Surface-emitting semiconductor light-emitting device

The surface-emitting semiconductor light-emitting device enhances light output through a photonic crystal layer and semiconductor layer design, achieving higher light intensity by managing current density and resistance.

JP7582915B2Active Publication Date: 2024-11-13KK TOSHIBA
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
JP2021120296
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-07-21
Publication Date
2024-11-13
Estimated Expiration
2041-07-21

AI Technical Summary

Technical Problem

Surface-emitting semiconductor light-emitting devices require improved light output.

Method used

A surface-emitting semiconductor light-emitting device with a photonic crystal layer featuring a specific periodic structure and protrusions, combined with a semiconductor layer design that varies impurity concentration to manage current density and resistance, enhancing light emission efficiency.

Benefits of technology

The device achieves higher light output intensity by controlling the propagation and resonance of laser light, increasing the Q value of optical resonance and improving light emission efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007582915000001
    Figure 0007582915000001
  • Figure 0007582915000002
    Figure 0007582915000002
  • Figure 0007582915000003
    Figure 0007582915000003
Patent Text Reader

Abstract

To provide a surface emission type semiconductor light-emitting device with high optical output.SOLUTION: A surface emission type semiconductor light-emitting device comprises: first and second semiconductor layers of a first conductivity type; an active layer between the first and second semiconductor layers; and a photonic crystal layer between the active layer and the second semiconductor layer. The photonic crystal layer includes first convex parts and second convex parts, and has a first region provided with the first convex parts and a second region provided with the second convex parts and surrounding the first region. An interval between the first convex parts adjacent to each other is wider than that of the second convex parts adjacent to each other. The second semiconductor layer includes: a first layer that covers the first convex parts and the second convex parts; and a second layer provided on the first layer. The first layer includes a portion buried between the adjacent second convex parts while having the same width as the interval between the adjacent second convex parts. The second layer includes a portion buried in a space between the adjacent first convex parts while having the same width as a width of the space.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The embodiment relates to a surface-emitting semiconductor light-emitting device. [Background technology]

[0002] There is a demand for improved light output from surface-emitting semiconductor light-emitting devices. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2006-332595 A Summary of the Invention [Problem to be solved by the invention]

[0004] The embodiments provide a surface emitting semiconductor light emitting device having high light output. [Means for solving the problem]

[0005] The surface-emitting semiconductor light-emitting device according to the embodiment includes a first semiconductor layer of a first conductivity type, an active layer provided on the first semiconductor layer, a photonic crystal layer provided on the active layer, and a second semiconductor layer of the first conductivity type provided on the photonic crystal layer. The photonic crystal layer includes a plurality of convex portions arranged along an upper surface of the active layer, the plurality of convex portions including a first convex portion and a second convex portion. The photonic crystal layer has a first region in which the first convex portion is provided, and a second region in which the second convex portion is provided and surrounds the first region, and the plurality of convex portions are provided such that a distance between adjacent first convex portions is wider than a distance between adjacent second convex portions. The second semiconductor layer includes a first layer covering the first convex portion and the second convex portion, and a second layer provided on the first layer. A first conductivity type impurity concentration of the first layer is lower than a first conductivity type impurity concentration of the second layer. The first layer covers the first convex portions leaving spaces between adjacent first convex portions, and includes a portion embedded between adjacent second convex portions with a width equal to the interval between adjacent second convex portions in a direction along the top surface of the active layer, and the second layer includes a portion embedded in the space with a width equal to the width of the space between adjacent first convex portions in a direction along the top surface of the active layer. [Brief description of the drawings]

[0006] [Figure 1] 1 is a schematic cross-sectional view showing a surface-emitting semiconductor light-emitting device according to an embodiment. [Diagram 2] 1 is a schematic plan view showing a surface-emitting semiconductor light-emitting device according to an embodiment. [Diagram 3] 2 is a schematic diagram showing a photonic crystal layer of a surface-emitting semiconductor light-emitting device according to an embodiment. FIG. [Figure 4] 5A to 5C are schematic cross-sectional views showing a manufacturing process of the surface-emitting semiconductor light-emitting device according to the embodiment. [Diagram 5] 10 is a schematic cross-sectional view showing a photonic crystal layer of a surface-emitting semiconductor light-emitting device according to a modified example of the embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] Hereinafter, the embodiments will be described with reference to the drawings. The same parts in the drawings are given the same numbers, and detailed descriptions thereof will be omitted as appropriate, and different parts will be described. Note that the drawings are schematic or conceptual, and the relationship between the thickness and width of each part, the size ratio between parts, etc. are not necessarily the same as the actual ones. Even when the same parts are shown, the dimensions and ratios of each part may be different depending on the drawing.

[0008] Furthermore, the arrangement and configuration of each part will be explained using the X-axis, Y-axis, and Z-axis shown in each figure. The X-axis, Y-axis, and Z-axis are mutually perpendicular and represent the X-direction, Y-direction, and Z-direction, respectively. In addition, the Z-direction may be described as upward and the opposite direction as downward.

[0009] 1(a) and (b) are schematic cross-sectional views showing a surface-emitting semiconductor light-emitting device 1 according to an embodiment. The surface-emitting semiconductor light-emitting device 1 is, for example, a surface-emitting QCL (Quantum Cascade Laser).

[0010] 1(a), the surface-emitting semiconductor light-emitting device 1 includes a semiconductor substrate 10, a first semiconductor layer 20, an active layer 30, a photonic crystal layer 40, a second semiconductor layer 50, a third semiconductor layer 60, a front electrode 70, an insulating film 80, and a back electrode 90. The surface-emitting semiconductor light-emitting device 1 also includes a light-emitting region 100 and an outer wall region 110. The outer wall region 110 is provided to surround the light-emitting region 100 (see FIG. 2(a)).

[0011] The semiconductor substrate 10 is, for example, an n-type InP substrate. The semiconductor substrate 10 may also be an n-type GaAs substrate. In the following description, the semiconductor substrate 10 is an InP substrate. When a GaAs substrate is used, a semiconductor crystal that is lattice-matched to GaAs is used, or a buffer layer that relieves lattice mismatch between the semiconductor substrate and the semiconductor layer is provided.

[0012] The first semiconductor layer 20 is provided on the semiconductor substrate 10. The first semiconductor layer 20 is, for example, an n-type InP layer. A semiconductor crystal layer serving as a buffer layer may be provided between the semiconductor substrate 10 and the first semiconductor layer 20.

[0013] The active layer 30 is provided on the first semiconductor layer 20. The active layer 30 has, for example, a quantum well structure that causes intersubband transition of carriers. The active layer 30 includes, for example, an n-type III-V compound semiconductor crystal doped with silicon, and emits light due to the subband transition of electrons.

[0014] The active layer 30 has, for example, a quantum well structure in which quantum well layers and barrier layers are alternately stacked in a direction perpendicular to the top surface of the first semiconductor layer 20, for example, in the Z direction. The quantum well layers include, for example, InGaAs crystals, and the barrier layers include, for example, AlInAs crystals.

[0015] The photonic crystal layer 40 is provided on the active layer 30. The photonic crystal layer 40 has a particular periodic structure and controls the propagation direction of light emitted from the active layer 30. The photonic crystal layer 40 includes, for example, an InGaAs crystal.

[0016] The second semiconductor layer 50 is provided on the photonic crystal layer 40. The second semiconductor layer 50 is, for example, an n-type InP layer. The second semiconductor layer 50 has, for example, a stacked structure including a first layer 50a and a second layer 50b.

[0017] The third semiconductor layer 60 is provided on the second semiconductor layer 50. The third semiconductor layer 60 is, for example, an n-type InGaAs layer. The third semiconductor layer 60 is provided as, for example, a contact layer. The third semiconductor layer 60 reduces the contact resistance of the front surface electrode 70.

[0018] The surface electrode 70 is provided on the third semiconductor layer 60. The surface electrode 70 is provided so as to reflect light emitted from the active layer 30. This makes it possible to reverse the propagation direction of light from the active layer 30 toward the surface electrode 70 to the direction toward the semiconductor substrate 10. The surface electrode 70 contains, for example, gold (Au).

[0019] 1(a), the light emitting region 100 has a mesa structure including a first semiconductor layer 20, an active layer 30, a photonic crystal layer 40, a second semiconductor layer 50, and a third semiconductor layer 60. An insulating film 80 covers the side surface of the mesa structure. The insulating film 80 is, for example, a silicon oxide film.

[0020] Outer wall region 110 includes semiconductor layers of the same stacked structure as light emitting region 100. The mesa structure of light emitting region 100 is formed by selectively removing the semiconductor layers between light emitting region 100 and outer wall region 110.

[0021] A part of the first semiconductor layer 20 is exposed between the light emitting region 100 and the outer wall region 110. The insulating film 80 is formed so as to cover the side surface of the mesa structure of the light emitting region 100, a part of the first semiconductor layer 20, and the outer wall region 110.

[0022] The front surface electrode 70 is formed so as to cover the side surface of the mesa structure and a part of the first semiconductor layer 20 via the insulating film 80. The front surface electrode 70 is provided so as to reflect light that passes through the side surface of the mesa structure toward the outside, and return the light to the inside of the light emitting region 100.

[0023] The back electrode 90 is provided on the back surface of the semiconductor substrate 10 opposite to the light emitting region 100. The back electrode 90 has a structure in which, for example, a titanium (Ti) layer and a gold (Au) layer are laminated. The Ti layer is provided between the semiconductor substrate 10 and the Au layer.

[0024] In the surface-emitting semiconductor light-emitting device 1, carriers (electrons) are injected into the active layer 30 by passing a current between the front electrode 70 and the back electrode 90. The active layer 30 generates QCL light by stimulated emission of light generated by energy relaxation of the carriers in the quantum wells and light guided by the photonic crystal layer 40. The QCL light is radiated to the outside from the back surface of the semiconductor substrate 10. The wavelength of the QCL light is, for example, 4.5 micrometers (μm).

[0025] 1(b) is a partial cross-sectional view showing photonic crystal layer 40. Photonic crystal layer 40 has, for example, a plurality of periodically arranged protrusions 40a and 40b, and functions as a two-dimensional diffraction grating.

[0026] The plurality of protruding portions 40a are provided in the high current density region HCD. The plurality of protruding portions 40b are provided in a peripheral region PHR surrounding the high current density region HCD. The protruding portions 40a and 40b are provided in, for example, a cylindrical or triangular prism shape.

[0027] The second semiconductor layer 50 has a stacked structure including a first layer 50a and a second layer 50b, and is provided on the photonic crystal layer 40. The first layer 50a is provided between the photonic crystal layer 40 and the second layer 50b. The second layer 50b contains a first conductivity type impurity at a higher concentration than the first conductivity type impurity of the first layer 50a. The concentration of the first conductivity type impurity of the first layer 50a is, for example, 1×10 15 cm -3 The concentration of the first conductivity type impurity in the second layer 50b is, for example, 1×10 17 cm -3 That's all.

[0028] The first layer 50a is provided so as to cover the protrusions 40a and 40b of the photonic crystal layer 40. The first layer 50a covers the protrusions 40a while leaving a space between adjacent protrusions 40a. The first layer 50a also has a portion embedded between adjacent protrusions 40b. The width of the portion embedded between adjacent protrusions 40b is equal to the distance between adjacent protrusions 40b.

[0029] The second layer 50b is provided on the first layer 50a and covers the protrusions 40a and 40b. The second layer 50b has a portion embedded in the space between adjacent protrusions 40a. The width of the portion embedded in the space between adjacent protrusions 40a is equal to the width of the space between adjacent protrusions 40a.

[0030] In other words, a portion of the second semiconductor layer 50 containing a high concentration of first-conductivity-type impurities extends between adjacent convex portions 40a, and no portion containing such a high concentration of first-conductivity-type impurities is provided between adjacent convex portions 40b. Therefore, in the high current density region HCD, the electrical resistance between adjacent convex portions 40a is small. On the other hand, in the peripheral region PHR, a portion containing a low concentration of first-conductivity-type impurities is embedded between adjacent convex portions 40b, and the electrical resistance is high. As a result, the driving current of the surface-emitting semiconductor light-emitting device 1 flows mainly in the high current density region HCD, and the current flowing in the peripheral region PHR is suppressed.

[0031] Photonic crystal layer 40 functions as a two-dimensional diffraction grating due to the difference in refractive index between the material of protrusions 40a and 40b and the material of second semiconductor layer 50. Photonic crystal layer 40 has the function of selecting the resonance wavelength of laser light and controlling the emission angle of the laser light.

[0032] Photonic crystal layer 40 is provided so that laser light is emitted in a direction approximately perpendicular to the boundary between active layer 30 and first semiconductor layer 20. "Approximately perpendicular" means, for example, that the angle of the propagation direction of the laser light with respect to the boundary between active layer 30 and first semiconductor layer 20 is not less than 81° and not more than 99°.

[0033] Furthermore, light of a desired wavelength resonates in the active layer 30 according to the design of the periodic structure of the photonic crystal layer 40, resulting in laser oscillation. Furthermore, by providing the photonic crystal layer 40, a difference occurs between the carrier density in the high current density region HCD and the carrier density in the peripheral region PHR during current injection. This changes the imaginary part of the complex refractive index in the active layer 30, making it possible to increase the Q value of optical resonance. In other words, the intensity of the laser light emitted from the active layer 30 can be increased.

[0034] 2(a) and (b) are schematic plan views showing a surface-emitting semiconductor light-emitting device 1 according to an embodiment. Fig. 2(a) is a plan view showing the front side of the surface-emitting semiconductor light-emitting device 1. Fig. 2(b) is a plan view showing the back side of the surface-emitting semiconductor light-emitting device 1.

[0035] 2(a), a light emitting region 100 is provided in the center of a semiconductor substrate 10 (laser chip). A high current density region HCD is provided in the center of the light emitting region 100, and a peripheral region PHR surrounds the high current density region HCD along the outer edge of the light emitting region 100.

[0036] The semiconductor substrate 10 and the light emitting region 100 have, for example, a square shape. The shape of the light emitting region 100 is not limited to this example. The light emitting region 100 may be, for example, a circular shape. The size Lsb of the semiconductor substrate 10 is, for example, 2000 μm. The size Lmr of the light emitting region 100 is, for example, 560 μm.

[0037] The outer wall region 110 is provided to surround the light emitting region 100. The outer wall region 110 has an outer size Lpw1 of, for example, 1600 μm. The outer wall region 110 has an inner size Lpw2 of, for example, 1200 μm.

[0038] The surface electrode 70 is provided inside the outer wall region 110 and covers the light emitting region 100. The surface electrode 70 has, for example, a square planar shape. The size Lfe of the surface electrode 70 is, for example, 1000 μm.

[0039] 2(b), the back electrode 90 is provided in the shape of, for example, a square frame. The light emitting region 100 is provided on the front surface side of the semiconductor substrate 10 at a position corresponding to the center of the inside of the back electrode 90. Note that the back electrode 90 is not limited to this example. The back electrode 90 may have any shape as long as it does not block the laser light emitted from the light emitting region 100 through the back surface of the semiconductor substrate 10.

[0040] 3(a) to 3(c) are schematic diagrams showing a photonic crystal layer 40 of a surface-emitting semiconductor light emitting device 1 according to an embodiment. Fig. 3(a) is a cross-sectional view showing the photonic crystal layer 40. Fig. 3(b) is a plan view illustrating an arrangement of convex portions 40a in a high current density region HCD. Fig. 3(c) is a plan view illustrating an arrangement of convex portions 40b in a peripheral region PHR.

[0041] 3(a), the height TP of the protrusions 40a and 40b in the Z direction is, for example, 0.8 to 2 μm. In this example, TP=0.85 μm. The distance DH between adjacent protrusions 40a in the high current density region HCD is, for example, 0.1 to 0.5 μm. In this example, DH=0.45 μm. The distance DL between adjacent protrusions 40b in the peripheral region PHR is, for example, 0.2 μm.

[0042] The first layer 50a of the second semiconductor layer 50 has a layer thickness TL in the Z direction of, for example, 0.1 to 0.8 μm in the portion provided on the top of the protrusion 40a. In this example, TL=0.13 μm. As a result, the first layer 50a covers the top and side of the protrusion 40a while leaving a space between adjacent protrusions 40a. Meanwhile, the first layer 50a is embedded so as not to leave a space between adjacent protrusions 40b.

[0043] 3(b), the protrusions 40a are provided, for example, in a cylindrical shape. The interval DH between adjacent protrusions 40a is, for example, the minimum interval in the XY plane. For example, when multiple protrusions 40a are arranged at equal intervals in the X direction and the Y direction, the interval DH is the interval in the X direction and the Y direction.

[0044] 3(c), the protrusions 40b are provided, for example, in a cylindrical shape. The interval DL between adjacent protrusions 40b is, for example, the minimum interval in the XY plane. For example, when multiple protrusions 40b are arranged at equal intervals in the X direction and the Y direction, the interval DL is the interval in the X direction and the Y direction.

[0045] The multiple protrusions 40b aligned in the X and Y directions have, for example, a diagonal interval Dd in the XY plane. When the interval Dd is wider than the interval DL in the X and Y directions, it is preferable that the first layer 50a of the second semiconductor layer 50 is embedded without leaving any space between adjacent protrusions 40b even in the diagonal direction.

[0046] 4(a) to 4(c) are schematic plan views showing a process for manufacturing the surface-emitting semiconductor light emitting device 1 according to the embodiment. 4(a) to 4(c) show a process for forming the second semiconductor layer 50 on the photonic crystal layer 40.

[0047] 4(a), initial layer 50aa is formed so as to cover protrusions 40a and 40b of photonic crystal layer 40. Initial layer 50aa is formed by using, for example, molecular beam epitaxial growth (MBE growth).

[0048] In the MBE growth, a molecular beam (MB) is irradiated from, for example, a direction inclined with respect to the Z direction perpendicular to the photonic crystal layer 40. During this, the photonic crystal layer 40 is rotated, for example, in the XY plane. Therefore, the initial layer 50aa is formed on the tops and side surfaces of the protrusions 40a and 40b. The initial layer 50aa is also formed on the bottom surfaces of the protrusions 40a and 40b, leaving spaces between the adjacent protrusions 40a and 40b.

[0049] As shown in FIG. 4(b), the MBE growth is continued and the thickness of the initial layer 50aa is increased to form a first layer 50a. The first layer 50a is formed to cover the multiple protrusions 40a while leaving spaces between the adjacent protrusions 40a. Meanwhile, the first layer 50a is formed to fill the spaces between the adjacent protrusions 40b and to cover the multiple protrusions 40b. For example, the width in the X direction of the portion of the first layer 50a filled between the adjacent protrusions 40b is the same as the interval DL between the adjacent protrusions 40b.

[0050] As shown in FIG. 4(c), a second layer 50b is formed on the first layer 50a. The second layer 50b is formed, for example, by MBE growth. The second layer 50b is doped with a first conductivity type impurity at a concentration higher than that of the first layer 50a. The second layer 50b is formed to a sufficient thickness to fill the space between adjacent protrusions 40a.

[0051] 5 is a schematic cross-sectional view showing a photonic crystal layer 40 of a surface-emitting semiconductor light emitting device 2 according to a modified example of the embodiment. The arrows in the figure indicate the relative magnitudes of the currents Id1 to Id3.

[0052] As shown in Fig. 5, photonic crystal layer 40 includes protrusions 40a, 40b, and 40c. Protrusion 40a is provided in high current density region HCD. Protrusion 40b is provided in peripheral region PHR. Protrusion 40c is provided in intermediate region IMR. Intermediate region IMR is provided between high current density region HCD and peripheral region PHR. In addition, intermediate region IMR is provided to surround high current density region HCD.

[0053] In the intermediate region IMR, the multiple protrusions 40c are arranged such that the interval DM between adjacent protrusions 40c in the X direction is, for example, narrower than the interval DH between adjacent protrusions 40a and wider than the interval DL between adjacent protrusions 40c. The interval DM in the intermediate region IMR is, for example, the minimum interval between adjacent protrusions 40c.

[0054] The second semiconductor layer 50 includes a first layer 50a, a second layer 50b, and a third layer 50c. The third layer 50c is provided between the first layer 50a and the second layer 50b. The first layer 50a, the second layer 50b, and the third layer 50c include the same material, for example, InP.

[0055] The third layer 50c contains a first conductivity type impurity at a higher concentration than the first conductivity type impurity of the first layer 50a. The second layer 50b contains a first conductivity type impurity at a higher concentration than the first conductivity type impurity of the third layer 50c. The concentration of the first conductivity type impurity of the first layer 50a is, for example, 1×10 15 cm -3 The concentration of the first conductivity type impurity in the second layer 50b is, for example, less than 1×10 17 cm -3 The concentration of the first conductivity type impurity in the third layer 50c is, for example, 1×10 15 cm -3 That's it, 1×10 16 cm -3 is less than.

[0056] The first layer 50a covers the multiple protrusions 40a in the high current density region HCD, leaving a first space SP1 between adjacent protrusions 40a. The first layer 50a also covers the multiple protrusions 40c in the intermediate region IMR, leaving a second space SP2 between adjacent protrusions 40c. The first layer 50a is provided to fill the gaps between adjacent protrusions 40b, and covers the multiple protrusions 40b. The first layer 50a includes a filling portion having a width in the X direction that is the same as the interval DL between adjacent protrusions 40b.

[0057] The third layer 50c is provided on the first layer 50a. The third layer 50c covers the multiple protrusions 40a in the high current density region HCD, leaving a first space SP1 between the adjacent protrusions 40a. The third layer 50a is provided in the intermediate region IMR so as to fill in the second space SP2 between the adjacent protrusions 40c, and covers the multiple protrusions 40b and the multiple protrusions 40c.

[0058] The second layer 50b is provided on the third layer 50c. The second layer 50b is provided so as to fill the first spaces SP1 between the adjacent protrusions 40a in the high current density region HCD, and covers the multiple protrusions 40a, the multiple protrusions 40b, and the multiple protrusions 40b.

[0059] In the surface-emitting type semiconductor light-emitting device 2, the current Id1 flowing in the high current density region HCD mainly flows between the adjacent convex portions 40a in which a part of the second layer 50b is embedded. The current density of the current Id1 is higher than the current density of the current Id2 flowing in the peripheral region PHR and the current Id3 flowing in the intermediate region IMR. Since a part of the third layer 50c is embedded between the adjacent convex portions 40c, the electrical resistance of the current path in the intermediate region IMR is lower than the electrical resistance of the current path in the peripheral region PHR in which a part of the first layer 50a is embedded between the adjacent convex portions 40b. Therefore, the current density of the current Id3 in the intermediate region IMR is higher than the current density of the current Id2 in the peripheral region PHR.

[0060] Thus, in the surface-emitting semiconductor light-emitting device 2, a difference occurs between the carrier density in the high current density region HCD and the carrier density in the peripheral region PHR and intermediate region IMR during current injection. This changes the imaginary part of the complex refractive index in the active layer 30, making it possible to increase the Q value of optical resonance. In other words, the intensity of the laser light emitted from the active layer 30 can be increased.

[0061] In the above embodiment, the first layer 50a and the second layer 50b of the second semiconductor layer 50 contain the same material. However, the material of the first layer 50a and the material of the second layer 50b may be different.

[0062] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims. [Explanation of symbols]

[0063] REFERENCE SIGNS LIST 1, 2... surface-emitting semiconductor light-emitting device, 10... semiconductor substrate, 20... first semiconductor layer, 30... active layer, 40... photonic crystal layer, 40a, 40b, 40c... convex portion, 50... second semiconductor layer, 50a... first layer, 50aa... initial layer, 50b... second layer, 50c... third layer, 60... third semiconductor layer, 70... front surface electrode, 80... insulating film, 90... rear surface electrode, 100... light-emitting region, 110... outer wall region, HCD... high current density region, IMR... intermediate region, PHR... peripheral region, SP1... first space, SP2... second space

Claims

1. a first semiconductor layer of a first conductivity type; an active layer provided on the first semiconductor layer; a photonic crystal layer provided on the active layer and including a plurality of convex portions arranged along an upper surface of the active layer, the plurality of convex portions including a first convex portion and a second convex portion, the photonic crystal layer having a first region in which the first convex portions are provided and a second region in which the second convex portions are provided and surrounding the first region, the plurality of convex portions being provided such that a distance between adjacent first convex portions is wider than a distance between adjacent second convex portions; a second semiconductor layer of a first conductivity type provided on the photonic crystal layer and including a first layer covering the first convex portion and the second convex portion, and a second layer provided on the first layer, wherein a first conductivity type impurity concentration of the first layer is lower than a first conductivity type impurity concentration of the second layer, the first layer covers the first convex portion while leaving a space between adjacent first convex portions, and has a portion embedded between adjacent second convex portions with a width equal to the interval between adjacent second convex portions in a direction along the top surface of the active layer, and the second layer includes a portion embedded in the space with a width equal to the width of the space between adjacent first convex portions in a direction along the top surface of the active layer; A surface-emitting semiconductor light-emitting device comprising:

2. the photonic crystal layer further includes a third region provided between the first region and the second region, the plurality of convex portions further include third convex portions provided in the third region, wherein an interval between adjacent third convex portions is narrower than an interval between adjacent first convex portions and wider than an interval between adjacent second convex portions; 2 . The surface-emitting semiconductor light-emitting device according to claim 1 , wherein the first layer of the second semiconductor layer is provided so as to cover the third convex portions while leaving another space between the adjacent third convex portions.

3. the second semiconductor layer further includes a third layer provided between the first layer and the second layer, the third layer contains a first conductivity type impurity at a concentration higher than a first conductivity type impurity concentration of the first layer and contains the first conductivity type impurity at a concentration lower than a first conductivity type impurity concentration of the second layer; The surface-emitting semiconductor light-emitting device according to claim 2 , wherein the third layer is arranged to cover the first convex portions while leaving the space between adjacent first convex portions, and to fill the other space between adjacent third convex portions.

4. 4. The surface-emitting semiconductor light-emitting device according to claim 1, wherein the first convex portion and the second convex portion have a cylindrical or triangular prism shape.

5. the interval between adjacent first protrusions is 0.1 to 0.5 micrometers; 5. The surface-emitting semiconductor light-emitting device according to claim 1, wherein the height of the first convex portion in a direction perpendicular to the upper surface of the active layer is 0.8 to 2.0 micrometers.

Citation Information

Patent Citations

  • Manufacturing method of photonic crystal waveguide for improving lateral far field of stripe laser

    CN102142657A

  • Semiconductor face light emitting element

    JP2001308457A

  • Two-dimensional photonic crystal face emitting laser

    JP2003273456A

  • Vertical cavity surface emitting laser device

    JP2006332595A

  • Surface emitting laser element

    JP2008311625A