Cutting blade and method for manufacturing the same
Patent Information
- Application Number
- JP2020045682
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-03-16
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2040-03-16
AI Technical Summary
【0016】 本発明の一つの態様の切断用ブレードおよび切断用ブレードの製造方法によれば、ブレード側面の摩耗を抑制して、刃痩せを低減できる。
Smart Images

Figure 0007576919000003 
Figure 0007576919000004 
Figure 0007576919000005
Abstract
Description
[Technical field]
[0001] The present invention relates to cutting blades and methods of making cutting blades. [Background technology]
[0002] 2. Description of the Related Art Conventionally, in the field of electronic material manufacturing, cutting blades are known that are used in a manufacturing method for cutting a material to be cut into individual pieces (see, for example, Patent Document 1). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2000-144477 A Summary of the Invention [Problem to be solved by the invention]
[0004] Conventional cutting blades have room for improvement in terms of suppressing side wear and reducing blade thinning.
[0005] An object of the present invention is to provide a cutting blade that can suppress wear on the blade side surfaces and reduce blade thinning, and a method for manufacturing the cutting blade. [Means for solving the problem]
[0006] One embodiment of the cutting blade of the present invention comprises a disk-shaped bond phase having a central axis, a plurality of abrasive grains dispersed in the bond phase, a cutting edge disposed on an outer periphery of the bond phase, and a coating layer provided on a side surface of the bond phase; The coating layer is Cu or Ni, The plurality of abrasive grains include a plurality of protruding abrasive grains protruding from a side surface of the bond phase, and the protruding abrasive grains are Abrasive grain size is #325abrasive grains are used, the multiple protruding abrasive grains are each exposed on the surface of the coating layer, the difference in the amount that each protruding abrasive grain protrudes from the side surface of the bond phase is 2 μm or less, the protruding abrasive grains have an embedded portion embedded in the bond phase and a protruding portion protruding from the side surface of the bond phase, and the embedded amount of the embedded portion from the side surface is greater than the protruding amount of the protruding portion from the side surface. Another aspect of the present invention is a method for manufacturing the above-mentioned cutting blade, comprising a bond phase preparation process for preparing the bond phase in which the plurality of abrasive grains are dispersed, an abrasive grain protrusion process for protruding the plurality of protruding abrasive grains from the side of the bond phase by performing lapping or etching on the side of the bond phase, a coating layer preparation process for preparing the coating layer on the side of the bond phase so as to be thicker than the protrusion amount, and an abrasive grain exposure process for polishing the surface of the coating layer to expose the plurality of protruding abrasive grains on the surface.
[0007] According to the cutting blade and its manufacturing method of the present invention, each protruding abrasive grain protruding from the side of the bond phase is exposed on the surface of the coating layer. These protruding abrasive grains contact the cut surface of the workpiece, thereby suppressing side wear of the cutting blade and reducing blade thinning. This maintains the processing quality and processing dimensions of the electronic material components cut into individual pieces from the workpiece and extends the tool life. In addition, since the difference between the protruding amounts of each protruding abrasive grain from the side of the bond phase is 2 μm or less, the multiple protruding abrasive grains contact the cut surface of the workpiece evenly, and the above-mentioned functions are stably obtained. In the above cutting blade, the protruding abrasive grain has an embedded portion embedded in the bond phase and a protruding portion protruding from a side surface of the bond phase, and the amount of embedment of the embedded portion from the side surface is greater than the amount of protrusion of the protruding portion from the side surface. In this case, the protruding abrasive grains are stably held in the bond phase, and the above-mentioned effects of the protruding abrasive grains can be stably obtained.
[0008] In the cutting blade, it is preferable that the distance between the surface of the coating layer and the top of the protruding abrasive grains in the axial direction in which the central axis extends is 1 μm or less.
[0009] In this case, the height difference (distance) between the surface of the coating layer and the tops of the protruding abrasive grains is kept small, within the range of 0 to 1 μm, so that chips are less likely to accumulate between the protruding abrasive grains exposed on the surface of the coating layer. Generally, chips adhering to the surface of the coating layer (i.e., the blade side surface) accelerate the progress of blade thinning, so according to the above-mentioned configuration of the present invention, it is possible to suppress the adhesion of chips to the surface of the coating layer, and to reduce blade thinning more stably.
[0010] In the above cutting blade, the bond phase is a metal bond phase or an electroformed bond phase. be It is preferred.
[0011] In this case, since the bond phase is a metallic bonding phase and the coating layer is made of metal, the side wear of the cutting blade is further suppressed.
[0012] In the above cutting blade, it is preferable that the thickness of the coating layer is equal to or smaller than the average grain size of the protruding abrasive grains.
[0013] In this case, the protruding abrasive grains are exposed on the surface of the coating layer while being partly embedded in the bond phase, i.e., while being held in the bond phase, and therefore the above-mentioned effects of the protruding abrasive grains can be stably obtained. Effect of the Invention
[0016] According to the cutting blade and the method of manufacturing the cutting blade of one aspect of the present invention, wear on the side surface of the blade can be suppressed, and blade thinning can be reduced. [Brief description of the drawings]
[0017] [Figure 1] FIG. 1 is a plan view showing a cutting blade according to the present embodiment. [Diagram 2] FIG. 2 is a cross-sectional view showing the cutting blade of the present embodiment. [Diagram 3] FIG. 3 is a cross-sectional view showing the vicinity of the cutting edge of the cutting blade of this embodiment. [Figure 4]FIG. 4 is a flowchart showing a method for manufacturing the cutting blade of this embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] A cutting blade 10 according to an embodiment of the present invention and a method for manufacturing the same will be described below with reference to the drawings. The cutting blade 10 of the present embodiment is used in the field of electronic material manufacturing, for example, in a manufacturing method for cutting a workpiece to separate it into individual pieces. Examples of the electronic material to be cut include resin molded materials such as BGA (Ball Grid Array).
[0019] 1 to 3, the cutting blade 10 includes a disk-shaped bond phase 1 having a central axis O, a plurality of abrasive grains 2 dispersed in the bond phase 1, a cutting edge 1A disposed on the outer periphery of the bond phase 1, and a coating layer 3 provided on the side surface of the bond phase 1. Note that in Figs. 2 and 3, the thickness of the cutting blade 10 is shown to be thicker than it actually is in order to easily explain the characteristic parts of the cutting blade 10 of this embodiment.
[0020] In this embodiment, the direction in which the central axis O of the bond phase 1 extends is called the axial direction. The axial direction corresponds to the thickness direction of the cutting blade 10. The axial direction may also be called the thickness direction. The direction perpendicular to the central axis O is called the radial direction. Of the radial directions, the direction approaching the central axis O is called the radially inner direction, and the direction away from the central axis O is called the radially outer direction. The direction rotating around the central axis O is called the circumferential direction.
[0021] The cutting blade 10 of this embodiment is in the shape of a circular ring. The cutting blade 10 is a so-called washer-type cutting blade. The axial dimension of the cutting blade 10 (hereinafter, sometimes simply referred to as thickness) is, for example, 0.2 mm or more and 0.5 mm or less.
[0022] The cutting blade 10 is detachably attached to the main shaft of a cutting device (dicer) (not shown) using a ring-shaped flange. The cutting blade 10 is rotated in the circumferential direction about the central axis O by the main shaft of the cutting device and moved in the radial direction relative to the material to be cut, and the cutting edge 1A protruding radially outward from the flange cuts into the material to cut it. In this embodiment, "cutting" is a concept that includes cutting processing and cutting processing such as groove processing. Therefore, the "cutting blade" may be rephrased as the "cutting blade."
[0023] In this embodiment, the bond phase 1 is a metal bond phase or an electroformed bond phase. That is, the bond phase 1 is a metallic bond phase. The bond phase 1 is made of a metal containing, for example, Cu-Sn or Ni as a main component.
[0024] As shown in FIG. 1 and FIG. 2, the bond phase 1 is an annular plate shape centered on a central axis O. That is, the disk shape of the above-mentioned "disk-shaped bond phase 1" in this embodiment includes an annular plate shape having a hole in the center of the disk. The bond phase 1 has an attachment hole 1B. The attachment hole 1B is located on the central axis O of the bond phase 1. The attachment hole 1B penetrates the bond phase 1 in the axial direction. The attachment hole 1B opens into a pair of side surfaces 1C facing the axial direction of the bond phase 1. The attachment hole 1B is a circular hole shape centered on the central axis O.
[0025] The thickness of the bond phase 1 is, for example, 0.15 mm or more and 0.45 mm or less. The cutting edge 1A has a circular ring shape centered on the central axis O. The cutting edge 1A is located on the outer circumferential surface of the bond phase 1.
[0026] The abrasive grains 2 are, for example, diamond abrasive grains or cBN abrasive grains. As shown in Fig. 3, the plurality of abrasive grains 2 includes a plurality of protruding abrasive grains 2a protruding in the axial direction from the side surface 1C of the bond phase 1. Specifically, the plurality of abrasive grains 2 include a plurality of protruding abrasive grains 2a protruding from the side surface 1C of the bond phase 1 and a plurality of embedded abrasive grains 2b that do not protrude from the side surface 1C of the bond phase 1.
[0027] The protruding abrasive grain 2a has an embedded portion 2c embedded in the bond phase 1 and a protruding portion 2d protruding from a side surface 1C of the bond phase 1. In this embodiment, the axial length of the embedded portion 2c (i.e., the embedded amount from the side surface 1C) is greater than the axial length of the protruding portion 2d (i.e., the protruding amount P from the side surface 1C). The embedded abrasive grain 2b is entirely embedded inside the bond phase 1.
[0028] The average grain size of the protruding abrasive grains 2a is, for example, 5 μm or more and 200 μm or less. As the protruding abrasive grains 2a and the embedded abrasive grains 2b, abrasive grains 2 of the same type and the same average grain size are used.
[0029] In this embodiment, the "average particle size" refers to a volume average diameter measured using a laser diffraction / scattering measuring device. The volume average diameter is an average diameter weighted based on the overall volume distribution of the abrasive grains 2, which are the object of measurement, including grains of small to large size. As the laser diffraction / scattering measuring device, for example, a model MT3300EXII-SDC manufactured by Microtrac Corporation can be used.
[0030] The coating layer 3 is made of a metal such as Cu or Ni. The coating layer 3 is provided on each of a pair of side surfaces 1C facing the axial direction of the bond phase 1. That is, a pair of coating layers 3 are provided. In this embodiment, the pair of coating layers 3 have the same thickness. The thickness of each coating layer 3 is smaller than the thickness of the bond phase 1. The thickness of each coating layer 3 is equal to or smaller than the average grain size of the protruding abrasive grains 2a. The thickness of each coating layer 3 is, for example, 2.5 μm or more and 150 μm or less.
[0031] The multiple protruding abrasive grains 2a are each exposed on a surface (outer surface) 3a facing the axial direction of the coating layer 3. The tops of the protruding abrasive grains 2a, i.e., the tops of the protruding abrasive grains 2a located at the ends of the protruding abrasive grains 2a opposite to the bond phase 1 in the axial direction, are disposed substantially flush with the surface 3a of the coating layer 3. More specifically, the distance D between the surface 3a of the coating layer 3 and the tops of the protruding abrasive grains 2a in the axial direction (height difference in the axial direction) is 1 μm or less. The distance D may also be referred to as the top protrusion amount D by which the tops of the protruding abrasive grains 2a protrude from the surface 3a of the coating layer 3.
[0032] The protruding amount P of the protruding abrasive grains 2a protruding in the axial direction from the side surface 1C of the bond phase 1 is, for example, 2.5 μm or more and 150 μm or less. The difference in the protruding amount P of each protruding abrasive grain 2a protruding from the side surface 1C of the bond phase 1 is 2 μm or less.
[0033] Next, a method for manufacturing the cutting blade 10 of this embodiment will be described with reference to Fig. 4. The method for manufacturing the cutting blade 10 of this embodiment includes a bond phase forming step S10, an abrasive grain protruding step S20, a coating layer forming step S30, and an abrasive grain exposing step S40.
[0034] In the bond phase preparation step S10, a bond phase 1 in which a plurality of abrasive grains 2 are dispersed is prepared. Specifically, when the bond phase 1 is composed of a metal bond phase, a mixed powder obtained by mixing the metal powder, which is the raw material of the bond phase 1, and the abrasive grains 2 is filled into a mold and pressed to form a disk shape, and then sintered under a predetermined pressure. In addition, when the bond phase 1 is composed of an electroformed bond phase, a base metal is placed in a plating solution containing the metal components that are the raw materials of the bond phase 1 and abrasive grains 2, and the bond phase 1 is precipitated to a predetermined thickness on the surface of the base metal while incorporating the abrasive grains 2, and this is then peeled off from the base metal and formed into a disk shape.
[0035] In the abrasive grain protrusion step S20, a plurality of protruding abrasive grains 2a are protruded from the side surface 1C of the bond phase 1. That is, the side surface 1C of the bond phase 1 is subjected to, for example, lapping or etching, to be dressed so that the protruding abrasive grains 2a protrude.
[0036] In the coating layer preparation step S30, a coating layer 3 is prepared on the side surface 1C of the bond phase 1 so as to be thicker than the protruding amount P of the protruding abrasive grains 2a from the side surface 1C. That is, for example, the bond phase 1 is placed in a plating solution containing a metal component that is the raw material of the coating layer 3, and a coating layer 3 having a thickness thicker than the protruding amount P of the protruding abrasive grains 2a is precipitated on the side surface 1C. By the coating layer preparation step S30, the protruding abrasive grains 2a, including their tops, are covered with the coating layer 3.
[0037] In the abrasive grain exposure step S40, the surface 3a of the coating layer 3 is polished to expose a plurality of protruding abrasive grains 2a on the surface 3a. That is, the surface 3a of the coating layer 3 is polished, and the polishing is stopped when the tops of the protruding abrasive grains 2a are exposed on the surface 3a, thereby arranging the surface 3a of the coating layer 3 and the tops of the protruding abrasive grains 2a to be approximately flush with each other. After the above steps S10 to S40, the cutting blade 10 is manufactured through an inner and outer diameter machining step (not shown) and the like.
[0038] According to the cutting blade 10 and the manufacturing method thereof of the present embodiment described above, each protruding abrasive grain 2a protruding from the side surface 1C of the bond phase 1 is exposed to the surface 3a of the coating layer 3. These protruding abrasive grains 2a are arranged substantially flush with the surface 3a of the coating layer 3 and contact the cut surface of the workpiece, thereby suppressing side wear of the cutting blade 10 and reducing blade thinning. This maintains good processing quality and processing dimensions of electronic material components cut into individual pieces from the workpiece, and extends the tool life. In addition, since the difference between the protruding amounts P, P of each protruding abrasive grain 2a protruding from the side surface 1C of the bond phase 1 is 2 μm or less, the multiple protruding abrasive grains 2a contact evenly with the cut surface of the workpiece, and the above-mentioned functions are stably obtained.
[0039] In this embodiment, the distance D between the surface 3a of the coating layer 3 and the top of the protruding abrasive grain 2a in the axial direction is 1 μm or less. In this case, the distance D, which is the difference in height between the surface 3a of the coating layer 3 and the tops of the protruding abrasive grains 2a, is kept small, within the range of 0 to 1 μm, so that chips are less likely to accumulate between the protruding abrasive grains 2a exposed on the surface 3a of the coating layer 3. Generally, chips adhering to the surface 3a of the coating layer 3 (i.e., the blade side surface) accelerate the progress of blade thinning, so according to the above-mentioned configuration of this embodiment, it is possible to suppress the adhesion of chips to the surface 3a of the coating layer 3, and to more stably reduce blade thinning.
[0040] In addition, in this embodiment, since the bond phase 1 is a metallic bonding phase and the coating layer 3 is made of metal, the side wear of the cutting blade 10 is further suppressed.
[0041] In this embodiment, the thickness of the coating layer 3 is equal to or smaller than the average grain size of the protruding abrasive grains 2a. In this case, the protruding abrasive grains 2a are exposed on the surface 3a of the coating layer 3 in a state where a part of the protruding abrasive grains 2a is embedded in the bond phase 1, that is, in a state where the protruding abrasive grains 2a are held in the bond phase 1. Therefore, the above-mentioned action and effect of the protruding abrasive grains 2a can be stably obtained.
[0042] In this embodiment, the embedded amount of the embedded portion 2c of the protruding abrasive grain 2a from the side surface 1C is greater than the protruding amount P of the protruding portion 2d from the side surface 1C. In this case, the protruding abrasive grains 2a are stably held in the bond phase 1, and the above-mentioned functional effects of the protruding abrasive grains 2a can be stably obtained.
[0043] The present invention is not limited to the above-described embodiment, and the configuration may be modified within the scope of the present invention, for example as described below.
[0044] Although not specifically shown, the cutting blade 10 may include a plurality of fillers dispersed in the bond phase 1. The plurality of fillers may also be dispersed in the coating layer 3.
[0045] In addition, the configurations (elements) described in the above-mentioned embodiments, modifications, and notes may be combined without departing from the spirit of the present invention, and addition, omission, substitution, and other modifications of the configurations are possible. Furthermore, the present invention is not limited to the above-mentioned embodiments, but is limited only by the claims. EXAMPLES
[0046] The present invention will be described in more detail below with reference to examples, although the present invention is not limited to these examples.
[0047] As an example of the present invention, the cutting blade 10 according to the above-described embodiment was prepared. The specifications of the cutting blade 10 are as follows. Bond phase 1 and abrasive grain 2: MD325-75HM633 Lapped product (That is, the bond phase 1 is made of a Cu-Sn alloy, the abrasive grains 2 have a grain size of #325, the concentration of the abrasive grains 2 is 75, and the side surface 1C of the bond phase 1 is sharpened by lapping. Note that the "concentration" is an index representing the content of the abrasive grains 2 dispersed in the bond phase 1. For example, a concentration of 100 indicates that the volume ratio (content) of the abrasive grains 2 in the bond phase 1 is 25%. The concentration of 75 indicates that the volume ratio of the abrasive grains 2 in the bond phase 1 is 18.75%.) Maximum protrusion of protruding abrasive grain 2a from side surface 1C: 30μm Material of coating layer 3: Cu (Example 1), Ni (Example 2) Coating layer 3 thickness: 28μm, 29μm, 30μm, 31μm (In the case where the thickness of the coating layer 3 is 29 μm and 30 μm, the distance D between the surface 3a of the coating layer 3 and the top of the protruding abrasive grain 2a (top protrusion amount) is 1 μm or less.) Blade dimensions: outer diameter 58mm, inner diameter 40mm, thickness 0.32mm (total thickness)
[0048] As a comparative example, a cutting blade was prepared in which the coating layer 3 was not provided on the side surface 1C of the bond phase 1. The specifications of the cutting blade of the comparative example were the same as those of the above-mentioned "bond phase 1 and abrasive grains 2" and "blade dimensions".
[0049] <Blade shape confirmation test> Using each of the cutting blades of the above-mentioned Examples and Comparative Examples, a predetermined number of grooves were cut into a dressing plate, and the amount of change in the cutting edge width was confirmed. The test conditions are as follows. -Dicer used: Tokyo Seimitsu A-WD100A · Dressing plate used: Tokyo Seimitsu A2-2mm Spindle speed: 15000m -1 Feed speed: 100mm / s Depth of cut: 1.5mm Number of grooves: 100 Measuring the cutting edge width: Grooves are made in the carbon and the shape of the grooves in the carbon is measured The results are shown in Table 1 below.
[0050] [Table 1]
[0051] As shown in Table 1, in Examples 1 and 2 of the present invention, the change in the cutting edge width before and after 100 grooves (cutting) was suppressed to a smaller amount than in the comparative example. In other words, in Examples 1 and 2, wear on the blade side was suppressed more than in the comparative example, and the blade thinning was reduced. Among Examples 1 and 2, it was confirmed that the change in the cutting edge width was significantly suppressed in Examples 1-2, 1-3, 2-2, and 2-3, in which the distance D between the surface 3a of the coating layer 3 and the top of the protruding abrasive grain 2a was 1 μm or less.
[0052] <Workpiece cutting confirmation test> Next, a predetermined number of workpieces were cut using each of the cutting blades of the above-mentioned examples and comparative examples, and the amount of change in the dimensions of the workpieces was confirmed. The test conditions are as follows. -Dicer used: Tokyo Seimitsu A-WD100A · Workpiece used: 5x5 dummy BGA workpiece Spindle speed: 30000m -1 Feed speed: 100mm / s Tape cut: 0.08mm Dimension measurement: Measure the dimensions of the cut workpieces for the first and 500th workpieces. The results are shown in Table 2 below.
[0053] [Table 2]
[0054] As shown in Table 2, in Examples 1 and 2 of the present invention, the change in the workpiece dimensions before and after cutting 500 workpieces was kept small compared to the comparative example. In other words, in Examples 1 and 2, wear on the blade side was suppressed more than in the comparative example, and the blade thinning was reduced. Among Examples 1 and 2, it was confirmed that the change in the workpiece dimensions was remarkably kept small, particularly in Examples 1-2, 1-3, 2-2, and 2-3, in which the distance D between the surface 3a of the coating layer 3 and the top of the protruding abrasive grain 2a was 1 μm or less. [Industrial Applicability]
[0055] According to the cutting blade and the manufacturing method of the cutting blade of the present invention, wear on the blade side can be suppressed and blade thinning can be reduced. As a result, the processing quality and processing dimensions of the electronic material components cut into individual pieces from the cut material can be maintained at a good level, and the tool life can be extended. Therefore, the cutting blade and the manufacturing method of the cutting blade of the present invention have industrial applicability. [Explanation of symbols]
[0056] 1...bond phase, 1A...cutting edge, 1C...side surface, 2...abrasive grain, 2a...protruding grain, 2c...embedded portion, 2d...protruding portion, 3...coating layer, 3a...surface, 10...cutting blade, D...distance, O...center axis, P...protruding amount, S10...bond phase preparation process, S20...abrasive grain protrusion process, S30...coating layer preparation process, S40...abrasive grain exposure process
Claims
1. A disk-shaped bond phase having a central axis; a plurality of abrasive grains dispersed in the bond phase; A cutting edge disposed on an outer periphery of the bond phase; A coating layer provided on a side surface of the bond phase, The coating layer is Cu or Ni, The plurality of abrasive grains include a plurality of protruding abrasive grains protruding from a side surface of the bond phase, As the protruding abrasive grains, abrasive grains having an abrasive grain size of #325 are used, The plurality of protruding abrasive grains are each exposed on a surface of the coating layer, The difference in the amount of protrusion of each of the protruding abrasive grains from the side surface of the bond phase is 2 μm or less; The protruding abrasive grains are an embedded portion embedded in the bond phase; A protrusion protruding from a side surface of the bond phase, an embedding amount of the embedding portion from the side surface is greater than an embedding amount of the protruding portion from the side surface; Cutting blade.
2. In the axial direction in which the central axis extends, the distance between the surface of the coating layer and the top of the protruding abrasive grain is 1 μm or less.
2. The cutting blade of claim 1.
3. The bond phase is a metal bond phase or an electroformed bond phase.
3. A cutting blade according to claim 1 or 2.
4. The thickness of the coating layer is equal to or less than the average grain size of the protruding abrasive grains. A cutting blade according to any one of claims 1 to 3.
5. A method for manufacturing a cutting blade according to any one of claims 1 to 4, comprising the steps of: a bond phase preparation step of preparing the bond phase in which the plurality of abrasive grains are dispersed; an abrasive grain protruding step of protruding the plurality of protruding abrasive grains from a side surface of the bond phase by performing a lapping process or an etching process on the side surface of the bond phase; a coating layer preparation step of preparing the coating layer on a side surface of the bond phase so as to have a thickness greater than the protrusion amount; and an abrasive grain exposing step of polishing a surface of the coating layer to expose the plurality of protruding abrasive grains on the surface. A method for manufacturing a cutting blade.
Citation Information
Patent Citations
Electrodeposition coated blade and its manufacture
JP2000144477A
Electroforming thin edge whetstone and its manufacturing method
JP2004136431A
Thin edge grinding wheel
JP2009006407A
Method of manufacturing thin-bladed whetstone
JP2009196058A