inside wall of the main body, and at least one of the plate members covers at least one part of the inside wall, and a buffer material is arranged at least one part between the inside wall and the plate member covering the inside wall.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a forming device for a glass sheet manufacturing facility. [Background technology]

[0002] Glass sheets can be manufactured continuously using processes such as, for example, the fusion process and the slit downdraw process.

[0003] For example, in the fusion method, molten glass obtained by melting glass raw materials is supplied to the top of a forming device (hereinafter referred to as a "forming device"). The forming device has a cross section that is roughly wedge-shaped with a downwardly pointed edge, and the molten glass flows down along two opposing side surfaces of the forming device. The molten glass flowing down along both side surfaces joins and is integrated at a lower end (also referred to as a "junction") of the forming device, and a glass ribbon is formed. Thereafter, the glass ribbon is pulled downward by a pulling member such as a roller while being slowly cooled, and is cut to a predetermined size (for example, Patent Document 1).

[0004] In the slit downdraw method, a forming device that contains molten glass has a slit-shaped opening at the bottom. The molten glass flows down through this opening and becomes a glass ribbon. The glass ribbon is then gradually cooled and cut to produce a glass sheet. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2016-028005 A Summary of the Invention [Problem to be solved by the invention]

[0006] In a manufacturing facility for manufacturing glass sheets by the above-mentioned method or another method, from the viewpoint of improving the manufacturing efficiency of glass sheets, it is desirable for the forming device to have a configuration that can withstand rapid temperature increase and decrease. However, in order to achieve this, it is necessary to use a material that is resistant to thermal shock for the forming device.

[0007] However, such materials having thermal shock resistance are often highly reactive with glass, and it is difficult to use them as materials for forming devices. Therefore, in conventional forming devices, the heating and cooling rates cannot be increased significantly, and therefore it is difficult to improve the production efficiency of glass sheets.

[0008] The present invention has been made in consideration of the above background, and an object of the present invention is to provide a forming device for use in a glass sheet manufacturing facility, which is capable of heating and cooling more quickly than conventional methods. [Means for solving the problem]

[0009] In the present invention, there is provided a forming apparatus for forming molten glass contained in a container to form a glass ribbon, comprising: The main body, a plurality of plate members disposed on a portion of the body that contacts the molten glass; having Each plate member has a thickness in the range of 0.5 mm to 100 mm and is made of a material that is inactive to the molten glass. The housing portion has an inner sidewall of the main body, and at least one of the plate members covers at least a portion of the inner sidewall, There is provided a molding apparatus, in which a buffer material is disposed at least partially between the inner side wall and the plate member covering the inner side wall. Effect of the Invention

[0010] The present invention can provide a forming apparatus for use in a glass sheet production facility, which is capable of heating and cooling more quickly than ever before. [Brief description of the drawings]

[0011] [Figure 1] 1 is a diagram showing a schematic configuration example of a glass sheet manufacturing facility having a forming device according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a schematic diagram showing a cross section taken along line AA of the glass plate manufacturing equipment shown in FIG. [Diagram 3] FIG. 2 is a schematic diagram showing a cross section parallel to the horizontal direction of a housing part of a molding device. [Figure 4] 1 is a schematic diagram showing a cross section parallel to the horizontal direction of one configuration example of a molding device according to one embodiment of the present invention. [Diagram 5] FIG. 11 is a perspective view showing a schematic configuration example of another manufacturing facility having a molding device according to an embodiment of the present invention. [Figure 6] 6 is a schematic cross-sectional view taken along line BB of the manufacturing equipment shown in FIG. 5. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0013] (Glass sheet manufacturing equipment having a forming device according to one embodiment of the present invention) First, with reference to Figs. 1 and 2, an outline of a glass sheet manufacturing facility having a forming device according to one embodiment of the present invention will be described.

[0014] 1 and 2 show a schematic configuration of a glass sheet manufacturing facility (hereinafter referred to as a "first manufacturing facility") 100 having a forming device according to an embodiment of the present invention. In the first manufacturing facility 100, glass sheets can be continuously manufactured by the fusion method.

[0015] FIG. 2 is a schematic cross-sectional view of the first manufacturing facility 100 taken along line AA in FIG.

[0016] 1 and 2, the first manufacturing facility 100 includes a molding device 110 according to an embodiment of the present invention, a furnace 150 that houses the molding device 110, and a plurality of rollers 160 disposed below the molding device 110. Although not shown in the drawings, the first manufacturing facility 100 further includes a cutting member below the furnace 150.

[0017] The forming apparatus 110 has a function of forming a glass ribbon GR from the molten glass MG. The forming apparatus 110 is connected to a supply pipe 105, and the molten glass MG is supplied to the forming apparatus 110 through the supply pipe 105.

[0018] The molding device 110 has a main body 120 and a plate member 130 .

[0019] The body 120 of the molding device 110 has a generally wedge-shaped cross section as shown in Fig. 2. More specifically, the body 120 has a recess 122 provided on an upper surface 121 of the body 120, a first side surface 124a and a second side surface 124b opposed to each other, and a lower end portion 129 which is an intersection of the first side surface 124a and the second side surface 124b.

[0020] The recess 122 is formed along the longitudinal direction of the main body 120, that is, along the X direction in FIGS.

[0021] The first side 124a has a first upper side 126a and a first lower side 128a. Similarly, the second side 124b has a second upper side 126b and a second lower side 128b.

[0022] The first upper side surface 126a and the second upper side surface 126b each extend in a substantially longitudinal direction (X direction) and a substantially vertical direction (Z direction) of the main body 120, and are therefore disposed substantially parallel to the XZ plane. On the other hand, the first lower side surface 128a and the second lower side surface 128b are inclined with respect to the vertical direction (Z direction) and are disposed so as to intersect with each other at a lower end portion 129 of the main body 120.

[0023] An upper portion of the first lower side surface 128a is connected to a lower portion of the first upper side surface 126a, and an upper portion of the second lower side surface 128b is connected to a lower portion of the second upper side surface 126b.

[0024] Furthermore, plate member 130 of forming device 110 is placed at least at a portion of the exposed surface of main body 120 that comes into direct contact with the glass.

[0025] For example, in the example shown in FIG. 2, the plate member 130 is arranged to cover the upper surface 121, the recess 122, the first side surface 124a (the first upper side surface 126a and the first lower side surface 128a), and the second side surface 124b (the second upper side surface 126b and the second lower side surface 128b) of the main body 120.

[0026] The molding device 110 has a shape that is substantially conformal to the shape of the main body 120. That is, the molding device 110 has an upper surface 111, a recess 112, a first side surface 114a (first upper side surface 116a and first lower side surface 118a), a second side surface 114b (second upper side surface 116b and second lower side surface 118b), and a lower end portion 119, all of which have shapes similar to the corresponding portions of the main body 120. In addition, all of these portions are formed by the exposed surface of the plate member 130.

[0027] Each roller 160 has a role of transporting the glass ribbon GR downward while adjusting the thickness of the glass ribbon GR.

[0028] In the present application, the portion of forming apparatus 110 that contains molten glass MG, including recess 112, is particularly referred to as “containing portion (of forming apparatus 110)” 140. Holding portion 170 is covered with plate member .

[0029] When a glass sheet is manufactured using such a first manufacturing facility 100 , first, molten glass MG is supplied to a forming device 110 via a supply pipe 105 .

[0030] The molten glass MG supplied to forming apparatus 110 is stored in storage section 170. However, when the molten glass MG is supplied in an amount exceeding the storage capacity of storage section 170, the molten glass MG overflows along first side surface 114a and second side surface 114b of forming apparatus 110 and flows downward.

[0031] As a result, first molten glass portion 190a is formed on first upper side surface 116a of forming apparatus 110, and second molten glass portion 190b is formed on second upper side surface 116b of forming apparatus 110.

[0032] First molten glass portion 190a then flows further downward along first lower side 118a of forming apparatus 110. Similarly, second molten glass portion 190b flows further downward along second lower side 118b of forming apparatus 110.

[0033] As a result, first molten glass portion 190a and second molten glass portion 190b reach lower end 119 of forming apparatus 110 and are integrated therein. In this way, glass ribbon GR is formed.

[0034] Thereafter, the glass ribbon GR is further pulled downward in the vertical direction by the rollers 160, and is gradually cooled in the process.

[0035] Thereafter, the glass ribbon GR that has been sufficiently cooled slowly is discharged from the furnace 150 and cut to a predetermined size by cutting means (not shown).

[0036] Through the above steps, glass sheets can be produced continuously.

[0037] (Molding device according to one embodiment of the present invention) The features of molding apparatus 110 according to one embodiment of the present invention will now be described in more detail.

[0038] From the viewpoint of improving the production efficiency of glass sheets, etc., a forming device included in a glass sheet production facility is desired to have a configuration capable of withstanding rapid temperature increases and decreases.

[0039] However, in conventional manufacturing equipment, the main parts of the molding equipment are often made of materials such as heat-resistant bricks, and there is a risk of the main body being damaged by thermal shock when the temperature is increased or decreased rapidly. Therefore, in conventional manufacturing equipment, there is a problem that the temperature increase and decrease rates cannot be increased very much. Here, damage caused by thermal shock includes either brittle fracture, which is caused by a temperature distribution caused in a material by a sudden temperature change, or ductile deformation, which is caused by a large temperature distribution caused in a material by a sudden temperature change, or both.

[0040] In order to deal with this problem, it is conceivable to use a material that is resistant to thermal shock as the material for the body of the molding device, but in general, materials with good thermal shock resistance are highly reactive with glass, making it difficult to use them for the body of the molding device.

[0041] In contrast, in first manufacturing equipment 100, as described above, the main portion of forming device 110 has main body 120 and plate member 130 having a thickness in the range of 0.5 mm to 100 mm. Moreover, plate member 130 is made of a material inactive to molten glass MG, and is placed in a location of main body 120 where it comes into contact with molten glass MG.

[0042] In the first manufacturing equipment 100 having such characteristics, the possibility that the main body 120 of the forming device 110 comes into contact with the molten glass MG during the manufacturing of the glass plate is significantly reduced because the main body 120 is protected by the plate member 130. Therefore, a material having thermal shock resistance can be selected for the main body 120.

[0043] Furthermore, the plate member 130 of the molding device 110 has a thickness in the range of 0.5 mm to 100 mm, and is characterized in that it is difficult to crack even when subjected to thermal shock.

[0044] Due to the above-mentioned effects, in the first manufacturing facility 100, the temperature of the forming device 110 can be increased and decreased quickly. This also makes it possible for the first manufacturing facility 100 to manufacture glass sheets more efficiently.

[0045] However, simply placing the plate member 130 on the main body 120 may cause problems in the receiving section 170 of the molding device 110 due to the difference in thermal expansion coefficient between the main body 120 and the plate member 130 .

[0046] Such a problem will be described below with reference to FIG.

[0047] Fig. 3 is a schematic cross-sectional view obtained when the accommodation unit 170 of the molding apparatus 110 is cut along the XY plane. In Fig. 3, some members such as the supply pipe 105 are omitted for clarity of the drawing.

[0048] As shown in FIG. 3, the accommodation section 170 of the molding device 110 is constituted by a plate member 130 disposed so as to cover the recess 122 of the main body 120 .

[0049] More specifically, the body 120 has first and second inner sidewalls 142a, 142b opposed to one another, and third and fourth inner sidewalls 142c, 142d opposed to one another.

[0050] 3, the first inner sidewall 142a and the second inner wall surface 142b extend in the YZ direction. Meanwhile, the third inner sidewall 142c and the fourth inner sidewall 142d extend in the XZ direction. The third inner sidewall 142c faces the first upper side surface 126a of the main body 120. The fourth inner sidewall 142d faces the second upper side surface 126b of the main body 120.

[0051] A first plate member 130A is installed on the first inner sidewall 142a, a second plate member 130B is installed on the second inner sidewall 142b, a third plate member 130C is installed on the third inner sidewall 142c, and a fourth plate member 130D is installed on the fourth inner sidewall 142d.

[0052] Further, a fifth plate member 130E is provided on the first upper side surface 126a of the main body 120, and a sixth plate member 130F is provided on the second upper side surface 126b of the main body 120.

[0053] In such a configuration of the housing section 170, a first case is assumed in which the thermal expansion coefficient of the plate member 130 is greater than the thermal expansion coefficient of the main body 120 at the operating temperature of the molding device 110 (for example, 1100° C.).

[0054] In this case, at the operating temperature of the molding device 110, the expansion of the first plate member 130A to the fourth plate member 130D is greater than the expansion of the first inner side wall 142a to the fourth inner side wall 142d of the main body 120. Therefore, the first inner side wall 142a to the fourth inner side wall 142d are subjected to stress by the expanded first plate member 130A to the fourth plate member 130D. This creates a risk that the main body 120 will be damaged.

[0055] In addition, the third plate member 130C and the fourth plate member 130D have larger dimensions than the first plate member 130A and the second plate member 130B, and therefore the expansion is more significant. As a result, the storage section 170 receives a larger force in the direction along the longitudinal direction (X direction) than in the direction perpendicular to the longitudinal direction (Y direction).

[0056] In order to suppress such a risk, it is necessary to predict the expansion difference between each part (first inner side wall 142a to fourth inner side wall 142d) of main body 120 and plate member 130 before operation (at room temperature) and adjust the dimensions of plate members 130A to 130D. However, there is a certain range for the operating temperature of molding device 110, and such adjustment is not easy.

[0057] Next, as a second case, a case will be considered in which the thermal expansion coefficient of the main body 120 is greater than the thermal expansion coefficient of the plate member 130 at the operating temperature of the molding device 110.

[0058] In this case, at the operating temperature of the molding device 110, the first inner side wall 142a to the fourth inner side wall 142d of the main body 120 expand more than the first plate member 130A to the fourth plate member 130D. As a result, a gap is generated between the main body 120 and the plate member 130, which increases the possibility that the plate member 130 may become misaligned or lose support and collapse.

[0059] Thus, simply installing the plate member 130 on the main body 120 may cause problems in the accommodation section 170 of the molding device 110.

[0060] In this regard, one embodiment of the present invention is a forming apparatus for forming a glass ribbon by forming molten glass contained in a container, comprising: The main body, a plurality of plate members disposed on a portion of the body that contacts the molten glass; having Each plate member has a thickness in the range of 0.5 mm to 100 mm and is made of a material that is inactive to the molten glass. The housing portion has an inner sidewall of the main body, and at least one of the plate members covers at least a portion of the inner sidewall, There is provided a molding apparatus, in which a buffer material is disposed at least partially between the inner side wall and the plate member covering the inner side wall.

[0061] In the molding device according to one embodiment of the present invention, a buffer material is disposed between the inner side wall of the main body and the plate member covering the inner side wall.

[0062] For example, in the example shown in FIG. 3, the cushioning material is disposed in at least one of the following locations: between the first inner side wall 142a of the main body 120 and the first plate member 130A, between the second inner side wall 142b and the second plate member 130B, between the third inner side wall 142c and the third plate member 130C, and between the fourth inner side wall 142d and the fourth plate member 130D.

[0063] The buffer material is selected from those that have a certain degree of elasticity at the operating temperature of the molding device 110 (for example, 1100° C.).

[0064] By providing such a buffer material, the above-mentioned problems that may arise due to the difference in thermal expansion behavior between the plate member 130 and the main body 120 can be significantly eliminated or reduced.

[0065] (Specific configuration example of a molding device according to one embodiment of the present invention) Next, a specific configuration example of a molding device according to an embodiment of the present invention will be described with reference to FIG.

[0066] FIG. 4 shows a schematic cross-sectional view of a molding apparatus according to one embodiment of the present invention (hereinafter referred to as a "first molding apparatus").

[0067] As shown in Fig. 4, the first molding apparatus 210 has a main body 220. The structure of the main body 220 is similar to that of the main body 120 of the molding apparatus 110 shown in Figs. 1 and 2 above, and details thereof will be omitted here.

[0068] Moreover, first shaping apparatus 210 further includes plate member 230 arranged at a portion of main body 220 that comes into contact with molten glass MG. Plate member 230 is configured by combining a plurality of plate members. For example, in the example shown in Fig. 4, plate member 230 includes first plate member 230A to sixth plate member 230F. Note that plate members 230A to 230F correspond to plate members 130A to 130F in shaping apparatus 110 described above, respectively.

[0069] The first molding device 210 further includes a cushioning material 240. The cushioning material 240 includes a first cushioning material 240A to a fourth cushioning material 240D.

[0070] The first cushioning material 240A is disposed between the first inner sidewall 242a of the main body 220 and the first plate member 230A in a top view. The second cushioning material 240B is disposed between the second inner sidewall 242b of the main body 220 and the second plate member 230B in a top view. Similarly, the third cushioning material 240C is disposed between the third inner sidewall 242c of the main body 220 and the third plate member 230C in a top view, and the fourth cushioning material 240D is disposed between the fourth inner sidewall 242d of the main body 220 and the fourth plate member 230D in a top view.

[0071] When such a buffer material 240 is provided, even if one expands relative to the other due to a difference in thermal expansion coefficient between the plate member 230 and the main body 220, the effect of this can be mitigated or suppressed.

[0072] For example, consider the above-mentioned first case (wherein the thermal expansion coefficient of the plate member 230 is greater than that of the main body 220 in the operating temperature range). In this case, while the molding apparatus 210 is in operation, the first plate member 230A to the fourth plate member 230D expand more than the corresponding inner side walls 242a to 242d of the main body 220, respectively. In particular, since the third plate member 230C and the fourth plate member 230D have large dimensions, their expansion along the longitudinal direction (X direction) of the first molding apparatus 210 becomes more significant.

[0073] However, in the first molding device 210, even if stress is generated along the X direction toward the first inner side wall 242a of the main body 220 due to the expansion of the third plate member 230C and the fourth plate member 230D, such stress is absorbed by the first cushioning material 240A.

[0074] Similarly, even if a stress occurs along the X direction toward the second inner side wall 242b of the main body 220, such a stress is absorbed by the second cushioning material 240B.

[0075] Furthermore, even if, for example, expansion of the first plate member 230A and the second plate member 230B generates stress along the Y direction toward the third inner side wall 242c and the fourth inner side wall 242d of the main body 220, these stresses are absorbed by the third cushioning material 240C and the fourth cushioning material 240D, respectively.

[0076] Next, consider the second case described above (where the thermal expansion coefficient of the main body 220 is greater than that of the plate member 230 in the operating temperature range). In this case, the first inner side wall 242a to the fourth inner side wall 242d of the main body 220 expand more than the first plate member 230A to the fourth plate member 230D during operation of the first molding device 210.

[0077] However, even if such expansion occurs, gaps are unlikely to occur between the first to fourth inner side walls 242a to 242d of the main body 220 and the first to fourth plate members 230A to 230D because the first to fourth cushioning materials 240A to 240D are present between them.

[0078] In particular, if each of the cushioning materials 240 is placed between the main body 220 and the plate member 230 in a pre-compressed state, the occurrence of a gap between them can be more reliably prevented.

[0079] As a result, in the second case, it is possible to significantly prevent the plate member 230 from shifting position during operation, or the plate member 230 from losing support and collapsing.

[0080] In this way, in either case, the first molding apparatus 210 can significantly avoid or reduce problems that may occur in the storage section 270 as described above.

[0081] In the first molding device 210, the cushioning material 240 is disposed at four locations in the storage section 270, that is, on the first inner side wall 242a to the fourth inner side wall 242d of the main body 220.

[0082] However, this is merely an example, and it is sufficient that the cushioning material 240 is disposed on at least one of the first inner side wall 242a to the fourth inner side wall 242d of the main body 220.

[0083] For example, the first molding device 210 may have only the first cushioning material 240A and / or the second cushioning material 240B.

[0084] In the first case described above, the expansion of the plate member 230 is more noticeable in the third plate member 230C and the fourth plate member 230D, which have larger dimensions. Therefore, by providing the first buffer material 240A and / or the second buffer material 240B, the influence of the expansion can be more effectively suppressed.

[0085] Furthermore, the first cushioning material 240A may be omitted.

[0086] In the first forming device 210 shown in Fig. 4, the supply pipe 205 is located near the first plate member 230A, but if the first buffer material 240A is omitted, the supply pipe 205, the first plate member 230A, and the main body 220 can be arranged without any gaps. Therefore, when the temperature changes from room temperature to the operating temperature range, the amount of displacement of each member relative to each other can be suppressed to a small amount. This also makes it possible to significantly suppress the molten glass MG from leaking out from the gaps in the first plate member 230A.

[0087] On the other hand, the second cushioning material 240B is present between the second plate member 230B facing the first plate member 230A and the second inner side wall 242b. Therefore, the second cushioning material 240B can effectively suppress the influence of dimensional changes due to thermal expansion of the third plate member 230C and the fourth plate member 230D, which have larger dimensions.

[0088] (Each component of the molding device) Next, each of the members constituting the molding apparatus according to one embodiment of the present invention will be described in more detail.

[0089] Here, as an example, the components of the first molding device 210 shown in Fig. 4 will be described. Therefore, the reference numerals used in Fig. 4 will be used to represent the respective components.

[0090] (Main body 220) The body 220 is constructed from a material that is resistant to thermal shock.

[0091] Specifically, the body 220 has a thermal conductivity of κ (W / mK) at room temperature and a thermal expansion coefficient of ρ (10 -6 / K), the ratio κ / ρ is 1 or greater.

[0092] Such materials have the characteristic that they are unlikely to be damaged even when they are rapidly heated from room temperature to the glass forming temperature (for example, 500° C. to 1500° C.) or rapidly cooled from the glass forming temperature to room temperature.

[0093] Examples of materials having a ratio κ / ρ of 1 or more include carbon (C) with a ratio κ / ρ of 23.5, silicon carbide (SiC) with a ratio κ / ρ of 60.0, silica sintered body with a ratio κ / ρ of 2.7, nickel (Ni) with a ratio κ / ρ of 7.3, molybdenum (Mo) with a ratio κ / ρ of 28.8, stainless steel with a ratio κ / ρ of 1.2, alumina sintered body with a ratio κ / ρ of 4.4, and mullite sintered body with a ratio κ / ρ of 1.2. The silica sintered body may contain 0.2 to 5% by weight of a component other than normal silica based on the total amount of the sintered body. The alumina sintered body may contain 0.2 to 10% by weight of a component other than normal alumina based on the total amount of the sintered body. The mullite sintered body may contain 0.5 to 5% by weight of a component other than normal mullite based on the total amount of the sintered body.

[0094] (Plate member 230) The plate member 230, that is, each of the plate members 230A to 230G, is made of a material that is inactive against the glass used. For example, the material for the plate member 230 includes metal oxides such as silicon oxide, zirconium oxide, aluminum oxide, and magnesium oxide. The plate member 230 may be made of only one type of metal oxide, or may be made of two or more types of metal oxides. The plate member 230 may also contain a composite oxide of two or more metals that constitute these metal oxides. The plate member 230 may also contain a metal such as molybdenum. Specifically, the plate member 230 may be made of one or more materials selected from the group consisting of quartz, zirconia, mullite, zircon, magnesia, alumina, and molybdenum. The impurities contained in the material that constitutes the plate member 230 are preferably 1% by weight or less of the total amount of the material.

[0095] The material that is inactive to the glass varies depending on the composition of the glass used. Therefore, as the material constituting the plate member 230, a material that is low in reactivity with the glass used, i.e., an inactive material, is appropriately selected.

[0096] As described above, the thickness of the plate member 230 is in the range of 0.5 mm to 100 mm. The thickness is preferably in the range of 0.75 mm to 50 mm, and more preferably in the range of 1 mm to 30 mm.

[0097] (Buffer material 240) The configuration of the cushioning material 240 is not particularly limited as long as it can provide the effects described above.

[0098] The buffer material 240 may include, for example, a heat-resistant felt. Such a felt may include, for example, at least one selected from the group consisting of carbon felt, alumina felt, silica felt, and zirconia felt.

[0099] Alternatively, the cushioning material 240 may comprise steel wool or the like.

[0100] As described above, the cushioning material 240 does not need to be provided on all of the inner side walls 242a to 242d of the main body 220, but may be provided in at least one location of the inner side walls 242a to 242d.

[0101] (Another glass sheet manufacturing facility having a forming device according to one embodiment of the present invention) Next, with reference to Figs. 5 and 6, a brief description will be given of another glass sheet manufacturing facility having a forming apparatus according to an embodiment of the present invention.

[0102] 5 and 6 show a schematic configuration example of another glass sheet manufacturing facility (hereinafter referred to as a "second manufacturing facility") 300 having a forming apparatus according to an embodiment of the present invention.

[0103] Fig. 5 shows a schematic perspective view of a part of the second manufacturing facility 300. Fig. 6 shows a schematic cross section of the second manufacturing facility 300 shown in Fig. 5 taken along line BB.

[0104] In the second production facility 300, glass sheets can be continuously produced by the slit downdraw method.

[0105] The second manufacturing facility 300 includes a molding device 310, a furnace 350 (not shown in FIG. 5 for clarity) that houses the molding device 310, and a plurality of rollers 360 disposed below the molding device 310. Although not shown in the figure, the second manufacturing facility 300 further includes a cutting member below the furnace 350.

[0106] The forming device 310 has a function of forming a glass ribbon GR from the molten glass MG. The forming device 310 is connected to a supply pipe (not shown), and the molten glass MG is supplied to the forming device 310 through the supply pipe.

[0107] The molding device 310 has a body 320 .

[0108] The molding device 310 has an elongated shape along the longitudinal direction (X direction). In particular, the body 320 of the molding device 310 has a "box-like" cross-sectional shape as shown in FIGS.

[0109] More specifically, the main body 320 has inner side walls (first inner side wall 321a to fourth inner side wall 321d), an inner bottom surface 325, an outer bottom surface 327, and a slit 329. The first inner side wall 321a and the second inner side wall 321b face each other, and the third inner side wall 321c and the second inner side wall 321d face each other. The first inner side wall 321a and the second inner side wall 321b extend perpendicularly to the longitudinal direction (X direction), and the third inner side wall 321c and the fourth inner side wall 321d extend parallel to the longitudinal direction (X direction). The slit 329 penetrates from the inner bottom surface 325 to the outer bottom surface 327.

[0110] Each roller 360 has a role of transporting the glass ribbon GR discharged from the forming device 310 downward while adjusting the thickness of the glass ribbon GR.

[0111] When a glass sheet is manufactured using such second manufacturing equipment 300, first, molten glass MG is supplied to a forming device 310 via a supply pipe (not shown).

[0112] The molten glass MG supplied to the forming apparatus 310 is first accommodated in the accommodation portion 370 .

[0113] Next, the molten glass MG flows downward through the slits 329 in the main body, and is cooled along the way, thereby forming a glass ribbon GR.

[0114] Thereafter, the glass ribbon GR is further pulled vertically downward by the rollers 360, and is gradually cooled in the process.

[0115] Thereafter, the glass ribbon GR that has been sufficiently cooled slowly is discharged from the furnace 350 and cut to a predetermined size by a cutting means (not shown).

[0116] In the second production facility 300, glass sheets can be continuously produced by the above steps.

[0117] Here, in the second manufacturing facility 300, as the molding device 310, a molding device according to an embodiment of the present invention is used.

[0118] That is, forming apparatus 310 has main body 320 and a plurality of plate members 330. Each plate member 330 has a thickness in the range of 0.5 mm to 100 mm. Moreover, each plate member 330 is made of a material that is inactive to molten glass MG, and is placed on main body 320 at a location where it will come into contact with the glass.

[0119] For example, in the example shown in FIGS. 5 and 6, plate member 330 is installed so as to cover the inner side walls (first inner side wall 321a to fourth inner side wall 321d) of main body 320, inner bottom surface 325, and slit 329.

[0120] The molding device 310 has a shape that is generally conformal to the shape of the main body 320. For example, the molding device 310 has an inner side surface 311, an inner bottom surface 315, and a slit 319, all of which have similar shapes to the corresponding portions of the main body 320. In addition, all of these portions are formed by the exposed surface of the plate member 330.

[0121] The molding apparatus 310 also includes one or more cushioning materials 340 .

[0122] For example, in the example shown in Figures 5 and 6, molding device 310 has first cushioning material 340A and third cushioning material 340C.

[0123] The first cushioning material 340A is disposed between the first inner sidewall 321a of the main body 320 and the plate member 330 disposed opposite the first inner sidewall 321a. The third cushioning material 340C is disposed between the fourth inner sidewall 321d of the main body 320 and the plate member 330 disposed opposite the fourth inner sidewall 321d.

[0124] However, this is merely an example. The number of inner side walls on which the cushioning material 340 is provided in the main body 320 may be one or four. The cushioning material 340 may be provided on any of the inner side walls among the first inner side wall 321a to the fourth inner side wall 321d.

[0125] In the second manufacturing equipment 300 having such characteristics, the possibility that the body 320 of the forming device 310 comes into contact with the glass during the manufacturing of the glass plate is significantly reduced because the body 320 is protected by the plate member 330. Therefore, a material having thermal shock resistance can be selected for the body 320.

[0126] Moreover, unlike a film such as a coating film, the plate member 330 of the molding device 310 is applied as a "plate" onto the main body 320. The plate member 330 has a thickness in the range of 0.5 mm to 100 mm. Therefore, the plate member 330 has a feature that it is difficult to crack even when subjected to thermal shock.

[0127] Furthermore, in the second manufacturing equipment 300, due to the effect of installing the buffer material 340, even if there is a difference between the thermal expansion coefficient of the main body 320 and the thermal expansion coefficient of the plate member 330, the problems described above that may arise in the accommodating section 370 can be significantly alleviated.

[0128] The configuration and features of a molding apparatus according to an embodiment of the present invention have been described above with reference to molding apparatuses 110, 210, and 310.

[0129] However, these are merely examples, and it will be apparent to one skilled in the art having reference to this application that the molding apparatus according to an embodiment of the present invention may have other configurations.

[0130] For example, the forming apparatus according to one embodiment of the present invention may be applied to a manufacturing apparatus for manufacturing glass sheets by a method other than the fusion method and the slit downdraw method.

[0131] In the above description, in order to easily explain the effect of the cushioning material, the characteristics of the configuration of the present invention have been described on the assumption that there is a significant difference in thermal expansion coefficient between the main body and the plate member. However, it is clear that the cushioning material can be used in the molding device according to one embodiment of the present invention even when there is only a slight difference or almost no difference in thermal expansion coefficient between the main body and the plate member. [Explanation of symbols]

[0132] 100 First manufacturing facility 105 Supply pipe 110 Molding equipment 111 Top surface of molding device 112 Recess of molding device 114a: First side of molding device 114b second side of molding device 116a: first upper surface of the molding device 116b second upper surface of the molding device 118a: first lower surface of molding device 118b second lower surface of the molding device 119 Lower end of molding device 120 Body 121 Top of the main body 122 Body recess 124a First side of the body 124b Second side of the body 126a: first upper surface of the body 126b second upper surface of the body 128a: first lower surface of the body 128b second lower surface of the body 129 Lower end of the body 130 Plate members 130A to 130F First to sixth plate members 142a to 142d first to fourth inner side walls 150 furnace 160 Lola 170 Storage unit 190a first molten glass portion 190b second molten glass portion 205 Supply pipe 210 First molding device 220 Main Unit 230 Plate members 230A to 230F First to sixth plate members 240 Cushioning material 240A~240D 1st~4th cushioning materials 242a to 242d: first inner side wall to fourth inner side wall 270 Storage unit 300 Second manufacturing facility 310 Molding equipment 311 Inside side of molding device 315 Inner bottom surface of molding device 319 Slit of molding device 320 Main Unit 321a to 321d: first inner side wall to fourth inner side wall 325 Bottom of the inside of the main body 327 External bottom surface of the main body 329 Body slit 330 Plate members 340 Cushioning material 340A First Buffer 340C Third Cushioning Material 350 furnace 360 Lola 370 Storage unit GR Glass Ribbon MG Molten Glass

Claims

1. A forming device for forming a glass ribbon by forming molten glass contained in a container, comprising: The main body, a plurality of plate members disposed on a portion of the body that contacts the molten glass; having Each plate member has a thickness in the range of 0.5 mm to 100 mm and is made of a material that is inactive with respect to the molten glass; The housing portion has an inner sidewall of the main body, and at least one of the plate members covers at least a portion of the inner sidewall, A molding apparatus, wherein a cushioning material is disposed at least partially between the inner side wall and the plate member covering the inner side wall.

2. The molding apparatus of claim 1 , wherein the cushioning material comprises heat resistant felt.

3. 3. The molding apparatus of claim 2, wherein the felt comprises at least one selected from the group consisting of carbon felt, alumina felt, silica felt, and zirconia felt.

4. The main body has, in the storage portion, a first inner side wall and a second inner side wall opposed to each other in a top view, the first inner side wall and the second inner side wall extending in a direction perpendicular to a longitudinal direction of the main body, The molding apparatus of claim 3, wherein the cushioning material is installed between the first inner sidewall and the plate member covering the first inner sidewall, and / or between the second inner sidewall and the plate member covering the second inner sidewall.

5. The forming apparatus has a supply pipe for molten glass connected to the main body, the first inner sidewall is closer to the supply pipe than the second inner sidewall; The molding apparatus according to claim 4 , wherein the buffer material is disposed between the second inner side wall and the plate member covering the second inner side wall.

6. The body has a thermal conductivity of κ (W / mK) at room temperature and a thermal expansion coefficient of ρ (10 -6 6. The molding apparatus according to claim 1, wherein the molding apparatus is made of a material having a ratio κ / ρ of 1 or more when κ=ρ / ρ.

7. 7. The molding apparatus according to claim 1, wherein the body is made of one or more materials selected from the group consisting of carbon (C), silicon carbide (SiC), sintered silica, nickel (Ni), molybdenum (Mo), and stainless steel.

8. 8. The molding apparatus according to claim 1, wherein the plate member is made of one or more materials selected from the group consisting of quartz, zirconia, mullite, zircon, and magnesia.

Citation Information

Patent Citations

  • To improve the thermal shock resistance of the zircon refractory

    JP1992502900A

  • Molding for producing glass plate

    JP1993139766A

  • Apparatus for forming plate glass

    JP2000335924A

  • Fire-resistant and creep-resistant multilayer used in glass manufacturing systems

    JP2011505319A

  • Apparatus for manufacturing glass plate, and method for manufacturing glass plate using the same

    JP2012031053A