Ceramic Susceptor
The ceramic susceptor addresses alignment and heat loss issues by integrating internal air pumping and a single material connecting rod, improving yield and reducing costs through enhanced component alignment and temperature uniformity.
Patent Information
- Application Number
- JP2024000122
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2023-11-07
- Filing Date
- 2024-01-04
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-01-04
AI Technical Summary
Conventional ceramic susceptors face challenges in aligning and joining components due to individual manufacturing of flow channels, leading to decreased yield and increased processing costs, along with issues of heat loss and temperature non-uniformity due to the need for a large shaft cross-sectional area and bending of heating elements to avoid flow paths.
A ceramic susceptor design that integrates an insulating plate, shaft, and mount with internal air pumping, allowing for vacuum and purge functions, and uses a single material connecting rod without an intermediate layer to reduce electrical resistance and shear stress, facilitating alignment and reducing heat loss.
Improves yield and reduces processing costs by enabling easier component alignment, minimizing heat loss, and enhancing temperature uniformity while preventing oxidation and electrical resistance issues.
Smart Images

Figure 0007577876000001 
Figure 0007577876000002 
Figure 0007577876000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a ceramic susceptor, and more particularly to a ceramic susceptor in which air is pumped through an internal space of a shaft. [Background technology]
[0002] In general, semiconductor devices or display devices are manufactured by sequentially stacking a plurality of thin film layers, including dielectric layers and metal layers, on a glass substrate, a flexible substrate, or a semiconductor wafer substrate, and then patterning the layers. The thin film layers are sequentially deposited on the substrate by a chemical vapor deposition (CVD) process or a physical vapor deposition (PVD) process. The CVD process includes a low pressure chemical vapor deposition (LPCVD) process, a plasma enhanced chemical vapor deposition (PECVD) process, a metal organic chemical vapor deposition (MOCVD) process, and the like.
[0003] In such CVD and PVD equipment, a ceramic susceptor is disposed to support a glass substrate, a flexible substrate, a semiconductor wafer substrate, etc. and to perform a heat treatment, etc. The ceramic susceptor may be installed in the CVD and PVD equipment and used to heat the substrate in a heat treatment process, etc. The ceramic susceptor may also include a radio frequency (RF) electrode and be used to generate plasma in an etching process, etc. of a thin film layer formed on a semiconductor wafer substrate.
[0004] FIG. 1A is a schematic cross-sectional view showing a conventional ceramic susceptor.
[0005] First, as shown in FIG. 1A, the conventional ceramic susceptor includes an insulating plate 10 coupled to a shaft 20, and the insulating plate 10 includes a heating element 12, such as a mesh-shaped element, disposed within a ceramic material. The heating element 12 is connected to a connecting rod 22 and receives power from an external power source via a mount 30. In addition, the conventional ceramic susceptor pumps air through a flow path 31 that penetrates the insulating plate 10, the shaft 20, and the mount 30 to fix a substrate 11, such as a semiconductor wafer, by using a vacuum chuck function during a semiconductor process. In particular, the flow path 31 is formed inside a side wall in the longitudinal direction of the shaft 20. However, in the conventional ceramic susceptor, it is difficult to align the flow path 31 in the process of bonding the insulating plate 10, the shaft 20, and the mount 30 after they are separately manufactured. Therefore, the production yield of the conventional ceramic susceptor is reduced, which results in an increase in processing costs.
[0006] Moreover, in such a conventional ceramic susceptor, the cross-sectional area of the shaft 20 must be made large in order to process the through flow passage 31 in the side wall of the shaft 20, which increases the problem of increased heat loss. In addition, as shown in Figures 1B and 1C, not only the heating element 12 but also the high-frequency electrode (not shown) arranged other than the heating element 12 must be bent in order to avoid the hole 33 through which the flow passage 31 in the side wall of the shaft 20 reaches the upper surface of the insulating plate 10 where the groove 15 is located, but this also causes problems of heat loss and reduced temperature uniformity in the surrounding zone AA. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] Korean Patent Application No. 10-2009-0020821 (March 11, 2009) [Patent Document 2] Korean Patent Application No. 10-2017-0168278 (December 8, 2017) [Patent Document 3] International Patent Application WO1999 / 56307 (November 4, 1999) Summary of the Invention [Problem to be solved by the invention]
[0008] Therefore, the present invention has been devised to solve the above-mentioned problems, and an object of the present invention is to provide a ceramic susceptor which allows air pumping through an internal space of a shaft, thereby enabling a vacuum chuck function and a purge function, so that the alignment and joining of parts can be easily performed, thereby improving yield and reducing processing costs, and which allows the vacuum chuck / purge function to be used simultaneously with an electrostatic chuck.
[0009] In addition, the connecting rod for power supply in the internal space of the shaft can be formed from a single material without an intermediate layer (KOVAR) for oxidation prevention, thereby providing a ceramic susceptor that can reduce electrical resistance and the effects of shear stress. [Means for solving the problem]
[0010] To summarize the features of the present invention, a ceramic susceptor according to one aspect of the present invention for achieving the above-mentioned object includes an insulating plate having an electrode disposed thereon; a shaft having one end connected to the insulating plate; a power supply rod connected to the electrode and extending to pass through an internal space of the shaft; and a separator coupled to the other end of the shaft and sealing the internal space of the shaft, wherein the insulating plate includes a first through passage penetrating between an upper surface and a lower surface to communicate with the internal space of the shaft, and the first through passage can be used to perform a vacuum chuck function and / or a purge function.
[0011] The ceramic susceptor may further include a mount connected to a lower portion of the shaft and including a second through passage that communicates an inner space of the shaft with the outside.
[0012] The first through-passage is maintained at a negative pressure lower than atmospheric pressure, so that the substrate placed on the insulating plate can be attracted.
[0013] A purge function can be performed by maintaining a positive pressure higher than atmospheric pressure through the first through passage.
[0014] The electrode may be a heating element, and the ceramic susceptor may further include an electrode for generating plasma disposed within the insulating plate and spaced apart from the electrode.
[0015] The insulating plate includes a second electrode disposed apart from the electrode for chucking and dechucking a substrate disposed on the insulating plate, and while maintaining the chucking of the substrate using the second electrode, a positive pressure higher than atmospheric pressure is maintained through the first through-passage, thereby simultaneously performing a purge function.
[0016] The ceramic susceptor may further include a connector embedded in the insulating plate and electrically connected to the electrode, and the power supply rod may be brazed and joined to the connector with a conductive filler.
[0017] The power supply rod may be extended as a single rod through the interior space of the shaft, contacting the connector, and through a mount at the bottom of the shaft.
[0018] The connector and the power supply rod may be made of the same material.
[0019] The electrode may be a heating element, an electrode for plasma generation, or a chuck electrode for electrostatic chucking function.
[0020] The electrode may be a heating element, and the ceramic susceptor may further include a chuck electrode for electrostatic chucking, the chuck electrode being disposed within the insulating plate and spaced apart from the electrode.
[0021] When performing a vacuum chuck function using the first through-passage, an electrostatic chuck function can be further performed using the electrode. Effect of the Invention
[0022] According to the ceramic susceptor of the present invention, air pumping for chucking a substrate is performed through the internal space of the shaft, which facilitates alignment and bonding of parts, thereby improving yield and reducing processing costs.
[0023] In addition, the present invention does not require machining of through holes in the side wall of the shaft, which allows the shaft cross-sectional area to be made smaller, thereby reducing heat loss compared to the prior art. Since the chucking or purging function can be achieved using the through passage on the central side, there is no need to bend the built-in heating element or electrode to avoid the through passage on the central side. Therefore, there is an advantage that the temperature uniformity can be improved in the zone surrounding the through passage (BB in Figure 2C) compared to the prior art.
[0024] In addition, since the connecting rod for supplying power to the inner space of the shaft can be formed of a single material without an intermediate layer (KOVAR) for stress buffering, the electrical resistance of the connecting rod can be reduced, and the occurrence of cracks or arching due to shear stress can be reduced.
[0025] In addition, a vacuum chuck function is realized by using the internal space at the center of the shaft, and an electrostatic chuck function is simultaneously used by the chuck electrode. Therefore, when the chucking force of the vacuum chuck function is weak in the low-pressure atmosphere of a semiconductor processing chamber, the electrostatic chuck electrode is used to supplement the chucking force, and when the chucking force of the electrostatic chuck electrode is weak in the high-temperature atmosphere of a semiconductor processing chamber, the vacuum chuck function is used to supplement the chucking force. Not only that, the vacuum in the internal space of the shaft at high temperatures can reduce the thermal conductivity of the shaft (vacuum reduces thermal conductivity) and reduce oxidation problems of the power supply rod inside the shaft (vacuum also reduces oxidation problems). [Brief description of the drawings]
[0026] The accompanying drawings, which are included as part of the detailed description to aid in understanding the present invention, provide examples of the present invention and, together with the detailed description, explain the technical concepts of the present invention.
[0027] [Figure 1A] FIG. 1 is a schematic cross-sectional view showing a conventional ceramic susceptor. [Figure 1B] 1B is an example of a heating element pattern when the ceramic susceptor in FIG. 1A is viewed from above. [Figure 1C] 1B is a top view of the ceramic susceptor in FIG. 1A, showing the upper surface of an insulating plate and the heating element thereunder superimposed thereon. [Figure 2A] 1 is a schematic cross-sectional view showing a ceramic susceptor according to an embodiment of the present invention. [Figure 2B] 2B is an example of a heating element pattern when the ceramic susceptor in FIG. 2A is viewed from above. [Figure 2C] 2B is a top view of the ceramic susceptor in FIG. 2A, showing the upper surface of an insulating plate and the heating element thereunder superimposed thereon. [Diagram 3] FIG. 2 is a cross-sectional view showing a connecting rod joint portion according to a first embodiment of the ceramic susceptor of the present invention. [Figure 4]FIG. 4 is a cross-sectional view showing a connecting rod joint portion according to a second embodiment of the ceramic susceptor of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0028] The present invention will be described in detail below with reference to the accompanying drawings. Here, the same components in each drawing are assigned the same reference numerals as much as possible. Also, detailed description of already known functions and / or configurations will be omitted. The contents disclosed below will be described with emphasis on parts necessary for understanding the operation of various embodiments, and description of elements that may make the gist of the description unclear will be omitted. Also, some components in the drawings may be exaggerated, omitted, or generally illustrated. The size of each component does not entirely reflect the actual size, and therefore the contents described herein are not limited by the relative sizes and intervals of the components depicted in each drawing.
[0029] When describing the embodiments of the present invention, if it is determined that a detailed description of a known technology related to the present invention may make the gist of the present invention unclear, the detailed description will be omitted. The terms described below are defined in consideration of the functions in the present invention, and may be changed according to the intention or practice of the user or operator. Therefore, the definitions should be based on the entire contents of this specification. The terms used in the detailed description are merely for describing the embodiments of the present invention and should not be limiting in any way. Unless otherwise specified, expressions in the singular form include the plural form. In this description, expressions such as "include" or "comprise" are intended to indicate certain features, numbers, steps, operations, elements, parts thereof, or combinations thereof, and should not be interpreted to exclude the presence or possibility of one or more features, numbers, steps, operations, elements, parts thereof, or combinations other than those described.
[0030] In addition, terms such as first and second may be used to describe various components, but these terms are not intended to limit the various components, and these terms are only used to distinguish one component from another component.
[0031] FIG. 2A is a schematic cross-sectional view showing a ceramic susceptor according to one embodiment of the present invention.
[0032] 2A, a ceramic susceptor 100 according to an embodiment of the present invention includes an insulating plate 110, a shaft 120, and a mount 140. The insulating plate 110, the shaft 120, and the mount 140 are connected in sequence, and a separator 130 may be provided between the shaft 120 and the mount 140 and formed at a longitudinal end of the shaft 120 to separate the internal spaces of the shaft 120 and the mount 140.
[0033] The ceramic susceptor 100 according to an embodiment of the present invention has a vacuum chuck structure that uses an air pump 500 to support a substrate 11 to be processed for various purposes, such as a semiconductor wafer, a glass substrate, a flexible substrate, or the like.
[0034] For this purpose, the insulating plate 110 is configured to have a heating element (electrode) 114 disposed (embedded) between the ceramic materials, and may further be configured to have another electrode 112 disposed (embedded) at a predetermined interval from the heating element 114 in some cases. The insulating plate 110 is configured to stably support a substrate to be processed, and to perform various semiconductor processes such as heating using the heating element 114 and / or supporting the substrate using the electrode 112, or a plasma enhanced chemical vapor deposition process or a dry etching process using plasma. The insulating plate 110 may be formed as a plate-like structure having a predetermined shape. For example, the insulating plate 110 may be formed as a circular plate-like structure, but is not necessarily limited thereto. Here, the ceramic material may be Al2O3, Y2O3, Al2O3 / Y2O3, ZrO2, AlC (autoclaved lightweight concrete), TiN, AlN, TiC, MgO, CaO, CeO2, TiO2, B x C y The ceramic powder may be at least one of the following: BN, SiO2, SiC, YAG, Mullite, and AlF3, and preferably aluminum nitride (AlN). The ceramic powder may be molded and sintered to form the insulating plate 110, and each ceramic powder may selectively contain about 0.1 to 10%, preferably about 1 to 5% of yttrium oxide powder.
[0035] The heating element (electrode) 114 may be formed in a flat coil shape or a flat plate shape using a heating wire (or a resistance wire). The heating element 114 may also be formed in a multi-layer structure for precise temperature control. The heating element 114 is connected to a power source provided to each heating element 114 through connecting rods 121 and 122 to receive power, and can function to heat the substrate 11 to be processed on the insulating plate 110 to a predetermined temperature in order to perform a substrate heating process, deposition process, etching process, etc. in a semiconductor process. The connecting rods 121 and 122 pass through the internal space of the shaft 120, pass through the separator 130, and extend to the outside through the mount 140.
[0036] The electrode 112 may be made of tungsten (W), molybdenum (Mo), silver (Ag), gold (Au), niobium (Nb), titanium (Ti), aluminum nitride (AlN), or an alloy thereof, and may be preferably made of molybdenum (Mo). The electrode 112 may be connected to a power supply terminal (e.g., ground) through another connecting rod (not shown). The connecting rod (not shown) for the electrode 112 may also extend through the inner space of the shaft 120, through the separator 130, and through the mount 140 to the outside. For example, the electrode 112 may be used as a chuck electrode for an electrostatic chuck function for supporting the substrate 11 placed on the insulating plate 110, or as a plasma generation electrode for a plasma generation function for processes such as plasma enhanced chemical vapor deposition or dry etching in a reactive ion etch (RIE) device.
[0037] The shaft 120 is in the shape of a pipe having a through hole, and is coupled to the lower surface of the insulating plate 110. The shaft 120 may be made of the same ceramic material as the insulating plate 100 and coupled thereto. Here, the ceramic material may be Al2O3, Y2O3, Al2O3 / Y2O3, ZrO2, AlC (autoclaved lightweight concrete), TiN, AlN, TiC, MgO, CaO, CeO2, TiO2, B x C y The ceramic powder may be at least one of the following: BN, SiO2, SiC, YAG, mullite, and AlF3, and preferably aluminum nitride (AlN). The ceramic powder may be molded and sintered to form the shaft 120, and each ceramic powder may optionally contain about 0.1 to 10%, preferably about 1 to 5%, of yttrium oxide powder.
[0038] The shaft 120 may be joined to the insulating plate 110 with a joining material 125 such as ceramic paste. In some cases, the shaft 120 may be mechanically joined to the insulating plate 110 with bolts, nuts, etc. The rods (121, 122, etc.) that supply power to the electrodes 112 and / or the heating element 114 are housed through an internal space penetrating the shaft 120 and extend outward through a mount 140 that has a sealed external form (e.g., a rigid body or a member having a hollow).
[0039] As shown in FIG. 2A, the mount 140 is connected to the end of the shaft 120 in the longitudinal direction. The mount 140 may be mechanically connected to the shaft 120 by sandwiching the separator 130 formed at the end of the shaft 120 in the longitudinal direction. The connection between the shaft 120 and the separator 130 may be mechanically connected using bolts, nuts, etc. Also, the connection between the shaft 120 and the separator 130 and the upper part of the mount 140 may be mechanically connected using bolts, nuts, etc., and may be sealed so as to be completely sealed. The periphery of the through holes of the separator 130 for the connecting rods (121, 122, etc.) penetrating the separator 130 may be sealed without gaps using a paste of a ceramic material as described above. The upper part of the mount 140 may be fastened so as to wrap around the separator 130. The area between the top of the mount 140 and the separator 130 or between the top of the mount 140 and the shaft 120, i.e., the joint between the shaft 120 with the separator 130 and the mount 140, may be sealed without gaps by a ceramic paste as described above.
[0040] The above-mentioned connection mount 140 and the separator 130 may be made of a metal material such as aluminum (Al) or may be made of the above-mentioned ceramic material. That is, the ceramic material may be Al2O3, Y2O3, Al2O3 / Y2O3, ZrO2, AlC (autoclaved lightweight concrete), TiN, AlN, TiC, MgO, CaO, CeO2, TiO2, B x C yThe ceramic powder may be at least one of the following: BN, SiO2, SiC, YAG, mullite, and AlF3, and preferably aluminum nitride (AlN). The ceramic powder may be molded and sintered to form the shaft 120, and each ceramic powder may optionally contain about 0.1 to 10%, preferably about 1 to 5%, of yttrium oxide powder.
[0041] The ceramic susceptor 100 according to an embodiment of the present invention functions as a vacuum chuck by pumping air through the inner space of the shaft 120, thereby facilitating alignment and joining for matching air flow paths of components such as the insulating plate 110, the shaft 120, and the mount 140, thereby improving yield and reducing processing costs. In addition, in the present invention, since the inner space of the shaft 120 is maintained at a vacuum (negative pressure) lower than atmospheric pressure, oxidation of the connecting rods 121 and 122 in the inner space of the shaft 120 is prevented, the connecting rods 121 and 122 can be embodied as a single rod rather than a double-connected structure 51 and 52 (see FIG. 3), and the material of the connecting rods 121 and 122 can be made of Mo, which is the same as the material of the connector 41 (see FIG. 3 and FIG. 4) electrically connected to the heating element 114 (or other electrode 112) of the insulating plate 110. In other words, by making it possible to form the connecting rods 121, 122 from a single material such as Mo without the intermediate layer 51 (KOVAR) (see FIG. 3) for stress buffering, it is possible to reduce the electrical resistance of the connecting rods 121, 122 and reduce the occurrence of cracks or arching due to shear stress.
[0042] In addition, the ceramic susceptor 100 according to the embodiment of the present invention realizes a vacuum chuck function by using the internal space of the shaft 120, and at the same time, the electrode 112 of the chuck electrode also enables an electrostatic chuck function.
[0043] To this end, the insulating plate 110 includes a first through passage 91 for communication between the upper surface on which the substrate 11 is placed and the internal space of the shaft 120 so that air is pumped through the internal space of the shaft 120 to function as a vacuum chuck. The first through passage 91 is formed to penetrate between the upper surface and the lower surface near the center of the insulating plate 110, and the upper surface on which the substrate 11 is placed and the internal space of the shaft 120 are fluidically connected by the first through passage 91. In addition, the mount 140 includes a second through passage 92 for communication between the internal space of the shaft 120 and the outside so that air (vacuum pumping) is pumped through the internal space of the shaft 120 to function as a vacuum chuck. When the air pump 500 is connected to the second through-passage 92 to perform air pumping, air is pumped through the first through-passage 91, the internal space of the shaft 120, and the second through-passage 92, and the internal space of the shaft 120 and the first through-passage 91 are maintained at a negative pressure lower than atmospheric pressure, thereby adsorbing the substrate 11 disposed on the insulating plate 110. In this manner, when the vacuum chuck function is performed using the first through-passage 91, the electrode 112 can be used as an electrostatic chuck electrode to further perform an electrostatic chuck function. When an electrostatic chuck function is simultaneously used by applying power for chucking and dechucking using the electrostatic chuck electrode 112 in addition to the vacuum chuck function using the first through-passage 91, if the chucking force of the vacuum chuck function is weak in a low-pressure atmosphere in a semiconductor processing chamber, the chucking force can be supplemented by using the electrostatic chuck electrode 112, and if the chucking force of the electrostatic chuck electrode 112 is weak in a high-temperature atmosphere in a semiconductor processing chamber, the vacuum chuck function can not only supplement the chucking force but also reduce the thermal conductivity of the shaft 120 due to the vacuum in the internal space of the shaft 120 at high temperatures (vacuum reduces thermal conductivity) and reduce oxidation problems of the power supply rod inside the shaft 120 (vacuum also reduces oxidation problems).
[0044] The inside of the mount 140 may be in the form of a rigid body or a member having a hollow. When the mount 140 is a rigid body, the mount 140 may be provided with a through hole for passing the connecting rods 121 and 122 and a through hole for forming the second through passage 92. When the mount 140 is in the form of a member having a hollow, the through hole for passing the connecting rods 121 and 122 may be provided between the upper end and the lower end of the mount 140 so as to pass through the mount 140, and a pipe-shaped member (e.g., made of metal or ceramic material) for the second through passage 92 may be provided between the upper end and the lower end of the mount 140.
[0045] FIG. 2B shows an example of a pattern of heating elements 114 when viewed from above the ceramic susceptor 100 of FIG. 2A.
[0046] FIG. 2C is a top view of the ceramic susceptor 100 of FIG. 2A, showing the upper surface of the insulating plate 110 and the heating element 114 thereunder superimposed thereon.
[0047] 2B and 2C, the ceramic susceptor 100 of the present invention does not require processing through holes in the sidewall of the shaft 120, which allows the cross-sectional area of the shaft 120 to be small. Therefore, the ceramic susceptor 100 of the present invention can reduce heat loss compared to the conventional technology (see FIGS. 1A to 1C), can realize a chucking or purging function using the through passage 91 on the central side, and does not require the built-in heating element 114 or electrode 112 to be bent to avoid the through passage on the central side, which has the effect of improving temperature uniformity in the zone (BB in FIG. 2C) around the through passage 91 compared to the conventional technology.
[0048] The ceramic susceptor 100 of the present invention as described above may be installed in a chamber of a CVD or PVD apparatus and used for heating using the heating element 114 and / or supporting a substrate using the electrode 112, or for a plasma-enhanced chemical vapor deposition process or a dry etching process using plasma. As described above, the ceramic susceptor 100 of the present invention is capable of chucking and dechucking the substrate 11 by negative pressure air pumping through the first through-passage 91, the internal space of the shaft 120, and the second through-passage 92, and at this time, the insulating plate 110 is configured to stably support the substrate to be processed and perform various semiconductor processes such as heating using the heating element 114 and / or supporting the substrate using the electrode 112, or for a plasma-enhanced chemical vapor deposition process or a dry etching process using plasma.
[0049] Meanwhile, the ceramic susceptor 100 of the present invention can perform not only chucking and dechucking of the substrate 11 using the first through-passage 91, but also a purge function by maintaining the first through-passage 91 at a pressure higher than the atmospheric pressure through positive air pumping through the first through-passage 91, the inner space of the shaft 120, and the second through-passage 92. At this time, the air pump 500 can perform pumping to inject air at a predetermined pressure higher than the atmospheric pressure through the second through-passage 92.
[0050] For example, purging can be performed by blowing air containing a specific gas (e.g., nitrogen gas, or an inert gas such as He or Ar) into the chamber of the above-mentioned CVD apparatus and PVD apparatus through the first through-flow passage 91 by positive pressure air pumping.
[0051] This can blow away particles accumulated in pockets, especially in the grooves 15, on the upper surface of the insulating plate 110 in the chamber. This purging function is preferably performed after the substrate 11 is chucked on the upper surface of the insulating plate 110, but may be performed when there is no substrate 11 on the upper surface of the insulating plate 110, if necessary. However, during this purging function, an electrode disposed in the insulating plate 110, i.e., the electrode 112 as shown in FIG. 2A, may be used to chuck and dechuck the substrate 11 placed on the upper surface of the plate 110 in addition to the heating element 114. That is, the electrode 112 may be a high frequency electrode disposed to receive power for generating plasma as described above, or may be an electrostatic chuck electrode (or chuck electrode) disposed to receive power for chucking and dechucking the substrate 11. The electrode 112 may function as an electrostatic chuck electrode as it is, and an additional chuck electrode may be formed at a predetermined distance from the electrode 112 to receive power for chucking and dechucking the substrate 11. That is, the heating element 114, the electrode 112, and an additional electrode for chucking and dechucking the substrate 11 may be formed in different layers in the insulating plate 110 at a predetermined distance apart.
[0052] FIG. 3 is a cross-sectional view showing a joint portion of connecting rods 121, 122 according to a first embodiment of a ceramic susceptor 100 of the present invention.
[0053] 3, the connecting rods 121 and 122 may be electrically connected to the connector 41 embedded in the insulating plate 110 so as to be electrically connected to the heating element 114 (or the electrode 112) of the insulating plate 110. In this case, the connecting rods 121 and 122 are configured in a double-connected structure, i.e., a first rod 51 and a second rod 52, through a support eyelet 70 coupled to a thread formed on a part of the inner circumferential surface of a predetermined opening of the insulating plate 110.
[0054] Here, the connector 41, the connecting rods 121 and 122, and the support eyelet 70 may be made of a conductive material, for example, tungsten (W), molybdenum (Mo), silver (Ag), nickel (Ni), gold (Au), niobium (Nb), titanium (Ti), or an alloy thereof. In particular, in the double-connected structure of the connecting rods 121 and 122, the connector 41 may be made of Mo, the first rod 51 may be made of KOVAR (Fe-Ni-Co alloy) material as an intermediate layer for stress buffering, and the second rod 52 may be made of Ni. Also, the connecting rods 121 and 122 may be connected to the connector 41 by brazing. For example, the conductive filler 50 may be injected around the exposed portion of the connector 41 in advance, the first rod 51 may be pushed into the inside of the support eyelet 70 to bring one end surface of the first rod 51 into close contact with the connector 41, and then the first rod 51 may be cooled and joined to be electrically connected. Next, the second conductive filler 60 is sufficiently injected into the upper part of the other end surface of the first rod 51, and one end surface of the second rod 52 is brought into close contact with the injected second conductive filler 60, and then heated at high temperature and cooled to bond them, thereby electrically connecting them.
[0055] Although the connection portion of the connecting rods 121, 122 may be embodied in this manner, in the present invention, since the internal space of the shaft 120 is maintained at a vacuum lower than atmospheric pressure, oxidation of the connecting rods 121, 122 in the internal space of the shaft 120 is prevented, the connector 41 and the single-rod connecting rods 121, 122 may both be formed of Mo.
[0056] FIG. 4 is a cross-sectional view showing a joint portion of connecting rods 121 and 122 according to a second embodiment of the ceramic susceptor of the present invention.
[0057] 4, the connecting rods 121 and 122 may be electrically connected to the connector 41 embedded in the insulating plate 110 so as to be electrically connected to the heating element 114 (or the electrode 112) of the insulating plate 110. Here, a case will be described in which the connecting rods 121 and 122 have a single rod connection structure through a support eyelet 70 coupled to a thread formed on a part of the inner circumferential surface of a predetermined opening of the insulating plate 110.
[0058] Here, the connector 41, the connecting rods 121, 122, and the support eyelets 70 may be made of a conductive material, for example, tungsten (W), molybdenum (Mo), silver (Ag), nickel (Ni), gold (Au), niobium (Nb), titanium (Ti), or an alloy thereof.
[0059] In particular, in the present invention, since the internal space of the shaft 120 is maintained at a vacuum lower than atmospheric pressure, oxidation of the connecting rods 121, 122 in the internal space of the shaft 120 is prevented, so the connecting rods 121, 122 can be embodied as a single rod instead of the double connection structure 51, 52 as shown in Fig. 3, and the material of the connecting rods 121, 122 can be made of Mo, which is the same as the material of the connector 41 electrically connected to the heating element 114 (or electrode 112) of the insulating plate 110. In other words, by making it possible to form the connecting rods 121, 122 from a single material such as Mo without the intermediate layer 51 (KOVAR) for stress buffering as shown in Fig. 3, the electrical resistance of the connecting rods 121, 122 can be reduced, and the occurrence of cracks or arching due to shear stress can be reduced.
[0060] Here, the connecting rods 121, 122 may be connected to the connector 41 by brazing. For example, the conductive filler 50 may be injected around the exposed portion of the connector 41 in advance, the connecting rods 121, 122 may be pushed into the inside of the support eyelet 70 to bring one end surface of the connecting rods 121, 122 into close contact with the connector 41, and the connecting rods 121, 122 may be heated at a high temperature and then cooled to join them, thereby electrically connecting them.
[0061] As described above, the ceramic susceptor 100 according to the present invention has the advantage that the alignment and bonding of parts can be facilitated by allowing air pumping for chucking the substrate through the internal space of the shaft 120, thereby improving the yield and reducing the processing cost. In addition, the present invention does not require the machining of through holes in the side walls of the shaft, thereby allowing the shaft cross-sectional area to be made small, thereby reducing heat loss compared to the prior art, and since the chucking or purging function can be achieved using the through passage 91 on the central side, it is not necessary to bend the built-in heating element or electrode to avoid the through passage on the central side, thereby improving the temperature uniformity in the zone BB around the through passage 91 compared to the prior art.
[0062] In addition, the connecting rods 121, 122 for supplying power to the internal space of the shaft can be formed of a single material without the intermediate layer 51 (KOVAR) for stress buffering, which reduces the electrical resistance of the connecting rods 121, 122 and also reduces the occurrence of cracks or arching due to shear stress.
[0063] In addition, the ceramic susceptor 100 according to an embodiment of the present invention may realize a vacuum chuck function using the internal space of the shaft 120, and simultaneously use an electrostatic chuck function through the electrode 112 of the chuck electrode.
[0064] As described above, the present invention has been described by specific matters such as specific components, limited embodiments, and drawings, but these are provided only to assist in a more general understanding of the present invention, and the present invention is not limited to the above embodiments, and a person having ordinary knowledge in the field to which the present invention belongs may make various modifications and variations within the scope of the essential characteristics of the present invention. Therefore, the idea of the present invention should not be limited to the described embodiments, and not only the scope of the claims described below, but also technical ideas that are equivalent or have equivalent modifications to the scope of the claims should be interpreted as being included in the scope of the present invention. [Explanation of symbols]
[0065] 110 Insulating plate 112 High Frequency Electrode 114 Heating element 120 Shaft 121,122 Connecting rod 91 First through passage 92 Second through passage
Claims
1. an insulating plate on which an electrode is disposed; a shaft having one end connected to the insulating plate; a power supply rod connected to the electrode and extending through the interior space of the shaft; a separator coupled to the other end of the shaft and sealing an internal space of the shaft; the insulating plate includes a first through passage extending between an upper surface and a lower surface thereof to communicate with an interior space of the shaft; A ceramic susceptor performing a vacuum chuck function and / or a purge function using an internal space of the shaft in which the power supply rod is housed and the first through passage.
2. The ceramic susceptor according to claim 1 , further comprising a mount connected to a lower portion of the shaft and including a second through passage that communicates an interior space of the shaft with the outside.
3. The ceramic susceptor according to claim 1 , wherein the first through passage is maintained at a negative pressure lower than atmospheric pressure to adsorb the substrate placed on the insulating plate.
4. The ceramic susceptor according to claim 1 , wherein a positive pressure higher than atmospheric pressure is maintained through the first through passage to perform a purge function.
5. The ceramic susceptor according to claim 1 , wherein the electrode is a heating element, and further comprises an electrode for generating plasma disposed in the insulating plate and spaced apart from the electrode.
6. the insulating plate includes a second electrode spaced apart from the electrode for chucking and dechucking a substrate disposed on the insulating plate; 2. The ceramic susceptor according to claim 1, wherein the second electrode is used to chuck the substrate while simultaneously performing a purge function by maintaining a positive pressure higher than atmospheric pressure through the first through passage.
7. a connector embedded in the insulating plate and electrically connected to the electrode, The ceramic susceptor according to claim 1 , wherein the power supply rod is brazed to the connector with a conductive filler.
8. 8. The ceramic susceptor of claim 7, wherein the power supply rod passes through the interior space of the shaft in contact with the connector as a single rod and extends through a mount at the bottom of the shaft.
9. 8. The ceramic susceptor of claim 7, wherein the connector and the power supply rod are made of the same material.
10. The ceramic susceptor according to claim 1 , wherein the electrode is a heating element, an electrode for generating plasma, or a chuck electrode for an electrostatic chuck function.
11. The ceramic susceptor according to claim 1 , further comprising a chuck electrode for electrostatic chuck function, the electrode being a heating element and spaced apart from the electrode within the insulating plate.
12. The ceramic susceptor according to claim 1 , wherein when the first through-passage is used to perform a vacuum chuck function, the electrode is further used to perform an electrostatic chuck function.
Citation Information
Patent Citations
Improved heater for substrate processing equipment for depositing tungsten
JP2002513091A
Heater for thin film vapor deposition
JP2007182622A
Vacuum chucking heater of axisymmetrical and uniform thermal profile
JP2009033178A
High-temperature vacuum chuck assembly
JP2011510488A
Susceptor and manufacturing method therefor
JP2012080103A