The decorative material with varying linear recesses and glitter ink-filled patterns effectively replicates the appearance and feel of a hairline metal surface, addressing misregistration and glitter reduction issues in conventional methods.

JP7585674B2Active Publication Date: 2024-11-19DAI NIPPON PRINTING CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2020153722
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-03-12
Filing Date
2020-09-14
Publication Date
2024-11-19
Estimated Expiration
2040-09-14

AI Technical Summary

Technical Problem

Conventional decorative materials with hairline-like uneven patterns struggle with misregistration of pattern layers, reduced glitter effect, and inability to replicate the natural texture and appearance of a hairline metal surface due to embossing issues and smooth surfaces.

Method used

A decorative material with a pattern forming layer featuring linear recesses filled with glitter ink, where the recesses can vary in width and depth, and the ink area within these recesses can differ, creating a more realistic hairline appearance.

Benefits of technology

The solution provides a decorative material that visually and tactually mimics a hairline metal surface with enhanced glitter effect and texture, offering a stronger impression of authenticity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007585674000001
    Figure 0007585674000001
  • Figure 0007585674000002
    Figure 0007585674000002
  • Figure 0007585674000003
    Figure 0007585674000003
Patent Text Reader

Abstract

To provide a decorative material adopting a configuration forming an uneven pattern comprising actual irregularities on the surface, capable of reproducing a design appearance of a hairline metal plate having small appearance unnaturalness, and impressing a hairline style more strongly.SOLUTION: A decorative material having a hairline style uneven pattern formed on the surface, incudes a pattern forming layer having the uneven pattern. In the pattern forming layer, a plurality of linear recesses which are linear grooves extending in one direction are arranged as the uneven pattern, and ink is arranged inside the linear recesses, and the ink includes brilliant ink.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a cosmetic material. [Background technology]

[0002] There are many different designs for decorative materials, including those with a hairline-like uneven pattern. A hairline is a polishing mark formed on a metal surface for the purpose of creating an aesthetic look, and is a striped uneven pattern formed by polishing. Such a hairline (uneven pattern) is composed of a collection of multiple thin, elongated concave stripes in a plan view, arranged in a parallel or nearly parallel positional relationship with each other along their extension direction. Therefore, a decorative material with a hairline-like uneven pattern is a decorative material formed from a material other than metal, and expresses an uneven pattern that imitates the hairline uneven pattern.

[0003] Conventionally, such hairline-patterned cosmetic materials have been made by printing a design using glittering ink on a colored base material, layering a transparent resin (thermoplastic resin) on top of this and heating it to soften it, and then embossing it to create a textured pattern consisting of linear depressions that mimic hairlines. In such decorative materials, the colored base material, which is a thermoplastic resin, inevitably expands and contracts during embossing, making it difficult to synchronize the positions of the linear depressions and the pattern (i.e., align them).In addition, because a thick resin (a resin layer for creating the unevenness for embossing) is required on top of the glossy ink, the glossy effect of the glossy ink is reduced, and it is not always possible to fully express a hairline pattern.

[0004] Therefore, attempts have been made to manufacture a cosmetic material that imitates the appearance of a hairline uneven pattern by only printing a pattern layer that is easy to align, without embossing the uneven pattern.For example, JP 2005-74637 A (Patent Document 1) discloses printing a hairline pattern pattern layer with black ink on the back side of a transparent resin sheet with a high gloss surface, and further printing a full-surface solid layer of metallic gloss ink (glossy ink) containing foil flakes of metal or pearl pigment on the back side of that, and printing a hairline pattern pattern layer with matte (low gloss) ink on the front side of the transparent resin sheet in registration with the hairline pattern pattern layer on the back side. In this decorative material, the hairline pattern picture layers on both the front and back of the transparent resin substrate are registered (both picture layers are synchronized at the same position in a plan view), so there is no unnatural appearance due to misregistration of the two picture layers, but the reproducibility (fidelity) of the design appearance of the hairline processed metal sheet surface is lower than in a form in which an uneven pattern consisting of actual unevenness is formed on the surface. Also, because the surface of the decorative material is smooth, the surface feels smooth as well, and it was not possible to reproduce the feel of the hairline uneven pattern on an actual metal surface. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2005-74637 A Summary of the Invention [Problem to be solved by the invention]

[0006] In view of the above problems, the present disclosure has an objective of providing a decorative material that adopts a form in which an uneven pattern consisting of actual unevenness is formed on the surface, that can reproduce the design appearance and feel of a hairline metal plate with a less unnatural appearance, and that can give a stronger impression of a hairline texture. [Means for solving the problem]

[0007] One aspect of the present disclosure is a decorative material having a hairline-like uneven pattern formed on its surface, the decorative material comprising a pattern-forming layer having an uneven pattern, the pattern-forming layer having a plurality of linear recesses, which are linear grooves extending in one direction as the uneven pattern, and ink is disposed inside the linear recesses, the ink containing a glittering ink. The ink may also contain a non-glittering colorant.

[0008] At least some of the linear recesses may be configured so that the width thereof changes as one moves in the extending direction of the linear recesses.

[0009] At least some of the linear recesses may be configured so that the depth changes as one moves in the extending direction of the linear recesses.

[0010] At least some of the linear recesses appearing in a cross section perpendicular to the direction in which the linear recesses extend may be configured such that, among adjacent linear recesses, the deeper linear recess has a larger ink area. Here, the linear recess that is configured so as to have a larger ink area may have higher glittering properties. Effect of the Invention

[0011] According to the present invention, a decorative material can be obtained that can give a strong impression of a hairline pattern both visually and to the touch. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is an enlarged plan view of a portion of the surface of a decorative material 10. As shown in FIG. [Diagram 2] FIG. 2 is an enlarged view of a portion of FIG. [Diagram 3] FIG. 3 is a diagram showing a part of the concave-convex shape of a plurality of linear concave portions along the line BB in FIG. [Figure 4] FIG. 4 is a perspective view showing a part of the decorative material 10, which is shown in a schematic manner to explain the configuration of the pattern-forming layer 12. As shown in FIG. [Diagram 5] FIG. 5 is a diagram for explaining one example of the shape of the linear recess 13. As shown in FIG. [Figure 6] FIG. 6 is a diagram for explaining one example of the shape of the linear recess 13. As shown in FIG. [Figure 7] FIG. 7 is a diagram for explaining one example of the configuration of the inking section 14. As shown in FIG. [Figure 8] FIG. 8 is a diagram illustrating a decorative material 10'. [Figure 9] FIG. 9 is a diagram showing a part of the grayscale image data (uneven pattern image data). [Figure 10] FIG. 10 is a diagram illustrating a scene where a concave-convex pattern is formed on a mold by a laser. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, the present disclosure will be described based on the embodiments shown in the drawings. The present invention is not limited to these embodiments. In the drawings shown below, the size and ratio of the components may be changed or exaggerated for ease of understanding. In addition, for ease of viewing, illustration of parts not necessary for explanation and repeated reference symbols may be omitted.

[0014] [Structure of decorative material] FIG. 1 is an enlarged plan view (top view) of a portion of a decorative material 10 according to one embodiment, viewed from the pattern-forming layer 12 side. For convenience, directional arrows (x, y, z), i.e., a coordinate system, are also shown in Fig. 1 and the following figures as necessary. Here, the x and y directions are in-plane directions in the decorative material 10, and the z direction is the thickness direction. Therefore, Fig. 1 is a view (plan view) of the decorative material 10 from the pattern-forming layer 12 side, particularly from the z direction. As can be seen from FIG. 1, the decorative material 10 of this embodiment is formed to have an uneven pattern that has a hairline look when viewed from above.

[0015] Figure 2 shows an enlarged view of the portion indicated by A in Figure 1. Figure 3 shows part of the shape of the unevenness (z direction) of linear depressions 13 in pattern forming layer 12 along the line (x direction) indicated by BB in Figure 2 (however, Figure 3 shows the uneven shape excluding ink portion 14). FIG. 4 is a perspective view showing an enlarged schematic view of a portion of the cosmetic material 10 in order to more clearly explain the configuration of the cosmetic material 10. As shown in FIG. 1 to 4, the decorative material 10 is configured to have a substrate 11 and a pattern-forming layer 12 provided on one surface of the substrate 11. Thus, in this embodiment, one surface of the substrate 11 is configured to function as the pattern-forming layer 12. In other words, in this embodiment, the substrate 11 itself has a single-layer configuration that also serves as the pattern-forming layer 12. However, this is not limited to this, and a multiple-layer configuration in which the substrate 11 and the pattern-forming layer 12 are separate, independent layers and both layers are laminated together may also be used.

[0016] Each component will be described in more detail below.

[0017] <Base material> The substrate 11 is a sheet-like member that holds the pattern-forming layer 12 and provides strength to the decorative material 10. The substrate 11 may be in the form of a film, a sheet, or a plate. Generally, substrates are called films, sheets, and plates in that order from relatively thin to thin, but in this embodiment, the difference in thickness between these substrates is not essential or important. Therefore, in this specification, the essence of the present invention and the interpretation of the claims will not change even if any of the terms film, sheet, and plate are appropriately replaced with other terms. 4, in a configuration in which the substrate 11 and the pattern-forming layer 12 are both formed as a single layer, the pattern-forming layer 12 itself also serves as the substrate 11. The substrate 11 also includes such a configuration.

[0018] The material of the substrate 11 is not particularly limited as long as it has the same functions as conventionally known decorative materials. For example, the substrate material is usually made of polyolefin resins such as polyethylene, polypropylene, olefin thermoplastic elastomers, and ionomers, acrylic resins such as polymethyl methacrylate and polybutyl methacrylate, thermoplastic polyester resins such as polyethylene terephthalate, polybutylene terephthalate, ethylene glycol-terephthalic acid-isophthalic acid copolymers, and polyester thermoplastic elastomers, vinyl chloride resins such as polyvinyl chloride (vinyl chloride homopolymers), vinyl chloride-vinyl acetate copolymers, and ethylene-vinyl chloride copolymers, thermoplastic resins such as thermoplastic urethane resins, polycarbonate resins, ABS resins (acrylonitrile-butadiene-styrene copolymers), and styrene resins, thermosetting resins such as melamine resins, unsaturated polyester resins, epoxy resins, and two-component curing urethane resins, or ionizing radiation curing resins in which monomers or prepolymers such as radical polymerization acrylates or cationic polymerization epoxys are cured by ionizing radiation (ultraviolet rays, electron beams, etc.). In addition, when the material of the base material is a resin, it may be colored with a known colorant. In addition, paper, nonwoven fabric, metal, wood, etc. can also be used in the form of a sheet, board, three-dimensional object, etc. by appropriately laminating it with the above-mentioned resin material.

[0019] When the substrate is colored with a known colorant, the hue of the substrate resulting from this coloring can be configured to have a predetermined relationship with the hue of the ink portion 14 provided in the pattern-forming layer 12, which will be described later. Specific details will be described later in relation to the ink portion 14.

[0020] There is no particular restriction on the thickness of the substrate, but in the case of a sheet-shaped substrate or a film-shaped substrate, the thickness can be, for example, about 20 μm or more and 1000 μm or less, and in the case of a plate-shaped substrate, the thickness can be, for example, about 1 mm or more and 20 mm or less.

[0021] <Pattern forming layer> In this embodiment, the pattern-forming layer 12 is provided on one surface of the substrate 11, and is a layer that imparts an uneven pattern to the decorative material, and in this embodiment, the substrate 11 itself has a surface (the upper side in FIG. 4, i.e., the surface on the +z direction side) that imparts an uneven pattern with a hairline look in a plan view to the decorative material 10, and the substrate 11 also serves as the pattern-forming layer 12 (in other words, the surface of the substrate 11 itself constitutes the pattern-forming layer 12). As can be seen particularly clearly from FIG. 4, the pattern-forming layer 12 comprises a recess 13 and an ink portion 14 arranged inside the recess 13. Each of these will be explained below.

[0022] {Linear recess} 1 to 4, the pattern-forming layer 12 is provided with a plurality of linear depressions 13, which are linear grooves. In this embodiment, the linear depressions 13 have the following configuration. By providing a plurality of linear depressions 13 on the surface of the decorative material 10, it is possible to impart a hairline-like design to the decorative material 10 in terms of not only the visual appearance but also the tactile feel.

[0023] In this embodiment, the linear recesses 13 are formed to extend parallel or approximately parallel in one direction (the y direction in this embodiment). Therefore, the linear recesses 13 are linear grooves (recessed lines) whose length is the size in the y direction, whose width is the size in the x direction, and whose depth is the size in the z direction. Here, the length of one linear recess 13 is not particularly limited. That is, the linear recesses 13 may be formed so that both ends in the length direction reach the ends (edges) of the decorative material, one end may not reach the end of the decorative material and the other end may reach the end of the decorative material, or both ends may be long enough not to reach the ends of the decorative material. And it is not necessary for one decorative material 10 to have any one of these, and they may be mixed in one decorative material 10. In addition, the fact that the linear recesses 13 "extend substantially parallel" in one direction does not mean that the extension directions of the multiple linear recesses 13 are all aligned in the same direction (that is, they extend completely parallel), but that the distribution of the extension directions of the linear recesses 13 is within 10 degrees in a plan view. In order to reproduce a hairline-like design appearance, it is more preferable that the distribution of the extension directions of the linear recesses 13 is within 5 degrees in a plan view.

[0024] The width (size in the width direction) of the linear recess 13 is not particularly limited, and can be typically in the range of 10 μm to 200 μm. The widths of the multiple linear recesses 13 may be the same, or may be different as shown in Figures 3 and 4.

[0025] FIG. 5 is a diagram for explaining one embodiment, focusing on one linear recess 13. The central diagram in FIG. 5 shows a plan view of the linear recess 13, the lower diagram in FIG. 5 shows an xz plan view of one end of the linear recess 13, and FIG. 5 shows an xz plan view of the other end. As can be seen from FIG. 5, when focusing on one linear recess 13, the width may change (become larger or smaller) as it moves in the longitudinal direction (the direction in which the linear recess 13 extends). This change may be continuous as shown in FIG. 5, or may be stepwise or irregular. Therefore, the change in width is not limited to increasing from one side to the other side, but may be increased halfway and then decreased halfway. Such linear depressions 13 may be included in at least a portion of the decorative material 10 .

[0026] The depth (size in the depth direction) of the linear recess 13 is not particularly limited and can be, for example, in the range of 5 μm to 100 μm. The linear recesses 13 may have the same depth, or may have different depths as shown in FIGS. 3 and 4. FIG. 6 is a diagram for explaining one embodiment, focusing on one linear recess 13. The central diagram in FIG. 6 is a diagram in which the linear recess 13 is cut in the yz plane along the longitudinal direction (y direction), the left diagram in FIG. 6 is a xz plan view of one end of the linear recess 13, and the right diagram in FIG. 6 is a xz plan view of the other end of the linear recess 13. As can be seen from FIG. 6, when focusing on one linear recess 13, the depth may change as it moves in the longitudinal direction (the direction in which the linear recess 13 extends). This change may be continuous as shown in FIG. 6, or may be stepwise or irregular. Therefore, the change in depth is not limited to becoming deeper from one side to the other side, but may be deeper halfway and then become shallower. Such linear depressions 13 may be included in at least a portion of the decorative material 10 .

[0027] The cross-sectional shape of the linear recess 13 in a direction (x direction) perpendicular to the longitudinal direction (y direction) is not particularly limited, and can be any shape, such as a semicircle, semi-ellipse, triangle, rectangle, pentagon, hexagon, or other polygon, or an irregular geometric shape. Among them, as shown in the upper diagram of FIG. 5, it is preferable that the ratio (W / D) of the width W to the depth D satisfies the following relationship. 0 <W / D≦15 This makes it possible to further improve the reproducibility of the hairline-like design appearance. However, in order to ensure that the glittering pigment in the glittering ink is filled inside the linear recesses 13, it is preferable that the depth D and width W are greater than the average value of the maximum diagonal length of the glittering pigment particles. For example, if the glittering pigment particles are polygonal prisms whose height is smaller than the minimum diagonal length of the upper and lower bases, the depth D and width W should be greater than the average maximum diagonal length of the polygons at the upper and lower bases for all particles.

[0028] {Ink Department} The ink portion 14 is a portion made of ink containing glittering ink and disposed inside the linear depressions 13. Here, "glittering" refers to a relatively high light reflectance, and a change in color tone (one or more of hue, brightness, and saturation), brightness, gloss, etc. depending on the combination of the incident direction of the illumination light and the line of sight of the observer, thereby providing a unique design as if the decorative material 10 were a metal product.

[0029] In this embodiment, the glitter ink of the ink portion 14 is one in which a glitter pigment is dispersed in a resin binder.

[0030] Examples of luster pigments that can be used include mica (mica) whose surface is coated with a thin film of titanium oxide or iron oxide, pearl pigments (pearl luster pigments) consisting of shells such as pearl oysters, bismuth oxychloride, basic lead carbonate, etc., scale-like flakes of metals such as aluminum, brass, gold, silver, copper, tin, nickel, etc., scale-like flakes of resin films with metal vapor deposition, and scale-like flakes made by laminating multiple resin films with different refractive indices to exhibit interference luster. The average particle size of these luster pigments can be appropriately selected depending on the desired luster and printability, but a particle size of 10 μm or more and 60 μm or less is usually preferred for luster expression. The average particle size of the particles is the volume-based median diameter (D50) measured by a laser diffraction / scattering particle size distribution measurement. The median diameter (D50) is the diameter (volume average diameter) at which the cumulative volume of the particles is half (50%) of the total when the particles are arranged in order from the smallest particle size.

[0031] Examples of resin binders that can be used include acrylic resins such as polymethyl methacrylate and polybutyl methacrylate; cellulose-based resins such as cellulose nitrate and cellulose acetate; thermoplastic resins such as vinyl chloride-vinyl acetate copolymers and thermoplastic polyester resins; thermosetting resins such as two-component curing urethane resins that use a polyol compound as the main component and an isocyanate compound as the curing agent, melamine resins and thermosetting polyester resins; and ionizing radiation curing resins that are made of a composition containing one or more of acrylate monomers or prepolymers, epoxy prepolymers, unsaturated polyester resins, and that are cured by crosslinking or polymerization when exposed to ionizing radiation such as ultraviolet rays or electron beams.

[0032] The ink portion may further contain a colorant that has no glittering (non-glittering) and a desired hue. The colorant is not particularly limited, but examples thereof include inorganic pigments consisting of particles such as carbon black, iron black, titanium white, antimony white, zinc white, yellow lead, titanium yellow, red oxide, cadmium red, ultramarine blue, and cobalt blue, and organic pigments or dyes such as quinacridone red, isoindolinone yellow, phthalocyanine blue, aniline black, azomethine azo black, and perylene black, or a mixture of two or more of these colorants. By containing a photoluminescent pigment and a colorant in the photoluminescent ink, the linear depressions filled with the photoluminescent ink not only obtain the metallic luster, pearlescent luster, or a luster similar to these due to the photoluminescent pigment, but also express a hue due to the colorant, thereby presenting a design appearance with a so-called "color metallic" or "color pearlescent" look.

[0033] When the glittering ink contains a colorant, the content of the glittering pigment and the colorant can be adjusted as appropriate according to the desired hairline appearance and design. Usually, the content of the glittering pigment can be in the range of 0.1 to 50 parts by mass, and the content of the colorant can be in the range of 0.1 to 50 parts by mass, relative to 100 parts by mass of the resin binder. The ratio of the glittering pigment content to the colorant content can be appropriately selected according to the desired hairline appearance and design, but the ratio of the glittering pigment content / colorant content is in the range of 5 / 95 to 95 / 5.

[0034] As described above, the ink portion may be formed by disposing the material containing the glittering ink in the linear recesses, thereby making it possible to provide a cosmetic material that can give a stronger impression of a hairline.

[0035] In addition to the above, the ink section can also be configured as follows. The brilliance of the ink portion may be within a predetermined range. Specifically, as shown in Fig. 7, a cross section perpendicular to the longitudinal direction of the linear depression 13 of the decorative material 10 (cross section along the xz plane) is taken, and two adjacent linear depressions 13 among the multiple linear depressions 13 that appear therein are considered.

[0036] Regarding the glitter caused by the glittering ink filled in the linear depressions 13, the glittering appearance visually recognized when the decorative material 10 is viewed in planar view increases as the glittering ink filling volume filled per unit length in the longitudinal direction of the linear depressions 13 increases. The glittering ink filling volume filled per unit length in the longitudinal direction of the linear depressions 13 is proportional to the area E of the ink portion 14 in the cross section of the linear depressions 13 as shown in Figure 7. This area E is a value obtained by integrating the width W(z) of the linear depressions 13 as a function of the depth direction z over the entire area of ​​the glittering ink (filled) portion 14 (entire filling depth D) in the depth direction z. However, as in the example of Figure 7, when the function W(z) of the width of the linear recess 13 in the depth direction is roughly the same, even if the area E of the ink portion 14 in the cross section of the linear recess 13 is proportional to the depth D of the ink portion 14, there is no problem in terms of design accuracy for the actual visual appearance of the decorative material.

[0037] Furthermore, the degree of change in the brilliance of the decorative material 10 in the in-plane direction of the surface of the decorative material, i.e., whether the brilliance is uniform across the entire in-plane area or the strength of the brilliance varies greatly from place to place in the in-plane area, in the visual appearance in plan view, is positively correlated with the strength of the brilliance between two adjacent linear recesses 13 as shown in FIG. 7, i.e., the area E of the ink portion 14 between two adjacent linear recesses 13. Even when the difference in the strength of the brilliance between two linear recesses 13 that are far apart from each other is relatively large, it has little impact on the magnitude of the in-plane change in the brilliance in the plan view of the visual appearance. By changing the depth of adjacent linear recesses 13 as shown in FIG. 7, a difference is created in the amount of brilliant ink (pigment concentration) filled in two adjacent linear recesses 13, and by providing a three-dimensional density gradation, it becomes possible to express a more realistic metallic texture and feel.

[0038] In the case of the form shown in FIG. 7, let the depth of one (the left side in the figure) of the two adjacent linear recesses 13 be D1 and the area of the ink portion 14 in this cross-section be E1, and the depth of the other (the right side in the figure) linear recess 13 be D2 and the area of the ink portion 14 in this cross-section be E2. In the case of FIG. 7, since the function W(z) of the width of the linear recess 13 in the depth direction is the same, it is configured such that the deeper linear recess 13 (the linear recess with depth D2 on the right side in this example) has a larger area of the ink portion 14 (i.e., E1 < E2) in this example.

[0039] Furthermore, the evaluation of the brilliance in this cross-section can also be configured such that the brilliance of the deeper linear recess 13 (the linear recess with D2 in this example) is higher. Here, since the decorative material of the present disclosure is an object to be visually and sensually recognized and appreciated in terms of design appearance, the evaluation of the brilliance of the decorative material 10 is that the evaluator visually and sensually evaluates the degree of change in the color tone (any one or more of hue, lightness, and chroma), luminance, gloss, etc. depending on the combination of the incident direction of the illumination light and the viewing direction of the observer, with the brilliance, i.e., the light reflectance being relatively high. However, such visual sensory evaluation is subjective and depends on individual differences and the evaluation environment. Therefore, when it is necessary to objectively compare and evaluate the glitteriness of cosmetic materials, it is appropriate to have multiple evaluators (preferably five or more) with different ages, sexes, occupations, hobbies, and preferences, and to evaluate the glitteriness by quantifying the evaluations using a graded relative evaluation such as "A, B, C" or "1, 2, 3, 4, 5," and then averaging the average value.

[0040] However, when a quantitative evaluation of the brilliance as a physical value is required due to the necessity of product design or quality control, for example, the following measurement evaluation method can be applied. (1) Evaluation based on the FI value measured using an X-Rite MA-68II multi-angle spectrophotometer. (2) Evaluation based on the indicators of "brightness" and "whiteness" obtained by the measurement and evaluation method for glittering coating films described in Japanese Patent No. 4152786 (JP Patent Publication No. 2004-286672).

[0041] When the substrate 11 is colored with a colorant, decorative materials exhibiting various design appearances can be obtained according to the combination of the hue of the substrate 11 and the color tone of the ink portion 14. For example, there are the following forms:

[0042] (Mode 1) Mode in which the color difference between the substrate 11 and the ink portion 14 is small Here, small color difference refers to the L standard defined by the CIE (International Commission on Illumination) in 1976 and adopted in JIS Z8781-5:2013. * a * b * In the color system, the color tone of the base material 11 is (L * 11 , a * 11 , b * 11 ), and the color tone of the ink portion 14 is (L * 14 , a * 14 , b * 14 ), ΔE * =〔(L* 14 -L * 11 ) 2 +(a * 14 -a * 11 ) 2 +(b * 14 -a * 11 ) 2 〕 0.5 Color difference ΔE defined as * satisfies the following relationship: ΔE * ≦3, More preferably, ΔE * <= 2 It is.

[0043] In the case of form 1, since the color difference between the base material 11 in the decorative material 10 and the ink portion 14 filled with the glittering ink is relatively small, even if the surface of the decorative material is worn or scratched and part of the ink portion 14 (glossy ink) filled in the linear recess 13 is lost, this has the unique effect of making such wear and scratches less noticeable.

[0044] (Mode 2) Mode in which the color difference between the substrate 11 and the ink portion 14 is large Form 2: Color difference ΔE * satisfies the following relationship: ΔE * >3. More preferably, ΔE * >5 It is.

[0045] In the case of form 2, the color difference between the substrate 11 in the decorative material 10 and the ink portion 14 filled with the glittering ink is relatively large, so that in appearance, the ink portion 14 has a high visual contrast with the background substrate 11. Therefore, a unique effect is achieved in that the design appearance of numerous scratches (streaks) of the hairline finish on the surface of the metal plate can be reproduced satisfactorily.

[0046] Form 2 is further divided into the following two forms (form 2-1, form 2-2) depending on the magnitude of the hue difference Δθ. (Type 2-1) Type with small hue difference Δθ In form 2-1, color difference ΔE * In addition to the above condition 3, L * a * b * Color space L * a * b * The hue θ corresponding to the deviation angle θ in the three-dimensional coordinate system is expressed as θ 11 , θ for the ink section 14 14 Then, the hue difference Δθ between the two is Δθ=|θ 14 -θ 11 |≦45 degrees, More preferably, Δθ=|θ 14 -θ 11 |≦20 degrees It is.

[0047] In the case of form 2-1, the color difference between the substrate 11 and the ink portion 14 in the decorative material 10 is relatively large (ΔE * >3), the decorative material has good reproducibility of the design appearance of the hairline finish on the metal plate surface, and the hue difference Δθ between the substrate 11 and the ink portion 14 is relatively small (hue difference Δθ≦45 degrees). Therefore, when the surface of the decorative material is worn or scratched and part of the ink portion 14 (glossy ink) filled in the linear recesses 13 is lost, the wear or scratch is less noticeable. Thus, two seemingly contradictory effects are achieved at the same time. In the case of the embodiment 2-1, under the condition that the hue difference Δθ between the substrate 11 and the ink portion 14 is relatively small, the color difference ΔE * In order to increase the difference in brightness, the difference in chroma, or the difference in brightness and chroma between the base material 11 and the ink portion 14 is increased, the color tone is designed so as to increase the difference in brightness, the difference in chroma, or the difference in brightness and chroma.

[0048] (Type 2-2) A type with a large hue difference Δθ In the case of Form 2-2, the color difference between the substrate 11 and the ink portion 14 in the decorative material 10 is relatively large (ΔE *>3), furthermore, the hue difference Δθ between the substrate 11 and the ink portion 14 is relatively large (hue difference Δθ>45 degrees, for example, the substrate 11 is a glitter ink with a green hue and the ink portion 14 is a glitter ink with a red hue). Therefore, the visual contrast between the ink portion 14 and the background substrate 11 is even greater. This results in an even better reproducibility of the design appearance of the hairline finish on the metal plate surface, and a unique effect of being able to reproduce an innovative design appearance that is different from an actual hairline-finished metal plate in which the inside and outside of the linear recesses are the same hue. In the case of the embodiment 2-2, the hue difference Δθ between the substrate 11 and the ink portion 14 is relatively large, and the color difference ΔE * becomes large regardless of the magnitude of the lightness and chroma difference between the substrate 11 and the ink portion 14, it is possible to select either a large or small lightness difference, chroma difference, or lightness and chroma difference between the substrate 11 and the ink portion 14. In this embodiment, the lightness and chroma difference between the substrate 11 and the ink portion 14 may be appropriately designed according to the desired design and appearance of the decorative material.

[0049] It is also preferable that the glittering ink that constitutes the ink portion 14 is not present in any area other than the inside of the linear depressions 13 (for example, the surface that becomes the relative convex portion between adjacent depressions 13). However, since there is a possibility that some of the materials (pigments and binders) that constitute the glittering ink may remain during the manufacturing process, their presence is permissible as long as it is within the range of such error. This is because the effect on the effect of the present invention is small if it is within such a range of error.

[0050] The pattern-forming layer 12 as described above makes it possible to provide a cosmetic material that is different from conventional cosmetic materials that express hairlines, and in particular, a cosmetic material that has an appearance that strongly expresses the characteristics of a hairline.

[0051] <Modification> A diagram for explaining a modified decorative material 10' is shown in Fig. 8. In the decorative material 10' of this example, a protective layer 15 is laminated on the decorative material 10. This protects the decorative material from contamination and damage.

[0052] Such a protective layer can be made of a transparent resin, transparent glass, etc. When a transparent resin is used, examples of the protective layer include a layer made of a thermoplastic resin or a cured resin. In addition, if the substrate 11 and the pattern-forming layer 12 alone can ensure sufficient surface durability such as stain resistance and scratch resistance for the intended application, the protective layer can be omitted.

[0053] Examples of thermoplastic resins include acrylic resins such as polymethyl(meth)acrylate and polyethyl(meth)acrylate, polyolefin resins such as polypropylene and polyethylene, fluorine resins such as polyvinyl fluoride and polyvinylidene fluoride, thermoplastic polyester resins such as polyethylene terephthalate (PET) and urethane-modified aromatic copolymer polyester (commercially available products include "Vylon" (registered trademark) manufactured by Toyobo Co., Ltd.), polycarbonate resins, vinyl chloride resins, acrylonitrile-butadiene-styrene resins (ABS resins), acrylonitrile-styrene-acrylic ester resins, etc. Incidentally, "(meth)acrylic" means acrylic or methacrylic.

[0054] The layer of the cured resin is a layer formed by curing a curable resin composition, and the curable resin composition is a composition containing a curable resin. Examples of the curable resin composition include a thermosetting resin composition containing a thermosetting resin and an ionizing radiation curable resin composition containing an ionizing radiation curable resin. Examples of the thermosetting resin include unsaturated polyester resin, polyurethane resin (including two-component curing polyurethane), epoxy resin, aminoalkyd resin, phenol resin, urea resin, diallyl phthalate resin, melamine resin, guanamine resin, melamine-urea co-condensation resin, silicon resin, polysiloxane resin, etc. The thermosetting resin composition may contain, as necessary, a component involved in the curing reaction of the thermosetting resin, such as a catalyst, a curing agent (including a crosslinking agent, a polymerization initiator, a polymerization accelerator, etc.), etc. Ionizing radiation curable resins are resins that undergo a cross-linking polymerization reaction upon irradiation with ionizing radiation, changing into a three-dimensional polymer structure. Ionizing radiation is electromagnetic waves and charged particle beams that have an energy quantum capable of polymerizing or cross-linking molecules, and includes ultraviolet rays (UV) and electron beams (EB), as well as electromagnetic waves such as X-rays and gamma rays, and charged particle beams such as alpha rays and ion beams, but ultraviolet rays (UV) or electron beams (EB) are usually used. Among ionizing radiation curable resins, electron beam curable resins can be made solvent-free, do not require a photopolymerization initiator, and can obtain stable curing properties. As the ionizing radiation curable resin, for example, a composition containing one or more monomers, oligomers, prepolymers, and the like having polymerizable unsaturated bonds such as (meth)acryloyl groups, epoxy groups, and the like in the molecule that can be crosslinked by irradiation with ionizing radiation can be used.

[0055] The thickness of the protective layer 15 is not particularly limited, but may be 0.1 μm or more and 20 μm or less. If it is thin, it has high durability against bending, etc. but has poor scratch resistance, and if it is thick, it has strong scratch resistance and scratch resistance, but is weak against deformation such as bending and cracks occur, so by setting the thickness within the above range, a well-balanced protective layer can be obtained. Therefore, it may be 1 μm or more and 10 μm or less.

[0056] [Method of manufacturing decorative material 10] Next, an example of a method for producing a cosmetic material will be described using the cosmetic material 10 as an example. However, the method for producing a cosmetic material is not limited to this. The manufacturing method described below includes a step of producing a grayscale image, a step of producing a copy image, a step of producing a plate, a step of forming a pattern-forming layer, and a step of filling with ink.

[0057] <Process for producing grayscale images> In the process of producing a grayscale image, the uneven pattern in plan view (hairline-like uneven pattern) to be expressed on the pattern forming layer 12 is produced as a grayscale image consisting of large and small optical densities. For example, in this embodiment, using graphic design drawing software "Illustrator" manufactured by Adobe Systems, grayscale image data can be produced in TIFF format with 8-bit image grayscale gradation (256 gradations) and a resolution of 2540 dpi.

[0058] <The process of creating a copy image> In the process of creating a plate image, the obtained original image is converted into a conversion program from density to unevenness, i.e., embossing plate depth, and the plate depth of the convex stripe pattern as a binary image is generated and positioned on a two-dimensional virtual plane, the XY plane, corresponding to the density gradation image of the pattern, to obtain the plate image as digital data. In this case, the minimum value of optical density (e.g., 0) is made to correspond to the minimum value of plate depth data (e.g., 0 μm) and the maximum value of optical density (e.g., 255) is made to correspond to the maximum value of plate depth data (e.g., 250 μm), thereby converting the grayscale image data consisting of the distribution of optical density P(X, Y) at each coordinate (X, Y) on a two-dimensional plane into embossed plate depth data H(X, Y) consisting of the distribution of plate depth D(X, Y) at the same coordinates.

[0059] Here, according to the conditions for generating the convex stripes, a planar image of the pattern forming layer as shown in Fig. 9 is generated as a binary image. In Fig. 9, the shading of the image represents the plate depth of the embossing plate (optical density corresponds to plate depth). The line segments of the uneven shape generated in this way correspond to the convex stripes in the decorative material. In this way, a plate image is obtained.

[0060] <The process of making the plate> In the process of preparing the plate, an embossed plate (a mold for decorative material) is prepared based on a copy image, which has a surface with a concave-convex pattern in which the concaves and convexes are reversed in plan view like the decorative material in Fig. 1. Specifically, the process of producing the concave-convex pattern includes the following steps (1) to (4).

[0061] (1) Metal roll preparation process A metal roll 20 for embossing was prepared as shown in Fig. 10. The metal roll 20 is a hollow iron cylinder having a rotary drive shaft 21 at both axial ends, the surface of which is plated with a copper layer. The surface of the metal roll 20 was roughened by grinding with a grindstone to prevent a decrease in engraving efficiency due to specular reflection of the engraving laser light.

[0062] (2) Laser engraving process As shown diagrammatically in Figure 10, a laser beam direct engraving machine is used to engrave the surface of the metal roll 20 prepared in step (1) based on the uneven pattern image data created in the plate image creation step. This forms an uneven shape on the surface that has the same shape in plan view as the uneven pattern on the decorative material surface as shown in Figure 1, but is an inverse uneven shape (where the parts that correspond to the convex stripes on the decorative material become concave stripes on the embossing plate surface). Therefore, the shape that the concave-convex pattern of the embossing plate should have is an inverted form of the concave-convex relationship of the concave-convex pattern of the decorative material described above, and can be considered in the same way.

[0063] The metal roll 20 is driven by an electric motor via its rotary drive shaft 21, and rotates around the rotary drive shaft 21 as a central axis. The surface of the metal roll 20 is scanned with a fiber laser beam P emitted from a laser head 22, which has an oscillation wavelength of 1024 nm, a laser spot diameter of 10 μm, and an output of 360 W. In this case, the laser beam is switched ON-OFF (switching between irradiation and non-irradiation) according to the density value of the uneven pattern image data created in step (1), and a recess having a depth of 10 μm is formed at the irradiation position by evaporating the metal by one laser beam irradiation. In this example, such scanning of the metal roll surface with the laser beam is repeated, for example, ten times. In addition, in order to prevent the evaporated metal from becoming powder and remaining or adhering to the surface of the metal roll 20, the laser beam irradiation is performed in a state where the engraving liquid T is sprayed from the engraving liquid outlet 23 onto the laser beam irradiation area on the surface of the metal roll 20. In this case, for example, at the position coordinates of the image density corresponding to a plate depth of 50 μm on the uneven pattern image data, the laser light is irradiated (ON) for only the first 5 scans out of a total of 25 scans, and the laser light is not irradiated (OFF) for the remaining 20 scans to obtain the desired depth. The scanning of the laser light is completed to form a desired uneven shape on the surface of the metal roll 20.

[0064] (3) Electrolytic polishing process After the engraving liquid is washed away, electrolytic polishing is performed to remove metal residue adhering to the surface of the metal roll 20.

[0065] (4) Chrome plating process After step (3), a chromium layer having a thickness of 10 μm was formed on the surface of the metal roll by plating.

[0066] In this manner, a plate (a decorative material forming die, in this embodiment an embossed plate) having a surface with an inverted uneven shape of the uneven pattern formed on the surface of the pattern forming layer 12 can be obtained.

[0067] <Process for forming pattern forming layer> Next, in the process of forming a pattern-forming layer, the base material 11 is embossed using the prepared plate (embossing plate) to obtain the decorative material 10. The embossing may be performed by any suitable known method, and is not particularly limited. Representative methods of embossing are, for example, as follows. A resin sheet made of a thermoplastic resin such as a polyolefin resin is used as the substrate. The substrate is heated and softened, and an embossing plate is pressed onto the surface of the substrate to form the concave-convex pattern of the embossing plate on the surface of the resin sheet. The resin sheet is then cooled and solidified to fix the concave-convex pattern on the resin sheet. The resin sheet with the concave-convex pattern formed thereon is then released from the embossing plate. Here, various embossing methods will be further explained. For example, there are the following methods (A) to (E).

[0068] (A) The resin sheet that serves as the base material is heated and softened, and an embossing plate is pressed against it to perform embossing. (B) The resin sheet (substrate) that serves as the surface sheet and the resin sheet (second substrate) that serves as the base sheet are thermally fused together by the heat and pressure of pressing the embossing plate, thereby performing embossing and lamination simultaneously using the doubling embossing method. (C) The resin sheet (substrate) to be used as the surface sheet is melt-extruded from a T-die and brought into contact with a cylindrical embossing plate that also serves as a cooling roller, and embossed simultaneously with the formation of the surface sheet. At this time, a resin sheet (second substrate) to be used as the base sheet inserted on the back side of the surface sheet is heat-sealed to perform doubling embossing simultaneously with the formation of the film. (D) As disclosed in JP-A-57-87318 and JP-A-7-32476, an uncured liquid material of an ionizing radiation curable resin is applied to the surface of a cylindrical embossing plate. A base sheet made of a resin sheet or the like is then placed on top of the coating, and the uncured liquid material is cured by irradiating with ionizing radiation to form a cured product. At this time, the cured product is adhered to the base sheet, and then released from the embossing plate to form a substrate made of the base sheet and the cured product on the base sheet, thereby embossing the substrate. (E) Impregnated paper, such as titanium paper, impregnated with uncured thermosetting resin such as melamine resin, is placed on a backing material such as core paper or wood plywood, and the layers are heat-pressed to laminate and integrate them to produce a thermosetting resin decorative material. At this time, an embossing plate is inserted into the surface side of the impregnated paper, and the surface is embossed at the same time as the thermosetting resin is impregnated and cured to form the decorative material.

[0069] The material of the substrate used in the embossing methods (A) to (C) is typically a thermoplastic resin, the material of the substrate used in the embossing method (D) is typically an ionizing radiation curable resin, and the material of the substrate used in the embossing method (E) is typically a thermosetting resin.

[0070] <Ink filling process> In the ink filling step, the linear recesses 13 formed on the surface of the substrate 11 are filled with glittering ink to form the ink portion 14. This is done by supplying ink (in an uncured state) of the material that is to become the ink portion 14 to the surface of the substrate 11 on which the linear recesses 13 are formed, and then scraping (wiping) the ink with a doctor blade. This makes it possible to remove excess ink and to push the ink into the linear recesses 13. The doctor blade is then moved parallel to the direction in which the linear recesses 13 extend (y direction). That is, this makes it possible to easily form the shape of the ink portion 14 as described above. The ink is then cured by an appropriate method to form the decorative material 10.

[0071] In this manner, the cosmetic material 10 can be obtained.

[0072] [Use of decorative materials] The uses of the decorative materials described above are not particularly limited, and examples thereof include interior materials for buildings such as walls, floors, and ceilings; exterior materials for building exterior walls, roofs, gates, walls, and fences; surface materials for fittings such as doors, window frames, and door frames, and fittings or fixtures such as moldings, baseboards, and handrails; surface materials for the housings of home appliances such as television sets and refrigerators, and office equipment such as copiers; surface materials for furniture such as chests of drawers, cupboards, desks, and dining tables; surface materials for containers such as boxes, glass bottles, and resin bottles; and interior or exterior materials for vehicles such as automobiles and railway cars, and transportation equipment such as ships and aircraft. [Explanation of symbols]

[0073] 10, 10' Decorative material 11 Base material 12 Pattern forming layer 13 Linear depressions (bumpy patterns) 14 Ink Department

Claims

1. A decorative material having a hairline-like unevenness on its surface, A pattern forming layer having the uneven pattern is provided, The pattern forming layer has a plurality of linear recesses, which are linear grooves extending in one direction, arranged as the uneven pattern, The decorative material has ink disposed inside the linear recess, the ink including a glittering ink.

2. The decorative material according to claim 1 , wherein at least some of the plurality of linear recesses have a width that changes as the linear recesses move in the extending direction.

3. The decorative material according to claim 1 or 2, wherein at least some of the plurality of linear recesses have a depth that changes as one moves in the extending direction of the linear recesses.

4. A decorative material as described in any one of claims 1 to 3, wherein at least some of the multiple linear depressions appearing in a cross section perpendicular to the direction in which the linear depressions extend are configured such that, among adjacent linear depressions, the deeper linear depression has a larger area of ​​the ink.

5. 5. The decorative material according to claim 4, wherein the linear depression configured so as to have a larger area of ​​the ink has higher glittering properties.

6. 6. The decorative material according to claim 1, wherein the ink also contains a non-glare colorant.

Citation Information

Patent Citations

  • Decorative sheet and decorative material laminated with the same

    EP2316643A1

  • Manufacture of uneven decorative laminated sheet

    JP1996011276A

  • Decorative sheet

    JP1996127111A

  • Scratch processed metal like decorative sheet and decorative material

    JP2005074637A

  • Decorated sheet for insert molding

    JP2008094074A