Strain gauges

The strain gauge with recessed resistors on a flexible base material enhances adhesion with the insulating resin layer, addressing the peeling issue and ensuring accurate strain detection.

JP7577908B2Active Publication Date: 2024-11-06MINEBEAMITSUMI INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2020185686
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-11-06
Publication Date
2024-11-06
Estimated Expiration
2040-11-06

AI Technical Summary

Technical Problem

The adhesion between the resistor and the insulating resin layer in strain gauges becomes weak when the resistor width becomes narrow, leading to a risk of peeling at their interface.

Method used

The strain gauge design includes a flexible base material with a resistor featuring recesses on its surface, increasing the contact area with an insulating resin layer to enhance adhesion.

Benefits of technology

This design improves the adhesion between the resistor and the insulating resin layer, preventing peeling and ensuring accurate strain detection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007577908000001
    Figure 0007577908000001
  • Figure 0007577908000002
    Figure 0007577908000002
  • Figure 0007577908000003
    Figure 0007577908000003
Patent Text Reader

Abstract

To provide a strain gauge that can increase the adhesion between a resistor and an insulating resin layer.SOLUTION: The strain gauge includes: a flexible base material; a resistor formed on the base material; and an insulating resin layer formed on the base material and covering the resistor. The resistor has a plurality of recessed parts recessed in the direction of the base material.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a strain gauge. [Background technology]

[0002] There is known a strain gauge that is attached to a measurement object to detect the strain of the measurement object. The strain gauge includes a resistor that detects the strain, and the resistor is formed on, for example, a base material. The strain gauge also includes, on the base material, an insulating resin layer that covers the resistor (for example, see Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2016-74934 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, when the width of the resistor is narrowed, it becomes difficult to ensure a sufficient contact area between the resistor and the insulating resin layer, which may cause peeling at the interface between the resistor and the insulating resin layer.

[0005] The present invention has been made in view of the above-mentioned points, and an object of the present invention is to provide a strain gauge capable of improving the adhesive strength between a resistor and an insulating resin layer. [Means for solving the problem]

[0006] This strain gauge has a flexible substrate, a resistor formed on the substrate, and an insulating resin layer formed on the substrate and covering the resistor, and the resistor has a plurality of recesses recessed from an upper surface toward the substrate. The recess has one bottom surface and four inner side surfaces connected to the bottom surface. is. Effect of the Invention

[0007] According to the disclosed technique, it is possible to provide a strain gauge capable of improving the adhesive strength between a resistor and an insulating resin layer. [Brief description of the drawings]

[0008] [Figure 1] FIG. 2 is a plan view illustrating the strain gauge according to the first embodiment. [Diagram 2] 1 is a cross-sectional view (part 1) illustrating a strain gauge according to a first embodiment. FIG. [Diagram 3] 4 is a cross-sectional view (part 2) illustrating the strain gauge according to the first embodiment. FIG. [Figure 4] 2 is a partial perspective view illustrating a resistor of the strain gauge according to the first embodiment. FIG. [Diagram 5] 4 is a cross-sectional view (part 3) illustrating the strain gauge according to the first embodiment. FIG. [Figure 6] 4 is a partial cross-sectional view illustrating a strain gauge according to a first modified example of the first embodiment. FIG. [Figure 7] 4 is a partial plan view illustrating an example of the positional relationship between a recess in a substrate and a recess in a resistor. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the drawings, the same components are designated by the same reference numerals, and duplicated explanations may be omitted.

[0010] First embodiment FIG. 1 is a plan view illustrating the strain gauge according to the first embodiment. FIG. 2 is a cross-sectional view illustrating the strain gauge according to the first embodiment, showing a cross section along the line AA in FIG. 1. FIG. 3 is a cross-sectional view illustrating the strain gauge according to the first embodiment, showing a cross section along the line BB in FIG. 1. FIG. 4 is a partial perspective view illustrating a resistor of the strain gauge according to the first embodiment. With reference to FIGS. 1 to 4, the strain gauge 1 has a substrate 10, a resistor 30, wiring 40, electrodes 50, and a cover layer 60. Note that in FIG. 1, for convenience, only the outer edge of the cover layer 60 is shown by a dashed line.

[0011] In this embodiment, for convenience, in the strain gauge 1, the side of the substrate 10 on which the resistor 30 is provided is referred to as the upper side or one side, and the side on which the resistor 30 is not provided is referred to as the lower side or the other side. Also, the surface on which the resistor 30 is provided in each portion is referred to as the one side or upper surface, and the surface on which the resistor 30 is not provided is referred to as the other side or lower surface. However, the strain gauge 1 can be used upside down or placed at any angle. Also, the planar view refers to the object being viewed from the normal direction of the upper surface 10a of the substrate 10, and the planar shape refers to the shape of the object viewed from the normal direction of the upper surface 10a of the substrate 10.

[0012] The substrate 10 is a flexible member that serves as a base layer for forming the resistor 30 and the like. The thickness of the substrate 10 is not particularly limited and can be appropriately selected depending on the purpose, and can be, for example, about 5 μm to 500 μm. In particular, a thickness of 5 μm to 200 μm is preferable in terms of the transferability of strain from the surface of the strain generator bonded to the lower surface of the substrate 10 via an adhesive layer or the like and dimensional stability against the environment, and a thickness of 10 μm or more is even more preferable in terms of insulation.

[0013] The substrate 10 can be formed from an insulating resin film such as PI (polyimide) resin, epoxy resin, PEEK (polyether ether ketone) resin, PEN (polyethylene naphthalate) resin, PET (polyethylene terephthalate) resin, PPS (polyphenylene sulfide) resin, LCP (liquid crystal polymer) resin, polyolefin resin, etc. The film refers to a flexible member having a thickness of about 500 μm or less.

[0014] Here, "formed from an insulating resin film" does not prevent the base material 10 from containing fillers, impurities, etc. in the insulating resin film. The base material 10 may be formed from an insulating resin film containing fillers such as silica or alumina.

[0015] Examples of materials other than resin for the substrate 10 include crystalline materials such as SiO2, ZrO2 (including YSZ), Si, Si2N3, Al2O3 (including sapphire), ZnO, perovskite ceramics (CaTiO3, BaTiO3), and amorphous glass. Metals such as aluminum, aluminum alloys (duralumin), and titanium may also be used as the material for the substrate 10. In this case, for example, an insulating film is formed on the metal substrate 10.

[0016] The resistor 30 is a thin film formed in a predetermined pattern on the substrate 10, and is a sensing part that generates a resistance change when strained. The resistor 30 may be formed directly on the upper surface 10a of the substrate 10, or may be formed on the upper surface 10a of the substrate 10 via another layer. For convenience, the resistor 30 is shown in FIG. 1 with a dark matte pattern.

[0017] The resistor 30 has a structure in which multiple elongated parts are arranged at regular intervals with their longitudinal direction in the same direction (the direction of line AA in FIG. 1), and the ends of adjacent elongated parts are alternately connected, folding back in a zigzag pattern as a whole. The longitudinal direction of the multiple elongated parts is the grid direction, and the direction perpendicular to the grid direction is the grid width direction (the direction perpendicular to line AA in FIG. 1).

[0018] One end in the longitudinal direction of the two elongated portions located at the outermost sides in the grid width direction is bent in the grid width direction to form terminal ends 30e1 and 30e2 in the grid width direction of the resistor 30. The terminal ends 30e1 and 30e2 in the grid width direction of the resistor 30 are electrically connected to the electrodes 50 via the wiring 40. In other words, the wiring 40 electrically connects the terminal ends 30e1 and 30e2 in the grid width direction of the resistor 30 to the electrodes 50.

[0019] The resistor 30 can be made of, for example, a material containing Cr (chromium), a material containing Ni (nickel), or a material containing both Cr and Ni. That is, the resistor 30 can be made of a material containing at least one of Cr and Ni. An example of a material containing Cr is a Cr mixed phase film. An example of a material containing Ni is Cu-Ni (copper nickel). An example of a material containing both Cr and Ni is Ni-Cr (nickel chromium).

[0020] Here, the Cr mixed phase film is a film in which Cr, CrN, Cr2N, etc. are mixed. The Cr mixed phase film may contain inevitable impurities such as chromium oxide.

[0021] The thickness of the resistor 30 is not particularly limited and can be appropriately selected depending on the purpose, and can be, for example, about 0.05 μm to 2 μm. In particular, it is preferable that the thickness of the resistor 30 is 0.1 μm or more in order to improve the crystallinity of the crystals constituting the resistor 30 (for example, the crystallinity of α-Cr). It is further preferable that the thickness of the resistor 30 is 1 μm or less in order to reduce cracks in the film and warping from the substrate 10 caused by the internal stress of the film constituting the resistor 30. The width of the resistor 30 can be optimized for the required specifications such as resistance value and lateral sensitivity, and can be, for example, about 5 μm to 100 μm in consideration of measures against disconnection.

[0022] For example, when the resistor 30 is a Cr mixed phase film, the stability of the gauge characteristics can be improved by making α-Cr (alpha chromium) which is a stable crystal phase the main component. Furthermore, by making the resistor 30 mainly of α-Cr, the gauge factor of the strain gauge 1 can be 10 or more, and the gauge factor temperature coefficient TCS and the resistance temperature coefficient TCR can be in the range of -1000 ppm / °C to +1000 ppm / °C. Here, the main component means that the target substance accounts for 50% by weight or more of the total substance constituting the resistor, but from the viewpoint of improving the gauge characteristics, the resistor 30 preferably contains 80% by weight or more of α-Cr, and more preferably contains 90% by weight or more of α-Cr. Note that α-Cr is Cr with a bcc structure (body-centered cubic lattice structure).

[0023] When the resistor 30 is a Cr mixed-phase film, the Cr mixed-phase film preferably contains 20% by weight or less of CrN and Cr2N. By containing 20% ​​by weight or less of CrN and Cr2N in the Cr mixed-phase film, a decrease in the gauge factor can be suppressed.

[0024] In addition, the ratio of Cr2N in CrN and Cr2N is preferably 80% by weight or more and less than 90% by weight, and more preferably 90% by weight or more and less than 95% by weight. When the ratio of Cr2N in CrN and Cr2N is 90% by weight or more and less than 95% by weight, the decrease in TCR (negative TCR) becomes more significant due to the Cr2N having semiconductor properties. Furthermore, by reducing the formation of ceramics, brittle fracture is reduced.

[0025] On the other hand, if a small amount of N2 or atomic N is mixed into the film, it will escape from the film due to the external environment (for example, a high temperature environment), causing a change in the film stress.By creating chemically stable CrN, it is possible to obtain a stable strain gauge without generating the unstable N mentioned above.

[0026] The wiring 40 is formed on the substrate 10 and is electrically connected to the resistor 30 and the electrodes 50. The wiring 40 has a first metal layer 41 and a second metal layer 42 laminated on the upper surface of the first metal layer 41. The wiring 40 is not limited to a straight line and can have any pattern. The wiring 40 can have any width and any length. For convenience, the wiring 40 and the electrodes 50 are shown in FIG. 1 with a matte finish that is thinner than the resistor 30.

[0027] The electrodes 50 are formed on the substrate 10 and are electrically connected to the resistor 30 via the wiring 40, and are formed, for example, in a substantially rectangular shape wider than the wiring 40. The electrodes 50 are a pair of electrodes for outputting to the outside a change in the resistance value of the resistor 30 caused by strain, and for example, a lead wire for external connection is joined to the electrodes 50.

[0028] The electrode 50 has a pair of first metal layers 51 and a second metal layer 52 laminated on the upper surface of each of the first metal layers 51. The first metal layers 51 are electrically connected to the ends 30e1 and 30e2 of the resistor 30 via the first metal layers 41 of the wiring 40. The first metal layers 51 are formed in a substantially rectangular shape in a plan view. The first metal layers 51 may be formed to have the same width as the wiring 40.

[0029] Although the resistor 30, the first metal layer 41, and the first metal layer 51 are given different reference numbers for convenience, they can be integrally formed from the same material in the same process. Therefore, the resistor 30, the first metal layer 41, and the first metal layer 51 have approximately the same thickness. Moreover, although the second metal layer 42 and the second metal layer 52 are given different reference numbers for convenience, they can be integrally formed from the same material in the same process. Therefore, the second metal layer 42 and the second metal layer 52 have approximately the same thickness.

[0030] The second metal layers 42 and 52 are formed of a material having a lower resistance than the resistor 30 (the first metal layers 41 and 51). The material of the second metal layers 42 and 52 is not particularly limited as long as it is a material having a lower resistance than the resistor 30, and can be appropriately selected according to the purpose. For example, when the resistor 30 is a Cr mixed phase film, the material of the second metal layers 42 and 52 can be Cu, Ni, Al, Ag, Au, Pt, etc., or an alloy of any of these metals, a compound of any of these metals, or a laminated film in which any of these metals, alloys, and compounds are appropriately laminated. The thickness of the second metal layers 42 and 52 is not particularly limited and can be appropriately selected according to the purpose, and can be, for example, about 3 μm to 5 μm.

[0031] The second metal layers 42 and 52 may be formed on a part of the upper surface of the first metal layers 41 and 51, or may be formed on the entire upper surface of the first metal layers 41 and 51. One or more other metal layers may be laminated on the upper surface of the second metal layer 52. For example, the second metal layer 52 may be a copper layer, and a gold layer may be laminated on the upper surface of the copper layer. Alternatively, the second metal layer 52 may be a copper layer, and a palladium layer and a gold layer may be sequentially laminated on the upper surface of the copper layer. By forming the top layer of the electrode 50 as a gold layer, the solder wettability of the electrode 50 can be improved.

[0032] In this way, the wiring 40 has a structure in which the second metal layer 42 is laminated on the first metal layer 41 made of the same material as the resistor 30. Therefore, the resistance of the wiring 40 is lower than that of the resistor 30, and it is possible to prevent the wiring 40 from functioning as a resistor. As a result, it is possible to improve the accuracy of strain detection by the resistor 30.

[0033] In other words, by providing the wiring 40 having a lower resistance than the resistor 30, the actual sensing portion of the strain gauge 1 can be limited to the local region where the resistor 30 is formed. Therefore, the accuracy of strain detection by the resistor 30 can be improved.

[0034] In particular, in a highly sensitive strain gauge with a gauge factor of 10 or more that uses a Cr mixed phase film as the resistor 30, making the wiring 40 lower in resistance than the resistor 30 and limiting the actual sensing part to the local region where the resistor 30 is formed has a significant effect on improving the strain detection accuracy. Making the wiring 40 lower in resistance than the resistor 30 also has the effect of reducing the lateral sensitivity.

[0035] However, depending on the required specifications, the wiring 40 and the electrodes 50 may be formed only from the first metal layers 41 and 51. In other words, the second metal layers 42 and 52 may be formed only when necessary.

[0036] The cover layer 60 (insulating resin layer) is formed on the base material 10, covers the resistor 30 and the wiring 40, and exposes the electrodes 50. A part of the wiring 40 may be exposed from the cover layer 60. By providing the cover layer 60 that covers the resistor 30 and the wiring 40, it is possible to prevent mechanical damage, etc. from occurring to the resistor 30 and the wiring 40. Furthermore, by providing the cover layer 60, it is possible to protect the resistor 30 and the wiring 40 from moisture, etc. The cover layer 60 may be provided so as to cover the entire portion except for the electrodes 50.

[0037] The cover layer 60 can be formed from an insulating resin such as PI resin, epoxy resin, PEEK resin, PEN resin, PET resin, PPS resin, or composite resin (e.g., silicone resin, polyolefin resin). The cover layer 60 may contain a filler or a pigment. There is no particular limit to the thickness of the cover layer 60 and it can be appropriately selected depending on the purpose, but it can be, for example, about 2 μm to 30 μm.

[0038] The resistor 30 has a plurality of recesses 30x recessed from the top surface toward the substrate 10. Therefore, the roughness of the top surface of the resistor 30 is greater than the roughness of the side surfaces of the resistor 30. By providing the recesses 30x that open to the top surface of the resistor 30, the area of ​​the top surface of the resistor 30, including the surface area of ​​the recesses 30x, can be increased. This increases the contact area between the resistor 30 and the cover layer 60, creating an anchor effect and improving the adhesion between the resistor 30 and the cover layer 60.

[0039] The recesses 30x are formed at least on the upper surface of the resistor 30, but may also be formed on the upper surfaces of the first metal layers 41 and 51. When the recesses 30x are formed on the upper surfaces of the first metal layers 41 and 51, the adhesion between the first metal layers 41 and 51 and the second metal layers 42 and 52, which are the upper layers, can be improved.

[0040] In conventional strain gauges, the resistor was relatively thick, so the adhesion between the resistor and the cover layer was rarely an issue. However, in recent years, resistors have become thinner, making it difficult to ensure the contact area between the resistor and the cover layer. In particular, when the resistor width is 20 μm or less, the adhesion between the resistor and the cover layer decreases, and there is a risk of the interface between the resistor and the cover layer peeling off. When the resistor width is 10 μm or less, the adhesion between the resistor and the cover layer decreases further, and there is a significant risk of the interface between the resistor and the cover layer peeling off.

[0041] In the strain gauge 1, the recess 30x is provided on the upper surface of the resistor 30 to improve the adhesion between the resistor 30 and the cover layer 60, thereby preventing the resistor 30 from peeling off from the cover layer 60. Providing the recess 30x on the upper surface of the resistor 30 is effective when the width of the resistor 30 is 20 μm or less, and is particularly effective when the width of the resistor 30 is 10 μm or less.

[0042] In order to improve the adhesion between the resistor 30 and the cover layer 60, it is necessary to make the area of ​​the upper surface of the resistor 30 as large as possible, and therefore it is preferable to provide a large number of fine recesses 30x on the upper surface of the resistor 30. If the area of ​​the upper surface of the resistor 30 without the recesses 30x is 1, the area of ​​the upper surface of the resistor 30 including the surface area of ​​the recesses 30x when the recesses 30x are formed is preferably 1.5 or more, and more preferably 2 or more. With such a surface area, the adhesion between the resistor 30 and the cover layer 60 can be sufficiently improved.

[0043] The recess 30x may have any shape, such as a cylindrical shape, an elliptical cylindrical shape, or a rectangular prism shape, but from the viewpoint of increasing the surface area, a rectangular prism shape is preferable. That is, the recess 30x preferably has one bottom surface and four inner side surfaces connected to the bottom surface. The width of the recess 30x is preferably 1 / 2 or less of the width of the resistor 30, and the depth of the resistor 30 is preferably 1 / 2 or less of the thickness of the resistor 30. In this way, disconnection of the resistor 30 can be prevented.

[0044] When viewed from the normal direction of the upper surface of the resistor 30, the recesses 30x are regularly arranged in a predetermined pattern on the upper surface of the resistor 30. Here, "regularly arranged" refers to an arrangement that is intentionally arranged so that the same pattern appears repeatedly. In this embodiment, the recesses 30x are arranged in a matrix, but this is not limited thereto, and they may be arranged, for example, in a staggered pattern, or in any other arbitrary arrangement as long as it is regular.

[0045] By regularly arranging the recesses 30x, a substantially uniform adhesion force is obtained between the resistor 30 and the cover layer 60 over the entire upper surface of the resistor 30. If the adhesion force varies depending on the location of the resistor 30, when the resistor 30 expands and contracts under strain, the resistor 30 expands and contracts differently depending on the location, and a correct strain output may not be obtained. In contrast, if the adhesion force between the resistor 30 and the cover layer 60 is substantially uniform over the entire upper surface of the resistor 30, a highly accurate strain output can be obtained.

[0046] To manufacture the strain gauge 1, first, a base material 10 is prepared, and a metal layer (for convenience, referred to as metal layer A) is formed on an upper surface 10a of the base material 10. Metal layer A is a layer that is finally patterned to become resistor 30, first metal layer 41, and first metal layer 51. Therefore, the material and thickness of metal layer A are similar to the material and thickness of resistor 30, first metal layer 41, and first metal layer 51 described above.

[0047] The metal layer A can be formed by, for example, a magnetron sputtering method using a target made of a raw material capable of forming the metal layer A. The metal layer A may be formed by a reactive sputtering method, a vapor deposition method, an arc ion plating method, a pulsed laser deposition method, or the like instead of the magnetron sputtering method.

[0048] From the viewpoint of stabilizing the gauge characteristics, it is preferable to vacuum-deposit a functional layer of a predetermined thickness as a base layer on the upper surface 10a of the base material 10 by, for example, conventional sputtering, before depositing the metal layer A.

[0049] In the present application, the functional layer refers to a layer having a function of promoting the crystal growth of at least the upper layer, the metal layer A (resistor 30). The functional layer preferably further has a function of preventing oxidation of the metal layer A due to oxygen and moisture contained in the base material 10, and a function of improving adhesion between the base material 10 and the metal layer A. The functional layer may further have other functions.

[0050] Since the insulating resin film that constitutes the substrate 10 contains oxygen and moisture, it is effective for the functional layer to have the function of preventing oxidation of the metal layer A, particularly when the metal layer A contains Cr, since Cr forms a self-oxidized film.

[0051] The material of the functional layer is not particularly limited as long as it has the function of promoting the crystal growth of at least the upper layer, the metal layer A (resistor 30), and can be appropriately selected depending on the purpose. For example, Cr (chromium), Ti (titanium), V (vanadium), Nb (niobium), Ta (tantalum), Ni (nickel), Y (yttrium), Zr (zirconium), Hf (hafnium), Si (silicon), C (carbon), Zn (zinc), Cu (copper), Bi (bismuth), and the like can be used. Examples of the metal include one or more metals selected from the group consisting of ruthenium (Ru), Fe (iron), Mo (molybdenum), W (tungsten), Ru (ruthenium), Rh (rhodium), Re (rhenium), Os (osmium), Ir (iridium), Pt (platinum), Pd (palladium), Ag (silver), Au (gold), Co (cobalt), Mn (manganese), and Al (aluminum), an alloy of any of the metals in this group, or a compound of any of the metals in this group.

[0052] Examples of the alloy include FeCr, TiAl, FeNi, NiCr, CrCu, etc. Examples of the compound include TiN, TaN, Si3N4, TiO2, Ta2O5, SiO2, etc.

[0053] When the functional layer is made of a conductive material such as a metal or alloy, the thickness of the functional layer is preferably 1 / 20 or less of the thickness of the resistor. In this range, the crystal growth of α-Cr can be promoted, and a part of the current flowing through the resistor can be prevented from flowing through the functional layer, which reduces the detection sensitivity of strain.

[0054] When the functional layer is made of a conductive material such as a metal or alloy, the thickness of the functional layer is preferably 1 / 50 or less of the thickness of the resistor. In this range, the crystal growth of α-Cr can be promoted, and the strain detection sensitivity can be further prevented from being reduced due to a part of the current flowing through the resistor flowing through the functional layer.

[0055] When the functional layer is made of a conductive material such as a metal or alloy, the thickness of the functional layer is more preferably 1 / 100 or less of the thickness of the resistor, which can further prevent a part of the current flowing through the resistor from flowing through the functional layer, thereby preventing a decrease in the strain detection sensitivity.

[0056] When the functional layer is made of an insulating material such as an oxide or a nitride, the thickness of the functional layer is preferably 1 nm to 1 μm, which can promote the crystal growth of α-Cr and can be easily formed without cracking the functional layer.

[0057] When the functional layer is made of an insulating material such as an oxide or nitride, the thickness of the functional layer is preferably 1 nm to 0.8 μm, which can promote the crystal growth of α-Cr and can be easily formed without cracking the functional layer.

[0058] When the functional layer is made of an insulating material such as an oxide or nitride, the thickness of the functional layer is more preferably 1 nm to 0.5 μm, which can promote the crystal growth of α-Cr and can be more easily formed without cracking the functional layer.

[0059] The planar shape of the functional layer is patterned to be substantially the same as the planar shape of the resistor shown in FIG. 1, for example. However, the planar shape of the functional layer is not limited to being substantially the same as the planar shape of the resistor. When the functional layer is made of an insulating material, it does not have to be patterned to be the same as the planar shape of the resistor. In this case, the functional layer may be formed in a solid shape at least in the region where the resistor is formed. Alternatively, the functional layer may be formed in a solid shape on the entire upper surface of the substrate 10.

[0060] Furthermore, when the functional layer is made of an insulating material, the functional layer is formed relatively thick, at a thickness of 50 nm to 1 μm, and formed in a solid form, so that the thickness and surface area of ​​the functional layer are increased, and the heat generated by the resistor can be dissipated to the substrate 10. As a result, the deterioration of the measurement accuracy of the strain gauge 1 due to self-heating of the resistor can be suppressed.

[0061] The functional layer can be formed in vacuum by conventional sputtering, for example, using a raw material capable of forming the functional layer as a target and introducing Ar (argon) gas into a chamber. By using conventional sputtering, the functional layer is formed while etching the upper surface 10a of the substrate 10 with Ar, so that the amount of the functional layer formed can be minimized and the effect of improving adhesion can be obtained.

[0062] However, this is just one example of a method for forming the functional layer, and the functional layer may be formed by other methods. For example, a method may be used in which the upper surface 10a of the substrate 10 is activated by a plasma treatment using Ar or the like before forming the functional layer, thereby improving adhesion, and then the functional layer is vacuum-formed by magnetron sputtering.

[0063] There are no particular restrictions on the combination of the material of the functional layer and the material of the metal layer A and can be selected appropriately depending on the purpose. For example, it is possible to use Ti for the functional layer and form a Cr mixed phase film with α-Cr (alpha chromium) as the main component for the metal layer A.

[0064] In this case, for example, the metal layer A can be formed by magnetron sputtering using a raw material capable of forming a Cr mixed phase film as a target and introducing Ar gas into a chamber. Alternatively, the metal layer A can be formed by reactive sputtering using pure Cr as a target and introducing an appropriate amount of nitrogen gas together with Ar gas into a chamber. In this case, the ratio of CrN and Cr2N contained in the Cr mixed phase film, and the ratio of Cr2N in CrN and Cr2N can be adjusted by changing the amount and pressure of the nitrogen gas introduced (nitrogen partial pressure) or by adjusting the heating temperature by providing a heating process.

[0065] In these methods, the growth surface of the Cr mixed-phase film is determined by the functional layer made of Ti, and a Cr mixed-phase film containing α-Cr, which has a stable crystal structure, as a main component, can be formed. Furthermore, the Ti constituting the functional layer is diffused into the Cr mixed-phase film, thereby improving the gauge characteristics. For example, the gauge factor of the strain gauge 1 can be set to 10 or more, and the gauge factor temperature coefficient TCS and the resistance temperature coefficient TCR can be set within the range of -1000 ppm / °C to +1000 ppm / °C. When the functional layer is made of Ti, the Cr mixed-phase film may contain Ti and TiN (titanium nitride).

[0066] When the metal layer A is a Cr mixed phase film, the functional layer made of Ti has all of the following functions: promoting the crystal growth of the metal layer A, preventing oxidation of the metal layer A due to oxygen and moisture contained in the base material 10, and improving the adhesion between the base material 10 and the metal layer A. The same applies when Ta, Si, Al, or Fe is used as the functional layer instead of Ti.

[0067] In this way, by providing a functional layer below the metal layer A, it is possible to promote crystal growth in the metal layer A, and to produce a metal layer A consisting of a stable crystal phase. As a result, it is possible to improve the stability of the gauge characteristics of the strain gauge 1. In addition, the material constituting the functional layer diffuses into the metal layer A, thereby improving the gauge characteristics of the strain gauge 1.

[0068] Next, a plurality of recesses 30x are formed in necessary portions of the metal layer A. The recesses 30x are formed at least in the region of the metal layer A that will become the resistor 30, but may also be formed in the regions that will become the first metal layers 41 and 51. The recesses 30x can be formed by, for example, a photolithography method. Depending on the shape of a mask used when etching the metal layer A, the recesses 30x can be formed in any shape.

[0069] Next, the second metal layer 42 and the second metal layer 52 are formed on the upper surface of the metal layer A. The second metal layer 42 and the second metal layer 52 can be formed by, for example, a photolithography method.

[0070] Specifically, first, a seed layer is formed by, for example, sputtering or electroless plating so as to cover the upper surface of the metal layer A. Next, a photosensitive resist is formed on the entire upper surface of the seed layer, and is exposed and developed to form openings that expose the regions in which the second metal layer 42 and the second metal layer 52 are to be formed. At this time, the pattern of the second metal layer 42 can be formed into any shape by adjusting the shape of the openings in the resist. For example, a dry film resist can be used as the resist.

[0071] Next, for example, the second metal layer 42 and the second metal layer 52 are formed on the seed layer exposed in the opening by electrolytic plating using the seed layer as a power supply path. The electrolytic plating method is preferable in that it has high tact and can form low-stress electrolytic plating layers as the second metal layer 42 and the second metal layer 52. By making the electrolytic plating layer thick and low-stress, it is possible to prevent warping of the strain gauge 1. The second metal layer 42 and the second metal layer 52 may be formed by electroless plating.

[0072] Next, the resist is removed. For example, the resist can be removed by immersing the resist in a solution that can dissolve the resist material.

[0073] Next, a photosensitive resist is formed on the entire upper surface of the seed layer, and is exposed and developed to be patterned into a planar shape similar to that of the resistor 30, the wiring 40, and the electrode 50 in Fig. 1. For example, a dry film resist can be used as the resist. Then, the resist is used as an etching mask to remove the metal layer A and the seed layer exposed from the resist, thereby forming the resistor 30, the wiring 40, and the electrode 50 in the planar shape of Fig. 1.

[0074] For example, unnecessary portions of the metal layer A and the seed layer can be removed by wet etching. If a functional layer is formed below the metal layer A, the functional layer is patterned by etching into the planar shape shown in Fig. 1, similar to the resistor 30, the wiring 40, and the electrode 50. At this point, a seed layer is formed on the resistor 30, the first metal layer 41, and the first metal layer 51.

[0075] Next, the second metal layer 42 and the second metal layer 52 are used as an etching mask to remove unnecessary seed layer exposed from the second metal layer 42 and the second metal layer 52, thereby forming the second metal layer 42 and the second metal layer 52. Note that the seed layer directly below the second metal layer 42 and the second metal layer 52 remains. For example, the unnecessary seed layer can be removed by wet etching using an etching solution that etches the seed layer but does not etch the functional layer, the resistor 30, the wiring 40, and the electrodes 50.

[0076] Thereafter, a cover layer 60 that covers the resistor 30 and the wiring 40 and exposes the electrodes 50 is provided on the upper surface 10a of the substrate 10, thereby completing the strain gauge 1. The cover layer 60 can be produced, for example, by laminating a semi-cured thermosetting insulating resin film on the upper surface 10a of the substrate 10 so as to cover the resistor 30 and the wiring 40 and expose the electrodes 50, and then heating and curing the film. The cover layer 60 may also be produced by applying a liquid or paste-like thermosetting insulating resin to the upper surface 10a of the substrate 10 so as to cover the resistor 30 and the wiring 40 and expose the electrodes 50, and then heating and curing the resin.

[0077] When a functional layer is provided on the upper surface 10a of the substrate 10 as an underlayer for the resistor 30, the first metal layer 41, and the first metal layer 51, the strain gauge 1 has a cross-sectional shape as shown in Fig. 5. The layer indicated by reference numeral 20 is the functional layer. When the functional layer 20 is provided, the planar shape of the strain gauge 1 is, for example, the same as that shown in Fig. 1. However, as described above, the functional layer 20 may be formed solidly on a part or all of the upper surface of the substrate 10.

[0078] First Modification of the First Embodiment In Modification 1 of the first embodiment, an example in which a recess is formed on the upper surface of the base material is shown. Note that in Modification 1 of the first embodiment, the description of the same components as those in the already described embodiments may be omitted.

[0079] Fig. 6 is a partial cross-sectional view illustrating a strain gauge according to a first modified example of the first embodiment, showing a cross section corresponding to the vicinity of part C in Fig. 2. Fig. 7 is a partial plan view illustrating the positional relationship between the recess of the substrate and the recess of the resistor.

[0080] 6 and 7, in the strain gauge 1A, the substrate 10 has a plurality of recesses 10x recessed from the top surface to the bottom surface. The resistor 30 is formed along the recesses 10x, and therefore the resistor 30 also has recesses 30y. That is, the recesses 30y are arranged within the recesses 10x when viewed from the normal direction of the top surface of the resistor 30. The size, arrangement, density, etc. of the recesses 30y can be the same as those of the recesses 30x. The cover layer 60 has an area that directly covers the recesses 30y, and further has an area that directly covers the recesses 10x.

[0081] The recesses 10x can be formed in the upper surface 10a of the substrate 10 by, for example, press processing using a mold. The recesses 10x may be formed by etching the upper surface 10a of the substrate 10. The recesses 30y can be formed by depositing or sputtering a material to become the resistor 30 on the upper surface 10a of the substrate 10 on which the recesses 10x are formed.

[0082] In the strain gauge 1A, by providing a recess 30y that opens into the upper surface of the resistor 30, it is possible to increase the area of ​​the upper surface of the resistor 30, including the surface area of ​​the recess 30y. As a result, as in the first embodiment, the contact area between the resistor 30 and the cover layer 60 increases, generating an anchor effect, and improving the adhesion between the resistor 30 and the cover layer 60.

[0083] In addition, in the strain gauge 1A, recesses 10x are formed even in areas where the resistor 30 is not formed. Therefore, the contact area between the substrate 10 and the cover layer 60 increases, generating an anchor effect, and improving the adhesion between the substrate 10 and the cover layer 60.

[0084] Although preferred embodiments have been described above in detail, the present invention is not limited to the above-described embodiments, and various modifications and substitutions can be made to the above-described embodiments without departing from the scope of the claims.

[0085] For example, the present invention is also applicable to a strain gauge having a plurality of resistors formed on a substrate. For example, the present invention is also applicable to a strain gauge having two resistors formed on a substrate that form a half-bridge circuit. Alternatively, the present invention is also applicable to a strain gauge having four resistors formed on a substrate that form a full-bridge circuit. [Explanation of symbols]

[0086] 1, 1A strain gauge, 10 substrate, 10a upper surface, 10x, 30x, 30y recess, 20 functional layer, 30 resistor, 30e1, 30e2 termination, 40 wiring, 50 electrode, 41, 51 first metal layer, 42, 52 second metal layer, 60 cover layer

Claims

1. A flexible substrate; A resistor formed on the substrate; an insulating resin layer formed on the base material and covering the resistor; the resistor includes a plurality of recesses recessed from an upper surface toward the substrate, The recess has a bottom surface and four inner sides connected to the bottom surface.

2. The strain gauge according to claim 1 , wherein the recesses are regularly arranged on the upper surface of the resistor when viewed in a normal direction of the upper surface of the resistor.

3. The strain gauge according to claim 1 or 2, wherein the roughness of the upper surface of the resistor is greater than the roughness of the side surface of the resistor.

4. 4. The strain gauge according to claim 1, wherein, when the area of ​​the upper surface of the resistor when the recess is not formed is taken as 1, the area of ​​the upper surface of the resistor including the surface area of ​​the recess when the recess is formed is 1.5 or more.

5. the base material includes a plurality of second recesses recessed in a direction from the upper surface to the lower surface, The resistor is formed along the second recess, The strain gauge according to claim 1 , wherein the recess is disposed within the second recess when viewed from a normal direction of an upper surface of the resistor.

6. The strain gauge according to claim 5 , wherein the insulating resin layer has a region covering the second recess.

7. The resistor is made of Cr, CrN, and Cr. 2 7. The strain gauge according to claim 1, which is formed from a film containing N.

8. 8. The strain gauge according to claim 7, having a gauge factor of 10 or more.

9. The CrN and Cr contained in the resistor 2 9. The strain gauge according to claim 7, wherein N is 20% by weight or less.

10. The CrN and the Cr 2 The Cr in N 2 10. The strain gauge according to claim 9, wherein the proportion of N is 80% by weight or more and less than 90% by weight.

Citation Information

Patent Citations

  • Strain sensor

    JP1998047911A

  • Strain sensor

    JP2014038088A

  • Alloy for strain gauge and strain gauge

    JP2016074934A

  • Strain gauge

    JP2019074420A

  • Strain gauge

    JP2019090723A