Manufacturing method of fluorescent light guide plate
By laminating thin resin films with quantum dots in a fluorescent light guide plate, the aggregation of quantum dots is prevented, significantly improving luminescence intensity and power generation efficiency.
Patent Information
- Application Number
- JP2022094020
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-06-09
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-06-09
AI Technical Summary
The luminescence intensity of quantum dot-based fluorescent light guide plates is significantly reduced due to the aggregation of quantum dots during the curing process, leading to a decrease in luminescence efficiency.
A fluorescent light guide plate is formed by laminating thin resin films containing quantum dots, which are dispersed in an organic solvent with an anti-aggregation agent, and cured quickly to prevent aggregation, maintaining high luminescence intensity.
The luminescence intensity per irradiation light intensity is increased by 10 to 12 times, enhancing the power generation efficiency of solar cells attached to the edge surface.
Smart Images

Figure 0007586143000001 
Figure 0007586143000002 
Figure 0007586143000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a fluorescent light guide plate that can be used in a photoelectric conversion device configured to concentrate sunlight and irradiate it to a photovoltaic cell, and a manufacturing method thereof, and more particularly to a fluorescent light guide plate that employs quantum dots as a fluorescent material dispersed within the plate, and a manufacturing method thereof. [Background technology]
[0002] In a photovoltaic power generation system, various configurations have been proposed for concentrating sunlight, which would otherwise be low in intensity, and irradiating it onto photovoltaic cells in order to increase the amount of power generated per photovoltaic cell such as a solar cell, or to reduce the number of photovoltaic cells used while improving the power generation efficiency in the system and reducing the cost or size of the system. For example, Patent Document 1 discloses a photovoltaic power generator in which a solar cell is attached to the side of a light-emitting converter in which magic-sized clusters, which are light-emitting bodies, are embedded in a plate-shaped transparent light-guiding element or in a thin film on the surface of the transparent light-guiding element. In such a photovoltaic power generator, when sunlight is irradiated onto the light-guiding element, the sunlight is absorbed by the light-emitting body, and the light is re-emitted from the light-emitting body in all directions. Most of the re-emitted light is guided to the side of the light-guiding element by internal reflection within the plate of the light-guiding element, and the solar energy is converted into electrical energy by the attached solar cell. According to such a configuration, the energy of sunlight irradiated to a wide area of the surface of the light guide element is collected to a small area of the side surface of the light guide element and can be collected by a solar cell with a small area covering the side surface, which is economically advantageous. In addition, Patent Document 2 by the applicant of the present application discloses a photoelectric conversion device that condenses sunlight and irradiates it to a photovoltaic cell to generate solar power using the photovoltaic cell, the photoelectric conversion device including a fluorescent light guide plate having a plate-like structure formed of a material having a refractive index different from that of the outside and in which a fluorescent material that absorbs sunlight and emits fluorescence is dispersed, and when sunlight is incident on one side of the plate, the fluorescence emitted from the fluorescent material is concentrated on the edge surface and emitted, a first photovoltaic cell placed on the surface of the fluorescent light guide plate and generates power when irradiated with sunlight, a lens layer superimposed on the fluorescent light guide plate and the first photovoltaic cell and configured to condense light incident from the outer surface to the first photovoltaic cell, and a second photovoltaic cell that generates power when irradiated with the fluorescence emitted from the edge surface of the fluorescent light guide plate.In such a photoelectric conversion device, sunlight irradiated onto its upper surface is concentrated by the lens layer onto the light-receiving surface of the first photovoltaic cell, and light that misses the light-receiving surface of the first photovoltaic cell is absorbed by a fluorescent substance in the fluorescent light guide plate and converted into fluorescence, which is then concentrated onto the second photovoltaic cell arranged on the edge surface of the fluorescent light guide plate, thereby recovering as much solar energy as possible even if the direction of the sunlight changes. Note that a configuration similar to the fluorescent light guide plate of the photoelectric conversion device in Patent Document 2 is also used in a solar-pumped laser device in Patent Document 3 by the same applicant as this application. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent Publication No. 2016-131249 [Patent Document 2] Patent Publication No. 2020-062642 [Patent Document 3] Patent Publication No. 2017-168662 Summary of the Invention [Problem to be solved by the invention]
[0004] Regarding the fluorescent material in the fluorescent light guide plate used for collecting sunlight as described above, quantum dots have a wide absorption wavelength, a narrow emission wavelength, and high quantum efficiency, and therefore are advantageously used as a fluorescent material for converting sunlight with a wide wavelength band into fluorescence. When forming a fluorescent light guide plate with quantum dots dispersed therein, typically, a transparent or translucent resin material is mixed into a solution in which the quantum dots are dispersed in an organic solvent such as toluene, and then the resin material is cured while evaporating the organic solvent, thereby forming a plate-shaped member with the quantum dots dispersed therein.
[0005] In this regard, according to research by the inventors of the present invention, when an organic solution containing quantum dots and a resin material (quantum dot-resin solution) is cured as it is to form a plate-like structure having a thickness (for example, about 3 mm or more) sufficient for use as a fluorescent light guide plate, it has been found that the ratio of the light intensity obtained at the edge surface of the plate-like structure to the light intensity irradiated on the light receiving surface of the plate-like structure (hereinafter referred to as "luminous intensity per irradiated light intensity") is significantly reduced, for example to about 1 / 14, compared to the case of a solution in a container having the same dimensions as the plate-like structure. This is thought to be because, when the thickness of the plate-like member of the resin after curing is sufficient for use as a fluorescent light guide plate, it takes a certain amount of time (usually about 24 hours) to evaporate the organic solvent from the quantum dot-resin solution and complete the curing of the resin material, during which the aggregation inhibitor (such as fatty acid such as oleic acid) coating the periphery of the quantum dots peels off, causing the quantum dots to aggregate, resulting in a decrease in the absorption rate or luminous efficiency of the quantum dots (deterioration of the quantum dots), etc. Therefore, the inventors of the present invention have studied the process of producing a fluorescent light guide plate from a quantum dot-resin solution, and have found that in a fluorescent light guide plate formed by spreading the quantum dot-resin solution into a thin film, quickly curing the thin film, and stacking the thin film to form a plate-like structure, the luminescence intensity per unit of irradiated light intensity is significantly increased, for example, by 10 to 12 times, compared to a case in which the quantum dot-resin solution is directly cured to the thickness of the fluorescent light guide plate. This is thought to be because, when the quantum dot-resin solution is cured into a thin film, the resin is cured in a shorter period of time, suppressing or avoiding aggregation of the quantum dots. This finding is utilized in the present invention.
[0006] Thus, a main object of the present invention is to improve the luminescence intensity per unit of irradiated light intensity in a fluorescent light guide plate using quantum dots as a fluorescent material. [Means for solving the problem]
[0007] According to one aspect of the present invention, the above-mentioned problem can be solved by providing a fluorescence light guide plate defined by a first surface, a second surface, and an edge surface connecting peripheral edges of the first and second surfaces, the fluorescence light guide plate having a plate-like structure formed from a material having a refractive index different from that of an exterior and having quantum dots dispersed therein that absorb at least a portion of components of sunlight and emit fluorescence, wherein when sunlight is incident on the first surface, the fluorescence emitted from the quantum dots is concentrated on the edge surface and emitted, The plate-like structure is a fluorescent light guide plate in which a plurality of resin thin films in which the quantum dots are dispersed are laminated. This is achieved by:
[0008] In the above configuration, the "fluorescent light guide plate" is basically a plate-like member configured such that, when light is incident from the broad surface (first surface) of the plate-like structure, the fluorescent material dispersed inside the plate is excited by the light to emit fluorescence, and the fluorescence is guided to the edge surface of the plate-like structure, where it is collected and emitted. The fluorescence emitted by the fluorescent material is emitted in the radial direction from the fluorescent material, and when the refractive index of the fluorescent light guide plate forming the plate-like structure is different from the refractive index of the outside, a part of the fluorescence is transmitted at the interface between the broad surface (first surface, second surface) of the plate-like structure and the outside, but the remaining fluorescence is reflected (when the refractive index of the fluorescent light guide plate is higher than the refractive index of the outside, a considerable amount of the fluorescence is reflected by total reflection.), and as a result, most of the light is collected on the edge surface of the plate-like structure and emitted from there. In such a fluorescent light guide plate, particularly in the present invention, quantum dots are used as the "fluorescent material" dispersed inside the plate-like structure.
[0009] In the case of the fluorescent light guide plate of the present invention, as described above, the plate-like structure is configured in a state in which a plurality of resin thin films in which quantum dots are dispersed are laminated. As already mentioned, when the quantum dot-resin solution is directly cured on the plate-like structure in which quantum dots are dispersed in the fluorescent light guide plate, the quantum dots are deteriorated. However, in the case of a plate-like structure in which the resin thin films in which quantum dots are dispersed, which are formed by thinly spreading the quantum dot-resin solution, are laminated, it has been found that the emission intensity of the quantum dots per unit of irradiation light intensity is significantly increased, for example, by about 10 to 12 times. Therefore, in the fluorescent light guide plate of the present invention, as described above, a plate-like structure in which a plurality of resin thin films in which quantum dots are dispersed are laminated is adopted, and the emission intensity per unit of irradiation light intensity in the fluorescent light guide plate is increased. Note that any quantum dots can be used, for example, CdSe, CdTe, PbS, perovskite quantum dots (CsPbX3, X = Cl, Br, I, etc.). The base resin of the resin thin film may be any transparent or translucent solid resin that has appropriate rigidity when cured, such as, but not limited to, a fluororesin such as tetrafluoroethylene-ethylene copolymer resin (ETFE) or polymethyl methacrylate resin.
[0010] In an embodiment, the plate-like structure in which the resin thin films are laminated in the fluorescent light guide plate of the present invention may be a plate-like structure in which multiple resin thin films and multiple transparent or light-transmitting film materials are alternately laminated. A single resin thin film may have a thickness less than 1 mm, typically about a few tenths of a millimeter, and handling such a thin film alone is troublesome and difficult, such as the thin film being torn. Therefore, by making the plate-like structure in a state in which transparent or light-transmitting film materials and resin thin films are alternately laminated, it becomes possible to make the handling of the plate-like structure easier. The transparent or light-transmitting film material may be any transparent or light-transmitting film, such as a polyester film.
[0011] The resin thin film constituting the plate-like structure of the above-mentioned fluorescent light guide plate of the present invention may be formed by any method, such as spreading a quantum dot-resin solution in which quantum dots and a resin material are dispersed in an organic solvent into a thin film, and drying and curing the solution. Therefore, according to another aspect of the present invention, the object of the present invention is to provide a method for manufacturing a fluorescent light guide plate defined by a first surface, a second surface, and an edge surface connecting the peripheries of the first and second surfaces, in which quantum dots that absorb at least a portion of the components of sunlight and emit fluorescence are dispersed inside the plate-like structure formed from a material having a refractive index different from that of the outside, in which when sunlight is incident from the first surface, the fluorescence emitted from the quantum dots is concentrated on the edge surface and emitted, comprising: A first step of preparing a quantum dot-resin solution in which quantum dots coated with an anti-aggregation agent and a resin material are dispersed in an organic solvent; a second step of forming a resin thin film having the quantum dots dispersed therein from the quantum dot-resin solution; a third step of laminating a plurality of the resin thin films to form the plate-like structure; This is achieved by a method comprising:
[0012] In the above configuration, the "organic solvent" may be any organic solvent that can be used to disperse quantum dots, such as toluene. When quantum dots aggregate in a solution, their absorption characteristics and luminescence characteristics may change or deteriorate, so an anti-aggregation agent is added when the quantum dots are dispersed in an organic solvent. As an anti-aggregation agent, a fatty acid having a hydrocarbon chain, such as oleic acid, is usually used, and in the present invention, a similar anti-aggregation agent is added to the quantum dot-resin solution. In a solution in the presence of the anti-aggregation agent, the quantum dots are in a state of being covered with the anti-aggregation agent, which is thought to prevent the quantum dots from aggregating (in this case, no decrease in the luminescence intensity of the quantum dots is observed).
[0013] In the method of the present invention, as described above, a resin thin film in which quantum dots are dispersed is formed from a quantum dot-resin solution, and a plate-like structure is formed by stacking a plurality of such resin thin films. As already mentioned, according to the configuration of the present invention, it is possible to significantly improve the emission intensity per unit of irradiated light intensity, compared to the one obtained by directly curing the quantum dot-resin solution to form a plate-like structure.
[0014] In an embodiment of the present invention, the resin thin film in which the quantum dots are dispersed may be formed by, more specifically, spreading the quantum dot-resin solution into a thin film, evaporating the organic solvent, and hardening the resin material. Therefore, the resin thin film laminated on the plate-like structure may be a thin film formed in this way. In such a configuration, it is difficult and impractical to detect the state of the thin film during and after its formation, but it is believed that the organic solvent quickly evaporates from the quantum dot-resin solution, and the resin hardens before the quantum dots aggregate, thereby suppressing deterioration of the quantum dots.
[0015] In addition, as described above, when the resin thin film in which quantum dots are dispersed is formed by spreading the quantum dot-resin solution in a thin film form, evaporating the organic solvent, and curing the resin material, the thickness of the formed resin thin film is thinner than 1 mm, typically about several tenths of a millimeter, so that in the resin thin film formation process, the quantum dot-resin solution is applied in a thin film form on a transparent or light-transmitting film material as described above, and then dried and cured to form a resin thin film, and the film material on which the resin thin film is formed is laminated to form a plate-like structure. In the embodiment, more specifically, the quantum dot-resin solution is applied in a thin film form on a transparent or light-transmitting film material to form a resin thin film, and a transparent or light-transmitting film material is further laminated on the formed resin thin film, and the quantum dot-resin solution is applied in a thin film form on the laminated film material to form a resin thin film. By repeating this operation, the resin thin film may be laminated to form a plate-like structure, and such a configuration makes it possible to easily and satisfactorily form a plate-like structure in which a plurality of resin thin films are laminated.
[0016] In the above-mentioned method of the present invention, in order to more reliably remove traces of organic solvent from the plate-like structure formed by laminating a thin resin film, a fourth step of further drying the plate-like structure may be carried out after formation of the plate-like structure.
[0017] In addition, for the purpose of protecting the plate-like structure formed by stacking resin thin films, a transparent or light-transmitting film material may be laminated on the upper and lower surfaces of a laminate consisting of multiple stacked resin thin films.
[0018] Furthermore, according to an experiment, it was found that the luminescence intensity per irradiated light intensity in the completed fluorescent light guide plate is improved when the resin thin film forming and laminating process is performed under an inert gas atmosphere rather than in the air. This is believed to be because oxygen in the air deteriorates the quantum dots or the anti-aggregation agent. Therefore, in the above method, the resin thin film forming and laminating process is preferably performed under an inert gas atmosphere such as argon gas or nitrogen gas. In addition, in order to prevent oxygen in the air from contacting the resin thin film as much as possible, the film material on which the resin thin film is formed or laminated on the resin thin film is preferably an oxygen-impermeable film.
[0019] In the fluorescent light guide plate, it is preferable that the fluorescence emitted from the quantum dots is reflected as much as possible at the first and second surfaces and collected at the edge surface. Therefore, a reflective mirror layer that reflects light without transmitting it may be laminated or applied to the second surface, which is not incident on the excitation light. On the other hand, it is necessary for light that excites the quantum dots from the outside to be incident on the first surface. Therefore, the plate-like structure may be configured so that the refractive index increases from the first surface to the second surface for each layer. With this configuration, total reflection of the light beam traveling from the inside of the plate-like structure to the first surface is likely to occur, so that the amount of light transmitted to the outside from the first surface among the fluorescence emitted from the quantum dots can be reduced as much as possible. Effect of the Invention
[0020] Thus, according to the present invention, in a fluorescent light guide plate having a plate-like structure made of a resin in which quantum dots are dispersed as a fluorescent material, the luminescence intensity per unit of irradiated light intensity can be increased. When solar cells are attached to the edge surface of such a fluorescent light guide plate, higher power generation efficiency can be obtained. The fluorescent light guide plate according to the present invention may be used for various purposes, and is advantageously used as a member for converting sunlight into fluorescence and collecting the light in, for example, the photoelectric conversion device for solar power generation in Patent Document 2 and the solar light pumped laser device described in Patent Document 3.
[0021] Other objects and advantages of the present invention will become apparent from the following description of preferred embodiments of the invention. [Brief description of the drawings]
[0022] [Figure 1] Fig. 1(A) is a schematic perspective view of one embodiment of a fluorescent light guide plate according to the present embodiment, Fig. 1(B) is a schematic perspective view of another embodiment of a fluorescent light guide plate according to the present embodiment, and Fig. 1(C) is a schematic cross-sectional view of yet another embodiment of a fluorescent light guide plate according to the present embodiment. [Diagram 2] 2(A) to (D) are schematic diagrams showing the process of forming a resin thin film from a quantum dot-resin solution and laminating the resin thin film to form a plate-like structure of a fluorescent light guide plate according to this embodiment. (A) shows the state in which the quantum dot-resin solution is placed on a film material, (B) shows the state in which the quantum dot-resin solution is spread into a thin film on the film material, (C) shows the state in which the solvent is evaporated from the thin-film quantum dot-resin solution to harden the resin, and (D) shows the state in which the next film material is laminated on the hardened resin thin film. [Diagram 3] FIG. 3 is a schematic cross-sectional view of the fluorescent light guide plate according to this embodiment when applied as a photoelectric conversion device. [Figure 4]4(A) to (C) are graphs showing the current I and power P obtained in a solar cell when the solar cell is attached to the edge surface of the fluorescent light guide plate and light is irradiated onto the fluorescent light guide plate. (A) is a plate-like structure formed by directly curing the quantum dot-resin solution to have the same thickness as the fluorescent light guide plate, (B) is a plate-like structure formed by stacking resin thin films formed from the quantum dot-resin solution according to the teachings of this embodiment, where the quantum dot concentration in the resin thin films is the same as in (A), and (C) is a plate-like structure formed by stacking resin thin films formed from the quantum dot-resin solution according to the teachings of this embodiment, where the total amount of quantum dots in the plate-like structure is the same as in (A). [Diagram 5] Fig. 5(A) is a schematic perspective view of a state in which a solar cell is attached to the edge surface of a fluorescent light guide plate, and Fig. 5(B) is a schematic cross-sectional view of a part of a fluorescent light guide plate for explaining the mechanism by which fluorescence from quantum dots is concentrated in the fluorescent light guide plate when the fluorescent light guide plate is irradiated with sunlight. [Figure 6] Fig. 6(A) is a schematic cross-sectional view of a quantum dot-resin solution placed in a mold in a process of curing the quantum dot-resin solution as it is to the thickness of a fluorescent light guide plate, and Fig. 6(B) is a schematic cross-sectional view of a plate-like structure of a fluorescent light guide plate obtained by curing the quantum dot-resin solution in the mold of (A). Fig. 6(C) is a schematic diagram showing the expected state of quantum dots in the quantum dot-resin solution, and Fig. 6(D) is a schematic diagram showing the expected state of quantum dots inside a plate-like structure obtained by curing the quantum dot-resin solution as it is in a certain thickness state. [Explanation of symbols]
[0023] 1...Fluorescent light guide plate 2…Plate structure 2m…Resin thin film 2f…Film material 2S: Quantum dot-resin solution 2a...Light receiving surface (upper surface, first surface) of the plate-shaped structure of the fluorescent light guide plate 2b... Back surface (lower surface, second surface) of the plate-like structure of the fluorescent light guide plate 2e...Edge surface of plate-like structure of fluorescent light guide plate 3, 3a…Photovoltaic cell 4...Lens layer 4a…Lens part 4b…Connection part 6…Quantum dots 6a…Quantum dot aggregates 7. Anti-agglomeration agents 7a...adhesive layer (second adhesive layer) 8...Reflective mirror (lower surface of fluorescent light guide plate) 10…Formwork 100...Photoelectric conversion device SL…Solar light FL: Fluorescence BEST MODE FOR CARRYING OUT THEINVENTION
[0024] Basic structure of fluorescent light guide plate 5(A) and (B), the fluorescent light guide plate 1, which is the subject of this embodiment, is basically a member of a plate-like structure 2 having a fluorescent substance dispersed therein. Specifically, as shown in the figure, the plate-like structure 2 of the fluorescent light guide plate 1 is defined by a light receiving surface 2a (front side, first surface) that receives light SL such as sunlight, a back side surface 2b (second surface) thereof, and an edge surface 2e that connects the light receiving surface 2a and the back side surface 2b, and is formed of a material having a higher refractive index for light than the external space and having a fluorescent substance 6 dispersed therein. The fluorescent substance 6 may be, for example, any fluorescent dye, but quantum dots, which have a wide absorption wavelength, a narrow emission wavelength, and high quantum efficiency, are more advantageously used. The base material of the plate-like structure 2 may be any material having transparency or translucency and a refractive index higher than that of air, such as fluororesin (refractive index 1.33), high-refractive polymethylmethacrylate resin (refractive index 1.60), polycarbonate resin (refractive index 1.59), polyester resin (refractive index 1.60), acrylic resin (1.49 to 1.53), silicon resin (1.43), quartz glass (1.54 to 1.55), etc. As shown in the figure, when light SL enters from the light-receiving surface 2a, the fluorescent material 6 inside is excited and emits fluorescence FL in all directions, but since the refractive index of the plate-like structure 2 is higher than that of the external space, total reflection of the fluorescence FL occurs at the light-receiving surface 2a and the back side surface 2b, and the fluorescence FL, except for a part of the light rays whose incident angle with respect to the light-receiving surface 2a and the back side surface 2b is smaller than the critical angle, is repeatedly reflected at the light-receiving surface 2a and the back side surface 2b and reaches the edge surface 2e. According to this configuration, the light received over the wide area of the light-receiving surface 2a can be converted into fluorescence by the fluorescent material 6 and then collected on the smaller area of the edge surface 2c, making it possible to concentrate the energy on the edge surface 2c. Therefore, with the fluorescent light guide plate 1 as shown in the figure, it is possible to convert light that arrives with low energy density, such as sunlight, into a higher density light, and for example, as shown in the figure, by arranging photovoltaic cells 3 on the edge surface 2e of the plate-like structure 2 to convert light energy into electrical energy, it becomes possible to recover light energy using only photovoltaic cells of smaller dimensions.
[0025] Typical method for forming the plate-like structure of the fluorescent light guide plate In forming the fluorescent light guide plate described above, typically, as shown diagrammatically in Figures 6(A) and (B), a resin solution 2S in which a fluorescent substance is dispersed in an organic solvent such as toluene and a resin material is dissolved is poured into a mold 10 having a depth corresponding to the thickness of the plate-like structure 2, the organic solvent in the resin solution 2S is evaporated within the mold 10, the resin material is hardened (H), and solidified into the shape of the plate-like structure 2, thereby forming the plate-like structure 2.
[0026] In this regard, according to the research of the inventors of the present invention, it was observed that, in particular, when quantum dots are used as the fluorescent material, the emission intensity per irradiated light intensity (the ratio of the light intensity obtained at the edge surface of the plate-like structure to the light intensity irradiated on the light-receiving surface of the plate-like structure) in the plate-like structure 2 after solidification is significantly lower than that in the state of the resin solution 2S. This is considered to be due to the deterioration of the quantum dots, that is, the decrease in the fluorescence intensity emitted from the quantum dots per irradiated light intensity, and one of the causes of such deterioration of the quantum dots is considered to be the aggregation of the quantum dots. More specifically, in a dispersion solution of quantum dots, a fatty acid having a hydrocarbon chain such as oleic acid is usually added as an anti-aggregation agent 7 to prevent the aggregation of the quantum dots, as shown in FIG. 6(C). It is considered that such an anti-aggregation agent 7 covers the periphery of each quantum dot due to its chemical properties, thereby preventing the aggregation of the quantum dots. However, as described above, when the resin solution (quantum dot-resin solution) 2S in which quantum dots are dispersed is cured, the organic solvent gradually evaporates over a certain period of time, and in the process in which the ratio of the organic solvent slowly decreases, the anti-aggregation agent 7 is detached from the periphery of the quantum dots 6 while the quantum dots 6 remain mobile, which may cause the quantum dots 6 to form aggregates 6a. When such aggregation of quantum dots occurs, the amount of fluorescence generated in response to the light energy received by the light receiving surface 2a of the fluorescent light guide plate 1 decreases, and the light energy transmitted to the edge surface 2e decreases. Therefore, it is advantageous to have a configuration that can avoid the aggregation of quantum dots when the quantum dot-resin solution is cured as described above.
[0027] Improvement of the plate-like structure of the fluorescent light guide plate according to the present embodiment The inventors of the present invention have conducted various studies on a method for avoiding the deterioration of quantum dots due to the aggregation of quantum dots as described above, and have found that the degree of deterioration of quantum dots is significantly alleviated by curing the quantum dot-resin solution to a resin thin film thinner than the thickness of the plate-like structure 2, rather than curing the quantum dot-resin solution to the thickness of the plate-like structure 2 from the beginning, and forming the plate-like structure 2 by stacking a plurality of such resin thin films 2m as shown in Fig. 1(A). This is because, in the case of a resin thin film formed from a quantum dot-resin solution, the time required for curing each thin film is considerably shorter than the case of curing the quantum dot-resin solution in a mold having a certain depth as shown in Fig. 6(A), (it is difficult and impractical to detect the state of the quantum dots in the thin film), and the resin hardens before the quantum dots aggregate, fixing the quantum dots, and maintaining the state in which each quantum dot is dispersed.
[0028] In the plate-like structure of the fluorescent light guide plate of the present embodiment, specifically, any quantum dot that can absorb light in the wavelength band of sunlight and is chemically stable in an organic solvent or resin may be used as the quantum dot, and for example, CdSe, CdTe, PbS, perovskite quantum dots (CsPbX3, X = Cl, Br, I, etc.) may be used. The base resin of the resin thin film may be any transparent or light-transmitting solid resin that has appropriate rigidity when hardened, and may be, for example, fluororesins such as tetrafluoroethylene-ethylene copolymer resin (ETFE) and polymethyl methacrylate resin, but is not limited thereto. As already mentioned, it is preferable that the resin has a refractive index as high as possible compared with the outside (air) so that the fluorescence from within the plate-like structure is reflected by the light receiving surface 2a and the back side surface 2b as much as possible. The thickness of the resin thin film may be any thickness less than 1 mm, specifically, may be several tenths of a mm, and typically may be about 0.3 mm. The thickness of the plate-like structure may be set arbitrarily depending on the application.
[0029] In addition, when forming the plate-like structure 2 by laminating the resin thin films, as shown in FIG. 1(B), the resin thin film 2m may be laminated in a state in which it is placed or attached on a transparent or light-transmitting film material 2f. That is, in the plate-like structure 2, the resin thin film 2m and the film material 2f may be alternately laminated. As the film material 2f, any transparent or light-transmitting film material such as a polyester film may be used. The thickness of the film material 2f may be, for example, 0.1 mm, but is not limited thereto. By handling the resin thin film 2m in a state in which it is placed or attached on the film material 2f, the lamination operation becomes easier, the risk of breaking the resin thin film 2m during the lamination operation is reduced, and the structural stability of the plate-like structure 2 is improved. In addition, it is preferable that the film material 2f is laminated on the outermost surface (light-receiving surface and back side surface) of the plate-like structure 2 in order to protect the resin thin film 2m. Furthermore, in order to protect the quantum dots from oxygen in the air (it has been observed that quantum dots are also deteriorated by oxygen), it is preferable that the film material 2f is non-permeable to oxygen. As already mentioned, it is preferable that the film material has a refractive index as high as possible compared to the outside (air) so that the fluorescence from within the plate-like structure is reflected by the light-receiving surface 2a and the back surface 2b as much as possible.
[0030] As a further advantageous embodiment, in a plate-like structure consisting of a laminate of a resin thin film and a film material, as shown in Fig. 1(C), materials may be selected so that the refractive index increases from the light-receiving surface 2a to the back surface 2b. With this configuration, the fluorescence from the quantum dots is less likely to transmit from the light-receiving surface side, and the fluorescence can be more reliably collected on the edge surface. A reflective layer that does not transmit light may be laminated on the back surface 2b to prevent the fluorescence from leaking from the back surface 2b.
[0031] Method for forming plate-like structure of fluorescent light guide plate according to the present embodiment The formation of the plate-like structure by laminating the resin thin films in this embodiment may be achieved by any method. For example, in one aspect of the method for forming the plate-like structure of the fluorescent light guide plate according to this embodiment, with reference to FIG. 2, the formation of the resin thin film 2m on the film material 2f and the lamination of the film material 2f on the resin thin film 2m may be repeated. In this aspect, specifically, first, the quantum dot-resin solution 2S is dripped onto the film material 2f (FIG. 2(A)), and spread into a thin film on the film material 2f using an applicator R or the like (FIG. 2(B)). Here, as already described, the quantum dot-resin solution 2S is prepared by dispersing the quantum dots and the anti-aggregation agent in a volatile organic solvent such as toluene that is usually used in this field, and further dissolving the resin material that will harden to become a resin. The respective concentrations of the quantum dots, the anti-aggregation agent, and the resin material may be adjusted according to suitability. In this embodiment, the quantum dot-resin solution 2S is spread into a thin film, and therefore may be adjusted by the applicator R to have a viscosity that allows spreading. If the concentration of the quantum dots is too high, the luminescence intensity of the quantum dots per unit of irradiated light intensity decreases, so the concentration may be adjusted through experiments or the like to optimize the luminescence intensity per unit of irradiated light intensity. The thickness of the solution when spread into a thin film may be any thickness less than 1 mm, and specifically, may be a few tenths of a mm.
[0032] Once the quantum dot-resin solution 2S is spread onto the film material 2f, it is left to stand, during which time the organic solvent evaporates (v), the resin material hardens, and the thin film is solidified (Figure 2(C)). In this case, since the solution is thin, the organic solvent evaporates quickly, for example, in about one minute, and the resin material hardens to form a solidified thin film. Thereafter, a new film material 2f is laminated onto the solidified thin film 2m (Figure 2(D)), and the above process from Figure 2(A) is repeated. The process cycle of Figures 2(A) to (D) may be repeated until the total thickness of the laminate of the resin thin film and film material reaches the thickness required for the plate-like structure.
[0033] Thereafter, although not shown, the laminate of the resin thin film and the film material may be left to dry in order to remove traces of the organic solvent in the resin thin film. After drying, the periphery may be cut in any manner to smooth the edges. Then, a photovoltaic cell or the like may be attached to the edges.
[0034] In addition, since the quantum dots in the solution are easily deteriorated when exposed to oxygen (possible causes include oxidation of the aggregation inhibitor), it is preferable to carry out the above series of steps in an atmosphere of an inert gas such as argon gas or nitrogen gas. According to an experiment on power generation efficiency described later, it has been found that the power generation efficiency increases when the above steps are carried out in an atmosphere of an inert gas.
[0035] Application Examples As already described, the fluorescent light guide plate 1 of this embodiment is advantageously used in a photoelectric conversion device 100 as illustrated in Fig. 3. Referring to Fig. 3, the photoelectric conversion device 100 includes the fluorescent light guide plate 1 made of a plate-like structure 2, a photovoltaic cell 3a placed on an upper surface 2a of the plate-like structure 2, a lens layer 4 superimposed on the upper surface 2a and the photovoltaic cell 3a, and a photovoltaic cell 3 arranged on an edge surface 2e of the plate-like structure 2. As illustrated, the electric power generated by each of the photovoltaic cells 3, 3a may be extracted to the outside through a power line (not shown).
[0036] In this configuration, the fluorescent light guide plate 1 is used as a substrate on which photovoltaic cells 3a that absorb sunlight and generate electricity are disposed, and at the same time, it receives light that is not irradiated to the photovoltaic cells 3a, converts the light into fluorescence by the quantum dots dispersed therein as described above, and collects the light on the edge surface 2e. A reflection mirror 8 that reflects light but does not transmit it may be applied to the lower surface 2b of the fluorescent light guide plate 1, thereby preventing the transmission of light from the lower surface 2b and allowing more light to reach the edge surface 2e.
[0037] The photovoltaic cell 3a mounted on the upper surface 2a of the fluorescent light guide plate 1 may be any type of solar cell or photoelectric conversion element that absorbs the light components of sunlight and generates electricity. As already mentioned, the wavelength band of sunlight is wide, and in the illustrated example, as will be described later, the sunlight SL is concentrated by the lens 4a and irradiated to the photovoltaic cell 3a, so that a photovoltaic cell that can absorb a wide wavelength band and has high power generation efficiency even when irradiated with a relatively high light intensity is advantageously used. Specifically, a III-V group multi-junction solar cell may be selected as the photovoltaic cell 3a. Other types of photovoltaic cells, such as CIS solar cells, crystalline silicon solar cells, amorphous silicon solar cells, and perovskite solar cells, may also be adopted as the photovoltaic cell 3a.
[0038] The lens layer 4 may have a layered structure having lens portions 4a formed to condense and irradiate sunlight onto each of the photovoltaic cells 3a, and connection portions 4b connecting the lens portions 4a. The lens layer 4 may be formed of a transparent or light-transmitting material having a refractive index higher than that of air, and specifically, the material may be silicone resin (refractive index 1.43), low-refractive polymethyl methacrylate (refractive index 1.40), or soda glass (refractive index 1.51). The material of the lens layer 4 may preferably have a refractive index lower than that of the plate-like structure 2 so that the light entering the fluorescent light guide plate 1 and the fluorescence emitted by the fluorescent light guide plate 1 are confined within the plate-like structure 2. In addition, in the lens layer 4, the lens portions 4a are formed to condense the light arriving at its outer surface (the surface opposite to the surface facing or close to the fluorescent light guide plate 2, the upper surface in the figure) onto the photovoltaic cells 3a. The shape of the lens portion 4a may be a spherical lens, but preferably it may be an aspherical-asymmetric lens adjusted so as to concentrate as many light components as possible that are incident on the lens surface at various angles of incidence, including not only direct light arriving as parallel light from sunlight, but also sunlight scattered by clouds or air, or sunlight reflected or scattered by buildings, etc., onto the photovoltaic cell 3a.
[0039] As the photovoltaic cell 3 on the edge surface 2e of the fluorescent light guide plate 1 that absorbs the fluorescent light (and sunlight) emitted from that surface to generate electricity, any type of solar cell or photoelectric conversion element that absorbs light components in the wavelength band of the fluorescent light may be used, and for example, a CIS solar cell, a crystalline silicon solar cell, an amorphous silicon solar cell, or a perovskite solar cell may be selected (although the more expensive III-V multi-junction solar cell may also be used).
[0040] It is preferable that the above-mentioned device can be deformed to some extent to fit the shape of the object where it is installed, such as the roof of a moving body, etc. Therefore, the fluorescent light guide plate and the lens layer may be made of a flexible material, and the entire device may be bendable.
[0041] In operation, when sunlight is irradiated from above the lens layer 4, the light incident on the lens portion 4a is first concentrated by the lens action onto the photovoltaic cell 3a, which receives the light and generates electricity. Typically, the lens portion 4a is shaped so that the light (sunlight) incident along its optical axis (perpendicular to the surface of the center portion of the lens portion 4a), i.e., the light with an incident angle of approximately 0°, is refracted toward the light receiving surface of the photovoltaic cell 3a (the upper surface in the figure). However, the greater the incident angle θ of the light incident on the lens portion 4a, the more the amount of light that passes through the lens portion 4a that deviates from the light receiving surface of the photovoltaic cell 3a increases, and as can be seen from the figure, if there are connection portions 4b between adjacent lens portions 4a in the lens layer 4, the light that is incident on these portions does not hit the photovoltaic cell 3a and is not used for power generation. In the device shown in the figure, the light that has missed the light-receiving surface of the photovoltaic cell 3a is received by the fluorescent light guide plate 1, and the quantum dots dispersed within the plate are excited by the sunlight and emit fluorescence when they miss the light from the photovoltaic cell 3a. The emitted fluorescence propagates to the edge surface 2e, where it is concentrated and emitted, and is recovered as electricity by the photovoltaic cell 3 arranged there.
[0042] Thus, with the above-mentioned configuration, even if part of the light condensed by the lens layer 4 misses the photovoltaic cell 3a, the energy can be extracted as electricity in the photovoltaic cell 3 via the fluorescent light guide plate 1, improving robustness against the incidence angle of sunlight incident on the lens layer 4. Furthermore, if there are connection parts 4b between adjacent lens parts 4a of the lens layer 4, the energy of sunlight that enters these parts is also converted into electricity, further improving the energy conversion efficiency.
[0043] Experimental Example The above-described effects of the present embodiment were confirmed by the following experiments. It should be understood that the following experimental examples are merely illustrative of the effectiveness of the present embodiment, and do not limit the scope of the present invention.
[0044] In the experiment, to put it simply, a quantum dot-resin solution in which quantum dots and a resin material are dispersed in an organic solvent is prepared, and the quantum dot-resin solution is poured into a mold with a certain depth and cured as it is to form a plate-like structure. A plate-like sample (previous example) was prepared by laminating a resin thin film formed from the quantum dot-resin solution on a transparent film material to form a plate-like structure. In order to evaluate the luminous intensity per irradiated light intensity, a photovoltaic cell was attached to the edge surface of each prepared plate-like sample, and each plate-like sample was irradiated with simulated sunlight using a solar simulator, the generated power was measured, and the power generation efficiency was calculated and compared. For comparison, the power generation efficiency was also calculated in the quantum dot-resin solution state in the same manner.
[0045] Regarding the preparation of the plate-shaped sample, in more detail, in the previous example, first, 2.13 ml of a quantum dot solution in which quantum dots PbS were dispersed in toluene at 10,000 ppm, 10 ml of toluene, 36 g of a fluororesin (Lumiflon (registered trademark) 910LM), and 12 g of a hexamethylene diisocyanate-based polyisocyanate (Duranate (registered trademark)) were mixed and stirred for 10 minutes to prepare a quantum dot-resin solution. The prepared quantum dot-resin solution was poured into a square mold with a depth of 4 mm, and left to dry at room temperature for 24 hours to harden. Note that when hardened, the toluene evaporates, so the thickness of the formed plate-shaped member became about 3 mm. Thereafter, the formed plate-shaped member was removed from the mold, and the four sides were cut with a pencil cutter to form edge surfaces, and a general-purpose photovoltaic cell (crystalline silicon solar cell) was attached to the edge surfaces using instant adhesive (α,α-cyanoacrylic acid ester).
[0046] In this embodiment, as the first embodiment, the same quantum dot-resin solution as in the previous embodiment was prepared, and the quantum dot-resin solution was dropped onto a transparent, gas-impermeable polyester film material (Lumirror (registered trademark) film T60) having a thickness of about 0.1 mm, and the quantum dot-resin solution was applied using a 125 μm applicator, and left to stand for 1 minute at room temperature to form a resin thin film. Then, a polyester film material was further laminated onto the formed resin thin film, and the formation of a resin thin film by dropping, applying, and drying the quantum dot-resin solution was repeated until the thickness of the laminate reached 3 mm. The above film material was further laminated on the top surface. After that, in order to remove traces of toluene in the cured resin, the product was left to stand for 30 minutes at room temperature, and, as in the previous embodiment, the four side surfaces were cut with a pencil cutter to form edge surfaces, and a general-purpose photovoltaic cell was attached to the entire edge surface using instant adhesive to create a plate-shaped sample. The above series of operations were all performed in a glove box under an argon atmosphere. In this state, the top and bottom of the plate-shaped member are covered with film material, and the edges are covered with instant adhesive and photovoltaic cells, so even if the plate-shaped member is exposed to the air, the resin will not come into contact with the air. In the case of this first embodiment, the quantum dot concentration in the resin is the same as in the previous example.
[0047] In addition, as a second embodiment, the quantum dot-resin solution was prepared in the same manner as in the previous embodiment, but with 4.26 ml of quantum dot solution and 8 ml of toluene, and the prepared quantum dot-resin solution was used to form and stack a resin thin film and bond a photovoltaic cell in the same manner as in the first embodiment, to create a plate-shaped sample. In this second embodiment, the total amount of quantum dots in the resin is the same as in the previous embodiment.
[0048] When measuring the amount of electricity generated in the quantum dot-resin solution state, the same quantum dot-resin solution as in the previous example was poured into a mold (depth 3 mm) with a photovoltaic cell attached to a glass periphery to prepare a sample for measurement.
[0049] The emission intensity per unit of irradiated light intensity on the plate-shaped samples was evaluated by applying a solar simulator to each plate-shaped sample at 100 mW / cm 2 The plate-shaped sample was irradiated with simulated sunlight of AM1.5 spectrum and the power generation (mW) of the photovoltaic cells attached to the four edge surfaces of the plate-shaped sample was measured. The power generation efficiency was calculated from the measured values using the following formula. Power generation efficiency (%) = Pt [mW] / (100 [mW / cm 2 ]×A[cm 2 ]) …(1) Here, Pt is the total power generated by the photovoltaic cell, and A is the area of the light-receiving surface of the plate-shaped sample. The power generation efficiency (%) corresponds to the ratio of the light intensity obtained at the edge surface of the plate-shaped structure to the light intensity irradiated on the light-receiving surface of the plate-shaped structure (the light emission intensity per unit of the irradiated light intensity).
[0050] In the results, first, referring to the characteristics of the generated power P and generated current I with respect to the generated voltage in the photovoltaic cell attached to each plate-shaped sample in Figs. 4(A) to (C), it can be seen that the generated power and generated current are significantly increased in both the first example (B) and the second example (C) of this embodiment compared to the conventional example (A). The maximum value of the power generation efficiency in each plate-shaped sample was 0.5% in the conventional example, whereas the maximum value of the power generation efficiency in the first example, in which the quantum dot concentration is the same as in the conventional example, was 5%, and the maximum value of the power generation efficiency in the second example, in which the total amount of quantum dots is the same as in the conventional example, was 6%. This corresponds to an improvement in the luminescence intensity per irradiated light intensity to 10 to 12 times that of the conventional example in this embodiment. In addition, since the maximum value of the power generation efficiency was 7% in the quantum dot-resin solution state, it can be seen that the deterioration of the quantum dots is significantly suppressed in this embodiment compared to the conventional example. These results show that in a fluorescent light guide plate, by constructing a plate-like structure by laminating thin resin films formed from a quantum dot-resin solution in accordance with the teachings of this embodiment, the luminescence intensity per unit of irradiated light intensity can be maintained at a state closer to that of the quantum dot-resin solution.
[0051] Thus, as described above, in the fluorescent light guide plate according to this embodiment, in which the plate-like structure is formed by laminating a plurality of resin thin films in which quantum dots are dispersed, the quantum dots are hardly deteriorated when the quantum dot-resin solution is cured directly to the thickness of the plate-like structure, and the luminescence intensity per unit of irradiated light intensity can be maintained at a higher level. The fluorescent light guide plate of this embodiment is expected to be advantageously used in solar light photoelectric conversion devices and solar light pumped laser devices.
[0052] The above description has been given in relation to the embodiment of the present invention, but it will be apparent to those skilled in the art that many modifications and changes can be easily made thereto, and that the present invention is not limited to the embodiment exemplified above, but can be applied to various devices without departing from the concept of the present invention.
Claims
1. A method for manufacturing a fluorescent light guide plate defined by a first surface, a second surface, and an edge surface connecting peripheral edges of the first and second surfaces, the fluorescent light guide plate having a plate-like structure formed from a material having a refractive index different from that of an exterior and having quantum dots dispersed therein that absorb at least a portion of components of sunlight and emit fluorescence, the fluorescent light guide plate having a plate-like structure formed from a material having a refractive index different from that of an exterior and in which, when sunlight is incident on the first surface, the fluorescence emitted from the quantum dots is concentrated on the edge surface and emitted, the method comprising the steps of: A first step of preparing a quantum dot-resin solution in which quantum dots coated with an anti-aggregation agent and a resin material are dispersed in an organic solvent; a second step of spreading the quantum dot-resin solution into a thin film, evaporating the organic solvent, and hardening the resin material to form a resin thin film having a thickness of less than 1 mm and having the quantum dots dispersed therein; a third step of stacking a plurality of the resin thin films so that the plurality of resin thin films are stacked to form the plate-like structure; The method includes:
2. 2. The method of claim 1, wherein in the second step, the quantum dot-resin solution is applied in a thin film form onto a transparent or light-transmitting film material to form the resin thin film, and in the third step, the film material on which the resin thin film is formed is laminated to form the plate-like structure.
3. The method of claim 2, comprising laminating a transparent or light-transmitting film material on the resin thin film formed in the second step, and repeatedly applying the quantum dot-resin solution in a thin film form onto the laminated film material to form the resin thin film, thereby laminating the resin thin film to form the plate-like structure.
4. 4. The method according to claim 1, further comprising a fourth step of further drying the plate-like structure after the formation of the plate-like structure.
5. 3. The method of claim 2, wherein the transparent or light-transmitting film material has a thickness of 0.1 mm.
6. 2. The method according to claim 1, wherein a transparent or light-transmitting film material is laminated on the upper and lower surfaces of a laminate consisting of a plurality of laminated resin thin films.
7. 2. The method of claim 1, wherein the second and third steps are carried out under an inert gas atmosphere.
8. 2. The method of claim 1, wherein the refractive index of the plate-like structure increases layer by layer from the first surface to the second surface.
Citation Information
Patent Citations
Planar fluorescent condenser with scattering particles and fluorescent quantum dots and method for preparing planar fluorescent condenser
CN106330084A
Solar power generator and manufacturing method of the same
JP2016131249A
Sunlight excitation laser device
JP2017168662A
Sunlight excitation laser device