Method and apparatus for forming a protective sidewall layer to inhibit bowing - Patents.com
The AFS layer in a two-step etching process addresses sidewall bowing in high aspect ratio etching, ensuring uniformity and reliability in semiconductor manufacturing by protecting sidewalls during etching, thus maintaining memory cell performance.
Patent Information
- Application Number
- JP2021066417
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-05-27
- Filing Date
- 2021-04-09
- Publication Date
- 2024-11-11
- Estimated Expiration
- 2041-04-09
AI Technical Summary
Conventional high aspect ratio etching processes in semiconductor manufacturing often result in sidewall bowing, leading to non-uniformity and potential performance issues in stacked structures like 3D-NAND, which affects memory cell durability and performance.
A two-step etching process involving the formation of an ammonium fluorosilicate (AFS) layer on sidewalls to protect them during etching, followed by controlled etching of the bottom surface, using plasma processing to maintain uniform aperture dimensions and prevent sidewall bowing.
The AFS layer effectively prevents sidewall bowing, ensuring uniformity and reliability of high aspect ratio etching, maintaining memory cell performance and durability by protecting sidewalls from over-etching and ion bombardment.
Smart Images

Figure 0007580327000004 
Figure 0007580327000005 
Figure 0007580327000006
Abstract
Description
[Technical field]
[0001] The present disclosure relates to semiconductor manufacturing equipment and generally to substrate processing methods and substrate processing apparatus. More specifically, the present disclosure relates to systems and methods for performing high aspect ratio etching in fabricating devices such as 3D-NAND and DRAM, and more particularly to a system that aids in high aspect ratio etching while suppressing sidewall etching, i.e. bowing. [Background technology]
[0002] Over time, new technologies have improved the way semiconductors are made, decreasing the size of individual integrated circuits (ICs, microelectronic circuits, microchips, or simply "chips") and the geometries of the components contained within an IC. Miniature active and passive semiconductor devices and connections are fabricated on a semiconductor substrate wafer (e.g., silicon). In forming such ICs, the wafer undergoes processes such as doping, ion implantation, etching, thin film deposition of various materials, and photolithographic patterning. The individual microcircuits are finally separated by dicing the wafer and packaged individually as ICs.
[0003] Processes that are particularly used when forming ICs on a substrate include atomic layer deposition (ALD), chemical vapor deposition (CVD), atomic layer etching (ALE), etc. In conventional processes, etching conditions are changed according to the depth of the pattern to be formed. For example, in conventional processes, the chamber pressure, radio frequency power, and flow rate ratio of process gases are changed according to the depth of the pattern to be formed.
[0004] The following Patent Document 1 describes a conventional method for performing high aspect ratio (HAR) etching in a three-dimensional stacked semiconductor memory.
[0005] Moreover, the following Patent Document 2 describes a process for removing a native oxide film on a substrate. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] US Patent Application Publication No. 2017 / 0372916 [Patent Document 2] Patent Publication No. 2010-165954 Summary of the Invention [Problem to be solved by the invention]
[0007] The present disclosure provides methods and apparatus that can perform high aspect ratio (HAR) etching without or with reduced "bowing" effects on the sidewalls of the etched features. [Means for solving the problem]
[0008] According to one embodiment, a substrate processing apparatus performs a method for etching a substrate. The method includes a first step of etching the substrate to form a first portion of a recess in the substrate as an etched feature. The first portion of the recess includes a bottom surface and a sidewall. The method also includes a second step of forming an ammonium fluorosilicate (AFS) layer in or on the sidewall, and then a third step of etching the bottom surface to form a second portion of the recess. The third step is performed while maintaining protection of the sidewall by the AFS layer.
[0009] The above paragraphs are intended to be general, and are not intended to limit the scope of the appended claims. The embodiments and advantages described herein will be best understood by reference to the following detailed description when considered in conjunction with the accompanying drawings, in which: [Brief description of the drawings]
[0010] [Figure 1] 1 is a diagram showing bowing occurring on the sidewall of a high aspect ratio recess in a semiconductor device; [Diagram 2]FIG. 1 illustrates an example of a substrate processing apparatus (SA), ie, a plasma processing (etching) system, according to the present disclosure. [Diagram 3] FIG. 1 illustrates an example of an inductively coupled plasma (ICP) device according to the present disclosure. [Figure 4] 2A-2C are a series of diagrams illustrating the transformation of a substrate through successive processing steps performed in accordance with a first embodiment of the present disclosure. [Diagram 5] 5A-5C are a series of diagrams illustrating the transformation of a substrate through successive processing steps carried out in accordance with a second embodiment of the present disclosure. [Figure 6] 1 is a flowchart of an example of a process flow that may be performed in accordance with the teachings of the present disclosure. [Figure 7] FIG. 1 is a block diagram of a control circuit for implementing the operations described herein on a computer. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The following description, in conjunction with the accompanying drawings, describes various embodiments of the subject matter of the present disclosure, and is not necessarily limited to the described embodiments. In the examples, specific details are described for the purpose of facilitating understanding of the subject matter of the present disclosure. However, it is clear to those skilled in the art that each embodiment can be practiced without such specific details. In some examples, well-known structures and components may be shown in block diagram form to avoid obscuring the concept of the subject matter of the present disclosure.
[0012] Throughout this specification, "one embodiment" or "embodiment" means that a particular feature, structure, characteristic, operation, or function described with respect to an embodiment is included in at least one embodiment of the presently disclosed subject matter. Thus, the phrases "in one embodiment" or "in an embodiment" used herein do not necessarily refer to the same embodiment. Moreover, the particular features, structures, characteristics, operations, or functions may be combined in any suitable manner in one or more embodiments. Furthermore, embodiments of the presently disclosed subject matter may include modifications and variations of the described embodiments.
[0013] In this specification and the appended claims, the singular forms "a" and "the" include the plural, unless expressly stated otherwise. That is, in this specification, terms such as "a" mean "one or more" unless expressly indicated otherwise. Furthermore, terms such as "left", "right", "top", "bottom", "front", "rear", "side", "height", "length", "width", "upper", "lower", "internal", "external", "inside", "outside", and the like, are used herein merely to indicate reference points and do not necessarily limit embodiments of the subject matter of the present disclosure to a particular orientation or configuration. Furthermore, terms such as "first", "second", "third", and the like, are used herein merely to specify the number of parts, components, reference points, actions, and / or functions, etc., described herein and do not necessarily limit embodiments of the subject matter of the present disclosure to a particular configuration or orientation.
[0014] The inventors have recognized that performing high aspect ratio (HAR) etching without creating a "bowing" effect on the sidewalls of the etched features becomes increasingly difficult as the dimensions of the stack structure increase. Throughout this disclosure, "recess" is used as a type of etched feature, and the terms "recess" and "etched feature" are used interchangeably herein. For example, in 3D-NAND, alternating deposited layers (often alternating SiO and SiN layers) form a stack structure. The stack somewhat resembles a high-rise building, containing multiple floors with multiple memory cells formed on each floor. Deep etching is required to define channels between cells, and ideally the etch is performed to ensure uniform hole size for all layers in the stack. If the etch is not performed properly, there will be a lack of uniformity for a particular hole, resulting in a variety of shapes, including bowing, as shown in region R1 of stack 202 in FIG. 1. Bowing results from over-etching the sidewalls, especially in the upper portion of stack 202. Bowing can also result from ions scattering from the beveled edge of the mask due to long exposure to etching. In high aspect ratio etching, ions travel in a straight line, but some ions bounce off the beveled edge of the mask and are sent to the sidewall of region R1. Furthermore, as shown in FIG. 1, a mask (amorphous carbon layer) 203 is placed on top of a stack 202 formed on a substrate 201. The beveled angle of the resist mask causes over-etching of the upper part of the sidewall of the stack 202, thus causing bowing in the opening dimension (diameter of the hole) and non-uniformity of the opening dimension along the entire depth of the hole. Such bowing should be avoided to maintain the durability and performance of the memory cell.
[0015] A configuration of a substrate processing apparatus SA according to an exemplary embodiment of the present disclosure will be described with reference to FIG. 2. The substrate processing apparatus SA includes a transfer module TM (operating at a lower pressure than the process modules PMx). The transfer module TM includes a transfer robot module TMR that transfers a wafer W between the plasma etching modules PM1, PM2, PM3, and PM4. The transfer module TM has a vacuum transfer chamber coupled to the load lock chambers LL1 and LL2. The plasma etching modules PM1, PM2, PM3, and PM4 are connected to the transfer module TM and partitioned from the load lock chambers LL1 and LL2. Although four plasma etching modules (PM1 to PM4) are shown, other configurations may be similarly adopted. For example, one or more of the plasma etching modules may be replaced by a stocker / changer. The stocker / changer is used as a storage location for wafers and tools such as electrostatic chucks that include replacement parts at their tops. The stockers may be located in any of the positions occupied by the plasma etching modules PM1, PM2, PM3, PM4, or may be located on the other side of each reaction chamber, away from the TM.
[0016] Each of the plasma etching modules PM1-PM4 may be configured as an ICP device, although one or more of these plasma etching modules may be other reaction chambers, such as a capacitively coupled plasma (CCP) device. The substrate processing described herein may be performed in any one of the plasma etching modules PM1, PM2, PM3, PM4. However, as an alternative, the plasma etching modules PM1, PM2, PM3, PM4 may be used in a cooperative manufacturing process, for example, where PM1 is used to form an ammonium silicofluoride (AFS) layer, PM2 performs the etching, and PM3 removes the AFS, with PM3 acting as a controllable heating chamber. As a further alternative, the formation of the AFS may be split between PM1 and PM2, and PM1 may deposit SiO 2 . x Form a layer of SiO in PM2 xThe AFS is formed using the starting material. Etching may then be performed in PM3, and residual AFS may be removed by heating in PM4. The above is merely an example, and if the process is distributed across multiple PMs, the transfer robot module TMR may be controlled by the controller MC to move a specific wafer between PMs, and any combination other than the above examples is possible. Alternatively, all steps may be performed within a single PM, or a composite combination thereof may be used.
[0017] The load lock chambers LL1 and LL2 can compartmentalize the environment between the transfer module TM and the loader module LM. The loader module LM has a carrier placement stage on which a carrier is placed. The carrier holds, for example, 25 wafers W, and is placed in front of the loader module LM when being loaded into or unloaded from the substrate processing apparatus SA. The loader robot module LMR transfers wafers between the carrier placement stage and the load lock chambers LL1 and LL2. The carriers are exchanged at the respective load ports LP1, LP2, LP3, and LP4 (in this example, multiple LPs).
[0018] The controller MC is a microcontroller in this example, although a computer such as that described in Figure 7 (either a local dedicated computer or a distributed computer) may be used in place of the controller circuitry configured with computer code to perform the control operations described herein. Additionally, the controller MC controls the operation of the substrate processing apparatus SA, including the execution of process recipes consistent with the process steps described herein.
[0019] FIG. 3 shows a schematic diagram of a plasma processing module PM, such as an inductively coupled plasma (ICP) system, coupled to a transfer module via a gate valve (not shown). Although an ICP system is shown as an example, other plasma processing modules PM, such as a capacitively coupled plasma (CCP) device, may be used as well. The device includes a reaction chamber 11, a dielectric (e.g., quartz) window 13, and a lower electrode 14. An inductive element (coil) 20 is disposed above the dielectric window 13. High frequency power is supplied from high frequency power sources 16 and 17 to the inductive element 20 and the lower electrode 14, respectively. This power coupling may include varying the frequency of the high frequency power sources 16 and 17. The lower electrode 14 includes an electrostatic chuck (ESC) 15 configured to support and hold a wafer W. A gas source 18 is connected to the reaction chamber 11 and configured to supply various process gases (described below) into the reaction chamber 11. An exhaust device 19, such as a turbo molecular pump (TMP), is connected to the reaction chamber 11 and configured to controllably exhaust the reaction chamber 11. When high frequency power is supplied to at least one of the coil 20 and the lower electrode 14 , a plasma 12 is generated in the vicinity of the wafer W between the dielectric window 13 and the lower electrode 14 .
[0020] In one embodiment, the plasma processing module PM may have a dedicated control circuit (e.g., a microcontroller or a computer as shown in FIG. 7) that operates exclusively or in cooperation with a controller MC (FIG. 2). The controller MC executes a control program stored in a memory and controls each part of the plasma processing module PM based on recipe data stored in the memory.
[0021] Figures 4A-4E illustrate a progression of processing steps performed on a semiconductor substrate that can reliably form deep etches in a stack while reducing bowing and maintaining uniform opening dimensions throughout the deep etches. Figure 4A is a diagram of a substrate including an etch layer 101 (e.g., a carbon-containing layer) on which a mask layer 102 is formed. In the mask layer 102, an open area (opening) OP is formed in which a recess, i.e., an etch feature, with a high aspect ratio, will be etched into the etch layer 101.
[0022] FIG. 4B is a view of the substrate after a first etch has been performed on the etching layer 101. As a result of the etch, an upper portion (or first portion) of the recess is formed. The etch may be performed using an oxygen plasma, for example, generated from O2, CO, or CO2 gases. The difference in height of the mask layer 102 between FIG. 4A and FIG. 4B indicates that a portion of the mask layer 102 has also been removed. Also, at the opening OP of the mask layer 102, a large portion of the etching layer 101 has been removed.
[0023] FIG. 4C is a diagram of a substrate that has undergone the first step of a two-step process to form an ammonium silicofluoride (AFS) layer (NH4)2SiF6 on the exposed mask surfaces, sidewalls, and bottom of the recesses. In FIG. 4C, silicon oxide SiO x The Si-containing precursor is formed by a CVD method or an atomic layer deposition-like (ALD-like) method. In one example of a CVD method, a plasma is generated using a deposition gas such as SiCl4 to form the Si-containing precursor. In one example of an ALD-like method, (1) a substrate is exposed to a Si-containing precursor, and (2) the Si-containing precursor is oxidized to convert the Si-containing precursor to SiO x (3) changing the SiO x Repeating steps (1) and (2) until a certain thickness is reached at a particular point of the layer 103. In this embodiment, a conformal SiO 2 film is deposited on the mask layer 102 and on the sidewalls and bottom of the recess by the ALD method. xForm layer 103. As described below, the AFS layer (FIG. 4D) can be formed as a conformal or subconformal layer.
[0024] In the second step of forming the AFS layer 104 (FIG. 4D), SiO x The layer 103 is transformed into an AFS layer 104, which is a process that converts NH3 / NF3, H2 / N2, or SF6 / H2 / N2 gases into NH x F y A plasma is generated and then SiO x The process includes exposing the etch layer 101 to the plasma to form the AFS layer 104. The AFS layer 104 acts as a sidewall protection layer, or protective film, that protects the upper portion of the sidewall from further etching while the etching layer 101 continues to etch the recess further. The thickness of the AFS layer 104 is related to the temperature of the substrate. To avoid the AFS layer 104 becoming too thin, the substrate temperature is typically kept at 50° C., but may be higher as long as it does not exceed 100° C., at which point sublimation of the AFS begins to occur. Note that the SiO x Plasma is used to form the AFS layer 104 on the layer, and this plasma may be generated from a gas supplied into the reaction chamber 11, or may be generated outside the reaction chamber 11 (so-called remote plasma) and supplied into the reaction chamber 11.
[0025] FIG. 4E is a view of the substrate after further etching. As shown, the flat portion of the AFS layer 104 has been removed and the mask layer 102 has been etched away. Furthermore, the depth of the recess has been significantly increased as a result of the etching (i.e., by etching the bottom surface of the first portion of the etched shape formed by the initial etching of FIG. 4B to form the second portion of the recess), but the upper portion of the sidewall (first portion) is protected from bowing due to the presence of the AFS (or protective layer) on the upper portion of the sidewall. Furthermore, the AFS layer 104 is substantially immune to ion bombardment of particles at the opening OP during the etching process. The AFS is highly sublimable, and therefore is easily removed when highly electron-ionized ions impinge on it. Ions impinge on the bottom surface at an angle close to vertical (90 degrees), but impinge on the sidewall at an acute angle. Thus, the AFS on the bottom surface is easily removed, but the AFS on the sidewall is more likely to remain, because the ions impart higher energy to the bottom surface than to the sidewall.
[0026] On the other hand, AFS has high radical resistance and therefore acts as a protection for the sidewall. After the deep etching is completed, the temperature in the reaction chamber is set to more than 100° C. to sublimate the remaining part of the AFS layer 104 on the sidewall.
[0027] Although the AFS layer 104 is described as an AFS layer in this embodiment, it should be understood that the AFS layer 104 is more generally a protective layer that protects the sidewalls from lateral etching (and associated bowing) while the bottom of the recess is vertically etched away. More generally, the protective layer 104 may be formed from AFS, or from another material, and may be provided without the use of a plasma. For example, in an alternative embodiment, the protective layer 104 is formed by exposing the etch layer 101, whether made from AFS or another material, to a gas such as HF or NH3. In this alternative embodiment, the protective layer 104 is formed from SiO xA layer 103 (e.g., a SiO2 layer) is etched by gas species containing N, F, and H, resulting in the formation of a protective layer 104, e.g., made of AFS, on the sidewalls. Alternatively, when a layer containing SiN, or a multi-layer structure of SiO / SiN, for example, is etched by species containing F and H, a protective layer, e.g., made of AFS, is formed during the etching.
[0028] With respect to the protective layer 104, under conditions where the SiO2-containing layer (whether the layers are formed individually as in Figures 4A-4E or the etch layer itself is SiO2 as described below with respect to Figures 5A-5D) is exposed to reactive species such as N, F, H, etc., a protective layer of another composition may be formed in addition to the protective layer containing AFS. The other compositions may include, for example, N and Si; H and Si; N, F and Si; N, H, F and Si. SiO x A layer is also formed on the mask (e.g., the embodiment of Figs. 4A-4E), and this SiO x Under conditions where the layer is exposed to N, F, and H reactive species, an AFS layer can form on the mask, which can act as a protective layer for the mask during subsequent etching.
[0029] 5A to 5D show the progression of a substrate as it undergoes a series of processing steps according to a second embodiment. x In the first embodiment, the etching layer is made of a material other than SiO. x The etching layer is targeted. In the example shown in the second embodiment, a sub-conformal AFS (described below) is formed, but it should be understood that both embodiments can form a conformal AFS or a sub-conformal AFS. An exemplary process for forming a sub-conformal AFS in the first and second embodiments is described after the following description of Figures 5A-5D for the second embodiment.
[0030] FIG. 5A shows an etching layer 101 (e.g., SiO xFIG. 1 is a diagram of a substrate including an etching layer 101 on which a mask layer 102 is formed. An opening OP is formed in the mask layer 102, in which an etching feature (e.g., a hole or recess) will be etched with a high aspect ratio. Examples of materials used to form the mask layer 102 include carbon, metal, polysilicon, and SiO 2 , which is the etching layer 101 in this embodiment. x Other materials that have sufficient etch selectivity to .
[0031] FIG. 5B shows the etching layer 101, i.e., SiO x FIG. 2 is a diagram of the substrate after an initial etch (first portion of the recess) has been performed on the C x F y C produced from (fluorocarbon) gases w F z The etching may be performed using a (fluorocarbon) plasma. Since there is a difference in height of the mask layer 102 between Figures 5A and 5B, it can be seen that a part of the mask layer 102 has been removed. In addition, in the opening OP, the etching layer 101 is largely removed to form a second part of the recess.
[0032] 5C is a diagram of a substrate with an AFS layer 110 formed on the sidewall surface of an etched shape (a recess in this embodiment). The AFS layer 110 is formed on the sidewall surface of the recess by generating plasma (active species) from NH3 / NF3, H2 / N2, or SF6 / H2 / N2 gas. The etched layer is made of SiO x The AFS layer 110 is therefore mainly made of SiO x The AFS sub-conformal layer 110 acts as a sidewall protection layer or protective film during the subsequent recess etch.
[0033] FIG. 5D is a view of the substrate after the substrate is subsequently etched to form the bottom (second portion) of the recess. As shown, the flat portion of the mask layer 102 is reduced by etching. Furthermore, although the depth of the recess is significantly increased as a result of the etching, the upper portion of the sidewall is protected from bowing due to the presence of the AFS film 110 on the sidewall, and this portion is substantially unaffected by ion bombardment of particles at the opening OP during the etching process. As described above, the AFS on the bottom surface can be easily removed, but the AFS on the sidewall is likely to remain on the sidewall due to the geometric advantage that high-energy ions directly bombard the bottom surface but only graze the sidewall.
[0034] On the other hand, AFS has high radical resistance and therefore acts as a protection for the sidewalls. After the deep etching (one or more etchings may be performed after the AFS layer is formed), the structure is thermally annealed by setting the temperature in the reaction vessel higher than 100° C. to sublimate the remaining part of the AFS layer 110 on the sidewalls. Note that, as for the first and second embodiments, the AFS formation step and the subsequent etching step of the etching layer 101 may be repeated multiple times.
[0035] Regarding the formation of a subconformal AFS on the sidewall of the recess, two examples are given below. The first example is the first embodiment (etching layer is SiO x The second example is applicable to the first embodiment (where the etching layer is SiO x (Other than the above) and the second embodiment (etching layer is SiO x (including
[0036] As a first example of the subconformal AFS formation applied to the first embodiment, first, a subconformal SiO xA step of forming a layer is carried out. This step can be performed by (i) adjusting the area where the Si-containing precursor is adsorbed (in this example, the top and side walls of the recess) and exposing this adsorption area to oxygen plasma until the desired thickness is reached so that the bottom of the recess is not too thick, or (ii) adsorbing the Si precursor on the entire surface and shortening the time of exposure to oxygen plasma compared to (i). The effects of (i) and (ii) are that SiO 2 is formed on the side walls (and top surface) of the mask. x At the bottom of the recess, SiO x Regardless of whether process (i) or process (ii) is performed, as described above, the SiO x NH x F y Subconformal SiO x The layer is transformed to a subconformal AFS.
[0037] As a second example of subconformal AFS formation that can be applied to either the first or second embodiment, the process can be performed on a SiO x for a shorter period of time. x F y This involves controlling the exposure to plasma for a shorter period of time. x F y Examples of the exposure include (i) SiO on the bottom surface of the recess. x Before it changes to AFS, SiO x The layer was then cooled to NH x F y (ii) removing SiO 2 from the sidewalls and / or bottom surface; x The SiO layer is not converted to AFS. x NH x F y The plasma is supplied.
[0038] Example of etching conditions for etching layer 101 [Table 1]
[0039] First step (SiO x Example of processing conditions for layer formation [Table 2]
[0040] SiO x Example of processing conditions to change to AFS [Table 3]
[0041] FIG. 6 is a flow chart of a high aspect ratio etching process with an AFS protection layer formed at least on the sidewalls of the recesses, according to the present disclosure. The process can be performed according to either the first or second embodiment. Prior to the process shown in FIG. 6, a substrate is obtained with an etching layer and a mask layer with an opening OP for forming the recesses. This initial preparation results in a structure as shown in FIG. 4A or FIG. 5A. The process starts with step S1, where a partial etching is performed in the opening OP, so as to obtain a structure as shown in FIG. 4B and FIG. 5B. As a result, an upper (or first) part of the recesses is formed. The process then proceeds to step S2, where a conformal or sub-conformal AFS is formed on at least the sidewalls of the first part of the recesses, as described above. As a result, a structure as shown in FIG. 4D (conformal) and FIG. 5C (sub-conformal) is obtained. Once the AFS is formed, the process proceeds to step S3, where a further etching is performed to form a second (lower) part of the recesses (see FIG. 4E and FIG. 5D). The recess opening dimensions are maintained because there is an AFS on the recess sidewalls that protects the sidewalls from over-etching and causing bowing, a problem with conventional high aspect ratio etch processes.
[0042] Thereafter, in step S4, a determination is made as to whether additional AFS needs to be formed to further protect the sidewalls before the etching step continues. If there is an insufficient amount of AFS remaining on the sidewalls to protect them during the subsequent etching step, the process returns to step S2, where additional AFS is formed on the sidewalls. However, if it is determined in step S4 that the amount of AFS is sufficient to protect the sidewalls during further etching to the final depth, the process proceeds to step S5, where etching continues until the final depth is reached. Any remaining AFS may then be removed by heating the reaction chamber to above 100° C. to sublimate the AFS. This determination can be controlled by a computer-based process in which the number of etching steps is recorded in the recipe. This process is performed by a controller MC that knows the number of etching steps so that it can determine whether additional AFS formation is not required for the currently repeated etching step. For example, if a total of six etching steps are required to form a high aspect ratio recess, the controller MC knows the number of etching steps and can determine that (for example) one, two, or three remaining etching steps can be performed without further replenishment of AFS on the sidewalls of the hole.
[0043] FIG. 7 is a block diagram of a processing circuit for performing the operations described herein on a computer, particularly with respect to the controller MC (FIG. 2). FIG. 7 illustrates a processing circuit 130 for controlling all the control operations (e.g., process recipes), statements, or blocks of the flow chart on a computer. These control operations, statements, or blocks represent portions of code that include one or more executable instructions for performing specific logical functions or steps of a module, segment, or process. Those skilled in the art will appreciate that alternative implementations are included within the scope of the exemplary embodiments of the present disclosure, and that functions may be performed in a different order than that shown or described, such as substantially simultaneously or in reverse order, depending on the functionality involved. The various elements, features, and operations described herein may be used independently of each other or may be combined in various ways. All possible combinations and subcombinations are included within the scope of the present disclosure.
[0044] In Fig. 7, the processing circuitry 130 includes a CPU 1200 that performs one or more control processes described above / below. Processing data and instructions can be stored in memory 1202. These processing data and instructions can be stored on a storage medium disk 1204, such as a hard disk drive (HDD) or a portable storage medium, or can be stored remotely. Furthermore, the claimed disclosure is not limited by the form of computer readable medium on which the instructions for the processes according to the disclosure are stored. For example, these instructions can be stored on a CD, DVD, flash memory, RAM, ROM, PROM, EPROM, EEPROM, hard disk, or any other information processing device, such as a server or computer with which the processing circuitry 130 communicates.
[0045] Additionally, the present disclosure as claimed may be provided as a utility application, a background daemon, a component of an operating system, or any combination thereof, and may be executed in conjunction with the CPU 1200 and an operating system known to those skilled in the art, such as Microsoft Windows (registered trademark), UNIX (registered trademark), Solaris (registered trademark), LINUX (registered trademark), Apple MAC-OS, etc.
[0046] The hardware elements constituting the processing circuit 130 can be realized by various circuit elements. Furthermore, each function of the above-described embodiments can be implemented by a circuit including one or more processing circuits. As shown in FIG. 7, the processing circuit includes a specific programmed processing device, such as a processing unit (CPU) 1200. The processing circuit also includes devices such as application specific integrated circuits (ASICs) or conventional circuit components configured to implement the described functions.
[0047] In Fig. 7, the processing circuitry 130 includes a CPU 1200 that performs the above-mentioned processes. The processing circuitry 130 may be a general-purpose computer or a specific dedicated machine. In one embodiment, the processing circuitry 1200 controls the voltage and the robot arm to replace the ESC without exposing the reaction chamber to the outside atmosphere. When the processing circuitry 1200 is programmed to replace the ESC in-situ, the processing circuitry 130 functions as a specific dedicated machine.
[0048] Alternatively or additionally, CPU 1200 may be implemented on an FPGA, ASIC, PLD, or may use discrete logic circuitry, as will be appreciated by those skilled in the art. Additionally, CPU 1200 may be implemented as multiple processing devices that cooperate to execute instructions of the processes of the present invention described above in parallel.
[0049] The processing circuitry 130 of FIG. 7 also includes a network controller 1206, such as an Intel Ethernet PRO network interface card from Intel Corporation, USA, for interfacing with a network 1228. As can be appreciated, the network 1228 may be a public network, such as the Internet, a private network, such as a LAN or WAN, or any combination thereof, and may also include subordinate networks, such as PSTN or ISDN. The network 1228 may also be wired, such as an Ethernet network, or wireless, such as a cellular network, including EDGE, 3G, and 4G wireless cellular systems. The wireless network may also be Wi-Fi, Bluetooth, or any other known form of wireless communication.
[0050] The processing circuitry 130 further includes a display device controller 1208, such as a graphics card or graphics adapter, for interfacing with a display device 1210, such as a monitor. A general purpose I / O interface 1212 interfaces with a keyboard and / or mouse 1214, and a touch panel 1216, which may be integral with or separate from the display device 1210. The general purpose I / O interface is also connected to various peripheral devices 1218, such as printers and scanners.
[0051] The general purpose storage controller 1224 is connected to the storage media disk 1204 via a communication bus 1226, such as ISA, EISA, VESA, PCI, etc., and all components of the processing circuit 130 are connected to each other. The display device 1210, keyboard and / or mouse 1214, as well as the general features and functions of the display device controller 1208, storage device controller 1224, network controller 1206, audio controller 1220, and general purpose I / O interface 1212 are not described herein for the sake of brevity, as they are well known.
[0052] The exemplary circuit elements described in this disclosure may be substituted with other elements and may have different structures than the examples described herein. Additionally, circuits configured to implement the features described herein may be implemented in multiple circuit units (e.g., chips) or may combine these features as circuits in a single chipset.
[0053] The functions and features described herein may also be performed by various components distributed on the system. For example, one or more processing devices may perform these functions, where the processing devices are distributed across multiple components communicating over a network. Distributed components may include various human interface and communication devices (display monitors, smartphones, tablets, personal digital assistants (PDAs), etc.), as well as one or more client and server machines that can share processing. The network may be a private network, such as a LAN or WAN, or a public network, such as the Internet. Inputs to the system may be received by direct input by a user or remotely as real-time or batch processing. Furthermore, some of the embodiments may be implemented on modules or hardware that are not identical to those described above. Thus, other embodiments are within the scope of the claims.
[0054] Although embodiments of the subject matter of the present disclosure have been described, those skilled in the art will understand that the above is merely illustrative, not limiting, and is presented by way of example only. Thus, although certain configurations have been described herein, other configurations may be employed. Numerous modifications and other embodiments (e.g., combinations, rearrangements, etc.) are possible from the present disclosure and are within the scope of one skilled in the art and are intended to be encompassed within the scope of the subject matter of the present disclosure and any equivalents thereof. Further embodiments may be obtained by combining, rearranging, or omitting features of the embodiments of the present disclosure within the scope of the present invention. Moreover, only certain features may be advantageously used, without the corresponding use of other features. Accordingly, the applicant intends to embrace all such alternatives, modifications, equivalents, and variations that are within the spirit and scope of the subject matter of the present disclosure. [Explanation of symbols]
[0055] LLx...load lock chamber x, LM...loader module, LMR...loader robot module, LPx...load port x, MC...controller (microcontroller, local or remote computer), PMx...processing module x, R1...area, SA...substrate processing apparatus, TM...transfer module, TMR(TR)...transfer robot module, W...wafer, 11...reaction chamber, 12: plasma, 13...dielectric window, 14...lower electrode, 15...electrostatic chuck, 16, 17...high frequency power source, 18...gas source, 19...exhaust device, 20...inductive element (coil), 101...etching layer, 102, 203...mask layer, 103...SiO x Layer, 104,110…AFS layer (film)
Claims
1. 1. A method of etching a substrate, comprising: a first step of etching the substrate to form a first portion of a recess in the substrate, the first portion of the recess including a bottom surface and a sidewall; a second step of forming an ammonium fluorosilicate (AFS) layer in or on said sidewalls; a third step of etching the bottom surface while protecting the sidewall with the AFS layer to form a second portion of the recess after the second step; A method comprising:
2. 10. The method of claim 1, wherein the second and third steps are carried out at a temperature less than 100°C.
3. The method of claim 1 , wherein the second step includes forming the AFS layer on a surface of the sidewall of the first portion of the recess.
4. The second step comprises: exposing the surface of the sidewall to a Si-containing precursor to form a precursor layer on the surface of the sidewall; The precursor layer is exposed to an oxygen plasma to oxidize the precursor layer, forming a SiO 2 forming a layer; The SiO 2 exposing the layer to a plasma containing N, F, and H species; The method of claim 3 further comprising:
5. The method of claim 1 , wherein the second step includes forming the AFS layer in the sidewalls of the first portion of the recess.
6. The substrate is made of SiO 2 layer, The second step is 2 The method of claim 1 , comprising exposing the layer to a plasma containing N, F, and H species.
7. the substrate includes a mask layer having an opening; The first step comprises: etching the substrate in the openings in the mask layer; etching the bottom surface of the first portion of the recess in the opening of the mask layer; The method of claim 1 , comprising at least one of:
8. The method of claim 1 further comprising the step of repeating said second and third steps.
9. 10. The method of claim 1, further comprising a fourth step after said third step of heating said substrate to above 100°C to remove said AFS layer.
10. The substrate is made of SiO x The method of claim 1 , further comprising a stack comprising alternating layers and SiN layers.
11. The substrate is made of SiO x 10. The method of claim 1, further comprising a stack comprising alternating layers and polysilicon layers.
12. The method of claim 1 , wherein the second step and the third step are carried out in the same reaction chamber.
13. The second step is carried out in a first reaction chamber; 10. The method of claim 1, wherein the third step is carried out in a second reaction chamber, the second reaction chamber being different from the first reaction chamber.
14. The method of claim 1 , wherein the second step includes forming the AFS layer as a conformal layer covering at least the sidewalls of the first portion of the recess.
15. 2. The method of claim 1, wherein the second step includes forming the AFS layer as a subconformal layer extending along the sidewalls from a top surface of the substrate to the bottom surface of the first portion of the recess.
16. 1. A method of etching a substrate, comprising: a first step of etching the substrate to form a first portion of a recess in the substrate, the first portion of the recess including a bottom surface and a sidewall; a second step of protecting said sidewalls with an ammonium fluorosilicate (AFS) layer; a third step of etching the bottom surface to form a second portion of the recess while protecting the sidewalls with the AFS layer; A method comprising:
17. 17. The method of claim 16, wherein the second step includes protecting the sidewalls of the first portion of the recess to prevent bowing of the sidewalls of the first portion of the recess during etching of the bottom surface.
18. 1. A method of etching a substrate, comprising: a first step of etching the substrate to form a first portion of a recess in the substrate, the first portion of the recess including a bottom surface and a sidewall; a second step of forming a protective layer in or on the sidewalls comprising N, F, H, and Si; a third step of etching the bottom surface while protecting the sidewall with the protective layer to form a second portion of the recess after the second step; A method comprising:
19. a chamber in which a wafer having a substrate to be etched is placed, the substrate having a mask layer having an opening; A gas source; A plasma generator; Controller circuit and The controller circuitry comprises: controlling the gas source and the plasma generator to generate a first plasma for etching the substrate in the opening in the mask layer to form a first portion of a recess in the substrate, the first portion including a bottom surface and a sidewall; controlling the gas source and the plasma generator to generate a second plasma containing N, F, and H species to form an ammonium fluorosilicate (AFS) layer in or on the sidewall; A substrate processing apparatus configured to control the gas source and the plasma generator to generate a third plasma to further etch the bottom surface and form a second portion of the recess after the AFS layer is formed, while protecting the sidewalls of the first portion of the recess from further etching with the AFS layer.
20. The substrate is made of SiO x Including an etching layer other than The controller circuit includes: controlling the gas source to expose the sidewall to a Si-containing precursor to form a precursor layer on a surface of the sidewall; The precursor layer is exposed to an oxygen plasma to oxidize the precursor layer and deposit SiO on the sidewall. 2 Controlling the plasma generator to form a layer; SiO on the sidewall 2 20. The substrate processing apparatus of claim 19, further configured to control the gas source and the plasma generator to generate the second plasma containing N, F, and H species for transforming a layer into an ammonium fluorosilicate (AFS) layer.
21. The substrate processing apparatus of claim 19, further comprising means for forming the AFS layer as a conformal or subconformal layer.
Citation Information
Patent Citations
Vacuum processing apparatus and vacuum processing method
JP2010165954A
Substrate processing system and substrate processing method
JP2016021546A
Etching processing method
JP2017228690A
Oxide film removing method and apparatus, and contact forming method and system
JP2018148193A
Method for removing silicon oxide film
JP2019024043A