Method and apparatus for reducing defects in a preclean chamber

A flexible metal foil liner attached to a frame at specific points in a pre-clean chamber addresses redeposition issues, enhancing wafer processing capacity and reducing contamination, thus extending maintenance intervals and improving kit life.

JP7576100B2Active Publication Date: 2024-10-30APPLIED MATERIALS INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2022564668
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-04-24
Filing Date
2021-04-20
Publication Date
2024-10-30
Estimated Expiration
2041-04-20

AI Technical Summary

Technical Problem

Pre-clean chambers in wafer level packaging face frequent maintenance due to redeposition of contaminants and etched materials on chamber surfaces, limiting the number of wafers that can be processed before cleaning is required.

Method used

A reusable process kit with a flexible metal foil liner attached to a frame at specific points, allowing stress relief and preventing redeposited material from contaminating the chamber, thereby extending the interval between cleanings.

Benefits of technology

The reusable process kit significantly increases the number of wafers that can be processed before maintenance is needed, reduces particle contamination, and maintains chamber uniformity, with improved kit life and reduced downtime.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007576100000001
    Figure 0007576100000001
  • Figure 0007576100000002
    Figure 0007576100000002
  • Figure 0007576100000003
    Figure 0007576100000003
Patent Text Reader

Abstract

The apparatus and method use a unique process kit to protect a processing volume of a process chamber. The process kit includes a shield having a frame configured to be insertable into the shield and a foil liner made of a metallic material that is attachable to the frame at specific points. The specific attachment points are spaced to provide an amount of flexibility based on the malleability of the metallic material. The amount of flexibility ranges from about 2.5 to about 4.5.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] SUMMARY OF THE PREFERRED EMBODIMENTS Embodiments of the present principles relate generally to wafer level packaging of semiconductor structures. [Background technology]

[0002] The process chamber can be configured to perform a pre-cleaning process. For example, such a pre-cleaning chamber can remove native oxides on metal contact pads of a substrate prior to physical vapor deposition (PVD) to deposit one or more barrier layers, e.g., titanium (Ti), copper (Cu), etc., on the substrate, and prior to removing other materials. Pre-cleaning chambers typically use ion bombardment (induced by RF plasma) to remove native oxides on metal contact pads and other materials by etching. The pre-cleaning process reduces the contact resistance between metal contacts on the substrate to improve the performance and power consumption of integrated circuits on the substrate and promote adhesion. To perform a plasma cleaning process, an integrated circuit is placed in a plasma chamber and a pump removes most of the air from the chamber. Electromagnetic energy (e.g., radio frequency) is applied to an inlet gas, such as argon, to excite the inlet gas into a plasma state. The plasma releases ions, which bombard the surface of the substrate to remove contaminants and / or materials from the substrate. Atoms or molecules of the contaminants and / or substrate material are etched from the substrate and are largely pumped out of the chamber. However, some of the contaminants and / or etched materials may be redeposited on the chamber surfaces. Typically, a process kit is used to reduce or prevent the deposition of contaminants and / or etched materials on the chamber surfaces. Re-sputtering of deposited materials onto the process kit is a major factor in determining when routine maintenance should be performed on a preclean chamber. Due to deposit buildup, a preclean chamber may be limited to 2000 wafers or less before routine maintenance is required.

[0003] Therefore, the inventors have provided embodiments that increase the number of wafers between required cleanings of the preclean chamber. Summary of the Invention

[0004] SUMMARY OF THE DISCLOSURE Methods and apparatus are provided herein for improving wafer run numbers between cleaning intervals.

[0005] In some embodiments, an apparatus for protecting a processing volume of a process chamber can include a frame configured to be insertable into a process kit shield and a foil liner made of a metallic material attachable to the frame at specific points, the specific points spaced to provide an amount of flexibility based on the malleability of the metallic material, the amount of flexibility being about 2.5 to about 4.5 GPa.

[0006] The apparatus may further include, where the amount of flexibility is further based on the internal stress of the material to be deposited on the foil liner, the frame is formed from aluminum, copper, titanium, or stainless steel, the foil liner is fabricated from aluminum, copper, titanium, nickel, or gold, the foil liner is aluminum and the specific points are spaced approximately 30 mm apart, the foil liner is rectangular or circular in shape, the frame is attachable to the process kit shield with threaded fasteners, a diffuser having the foil liner attached to its bottom portion, the diffuser having a removable cap at its bottom portion and the foil liner attached to the removable cap, the frame is approximately 3 mm thick, and / or the foil liner is attachable to the frame using a fiber laser with pulsing capabilities.

[0007] In some embodiments, an apparatus for processing a semiconductor structure can include a chamber body having a processing volume, a process kit enclosing at least a portion of the processing volume, a frame inserted into the process kit, and a foil liner made of a metallic material attached to the frame at specific points, the specific points spaced to provide an amount of flexibility based on the malleability of the metallic material, the amount of flexibility being between about 2.5 and about 4.5.

[0008] The apparatus may further include, wherein the amount of flexibility is further based on the internal stress level of the material to be deposited on the foil liner, the frame is formed from aluminum, copper, titanium, or stainless steel, the foil liner is fabricated from aluminum, copper, titanium, nickel, or gold, the foil liner is aluminum and the specific points are spaced approximately 30 mm apart, and / or the frame is attachable to a process kit with threaded fasteners.

[0009] In some embodiments, a method of protecting a process kit can include forming a frame that is attachable to at least a portion of the process kit in a pre-clean chamber, attaching the frame to an inner surface of the process kit, and attaching a foil liner to the inner surface of the frame at specific points spaced apart to achieve an amount of flexibility based on the malleability of the material forming the foil liner, where the amount of flexibility per GPa ranges from about 2.5 to about 4.5.

[0010] The method may further include, wherein the amount of flexibility is further based on an internal stress level of the material to be deposited on the foil liner, and / or the material to be deposited on the foil liner is silicon nitride, silicon oxide, or a polymer.

[0011] Other and further embodiments are disclosed below.

[0012] Embodiments of the present principles, briefly summarized above and discussed in more detail below, can be understood by reference to exemplary embodiments of the present principles as illustrated in the accompanying drawings, which, however, depict only typical embodiments of the present principles and therefore should not be considered limiting in scope, as the present principles may admit of other equally effective embodiments. [Brief description of the drawings]

[0013] [Figure 1] 1 is a cross-sectional view of a process chamber in accordance with some embodiments of the present principles. [Diagram 2] 1 is a cross-sectional view of a top shield with a reusable process kit according to some embodiments of the present principles. [Diagram 3] 1 is a cut away view of a cross section of a top shield and an isometric view of a frame according to some embodiments of the present principles; [Figure 4] FIG. 13 is a cross-sectional isometric view of a frame mounted to an upper shield according to some embodiments of the present principles. [Diagram 5] 1 is a cross-sectional view of a rectangular foil liner in accordance with some embodiments of the present principles; [Figure 6] 1 is a cross-sectional view of a circular foil liner in accordance with some embodiments of the present principles; [Figure 7] FIG. 1 is an isometric view of a portion of a foil liner material according to some embodiments of the present principles. [Figure 8] FIG. 1 is a side view of a diffuser according to some embodiments of the present principles. [Figure 9] 1 illustrates a method of attaching a frame and foil liner to a process kit in accordance with some embodiments of the present principles. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] For ease of understanding, wherever possible, the same reference numbers have been used to designate identical elements common to the figures. The figures are not drawn to scale and may be simplified for clarity. Elements and features of one embodiment may be beneficially incorporated in other embodiments without further recitation.

[0015] The method and apparatus utilize a reusable process kit that dramatically increases the number of wafers that can be run before routine maintenance or cleaning is required. The reusable process kit can be used in a pre-clean chamber, but the principles can also be applied to other chambers. The reusable process kit includes a reusable frame that is used to support a metal foil liner, which is attached to the frame in a manner that allows the foil liner to maintain a certain flexibility that prevents deposition particle contamination in the chamber. The flexibility of the foil liner allows re-sputter deposits that occur during cleaning to adhere to the foil liner and remain attached even in the case of high stress deposition. The flexibility of the foil liner improves the high stress in the deposits, thereby allowing the deposits to remain attached to the foil liner instead of flaking off and contaminating the chamber. The enhanced bond between the deposits and the foil liner allows the reusable process kit to be utilized for an extremely large number of wafers, sometimes two to three times more than the number of wafers in a chamber using a conventional process kit, before the reusable process kit needs to be replaced. Additionally, the chamber non-uniformity percentage (NU%) is maintained throughout the extended process kit life.

[0016] Pre-clean chambers that process materials such as silicon nitride, silicon oxide, polymers, and metals suffer from short process kit life. The reusable process kit of the present principles improves kit life by more than 2 times and provides a re-use job turnaround time of less than 3 hours, as opposed to about 3 days or more for conventional process kits. The design of metal foil liners and frames with various patterns and pitches allows for faster replacement or refurbishment of process kits than conventional arc spray processes or other types of coatings. Moreover, the reusable process kits help improve the performance of pre-clean chambers. The benefits of using reusable process kits include an improvement in mean wafer before cleaning (MWBC) by more than 2 times, reduced particle counts, and extended kit life with less than 2% NU% drift. The reusable process kits further provide lower process kit re-use costs, faster process kit re-use job turnaround times, and better throughput.

[0017] FIG. 1 illustrates a cross-sectional view of a process chamber (e.g., a plasma processing chamber) having a process kit according to some embodiments. In some embodiments, the plasma processing chamber is a pre-clean processing chamber. However, other types of process chambers configured for different processes may also use or be modified to use the reusable process kit embodiments described herein. The chamber 100 is a vacuum chamber suitably adapted to maintain a sub-atmospheric pressure within an interior volume 120 during substrate processing. In some embodiments, the chamber 100 can maintain a pressure of about 1 mTorr to about 10 mTorr. The chamber 100 includes a chamber body 106 covered by a lid 104 that encloses a processing volume 119 located in the upper half of the interior volume 120. In some embodiments, the chamber 100 includes an adapter 180 disposed between the chamber body 106 and the lid 104 and resting on a sidewall of the chamber body 106. The chamber 100 includes a process kit that encloses various chamber components to prevent undesired reactions between such components and etched materials and other contaminants. The chamber body 106, adapter 180, and lid 104 may be made of a metal, such as aluminum. The chamber body 106 may be grounded via a bond 115 to ground.

[0018] A substrate support 124 is disposed within the interior volume 120 for supporting and holding a substrate 122, such as, for example, a semiconductor wafer or other such substrate that can be electrostatically held. The substrate support 124 may generally include a pedestal 136 and a hollow support shaft 112 for supporting the pedestal 136. The pedestal 136 includes an electrostatic chuck 150. In some embodiments, the electrostatic chuck 150 includes a dielectric plate. The hollow support shaft 112 includes conduits for supplying, for example, backside gas, process gas, fluids, coolant, power, and the like, to the electrostatic chuck 150. In some embodiments, the substrate support 124 includes an edge ring 187 disposed about the electrostatic chuck 150. In some embodiments, the edge ring 187 is made of alumina (Al2 O 3 A slit valve 184 may be coupled to the chamber body 106 to facilitate transferring the substrate 122 in and out of the interior volume 120.

[0019] The process kit includes an upper shield 117 that surrounds the substrate support 124. The upper shield 117 can be configured to rest on the adapter 180 and define a processing volume 119. In some embodiments, the upper shield 117 is fabricated from a metal, such as aluminum. The process kit can include a lower shield 105 that surrounds the substrate support 124, which can be coupled to a pedestal 136. In some embodiments, the lower shield 105 is fabricated from a metal, such as aluminum. The hollow support shaft 112 is coupled to a lift mechanism 113, such as an actuator or motor, that provides vertical movement of the electrostatic chuck 150 between an upper processing position and a lower transfer position. A bellows assembly 110 is disposed about the hollow support shaft 112 and coupled between the electrostatic chuck 150 and a bottom surface 126 of the chamber 100 to provide a flexible seal that allows vertical movement of the electrostatic chuck 150 while reducing or preventing vacuum loss from within the chamber 100. Bellows assembly 110 further includes a lower bellows flange 164 in contact with an O-ring 165 or other suitable sealing element that contacts bottom surface 126 to help prevent degradation of the chamber vacuum.

[0020] The substrate lift 130 may include lift pins 109 mounted on a platform 108 connected to a shaft 111 coupled to a second lift mechanism 132 for raising and lowering the substrate lift 130 so that the substrate 122 can be placed on or removed from the electrostatic chuck 150. The electrostatic chuck 150 may include through holes to accommodate the lift pins 109. A bellows assembly 131 is coupled between the substrate lift 130 and the bottom surface 126 to provide a flexible seal to maintain a vacuum in the chamber during vertical movement of the substrate lift 130. The hollow support shaft 112 includes conduits for coupling the backside gas supply 141, the chucking power supply 140, and the RF power supply 190 to the electrostatic chuck 150. In some embodiments, the chucking power supply 140 provides DC power to the electrostatic chuck 150 via a conduit 154 to hold the substrate 122. In some embodiments, the RF energy provided by the RF power supply 190 may have a frequency of about 10 MHz or greater. In some embodiments, the RF power source 190 may have a frequency of about 13.56 MHz.

[0021] The backside gas supply 141 is disposed outside the chamber body 106 and supplies gas to the electrostatic chuck 150. The electrostatic chuck 150 may include a gas channel 138 extending from a lower surface of the electrostatic chuck 150 to an upper surface 152 of the electrostatic chuck 150. The gas channel 138 is configured to supply a backside gas, such as nitrogen (N), argon (Ar), or helium (He), to the upper surface 152 of the electrostatic chuck 150 to act as a heat transfer medium. The gas channel 138 is in fluid communication with the backside gas supply 141 via a gas conduit 142 to control the temperature and / or temperature profile of the substrate 122 during use. For example, the backside gas supply 141 may supply gas to cool the substrate 122 during use. The chamber 100 is coupled to and in fluid communication with a vacuum system 114 that includes a throttle valve (not shown) and a pump (not shown) used to evacuate the chamber 100. In some embodiments, the vacuum system 114 is coupled to a pump port disposed on a bottom surface 126 of the chamber body 106. The pressure inside the chamber 100 can be adjusted by adjusting a throttle valve and / or a vacuum pump. In some embodiments, the pump has a flow rate of about 1900 liters per second to about 3000 liters per second.

[0022] The chamber 100 is also coupled to and in fluid communication with a process gas supply 118 that can supply one or more process gases to the chamber 100 for processing a substrate disposed therein. In some embodiments, the lid 104 includes a port through which gas from the process gas supply 118 can be introduced into the interior volume 120. In some embodiments, the process gas supply 118 supplies argon (Ar) gas. In some embodiments, a diffuser 182 is coupled to the top shield 117 to inject gas from the process gas supply 118 into the processing volume 119 from the center of the top shield 117. In operation, for example, a plasma 102 can be created in the interior volume 120 to perform one or more processes. The plasma 102 can be created by coupling power from a plasma power source (e.g., an RF power source 190) to a process gas through the electrostatic chuck 150 to ignite the process gas and create the plasma 102. The RF power source 190 is also configured to attract ions from the plasma toward the substrate 122.

[0023] A controller 170 is provided and may be coupled to various components of the chamber 100 to control its operation. The controller 170 includes a central processing unit (CPU) 172, a memory 174, and support circuits 176. The controller 170 may control the chamber 100 directly or through a computer (or controller) associated with a particular process chamber and / or support system components. The controller 170 may be one of any form of general-purpose computer processor that may be used in an industrial environment to control various chambers and sub-processors. The memory or computer readable medium 174 of the controller 170 may be one or more of readily available memories such as random access memory (RAM), read only memory (ROM), floppy disk, hard disk, optical storage media (e.g., compact disk or digital video disk), flash drive, or any other form of local or remote digital storage. The support circuits 176 are coupled to the CPU 172 to support the processor in a conventional manner. The circuits include cache, power supplies, clock circuits, input / output circuits and subsystems, and the like. Methods for controlling the chamber 100 and / or processes may be stored in memory 174 as software routines that may be executed or called to control operation of the chamber 100 in the manner described herein. The software routines may also be stored and / or executed by a second CPU (not shown) that is located remotely from the hardware controlled by CPU 172.

[0024] FIG. 2 illustrates a cross-sectional view 200 of a top shield 217 with a reusable process kit 202 according to some embodiments. The reusable process kit 202 includes a metal foil liner that is attached in a particular manner to a frame that is secured to the top shield 217. The foil liner can be fabricated from a variety of materials such as gold, aluminum, copper, nickel, and / or titanium. The material of the foil liner can be selected based on the type of material that will be deposited on the foil liner during processing. The material of the foil liner can be selected based on the amount of internal stress present in the deposited material. In some embodiments, the foil liner has a thickness of about 25 μm to about 225 μm. In some embodiments, the foil liner is welded to the frame at specific points at specific intervals using a pulsed laser to allow for a specific amount of flexibility in the foil liner based on the malleability of the metal material used to form the foil liner. In some embodiments, the foil liner is textured to promote adhesion of the deposition to the foil liner. In some embodiments, the surface roughness has a value of about 5 Ra (average roughness in microinches) to about 20 Ra. The reusable process kit 202 can double the time between changes while preventing delamination and reducing particulate contamination by more than 10 times compared to conventional process kits.

[0025] FIG. 3 illustrates a cross-sectional view 300A of an upper shield 302 and an isometric cutaway view 300B of a frame 308, according to some embodiments. The upper shield 302 includes a diffuser 304 (see, for example, diffuser 182 in FIG. 1) and is modified with a series of attachment points 306 for a frame 308. In some embodiments, the attachment points 306 can include, but are not limited to, threaded holes for receiving threaded fasteners or the like. The frame 308 can be formed from aluminum, copper, stainless steel, and / or titanium, or the like. The frame 308 can be formed from any material that is not exposed to plasma and can support a foil liner. In some embodiments, the frame 308 has a thickness 320 of about 2 mm to about 4 mm. In some embodiments, the frame 308 has a thickness of about 3 mm. In some embodiments, the frame 308 includes through holes 310. The through holes 310 may be chamfered on the inner side 312 of the frame 308 to mate with the chamfered head of a threaded fastener. The frame 308 is insertable 314 into the top shield 302, with the outer surface 318 of the frame 308 mating with the inner surface 316 of the top shield 302. Figure 4 shows a cross-sectional view 400 of the frame 308 inserted into the top shield 302 according to some embodiments. In some embodiments, the frame 308 is secured to the top shield 302 using a threaded fastener 402 with a chamfered head that mates with the chamfered through hole of the frame 308 and mates with a thread in a threaded hole in the top shield 302. The threaded fastener 402 is countersunk in the frame 308 so as not to interfere with the attachment of the foil liner.

[0026] FIG. 5 shows a cross-sectional view 500 of a rectangular foil liner 502 according to some embodiments. The pre-clean chamber is similar to a plasma etch chamber, which uses plasma to etch away material from the wafer. During the etch process, material on the wafer will be re-sputtered and redeposited on the shield. Materials such as silicon nitride, silicon oxide, or polymers have very high internal stress, almost twice as much as other materials. High internal stress materials cause stress buildup on the shield of the process kit, which leads to cracking of the redeposited material, which will peel off from the shield and contaminate the environment. The method and apparatus of the present principles alleviates the stress of the redeposited material, thereby reducing particulate contamination.

[0027] The inventors have found that attaching the foil liner to the frame 308 using a uniform adhesive covering the entire surface of the foil liner prevents deformation (and stress relief) of the foil liner and does not provide any improvement in terms of particle contamination and process kit life compared to conventional process kits. The inventors have found that if the foil liner is instead attached at specific points with specific spacing, the foil liner remains flexible and provides dramatically better deposition adhesion and stress relief, substantially reducing particle contamination. The stress build-up of the shield is reduced by the flexibility of the foil liner, which significantly extends the life of the process kit. The flexibility of the foil liner allows for stress relief from deformation and prevents redeposition cracking and spalling. By attaching the foil liner at different attachment points with specific distances or pitches, the flexibility of the foil liner can be adjusted to reduce particle formation. A very high density of pitch reduces the flexibility of the foil liner and increases particle dropout. A lower pitch density, in other words fewer attachment points, allows the foil liner to be more flexible, so fewer particles are formed.

[0028] In addition, the inventors have found that the use of a short pulse laser provides a way to spot weld the foil liner to the frame without damaging the foil liner or the frame. The very short pulse time prevents the laser from melting through the material and potentially damaging the underlying shield or process kit. The short pulse laser was then used to weld the foil liner to the frame at various points at various intervals. In some embodiments, a fiber laser is used to weld the foil liner to the frame. The inventors have found that when using very thin aluminum for the foil liner, a spacing or pitch pattern of about 30 mm or greater results in a significant reduction in particle contamination. When the pitch pattern is significantly less than 30 mm (e.g., about 15 mm) for a given thin aluminum foil liner, the reduction in particle contamination was negligible. The inventors have found that the malleability of the material used for the foil liner also directly impacts the pitch pattern. Materials with higher malleability can be spaced less than 30 mm and still result in a significant reduction in particle contamination. Similarly, materials with lower malleability can be spaced greater than 30 mm to provide a significant reduction in particulate contamination. Additionally, NU% will not exceed 2% over the life of the kit.

[0029] For simplicity, the following examples use foil liners constructed from thin aluminum material. The rectangular foil liner 502 in FIG. 5 shows a pitch pattern of weld points 504 of about 30 mm or more. The distance A 506 between the rows of weld points 504 and the distance B 508 between the columns of weld points 504 are both equal to about 30 mm. In a rectangular or square foil liner, maintaining the distance between each weld point is fairly easy to achieve. FIG. 6 shows a cross-sectional view 600 of a circular foil liner 602 according to some embodiments. In the example of the circular foil liner 602, the weld points 608 are arranged in rays emanating from a center point 610. As can be seen in FIG. 6, it is more difficult to maintain the pitch spacing (radial line spacing 606 and spacing between rays 604) at about 30 mm. The inventors have found that attempting to maintain an average spacing of 30 mm for the weld points of a circular foil liner still results in a significant reduction in particulate contamination.

[0030] 7 shows an isometric view 700 of a portion 702 of a foil liner material according to some embodiments. The attachment point pitch, or in some embodiments, weld pitch, is used to achieve a desired amount of flexibility of the attached foil liner for stress relief of the redeposited material. The desired pitch is related to the thickness 710 of the foil liner and the elastic modulus (malleability) of the material used for the foil liner. Mounting point pitch (mm) ∝ Film thickness (mm) × Elastic modulus (GPa) (Equation 1) The mounting point pitch is L=f·t·E (formula 2) where L is the distance 706, 708 between the attachment points 704, t is the thickness 710 of the foil liner, E is the elastic modulus of the foil liner material, and f is a proportionality constant. The proportionality constant f, which can be considered as the amount of flexibility, varies depending on the stress of the resputtered material deposited on the foil liner. The amount of flexibility is f=L / (t·E) (Equation 3) It can be expressed as:

[0031] For example, if a copper foil liner is used for silicon nitride etching, a mounting point pitch distance of 30 mm is used to achieve good particle performance (reducing particle contamination). In this example, the thickness of the attached copper foil liner may be 70 μm, and the elastic modulus of copper is 117 GPa. Therefore, the amount of flexibility (f) is: f=30mm / (0.07mm×117GPa)=3.66 / GPa (Formula 4) The amount of flexibility (f) per GPa can be varied between about 2.5 and about 4.5 for different resputtered material stresses to achieve significant particle contamination reduction.

[0032] As a further example of attachment point pitch, if the foil liner is formed from aluminum having a thickness of 100 μm, an elastic modulus of 67 Gpa, and an amount of flexibility of f=3.66, the attachment pitch may be: L(mm)=3.66×0.1×67=24.5mm (Formula 5) In another example, if the foil liner is made of pure nickel with a thickness of 50 μm, a modulus of elasticity of 170 Gpa, and a flexibility amount=4.0, the attachment point pitch is: L(mm)=4.0×0.05×170=34.0mm (Formula 6) It can be defined as:

[0033] The attachment point pitch can range from about 10 mm to about 40 mm or more, depending on the properties of the material used in the foil liner and / or the amount of flexibility desired to reduce internal stresses in a particular type of deposition material. The ability to account for numerous parameters allows for a great deal of flexibility in applying the apparatus and methods of the present principles to achieve superior particle control within the process chamber.

[0034] FIG. 8 shows an isometric view 800 of a diffuser 802 according to some embodiments. The diffuser 802 (see diffuser 182 in FIG. 1) is exposed to the process volume 119 at a bottom exterior surface 816. The diffuser 802 has a sidewall gas outlet 804 that is an integral part of the pre-clean chamber process. The inventors have devised a new diffuser structure with a removable cap 808 that can be removably attached to the diffuser 802. In some embodiments, the cap 808 includes internal threads 814 that mate with the external threads 806 of the diffuser 802. In some embodiments, the cap 808 can be friction-fit or press-fit to the diffuser 802 or the like. The bottom exterior surface 816 of the cap 808 has a foil liner 810 attached with weld points 812 at specific intervals. During process kit maintenance, the cap 808 can be easily replaced with minimal downtime. The diffuser 802 is a very small part and the foil liner 810 is mounted in such a way that it does not affect the sidewall gas outlets 804. When the diffuser 802 is installed in the chamber 100, a small circular gap remains around the diffuser 802, allowing gas to enter the processing volume 119. If the gas were blocked, uniformity would be adversely affected. The foil liner 810 is mounted such that the circular gap is unblocked, allowing gas to flow freely into the processing volume 119.

[0035] In some embodiments, when maintenance is required, the process kit can be removed together with the frame and foil liner. The foil liner can then be removed from the frame, and in some circumstances, the frame can be removed from the process kit or shield. Because the process kit or shield is protected by the frame and foil liner, the process kit or shield will require little or no cleaning. In other cases, the frame can remain attached to the shield and a new foil liner can be installed in situ on the frame in the shield. Because the frame can be reused or recycled and the deposits on the foil liner are removed along with the foil liner, the maintenance process can be performed in 3 hours or less, compared to a conventional process that requires more than 3 days. In some embodiments, the frame and foil liner can be inserted together as a single unit into the shield. The attachment points on the frame allow the foil liner to remain undisturbed during installation or removal from the shield. A spare frame and foil liner unit can then be kept as a full reserve for quick replacement at the time of maintenance.

[0036] FIG. 9 is a method 900 of attaching a frame and a foil liner to a process kit according to some embodiments. In block 902, a frame is formed that is attachable to at least a portion of the process kit of the preclean chamber. The frame can be formed from materials such as aluminum, copper, and / or titanium. In block 904, the frame is attached to an inner surface of the process kit. In some embodiments, the frame can be attached to the process kit with threaded fasteners. In block 906, the foil liner is attached to the inner surface of the frame at specific points that are spaced to achieve an amount of flexibility based on the malleability of the material forming the foil liner. Different types of materials will have different malleability levels, which directly impacts the attachment point spacing to achieve a specific flexibility that will result in a significant reduction in particle contamination. The amount of flexibility can be calculated using Equation 3 above. In some embodiments, the amount of flexibility per GPa to achieve a significant reduction in particle contamination ranges from about 2.5 to about 4.5. In some embodiments, the type of material redeposited on the foil liner will be used to adjust the amount of flexibility to achieve superior particle control.

[0037] Embodiments according to the present principles may be realized in hardware, firmware, software, or any combination thereof. Embodiments may also be implemented as instructions stored using one or more computer-readable media, which may be read and executed by one or more processors. A computer-readable medium may include any mechanism for storing or transmitting information in a form readable by a machine (e.g., a computing platform, or a "virtual machine" running on one or more computing platforms). For example, a computer-readable medium may include any suitable form of volatile or non-volatile memory. In some embodiments, a computer-readable medium may include a non-transitory computer-readable medium.

[0038] While the forgoing is directed to embodiments of the present principles, other and further embodiments of the principles may be devised without departing from the basic scope thereof.

Claims

1. 1. An apparatus for protecting a processing volume of a process chamber, comprising: a frame configured to be insertable within the process kit shield; a foil liner made of a metallic material, attachable to the frame at particular points, the particular points spaced to provide an amount of flexibility based on malleability of the metallic material, the amount of flexibility being from about 2.5 to about 4.5 per GPa, the amount of flexibility being determined by f=L / (t·E), where f is the amount of flexibility, L is the spacing of the particular points, t is the thickness of the foil liner, and E is the elastic modulus of the metallic material; 13. An apparatus comprising:

2. The apparatus of claim 1 , wherein the amount of flexibility is further based on an internal stress of a material to be deposited on the foil liner.

3. The apparatus of claim 1 , wherein the frame is formed from aluminum, copper, titanium, or stainless steel.

4. The apparatus of claim 1 , wherein the foil liner is made of aluminum, copper, titanium, nickel, or gold.

5. The apparatus of claim 1 , wherein the foil liner is aluminum and the particular points are spaced approximately 30 mm apart.

6. The apparatus of claim 1 , wherein the foil liner is rectangular or circular in shape.

7. The apparatus of claim 1 , wherein the frame is attachable to the process kit shield with threaded fasteners.

8. A diffuser having the foil liner attached to its bottom portion. The apparatus of claim 1 further comprising:

9. The apparatus of claim 8 , wherein the diffuser has a removable cap at the bottom portion, and the foil liner is attached to the removable cap.

10. The apparatus of claim 1 , wherein the frame is approximately 3 mm thick.

11. The apparatus of claim 1 , wherein the foil liner is attachable to the frame using a fiber laser with pulsing capabilities.

12. 1. An apparatus for processing a semiconductor structure, comprising: a pre-clean chamber having a chamber body with a processing volume; a process kit enclosing at least a portion of the processing volume; A frame that is inserted into the process kit; a foil liner made of a metallic material attached to the frame at particular points, the particular points spaced to provide an amount of flexibility based on malleability of the metallic material, the amount of flexibility being between about 2.5 and about 4.5, the amount of flexibility being determined by f=L / (t·E), where f is the amount of flexibility, L is the spacing between the particular points, t is the thickness of the foil liner, and E is the elastic modulus of the metallic material; 13. An apparatus comprising:

13. The apparatus of claim 12 , wherein the amount of flexibility is further based on an internal stress level of a material to be deposited on the foil liner.

14. The apparatus of claim 12 , wherein the frame is formed from aluminum, copper, titanium, or stainless steel.

15. The apparatus of claim 12 , wherein the foil liner is made of aluminum, copper, titanium, nickel, or gold.

16. 13. The apparatus of claim 12, wherein the foil liner is aluminum and the particular points are spaced approximately 30 mm apart.

17. The apparatus of claim 12 , wherein the frame is attachable to the process kit with threaded fasteners.

18. 1. A method for protecting a process kit, comprising: forming a frame that is attachable to at least a portion of a process kit of a pre-clean chamber; attaching the frame to an inner surface of the process kit; attaching the foil liner to an inner surface of the frame at specific points spaced to achieve an amount of flexibility based on the malleability of the material forming the foil liner, the amount of flexibility being in the range of about 2.5 to about 4.5 GPa, the amount of flexibility being determined by f=L / (t·E), where f is the amount of flexibility, L is the spacing of the specific points, t is the thickness of the foil liner, and E is the modulus of elasticity of the material forming the foil liner; A method comprising:

19. The method of claim 18 , wherein the amount of flexibility is further based on an internal stress level of a material to be deposited on the foil liner.

20. The method of claim 18 , wherein the material to be deposited on the foil liner is silicon nitride, silicon oxide, or a polymer.

Citation Information

Patent Citations

  • Film forming apparatus and shield member

    JP2012229479A

  • Process kit shield and its usage

    JP2012501387A

  • High-conductance process kit

    JP2018502458A

  • Foil Sheet Assemblies For Ion Implantation

    US20190304738A1

  • Processing chamber with heated chamber liner

    US8444926B2