Polymer solution, photosensitive resin composition

A polymer solution with specific structural units and a photosensitizer enhances sensitivity and reduces yellowing and heat discoloration in photosensitive resin compositions, addressing performance limitations in liquid crystal display devices and solid-state image sensors.

JP7585658B2Active Publication Date: 2024-11-19SUMITOMO BAKELITE CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2020140688
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-04-27
Filing Date
2020-08-24
Publication Date
2024-11-19
Estimated Expiration
2040-08-24

AI Technical Summary

Technical Problem

Existing photosensitive resin compositions used for forming color filters and black matrices in liquid crystal display devices and solid-state image sensors face challenges in sensitivity, yellowing, and heat discoloration resistance, limiting their performance and productivity.

Method used

A polymer solution containing a specific polymer structure represented by general formulas (NB), (1), and (2) with thiol and alkoxy groups, along with a photosensitizer, is developed to enhance sensitivity, reduce yellowing, and improve heat resistance.

Benefits of technology

The solution provides a cured resin product with improved sensitivity, transparency, and developability, suitable for high-performance films and filters in display devices and imaging sensors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007585658000076
    Figure 0007585658000076
  • Figure 0007585658000001
    Figure 0007585658000001
  • Figure 0007585658000002
    Figure 0007585658000002
Patent Text Reader

Abstract

To provide a polymer solution which has good sensitivity and can form a resin cured product having excellent transparency with reduced yellowing and also having excellent developability.SOLUTION: The polymer solution comprises: a polymer obtained by esterification, with a hydroxy group-containing poly- and / or mono(meth)acrylate, of at least some of acid anhydride groups in a polymer comprising a structural unit represented by general formula (NB) and a structural unit derived from maleic anhydride; and a compound having a thiol group and an alkoxy group, or an oligomer thereof.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a polymer solution and a photosensitive resin composition. [Background technology]

[0002] Liquid crystal display devices and solid-state imaging devices are usually equipped with color filters and black matrices. The color filters and black matrices are configured by forming structures such as colored patterns and protective films on a substrate. Among these structures, the colored patterns and protective films are mainly formed by photolithography using a photosensitive resin composition.

[0003] Various studies have been conducted on photosensitive resin compositions, and for example, Patent Document 1 describes a photosensitive resin composition containing an alkali-soluble resin having at least a group having an acidic group and two or more different polymerizable unsaturated groups in at least a side chain, a polymerizable compound, and a photopolymerization initiator. In addition, an example of Patent Document 1 describes that a methacrylic acid / allyl methacrylate / glycidyl adduct was synthesized as the alkali-soluble resin, and used to prepare a photosensitive resin composition. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] International Publication No. 2012 / 147706 Summary of the Invention [Problem to be solved by the invention]

[0005] Photosensitive resin compositions for forming color filters and black matrices use resins that undergo a polymerization reaction and harden when exposed to light. Color filters and black matrices are produced by patterning the photosensitive resin composition through exposure and development, and then hardening the pattern.

[0006] Although "high sensitivity" seems to be a common issue for photosensitive resin compositions, higher levels of sensitivity are required due to the increasing complexity and popularity of display devices and imaging devices. The higher the sensitivity of the photosensitive resin composition, the shorter the time required for exposure, which can improve productivity. Furthermore, the cured product of the photosensitive resin composition is required to be suppressed from yellowing and to have excellent transparency and heat discoloration resistance. In Patent Document 1, there is room for improvement in these characteristics. [Means for solving the problem]

[0007] The present inventors have discovered that by improving the polymer used in the photosensitive resin composition and the formulation of the composition, it is possible to obtain a cured resin product that has good sensitivity and high resistance to heat discoloration with suppressed yellowing, and have arrived at the present invention.

[0008] According to the present invention, A structural unit represented by general formula (NB), A polymer comprising a structural unit represented by general formula (1) and at least one structural unit selected from a structural unit represented by general formula (2); and A polymer solution is provided that includes a compound having a thiol group and an alkoxy group, or an oligomer thereof. [ka] (In the general formula (NB), R 1 , R 2 , R 3 and R 4 are each independently a hydrogen atom or an organic group having 1 to 30 carbon atoms, and a1 is 0, 1 or 2. [ka] (In general formula (1), R p is a group having two or more (meth)acryloyl groups. [ka] (In general formula (2), R s is a group having one (meth)acryloyl group. According to the present invention, A photosensitive resin composition is provided that includes a polymer solution and a photosensitizer. Effect of the Invention

[0009] The polymer solution of the present invention can provide a cured resin product that has good sensitivity, reduced yellowing, excellent transparency, and excellent developability. In other words, the polymer solution of the present invention can provide a cured resin product that has a good balance of these properties. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a diagram (cross-sectional view) illustrating a schematic example of the structure of a liquid crystal display device and / or a solid-state imaging device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In all drawings, similar components are given similar symbols and their explanations are omitted as appropriate. In addition, all drawings are for explanatory purposes only. The shapes and dimensional ratios of each member in the drawings do not necessarily correspond to actual objects. In this specification, the expression "a to b" in the explanation of a numerical range means a or more and b or less, unless otherwise specified. For example, "5 to 90%" means "5% or more and 90% or less."

[0012] In the description of groups (atomic groups) in this specification, when a description is made without specifying whether the group is substituted or unsubstituted, the description includes both groups having no substituents and groups having a substituent. For example, the term "alkyl group" includes not only alkyl groups having no substituents (unsubstituted alkyl groups) but also alkyl groups having a substituent (substituted alkyl groups).

[0013] In this specification, the term "(meth)acrylic" refers to a concept that includes both acrylic and methacrylic. The same applies to similar terms such as "(meth)acrylate."

[0014] In particular, the term "(meth)acrylic group" in this specification represents a concept that encompasses an acryloyl group represented by -C(=O)-CH=CH2 and a methacryloyl group represented by -C(=O)-C(CH3)=CH2.

[0015] The polymer solution of this embodiment is A polymer P comprising a predetermined structural unit; and A compound Q having a thiol group and an alkoxy group or an oligomer thereof.

[0016] [Polymer P] The polymer P of this embodiment is A structural unit represented by the following general formula (NB), It contains at least one structural unit selected from the structural unit represented by the following general formula (1) and the structural unit represented by the following general formula (2). In other words, it contains a structural unit represented by general formula (NB) and either or both of the structural unit represented by general formula (1) and the structural unit represented by general formula (2). These structural units typically constitute the main chain of the polymer P.

[0017] [ka]

[0018] In the general formula (NB), R 1 , R 2 , R 3 and R 4 each independently represents a hydrogen atom or an organic group having 1 to 30 carbon atoms; a1 is 0, 1 or 2.

[0019] [ka]

[0020] In general formula (1), R p is a group having two or more (meth)acryloyl groups.

[0021] [ka]

[0022] In general formula (2), R s is a group having one (meth)acryloyl group.

[0023] The polymer P used in the polymer solution of this embodiment contains a structural unit represented by general formula (1) and / or a structural unit represented by general formula (2). In other words, the polymer P contains either one or both of the structural unit represented by general formula (1) and the structural unit represented by general formula (2). As a result, the photosensitive resin composition containing the polymer P has excellent sensitivity when subjected to a photolithography method. This is considered to be because the (meth)acryloyl group contained in the structural unit represented by general formula (1) or general formula (2) promotes the curing reaction (polymerization reaction). The polymer P also contains a structural unit represented by general formula (NB). This structural unit (NB) is chemically robust. Therefore, the polymer P containing this structural unit is stable with a small weight loss when subjected to a heat treatment. Therefore, the photosensitive resin composition containing the polymer P can be suitably used for producing a film or a filter for use in a liquid crystal display device or a solid-state imaging device that requires heat resistance.

[0024] In a preferred embodiment, the polymer P contains a structural unit represented by general formula (1) or a structural unit represented by general formula (2) as an essential component, and in a more preferred embodiment, the polymer P contains a structural unit represented by general formula (1) as an essential component. Since the structural unit represented by general formula (1) has at least two (meth)acryloyl groups, the polymer P containing the structural unit has higher sensitivity in photolithography processing.

[0025] In one embodiment, the polymer P may contain a structural unit represented by general formula (3) in addition to the structural units described above. By containing the structural unit represented by general formula (3), the polymer P has high alkali solubility. As a result, the photosensitive resin composition containing the polymer P has excellent developability when subjected to a photolithography process using an alkaline aqueous solution as a developer.

[0026] [ka]

[0027] In one embodiment, the polymer P may contain a structural unit represented by general formula (MA) in addition to the above structural units. The structural unit represented by general formula (MA) is ring-opened by an alkaline developer to generate two carboxyl groups. Therefore, the polymer P containing this structural unit has excellent developability. When the polymer P contains a structural unit represented by general formula (MA), the structural unit represented by general formula (MA) preferably accounts for 1 to 10 mol %, more preferably 2 to 7 mol %, of all the structural units of the polymer P.

[0028] [ka]

[0029] In the structural unit represented by the general formula (NB) constituting the polymer P, R 1 ~R 4 Examples of the organic group having 1 to 30 carbon atoms that can constitute the above group include substituted or unsubstituted, linear or branched alkyl groups having 1 to 30 carbon atoms, and more specific examples thereof include alkyl groups, alkenyl groups, alkynyl groups, alkylidene groups, aryl groups, aralkyl groups, alkaryl groups, cycloalkyl groups, alkoxy groups, heterocyclic groups, and carboxyl groups.

[0030] Examples of the alkyl group include a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, an isobutyl group, a sec-butyl group, a tert-butyl group, a pentyl group, a neopentyl group, a hexyl group, a heptyl group, an octyl group, a nonyl group, and a decyl group. Examples of the alkenyl group include an allyl group, a pentenyl group, and a vinyl group. The alkynyl group includes, for example, an ethynyl group.

[0031] Examples of the alkylidene group include a methylidene group and an ethylidene group. Examples of the aryl group include a tolyl group, a xylyl group, a phenyl group, a naphthyl group, and an anthracenyl group. Examples of the aralkyl group include a benzyl group and a phenethyl group. Examples of the alkaryl group include a tolyl group and a xylyl group. Examples of the cycloalkyl group include an adamantyl group, a cyclopentyl group, a cyclohexyl group, and a cyclooctyl group.

[0032] Examples of the alkoxy group include a methoxy group, an ethoxy group, an n-propoxy group, an isopropoxy group, an n-butoxy group, a sec-butoxy group, an isobutoxy group, a tert-butoxy group, an n-pentyloxy group, a neopentyloxy group, and an n-hexyloxy group. Examples of the heterocyclic group include an epoxy group and an oxetanyl group. In the structural unit represented by the general formula (NB), R 1 , R 2 , R 3 and R 4 is preferably hydrogen or an alkyl group, and more preferably hydrogen.

[0033] In addition, R 1 , R 2 , R 3 and R 4The hydrogen atoms in the organic group having 1 to 30 carbon atoms may be substituted with any atomic group. For example, they may be substituted with a fluorine atom, a hydroxyl group, a carboxyl group, or the like. More specifically, R 1 , R 2 , R 3 and R 4 As the organic group having 1 to 30 carbon atoms, a fluorinated alkyl group or the like may be selected. In the structural unit represented by formula (NB), a1 is preferably 0 or 1, and more preferably 0.

[0034] The proportion of the structural units represented by formula (NB) in all structural units of the polymer P is preferably from 10 to 90 mol %, more preferably from 30 to 70 mol %, and further preferably from 40 to 60 mol %.

[0035] In one embodiment, it is preferable that polymer P has either or both of a structural unit represented by general formula (1), in other words, a structural unit containing two or more (meth)acryloyl groups (-C(=O)-CH=CH2), and a structural unit represented by general formula (2), because this can further improve the sensitivity of polymer P in exposure processing.

[0036] In the structural unit represented by the general formula (1) which can constitute the polymer P, R p R is a group containing two or more (meth)acryloyl groups, preferably a group containing 2 to 6 (meth)acryloyl groups, and more preferably a group containing 3 to 5 (meth)acryloyl groups. p By optimizing the number of (meth)acryloyl groups contained in, the sensitivity of the polymer P containing the same can be further increased in exposure treatment. In addition, it becomes easier to achieve a high degree of compatibility between the sensitivity and alkali solubility of the polymer P. Furthermore, the heat resistance of the polymer P can be improved. Rp is preferably a group represented by general formula (1b) or a group represented by general formula (1c). By using such a group, the above-mentioned various effects tend to be easily obtained.

[0037] In general formula (1), Rp is preferably a group represented by general formula (1b), a group represented by general formula (1c), or a group represented by general formula (1d). By being such a group, it is easy to obtain the above-mentioned various effects.

[0038] [ka]

[0039] In general formula (1b), k is 2 or 3; R is a hydrogen atom or a methyl group, and multiple R may be the same or different.

[0040] X 1 is a single bond, an alkylene group having 1 to 6 carbon atoms, or a group represented by -ZX- (Z is -O- or -OCO-, and X is an alkylene group having 1 to 6 carbon atoms), and there are multiple X 1 may be the same or different,

[0041] X 1 ' is a single bond, an alkylene group having 1 to 6 carbon atoms, or a group represented by -X'-Z'- (X' is an alkylene group having 1 to 6 carbon atoms, and Z' is -O- or -COO-), X 2 is a k+1 valent organic group having 1 to 12 carbon atoms.

[0042] R is preferably a hydrogen atom in view of further improving sensitivity (ease of polymerization) and the like. Although k may be 2 or 3, it is preferably 3 from the viewpoints of availability of raw materials and further improvement of sensitivity.

[0043] X 1 When is an alkylene group having 1 to 6 carbon atoms, the alkylene group may be linear or branched. X 1 When X is an alkylene group having 1 to 6 carbon atoms, 1is preferably a linear alkylene group, more preferably a linear alkylene group having 1 to 3 carbon atoms, and further preferably -CH2- (methylene group).

[0044] X 1 When is a group represented by -ZX- (Z is -O- or -OCO-, and X is an alkylene group having 1 to 6 carbon atoms), the alkylene group having 1 to 6 carbon atoms of X may be linear or branched.

[0045] The alkylene group having 1 to 6 carbon atoms for X is preferably a linear alkylene group, more preferably a linear alkylene group having 1 to 3 carbon atoms, and further preferably -CH2-CH2- (ethylene group) or -CH2-CH(CH3)-. X 1 When X' is an alkylene group having 1 to 6 carbon atoms, specific embodiments thereof are the same as those of X1. X 1 When X′ is a group represented by —X′-Z′-, specific embodiments of X′ are the same as those of X described above.

[0046] X 2 The k+1 valent organic group having 1 to 12 carbon atoms can be any group obtained by removing k+1 hydrogen atoms from any organic compound. The "any organic compound" here is, for example, an organic compound having a molecular weight of 300 or less, preferably 200 or less, and more preferably 100 or less.

[0047] X 2 is, for example, a group in which k+1 hydrogen atoms have been removed from a linear or branched hydrocarbon having 1 to 12 carbon atoms (preferably 1 to 6 carbon atoms). More preferably, it is a group in which k+1 hydrogen atoms have been removed from a linear hydrocarbon having 1 to 3 carbon atoms. The hydrocarbon here may contain an oxygen atom (for example, an ether bond or a hydroxyl group). In addition, the hydrocarbon is preferably a saturated hydrocarbon.

[0048] In another embodiment, X 2may be a group containing a cyclic structure. Examples of the group containing a cyclic structure include a group containing an alicyclic structure and a group containing a heterocyclic structure (for example, an isocyanuric acid structure).

[0049] [ka]

[0050] In general formula (1c), k, R, X 1 and X 2 respectively represent R, k, X1 and X in general formula (1b). 2 wherein a plurality of R's may be the same or different, and a plurality of X's may be the same or different,

[0051] X 3 is a divalent organic group having 1 to 6 carbon atoms, X 4 and X 5 each independently represents a single bond or a divalent organic group having 1 to 6 carbon atoms, X 6 is a divalent organic group having 1 to 6 carbon atoms. R, k, X 1 and X 2 Specific embodiments, preferred embodiments, etc. of are the same as those explained for general formula (1b).

[0052] X 3 and X 6 Examples of the divalent organic group having 1 to 6 carbon atoms include a group in which two hydrogen atoms have been removed from a linear or branched hydrocarbon having 1 to 6 carbon atoms. The hydrocarbon may contain an oxygen atom (for example, an ether bond or a hydroxyl group). The hydrocarbon is preferably a saturated hydrocarbon.

[0053] X 4 and X 5The divalent organic group having 1 to 6 carbon atoms may be a linear or branched alkylene group. The linear or branched alkylene group preferably has 1 to 3 carbon atoms.

[0054] [ka]

[0055] In the general formula (1d), n is an integer of 2 to 5, and preferably 2 or 3. When polymer P contains a structural unit represented by general formula (1), the proportion of the structural unit represented by general formula (1) in all structural units of polymer P is preferably 3 to 40 mol %, more preferably 3 to 30 mol %.

[0056] In the structural unit represented by the general formula (2) which can constitute the polymer P, R S is a group containing only one (meth)acryloyl group. In particular, in the design of a normal photosensitive resin composition, when the curability is increased in order to increase the sensitivity, the curing tends to proceed too much and the developability tends to deteriorate, while when the developability is improved, the curing tends to be insufficient. Therefore, it is preferable that the polymer P contains either or both of the structural unit represented by the general formula (1) and the structural unit represented by the general formula (2), thereby achieving a good balance between the sensitivity and the developability. R S is, for example, a group represented by the following general formula (2a).

[0057] [ka]

[0058] In the general formula (2a), X 10 is a divalent organic group, and R is a hydrogen atom or a methyl group. X 10 The total number of carbon atoms is preferably 1 to 30, more preferably 1 to 20, and further preferably 1 to 10. In the general formula (2a), X10 is a divalent organic group, and R is a hydrogen atom or a methyl group. X 10 The total number of carbon atoms is preferably 1 to 30, more preferably 1 to 20, and further preferably 1 to 10.

[0059] X 10 As the divalent organic group, for example, an alkylene group is preferable. A part of -CH2- in this alkylene group may be an ether group (-O-). The alkylene group may be linear or branched, but is more preferably linear.

[0060] X 10 The divalent organic group X is more preferably a linear alkylene group having a total of 3 to 6 carbon atoms. 10 The number of carbon atoms (X 10 By appropriately selecting the chain length of the structural unit represented by general formula (2), the structural unit represented by general formula (2) can be more easily involved in the crosslinking reaction, thereby increasing the sensitivity.

[0061] X 10 The divalent organic group (for example, an alkylene group) may be substituted with any substituent, such as an alkyl group, an aryl group, an alkoxy group, or an aryloxy group.

[0062] Also, X 10 The divalent organic group may be any group other than an alkylene group, for example, a divalent group formed by linking one or more groups selected from an alkylene group, a cycloalkylene group, an arylene group, an ether group, a carbonyl group, a carboxy group, and the like.

[0063] When polymer P contains a structural unit represented by general formula (2), the proportion of the structural unit represented by general formula (2) in all structural units of polymer P is preferably 5 to 40 mol %, more preferably 10 to 30 mol %.

[0064] When polymer P contains both structural units represented by general formula (1) and structural units represented by general formula (2), the total content of structural units represented by general formula (1) and structural units represented by general formula (2) in polymer P is preferably 5 to 60 mol %, more preferably 10 to 50 mol %, and even more preferably 10 to 40 mol %, based on all structural units constituting polymer P.

[0065] The content (ratio) of each structural unit contained in polymer P can be determined by the amount (molar amount) of the raw materials used in synthesizing the polymer, the amount of the raw materials remaining after synthesis, and various spectra (e.g., IR spectrum, 1 H-NMR spectrum, 13 It can be estimated / calculated from the presence and peak area of ​​the C-NMR spectrum.

[0066] The weight average molecular weight Mw of the polymer P is, for example, 1000 to 20000, preferably 2000 to 18000, more preferably 3000 to 14000, and further preferably 3000 to 12000. By appropriately adjusting the weight average molecular weight, it is possible to adjust the sensitivity and the solubility in an alkaline developer.

[0067] The dispersity of the polymer P (weight average molecular weight Mw / number average molecular weight Mn) is preferably 1.0 to 5.0, more preferably 1.0 to 4.0, and further preferably 1.0 to 3.0. By appropriately adjusting the dispersity, the physical properties of the polymer P can be made uniform, which is preferable. These values ​​can be determined by gel permeation chromatography (GPC) measurement using polystyrene as a standard substance.

[0068] The glass transition temperature of the polymer P is preferably 150 to 250° C., more preferably 170 to 230° C. The polymer P has a relatively high glass transition temperature due to the inclusion of a structural unit represented by the general formula (NB). This is preferable in that a pattern formed on a substrate can be stably present when producing a liquid crystal display device or a solid-state imaging device. The glass transition temperature can be determined, for example, by differential thermal analysis (DTA).

[0069] (Thioether Group-Containing Polymer P1) From the viewpoint of the effects of the present invention, the polymer P of this embodiment preferably contains a thioether group-containing polymer P1. The thioether group-containing polymer P1 of this embodiment preferably has a structure represented by the following general formula (P): The structural unit A and the structural unit B in general formula (P) typically constitute the main chain of the polymer P1.

[0070] [ka]

[0071] In general formula (P), p, q and r respectively represent the molar contents of A, B and C in the polymer, and p+q+r=1. p is greater than 0, and is preferably 0.25 to 0.75. q is greater than 0, and is preferably 0.25 to 0.75. The value of r is 0 or more, and preferably 0 to 0.5. p, q or r may be the same or different for each of the n structural units in [ ]. n is an integer from 1 to 6. X is hydrogen or an organic group having 1 to 30 carbon atoms. Y is a monovalent to hexavalent organic group (i) having 1 to 30 carbon atoms derived from a difunctional or higher functional thiol group-containing compound, and is bonded to the structural unit in [ ]n via a thioether group derived from the thiol group.

[0072] A contains a structural unit represented by general formula (NB). B contains at least one structural unit selected from the structural units represented by general formula (1) and the structural units represented by general formula (2). C contains a structural unit derived from a copolymerizable compound having a double bond. A plurality of As, Bs or Cs may be the same or different. In general formula (P), the order in which A, B and C are bonded is not particularly limited, and any of A, B and C may be bonded to Y.

[0073] [ka]

[0074] In the general formula (NB), R 1 , R 2 , R 3 and R 4 each independently represents a hydrogen atom or an organic group having 1 to 30 carbon atoms; a1 is 0, 1 or 2.

[0075] [ka]

[0076] In general formula (1), R p is a group having two or more (meth)acryloyl groups.

[0077] [ka]

[0078] In general formula (2), R s is a group having one (meth)acryloyl group.

[0079] The thioether group-containing polymer P1 of this embodiment contains a structural unit represented by general formula (1) and / or a structural unit represented by general formula (2) as the structural unit B. In other words, the structural unit B contains either one or both of the structural unit represented by general formula (1) and the structural unit represented by general formula (2). This allows the photosensitive resin composition containing the thioether group-containing polymer P1 to have excellent sensitivity when subjected to a photolithography method.

[0080] This is believed to be because the (meth)acryloyl group contained in the structural unit represented by general formula (1) or general formula (2) promotes the curing reaction (polymerization reaction). The thioether group-containing polymer P1 also contains a structural unit represented by general formula (NB) as the structural unit A. This structural unit is chemically robust. Therefore, the thioether group-containing polymer P1 containing this structural unit is stable with a small weight loss when subjected to heat treatment. Therefore, the photosensitive resin composition containing the thioether group-containing polymer P1 can be suitably used for producing films and filters for use in liquid crystal displays and solid-state imaging devices that require heat resistance.

[0081] In a preferred embodiment, the thioether group-containing polymer P1 contains a structural unit represented by general formula (1) as an essential component. Since the structural unit represented by general formula (1) has at least two (meth)acryloyl groups, the (meth)acrylic resin (a) containing the structural unit has high sensitivity in photolithography processing.

[0082] In one embodiment, the thioether group-containing polymer P1 may contain, in addition to the above structural units, a structural unit represented by the general formula (3) as the structural unit B. By containing the structural unit represented by the general formula (3), the thioether group-containing polymer P1 has high alkali solubility. As a result, a photosensitive resin composition containing the thioether group-containing polymer P1 has excellent developability when subjected to a photolithography process using an alkaline aqueous solution as a developer.

[0083] In one embodiment, the thioether group-containing polymer P1 may contain a structural unit represented by the general formula (MA) as the structural unit B in addition to the above structural units. The structural unit represented by the general formula (MA) is ring-opened by an alkaline developer to generate two carboxyl groups. Therefore, the thioether group-containing polymer P1 containing this structural unit has excellent developability. When the thioether group-containing polymer P1 contains a structural unit represented by the general formula (MA), the structural unit represented by the general formula (MA) is preferably 1 to 10 mol %, more preferably 2 to 7 mol %, of all structural units of the thioether group-containing polymer P1.

[0084] In one embodiment, the thioether group-containing polymer P1 may include a divalent structural unit C derived from a copolymerizable compound having a double bond. The structural unit C includes at least one structural unit derived from, for example, substituted or unsubstituted indene, maleimide, styrene, acenaphthylene, norbornadiene, dihydrofuran, terpene compounds (e.g., pinene, limonene, etc.), linear alkenes (e.g., pentene, etc.), cyclic alkenes (cyclohexene, etc.), cyclododecatriene, tricycloundecene, dialkyl fumarates (e.g., dimethyl fumarate, ethyl fumarate, dibutyl fumarate, etc.), coumarin, (meth)acrylic acid compounds (e.g., methyl methacrylate, methyl acrylate), vinyl acetate, vinyl ethers (e.g., 2-hydroxyethyl vinyl ether, etc.), and the like. Substituents that these monomers may have include alkyl groups, aryl groups, etc. More specifically, substituted indenes include methylindene, etc. Substituted maleimides include cyclohexylmaleimide, phenylmaleimide, etc. Substituted styrenes include methylstyrene, vinyltoluene, etc.

[0085] Among these, the structural unit C preferably includes a structural unit represented by general formula (4) (a divalent structural unit derived from a substituted or unsubstituted indene), a structural unit represented by general formula (5) (a divalent structural unit derived from a substituted or unsubstituted maleimide), a structural unit represented by general formula (6) (a divalent structural unit derived from a substituted or unsubstituted styrene), or a structural unit represented by general formula (7) (a divalent structural unit derived from a substituted or unsubstituted norbornadiene).

[0086] [ka]

[0087] In the general formula (4), R 1 and R 2 Each of R independently represents a hydrogen atom, an alkyl group, or an aryl group. 3 represents a hydrogen atom, an alkyl group, or an aryl group. 4 ~R 6 Each of R independently represents a hydrogen atom, an alkyl group, or an aryl group. 7 ~R 10 each independently represents a hydrogen atom, a hydroxyl group, or an organic group having 1 to 30 carbon atoms.

[0088] In the thioether group-containing polymer P1 represented by the above general formula (P), X is hydrogen or an organic group having 1 to 30 carbon atoms. The organic group having 1 to 30 carbon atoms is the above-mentioned R 1 ~R 4 The carbon number of the organic group having 1 to 30 is the same as that of the organic group having 1 to 30 carbon atoms.

[0089] In the thioether group-containing polymer P1 represented by the above general formula (P), Y is a monovalent to hexavalent organic group (i) having 1 to 30 carbon atoms derived from a thiol group-containing compound having one or more functionalities. In this embodiment, the number of functional groups is the number of thiol groups. That is, the thiol group-containing compound contains one or more thiol groups, and the organic group (i) bonds to the structural unit in [ ]n via 1 to 6 thioether groups derived from the thiol groups. The organic group (i) may have a thiol group that is not involved in the bond with the structural unit in [ ]n, and the thioether group-containing polymer P1 can be obtained as a mixture of resins having n numbers (bond numbers) of 1 to 6. The organic group (i) having 1 to 30 carbon atoms is monofunctional or more, preferably difunctional or more, more preferably trifunctional or more. The upper limit is not particularly limited, but is 6 or less functional. The valence of the organic group (i) having 1 to 30 carbon atoms is, from the viewpoint of the effects of the present invention, monovalent to hexavalent, preferably divalent to hexavalent, and more preferably trivalent to hexavalent.

[0090] The monovalent to hexavalent organic group (i) having 1 to 30 carbon atoms may contain one or more atoms selected from O, N, S, P, and Si. Examples of the monovalent to hexavalent organic group (i) having 1 to 30 carbon atoms include alkyl groups, alkenyl groups, alkynyl groups, alkylidene groups, aryl groups, aralkyl groups, alkaryl groups, cycloalkyl groups, alkoxy groups, and heterocyclic groups each having 1 to 6 thioether groups (-S-* (* is a bond)).

[0091] Examples of alkyl groups include methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, sec-butyl, tert-butyl, pentyl, neopentyl, hexyl, heptyl, octyl, nonyl, and decyl groups. Examples of alkenyl groups include allyl, pentenyl, and vinyl groups.

[0092] Alkynyl groups include ethynyl groups. Examples of the alkylidene group include a methylidene group and an ethylidene group. Examples of the aryl group include a tolyl group, a xylyl group, a phenyl group, a naphthyl group, and an anthracenyl group. Aralkyl groups include, for example, benzyl and phenethyl groups. Examples of the alkaryl group include a tolyl group and a xylyl group.

[0093] Cycloalkyl groups include, for example, adamantyl, cyclopentyl, cyclohexyl, and cyclooctyl groups. Examples of alkoxy groups include methoxy, ethoxy, n-propoxy, isopropoxy, n-butoxy, s-butoxy, isobutoxy, t-butoxy, n-pentyloxy, neopentyloxy, and n-hexyloxy groups. Examples of the heterocyclic group include an epoxy group and an oxetanyl group.

[0094] Examples of the mono- or higher functional thiol group-containing compound include compounds represented by the following chemical formulas (s-1) to (s-23).

[0095] [ka]

[0096] [ka]

[0097] [ka]

[0098] [ka]

[0099] [ka]

[0100]

change

[0101]

change

[0102]

change

[0103]

change

[0104]

change

[0105]

change

[0106]

change

[0107]

change

[0108]

change

[0109]

change

[0110] [ka]

[0111] [ka]

[0112] [ka]

[0113] [ka]

[0114] [ka]

[0115] [ka]

[0116] [ka]

[0117] [ka]

[0118] The mono- or higher functional thiol group-containing compound may be used alone or in combination of two or more. The monovalent to hexavalent organic group (i) having 1 to 30 carbon atoms has a thioether group (-S-* (* is a bond)) derived from the thiol group of the thiol group-containing compound at its terminal, and bonds to the structural unit in [ ]n via the thioether group. The organic group (i) may have a thiol group that is not involved in the bond to the structural unit in [ ]n.

[0119] When a compound represented by the chemical formula (s-2) is used as the monofunctional or higher thiol group-containing compound, the thioether group-containing polymer P1 of this embodiment can have, for example, a structure represented by the following general formula (I).

[0120] [ka]

[0121] In the general formula (I), A, B, C, X, p, q and r have the same meanings as in the general formula (P). A, B, C, X, p, q and r contained in the structural units in the four brackets [ ] may be the same or different.

[0122] In the general formula (I), the order of bonding of A, B, and C is not particularly limited, and any of A, B, and C may be bonded to the thioether group. In addition, in the general formula (I), an example is shown in which the compound represented by the chemical formula (s-2) is bonded to the four structural units in [ ] via thioether groups derived from the four mercapto groups, but the structure may be one in which 1 to 3 structural units in [ ] are bonded. In this embodiment, the thioether group-containing polymer P1 can be obtained as a mixture containing at least one compound in which 1 to 4 structures in [ ] are bonded.

[0123] The weight average molecular weight Mw of the thioether group-containing polymer P1 is, for example, 1,000 to 15,000, preferably 1,500 to 12,000, more preferably 2,000 to 10,000, and further preferably 3,000 to 8,000. By appropriately adjusting the weight average molecular weight, it is possible to adjust the sensitivity and the solubility in an alkaline developer.

[0124] The dispersity (weight average molecular weight Mw / number average molecular weight Mn) of the thioether group-containing polymer P1 is preferably 1.0 to 5.0, more preferably 1.0 to 4.0, and even more preferably 1.0 to 3.0. By appropriately adjusting the dispersity, the physical properties of the thioether group-containing polymer P1 can be made uniform, which is preferable. These values ​​can be determined by gel permeation chromatography (GPC) measurement using polystyrene as a standard substance.

[0125] The glass transition temperature of the thioether group-containing polymer P1 is preferably 150 to 250° C., more preferably 170 to 230° C. The thioether group-containing polymer P1 has a relatively high glass transition temperature due to the inclusion of a structural unit represented by the general formula (NB). This is preferable in that a pattern formed on a substrate can be stably present in the manufacture of a liquid crystal display device or a solid-state imaging device. The glass transition temperature can be determined, for example, by differential thermal analysis (DTA).

[0126] The content (ratio) of each structural unit contained in the thioether group-containing polymer P1 of the present embodiment can be determined by the amount (molar amount) of raw materials charged during polymer synthesis, the amount of raw materials remaining after synthesis, the peak areas of various spectra (for example, 1 It can be estimated / calculated from the H-NMR peak area, etc.

[0127] (Production method of polymer P) The polymer P of this embodiment may be produced (synthesized) by any method. For example, a preparation step of preparing a raw material polymer containing a structural unit represented by the above general formula (MA) and a structural unit represented by the above general formula (2); a reaction step of reacting the raw polymer with a compound having a hydroxy group and two or more (meth)acryloyl groups in the presence of a basic catalyst; As a result, a polymer P containing a structural unit represented by the above general formula (1) and a structural unit represented by the above general formula (2) can be produced. Hereinafter, the method for producing (synthesizing) the polymer P of this embodiment through these steps will be described.

[0128] ·Preparation process The raw material polymer can typically be obtained by polymerizing (addition polymerizing) a monomer represented by the following general formula (NBm) with maleic anhydride. R in the general formula (NBm) 1 , R 2 , R 3 and R 4 The definition of a1 is the same as that in formula (NB). The same also applies to preferred embodiments.

[0129] [ka]

[0130] Examples of the monomer represented by the general formula (NBm) include norbornene, bicyclo[2.2.1]-hept-2-ene (trivial name: 2-norbornene), 5-methyl-2-norbornene, 5-ethyl-2-norbornene, 5-butyl-2-norbornene, 5-hexyl-2-norbornene, 5-decyl-2-norbornene, 5-allyl-2-norbornene, 5-(2-propenyl)-2-norbornene, 5-(1-methyl-4-pentenyl)-2-norbornene, 5-ethynyl-2-norbornene, 5-benzyl-2-norbornene, 5-phenethyl-2-norbornene, 2-acetyl-5-norbornene, methyl 5-norbornene-2-carboxylate, and 5-norbornene-2,3-dicarboxylic anhydride.

[0131] In the polymerization, the monomer represented by the general formula (NBm) may be used alone or in combination of two or more kinds. Although there is no limitation on the polymerization method, radical polymerization using a radical polymerization initiator is preferable. As the polymerization initiator, for example, an azo compound, an organic peroxide, etc. can be used.

[0132] Specific examples of the azo compound include azobisisobutyronitrile (AIBN), dimethyl 2,2'-azobis(2-methylpropionate), and 1,1'-azobis(cyclohexanecarbonitrile) (ABCN).

[0133] Examples of organic peroxides include hydrogen peroxide, di-tert-butyl peroxide (DTBP), benzoyl peroxide (benzoyl peroxide, BPO), and methyl ethyl ketone peroxide (MEKP). The polymerization initiator may be used alone or in combination of two or more kinds.

[0134] As the polymerization solvent, for example, an organic solvent such as diethyl ether, tetrahydrofuran, toluene, methyl ethyl ketone, etc. The polymerization solvent may be a single solvent or a mixed solvent.

[0135] The monomer represented by the general formula (NBm), maleic anhydride, and a polymerization initiator are dissolved in a solvent and charged into a reaction vessel, and then the mixture is heated to cause addition polymerization. The heating temperature is, for example, 50 to 80° C., and the heating time is, for example, 5 to 20 hours.

[0136] The molar ratio of the monomer represented by the general formula (NBm) to maleic anhydride when they are charged into a reaction vessel is preferably 0.5:1 to 1:0.5. From the viewpoint of controlling the molecular structure, the molar ratio is preferably 1:1. Through such a process, a "raw polymer" can be obtained.

[0137] The raw polymer may be any of random copolymers, alternating copolymers, block copolymers, and periodic copolymers. Typically, it is a random copolymer or an alternating copolymer. Maleic anhydride is generally known as a monomer with strong alternating copolymerizability. After synthesis of the raw polymer, a step of removing low molecular weight components such as unreacted monomers, oligomers, and residual polymerization initiators may be carried out.

[0138] Specifically, the organic layer containing the synthesized raw polymer and low molecular weight components is concentrated and then mixed with an organic solvent such as tetrahydrofuran (THF) to obtain a solution. This solution is then mixed with a poor solvent such as methanol to precipitate the monomer. The precipitate is filtered and dried to increase the purity of the raw polymer.

[0139] Reaction process In the presence of a basic catalyst, the above-mentioned raw polymer is reacted with a compound having a hydroxy group and two or more (meth)acryloyl groups, whereby the structural unit of general formula (MA) contained in the raw polymer is ring-opened and the structural unit of general formula (1) is formed. More specifically, first, a solution is prepared by dissolving a raw material polymer in an appropriate organic solvent.

[0140] Examples of organic solvents that can be used include single solvents or mixed solvents such as methyl ethyl ketone (MEK), propylene glycol monomethyl ether acetate (PGMEA), dimethylacetamide (DMAc), N-methylpyrrolidone (NMP), and tetrahydrofuran (THF). However, the organic solvent is not limited to these, and various organic solvents used in the synthesis of organic compounds and polymers can be used.

[0141] Next, a polyfunctional (meth)acrylic compound having a hydroxyl group is added to the above solution, and a basic catalyst is further added. Then, the solution is mixed appropriately to obtain a homogeneous solution.

[0142] Examples of the polyfunctional (meth)acrylic compound having a hydroxy group include a compound represented by the following general formula (1b-m), a compound represented by the following general formula (1c-m), or a compound represented by the following general formula (1d-m). k, R, and X in general formula (1b-m) 1 , X 1 ' and X 2 The definition and specific embodiments of are the same as those in general formula (1b). k, R, and X in general formula (1c-m) 1 , X 2 , X 3 , X 4 , X 5 and X 6 The definition and specific embodiments of are the same as those in general formula (1c). The definition of n in general formula (1d-m) is the same as that in general formula (1d).

[0143] [ka]

[0144] [ka]

[0145] [ka]

[0146] As the polyfunctional (meth)acrylic compound having a hydroxy group, those which can be preferably used are shown below. It is also possible to use the compounds shown below in which some or all of the acryloyl groups are replaced with (meth)acryloyl groups (or vice versa).

[0147] [ka]

[0148] [ka]

[0149] [ka]

[0150] [ka]

[0151] [ka]

[0152] [ka]

[0153] As the basic catalyst, amine compounds and nitrogen-containing heterocyclic compounds known in the field of organic synthesis can be appropriately used. For example, amine compounds or nitrogen-containing heterocyclic compounds such as triethylamine, pyridine, and dimethylaminopyridine can be used as catalysts. The amount of the basic catalyst used can be, for example, about 10 to 60 parts by mass per 100 parts by mass of the raw material polymer. Note that if an excessive amount of the basic catalyst is used, the amount of acid required for neutralization increases, and purification may become complicated.

[0154] The solution is heated preferably at 60 to 80° C. for about 3 to 9 hours to open the structural units of general formula (MA) contained in the raw polymer and form structural units of general formula (1).

[0155] For example, a monofunctional (meth)acrylic compound having a hydroxyl group can be added to the reaction system during the heating, thereby producing a structural unit represented by the above-mentioned general formula (2) in the polymer P.

[0156] From the viewpoint of steric hindrance of the reaction, etc., monofunctional (meth)acrylic compounds having a hydroxyl group tend to react more easily with the raw material polymer than polyfunctional (meth)acrylic compounds having a hydroxyl group. Therefore, when generating the structural unit represented by the above-mentioned general formula (2) in the polymer P, it is preferable to add the monofunctional (meth)acrylic compound having a hydroxyl group to the reaction system rather than to charge it in the reaction system from the beginning. Examples of the monofunctional (meth)acrylic compound having a hydroxy group include compounds represented by the following general formula (2a-m). In general formula (2a-m), X 10 The definition of R is the same as that in general formula (2a).

[0157] [ka]

[0158] Specific examples of the compound represented by general formula (2a-m) include 2-hydroxyethyl (meth)acrylate, 4-hydroxybutyl (meth)acrylate, 1,4-cyclohexanedimethanol mono(meth)acrylate, 2-hydroxypropyl (meth)acrylate, 2-hydroxybutyl (meth)acrylate, 2-hydroxy-3-phenoxypropyl (meth)acrylate, and 2-(meth)acryloyloxyethyl-2-hydroxyethyl-phthalic acid. After the reaction step, the reaction is stopped by diluting the reaction solution with an organic solvent and adding an acid to neutralize the basic catalyst.

[0159] The polymer P of the present embodiment can be obtained by the above steps, but the following steps may be further carried out as appropriate in order to remove unnecessary components other than the desired polymer.

[0160] First, the reaction solution diluted with an organic solvent and to which an acid (such as formic acid) has been added is vigorously stirred in a separatory funnel for at least 3 minutes. This is left to stand for 30 minutes or more to separate into an organic phase and an aqueous phase, and the aqueous phase is removed. In this way, an organic solution of the polymer is obtained.

[0161] An excess amount of toluene is added to the obtained organic solution of polymer P to reprecipitate the polymer, and the polymer powder obtained by the reprecipitation is further washed several times with toluene. The resulting organic solution of thioether group-containing (meth)acrylic resin (a) is purified using a reprecipitation method or a liquid-liquid extraction method. In the reprecipitation method, the resulting organic solution of thioether group-containing (meth)acrylic resin (a) is added to an excess amount of toluene or water to reprecipitate the polymer. The polymer powder obtained by reprecipitation is further washed several times with toluene or water. Furthermore, in order to remove formic acid and the basic catalyst, the obtained polymer powder is washed with ion-exchanged water several times (about 1 to 3 times). The polymer powder washed with ion-exchanged water is dried, for example, at 30 to 60° C. for 16 hours or more to obtain a high-purity polymer. In the liquid-liquid extraction method, water is added to the obtained organic solution of polymer P, and the solution is vigorously stirred in a separatory funnel for at least 3 minutes. This is left to stand for at least 30 minutes, and the solution is separated into an organic phase and an aqueous phase, and the aqueous phase is removed. Water is then added to the organic solution of the polymer after the water has been removed, and the solution is vigorously stirred in a separatory funnel for at least 3 minutes. This is left to stand for at least 30 minutes, and the solution is separated into an organic phase and an aqueous phase, and the aqueous phase is removed. In this way, an organic solution of the polymer is obtained. If necessary, the steps of adding water and removing the aqueous phase may be further carried out. The obtained organic solution of the polymer is concentrated by heating under reduced pressure using a rotary evaporator, and then the final solvent (PGMEA, etc.) is added to dilute the solution, and this process is repeated to obtain a solution of polymer P dissolved in the final solvent.

[0162] <Method of producing thioether group-containing polymer P1> The method for producing the thioether group-containing polymer P1 can be carried out in the same manner as in the method for producing the polymer P described above, except that in the preparation step of preparing a raw material polymer, a raw material polymer containing a structural unit represented by the above-mentioned general formula (MA), a structural unit represented by the above-mentioned general formula (NB), and the monovalent to hexavalent organic group (i) having 1 to 30 carbon atoms is prepared.

[0163] The raw material polymer can be prepared by polymerizing (addition polymerizing) a monomer composition containing a monomer represented by general formula (NBm) and maleic anhydride in the presence of the difunctional or higher functional thiol group-containing compound.

[0164] The monomer composition may contain other monomers in addition to the above monomers. The other monomer is not particularly limited as long as it is a copolymerizable compound having a double bond, and a known compound can be used, which can be polymerized with the monomer represented by the general formula (NBm) and maleic anhydride. Examples of the other monomer include substituted or unsubstituted indene, maleimide, styrene, acenaphthylene, norbornadiene, dihydrofuran, terpene compounds (e.g., pinene, limonene, etc.), linear alkenes (e.g., pentene, etc.), cyclic alkenes (cyclohexene, etc.), cyclododecatriene, tricycloundecene, dialkyl fumarates (e.g., dimethyl fumarate, ethyl fumarate, dibutyl fumarate, etc.), coumarin, (meth)acrylic acid compounds (e.g., methyl methacrylate, methyl acrylate), vinyl acetate, vinyl ethers (e.g., 2-hydroxyethyl vinyl ether, etc.), and the like. In this process, the monomer represented by the general formula (2m), maleic anhydride, and, if necessary, other monomers can be polymerized (addition polymerized) in the presence of the thiol group-containing compound having one or more functional groups.

[0165] Examples of the monofunctional or more thiol group-containing compound include, but are not limited to, the compounds represented by the above chemical formulas (s-1) to (s-23). ​​The monofunctional or more thiol group-containing compound may be used alone or in combination of two or more.

[0166] The synthesis of the raw material polymer is carried out by dissolving the monomer represented by the general formula (NBm), maleic anhydride and a polymerization initiator in a solvent and charging the solution into a reaction vessel, and then heating the mixture while dropping the monofunctional or higher thiol group-containing compound to cause addition polymerization. The heating temperature is, for example, 50 to 80°C, and the heating time is, for example, 5 to 20 hours. The "raw material polymer" can be obtained by such a process.

[0167] Next, in the same manner as in the production method of the polymer P described above, a reaction step is carried out in which the raw polymer is reacted with a compound having a hydroxy group and two or more (meth)acryloyl groups in the presence of a basic catalyst, and a washing step is appropriately carried out to obtain a thioether group-containing polymer P1.

[0168] [Compound Q having a thiol group and an alkoxy group or its oligomer] The polymer solution of this embodiment contains a polymer P and a compound Q having a thiol group and an alkoxy group or an oligomer thereof. As long as the compound Q has a thiol group and an alkoxy group, a known compound can be used as long as the effects of the present invention are achieved.

[0169] In the present embodiment, from the viewpoint of the effects of the present invention, the alkoxy group contained in compound Q is preferably an alkoxy group having 1 to 3 carbon atoms, and also preferably has a structure in which a thiol group and an alkoxy group are bonded to an organic chain which may contain one or more atoms selected from O, N, S, P, and Si. Specifically, the compound Q preferably includes a compound represented by the following general formula (a).

[0170] [ka]

[0171] In general formula (a), R each independently represents an alkoxy group having 1 to 3 carbon atoms or an alkyl group having 1 to 3 carbon atoms, and at least two R are alkoxy groups having 1 to 3 carbon atoms. L represents an m+n valent organic chain which may contain one or more atoms selected from O, N, S, P and Si.

[0172] In this embodiment, examples of the m+n valent organic chain of L include a linear or branched alkylene group (m+n:2) having 1 to 10 carbon atoms, an m+n valent group derived from a linear or branched alkane having 1 to 20 carbon atoms, and an m+n valent group derived from a substituted or unsubstituted siloxane.

[0173] X represents a single bond, or a divalent organic group which may contain a carbonyl group, a (thio)ester group or a (thio)amide group. In this embodiment, X is preferably a single bond or an alkylene ester group having 1 to 10 carbon atoms.

[0174] Q represents a single bond, or a divalent organic group which may contain a carbonyl group, a (thio)ester group, or a (thio)amide group. In this embodiment, Q is preferably a single bond or an alkylene ester group having 1 to 10 carbon atoms. The molar ratio of m:n is 1:1 to 1:8, and m+n is 2 to 20. The weight average molecular weight of the compound is 100-2,000.

[0175] Examples of compound Q include 3-mercaptopropylmethyldimethoxysilane (KBM-802, manufactured by Shin-Etsu Silicones), 3-mercaptopropyltrimethoxysilane (KBM-803, manufactured by Shin-Etsu Silicones), (3-mercaptopropyl)triethoxysilane, a siloxane chain-containing multifunctional silane coupling agent (KR-519, manufactured by Shin-Etsu Silicones), and an organic chain-containing multifunctional silane coupling agent having the following structural unit:

[0176] [ka]

[0177] In the above general formula, a:b (molar ratio) is 2:1 to 4:1. The weight average molecular weight is 1000 to 1500. * is a bond. Examples of the compound include X-12-1154 (manufactured by Shin-Etsu Silicones). The compound Q or its oligomer may be used alone or in combination of two or more kinds.

[0178] In the polymer solution of the present embodiment, the compound Q or its oligomer is present in an amount of 0.25 to 20 mass %, preferably 1.0 to 15 mass %, and more preferably 2.0 to 12 mass %, relative to the polymer P, from the viewpoint of the effects of the present invention.

[0179] [Compounds having two or more (meth)acryloyl groups (polyfunctional (meth)acrylic compounds)] The polymer solution of the present embodiment may contain a compound having two or more (meth)acryloyl groups, together with the polymer P and the compound Q or its oligomer. By containing such a compound, the alkali solubility of the polymer solution is further improved, and further yellowing of the polymer solution is further reduced, making it possible to obtain a cured product with excellent transparency.

[0180] Examples of compounds having two or more (meth)acryloyl groups (referred to as "polyfunctional (meth)acrylic compounds" in this specification) that may be used in the polymer solution of this embodiment include, but are not limited to, compounds represented by the following general formula (1b-p), compounds represented by general formula (1c-p), and compounds represented by general formula (1d-p).

[0181] k, R, and X in general formula (1b-p) 1 , X 1 ' and X 2 The definitions and specific embodiments of are the same as those in the above general formula (1b). 1 , X2 , X 3 , X 4 , X 5 and X 6 The definition and specific embodiments of are the same as those in the above general formula (1c).

[0182] In general formulae (1b-p), (1c-p) and (1d-p), Y is a hydrogen atom, a (meth)acryloyl group, or a combination thereof. The compounds in which Y is a hydrogen atom in general formula (1b-p), general formula (1c-p) and general formula (1d-p) may be unreacted monomers (i.e., compounds represented by general formula (1b-p), general formula (1c-p) and general formula (1d-p)) or may be added separately. In the general formula (1d-p), n is an integer of 2 or more, preferably an integer of 2 to 5, and more preferably an integer of 2 to 3.

[0183] [ka]

[0184] [ka]

[0185] [ka]

[0186] Specific examples of the polyfunctional (meth)acrylic compound represented by general formula (1b-p) include, but are not limited to, compounds having the following structures, in which Y represents a hydrogen atom, a (meth)acryloyl group, or a combination thereof.

[0187] [ka]

[0188] [ka]

[0189] [ka]

[0190] Specific examples of the polyfunctional (meth)acrylic compound represented by general formula (1c-p) include, but are not limited to, the following compounds.

[0191] [ka]

[0192] [ka]

[0193] [ka]

[0194] In the resin composition of the present embodiment, the polyfunctional (meth)acrylic compound is preferably blended in an amount such that the peak area derived from the polyfunctional (meth)acrylic compound in a gel permeation chromatography (GPC) chart of the resin composition is 5 to 100% of the peak area of ​​the photosensitive resin, more preferably 10 to 90%. By blending the polyfunctional (meth)acrylic compound in the above range, the resulting resin composition has excellent alkali solubility.

[0195] [Compounds having one (meth)acryloyl group] The polymer solution of this embodiment may contain a compound having one (meth)acryloyl group (referred to as a "monofunctional (meth)acrylic compound" in this specification) together with the polymer P and the compound Q or its oligomer. By containing the monofunctional (meth)acrylic compound, the alkali solubility of the resulting polymer solution is improved, and further yellowing is reduced.

[0196] Examples of the monofunctional (meth)acrylic compound that may be used in the polymer solution of the present embodiment include compounds represented by the following general formula (2a-m): The monofunctional (meth)acrylic compound may be an unreacted monomer, or may be added separately. In general formula (2a-m), X 10 The definition of R is the same as that in general formula (2a).

[0197] [ka]

[0198] Specific examples of the compound represented by general formula (2a-m) include 2-hydroxyethyl (meth)acrylate, 4-hydroxybutyl (meth)acrylate, 1,4-cyclohexanedimethanol mono(meth)acrylate, 2-hydroxypropyl (meth)acrylate, 2-hydroxybutyl (meth)acrylate, 2-hydroxy-3-phenoxypropyl (meth)acrylate, and 2-(meth)acryloyloxyethyl-2-hydroxyethyl-phthalic acid.

[0199] When the polyfunctional (meth)acrylic compound is blended in the polymer solution of this embodiment, it is blended in an amount such that the peak area attributable to the polyfunctional (meth)acrylic compound in a gel permeation chromatography (GPC) chart of the polymer solution is preferably 5 to 100%, more preferably 10 to 90%, of the peak area of ​​polymer P. By blending the polyfunctional (meth)acrylic compound in the above range, the resulting polymer solution has excellent alkali solubility.

[0200] When a monofunctional (meth)acrylic compound is blended in the polymer solution of this embodiment, the amount is preferably such that the peak area attributable to the monofunctional (meth)acrylic compound in a gel permeation chromatography (GPC) chart of the polymer solution is 5 to 50%, more preferably 10 to 35%, of the peak area of ​​polymer P. By blending the monofunctional (meth)acrylic compound in the above range, the resulting polymer solution has better alkali solubility.

[0201] <Polymer solution> The polymer solution of the present embodiment contains the above-mentioned polymer P, the above-mentioned compound Q or its oligomer, and a polyfunctional (meth)acrylic compound or a monofunctional (meth)acrylic compound added as necessary. By providing the above-mentioned configuration, the alkali dissolution rate can be, for example, 150 nm / s or more, and preferably 300 nm / s or more.

[0202] The polymer solution of the present embodiment typically contains an organic solvent and is provided in the form of a liquid or varnish. The organic solvent may be one or more of ketone-based solvents, ester-based solvents, ether-based solvents, alcohol-based solvents, lactone-based solvents, carbonate-based solvents, etc.

[0203] Specific examples of the organic solvent include propylene glycol monomethyl ether acetate, propylene glycol monomethyl ether, γ-butyrolactone, N-methylpyrrolidone, cyclohexanone, etc. These may be used alone or in combination of two or more. The amount of the organic solvent used is not particularly limited, but is used in such an amount that the concentration of the non-volatile components becomes, for example, 10 to 70% by mass, and preferably 15 to 60% by mass.

[0204] (Preparation of polymer solution) The polymer solution of the present embodiment can be prepared by mixing the above components by a known method. The polymer solution of the present embodiment is used as a resin material for the photosensitive resin composition described below.

[0205] <Photosensitive resin composition> The photosensitive resin composition of this embodiment includes the above-mentioned polymer P, the above-mentioned compound Q or its oligomer, a polyfunctional (meth)acrylic compound or a monofunctional (meth)acrylic compound added as necessary, and a photosensitizer. That is, the photosensitive resin composition of this embodiment includes the above-mentioned polymer solution (varnish, resin composition) of this embodiment and a photosensitizer. Each component will be described below.

[0206] [Photosensitizer] The photosensitizer used in the photosensitive resin composition of the present embodiment includes a photoradical polymerization initiator. As the photoradical polymerization initiator, a known compound can be used, for example, 2,2-diethoxyacetophenone, 2,2-dimethoxy-2-phenylacetophenone, 1-hydroxycyclohexyl phenyl ketone, 2-hydroxy-2-methyl-1-phenylpropan-1-one, 1-[4-(2-hydroxyethoxy)phenyl]-2-hydroxy-2-methyl-1-propan-1-one, 2-hydroxy-1-{4-[4-(2-hydroxy-2-methylpropionyl)benzyl]phenyl}-2-methyl ... -one, 2-methyl-1-(4-methylthiophenyl)-2-morpholinopropan-1-one, 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-butanone-1, 2-(dimethylamino)-2-[(4-methylphenyl)methyl]-1-[4-(4-morpholinyl)phenyl]-1-butanone and other alkylphenone compounds; benzophenone, 4,4'-bis(dimethylamino)benzophenone, 2-carboxybenzophenone and other benzophenone compounds; benzoin methyl ether, benzoin ethyl benzoin compounds such as benzoin isopropyl ether, benzoin isobutyl ether, etc.; thioxanthone compounds such as thioxanthone, 2-ethylthioxanthone, 2-isopropylthioxanthone, 2-chlorothioxanthone, 2,4-dimethylthioxanthone, 2,4-diethylthioxanthone, etc.; 2-(4-methoxyphenyl)-4,6-bis(trichloromethyl)-s-triazine, 2-(4-methoxynaphthyl)-4,6-bis(trichloromethyl)-s-triazine, 2-(4-ethoxynaphthyl)- halomethylated triazine compounds such as 4,6-bis(trichloromethyl)-s-triazine and 2-(4-ethoxycarbonylnaphthyl)-4,6-bis(trichloromethyl)-s-triazine; halomethylated oxadiazole compounds such as 2-trichloromethyl-5-(2'-benzofuryl)-1,3,4-oxadiazole, 2-trichloromethyl-5-[β-(2'-benzofuryl)vinyl]-1,3,4-oxadiazole, 4-oxadiazole, and 2-trichloromethyl-5-furyl-1,3,4-oxadiazole;Biimidazole compounds such as 2,2'-bis(2-chlorophenyl)-4,4',5,5'-tetraphenyl-1,2'-biimidazole, 2,2'-bis(2,4-dichlorophenyl)-4,4',5,5'-tetraphenyl-1,2'-biimidazole, and 2,2'-bis(2,4,6-trichlorophenyl)-4,4',5,5'-tetraphenyl-1,2'-biimidazole; 1,2-octanedione, 1-[4-(phenylthio)-2-(O-benzoyloxime)], ethanone, Examples of the photoradical polymerization initiator include oxime ester compounds such as 1-[9-ethyl-6-(2-methylbenzoyl)-9H-carbazol-3-yl]-, 1-(O-acetyloxime); titanocene compounds such as bis(η5-2,4-cyclopentadiene-1-yl)-bis(2,6-difluoro-3-(1H-pyrrol-1-yl)-phenyl)titanium; benzoic acid ester compounds such as p-dimethylaminobenzoic acid and p-diethylaminobenzoic acid; and acridine compounds such as 9-phenylacridine. The photoradical polymerization initiator may be used alone or in combination of two or more kinds. The photoradical polymerization initiator is used in an amount of, for example, 1 to 20 parts by mass, or preferably 3 to 10 parts by mass, relative to 100 parts by mass of polymer P.

[0207] The photosensitive resin composition of the present embodiment contains the above components, and thus has high sensitivity in photolithography processing and excellent alkali solubility. Therefore, the photosensitive resin composition has excellent developability and excellent processability in photolithography. In addition, since yellowing of the photosensitive resin composition is suppressed, an article obtained by curing the photosensitive resin composition has transparency.

[0208] In the photosensitive resin composition of the present embodiment, the polyfunctional (meth)acrylic compound is preferably blended in an amount such that the peak area derived from the polyfunctional (meth)acrylic compound in a gel permeation chromatography (GPC) chart of the photosensitive resin composition is 5 to 50%, more preferably 10 to 35%, of the peak area of ​​polymer P. By blending the polyfunctional (meth)acrylic compound in the above range, the obtained photosensitive resin composition has excellent alkali solubility.

[0209] The photosensitive resin composition of the present embodiment may contain a compound having one (meth)acryloyl group (monofunctional (meth)acrylic compound) in addition to the above-mentioned polymer P, polyfunctional (meth)acrylic compound, and photosensitizer. The monofunctional (meth)acrylic compound is the same as that described above. By containing the monofunctional (meth)acrylic compound, the alkali solubility of the obtained photosensitive resin composition is further improved and yellowing is reduced.

[0210] When the photosensitive resin composition of the present embodiment contains a monofunctional (meth)acrylic compound, the amount of the compound is preferably such that the peak area derived from the monofunctional (meth)acrylic compound in a gel permeation chromatography (GPC) chart of the photosensitive resin composition is 5 to 50%, more preferably 10 to 35%, of the peak area of ​​polymer P. By adding the monofunctional (meth)acrylic compound in the above range, the obtained photosensitive resin composition has excellent alkali solubility.

[0211] In one embodiment, the photosensitive resin composition may contain a colorant. By containing a colorant, the composition can be preferably used as a material for forming a color filter of a liquid crystal display device or a solid-state image sensor. As the colorant, various pigments or dyes can be used. As the pigment, an organic pigment or an inorganic pigment can be used.

[0212] Examples of organic pigments that can be used include azo pigments, phthalocyanine pigments, quinacridone pigments, perylene pigments, perinone pigments, isoindolinone pigments, isoindoline pigments, dioxazine pigments, thioindigo pigments, anthraquinone pigments, quinophthalone pigments, metal complex pigments, diketopyrrolopyrrole pigments, xanthene pigments, pyrromethene pigments, and dye lake pigments.

[0213] Examples of inorganic pigments that can be used include white pigments and extender pigments (titanium oxide, zinc oxide, zinc sulfide, clay, talc, barium sulfate, calcium carbonate, etc.), chromatic pigments (yellow lead, cadmium-based pigments, chrome vermilion, nickel titanium, chrome titanium, yellow iron oxide, red iron oxide, zinc chromate, red lead, ultramarine, Prussian blue, cobalt blue, chrome green, chromium oxide, bismuth vanadate, etc.), luster pigments (pearl pigments, aluminum pigments, bronze pigments, etc.), and fluorescent pigments (zinc sulfide, strontium sulfide, strontium aluminate, etc.).

[0214] As the dye, for example, known dyes described in JP-A-2003-270428, JP-A-9-171108, JP-A-2008-50599, etc. can be used. When the photosensitive resin composition contains a colorant, the photosensitive resin composition may contain only one type of colorant, or may contain two or more types of colorants.

[0215] Colorants (particularly pigments) having an appropriate average particle size can be used depending on the purpose and application. When transparency is required, such as in color filters, a small average particle size of 0.1 μm or less is preferred, while when hiding properties are required, such as in paints, a large average particle size of 0.5 μm or more is preferred.

[0216] Depending on the purpose and use, the colorant may be subjected to surface treatment such as rosin treatment, surfactant treatment, resin-based dispersant treatment, pigment derivative treatment, oxide film treatment, silica coating, wax coating, etc.

[0217] When the photosensitive resin composition contains a colorant, the amount of the colorant may be appropriately set depending on the purpose and use. In order to achieve a balance between the coloring concentration and the dispersion stability of the colorant, the amount of the colorant is preferably 3 to 70 mass %, more preferably 5 to 60 mass %, and even more preferably 10 to 50 mass % based on the total non-volatile components (components excluding the solvent) of the photosensitive resin composition.

[0218] In one embodiment, the photosensitive resin composition may contain a light-shielding agent. By containing a light-shielding agent, the composition can be preferably used as a material for forming a black matrix of a liquid crystal display device or a solid-state image sensor.

[0219] As the light-shielding agent, any known light-shielding agent can be used without any particular limitation. For example, black pigments such as carbon black, bone black, graphite, iron black, and titanium black can be used as the light-shielding agent. When the photosensitive resin composition contains a light-shielding agent, the photosensitive resin composition may contain only one type of light-shielding agent, or may contain two or more types of light-shielding agents.

[0220] When the photosensitive resin composition contains a light-shielding agent, the amount of the light-shielding agent may be appropriately set depending on the purpose and use. In order to achieve a balance between the light-shielding performance and the dispersion stability of the light-shielding agent, the amount of the light-shielding agent is preferably 3 to 70 mass %, more preferably 5 to 60 mass %, and even more preferably 10 to 50 mass % based on the total non-volatile components (components excluding the solvent) of the photosensitive resin composition.

[0221] The photosensitive resin composition typically contains a solvent. As the solvent, an organic solvent is preferably used. Specifically, one or more of ketone-based solvents, ester-based solvents, ether-based solvents, alcohol-based solvents, lactone-based solvents, carbonate-based solvents, etc. can be used.

[0222] Examples of solvents include propylene glycol monomethyl ether (PGME), propylene glycol monomethyl ether acetate (PGMEA), ethyl lactate, methyl isobutyl carbinol (MIBC), gamma butyrolactone (GBL), N-methylpyrrolidone (NMP), methyl-n-amyl ketone (MAK), diethylene glycol monomethyl ether, diethylene glycol dimethyl ether, diethylene glycol methyl ethyl ether, cyclohexanone, or mixtures thereof. The amount of the solvent used is not particularly limited, but is used in an amount such that the concentration of non-volatile components becomes, for example, 10 to 70% by mass, and preferably 15 to 60% by mass. In one embodiment, the photosensitive resin composition may contain a crosslinking agent.

[0223] The crosslinking agent is not particularly limited as long as it is capable of crosslinking a polymer (capable of chemically bonding with a polymer) by the action of an active chemical species generated from a photopolymerization initiator. The crosslinking agent may form a bond by reacting with itself instead of only chemically bonding with the polymer.

[0224] The crosslinking agent is preferably, for example, a polyfunctional compound having two or more polymerizable double bonds in one molecule, and more preferably a polyfunctional (meth)acrylic compound having two or more (meth)acryloyl groups in one molecule (however, the crosslinking agent does not fall under the above-mentioned polymer). It is preferable to use a crosslinking agent having the same type of crosslinking group as the crosslinking group (polymerizable double bond) of the polymer in terms of uniform curing property, further improvement of sensitivity, etc. There is no particular upper limit to the number of functions (the number of polymerizable double bonds) per molecule of the crosslinking agent, but it is, for example, 8 or less, and preferably 6 or less.

[0225] Specific examples of the crosslinking agent include the following: Ethylene glycol di(meth)acrylate, diethylene glycol di(meth)acrylate, polyethylene glycol di(meth)acrylate, propylene glycol di(meth)acrylate, butylene glycol di(meth)acrylate, hexanediol di(meth)acrylate, cyclohexanedimethanol di(meth)acrylate, bisphenol A alkylene oxide di(meth)acrylate, bisphenol F alkylene oxide di(meth)acrylate, trimethylolpropane tri(meth)acrylate, ditrimethylolpropane tetra(meth)acrylate, glycerin tri(meth)acrylate, pentaerythritol tetra(meth)acrylate, dipentaerythritol penta(meth)acrylate, dipentaerythritol hexa(meth)acrylate, ethylene oxide adduct trimethylolpropane tri(meth)acrylate, ethylene oxide adduct Polyfunctional (meth)acrylates such as ditrimethylolpropane tetra(meth)acrylate, ethylene oxide-added pentaerythritol tetra(meth)acrylate, ethylene oxide-added dipentaerythritol hexa(meth)acrylate, propylene oxide-added trimethylolpropane tri(meth)acrylate, propylene oxide-added ditrimethylolpropane tetra(meth)acrylate, propylene oxide-added pentaerythritol tetra(meth)acrylate, propylene oxide-added dipentaerythritol hexa(meth)acrylate, ε-caprolactone-added trimethylolpropane tri(meth)acrylate, ε-caprolactone-added ditrimethylolpropane tetra(meth)acrylate, ε-caprolactone-added pentaerythritol tetra(meth)acrylate, and ε-caprolactone-added dipentaerythritol hexa(meth)acrylate.

[0226] Polyfunctional vinyl ethers such as ethylene glycol divinyl ether, diethylene glycol divinyl ether, polyethylene glycol divinyl ether, propylene glycol divinyl ether, butylene glycol divinyl ether, hexanediol divinyl ether, bisphenol A alkylene oxide divinyl ether, bisphenol F alkylene oxide divinyl ether, trimethylolpropane trivinyl ether, ditrimethylolpropane tetravinyl ether, glycerin trivinyl ether, pentaerythritol tetravinyl ether, dipentaerythritol pentavinyl ether, dipentaerythritol hexavinyl ether, ethylene oxide-added trimethylolpropane trivinyl ether, ethylene oxide-added ditrimethylolpropane tetravinyl ether, ethylene oxide-added pentaerythritol tetravinyl ether, and ethylene oxide-added dipentaerythritol hexavinyl ether.

[0227] Vinyl ether group-containing (meth)acrylic acid esters such as 2-vinyloxyethyl (meth)acrylate, 3-vinyloxypropyl (meth)acrylate, 1-methyl-2-vinyloxyethyl (meth)acrylate, 2-vinyloxypropyl (meth)acrylate, 4-vinyloxybutyl (meth)acrylate, 4-vinyloxycyclohexyl (meth)acrylate, 5-vinyloxypentyl (meth)acrylate, 6-vinyloxyhexyl (meth)acrylate, 4-vinyloxymethylcyclohexylmethyl (meth)acrylate, p-vinyloxymethylphenylmethyl (meth)acrylate, 2-(vinyloxyethoxy)ethyl (meth)acrylate, and 2-(vinyloxyethoxyethoxyethoxy)ethyl (meth)acrylate.

[0228] Polyfunctional allyl ethers such as ethylene glycol diallyl ether, diethylene glycol diallyl ether, polyethylene glycol diallyl ether, propylene glycol diallyl ether, butylene glycol diallyl ether, hexanediol diallyl ether, bisphenol A alkylene oxide diallyl ether, bisphenol F alkylene oxide diallyl ether, trimethylolpropane triallyl ether, ditrimethylolpropane tetraallyl ether, glycerin triallyl ether, pentaerythritol tetraallyl ether, dipentaerythritol pentaallyl ether, dipentaerythritol hexaallyl ether, ethylene oxide-added trimethylolpropane triallyl ether, ethylene oxide-added ditrimethylolpropane tetraallyl ether, ethylene oxide-added pentaerythritol tetraallyl ether, and ethylene oxide-added dipentaerythritol hexaallyl ether. Allyl group-containing (meth)acrylic acid esters such as allyl (meth)acrylate.

[0229] Polyfunctional (meth)acryloyl group-containing isocyanurates such as tri(acryloyloxyethyl)isocyanurate, tri(methacryloyloxyethyl)isocyanurate, alkylene oxide-added tri(acryloyloxyethyl)isocyanurate, and alkylene oxide-added tri(methacryloyloxyethyl)isocyanurate. Polyfunctional allyl group-containing isocyanurates such as triallyl isocyanurate.

[0230] Polyfunctional urethane (meth)acrylates obtained by reacting polyfunctional isocyanates such as tolylene diisocyanate, isophorone diisocyanate, and xylylene diisocyanate with hydroxyl group-containing (meth)acrylic acid esters such as 2-hydroxyethyl (meth)acrylate and 2-hydroxypropyl (meth)acrylate. Polyfunctional aromatic vinyls such as divinylbenzene.

[0231] Of these, trifunctional (meth)acrylates such as trimethylolpropane tri(meth)acrylate and pentaerythritol tri(meth)acrylate, tetrafunctional (meth)acrylates such as pentaerythritol tetra(meth)acrylate and ditrimethylolpropane tetra(meth)acrylate, and hexafunctional (meth)acrylates such as dipentaerythritol hexa(meth)acrylate are preferred.

[0232] When the photosensitive resin composition contains a crosslinking agent, the photosensitive resin composition may contain only one type of crosslinking agent, or may contain two or more types. When the photosensitive resin composition contains a crosslinking agent, the amount of the crosslinking agent may be appropriately set according to the purpose and use. As an example, the amount of the crosslinking agent may be usually 30 to 70 parts by mass, preferably about 40 to 60 parts by mass, relative to 100 parts by mass of the polymer P.

[0233] The photosensitive resin composition may contain components such as a filler, a binder resin other than the above-mentioned polymer, an acid generator, a heat resistance improver, a developing aid, a plasticizer, a polymerization inhibitor, an ultraviolet absorber, an antioxidant, a matting agent, an antifoaming agent, a leveling agent, a surfactant, an antistatic agent, a dispersant, a slip agent, a surface modifier, a thixotropic agent, a thixotropic aid, a silane coupling agent, and a polyhydric phenol compound depending on various purposes and required properties.

[0234] [Films, color filters, black matrices, liquid crystal displays and solid-state imaging devices] A patterned film can be obtained by forming a film using the above-mentioned photosensitive resin composition, and then exposing and developing the film to form a pattern. This film is applied to color filters, black matrices, and the like. That is, a color filter can be obtained by forming a pattern using a photosensitive resin composition containing a colorant. Also, a black matrix can be obtained by forming a pattern using a photosensitive resin composition containing a light-shielding agent. Then, a liquid crystal display device or a solid-state imaging device equipped with a color filter or a black matrix can be manufactured. A typical procedure for forming a pattern will now be described.

[0235] (Photosensitive resin film formation) For example, the above-mentioned photosensitive resin composition is applied onto any substrate and dried as necessary to obtain a photosensitive resin film.

[0236] The substrate to which the composition is applied is not particularly limited, and examples thereof include glass substrates, silicon wafers, ceramic substrates, aluminum substrates, SiC wafers, GaN wafers, and copper-clad laminates. The substrate may be an unprocessed substrate or a substrate having electrodes or elements formed on its surface, and may be surface-treated to improve adhesion.

[0237] The method for applying the photosensitive resin composition is not particularly limited, and may be spin coating using a spinner, spray coating using a spray coater, dipping, printing, roll coating, an inkjet method, or the like.

[0238] The photosensitive resin composition applied onto the substrate is typically dried by heating using a hot plate, hot air, an oven, etc. The heating temperature is usually 80 to 140° C., and preferably 90 to 120° C. The heating time is usually 30 to 600 seconds, and preferably about 30 to 300 seconds.

[0239] The thickness of the photosensitive resin film is not particularly limited and may be adjusted appropriately depending on the pattern to be finally obtained, but is usually 0.5 to 10 μm, preferably 1 to 5 μm. The thickness can be adjusted by the content of the solvent in the photosensitive resin composition, the coating method, etc.

[0240] (exposure) Exposure is typically carried out by applying actinic rays to the photosensitive resin film through an appropriate photomask.

[0241] Examples of actinic rays include X-rays, electron beams, ultraviolet rays, and visible rays. In terms of wavelength, light of 200 to 500 nm is preferred. In terms of pattern resolution and ease of handling, the light source is preferably g-ray, h-ray, or i-ray from a mercury lamp, and particularly preferably i-ray. Two or more light rays may be mixed and used. As the exposure device, a contact aligner, a mirror projection, or a stepper is preferred. The amount of light for exposure may be appropriately adjusted depending on the amount of photosensitizer in the photosensitive resin film, but is, for example, 100 to 500 mJ / cm 2 That's about it.

[0242] After exposure, the photosensitive resin film may be heated again (post-exposure bake) if necessary. The temperature is, for example, 70 to 150° C., and preferably 90 to 120° C. The time is, for example, 30 to 600 seconds, and preferably 30 to 300 seconds. Post-exposure bake promotes the reaction caused by the radicals generated from the photoradical polymerization initiator, and further accelerates the curing reaction.

[0243] (developing) The exposed photosensitive resin film can be developed with an appropriate developer to obtain a pattern, and a substrate having a pattern can be produced.

[0244] In the development step, development can be carried out using an appropriate developer, for example, by a dipping method, a paddle method, a rotary spray method, etc. By development, the exposed area (in the case of a positive type) or the unexposed area (in the case of a negative type) of the photosensitive resin film is dissolved and removed, thereby obtaining a pattern. There is no particular limitation on the type of developer that can be used, and for example, an alkaline aqueous solution or an organic solvent can be used.

[0245] Specific examples of the alkaline aqueous solution include: (i) aqueous inorganic alkaline solutions such as sodium hydroxide, sodium carbonate, sodium silicate, and ammonia; (ii) aqueous organic amine solutions such as ethylamine, diethylamine, triethylamine, and triethanolamine; and (iii) aqueous solutions of quaternary ammonium salts such as tetramethylammonium hydroxide and tetrabutylammonium hydroxide.

[0246] Specific examples of the organic solvent include ketone-based solvents such as cyclopentanone, ester-based solvents such as propylene glycol monomethyl ether acetate (PGMEA) and butyl acetate, and ether-based solvents such as propylene glycol monomethyl ether. The developer may contain, for example, a water-soluble organic solvent such as methanol or ethanol, a surfactant, or the like.

[0247] In this embodiment, it is preferable to use an alkaline aqueous solution as the developer, and it is more preferable to use tetramethylammonium hydroxide, an aqueous sodium carbonate solution, or an aqueous potassium hydroxide solution. The concentration of the aqueous alkaline solution is preferably 0.1 to 10% by mass, and more preferably 0.5 to 5% by mass. Through the above steps, a pattern can be obtained / a substrate having a pattern can be manufactured, but various treatments may be carried out after development.

[0248] For example, after development, the pattern and the substrate may be washed with a rinse solution. Examples of the rinse solution include distilled water, methanol, ethanol, isopropanol, and propylene glycol monomethyl ether. These may be used alone or in combination of two or more.

[0249] The pattern thus obtained may be heated to be sufficiently cured. The heating temperature is typically 150 to 400°C, preferably 160 to 300°C, and more preferably 200 to 250°C. The heating time is not particularly limited, but is, for example, within the range of 15 to 300 minutes. This heat treatment can be performed using a hot plate, an oven, a temperature-programmable heating oven, or the like. The atmospheric gas used in the heat treatment may be air or an inert gas such as nitrogen or argon. Heating may also be performed under reduced pressure. FIG. 1 shows a schematic diagram of an example of the structure of a liquid crystal display device and / or a solid-state imaging device that includes a color filter and / or a black matrix.

[0250] A black matrix 11 and a color filter 12 are formed on a substrate 10. In addition, a protective film 13 and a transparent electrode layer 14 are provided on the black matrix 11 and the color filter 12.

[0251] The substrate 10 is usually made of a material that transmits light, such as glass, polyester, polycarbonate, polyolefin, polysulfone, a polymer of a cyclic olefin, etc. The substrate 10 may be subjected to a corona discharge treatment, an ozone treatment, a chemical treatment, etc., as necessary. The substrate 10 is preferably made of glass. The black matrix 11 is made of, for example, a cured product of a photosensitive resin composition containing a light-shielding agent.

[0252] There are usually three colors, red, green, and blue, for the color filter 12. The color filter 12 is made of a cured product of a photosensitive resin composition containing a coloring agent corresponding to each color.

[0253] Although the embodiments of the present invention have been described above, these are merely examples of the present invention, and various configurations other than those described above can be adopted. Furthermore, the present invention is not limited to the above-described embodiments, and modifications and improvements within the scope of the present invention are included in the present invention. EXAMPLES

[0254] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these.

[0255] The compounds used in the examples may be indicated by the following abbreviations or trade names. ·MA: Maleic anhydride ·NB: 2-Norbornene MEK: Methyl ethyl ketone ·PEMP: Pentaerythritol tetrakis(3-mercaptopropionate) 4-HBA: 4-Hydroxybutyl acrylate ·PGMEA: Propylene glycol monomethyl ether acetate KBM-803: 3-mercaptopropyltrimethoxysilane (Shin-Etsu Silicone Co., Ltd.) KBM-802: 3-mercaptopropylmethyldimethoxysilane (Shin-Etsu Silicone Co., Ltd.) X-12-1154: Organic chain-containing multifunctional silane coupling agent (Shin-Etsu Silicone Co., Ltd.) · KR-519: Polyfunctional silane coupling agent containing siloxane chains (manufactured by Shin-Etsu Silicone Co., Ltd.) KBM-3066: 1,6-bis(trimethoxysilyl)hexane (Shin-Etsu Silicone Co., Ltd.) ·KBM-3103C: Decyltrimethoxysilane (Shin-Etsu Silicone Co., Ltd.) ·KBM-5103: 3-acryloxypropyltrimethoxysilane (Shin-Etsu Silicone Co., Ltd.)

[0256] A-TMM-3LM-N: A mixture of the following two compounds. The amount of the compound on the left in the mixture based on gas chromatography is approximately 57% (manufactured by Shin-Nakamura Chemical Co., Ltd.)

[0257] [ka]

[0258] <Synthesis of raw polymer> First, a raw material polymer containing maleic anhydride structural units and 2-norbornene structural units (not containing a (meth)acryloyl group) was synthesized. Details are shown below.

[0259] (Synthesis of raw polymer 1) In a suitable sized reaction vessel equipped with a stirrer and condenser, 353.02g (3.6 mol) of maleic anhydride, 338.94g (3.6 mol) of 2-norbornene (NB), and 33.16g (0.144 mol) of dimethyl 2,2'-azobis(2-methylpropionate) were weighed out and dissolved in a mixed solvent of 1030.1g of methyl ethyl ketone and 113.0g of toluene to prepare a solution. Nitrogen was bubbled through this solution for 30 minutes to remove oxygen, and then the solution was heated at 65°C for 1.5 hours with stirring, and then further heated at 80°C for 6 hours to polymerize the maleic anhydride and 2-norbornene, producing a polymerized solution. The polymerization solution obtained above was dropped into 8519.9 g of methanol to precipitate a white solid. The obtained white solid was vacuum dried at a temperature of 120° C. to obtain 607.5 g of a polymer (raw polymer 1) having a structural unit derived from 2-norbornene and a structural unit derived from maleic anhydride. The resulting polymer was measured by gel permeation chromatography (GPC) to find that it had a weight average molecular weight Mw of 7,000 and a polydispersity (weight average molecular weight Mw) / (number average molecular weight Mn) of 1.82.

[0260] (Synthesis of raw polymer 2) In a reaction vessel equipped with a stirrer, a cooling tube, and a dropping funnel, 602.56 g of a 75% toluene solution of 2-norbornene (NB equivalent: 451.92 g, 4.8 mol), maleic anhydride (MA, 470.69 g, 4.8 mol), and 2281.74 g of methyl ethyl ketone (MEK) were added and stirred to dissolve. Next, the dissolved oxygen in the system was removed by nitrogen bubbling, and then the mixture was heated. When the internal temperature reached 80°C, a solution of 2,2'-azobisisobutyrate dimethyl (Wako Pure Chemical Industries, trade name: V-601, 44.21 g, 0.19 mol) and pentaerythritol tetrakis (3-mercaptopropionate) (PEMP, 93.82 g, 0.19 mol) dissolved in MEK 193.4 g was added over 1 hour. The mixture was then further reacted at 80°C for 7 hours. The reaction mixture was then cooled to room temperature. The polymerization solution obtained above was dropped into 3686.4 g of methanol to precipitate a white solid. The obtained white solid was washed with 3686.4 g of methanol and then vacuum dried at a temperature of 120° C. to obtain 910.1 g of a polymer (raw polymer 2) having a structural unit derived from 2-norbornene and a structural unit derived from maleic anhydride. The resulting polymer was measured by gel permeation chromatography (GPC) to find that it had a weight average molecular weight Mw of 3,500 and a polydispersity (weight average molecular weight Mw) / (number average molecular weight Mn) of 1.62.

[0261] [Confirmation of the thioether structure contained in raw polymer 2] PEMP alone, as shown in the following chemical formula: 13 By C-NMR measurement, peak a derived from carbon a was confirmed at about 19.0 ppm, and peak b derived from carbon b was confirmed at about 62.0 ppm. [ka] Raw polymer 2 synthesized using PEMP 13In the C-NMR measurement, the appearance of peak b derived from carbon b was confirmed at around 62.0 ppm. In the GPC measurement of the reaction solution, no peak of PEMP alone was observed, and no unreacted PEMP remained, confirming that PEMP was incorporated into raw material polymer 2. In addition, raw polymer 2 13 In the C-NMR measurement, the peak a derived from carbon a was not confirmed, and instead, a peak c corresponding to thioether (RS-R') appeared at about 28 ppm. The integral value of this peak c is approximately twice the integral value of peak b, so that the raw material polymer 2 has a skeleton having a thioether group as shown below, and the thiol group has disappeared. It is considered that the polymer of the example synthesized using the raw material polymer 2 also has a similar skeleton. [ka] 13 The conditions for C-NMR measurement are as follows: (Test conditions) The measurement sample was prepared by adding a measurement solvent to a weighed sample to adjust its concentration, and then pouring a specified amount into a sample tube for NMR measurement. Measurement equipment: JEOL JNM-ECA400 superconducting FT-NMR equipment ·Resonance frequency: 100.53MHz Measurement nucleus: 13 C Measurement method: NNE measurement (inverse gate decoupling method) Pulse width: 3.83μsec Pulse repetition time: 30s Number of times: 4096 ·Measurement temperature: room temperature Measurement solvent: DMSO-d6 (deuterated dimethyl sulfoxide) Sample concentration: 20% (w / v)

[0262] [Amount of sulfur in raw polymer 2] The amount of sulfur in the obtained raw polymer 2 was confirmed by flask combustion and elemental analysis by ion chromatography, and it was confirmed that elemental sulfur was present in the polymer. In addition, the peak derived from PEMP disappeared in the GPC measurement of the reaction solution before the addition of methanol, and it was confirmed that PEMP was incorporated into the polymer. As a result of elemental analysis, the sulfur content in Raw Material Polymer 2 was found to be 2.4 wt %. The elemental analysis method is as follows. -Test items Determination of total sulfur by flask combustion-ion chromatography. -Test Method Flask combustion - ion chromatography method (1) Approximately 50 mg of a sample is completely combusted in a sealed flask with oxygen replaced inside. (2) The gas generated is collected in the hydrogen peroxide absorbing solution that has already been added to the flask, and the test liquid is adjusted to 50 ml. (3) The test solution and the standard solution are introduced into the ion chromatography analyzer, the concentration of sulfate ions is determined using the calibration curve method, and the amount of sulfur contained in the sample is calculated. -Equipment used Dionex ICS-3000 ion chromatograph

[0263] [Example 1] <Preparation of polymer solution> A polymer solution 1 containing a photosensitive resin 1 (polymer P) was prepared by ring-opening the MA unit of raw material polymer 1 with a trifunctional (meth)acrylic compound, a monofunctional (meth)acrylic compound, and water. Details are described below. First, 100.30g of MEK was added to 60.00g of raw polymer 1 (0.312 moles of MA) to prepare a solution. Next, 58.12g of A-TMM-3LM-N was added to this solution, and then 18.00g (0.178 moles) of triethylamine was added and reacted at a temperature of 70°C for 2 hours. After that, 56.27g (0.390 moles) of 4-HBA was added and reacted at a temperature of 70°C for 4 hours to prepare a reaction solution. Next, 3.00 g (0.167 mol) of water was added to the resulting reaction solution without post-treatment, and the reaction was allowed to proceed at 70° C. for 2 hours. The resulting reaction solution was diluted with MEK and treated with an aqueous formic acid solution and an aqueous citric acid solution to remove the aqueous phase from the reaction solution. Liquid-liquid extraction and subsequent solvent replacement were then carried out according to the following procedure. Liquid-liquid extraction: The reaction solution was diluted with MEK, then water was added and treated to remove the aqueous phase from the reaction solution, and the same procedure was repeated once more. Solvent replacement: The resulting reaction mixture was subjected to solvent removal at 50°C under reduced pressure using a rotary evaporator. When it was confirmed that the solid content of the polymer solution was 27±2% by mass as measured by a heat-drying moisture meter, the solvent removal operation was discontinued. After that, PGMEA was added so that the solid content was 18% by mass, and mixed until uniform. The same operation was performed to remove the solvent at 50°C under reduced pressure, and the solid content was adjusted to 27±2% by mass as measured by a heat-drying moisture meter. Then, PGMEA was added so that the solid content was 18% by mass, and the operation of mixing until uniform was repeated two more times. After that, the solvent was removed or PGMEA was added so that the solid content was 30±3% by mass, and the mixture was stirred until uniform. The above operation removed the solvent used in the reaction, and the solvent was replaced with PGMEA. Next, 5% by weight of KBM-803 was mixed with the solid content of the polymer solution (resin composition) as compound Q. As a result, a photosensitive resin 1 in which the structural units derived from maleic anhydride in the raw polymer were ring-opened with A-TMM-3LM-N, 4-HBA, and water, and a polymer solution (resin composition) 1 containing residual (free) A-TMM-3LM-N, residual (free) 4-HBA, and KBM-803 as compound Q were obtained. The obtained polymer solution 1 was analyzed by gel permeation chromatography to measure the amounts of photosensitive resin 1, free polyfunctional (meth)acrylic compound, and free monofunctional (meth)acrylic compound contained in polymer solution 1, as well as the weight average molecular weight and polydispersity of photosensitive resin 1. The results are shown in Table 1. The amount of free (meth)acrylic compound is shown as the ratio (%) of the peak area of ​​the free (meth)acrylic compound to the peak area of ​​the photosensitive resin in a gel permeation chromatography (GPC) chart of the resin mixture. The measurement conditions for gel permeation chromatography are as follows. The GPC measurement device used was a Tosoh HLC-8320GPC EcoSEC. The column temperature was set to 40.0°C, and the pump flow rate was set to 0.350 mL / min. Peak position (retention time) Photosensitive resin: Peaks detected before 20 minutes (peaks with shorter retention times and larger molecular weights than A-TMM-3LM-N and 4-HBA) A-TMM-3LM-N: Sum of two peaks, 20.0-20.6 minutes and 20.6-21.5 minutes 4-HBA: 21.7 to 22.4 minutes Measurement conditions: Analysis was performed using a differential refractive index detector (RI detector).

[0264] [Alkaline dissolution rate of polymer solution] Polymer solution 1 was spin-coated onto a wafer, the PGMEA was dried, and the wafer was pre-baked at a temperature of 100° C. for 2 minutes to prepare a resin film having a thickness of about 2 μm. The resin film was immersed together with the wafer in a 2% aqueous sodium carbonate solution at 23° C. to measure the dissolution rate of the resin film. The results are shown in Table 1. The dissolution rate was calculated by visually observing the immersed wafer and measuring the time it took for the resin film to dissolve and the interference pattern to disappear, then dividing that time by the film thickness. The results are shown in Table 1. If the alkali dissolution rate is 140 nm / s or higher, it can be used without problems as a photosensitive material. In particular, if it is 300 nm / s or higher, it can be considered to be particularly good.

[0265] <Preparation of Photosensitive Resin Composition> Photosensitive resin composition 1 was obtained by dissolving the following components in PGMEA so that the total solid concentration was 30% by mass. Polymer solution 1:100 parts by weight (Here, for polymer solution 1, the solid content (total amount of the photosensitive resin, the polyfunctional (meth)acrylic compound, and the component added later) was weighed out to be 100 parts by mass. The same applies to the other polymer solutions.) Multifunctional acrylate (dipentaerythritol hexaacrylate, manufactured by Shin-Nakamura Chemical Co., Ltd., A-DPH): 50 parts by mass Photopolymerization initiator (BASF, Ingacure OXE01): 5 parts by weight Adhesion aid (KBM-403, manufactured by Shin-Etsu Chemical Co., Ltd.): 1 part by weight Surfactant (DIC Corporation, F-556): 0.5 parts by weight

[0266] [Yellow Index] The photosensitive resin composition was prepared so that the total solid content concentration was 30% by mass. The same applies to the following examples and comparative examples. The obtained photosensitive resin composition was spin-coated on Eagle XG glass (manufactured by Corning, thickness 0.5 mm) and baked on a hot plate at 100° C. for 120 seconds to obtain a thin film with a thickness of about 3.0 μm (±0.1 μm). This thin film was irradiated with 100 mJ / cm using a Canon g+h+i line mask aligner (PLA-600F). 2 The sample was exposed to g+h+i rays at an exposure dose of 1000 x 1000. After exposure, the thin film was developed in a 2.0 mass % sodium carbonate aqueous solution at 23°C for 60 seconds (immersion with the wafer), resulting in a 100 mJ / cm 2 A thin film was obtained which was exposed and developed at an exposure dose of 100 nm. The thin film was heat-treated in air at 230°C for 30 minutes. After cooling in air at room temperature, the thin film was again heat-treated in air at 230°C for 30 minutes. The same procedure was repeated, and heat treatment in air for 30 minutes was performed three times in total. The yellow index (YI) of the thin film obtained by the above method was measured three times at different measurement points using a color difference meter CR-5 (Konica Minolta), and the average value was taken as the YI value. The measurement type was transmission measurement, and uncoated Eagle XG glass (Corning, thickness 0.5 mm) was used for 100% calibration. The results are shown in Table 2. If the yellow index is 1.20 or less, the heat discoloration resistance can be considered good.

[0267] [Alkaline dissolution rate of photosensitive resin composition (2.0 mass% sodium carbonate aqueous solution)] The photosensitive resin composition was prepared so that the total solid content concentration was 30% by mass. The same applies to the following examples and comparative examples. The obtained photosensitive resin composition was spin-coated onto a wafer, the PGMEA was dried, and the wafer was pre-baked at a temperature of 100° C. for 2 minutes to prepare a resin film having a thickness of about 2 μm. This resin film was immersed together with the wafer in a 2% aqueous sodium carbonate solution at 23° C., and the dissolution rate of the resin film was measured. The dissolution rate was calculated by measuring the time it took for the resin film to dissolve and the interference pattern to disappear by visually observing the immersed wafer, and then dividing that time by the film thickness. The results are shown in Table 2.

[0268] [Sensitivity evaluation 1 of photosensitive resin composition (exposure dose at which the remaining film rate is 90% or more)] The photosensitive resin composition was prepared so that the total solid content concentration was 30% by mass. The same applies to the following examples and comparative examples. The obtained photosensitive resin composition was spin-coated on a 3-inch silicon wafer treated with HMDS (hexamethyldisilazane) and baked on a hot plate at 100° C. for 120 seconds to obtain a thin film A having a thickness of about 3.0 μm (±0.3 μm). This thin film A was irradiated with 100 mJ / cm 2 using a Canon g+h+i line mask aligner (PLA-501F) through a photomask having a gradation of light shielding rate of 1 to 100%. 2 The sample was exposed to g+h+i rays at an exposure dose of 1000 x 1000. After exposure, the thin film was developed in a 2.0 mass% sodium carbonate aqueous solution at 23°C for 60 seconds (immersion with the wafer), resulting in a light output of 1 to 100 mJ / cm. 2 Thin film B was obtained by exposure and development at each exposure dose. From the film thicknesses of Thin Film A and Thin Film B obtained by the above method, the remaining film rate was calculated according to the following formula. Remaining film rate (%) = (film thickness of thin film B at each exposure dose / film thickness of thin film A) x 100 The exposure dose at which the residual film ratio was 90% or more was determined as the sensitivity of each photosensitive resin composition. The results are shown in Table 2. The exposure dose at which the residual film ratio was 90% or more was 50 mJ / cm 2 If it is within the range below, it can be used as a photosensitive composition without any problem.

[0269] [Sensitivity evaluation 2 of photosensitive resin composition (film remaining rate after exposure at low exposure dose)] (5mJ / cm 2 (Remaining film rate at exposure dose of The photosensitive resin composition was prepared so that the total solid content concentration was 30% by mass. The same applies to the following examples and comparative examples. The obtained photosensitive resin composition was spin-coated on a 3-inch silicon wafer that had been treated with HMDS (hexamethyldisilazane), and baked on a hot plate at 100° C. for 120 seconds to obtain a thin film A having a thickness of 3.0 μm (±0.3 μm). This thin film A was irradiated with 5 mJ / cm 2 using a Canon g+h+i line mask aligner (PLA-501F) through a photomask having a gradation of light shielding rate of 1 to 100%. 2 The sample was exposed to g+h+i rays at an exposure dose of 1000 x 1000. After the exposure, the thin film was developed in a 2.0 mass % aqueous sodium carbonate solution at 23° C. for 60 seconds (immersion with the wafer) to obtain a thin film B. The remaining film ratio was calculated from the film thicknesses of Thin Film A and Thin Film B obtained by the above method using the following formula. The results are shown in Table 2. Remaining film rate (%) = (film thickness of thin film B at each exposure dose / film thickness of thin film A) x 100

[0270] [Examples 2 to 3, Comparative Examples 1 to 3] For Examples 2 to 3, the polymer solutions 2 to 6 and the photosensitive resin compositions 2 to 6 were prepared in the same manner as in Example 1, except that the type and amount of compound Q were changed as shown in Table 1, and for Comparative Examples 1 to 3, compound Q was either not added or was replaced with a compound other than compound Q (a silane coupling agent) and the amount added was changed as shown in Table 1. The results of the physical property measurements are shown in Tables 1 and 2.

[0271] [Example 4] <Preparation of polymer solution> A polymer solution 7 containing a photosensitive resin 2 (polymer P) was prepared by ring-opening the MA unit of raw material polymer 2 with a trifunctional (meth)acrylic compound, a monofunctional (meth)acrylic compound, and water. Details are described below. First, 100.30g of MEK was added to 60.00g of raw polymer 2 (0.312 moles of MA) to prepare a solution. Next, 58.12g of A-TMM-3LM-N was added to this solution, and then 18.00g (0.178 moles) of triethylamine was added and reacted at a temperature of 70°C for 2 hours. After that, 56.27g (0.390 moles) of 4-HBA was added and reacted at a temperature of 70°C for 4 hours to prepare a reaction solution. Next, 3.00 g (0.167 mol) of water was added to the resulting reaction solution without post-treatment, and the reaction was allowed to proceed at 70° C. for 2 hours. The resulting reaction solution was diluted with MEK and treated with an aqueous formic acid solution and an aqueous citric acid solution to remove the aqueous phase from the reaction solution. Liquid-liquid extraction and subsequent solvent replacement were then carried out according to the following procedure. Liquid-liquid extraction: The reaction solution was diluted with MEK, then water was added and treated to remove the aqueous phase from the reaction solution, and the same procedure was repeated once more. Solvent replacement: The resulting reaction mixture was subjected to solvent removal at 50°C under reduced pressure using a rotary evaporator. When it was confirmed that the solid content of the polymer solution was 27±2% by mass as measured by a heat-drying moisture meter, the solvent removal operation was discontinued. After that, PGMEA was added so that the solid content was 18% by mass, and mixed until uniform. The same operation was performed to remove the solvent at 50°C under reduced pressure, and the solid content was adjusted to 27±2% by mass as measured by a heat-drying moisture meter. Then, PGMEA was added so that the solid content was 18% by mass, and the operation of mixing until uniform was repeated two more times. After that, the solvent was removed or PGMEA was added so that the solid content was 30±3% by mass, and the mixture was stirred until uniform. The above operation removed the solvent used in the reaction, and the solvent was replaced with PGMEA. Next, 2% by weight of KBM-803 was mixed with the solid content of the polymer solution (resin composition) as compound Q. As a result, a photosensitive resin 2 in which the structural units derived from maleic anhydride in the raw polymer were ring-opened with A-TMM-3LM-N, 4-HBA, and water, and a polymer solution (resin composition) 7 containing residual (free) A-TMM-3LM-N, residual (free) 4-HBA, and KBM-803 as compound Q were obtained. The obtained polymer solution 7 was analyzed by gel permeation chromatography to measure the amounts of photosensitive resin 2, free polyfunctional (meth)acrylic compound, and free monofunctional (meth)acrylic compound contained in polymer solution 7, as well as the weight average molecular weight and polydispersity of the photosensitive resin. The results are shown in Table 1. The amount of free (meth)acrylic compound is shown as the ratio (%) of the peak area of ​​the free (meth)acrylic compound to the peak area of ​​the photosensitive resin in a gel permeation chromatography (GPC) chart of the resin mixture. The measurement conditions for gel permeation chromatography are as follows. The GPC measurement device used was a Tosoh HLC-8320GPC EcoSEC. The column temperature was set to 40.0°C, and the pump flow rate was set to 0.350 mL / min. Peak position (retention time) Photosensitive resin: Peaks detected before 20 minutes (peaks with shorter retention times and larger molecular weights than A-TMM-3LM-N and 4-HBA) A-TMM-3LM-N: Sum of two peaks, 20.0-20.6 minutes and 20.6-21.5 minutes 4-HBA: 21.7 to 22.4 minutes Measurement conditions: Analysis was performed using a differential refractive index detector (RI detector). The physical property measurement results are shown in Table 1.

[0272] <Preparation of Photosensitive Resin Composition> Photosensitive resin composition 7 was obtained by dissolving the following components in PGMEA so that the total solids concentration was 30% by mass. Polymer solution 7: 100 parts by weight (Here, the polymer solution 7 was weighed so that the solid content (the total amount of the photosensitive resin, the polyfunctional (meth)acrylic compound, and the components added later) was 100 parts by mass.) Multifunctional acrylate (dipentaerythritol hexaacrylate, manufactured by Shin-Nakamura Chemical Co., Ltd., A-DPH): 50 parts by mass Photopolymerization initiator (BASF, Ingacure OXE01): 5 parts by weight Adhesion aid (KBM-403, manufactured by Shin-Etsu Chemical Co., Ltd.): 1 part by weight Surfactant (DIC Corporation, F-556): 0.5 parts by weight The physical property measurement results are shown in Tables 1 and 2.

[0273] [Example 5, Comparative Examples 4 to 10] Example 5 was prepared in the same manner as Example 4, except that the type and amount of compound Q were changed as shown in Table 1, and Comparative Examples 4 to 10 were prepared in the same manner as Example 4, except that compound Q was not added or was replaced with a compound other than compound Q (a silane coupling agent) and the amount added was changed as shown in Table 1. The results of measuring the physical properties are shown in Tables 1 and 2.

[0274] [Comparative Examples 11 to 17] Photosensitive resin 3 (polymer P) was prepared in the same manner as in Example 1, using 38.75 g of A-TMM-3LM-N and 99.71 g of MEK. Polymer solutions 16 to 22 and photosensitive resin compositions 16 to 22 were prepared in the same manner as in Example 1, except that compound Q was either not added or was replaced with a compound other than compound Q (a sulfide compound or a thiol compound) and the amount added was changed as shown in Table 1. The results of measuring the physical properties are shown in Tables 1 and 2.

[0275] [Example 6, Comparative Example 18] A photosensitive resin 4 (polymer P) was prepared by ring-opening the MA unit of raw material polymer 1 with a monofunctional (meth)acrylic compound. The details are described below. First, 18.44 g of MEK was added to 10.00 g of raw polymer 1 (0.052 mol in terms of MA) to prepare a solution. Next, 9.38 g (0.065 mol) of 4-HBA was added to this solution, and then 3.00 g (0.030 mol) of triethylamine was added. The mixture was reacted at a temperature of 70° C. for 6 hours to prepare a reaction solution. The resulting reaction solution was diluted with MEK and treated with an aqueous citric acid solution to remove the aqueous phase from the reaction solution. The polymer was then purified by the following procedure. The polymer was reprecipitated with an excess amount of water. The polymer powder obtained by reprecipitation was washed with an excess amount of water twice. The reaction product was dried at 40°C for 12 hours. The polymer obtained was dissolved in propylene glycol monomethyl ether acetate (PGMEA) to prepare a solution with a solid content concentration of 30 mass%, and photosensitive resin 4 (polymer P) was prepared. Polymer solutions 23 to 24 and photosensitive resin compositions 23 to 24 were prepared in the same manner as in Example 1, except that either compound Q was added as in Example 1 or no compound was added. The results of measuring the physical properties are shown in Tables 1 and 2.

[0276] [Table 1]

[0277] [Table 2]

[0278] As shown in Table 2, Examples 1 to 3 in which "compound Q having a thiol group and an alkoxy group" was added to Comparative Example 1 (no chain transfer agent in the polymer chain, molar ratio of polyfunctional acrylate to maleic anhydride: 0.375) had a low yellow index and excellent transparency, and 2 However, in Comparative Examples 2 and 3 in which a silane coupling agent other than Compound Q was added, no effect of addition was observed. Examples 4 and 5, in which Compound Q was added to Comparative Example 4 (containing a chain transfer agent in the polymer chain, molar ratio of polyfunctional acrylate to maleic anhydride: 0.375), had a low yellow index and excellent transparency, and 2 However, in Comparative Examples 5 to 10 in which a silane coupling agent other than Compound Q was added, no effect of addition was observed. In Comparative Examples 12 to 17, in which a compound not included in Compound Q (a sulfide compound or a thiol compound) was added to Comparative Example 11 (no chain transfer agent in the polymer chain, molar ratio of polyfunctional acrylate to maleic anhydride: 0.25), no addition effect was observed. Furthermore, Example 6, in which Compound Q was added to Comparative Example 18 (no chain transfer agent in the polymer chain, molar ratio of monofunctional acrylate to maleic anhydride: 1.25), had a low yellow index and excellent transparency, and had an optical transparency of 5 mJ / cm 2 The residual film ratio at this exposure dose was significantly improved, and the exposure dose at which the residual film ratio reached 90% or more was significantly reduced, thereby improving the sensitivity.

[0279] As described above, the photosensitive resin composition containing the polymer solution of the Examples had a higher residual film ratio at low exposure doses compared to the Comparative Examples. Furthermore, since the exposure dose at which the residual film ratio was 90% or more was also low, it was possible to provide a resin cured product (film) that was cured at low exposure doses, had high sensitivity, reduced yellowing, and excellent transparency. Furthermore, the alkali dissolution rate of the photosensitive resin composition of the Examples was not affected by compound Q. In other words, the photosensitive resin composition of the Examples had an excellent balance of these physical properties.

[0280] <Production of color filters> A suitable amount of pigment dispersion NX-061 (green, manufactured by Dainichiseika Color & Chemicals Mfg. Co., Ltd.) was further added to the photosensitive resin compositions prepared in Examples 1 to 6 to prepare colored photosensitive resin compositions. This was formed into a film on a substrate, and then exposed to light and developed with an alkali to form a green color filter. In addition, by using the same company's NX-053 (blue) or NX-032 (red) as the pigment dispersion liquid instead of NX-061, it was possible to form blue or red color filters.

[0281] <Preparation of black matrix> A suitable amount of carbon black dispersion NX-595 (manufactured by Dainichiseika Color & Chemicals Mfg. Co., Ltd.) was further added to the photosensitive resin compositions prepared in Examples 1 to 6 to prepare black photosensitive resin compositions. This was applied to a substrate as a film, and then exposed to light and developed with an alkaline solution to form a black matrix. [Explanation of symbols]

[0282] 10 Substrate 11 Black Matrix 12 Color Filters 13 Protective film 14 Transparent electrode layer

Claims

1. A structural unit represented by general formula (NB), A polymer comprising a structural unit represented by general formula (1) and at least one structural unit selected from a structural unit represented by general formula (2); and A compound having a thiol group and an alkoxy group or an oligomer thereof, The compound having a thiol group and an alkoxy group includes a compound represented by the following general formula (a): A polymer solution, in which the compound having a thiol group and an alkoxy group or an oligomer thereof is present in an amount of 0.25% by mass or more and 20% by mass or less relative to the polymer. 【Chemistry 1】 (In the general formula (NB), R 1 , R 2 , R 3 and R 4 are each independently a hydrogen atom or an organic group having 1 to 30 carbon atoms, and a1 is 0, 1 or 2. 【Chemistry 2】 (In general formula (1), R p is a group having two or more (meth)acryloyl groups. 【Chemistry 3】 (In general formula (2), R s is a group having one (meth)acryloyl group. 【Chemistry 4】 (In general formula (a), R each independently represents an alkoxy group having 1 to 3 carbon atoms or an alkyl group having 1 to 3 carbon atoms, and at least two R are alkoxy groups having 1 to 3 carbon atoms. L represents an m+n valent organic chain which may contain one or more atoms selected from O, N, S, P and Si. X represents a single bond or a divalent organic group which may contain a carbonyl group, a (thio)ester group or a (thio)amide group. Q represents a single bond, or a divalent organic group which may contain a carbonyl group, a (thio)ester group, or a (thio)amide group. The molar ratio m:n is 1:1 to 1:8, and the weight average molecular weight of the compound is 100 to 2000.

2. The polymer solution of claim 1 further comprising a compound having two or more (meth)acryloyl groups.

3. The polymer solution according to claim 1 or 2, further comprising a compound having one (meth)acryloyl group.

4. The polymer solution according to any one of claims 1 to 3, wherein the polymer further comprises a structural unit represented by general formula (3). 【Chemistry 5】

5. The polymer solution according to any one of claims 1 to 4, wherein the polymer further comprises a structural unit represented by general formula (MA). 【Chemistry 6】

6. The polymer solution according to any one of claims 1 to 5, wherein the weight average molecular weight of the polymer is 1,000 or more and 20,000 or less.

7. The polymer solution according to any one of claims 1 to 6, further comprising an organic solvent.

8. 8. The polymer solution according to claim 7, wherein the organic solvent is at least one selected from propylene glycol monomethyl ether acetate, propylene glycol monomethyl ether, γ-butyrolactone, N-methylpyrrolidone, and cyclohexanone.

9. The polymer solution according to any one of claims 1 to 8, which is used for forming a color filter or a black matrix.

10. A photosensitive resin composition comprising the polymer solution according to any one of claims 1 to 9 and a photosensitizer.

Citation Information

Patent Citations

  • Photopolymerizing composition for color filter and color filter

    JP1998282325A

  • Polymer, method for producing polymer, photosensitive resin composition, pattern, color filter, black matrix, liquid crystal display device and solid state image sensor

    JP2020023654A

  • Photosensitive resin composition, pattern, color filter, black matrix, display device, imaging element, and method for producing display device or imaging element

    JP2020024356A

  • Photosensitive resin composition, color filter, protective film, photospacer, substrate for liquid crystal display devices, liquid crystal display device, and solid-state imaging element

    WO2012147706A1

  • Negative photosensitive resin composition, resin cured film, partition wall and optical element

    WO2014069478A1