Resin-coated materials

The resin-coated member with peeling and non-peeling regions addresses adhesion and releasability issues, enhancing corrosion resistance and waterproof properties by using peeling agents and non-peeling materials.

JP7579115B2Active Publication Date: 2024-11-07IHI INFRASTRUCTURE SYST CO LTD +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2020191754
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-11-18
Publication Date
2024-11-07
Estimated Expiration
2040-11-18

AI Technical Summary

Technical Problem

Existing resin-coated members face issues with balanced adhesion and releasability, leading to prolonged peeling times when tightly adhered and increased corrosion when loosely adhered, compromising corrosion resistance and waterproof properties.

Method used

A resin-coated member with a peeling region made of a peeling agent and a non-peeling region without the peeling agent, using materials like fluororesin and polyvinyl alcohol resin, to enhance balanced adhesion and releasability.

Benefits of technology

The configuration improves both adhesion and releasability, preventing corrosion and water ingress while ensuring efficient resin layer removal.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007579115000001
    Figure 0007579115000001
  • Figure 0007579115000002
    Figure 0007579115000002
  • Figure 0007579115000003
    Figure 0007579115000003
Patent Text Reader

Abstract

To provide a resin-coated member including a resin layer that has improved peelability and adhesion in a balanced manner.SOLUTION: A resin-coated member 10 includes a member 12, and a resin layer 14 that coats the surface of the member 12 and is formed of transparent polyurea resin. The resin-coated member 10 includes a peeling region 16 that is provided between the member 12 and the resin layer 14 and comprises a peeling layer 20 formed of a peeling agent, and a non-peeling region 18 that is provided between the member 12 and the resin layer 14 and does not comprise the peeling layer 20.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a resin-coated member. [Background technology]

[0002] Conventionally, the surfaces of components such as steel members used in structures such as plants, bridges, and water gates have been covered with resin sheets to improve the corrosion resistance, waterproofing, and other properties of the components (see Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 5059222 Summary of the Invention [Problem to be solved by the invention]

[0004] Incidentally, when a resin layer such as a resin sheet covering a member such as a steel member deteriorates over time, the deteriorated resin layer is peeled off from the member, and then a new resin layer is applied again. Also, when the member is painted, when the coating deteriorates over time, the resin layer is peeled off, and then the member is repainted and then coated with a new resin layer.

[0005] Here, when peeling off the resin layer from the member, if the resin layer and the member are strongly adhered to each other, the peeling off operation of the resin layer as described above may take a long time. On the other hand, if the adhesion between the resin layer and the member is low, the resin layer is easily peeled off from the member, and corrosive media such as water are easily allowed to enter through the gap between the resin layer and the member. This may result in a decrease in corrosion resistance, waterproofing, etc.

[0006] Therefore, an object of the present disclosure is to provide a resin-coated member that can improve the releasability and adhesion of a resin layer in a well-balanced manner. [Means for solving the problem]

[0007] The present disclosure For constructing steel structures The resin-coated member is steel The member and steel A resin layer formed of a transparent polyurethane resin and covering the surface of the member; steel provided between the member and the resin layer, One or more resins selected from the group consisting of fluororesin, polyvinyl alcohol resin, vinyl acetate resin, acrylic resin, and silicone resin. A release region formed of a release layer formed of a release agent; steel and a non-peeling region that is provided between the member and the resin layer and does not include the peel layer.

[0008] In the resin-coated member according to the present disclosure, a plurality of the peeled regions may be provided and may be spaced apart from each other.

[0009] In the resin-coated member according to the present disclosure, steel The outer periphery between the member and the resin layer may be formed by the non-peeled region.

[0010] In the resin-coated member according to the present disclosure, the peeled-off region may be provided in a dot or line shape. Effect of the Invention

[0011] According to the resin-coated member having the above configuration, the releasability and adhesion of the resin layer can be improved in a well-balanced manner. [Brief description of the drawings]

[0012] [Figure 1] 1 is a schematic cross-sectional view showing a configuration of a resin-coated member in a first embodiment of the present disclosure. FIG. [Diagram 2] FIG. 2 is a schematic plan view showing a configuration of a resin-coated member in the first embodiment of the present disclosure. [Diagram 3] 2 is a diagram showing a peeled region formed in a circular dot shape larger than the peeled region shown in FIG. 1 in the first embodiment of the present disclosure. FIG. [Figure 4] 1 is a diagram showing a peeled region formed irregularly in a circular dot pattern in the first embodiment of the present disclosure. FIG. [Diagram 5]1 is a diagram showing a peeling region formed in a quadrangular dot pattern in the first embodiment of the present disclosure. FIG. [Figure 6] 1 is a diagram showing a peeling region formed in a rectangular line shape in the first embodiment of the present disclosure. FIG. [Figure 7] 4 is a flowchart showing a method for manufacturing a resin-coated member in the first embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] First Embodiment A first embodiment of the present disclosure will be described in detail below with reference to the drawings. Fig. 1 is a schematic cross-sectional view showing the configuration of a resin-coated member 10. Fig. 2 is a schematic plan view showing the configuration of the resin-coated member 10. The resin-coated member 10 includes a member 12 and a resin layer 14 that coats the surface of the member 12.

[0014] The member 12 is composed of a metal member formed of a metal material such as steel, a concrete member formed of a concrete material, or the like. The member 12 is, for example, a structural member used in structures such as plants, bridges, and water gates. The member 12 is, for example, composed of a flat plate member, or the like. The member 12 may be painted to improve corrosion resistance, waterproofing, and the like, and a coating film may be provided on the surface of the member 12.

[0015] The resin layer 14 is coated on the surface of the member 12 and is made of resin. By covering the surface of the member 12 with the resin layer 14, the surface of the member 12 can be protected. For example, by covering the surface of the member 12 with the resin layer 14, the corrosion resistance and waterproofing properties of the member 12 can be improved. In addition, by covering the surface of the member 12 with the resin layer 14, damage such as scratches on the surface of the member 12 can be suppressed. The thickness of the resin layer 14 can be, for example, 100 μm to 3 mm. The resin layer 14 can be made of a thermoplastic resin, a thermosetting resin, or the like. For example, a polyurea resin, a urethane resin, a polyvinyl chloride resin, or the like can be used as the resin of the resin layer 14.

[0016] The resin layer 14 is preferably made of a highly elastic resin. When the resin layer 14 is made of a highly elastic resin, the resin layer 14 has a high elastic force. This allows the resin layer 14 to follow even if microcracks or the like occur, and thus prevents the resin layer 14 from breaking. For example, a polyurea resin may be used as such a highly elastic resin.

[0017] The resin layer 14 is preferably made of a transparent resin. Since the resin layer 14 is transparent, it is possible to inspect and observe the surface state of the member 12 from the outside. For example, a transparent polyurethane resin is preferably used as such a transparent resin.

[0018] The resin-coated member 10 has a peeling region 16 provided between the member 12 and the resin layer 14, and a non-peeling region 18 provided between the member 12 and the resin layer 14. By providing the peeling region 16 and the non-peeling region 18 between the member 12 and the resin layer 14, it is possible to improve the peelability and adhesion of the resin layer 14 in a well-balanced manner. Next, the peeling region 16 and the non-peeling region 18 will be described in detail.

[0019] The peeling region 16 is provided between the member 12 and the resin layer 14, and is composed of a peeling layer 20 formed of a release agent. By providing the peeling layer 20, at least one of the adhesion between the resin layer 14 and the peeling layer 20 and the adhesion between the member 12 and the peeling layer 20 can be made smaller than the adhesion between the member 12 and the resin layer 14. In the peeling region 16, the adhesion between the member 12 and the resin layer 14 is reduced by interposing the peeling layer 20 therebetween, so that when peeling the resin layer 14 from the member 12, the resin layer 14 can be easily peeled off.

[0020] The release layer 20 is formed of a release agent, such as a fluororesin, a polyvinyl alcohol resin, a vinyl acetate resin, an acrylic resin, a silicone resin, or a water-soluble resin.

[0021] At least one peeled region 16 is required, and a plurality of peeled regions 16 may be provided. When a plurality of peeled regions 16 are provided, the peeled regions 16 may be provided spaced apart from each other. Even if peeling occurs between the member 12 and the resin layer 14 in one of the peeled regions 16 during use of the resin-coated member 10, the peeled regions 16 are discontinuous and do not contact each other, so that a chain reaction of peeling is suppressed. As a result, even if a corrosive medium such as water enters the gap between the member 12 and the resin layer 14 from the peeled portion of the peeled region 16, the corrosive medium is surrounded by the non-peeled region 18, so that further diffusion of the corrosive medium can be suppressed.

[0022] The peeled regions 16 can be provided between the member 12 and the resin layer 14 in the form of dots (points) or lines (lines). The shape of the peeled regions 16 can be, for example, a circle or a polygon. All the peeled regions 16 may be formed to have the same size, or may be formed to have different sizes. The peeled regions 16 may be provided in a regular arrangement, or may be provided in an irregular arrangement.

[0023] For example, in the resin-coated member 10 shown in Figs. 1 and 2, the peeled regions 16 are formed in a circular dot pattern. Figs. 3 to 5 are schematic plan views showing the configurations of other peeled regions 22, 24, 26, and 28. Fig. 3 is a view showing a peeled region 22 formed in a circular dot pattern larger than the peeled region 16 shown in Fig. 1. Fig. 4 is a view showing a peeled region 24 formed in an irregular circular dot pattern. Fig. 5 is a view showing a peeled region 26 formed in a rectangular dot pattern. Fig. 6 is a view showing a peeled region 28 formed in a rectangular line pattern. Note that the configurations of the peeled regions 16, 22, 24, 26, and 28 shown in Figs. 1 to 6 are merely examples, and the configuration of the peeled region is not limited to these.

[0024] The non-peeling region 18 is provided between the member 12 and the resin layer 14, and is configured not to include the peeling layer 20. Since the non-peeling region 18 does not include the peeling layer 20, the resin layer 14 and the member 12 are in direct contact with each other. This enhances the adhesion between the member 12 and the resin layer 14 in the non-peeling region 18. Since the adhesion between the member 12 and the resin layer 14 is enhanced in this manner in the non-peeling region 18, it is possible to suppress the intrusion of a corrosive medium such as water between the member 12 and the resin layer 14.

[0025] The outer periphery between the member 12 and the resin layer 14 can be formed as a non-peeling region 18. It is preferable that the entire periphery of the outer periphery between the member 12 and the resin layer 14 is formed as a non-peeling region 18. In the outer periphery between the member 12 and the resin layer 14, the adhesion between the member 12 and the resin layer 14 is increased, so that the intrusion of corrosive media such as water from the outside of the resin-coated member 10 can be suppressed.

[0026] The adhesive force between the resin layer 14 and the release layer 20 is preferably greater than the adhesive force between the member 12 and the release layer 20. When the resin layer 14 is peeled off from the resin-coated member 10, the release layer 20 adheres to the resin layer 14, so that the resin layer 14 and the release layer 20 can be peeled off substantially simultaneously. This prevents the release layer 20 from remaining on the surface of the member 12, so that the peeling operation of the resin layer 14 can be performed efficiently. For example, in the case where the member 12 is formed of stainless steel, the resin layer 14 is formed of a polyurethane resin, and the release layer 20 is formed of a polyvinyl alcohol resin, the resin layer 14 and the release layer 20 can be peeled off substantially simultaneously when the resin layer 14 is peeled off, so that the release layer 20 can be prevented from remaining on the surface of the member 12.

[0027] Next, a description will be given of a method for manufacturing the resin-coated member 10. Fig. 7 is a flowchart showing a method for manufacturing the resin-coated member 10. The method for manufacturing the resin-coated member 10 includes a release layer forming step (S10) and a resin layer forming step (S12).

[0028] The release layer forming step (S10) is a step of forming a release layer 20 with a release agent only on a part of the surface of the member 12, thereby forming a release region 16 consisting of the release layer 20 and a non-release region 18 not including the release layer 20. First, before forming the release layer 20 on the surface of the member 12, it is advisable to pretreat the surface of the member 12. When the member 12 is a metal member, the member 12 can be pretreated by pickling, mechanical polishing, degreasing, or the like. These pretreatments can be performed by general pretreatment methods for metal materials.

[0029] Next, a method for forming the release layer 20 will be described. The release layer 20 can be formed by spraying or stamping a release agent. The release layer 20 may be formed using a sheet material having holes through which the release agent can pass and holes through which the release agent cannot pass, such as a silk screen, or a mesh material. The release agent may be the above-mentioned fluororesin or other release agent. The release agent may be any of those generally available on the market.

[0030] The resin layer forming step (S12) is a step of coating the surface of the member 12 provided with the release layer 20 with a resin to form a resin layer 14. The resin layer 14 can be formed by spraying or applying an uncured resin onto the surface of the member 12 provided with the release layer 20, and then curing the resin by heating or the like. The resin may be the above-mentioned polyurea resin or the like. The resin may be any resin that is generally available on the market. In this manner, the resin-coated member 10 can be manufactured.

[0031] As described above, the resin-coated member having the above-mentioned configuration includes a member and a resin layer that is coated on the surface of the member and is made of resin, and has a release region that is provided between the member and the resin layer and is made of a release layer formed of a release agent, and a non-release region that is provided between the member and the resin layer and does not include a release layer, thereby making it possible to improve the releasability and adhesion of the resin layer in a well-balanced manner.

[0032] For example, when the surface of a member is painted, the surface of the member may be repainted due to deterioration of the coating film over time. In such a case, the resin layer of the resin-coated member is peeled off, the deteriorated coating film on the surface of the member is removed, and the surface of the member is repainted. Usually, the adhesion between the member and the resin layer is high, so that when peeling the resin layer from the resin-coated member, the resin layer is difficult to peel off from the member, and a great deal of effort is required. In contrast, when a peeling region is provided between the member and the resin layer, the resin layer is easily peeled off from the member, so that the resin layer can be easily peeled off. In addition, in the non-peeling region, the adhesion between the member and the resin layer is high, so that anticorrosiveness, waterproofness, etc. can be ensured during use of the resin-coated member. [Explanation of symbols]

[0033] 10 Resin-coated parts 12 Materials 14 Resin layer 16 Peeling Area 18 Non-peeling area 20 Peeling layer

Claims

1. A resin-coated member for use in constructing a steel structure, comprising: A steel member; A resin layer formed of a transparent polyurethane resin and coated on the surface of the steel member; Equipped with a release region provided between the steel member and the resin layer, the release region being made of a release layer formed of one or more release agents selected from a fluororesin, a polyvinyl alcohol resin, a vinyl acetate resin, an acrylic resin, and a silicone resin; a non-peeling region provided between the steel member and the resin layer and not including the peeling layer; A resin-coated member having the above structure.

2. The resin-coated member according to claim 1, The resin-coated member has a plurality of peelable regions that are spaced apart from each other.

3. The resin-coated member according to claim 1 or 2, A resin-coated member, wherein an outer periphery between the steel member and the resin layer is formed as the non-peeling region.

4. The resin-coated member according to any one of claims 1 to 3, The peelable regions are provided in a dot or line pattern in the resin-coated member.

Citation Information

Patent Citations

  • JP1975059222A

  • Lid material of container

    JP1989009185A

  • Packaging material for aromatic

    JP1992212840A

  • Panel for construction

    JP2004169494A