Multilayer Ceramic Capacitors
The multilayer ceramic capacitor addresses chipping issues by incorporating a curved ridgeline and non-overlapping internal electrodes, enabling a thinner side margin portion without compromising structural integrity.
Patent Information
- Application Number
- JP2023021412
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-02-15
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2040-01-17
AI Technical Summary
Reducing the thickness of the side margin portion in multilayer ceramic capacitors leads to a smaller radius of curvature at the ridgeline, increasing the likelihood of chipping.
The multilayer ceramic capacitor design features a curved first ridgeline portion with a larger radius of curvature and a thinner side margin portion, ensuring the internal electrodes do not overlap with the ridgeline, and using dielectric layers with specific thicknesses to support this structure.
This design effectively suppresses chipping while allowing for a thinner side margin portion, maintaining structural integrity and reducing the risk of damage.
Smart Images

Figure 0007586206000001 
Figure 0007586206000002 
Figure 0007586206000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a multilayer ceramic capacitor. [Background technology]
[0002] 2. Description of the Related Art Multilayer ceramic capacitors are known that have a structure in which a laminate is formed by alternately stacking a plurality of dielectric layers and internal electrodes, and external electrodes are formed on both end faces of the laminate.
[0003] As one such multilayer ceramic capacitor, Patent Document 1 describes a multilayer ceramic capacitor that is said to be capable of preventing cracks and peeling at the bonding interface between a laminated portion in which dielectric layers and internal electrodes are laminated in a laminate and a side margin portion that is disposed on the side of the laminated portion and covers the periphery of the internal electrodes. Patent Document 1 also describes a method for producing an unfired laminate by providing an unfired side margin portion on the side of a laminated chip obtained by stacking and cutting a plurality of ceramic green sheets on which internal electrode patterns are formed. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2019-79977 A Summary of the Invention [Problem to be solved by the invention]
[0005] Here, it is preferable to make the thickness of the side margins, which do not contribute to the capacitance of the capacitor, as thin as possible. If the thickness of the side margins is made thin, the radius of curvature of the ridges of the laminate becomes small, but the small radius of curvature makes the ridges of the multilayer ceramic capacitor more susceptible to chipping.
[0006] The present invention is devised to solve the above-mentioned problems, and has an object to provide a multilayer ceramic capacitor that can suppress chipping even when the thickness of the side margin portion is reduced. [Means for solving the problem]
[0007] The multilayer ceramic capacitor of the present invention is a laminate including a plurality of laminated dielectric layers and a plurality of internal electrodes, the laminate having a first main surface and a second main surface facing each other in a lamination direction of the dielectric layers and the internal electrodes, a first side surface and a second side surface facing each other in a width direction perpendicular to the lamination direction, and a first end surface and a second end surface facing each other in a length direction perpendicular to the lamination direction and the width direction; external electrodes electrically connected to the internal electrodes and provided on the first end surface and the second end surface of the laminate; Equipped with a first ridge portion connecting a straight line connecting one ends of two of the internal electrodes positioned outermost in the stacking direction and one of the first main surface and the second main surface has a first curved line, and a second ridge portion connecting one of the first main surface and the second main surface and one of the first side surface and the second side surface has a second curved line, When viewed in the stacking direction, ends of all of the internal electrodes are located so as not to overlap with the first ridge portion, the dielectric layers include outer-layer dielectric layers positioned between the internal electrode positioned at the outermost side in the stacking direction and the first main surface of the laminate, and between the internal electrode positioned at the outermost side in the stacking direction and the second main surface of the laminate, and inner-layer dielectric layers positioned between a plurality of the internal electrodes adjacent to each other in the stacking direction, The thickness of the outer dielectric layer is smaller than the radius of curvature of the first curve. Effect of the Invention
[0008] In the multilayer ceramic capacitor of the present invention, a first ridge line connecting a straight line connecting one ends of two internal electrodes located on the outermost sides in the stacking direction with one of the first and second main surfaces has a first curved line, and a second ridge line connecting one of the first and second main surfaces with one of the first and second side surfaces has a second curved line. That is, since the shape of the first ridge line of the structure before the side margin is formed is a curved shape, the radius of curvature of the second ridge line located on the surface of the multilayer ceramic capacitor can be made large. This makes it possible to suppress chipping even when the thickness of the side margin is made thin. [Brief description of the drawings]
[0009] [Figure 1] 1 is a perspective view illustrating a multilayer ceramic capacitor according to a first embodiment of the present invention. [Diagram 2] 2 is a schematic cross-sectional view taken along line II-II of the multilayer ceramic capacitor shown in FIG. [Diagram 3] 3 is a schematic cross-sectional view taken along line III-III of the multilayer ceramic capacitor shown in FIG. [Figure 4] 1 is an enlarged view of an end portion in the width direction of an internal electrode when a laminate is cut at a central position in the longitudinal direction and a cross section defined by the width direction and lamination direction is viewed. FIG. [Diagram 5] 1A and 1B are diagrams for explaining an example of a method for manufacturing a multilayer ceramic capacitor, in which (a) is a schematic diagram showing a ceramic green sheet on which a conductive film is formed, and (b) is a schematic diagram showing a state in which the ceramic green sheets on which the conductive film is formed are laminated. [Figure 6] 1 is a perspective view showing an example of the appearance of an unfired structure produced during the manufacture of a multilayer ceramic capacitor; [Figure 7] 1 is a side view of a fired structure produced during the manufacture of a multilayer ceramic capacitor. FIG. [Figure 8]FIG. 2 is a cross-sectional view of a multilayer ceramic capacitor according to a reference embodiment, the cross-sectional view being defined in the width direction and the lamination direction by cutting a laminate at a central position in the length direction. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] The features of the present invention will be described in detail below with reference to embodiments of the present invention.
[0011] Fig. 1 is a perspective view showing a multilayer ceramic capacitor 10 according to a first preferred embodiment of the present invention. Fig. 2 is a schematic cross-sectional view taken along line II-II of the multilayer ceramic capacitor 10 shown in Fig. 1. Fig. 3 is a schematic cross-sectional view taken along line III-III of the multilayer ceramic capacitor 10 shown in Fig. 1.
[0012] 1 to 3, the multilayer ceramic capacitor 10 is an electronic component having an overall rectangular parallelepiped shape, and includes a laminate 11 and a pair of external electrodes 20a, 20b. The pair of external electrodes 20a, 20b are disposed to face each other as shown in FIG.
[0013] Here, the direction in which the pair of external electrodes 20a, 20b face each other is defined as the length direction L of the multilayer ceramic capacitor 10, the direction in which the dielectric layers 12 and the internal electrodes 13a, 13b, which will be described later, are stacked is defined as the stacking direction T, and the direction perpendicular to both the length direction L and the stacking direction T is defined as the width direction W. Any two directions out of the length direction L, the stacking direction T, and the width direction W are perpendicular to each other.
[0014] 3 is a cross-sectional view of the laminate 11 cut at the center position in the length direction L, defined by the width direction W and the lamination direction T. The center position of the laminate 11 in the length direction L and the center position of the multilayer ceramic capacitor 10 in the length direction L are the same position.
[0015] The laminate 11 has a first end face 15a and a second end face 15b facing each other in the longitudinal direction L, a first main surface 16a and a second main surface 16b facing each other in the stacking direction T, and a first side surface 17a and a second side surface 17b facing each other in the width direction W.
[0016] The corners and ridges of laminate 11 are rounded. Here, a corner is a portion where three faces of laminate 11 intersect, and a ridge is a portion where two faces of laminate 11 intersect.
[0017] The dimension of the multilayer ceramic capacitor 10 in the length direction L is, for example, 0.4 mm or more and 3.2 mm or less, the dimension in the width direction W is, for example, 0.2 mm or more and 1.6 mm or less, and the dimension in the stacking direction T is, for example, 0.2 mm or more and 1.6 mm or less. However, the dimensions of the laminate 11 are not limited to the above-mentioned numerical values. The dimensions of the laminate 11 can be measured with a micrometer or an optical microscope.
[0018] 2 and 3, the laminate 11 includes a plurality of laminated dielectric layers 12, a plurality of internal electrodes 13a, 13b, and a side margin portion 14. The internal electrodes 13a, 13b include a first internal electrode 13a and a second internal electrode 13b. As shown in Fig. 3, the first internal electrodes 13a and the second internal electrodes 13b are alternately laminated with the dielectric layers 12 interposed therebetween, and side margin portions 14 are provided on both outer sides in the width direction W.
[0019] As shown in Figures 2 and 3, the dielectric layer 12 includes an outer layer dielectric layer 121 located outside in the stacking direction T of the internal electrodes 13a, 13b located at the outermost positions in the stacking direction T, and an inner layer dielectric layer 122 located between two internal electrodes 13a, 13b adjacent to each other in the stacking direction T.
[0020] More specifically, the outer dielectric layer 121 is a layer located between the inner electrodes 13a, 13b located on the outermost sides in the stacking direction T and the first and second main surfaces 16a, 16b of the laminate 11. The inner dielectric layer 122 is a layer located between the first inner electrode 13a and the second inner electrode 13b adjacent to each other in the stacking direction T. The thickness of the outer dielectric layer 121 is, for example, 5 μm or more and 50 μm or less, and is preferably smaller than the radius of curvature of the first curve 18a described later. The thickness of the inner dielectric layer 122 is, for example, 0.35 μm or more and 1.8 μm or less.
[0021] The dielectric layer 12 is made of a ceramic material whose main components are, for example, BaTiO3, CaTiO3, SrTiO3, CaZrO3, etc. These main components may also contain sub-components such as Mn compounds, Fe compounds, Cr compounds, Co compounds, and Ni compounds.
[0022] The side margin portion 14 is a region located between the first side surface 17a of the laminate 11 and the internal electrodes 13a, 13b, and between the second side surface 17b of the laminate 11 and the internal electrodes 13a, 13b in the width direction W. In other words, when an arbitrary cross section including the length direction L and width direction W of the laminate 11 is viewed from the stacking direction T, the side margin portion 14 is a region where neither the first internal electrode 13a nor the second internal electrode 13b is present.
[0023] The dimension L1 (see FIG. 3) of the side margin portion 14 in the width direction W, that is, the thickness of the side margin portion 14, is not less than 5 μm and not more than 50 μm.
[0024] As one example, the side margin portion 14 is made of resin and glass. In this case, the resin may be a thermosetting resin such as an epoxy resin. As another example, the side margin portion 14 is made of ceramic containing alumina and glass.
[0025] The first internal electrode 13a is extended to the first end face 15a of the laminate 11, but is not extended to the second end face 15b. The second internal electrode 13b is extended to the second end face 15b of the laminate 11, but is not extended to the first end face 15a.
[0026] The first internal electrode 13a includes a counter electrode portion that faces the second internal electrode 13b, and an extended electrode portion that is extended from the counter electrode portion to the first end face 15a of the laminate 11. The second internal electrode 13b includes a counter electrode portion that faces the first internal electrode 13a, and an extended electrode portion that is extended from the counter electrode portion to the second end face 15b of the laminate 11.
[0027] A capacitance is formed by the opposing electrode portion of the first internal electrode 13a and the opposing electrode portion of the second internal electrode 13b facing each other via the dielectric layer 12, and thus the electrode portion functions as a capacitor.
[0028] The first internal electrode 13a and the second internal electrode 13b contain, for example, metals such as Ni, Cu, Ag, Pd, and Au, or an alloy of Ag and Pd, etc. The first internal electrode 13a and the second internal electrode 13b may further contain dielectric particles having the same composition as the ceramic contained in the dielectric layer 12.
[0029] The thickness of the first internal electrode 13a and the second internal electrode 13b is, for example, 0.3 μm or more and 1.0 μm or less. The number of stacked internal electrodes including the first internal electrode 13a and the second internal electrode 13b is, for example, 100 sheets or more and 800 sheets or less.
[0030] Fig. 4 is an enlarged view of the ends of the internal electrodes 13a, 13b in the width direction W when the laminate 11 is cut at the center position in the length direction L and a cross section defined by the width direction W and the lamination direction T is viewed. In Fig. 3, the ends of the internal electrodes 13a, 13b in the width direction W appear to be aligned, but in reality, as shown in Fig. 4, which is an enlarged view, the ends of the internal electrodes 13a, 13b in the width direction W are not aligned.
[0031] 4 shows only the ends of some of the internal electrodes 13a, 13b, but in the multilayer ceramic capacitor 10 of this embodiment, when the laminate 11 is cut at the center position in the length direction L and a cross section defined by the width direction W and the stacking direction T is viewed, it is preferable that the variation in the distance in the width direction W from a straight line 30 connecting one ends of the two internal electrodes 13a, 13b positioned on the outermost sides in the stacking direction T to the end of each of the multiple internal electrodes 13a, 13b is 0.2 or less. The variation in the distance is a value obtained by dividing the deviation of the internal electrodes 13a, 13b from the average value of the distance by the average value of the distance. For example, when the distances in the width direction W from the straight line 30 to the ends of the internal electrodes 13a, 13b are L1, L2, L3, ..., Ln (n is the total number of the internal electrodes 13a, 13b), and the average value of all the distances ((L1+L2+L3+...+Ln) / n) is La, the deviations of the distances from the average value of the internal electrodes 13a, 13b are (L1-La), (L2-La), (L3-La), ..., (Ln-La), and the variations are (L1-La) / La, (L2-La) / La, (L3-La) / La, ..., (Ln-La) / La. It is preferable that all of these variations are 0.2 or less.
[0032] For example, by forming the side margin portion 14 separately, rather than fabricating the dielectric layer 12 and the side margin portion 14 integrally, as in the manufacturing method described below, a structure can be obtained in which the ends of the internal electrodes 13a, 13b are aligned within a certain range.
[0033] Here, when looking at the cross section shown in Fig. 3, that is, the cross section defined by the width direction W and the stacking direction T by cutting the laminate 11 at the center position in the length direction L, the straight line 30 connecting one end of the two internal electrodes 13a, 13b located on the outermost sides in the stacking direction T and one of the first main surface 16a and the second main surface 16b has a first curved line 18a with a curvature radius of 10 µm or more. In Fig. 3, the straight line 30 connecting one end of the first internal electrode 13a and the second internal electrode 13b located on both outer sides in the stacking direction T located on the first side surface 17a side is shown, but the same is true when a straight line connecting the other ends located on the second side surface 17b side is drawn. In other words, the first ridge line 18 located on the second side surface 17b side also has a first curved line 18a with a curvature radius of 10 µm or more.
[0034] Also, when looking at the cross section shown in FIG. 3, the second ridge portion 19 connecting one of the first main surface 16a and the second main surface 16b and one of the first side surface 17a and the second side surface 17b has a second curve 19a whose radius of curvature is smaller than that of the first curve 18a. That is, the radius of curvature of the first curve 18a located on the inside is larger than that of the second curve 19a located on the outside. Preferably, the radius of curvature of the first curve 18a is 10% or more larger than that of the second curve 19a. In the cross section shown in FIG. 3, there are four second ridge portions 19, each of which has a second curve 19a whose radius of curvature is 8 μm or more.
[0035] These radii of curvature depend on the size of the laminate 11. When the dimension of the laminate 11 in the stacking direction T is 0.3 mm and the dimension in the width direction W is 0.3 mm, the radius of curvature of the second curve 19a is 13 μm or more and 24 μm or less, and the radius of curvature of the first curve 18a is 16 μm or more and 28 μm or less. When the dimension of the laminate 11 in the stacking direction T is 0.5 mm and the dimension in the width direction W is 0.5 mm, the radius of curvature of the second curve 19a is 25 μm or more and 42 μm or less, and the radius of curvature of the first curve 18a is 30 μm or more and 50 μm or less. When the dimension of the laminate 11 in the stacking direction T is 1.25 mm and the dimension in the width direction W is 1.25 mm, the radius of curvature of the second curve 19a is 33 μm or more and 167 μm or less, and the radius of curvature of the first curve 18a is 40 μm or more and 200 μm or less. When the dimension of the laminate 11 in the stacking direction T is 1.6 mm and the dimension in the width direction W is 1.6 mm, the radius of curvature of the second curve 19a is 42 μm or more and 167 μm or less, and the radius of curvature of the first curve 18a is 50 μm or more and 200 μm or less.
[0036] Here, the radius of curvature of the first curve 18a of the first ridgeline 18 and the radius of curvature of the second curve 19a of the second ridgeline 19 are determined by cutting the laminate 11 at the center position in the length direction L or polishing it up to the center position to expose a cross section defined by the width direction W and the stacking direction T, and observing the first ridgeline 18 and the second ridgeline 19 in the cross section with a scanning electron microscope. The radius of curvature of the curves can be determined by a known method.
[0037] An extension of the above-mentioned straight line 30 intersects with the second curved line 19a. That is, due to the presence of the side margin portion 14, the first side surface 17a and the second side surface 17b are located outside the ends of the internal electrodes 13a, 13b in the width direction W. Therefore, an extension of the straight line 30 connecting one ends of the two internal electrodes 13a, 13b located on the outermost sides in the stacking direction T intersects with the second curved line 19a.
[0038] Here, if the ridgeline of the structure before the side margins are formed is a right angle, reducing the thickness of the side margins reduces the radius of curvature of the ridgeline on the surface of the multilayer ceramic capacitor, making chipping more likely to occur. However, in the multilayer ceramic capacitor 10 of this embodiment, the first ridgeline 18 of the structure before the side margins 14 are formed is curved, so that the radius of curvature of the second ridgeline 19 located on the surface of the multilayer ceramic capacitor 10 can be made large. Therefore, even if the thickness of the side margins 14 is reduced, chipping can be suppressed.
[0039] That is, in the multilayer ceramic capacitor 10 of this embodiment, the thickness of the side margin portion 14 can be reduced and the occurrence of chipping can be suppressed.
[0040] Here, the thickness of the dielectric layer 12 and the thickness of each of the first inner electrode 13a and the second inner electrode 13b can be measured by the following method.
[0041] First, a cross section defined by the stacking direction T and width direction W at the center of the length direction L of the laminate 11, in other words, a surface perpendicular to the length direction L of the laminate 11 is polished to the center of the length direction L to expose the cross section, and the cross section is observed with a scanning electron microscope. Next, the thickness of the dielectric layer 12 is measured on a total of five lines, including a center line along the stacking direction T that passes through the center of the exposed cross section, and two lines drawn equally spaced on each side of the center line. The average of these five measured values is defined as the thickness of the dielectric layer 12.
[0042] In order to obtain a more accurate measurement, the laminate 11 is divided into an upper portion, a central portion, and a lower portion in the stacking direction T, and the above-mentioned five measurement values are obtained for each of the upper portion, the central portion, and the lower portion, and the average value of all the measurement values obtained is regarded as the thickness of the dielectric layer 12.
[0043] The method for measuring the thickness of the dielectric layer 12 has been described above, but the thicknesses of the first internal electrode 13a and the second internal electrode 13b can also be measured using a scanning electron microscope in a similar manner to the method for measuring the thickness of the dielectric layer 12, on the same cross section as the cross section where the thickness of the dielectric layer 12 was measured.
[0044] The first external electrode 20a is provided on the first end face 15a of the laminate 11. In this embodiment, the first external electrode 20a is formed on the entire first end face 15a of the laminate 11, and is formed so as to extend from the first end face 15a to the first main face 16a, the second main face 16b, the first side face 17a, and the second side face 17b. The first external electrode 20a is electrically connected to the first internal electrode 13a.
[0045] The second external electrode 20b is provided on the second end face 15b of the laminate 11. In this embodiment, the second external electrode 20b is formed on the entire second end face 15b of the laminate 11, and is formed so as to extend from the second end face 15b around the first main face 16a, the second main face 16b, the first side face 17a, and the second side face 17b. The second external electrode 20b is electrically connected to the second internal electrode 13b.
[0046] The first external electrode 20a and the second external electrode 20b each include, for example, a base electrode layer and a plating layer disposed on the base electrode layer.
[0047] The base electrode layer includes at least one layer selected from the group consisting of a baked electrode layer, a resin electrode layer, and a thin-film electrode layer, as described below.
[0048] The baked electrode layer is a layer containing glass and metal, and may be a single layer or multiple layers. The baked electrode layer contains, for example, metals such as Cu, Ni, Ag, Pd, and Au, or an alloy of Ag and Pd.
[0049] The baked electrode layer is formed by applying a conductive paste containing glass and metal to the laminate and baking the applied paste. The baking may be performed simultaneously with or after the firing of the laminate.
[0050] The resin electrode layer can be formed, for example, as a layer containing conductive particles and a thermosetting resin. When forming a resin electrode layer, it may be formed directly on the ceramic body without forming a baked electrode layer. The resin electrode layer may be a single layer or multiple layers.
[0051] The thin-film electrode layer is, for example, a layer of 1 μm or less in thickness in which metal particles are deposited, and can be formed by a known thin-film formation method such as a sputtering method or a vapor deposition method.
[0052] The plating layer disposed on the base electrode layer includes at least one of metals such as Cu, Ni, Ag, Pd, and Au, or an alloy of Ag and Pd. The plating layer may be a single layer or multiple layers. However, the plating layer is preferably a two-layer structure of a Ni plating layer and a Sn plating layer. The Ni plating layer prevents the base electrode layer from being eroded by solder when mounting the multilayer ceramic capacitor 10. The Sn plating layer improves the wettability of the solder when mounting the multilayer ceramic capacitor 10.
[0053] The first external electrode 20a and the second external electrode 20b may not include the above-mentioned base electrode layer, and may be composed of a plating layer disposed directly on the laminate 11. In this case, the plating layer is directly connected to the first internal electrode 13a or the second internal electrode 13b.
[0054] (An example of a manufacturing method for a multilayer ceramic capacitor) An example of a method for manufacturing the multilayer ceramic capacitor 10 having the above-mentioned structure will be described below. Fig. 5 is a diagram for explaining an example of the method for manufacturing the multilayer ceramic capacitor 10, in which (a) is a schematic diagram showing a ceramic green sheet on which a conductive film is formed, and (b) is a schematic diagram showing a state in which the ceramic green sheets on which the conductive film is formed are laminated.
[0055] First, there are prepared ceramic green sheets for forming the outer dielectric layer 121 and ceramic green sheets for forming the inner dielectric layer 122. These ceramic green sheets may be any known ceramic green sheets.
[0056] Next, as shown in FIG. 5(a), the internal electrode paste is printed in stripes on the surfaces of the prepared ceramic green sheets 50a and 50b, and then dried. The ceramic green sheets 50b are laminated alternately with the ceramic green sheets 50a. Here, the direction in which the internal electrode paste extends in stripes is the X direction, and the direction perpendicular to the X direction on the ceramic green sheets is the Y direction. In this manner, the conductive film 52a (52b) that will become the first internal electrode 13a (second internal electrode 13b) is formed. Various printing methods can be used, such as screen printing, inkjet printing, and gravure printing.
[0057] Next, after laminating the ceramic green sheets for constituting the outer dielectric layer 121, a plurality of ceramic green sheets 50a, 50b on which the conductive films 52a, 52b are formed are laminated while being shifted from each other in the Y direction as shown in Fig. 5(b). Then, a ceramic green sheet for constituting the outer dielectric layer 121 is laminated thereon to obtain a mother laminate.
[0058] Next, the mother laminate is pressed by a method such as a rigid press, a hydrostatic press, etc. Then, the pressed mother laminate is cut into a chip shape to obtain a structure 60 shown in FIG.
[0059] 6, only the conductive film 52a of the ceramic green sheet 50a is exposed on one end face of the structure 60, and only the conductive film 52b of the ceramic green sheet 50b is exposed on the other end face. Also, on both side faces of the structure 60, the conductive film 52a of the ceramic green sheet 50a and the conductive film 52b of the ceramic green sheet 50b are exposed.
[0060] Next, the structure 60 is fired at a predetermined firing temperature. The firing temperature depends on the materials of the dielectric layers 12 and the internal electrodes 13a and 13b, but is, for example, 900° C. or higher and 1300° C. or lower.
[0061] Next, for example, sandblasting or barrel polishing is performed so that the corners and ridges of the fired structure have a rounded curved shape. Here, the first ridge 18 is processed so that the first curve 18a is formed in the completed multilayer ceramic capacitor 10. Note that the structure 60 before firing may be processed so that the corners and ridges have a rounded curved shape before firing.
[0062] Next, a ceramic green sheet for the side margin portion is prepared to form the side margin portion 14. The ceramic green sheet for the side margin portion can be produced using a ceramic slurry containing alumina, glass, an organic binder, an organic solvent, and the like. The prepared ceramic green sheet for the side margin portion is then placed against the side surface of the structure where the internal electrodes are exposed, and pressed and punched out to form a layer that will become the side margin portion 14. A layer that will become the side margin portion 14 is also formed on the opposite side surface in a similar manner. The side margin portion 14 may be formed by spraying the material or by coating.
[0063] Next, a process is performed so that the corners and ridges have a rounded curved shape. Here, the process is performed so that the second ridges 19 described above have a shape having a second curve 19a in the completed multilayer ceramic capacitor 10.
[0064] Next, a paste for external electrodes is applied to both end faces of the structure, and then the structure is fired at a predetermined firing temperature, for example, 800° C. or higher and 900° C. or lower.
[0065] Thereafter, a plating layer is formed as necessary. That is, when the external electrodes 20a, 20b include a plating layer, the plating layer is formed on the base electrode layer.
[0066] By the above-mentioned manufacturing method, the multilayer ceramic capacitor 10 having the side margin portion 14 made of ceramic containing alumina and glass is manufactured. However, the above-mentioned manufacturing method is only an example, and the manufacturing method of the multilayer ceramic capacitor 10 is not limited to the above-mentioned manufacturing method.
[0067] (Another Example of the Manufacturing Method of a Multilayer Ceramic Capacitor) When the side margin portion 14 of the multilayer ceramic capacitor 10 is made of resin and glass, it can be manufactured by the following method. However, since the process up to obtaining a fired structure with rounded corners and ridges is the same as the manufacturing method described above, a detailed explanation is omitted.
[0068] The first external electrode 20a and the second external electrode 20b are formed on both end faces of the fired structure, which has rounded corners and ridges. That is, an external electrode paste is applied to the entire end faces of the fired structure and to parts of both main faces and both side faces, and then baked to form a base electrode layer, and then a plating layer is formed on the base electrode layer.
[0069] 7, the first internal electrode 13a and the second internal electrode 13b are exposed on the side surfaces of the fired structure 70, so the first external electrode 20a and the second external electrode 20b are formed to prevent short circuits. Specifically, the first external electrode 20a is formed in an area where the second internal electrode 13b is not drawn out, and the second external electrode 20b is formed in an area where the first internal electrode 13a is not drawn out.
[0070] Finally, to form the side margin portion 14, a resin containing glass is applied to the side surface of the structure 70 where the first internal electrode 13a and the second internal electrode 13b are exposed. For example, the side margin portion 14 is formed by applying a thermoplastic resin containing glass and then heating it. The resin is applied so that the second ridge portion 19 described above has a shape having the second curved line 19a in the completed multilayer ceramic capacitor 10.
[0071] By the above method, the multilayer ceramic capacitor 10 having the side margin portion 14 made of resin and glass is manufactured.
[0072] <Reference embodiment> In the multilayer ceramic capacitor 10 according to the first preferred embodiment, the ends of all of the internal electrodes 13a, 13b are arranged so as not to overlap the first edge portion .
[0073] In contrast to this, in the multilayer ceramic capacitor of the reference embodiment, the end of the internal electrode located on the outermost side in the lamination direction is located in a position overlapping the first edge portion.
[0074] FIG. 8 is a cross-sectional view of a multilayer ceramic capacitor 10A in a reference embodiment, and similar to the cross-sectional view shown in FIG. 3, is a cross-sectional view defined by a width direction W and a stacking direction T, cutting the laminate 11 at the center position in the length direction L.
[0075] 8, the ends of the first internal electrode 13a and the second internal electrode 13b located on the outermost sides in the stacking direction are positioned to overlap the first ridge portion 18. That is, compared to the multilayer ceramic capacitor 10 in the first embodiment, the multilayer ceramic capacitor 10A in the reference embodiment can arrange the internal electrodes 13a, 13b further outward in the stacking direction T. Therefore, in a multilayer ceramic capacitor of the same size, the number of internal electrodes 13a, 13b can be increased, and the capacitance of the capacitor can be increased.
[0076] 8, in the multilayer ceramic capacitor 10A according to the reference embodiment, the dimension in the width direction W of the internal electrodes 13a, 13b positioned on the outermost side in the stacking direction T is smaller than the dimension in the width direction W of the other internal electrodes 13a, 13b. Therefore, even if the thickness of the side margin portion 14 is thin and the radius of curvature of the second ridge portion 19 is large, it is possible to prevent the interval between the end of the internal electrodes 13a, 13b positioned on the outermost side in the stacking direction T and the second ridge portion 19 from becoming shorter, and the moisture resistance of the multilayer ceramic capacitor 10A can be ensured.
[0077] The present invention is not limited to the above-described embodiment, and various applications and modifications are possible within the scope of the present invention. [Explanation of symbols]
[0078] 10, 10A Multilayer Ceramic Capacitor 11 Laminate 12 Dielectric layer 13a First internal electrode 13b Second internal electrode 14 Side margin 18 First Ridge 18a First Curve 19 Second Ridge 19a Second Curve 20a First external electrode 20b Second external electrode 50a, 50b Ceramic green sheet 60 Structure before firing 70 Structure after firing 121 Outer dielectric layer 122 Inner dielectric layer
Claims
1. a laminate including a plurality of laminated dielectric layers and a plurality of internal electrodes, the laminate having a first main surface and a second main surface facing each other in a lamination direction of the dielectric layers and the internal electrodes, a first side surface and a second side surface facing each other in a width direction perpendicular to the lamination direction, and a first end surface and a second end surface facing each other in a length direction perpendicular to the lamination direction and the width direction; external electrodes electrically connected to the internal electrodes and provided on the first end surface and the second end surface of the laminate; Equipped with a first ridge portion connecting a straight line connecting one ends of two of the internal electrodes positioned outermost in the stacking direction and one of the first main surface and the second main surface has a first curved line, and a second ridge portion connecting one of the first main surface and the second main surface and one of the first side surface and the second side surface has a second curved line, When viewed in the lamination direction, ends of all the internal electrodes are located at positions that do not overlap with the first ridge portion, the dielectric layers include outer-layer dielectric layers positioned between the internal electrode positioned at the outermost side in the stacking direction and the first main surface of the laminate, and between the internal electrode positioned at the outermost side in the stacking direction and the second main surface of the laminate, and inner-layer dielectric layers positioned between a plurality of the internal electrodes adjacent to each other in the stacking direction, 1. A multilayer ceramic capacitor, comprising: an outer dielectric layer having a thickness smaller than a radius of curvature of the first curve; and a radius of curvature of the first curve being 10% or more larger than a radius of curvature of the second curve.
2. 2. The multilayer ceramic capacitor according to claim 1, wherein, when the laminate is cut at a central position in the longitudinal direction and a cross section defined by the width direction and the stacking direction is viewed, a variation in distance in the width direction from a straight line connecting one ends of two of the internal electrodes positioned outermost in the stacking direction to an end of each of the plurality of internal electrodes is 0.2 or less.
3. 3. The multilayer ceramic capacitor according to claim 1, wherein an extension of the straight line intersects with the second curve.
4. The multilayer ceramic capacitor according to any one of claims 1 to 3, characterized in that a radius of curvature of the first curve is 16 μm or more and 28 μm or less when the dimension of the laminate in the stacking direction is 0.3 mm and the dimension in the width direction is 0.3 mm, 30 μm or more and 50 μm or less when the dimension of the laminate in the stacking direction is 0.5 mm and the dimension in the width direction is 0.5 mm, 40 μm or more and 200 μm or less when the dimension of the laminate in the stacking direction is 1.25 mm and the dimension in the width direction is 1.25 mm, and 50 μm or more and 200 μm or less when the dimension of the laminate in the stacking direction is 1.6 mm and the dimension in the width direction is 1.6 mm.
5. 5. The multilayer ceramic capacitor according to claim 1, wherein side margin portions located in the width direction between the first side surface and the internal electrode and between the second side surface and the internal electrode are made of resin and glass.
6. 5. The multilayer ceramic capacitor according to claim 1, wherein side margin portions located in the width direction between the first side surface and the internal electrode and between the second side surface and the internal electrode are made of a ceramic containing alumina and glass.
7. 7. The multilayer ceramic capacitor according to claim 5, wherein the side margin portion has a dimension in the width direction of 5 [mu]m or more and 50 [mu]m or less.
Citation Information
Patent Citations
Laminated electronic component
JP2003007566A
Multilayer electronic component
JP2011233696A
Multilayer ceramic capacitor and manufacturing method of multilayer ceramic capacitor
JP2019079977A