Strain gauges
The strain gauge with recessed insulating resin and laminated metal structure addresses moisture penetration issues in high-temperature, high-humidity environments, enhancing accuracy by preventing corrosion and maintaining resistor integrity.
Patent Information
- Application Number
- JP2020180489
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-10-28
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2040-10-28
AI Technical Summary
Strain gauges used in high-temperature, high-humidity environments are prone to moisture penetration through the insulating resin layer, leading to corrosion of the wiring due to the concentration of dirt and generation of acid or alkali-inclined base points.
A strain gauge design featuring a flexible base material with a resistor and wiring covered by an insulating resin layer that includes recesses to prevent moisture penetration, utilizing a Cr mixed phase film for the resistor and a laminated metal structure for the wiring to enhance stability and accuracy.
The design effectively suppresses moisture penetration, preventing corrosion of the wiring and improving the accuracy of strain detection by maintaining the integrity of the resistor and wiring.
Smart Images

Figure 0007577907000001 
Figure 0007577907000002 
Figure 0007577907000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a strain gauge. [Background technology]
[0002] There is known a strain gauge that is attached to a measurement object to detect strain of the measurement object. The strain gauge includes a resistor that detects strain, and the resistor is formed on, for example, a substrate. The resistor is connected to an electrode via, for example, a wiring. The strain gauge also includes, on the substrate, an insulating resin layer that covers, for example, the resistor and the wiring (see, for example, Patent Document 1). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2016-74934 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, for example, when a strain gauge is used in a high-temperature and high-humidity environment, water droplets may adhere to the upper surface of the insulating resin layer and evaporate, collecting and concentrating dirt on the upper surface of the insulating resin layer. When the dirt is concentrated, base points that are inclined to acid or alkali are generated, deteriorating the insulating resin layer, and as a result, the penetration of moisture causes corrosion of the wiring covered by the insulating resin layer.
[0005] The present invention has been made in consideration of the above-mentioned points, and has an object to provide a strain gauge that can suppress the penetration of moisture from an insulating resin layer that covers wiring. [Means for solving the problem]
[0006] This strain gauge includes a flexible substrate, a resistor formed on the substrate, wiring formed on the substrate and electrically connected to the resistor, and an insulating resin layer formed on the substrate and covering the resistor and the wiring, the insulating resin layer having a plurality of recesses recessed from an upper surface toward the substrate. The recess has one bottom surface and four inner side surfaces connected to the bottom surface. is. Effect of the Invention
[0007] According to the disclosed technique, it is possible to provide a strain gauge capable of suppressing the penetration of moisture through an insulating resin layer that covers wiring. [Brief description of the drawings]
[0008] [Figure 1] FIG. 2 is a plan view illustrating the strain gauge according to the first embodiment. [Diagram 2] 1 is a cross-sectional view (part 1) illustrating a strain gauge according to a first embodiment. FIG. [Diagram 3] 4 is a cross-sectional view (part 2) illustrating the strain gauge according to the first embodiment. FIG. [Figure 4] 2 is a partial perspective view illustrating a cover layer of the strain gauge according to the first embodiment. FIG. [Diagram 5] 4 is a cross-sectional view (part 3) illustrating the strain gauge according to the first embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the drawings, the same components are denoted by the same reference numerals, and duplicated explanations may be omitted.
[0010] First Embodiment FIG. 1 is a plan view illustrating the strain gauge according to the first embodiment. FIG. 2 is a cross-sectional view illustrating the strain gauge according to the first embodiment, showing a cross section along the line AA in FIG. 1. FIG. 3 is a cross-sectional view illustrating the strain gauge according to the first embodiment, showing a cross section along the line BB in FIG. 1. FIG. 4 is a partial perspective view illustrating a cover layer of the strain gauge according to the first embodiment. With reference to FIGS. 1 to 4, the strain gauge 1 has a substrate 10, a resistor 30, wiring 40, electrodes 50, and a cover layer 60. Note that in FIG. 1, for convenience, only the outer edge of the cover layer 60 is shown by a dashed line.
[0011] In this embodiment, for convenience, in the strain gauge 1, the side of the substrate 10 on which the resistor 30 is provided is referred to as the upper side or one side, and the side on which the resistor 30 is not provided is referred to as the lower side or the other side. Also, the surface on which the resistor 30 is provided in each portion is referred to as the one side or upper surface, and the surface on which the resistor 30 is not provided is referred to as the other side or lower surface. However, the strain gauge 1 can be used upside down or placed at any angle. Also, the planar view refers to the object being viewed from the normal direction of the upper surface 10a of the substrate 10, and the planar shape refers to the shape of the object viewed from the normal direction of the upper surface 10a of the substrate 10.
[0012] The substrate 10 is a flexible member that serves as a base layer for forming the resistor 30 and the like. The thickness of the substrate 10 is not particularly limited and can be appropriately selected depending on the purpose, and can be, for example, about 5 μm to 500 μm. In particular, a thickness of 5 μm to 200 μm is preferable in terms of the transferability of strain from the surface of the strain generator bonded to the lower surface of the substrate 10 via an adhesive layer or the like and dimensional stability against the environment, and a thickness of 10 μm or more is even more preferable in terms of insulation.
[0013] The substrate 10 can be formed from an insulating resin film such as PI (polyimide) resin, epoxy resin, PEEK (polyether ether ketone) resin, PEN (polyethylene naphthalate) resin, PET (polyethylene terephthalate) resin, PPS (polyphenylene sulfide) resin, LCP (liquid crystal polymer) resin, polyolefin resin, etc. The film refers to a flexible member having a thickness of about 500 μm or less.
[0014] Here, "formed from an insulating resin film" does not prevent the base material 10 from containing fillers, impurities, etc. in the insulating resin film. The base material 10 may be formed from an insulating resin film containing fillers such as silica or alumina.
[0015] Examples of materials other than resin for the substrate 10 include crystalline materials such as SiO2, ZrO2 (including YSZ), Si, Si2N3, Al2O3 (including sapphire), ZnO, perovskite ceramics (CaTiO3, BaTiO3), and amorphous glass. Metals such as aluminum, aluminum alloys (duralumin), and titanium may also be used as the material for the substrate 10. In this case, for example, an insulating film is formed on the metal substrate 10.
[0016] The resistor 30 is a thin film formed in a predetermined pattern on the substrate 10, and is a sensing part that generates a resistance change when strained. The resistor 30 may be formed directly on the upper surface 10a of the substrate 10, or may be formed on the upper surface 10a of the substrate 10 via another layer. For convenience, the resistor 30 is shown in FIG. 1 with a dark matte pattern.
[0017] The resistor 30 has a structure in which multiple elongated parts are arranged at regular intervals with their longitudinal direction in the same direction (the direction of line AA in FIG. 1), and the ends of adjacent elongated parts are alternately connected, folding back in a zigzag pattern as a whole. The longitudinal direction of the multiple elongated parts is the grid direction, and the direction perpendicular to the grid direction is the grid width direction (the direction of line BB in FIG. 1).
[0018] One end in the longitudinal direction of the two elongated portions located at the outermost sides in the grid width direction is bent in the grid width direction to form terminal ends 30e1 and 30e2 in the grid width direction of the resistor 30. The terminal ends 30e1 and 30e2 in the grid width direction of the resistor 30 are electrically connected to the electrodes 50 via the wiring 40. In other words, the wiring 40 electrically connects the terminal ends 30e1 and 30e2 in the grid width direction of the resistor 30 to the electrodes 50.
[0019] The resistor 30 can be made of, for example, a material containing Cr (chromium), a material containing Ni (nickel), or a material containing both Cr and Ni. That is, the resistor 30 can be made of a material containing at least one of Cr and Ni. An example of a material containing Cr is a Cr mixed phase film. An example of a material containing Ni is Cu-Ni (copper nickel). An example of a material containing both Cr and Ni is Ni-Cr (nickel chromium).
[0020] Here, the Cr mixed phase film is a film in which Cr, CrN, Cr2N, etc. are mixed. The Cr mixed phase film may contain inevitable impurities such as chromium oxide.
[0021] The thickness of the resistor 30 is not particularly limited and can be appropriately selected depending on the purpose, and can be, for example, about 0.05 μm to 2 μm. In particular, it is preferable that the thickness of the resistor 30 is 0.1 μm or more in order to improve the crystallinity of the crystals constituting the resistor 30 (for example, the crystallinity of α-Cr). It is further preferable that the thickness of the resistor 30 is 1 μm or less in order to reduce cracks in the film and warping from the substrate 10 caused by the internal stress of the film constituting the resistor 30. The width of the resistor 30 can be optimized for the required specifications such as resistance value and lateral sensitivity, and can be, for example, about 10 μm to 100 μm in consideration of measures against disconnection.
[0022] For example, when the resistor 30 is a Cr mixed phase film, the stability of the gauge characteristics can be improved by making α-Cr (alpha chromium) which is a stable crystal phase the main component. Furthermore, by making the resistor 30 mainly of α-Cr, the gauge factor of the strain gauge 1 can be 10 or more, and the gauge factor temperature coefficient TCS and the resistance temperature coefficient TCR can be in the range of -1000 ppm / °C to +1000 ppm / °C. Here, the main component means that the target substance accounts for 50% by weight or more of the total substance constituting the resistor, but from the viewpoint of improving the gauge characteristics, the resistor 30 preferably contains 80% by weight or more of α-Cr, and more preferably contains 90% by weight or more of α-Cr. Note that α-Cr is Cr with a bcc structure (body-centered cubic lattice structure).
[0023] When the resistor 30 is a Cr mixed-phase film, the Cr mixed-phase film preferably contains 20% by weight or less of CrN and Cr2N. By containing 20% by weight or less of CrN and Cr2N in the Cr mixed-phase film, a decrease in the gauge factor can be suppressed.
[0024] In addition, the ratio of Cr2N in CrN and Cr2N is preferably 80% by weight or more and less than 90% by weight, and more preferably 90% by weight or more and less than 95% by weight. When the ratio of Cr2N in CrN and Cr2N is 90% by weight or more and less than 95% by weight, the decrease in TCR (negative TCR) becomes more significant due to the Cr2N having semiconductor properties. Furthermore, by reducing the formation of ceramics, brittle fracture is reduced.
[0025] On the other hand, if a small amount of N2 or atomic N is mixed into the film, it will escape from the film due to the external environment (for example, a high temperature environment), causing a change in the film stress.By creating chemically stable CrN, it is possible to obtain a stable strain gauge without generating the unstable N mentioned above.
[0026] The wiring 40 is formed on the substrate 10 and is electrically connected to the resistor 30 and the electrodes 50. The wiring 40 has a first metal layer 41 and a second metal layer 42 laminated on the upper surface of the first metal layer 41. The wiring 40 is not limited to a straight line and can have any pattern. The wiring 40 can have any width and any length. For convenience, the wiring 40 and the electrodes 50 are shown in FIG. 1 with a matte finish that is thinner than the resistor 30.
[0027] The electrodes 50 are formed on the substrate 10 and are electrically connected to the resistor 30 via the wiring 40, and are formed, for example, in a substantially rectangular shape wider than the wiring 40. The electrodes 50 are a pair of electrodes for outputting to the outside a change in the resistance value of the resistor 30 caused by strain, and for example, a lead wire for external connection is joined to the electrodes 50.
[0028] The electrode 50 has a pair of first metal layers 51 and a second metal layer 52 laminated on the upper surface of each of the first metal layers 51. The first metal layers 51 are electrically connected to the ends 30e1 and 30e2 of the resistor 30 via the first metal layers 41 of the wiring 40. The first metal layers 51 are formed in a substantially rectangular shape in a plan view. The first metal layers 51 may be formed to have the same width as the wiring 40.
[0029] Although the resistor 30, the first metal layer 41, and the first metal layer 51 are given different reference numbers for convenience, they can be integrally formed from the same material in the same process. Therefore, the resistor 30, the first metal layer 41, and the first metal layer 51 have approximately the same thickness. Moreover, although the second metal layer 42 and the second metal layer 52 are given different reference numbers for convenience, they can be integrally formed from the same material in the same process. Therefore, the second metal layer 42 and the second metal layer 52 have approximately the same thickness.
[0030] The second metal layers 42 and 52 are formed of a material having a lower resistance than the resistor 30 (the first metal layers 41 and 51). The material of the second metal layers 42 and 52 is not particularly limited as long as it is a material having a lower resistance than the resistor 30, and can be appropriately selected according to the purpose. For example, when the resistor 30 is a Cr mixed phase film, the material of the second metal layers 42 and 52 can be Cu, Ni, Al, Ag, Au, Pt, etc., or an alloy of any of these metals, a compound of any of these metals, or a laminated film in which any of these metals, alloys, and compounds are appropriately laminated. The thickness of the second metal layers 42 and 52 is not particularly limited and can be appropriately selected according to the purpose, and can be, for example, about 3 μm to 5 μm.
[0031] The second metal layers 42 and 52 may be formed on a part of the upper surface of the first metal layers 41 and 51, or may be formed on the entire upper surface of the first metal layers 41 and 51. One or more other metal layers may be laminated on the upper surface of the second metal layer 52. For example, the second metal layer 52 may be a copper layer, and a gold layer may be laminated on the upper surface of the copper layer. Alternatively, the second metal layer 52 may be a copper layer, and a palladium layer and a gold layer may be sequentially laminated on the upper surface of the copper layer. By forming the top layer of the electrode 50 as a gold layer, the solder wettability of the electrode 50 can be improved.
[0032] In this way, the wiring 40 has a structure in which the second metal layer 42 is laminated on the first metal layer 41 made of the same material as the resistor 30. Therefore, the resistance of the wiring 40 is lower than that of the resistor 30, and it is possible to prevent the wiring 40 from functioning as a resistor. As a result, it is possible to improve the accuracy of strain detection by the resistor 30.
[0033] In other words, by providing the wiring 40 having a lower resistance than the resistor 30, the actual sensing portion of the strain gauge 1 can be limited to the local region where the resistor 30 is formed. Therefore, the accuracy of strain detection by the resistor 30 can be improved.
[0034] In particular, in a highly sensitive strain gauge with a gauge factor of 10 or more that uses a Cr mixed phase film as the resistor 30, making the wiring 40 lower in resistance than the resistor 30 and limiting the actual sensing part to the local region where the resistor 30 is formed has a significant effect on improving the strain detection accuracy. Making the wiring 40 lower in resistance than the resistor 30 also has the effect of reducing the lateral sensitivity.
[0035] The cover layer 60 (insulating resin layer) is formed on the base material 10, covers the resistor 30 and the wiring 40, and exposes the electrodes 50. A part of the wiring 40 may be exposed from the cover layer 60. By providing the cover layer 60 that covers the resistor 30 and the wiring 40, it is possible to prevent mechanical damage, etc. from occurring to the resistor 30 and the wiring 40. Furthermore, by providing the cover layer 60, it is possible to protect the resistor 30 and the wiring 40 from moisture, etc. The cover layer 60 may be provided so as to cover the entire portion except for the electrodes 50.
[0036] The cover layer 60 can be formed from an insulating resin such as PI resin, epoxy resin, PEEK resin, PEN resin, PET resin, PPS resin, or composite resin (e.g., silicone resin, polyolefin resin). The cover layer 60 may contain a filler or a pigment. There is no particular limit to the thickness of the cover layer 60 and it can be appropriately selected depending on the purpose, but it can be, for example, about 2 μm to 30 μm.
[0037] The cover layer 60 has a plurality of recesses 60x recessed from the top surface toward the substrate 10. Therefore, the roughness of the top surface of the cover layer 60 is greater than the roughness of the side surfaces of the cover layer 60. By providing the recesses 60x that open into the top surface of the cover layer 60, the area of the top surface of the cover layer 60, including the surface area of the recesses 60x, can be increased. This allows the top surface of the cover layer 60 to exhibit high water repellency and prevent moisture penetration.
[0038] As mentioned above, when a conventional strain gauge is used in a high-temperature and high-humidity environment, water droplets may adhere to the top surface of the cover layer and evaporate, collecting and concentrating dirt on the top surface of the cover layer. When the dirt is concentrated, base points that are inclined to acid or alkali are generated, deteriorating the cover layer, and as a result, the penetration of moisture causes corrosion of the wiring covered by the cover layer.
[0039] In the present application, the cover layer 60 having the multiple recesses 60x exhibits high water repellency and prevents the penetration of moisture, thereby suppressing corrosion of the wiring 40 covered by the cover layer 60. In particular, when the second metal layer 42 of the wiring 40 contains copper, copper is easily corroded, so it is effective to provide the recesses 60x on the upper surface of the cover layer 60 to prevent the penetration of moisture.
[0040] In order for the upper surface of the cover layer 60 to exhibit high water repellency, it is necessary to make the area of the upper surface of the cover layer 60 as large as possible, so it is preferable to provide a large number of fine recesses 60x on the upper surface of the cover layer 60. If the area of the upper surface of the cover layer 60 when the recesses 60x are not formed is 1, the area of the upper surface of the cover layer 60 including the surface area of the recesses 60x when the recesses 60x are formed is preferably 1.36 or more, and more preferably 2.00 or more. With such a surface area, the upper surface of the cover layer 60 exhibits high water repellency and can sufficiently suppress the penetration of moisture from the upper surface of the cover layer 60.
[0041] For example, if the recesses 60x are cubes with a width of 10 μm and a pitch of 20 μm (aspect ratio 1:2), and the area of the top surface of the cover layer 60 when the recesses 60x are not formed is set to 1, the area of the top surface of the cover layer 60 including the surface area of the recesses 60x when the recesses 60x are formed is 1.36. Also, if the recesses 60x are cubes with a width of 10 μm and a pitch of 10 μm (aspect ratio 1:1), and the area of the top surface of the cover layer 60 when the recesses 60x are not formed is set to 1, the area of the top surface of the cover layer 60 including the surface area of the recesses 60x when the recesses 60x are formed is 2.00.
[0042] The recesses 60x may have any shape, such as a cylindrical shape, an elliptical cylindrical shape, or a rectangular prism shape, but from the viewpoint of increasing the surface area, a rectangular prism shape is preferable. That is, the recesses 60x preferably have one bottom surface and four inner side surfaces connected to the bottom surface. When the recesses 60x have a rectangular prism shape, the recesses 60x may have, for example, a length of about 5 to 15 μm, a width of about 5 to 15 μm, and a depth of about 5 to 15 μm. The interval between adjacent recesses 60x may be, for example, about 5 to 15 μm.
[0043] The number density of the recesses 60x on the upper surface of the cover layer 60 is 900 pieces / mm 2 More preferably, it is 2500 pieces / mm 2 With such a number density, the upper surface of the cover layer 60 exhibits high water repellency, and the penetration of moisture from the upper surface of the cover layer 60 can be sufficiently suppressed.
[0044] For example, if the recesses 60x are cubes with a width of 10 μm and a pitch of 20 μm (aspect ratio 1:2), the number density of the recesses 60x on the upper surface of the cover layer 60 is 900 pieces / mm 2 In addition, if the recesses 60x are cubes with a width of 10 μm and a pitch of 10 μm (aspect ratio 1:1), the number density of the recesses 60x on the upper surface of the cover layer 60 is 2500 pieces / mm 2 It becomes.
[0045] When viewed from the normal direction of the upper surface of the cover layer 60, the recesses 60x are regularly arranged in a predetermined pattern on the upper surface of the cover layer 60. Here, "regularly arranged" refers to an arrangement that is intentionally arranged so that the same pattern appears repeatedly. In this embodiment, the recesses 60x are arranged in a matrix, but this is not limited thereto, and they may be arranged, for example, in a staggered pattern, or in any other arbitrary arrangement as long as it is regular.
[0046] By regularly arranging the recesses 60x, almost uniform water repellency can be obtained over the entire upper surface of the cover layer 60. The upper surface of the cover layer 60 preferably has a contact angle with water of 90 degrees or more, and more preferably 120 degrees or more. With such a contact angle, the upper surface of the cover layer 60 exhibits high water repellency and can sufficiently suppress the penetration of water from the upper surface of the cover layer 60.
[0047] To manufacture the strain gauge 1, first, a base material 10 is prepared, and a metal layer (for convenience, referred to as metal layer A) is formed on an upper surface 10a of the base material 10. Metal layer A is a layer that is finally patterned to become resistor 30, first metal layer 41, and first metal layer 51. Therefore, the material and thickness of metal layer A are similar to the material and thickness of resistor 30, first metal layer 41, and first metal layer 51 described above.
[0048] The metal layer A can be formed by, for example, a magnetron sputtering method using a target made of a raw material capable of forming the metal layer A. The metal layer A may be formed by a reactive sputtering method, a vapor deposition method, an arc ion plating method, a pulsed laser deposition method, or the like instead of the magnetron sputtering method.
[0049] From the viewpoint of stabilizing the gauge characteristics, it is preferable to vacuum-deposit a functional layer of a predetermined thickness as a base layer on the upper surface 10a of the base material 10 by, for example, conventional sputtering, before depositing the metal layer A.
[0050] In the present application, the functional layer refers to a layer having a function of promoting the crystal growth of at least the upper layer, the metal layer A (resistor 30). The functional layer preferably further has a function of preventing oxidation of the metal layer A due to oxygen and moisture contained in the base material 10, and a function of improving adhesion between the base material 10 and the metal layer A. The functional layer may further have other functions.
[0051] Since the insulating resin film that constitutes the substrate 10 contains oxygen and moisture, it is effective for the functional layer to have the function of preventing oxidation of the metal layer A, particularly when the metal layer A contains Cr, since Cr forms a self-oxidized film.
[0052] The material of the functional layer is not particularly limited as long as it has the function of promoting the crystal growth of at least the upper layer, the metal layer A (resistor 30), and can be appropriately selected depending on the purpose. For example, Cr (chromium), Ti (titanium), V (vanadium), Nb (niobium), Ta (tantalum), Ni (nickel), Y (yttrium), Zr (zirconium), Hf (hafnium), Si (silicon), C (carbon), Zn (zinc), Cu (copper), Bi (bismuth), and the like can be used. Examples of the metal include one or more metals selected from the group consisting of ruthenium (Ru), Fe (iron), Mo (molybdenum), W (tungsten), Ru (ruthenium), Rh (rhodium), Re (rhenium), Os (osmium), Ir (iridium), Pt (platinum), Pd (palladium), Ag (silver), Au (gold), Co (cobalt), Mn (manganese), and Al (aluminum), an alloy of any of the metals in this group, or a compound of any of the metals in this group.
[0053] Examples of the alloy include FeCr, TiAl, FeNi, NiCr, CrCu, etc. Examples of the compound include TiN, TaN, Si3N4, TiO2, Ta2O5, SiO2, etc.
[0054] When the functional layer is made of a conductive material such as a metal or alloy, the thickness of the functional layer is preferably 1 / 20 or less of the thickness of the resistor. In this range, the crystal growth of α-Cr can be promoted, and a part of the current flowing through the resistor can be prevented from flowing through the functional layer, which reduces the detection sensitivity of strain.
[0055] When the functional layer is made of a conductive material such as a metal or alloy, the thickness of the functional layer is preferably 1 / 50 or less of the thickness of the resistor. In this range, the crystal growth of α-Cr can be promoted, and the strain detection sensitivity can be further prevented from being reduced due to a part of the current flowing through the resistor flowing through the functional layer.
[0056] When the functional layer is made of a conductive material such as a metal or alloy, the thickness of the functional layer is more preferably 1 / 100 or less of the thickness of the resistor, which can further prevent a part of the current flowing through the resistor from flowing through the functional layer, thereby preventing a decrease in the strain detection sensitivity.
[0057] When the functional layer is made of an insulating material such as an oxide or nitride, the thickness of the functional layer is preferably 1 nm to 1 μm, which can promote the crystal growth of α-Cr and can be easily formed without cracking the functional layer.
[0058] When the functional layer is made of an insulating material such as an oxide or nitride, the thickness of the functional layer is preferably 1 nm to 0.8 μm, which can promote the crystal growth of α-Cr and can be easily formed without cracking the functional layer.
[0059] When the functional layer is made of an insulating material such as an oxide or nitride, the thickness of the functional layer is more preferably 1 nm to 0.5 μm, which can promote the crystal growth of α-Cr and can be more easily formed without cracking the functional layer.
[0060] The planar shape of the functional layer is patterned to be substantially the same as the planar shape of the resistor shown in FIG. 1, for example. However, the planar shape of the functional layer is not limited to being substantially the same as the planar shape of the resistor. When the functional layer is made of an insulating material, it does not have to be patterned to be the same as the planar shape of the resistor. In this case, the functional layer may be formed in a solid shape at least in the region where the resistor is formed. Alternatively, the functional layer may be formed in a solid shape on the entire upper surface of the substrate 10.
[0061] Furthermore, when the functional layer is made of an insulating material, the functional layer is formed relatively thick, at a thickness of 50 nm to 1 μm, and formed in a solid form, so that the thickness and surface area of the functional layer are increased, and the heat generated by the resistor can be dissipated to the substrate 10. As a result, the deterioration of the measurement accuracy of the strain gauge 1 due to self-heating of the resistor can be suppressed.
[0062] The functional layer can be formed in vacuum by conventional sputtering, for example, using a raw material capable of forming the functional layer as a target and introducing Ar (argon) gas into a chamber. By using conventional sputtering, the functional layer is formed while etching the upper surface 10a of the substrate 10 with Ar, so that the amount of the functional layer formed can be minimized and the effect of improving adhesion can be obtained.
[0063] However, this is just one example of a method for forming the functional layer, and the functional layer may be formed by other methods. For example, a method may be used in which the upper surface 10a of the substrate 10 is activated by a plasma treatment using Ar or the like before forming the functional layer, thereby improving adhesion, and then the functional layer is vacuum-formed by magnetron sputtering.
[0064] There are no particular restrictions on the combination of the material of the functional layer and the material of the metal layer A and can be selected appropriately depending on the purpose. For example, it is possible to use Ti for the functional layer and form a Cr mixed phase film with α-Cr (alpha chromium) as the main component for the metal layer A.
[0065] In this case, for example, the metal layer A can be formed by magnetron sputtering using a raw material capable of forming a Cr mixed phase film as a target and introducing Ar gas into a chamber. Alternatively, the metal layer A can be formed by reactive sputtering using pure Cr as a target and introducing an appropriate amount of nitrogen gas together with Ar gas into a chamber. In this case, the ratio of CrN and Cr2N contained in the Cr mixed phase film, and the ratio of Cr2N in CrN and Cr2N can be adjusted by changing the amount and pressure of the nitrogen gas introduced (nitrogen partial pressure) or by adjusting the heating temperature by providing a heating process.
[0066] In these methods, the growth surface of the Cr mixed-phase film is determined by the functional layer made of Ti, and a Cr mixed-phase film containing α-Cr, which has a stable crystal structure, as a main component, can be formed. Furthermore, the Ti constituting the functional layer is diffused into the Cr mixed-phase film, thereby improving the gauge characteristics. For example, the gauge factor of the strain gauge 1 can be set to 10 or more, and the gauge factor temperature coefficient TCS and the resistance temperature coefficient TCR can be set within the range of -1000 ppm / °C to +1000 ppm / °C. When the functional layer is made of Ti, the Cr mixed-phase film may contain Ti and TiN (titanium nitride).
[0067] When the metal layer A is a Cr mixed phase film, the functional layer made of Ti has all of the following functions: promoting the crystal growth of the metal layer A, preventing oxidation of the metal layer A due to oxygen and moisture contained in the base material 10, and improving the adhesion between the base material 10 and the metal layer A. The same applies when Ta, Si, Al, or Fe is used as the functional layer instead of Ti.
[0068] In this way, by providing a functional layer below the metal layer A, it is possible to promote crystal growth in the metal layer A, and to produce a metal layer A consisting of a stable crystal phase. As a result, it is possible to improve the stability of the gauge characteristics of the strain gauge 1. In addition, the material constituting the functional layer diffuses into the metal layer A, thereby improving the gauge characteristics of the strain gauge 1.
[0069] Next, the second metal layer 42 and the second metal layer 52 are formed on the upper surface of the metal layer A. The second metal layer 42 and the second metal layer 52 can be formed by, for example, a photolithography method.
[0070] Specifically, first, a seed layer is formed by, for example, sputtering or electroless plating so as to cover the upper surface of the metal layer A. Next, a photosensitive resist is formed on the entire upper surface of the seed layer, and is exposed and developed to form openings that expose the regions in which the second metal layer 42 and the second metal layer 52 are to be formed. At this time, the pattern of the second metal layer 42 can be formed into any shape by adjusting the shape of the openings in the resist. For example, a dry film resist can be used as the resist.
[0071] Next, for example, the second metal layer 42 and the second metal layer 52 are formed on the seed layer exposed in the opening by electrolytic plating using the seed layer as a power supply path. The electrolytic plating method is preferable in that it has high tact and can form low-stress electrolytic plating layers as the second metal layer 42 and the second metal layer 52. By making the electrolytic plating layer thick and low-stress, it is possible to prevent warping of the strain gauge 1. The second metal layer 42 and the second metal layer 52 may be formed by electroless plating.
[0072] Next, the resist is removed. For example, the resist can be removed by immersing the resist in a solution that can dissolve the resist material.
[0073] Next, a photosensitive resist is formed on the entire upper surface of the seed layer, and is exposed and developed to be patterned into a planar shape similar to that of the resistor 30, the wiring 40, and the electrode 50 in Fig. 1. For example, a dry film resist can be used as the resist. Then, the resist is used as an etching mask to remove the metal layer A and the seed layer exposed from the resist, thereby forming the resistor 30, the wiring 40, and the electrode 50 in the planar shape of Fig. 1.
[0074] For example, unnecessary portions of the metal layer A and the seed layer can be removed by wet etching. If a functional layer is formed below the metal layer A, the functional layer is patterned by etching into the planar shape shown in Fig. 1, similar to the resistor 30, the wiring 40, and the electrode 50. At this point, a seed layer is formed on the resistor 30, the first metal layer 41, and the first metal layer 51.
[0075] Next, the second metal layer 42 and the second metal layer 52 are used as an etching mask to remove unnecessary seed layer exposed from the second metal layer 42 and the second metal layer 52, thereby forming the second metal layer 42 and the second metal layer 52. Note that the seed layer directly below the second metal layer 42 and the second metal layer 52 remains. For example, the unnecessary seed layer can be removed by wet etching using an etching solution that etches the seed layer but does not etch the functional layer, the resistor 30, the wiring 40, and the electrodes 50.
[0076] Thereafter, a cover layer 60 is provided on the upper surface 10a of the substrate 10 to cover the resistor 30 and the wiring 40 and expose the electrodes 50. Specifically, a semi-cured thermosetting insulating resin film is first prepared with a plurality of recesses 60x formed on the upper surface by a mold or the like. Then, for example, the semi-cured thermosetting insulating resin film is laminated on the upper surface 10a of the substrate 10 so as to cover the resistor 30 and the wiring 40 and expose the electrodes 50. The semi-cured thermosetting insulating resin film is then heated and pressurized to be cured, thereby forming the cover layer 60. The lamination is preferably performed in a vacuum atmosphere. The strain gauge 1 is completed by the above steps.
[0077] Alternatively, a method may be considered in which a thermosetting insulating resin film without the recesses 60x formed on the upper surface is prepared, and laminated on the upper surface 10a of the substrate 10 so as to cover the resistor 30 and the wiring 40 and expose the electrodes 50, and then the recesses 60x are formed using a mold or the like. However, in this case, stress may be applied to the resistor 30 and the like when the recesses 60x are formed using a mold or the like, which may result in disconnection or the like. For this reason, a method is preferred in which a semi-cured thermosetting insulating resin film with a plurality of recesses 60x formed on the upper surface in advance is laminated on the substrate 10.
[0078] When a functional layer is provided on the upper surface 10a of the substrate 10 as an underlayer for the resistor 30, the first metal layer 41, and the first metal layer 51, the strain gauge 1 has a cross-sectional shape as shown in Fig. 5. The layer indicated by reference numeral 20 is the functional layer. When the functional layer 20 is provided, the planar shape of the strain gauge 1 is, for example, the same as that shown in Fig. 1. However, as described above, the functional layer 20 may be formed solidly on a part or all of the upper surface of the substrate 10.
[0079] Although preferred embodiments have been described above in detail, the present invention is not limited to the above-described embodiments, and various modifications and substitutions can be made to the above-described embodiments without departing from the scope of the claims.
[0080] For example, the present invention is also applicable to a strain gauge having a plurality of resistors formed on a substrate. For example, the present invention is also applicable to a strain gauge having two resistors formed on a substrate that form a half-bridge circuit. Alternatively, the present invention is also applicable to a strain gauge having four resistors formed on a substrate that form a full-bridge circuit. [Explanation of symbols]
[0081] 1 strain gauge, 10 substrate, 10a upper surface, 20 functional layer, 30 resistor, 30e1, 30e2 termination, 40 wiring, 50 electrode, 41, 51 first metal layer, 42, 52 second metal layer, 60 cover layer, 60x recess
Claims
1. A flexible substrate; A resistor formed on the substrate; A wiring formed on the base material and electrically connected to the resistor; an insulating resin layer formed on the base material and covering the resistor and the wiring; the insulating resin layer has a plurality of recesses recessed from an upper surface toward the base material, The recess has a bottom surface and four inner sides connected to the bottom surface.
2. The strain gauge according to claim 1 , wherein the recesses are regularly arranged on the upper surface of the insulating resin layer when viewed from a normal direction of the upper surface of the insulating resin layer.
3. The strain gauge according to claim 1 or 2, wherein a roughness of the upper surface of the insulating resin layer is greater than a roughness of a side surface of the insulating resin layer.
4. 4. The strain gauge according to claim 1, wherein, when an area of the upper surface of the insulating resin layer when the recess is not formed is taken as 1, an area of the upper surface of the insulating resin layer including a surface area of the recess when the recess is formed is 1.36 or more.
5. 5. The strain gauge according to claim 1, wherein the upper surface of the insulating resin layer has a contact angle with water of 90 degrees or more.
6. 6. The strain gauge according to claim 1, wherein the wiring includes a first metal layer formed of the same material as the resistor, and a second metal layer formed on an upper surface of the first metal layer.
7. The strain gauge of claim 6 , wherein the second metal layer comprises copper.
8. The resistor is made of Cr, CrN, and Cr. 2 8. The strain gauge according to claim 1, which is formed from a film containing N.
9. 9. The strain gauge according to claim 8, having a gauge factor of 10 or more.
10. The CrN and Cr contained in the resistor 2 10. The strain gauge according to claim 8, wherein N is 20% by weight or less.
11. The CrN and the Cr 2 The Cr in N 2 11. The strain gauge according to claim 10, wherein the proportion of N is 80% by weight or more and less than 90% by weight.
Citation Information
Patent Citations
Deformation quantity measuring apparatus, adjusting method and judging method
JP2007266079A
Strain sensor
JP2014038088A
Alloy for strain gauge and strain gauge
JP2016074934A
Strain gauge
JP2019090723A
Strain gauge
JP2019100883A