tire
By positioning electronic components at intersections of tire constituents and using protective rubber sheets, the tire design addresses movement and stress issues, ensuring reliable and durable electronic functionality.
Patent Information
- Application Number
- JP2023074993
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-04-28
- Publication Date
- 2024-11-20
- Estimated Expiration
- 2039-06-19
AI Technical Summary
Existing tire designs with embedded electronic components, such as RFID tags, face issues with movement during deformation, stress concentration, and inconsistent placement, leading to potential functional failure and reduced communication quality.
The tire design incorporates electronic components at intersections of at least three tire constituent members, including fiber and rubber elements, with a protective rubber sheet covering, ensuring stable positioning and protection against deformation.
This configuration effectively suppresses movement and stress on electronic components, maintains functional integrity, and ensures consistent placement, enhancing communication reliability and durability.
Smart Images

Figure 0007587631000001 
Figure 0007587631000002 
Figure 0007587631000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a tire having an embedded electronic component. [Background technology]
[0002] Conventionally, tires with electronic components such as RFID tags embedded in the rubber structure are known. Such tires can perform manufacturing management, usage history management, and the like, by communicating between an RFID tag embedded in the tire and an external reader. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2016-37236 A [Patent Document 2] JP 2016-49920 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the technology disclosed in Patent Document 1, the RF tag is disposed between the stiffener and the side rubber, and is not in contact with fiber members such as the carcass ply. Therefore, the RF tag moves significantly when the tire deforms, which may make it difficult to protect the RF tag. In addition, the technology shown in Patent Document 2 shows a configuration in which the RF tag is sandwiched between the carcass ply made of a fiber layer and the cord reinforcement layer. In this way, when the RF tag is completely sandwiched between two fiber layers, stress is generated between the fiber layer and the RF tag during the sandwiching process, and the fiber layer and the RF tag may be affected by the stress at that time. In addition, when the RF tag is simply placed so as to be sandwiched between two rubber members, it is difficult to set a standard for the placement position, and the placement positions of the electrical components may vary. As a result, there is a possibility that the electrical components may be placed in an undesirable position and may not be able to maintain their function.
[0005] The present invention has been made in consideration of the above-mentioned problems, and has an object to provide a tire that can effectively suppress movement of electronic components when the tire deforms and effectively protect the electronic components. [Means for solving the problem]
[0006] (1) A tire of the present invention (e.g., tire 1) includes a plurality of tire components constituting the tire and an electronic component (e.g., RFID tag 40), the plurality of tire components including a rubber component and a fiber component, and the electronic component is disposed at an intersection of at least three tire components including at least one of the fiber components.
[0007] (2) In the tire of (1), each of the three tire constituent members including the one fiber member may be annular members formed in an annular shape.
[0008] (3) In the tire according to (1) or (2), the electronic component may be disposed at a position where at least three tire constituent members including at least two of the fiber members intersect.
[0009] (4) In the tire of (3), the fiber member includes a carcass ply (e.g., carcass ply 23) and a steel belt (e.g., steel belt 26) arranged radially outward of the carcass ply, and the rubber member includes a shoulder pad (e.g., shoulder pad 38) arranged between the carcass ply and the steel belt at the tire widthwise outer portion, and the electronic component may be arranged at a position where the carcass ply, the steel belt, and the shoulder pad intersect.
[0010] (5) In the tires of (1) to (4), at least a portion of the electronic component may be covered by a covering rubber sheet (e.g., covering rubber sheets 431, 432), and the covering rubber sheet covering the electronic component may be disposed at a position where at least three tire components including at least one fiber member intersect.
[0011] (6) In the tire of (5), the three tire constituent members include a first tire constituent member made of a fibrous member, a second tire constituent member made of a rubber member having a tapered end in a cross-sectional view in the tire width direction and arranged so as to cover a portion of the first tire constituent member, and a third tire constituent member covering at least a boundary portion between the fibrous member and the rubber member, and the covering rubber sheet may be arranged to straddle the first tire constituent member and the second tire constituent member at the boundary portion between the first tire constituent member and the second tire constituent member, and be covered by the third tire constituent member.
[0012] (7) A manufacturing method for manufacturing a tire of (6) may include a step of attaching the covering rubber sheet at a boundary between a first tire component and a second tire component so as to straddle a first tire component and a second tire component, and a step of attaching the third tire component so as to cover the covering rubber sheet attached to the boundary between the first tire component and the second tire component. Effect of the Invention
[0013] According to the present invention, it is possible to provide a tire that can effectively suppress the movement of electronic components when the tire deforms, and can suitably protect the electronic components. [Brief description of the drawings]
[0014] [Figure 1] 1 is a view showing a half cross section in the tire width direction of a tire according to a first embodiment of the present invention. [Diagram 2] 1 is a partially enlarged cross-sectional view of a tire according to a first embodiment of the present invention. [Figure 3A] FIG. 2 is a diagram showing an RFID tag protected by a protective member in a tire according to a first embodiment of the present invention. [Figure 3B] FIG. 3B is a diagram showing a cross section bb of FIG. 3A. [Figure 3C] FIG. 3B is a diagram showing a cross section cc of FIG. 3A. [Figure 4] FIG. 4 is a partially enlarged cross-sectional view of a tire according to a second embodiment of the present invention. [Figure 5A] FIG. 11 is a diagram showing the peripheral portion of a protective member during a tire manufacturing process according to a second embodiment of the present invention, as viewed from the outer side in the tire width direction. [Figure 5B] FIG. 10 is a diagram showing a peripheral portion of a protective member in a modified example of a manufacturing process for a tire according to a second embodiment of the present invention, as viewed from the outer side in the tire width direction. [Figure 5C] FIG. 11 is a diagram showing an annular rubber sheet as a modified example of a protective member in a tire according to a second embodiment of the present invention. [Figure 6] FIG. 11 is a partially enlarged cross-sectional view of a tire according to a modified example of the second embodiment of the present invention. [Figure 7] FIG. 5 is a partially enlarged cross-sectional view of a tire according to a third embodiment of the present invention. [Figure 8] FIG. 11 is a partially enlarged cross-sectional view of a tire according to a fourth embodiment of the present invention. [Figure 9] FIG. 11 is a partially enlarged cross-sectional view of a tire according to a fifth embodiment of the present invention. [Figure 10] FIG. 11 is a partially enlarged cross-sectional view of a tire according to a sixth embodiment of the present invention. [Figure 11]FIG. 13 is a cross-sectional view of the spring antenna before the RFID tag is sandwiched between rubber sheets when no rubber is filled inside the spring antenna. [Figure 12] FIG. 13 is a cross-sectional view of the spring antenna after the RFID tag is sandwiched between rubber sheets when no rubber is filled inside the spring antenna. [Figure 13] FIG. 13 is a cross-sectional view of the spring antenna after the RFID tag is sandwiched between rubber sheets when no rubber is filled inside the spring antenna. [Figure 14] FIG. 13 is a diagram showing an RFID tag in a tire according to a seventh embodiment of the present invention before rubber is filled inside the spring antenna. [Figure 15] FIG. 13 is a diagram showing an RFID tag after rubber has been filled inside a spring antenna in a tire according to a seventh embodiment of the present invention. [Figure 16] FIG. 13 is a diagram showing an RFID tag before being sandwiched between rubber sheets in a tire according to a seventh embodiment of the present invention. [Figure 17] FIG. 13 is a diagram showing an RFID tag sandwiched between rubber sheets in a tire according to a seventh embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] First Embodiment Hereinafter, a first embodiment of the present invention will be described with reference to the drawings. Fig. 1 is a diagram showing a half cross section in the tire width direction of a tire 1 according to this embodiment. The basic structure of the tire is symmetrical in the cross section in the tire width direction, so a cross section of the right half is shown here. In the figure, the symbol S1 indicates the tire equatorial plane. The tire equatorial plane S1 is a plane that is perpendicular to the tire rotation axis and is located at the center in the tire width direction. Here, the tire width direction is a direction parallel to the tire rotation axis, and corresponds to the left-right direction on the paper surface in the cross-sectional view of Fig. 1. In Fig. 1, this direction is illustrated as tire width direction X. The inner side in the tire width direction is the direction approaching the tire equatorial plane S1, which is the left side on the paper in Fig. 1. The outer side in the tire width direction is the direction away from the tire equatorial plane S1, which is the right side on the paper in Fig. 1. The tire radial direction is a direction perpendicular to the tire rotation axis, and is the up-down direction on the paper surface in Fig. 1. In Fig. 1, this direction is illustrated as tire radial direction Y. The outer side in the tire radial direction is the direction away from the tire rotation axis, and is the upper side on the paper in Fig. 1. The inner side in the tire radial direction is the direction approaching the tire rotation axis, and is the lower side on the paper in Fig. 1. The same applies to Figures 2, 4, and 6 to 10.
[0016] The tire 1 is, for example, a tire for trucks or buses, and has a pair of beads 11 provided on both sides in the tire width direction, a tread 12 that forms a contact surface with the road surface, and a pair of sidewalls 13 extending between the pair of beads 11 and the tread 12.
[0017] The bead 11 includes an annular bead core 21 formed by winding a metal bead wire covered with rubber several times, and a tapered bead filler 22 extending outward in the tire radial direction of the bead core 21. The bead filler 22 is composed of a first bead filler 221 covering the outer periphery of the bead core 21, and a second bead filler 222 arranged on the outer side of the first bead filler 221 in the tire radial direction. The second bead filler 222 is composed of rubber having a higher modulus than the inner liner 29 and the sidewall rubber 30 described later. The first bead filler 221 is composed of rubber having an even higher modulus than the second bead filler 222. Note that the first bead filler 221 may not cover the outer periphery of the bead core 21 as long as at least a part of it is arranged on the outer side of the bead core 21 in the tire radial direction. The bead filler 22 may be formed of one type of rubber. In other words, the first bead filler 221 and the second bead filler 222 do not have to be separated. The bead core 21 is a member that serves to fix an air-filled tire to the rim of a wheel (not shown). The bead filler 22 is a member that is provided to increase the rigidity of the periphery of the bead and ensure high maneuverability and stability.
[0018] A carcass ply 23 constituting a ply that forms the framework of the tire is embedded inside the tire 1. The carcass ply 23 extends from one bead core to the other bead core. That is, the carcass ply 23 is embedded in the tire 1 in a manner that passes between a pair of bead cores 21, a pair of sidewalls 13, and the tread 12. 1, the carcass ply 23 includes a ply body 24 extending from one bead core to the other bead core and extending between the tread 12 and the bead 11, and a ply turn-up portion 25 turned up around the bead core 21. Here, a turn-up end 25A of the ply turn-up portion 25 is located radially inward of an outer end 22A of the bead filler 22 in the tire radial direction. The carcass ply 23 is composed of a plurality of ply cords extending in the tire width direction. The plurality of ply cords are arranged side by side in the tire circumferential direction. The ply cord is made of a metal steel cord or an insulating organic fiber cord made of polyester, polyamide, or the like, and is covered with rubber.
[0019] In the tread 12, multiple layers of steel belts 26 are provided on the tire radially outer side of the carcass ply 23. The steel belts 26 are composed of multiple steel cords covered with rubber. By providing the steel belts 26, the rigidity of the tire is ensured and the contact state between the tread 12 and the road surface is improved. In this embodiment, four layers of steel belts 26 are provided, but the number of stacked steel belts 26 is not limited to this.
[0020] A tread rubber 28 is provided on the radially outer side of the steel belt 26. A tread pattern (not shown) is provided on the outer surface of the tread rubber 28, and this outer surface becomes the contact surface that comes into contact with the road surface.
[0021] A shoulder pad 38 serving as a pad is provided in the vicinity of the outer side in the tire width direction of the tread 12, i.e., in the end region in the tire width direction of the steel belt 26 and the tread rubber 28, in the region between the carcass ply 23, and the steel belt 26 and the tread rubber 28. This shoulder pad 38 extends to the outer region in the tire radial direction of the sidewall 13, and a part of it forms an interface with a sidewall rubber 30 described below. That is, in the outer region in the tire radial direction of the sidewall 13, a part of the shoulder pad 38 is present on the inner side in the tire width direction of the sidewall rubber 30. In other words, in the extending portion of the shoulder pad 38, from the inner cavity side of the tire toward the outer surface side of the tire, the extending portion of the shoulder pad 38 and the sidewall rubber 30 are laminated in this order on the carcass ply 23. That is, in a part of the carcass ply 23, the shoulder pad 38 and the sidewall rubber 30 are laminated. The shoulder pad 38 is made of a rubber member having cushioning properties, and exhibits a cushioning function between the carcass ply 23 and the steel belt 26. In addition, since the shoulder pad 38 is made of rubber having low heat generation properties, by extending it to the sidewall 13, heat generation can be effectively suppressed. In this manner, the shoulder pad 38 is disposed on the tire outer surface side of the carcass ply 23 and on the tire inner cavity side of the tread rubber 28 and the sidewall rubber 30 .
[0022] An inner liner 29 serving as a rubber layer constituting the inner wall surface of the tire 1 is provided on the tire cavity side of the carcass ply 23 in the beads 11, sidewalls 13, and tread 12. The inner liner 29 is made of air-permeable resistant rubber and prevents air in the tire cavity from leaking to the outside.
[0023] In the sidewall 13, a sidewall rubber 30 that constitutes the outer wall surface of the tire 1 is provided on the outer side of the carcass ply 23 in the tire width direction. This sidewall rubber 30 is the part that bends the most when the tire performs its cushioning function, and flexible rubber having fatigue resistance is usually used for this sidewall rubber.
[0024] A steel chafer 31 is provided as a reinforcing ply on the tire radially inner side of the carcass ply 23 provided around the bead core 21 of the bead 11 so as to cover at least a part of the carcass ply 23. The steel chafer 31 also extends on the tire width direction outer side of the ply turn-up portion 25 of the carcass ply 23, and an end 31A of the steel chafer 31 is located on the tire radially inner side of the turn-up end 25A of the carcass ply 23. The steel chafer 31 is a metal reinforcing layer made of metal steel cords and is covered with rubber.
[0025] A rim strip rubber 32 is provided on the inner side in the tire radial direction of the steel chafer 31. This rim strip rubber 32 is arranged along the outer surface of the tire and is connected to the sidewall rubber 30. This rim strip rubber 32 and the sidewall rubber 30 are rubber members that make up the outer surface of the tire.
[0026] A first pad 35 is provided on the tire radial outer side of the end portion 31A of the steel chafer 31 and on the tire width direction outer side of the turned-up portion 25 of the carcass ply 23 and the bead filler 22. This first pad 35 is provided on at least the tire width direction outer side of the turned-up end 25A of the carcass ply 23. The tire radial outer side of the first pad 35 is formed to taper toward the tire radial outer side.
[0027] Furthermore, a second pad 36 is provided so as to cover the outer side in the tire width direction of the first pad 35. More specifically, the second pad 36 is provided so as to cover the outer side in the tire width direction of a part of the steel chafer 31, the first pad 35, a part of the second bead filler 222, and a part of the ply body 24 of the carcass ply 23. A sidewall rubber 30 is arranged on the outer side in the tire width direction of the tire radial outer region of the second pad 36, and a rim strip rubber 32 is arranged on the outer side in the tire width direction of the tire radial inner region of the second pad 36. In other words, the second pad 36 is provided between the first pad 35 etc. and the rim strip rubber 32 and the sidewall rubber 30 which are members constituting the outer surface of the tire.
[0028] The first pad 35 and the second pad 36 constitute a pad member 34, and this pad member 34 is made of rubber having a higher modulus than the modulus of the outer portion (second bead filler 222) of the bead filler 22 in the tire radial direction. More specifically, the second pad 36 is made of rubber having a higher modulus than the second bead filler 222, and the first pad 35 is made of rubber having an even higher modulus than the second pad 36. The first pad 35 and the second pad 36 have the function of mitigating sudden distortion caused by localized changes in rigidity at the turned-up end 25A of the carcass ply 23 and the end 31A of the steel chafer 31.
[0029] A rubber sheet 37 serving as a reinforcing rubber sheet is disposed between the bead filler 22 and the pad member 34 near the turned-up end 25A of the carcass ply 23. The rubber sheet 37 is disposed so as to cover the turned-up end 25A of the carcass ply 23 from the inner side in the tire width direction. The rubber sheet 37 is made of rubber having a higher modulus than the second bead filler 222. More preferably, the rubber sheet 37 is made of rubber having a modulus approximately equal to that of the first pad .
[0030] Generally, stress is likely to concentrate at the folded end 25A of the carcass ply 23. However, by providing the rubber sheet 37 as the reinforcing rubber sheet described above, it becomes possible to effectively suppress the concentration of stress. In this embodiment, the pad member 34 is composed of the first pad 35 and the second pad 36, but the pad member 34 may be composed of a single member. However, as described above, by adopting a configuration in which the pad member 34 is composed of the first pad 35 and the second pad 36 and further includes the rubber sheet 37, it is possible to more effectively suppress the concentration of stress.
[0031] In this embodiment, the position of the tire radial direction outer end 37A of the rubber sheet 37 is located radially inward of the tire radial direction outer end 22A of the bead filler 22. However, the position of the tire radial direction outer end 37A of the rubber sheet 37 may be substantially aligned with the position of the tire radial direction outer end 22A of the bead filler 22. 1, it is preferable to adopt a mode in which the rubber sheet 37 is disposed so as to cover the folded end 25A of the carcass ply 23 from the inner side in the tire width direction, but a configuration in which the folded end 25A of the carcass ply 23 is covered from the outer side in the tire width direction may be adopted. Even in this case, it is possible to reduce the concentration of stress.
[0032] In the tire 1 of this embodiment, an RFID tag 40 is embedded as an electronic component. The RFID tag 40 is a passive transponder equipped with an RFID chip and an antenna for communicating with an external device, and performs wireless communication with a reader (not shown) as the external device. As the antenna, various types of antennas such as a coil-shaped spring antenna, a plate-shaped antenna, and a rod-shaped antenna may be used. For example, the antenna may be formed by printing a predetermined pattern on a flexible substrate. The antenna is set to an optimized antenna length according to the frequency band to be used, etc. Identification information such as a serial number and a part number is stored in a memory unit in the RFID chip.
[0033] FIG. 2 is an enlarged cross-sectional view showing the periphery of the embedded portion of the RFID tag 40 in the tire 1 of FIG. The RFID tag 40 (including a state where at least a part of it is covered by a protective member 43 described later) is disposed at a position where at least three tire constituent members constituting the tire 1 intersect. Specifically, the multiple tire constituent members include a rubber member and a fiber member, and the RFID tag 40 is disposed at a position where at least three tire constituent members including at least one fiber member intersect. More specifically, the RFID tag 40 is disposed at a position where at least three rubber members including at least one fiber member and at least one rubber member intersect. Here, the fiber members constituting the tire 1 include fiber members covered with rubber, and include, for example, the carcass ply 23, the steel belt 26, the steel chafer 31, etc. The tire 1 of this embodiment includes a carcass ply 23 as a fibrous member, a steel belt 26 as a fibrous member arranged on the tire radial direction outer side of the carcass ply 23, and a shoulder pad 38 as a rubber member arranged between the carcass ply 23 and the steel belt 26 in the tire width direction outer region, and the RFID tag 40 is arranged at a position where the carcass ply 23, the steel belt 26, and the shoulder pad 38 intersect. That is, in this embodiment, the RFID tag 40 is arranged at a position where three tire constituent members including two fibrous members intersect.
[0034] More preferably, the RFID tag 40 is integrally covered with a protective member 43 made of a covering rubber sheet described later, and this protective member 43 is disposed at a position where three tire constituent members including two fiber members intersect. Specifically, this protective member 43 is sandwiched between the carcass ply 23 and the steel belt 26, and contacts the shoulder pad 38 on the outer side in the tire width direction.
[0035] Here, the carcass ply 23, the steel belt 26, and the shoulder pad 38 are each annular tire constituent members that constitute the annular tire 1. The protective member 43 that holds the RFID tag 40 is disposed so as to be in contact with the carcass ply 23, the steel belt 26, and the shoulder pad 38.
[0036] By arranging the RFID tag 40 in such a position, the RFID tag 40 is surrounded by the carcass ply 23, the steel belt 26, and the shoulder pad 38, which effectively suppresses movement of the RFID tag 40 when the tire deforms and provides suitable protection for the RFID tag 40. In this embodiment, the RFID tag 40 is sandwiched between the carcass ply 23 and the steel belt 26 and in contact with the shoulder pad 38 on the outer side in the tire width direction, so that the RFID tag is firmly protected by the two fiber members, while the shoulder pad 38, which is a rubber member in contact with it, can alleviate any generated stress.
[0037] Furthermore, by using the intersection point of the three members as the reference for the placement position of the RFID tag 40, it is possible to reduce variation in the placement position of the RFID tag 40. This also reduces the possibility that the RFID tag 40 will be mistakenly placed in an undesirable position, and the function of the RFID tag 40 can be maintained appropriately.
[0038] Furthermore, in such a position, the RFID tag 40 can be placed as far as possible on the inside in the tire width direction from the end 26A of the steel belt 26, so that it is less susceptible to the stress generated around the end 26A of the steel belt 26.
[0039] The shoulder pad 38 has cushioning properties, so that if the RFID tag 40 is placed on this portion, distortion occurring around the RFID tag 40 can be absorbed. In addition, the shoulder pad has low heat generation properties, so the RFID tag 40 provided in such a position is less susceptible to heat generated by the rubber during use. Considering these points, the position where the carcass ply 23, the steel belt 26, and the shoulder pad 38 intersect is a suitable position for embedding the RFID tag 40.
[0040] Furthermore, if the RFID tag 40 is disposed at the intersection of the carcass ply 23, the steel belt 26, and the shoulder pad 38, the RFID tag 40 will not be removed even in the case of retreading. In other words, since the portion of the tread rubber 28 that is removed during retreading is at least on the outer side of the steel belt 26 in the tire radial direction, if the RFID tag 40 is disposed at the intersection of the carcass ply 23, the steel belt 26, and the shoulder pad 38, the RFID tag 40 will not be removed and can continue to be used. In this respect, too, the intersection of the carcass ply 23, the steel belt 26, and the shoulder pad 38 is a suitable position for embedding the RFID tag 40.
[0041] In addition, taking the modulus of the shoulder pad 38 as a reference, the sidewall rubber 30 preferably has a modulus that is 0.4 to 0.7 times that of the shoulder pad 38. In addition, the tread rubber 28 preferably has a modulus that is 0.4 to 0.9 times that of the shoulder pad 38. By setting the modulus in this range, it is possible to maintain a balance between flexibility and rigidity as a tire. The modulus refers to the 100% elongation modulus (M100) measured in an atmosphere of 23° C. in accordance with “3.7 Stress at a given elongation, S” of JIS K6251:2010.
[0042] Here, the RFID tag 40 is covered with covering rubber sheets 431 and 432 that constitute a protective member 43 . This will be described with reference to FIGS. 3A to 3C.
[0043] Fig. 3A is a diagram showing an RFID tag 40 covered with a protective member 43 formed of a rubber sheet. In Fig. 3A, the RFID tag 40 is covered and hidden by a covering rubber sheet 431 described later. Fig. 3B is a cross-sectional view taken along line bb in Fig. 3A, and Fig. 3C is a cross-sectional view taken along line cc in Fig. 3A.
[0044] The RFID tag 40 includes an RFID chip 41 and an antenna 42 for communicating with an external device. As the antenna 42, various types of antennas such as a coil spring antenna, a plate antenna, and a rod antenna may be used. For example, the antenna may be an antenna formed by printing a predetermined pattern on a flexible substrate. In consideration of communication properties and flexibility, a coil spring antenna is most preferable. The antenna is set to an optimized antenna length according to the frequency band to be used, etc.
[0045] The protective member 43 is composed of two covering rubber sheets 431 and 432 that sandwich the RFID tag 40 to protect it.
[0046] The protective member 43 is made of, for example, rubber having a predetermined modulus. Here, the modulus refers to the 100% elongation modulus (M100) measured in an atmosphere of 23° C. in accordance with “3.7 Stress at a given elongation, S” of JIS K6251:2010.
[0047] The rubber used for the protective member 43 has a modulus at least higher than that of the sidewall rubber 30. For example, rubber having a modulus higher than that of the sidewall rubber 30 and lower than that of the shoulder pad 38 is used.
[0048] For example, it is more preferable to use rubber having a modulus 1.1 to 1.8 times that of the sidewall rubber 30 as the standard for the rubber used in the protective member 43. In this case, the rubber used in the shoulder pad 38 may have a modulus 1.6 to 3 times that of the sidewall rubber, for example, about twice as much. If emphasis is placed on strengthening the protection of the RFID tag 40, the rubber used for the protection member 43 may have a higher modulus than the shoulder pad .
[0049] The protective member 43 may be made of rubber mixed with short fiber filler. As the short fiber filler, for example, insulating short fibers such as organic short fibers such as aramid short fibers and cellulose short fibers, ceramic short fibers such as alumina short fibers, and inorganic short fibers such as glass short fibers can be used. By mixing such short fiber filler into rubber, the strength of the rubber can be increased. Also, a rubber sheet in a vulcanized state may be used as the protective member 43. A rubber sheet in a vulcanized state does not undergo plastic deformation like raw rubber, and therefore can adequately protect the RFID tag 40. However, in consideration of the ease of attachment during the manufacturing process and the stabilization of the rubber structure by integration with other rubber members during vulcanization, it is more preferable to use a rubber sheet of a predetermined thickness in a pre-vulcanized state as the protective member 43.
[0050] Moreover, an organic fiber layer made of polyester fiber, polyamide fiber, or the like may be provided as the protective member 43. It is also possible to embed an organic fiber layer between the two covering rubber sheets 431 and 432.
[0051] Next, a manufacturing process of the tire 1 will be described. The RFID tag 40 covered with the protective member 43 is attached before the vulcanization step in the tire manufacturing process. In the manufacturing process of the tire 1 in this embodiment, the protection member 43 covering the RFID tag 40 is attached to the carcass ply 23.
[0052] Thereafter, the shoulder pad 38 is attached to the carcass ply 23. At this time, the attachment positions of the protective member 43 and the shoulder pad 38 are determined so that the position of the protective member 43 covering the RFID tag 40 and the position of the inner end 38A in the tire width direction of the shoulder pad 38 almost coincide with each other. Here, the position overlapping with the protective member 43 near the inner end 38A in the tire width direction of the shoulder pad 38 may be partially removed. After the shoulder pad 38 is attached to the carcass ply 23, the RFID tag 40 may be attached so as to press against the tire width direction inner end 38A of the shoulder pad 38, the end of which has a tapered shape in a cross section in the tire width direction (see Figs. 1 and 2). At this time, a protective member covering the RFID tag 40 may be attached to the boundary between the carcass ply 23 and the shoulder pad 38 so as to straddle the carcass ply 23 and the shoulder pad 38.
[0053] Further, after that, the steel belt 26 is attached so as to cover the radially outer side of the carcass ply 23 and the shoulder pad 38. As a result, the RFID tag 40 covered with the protective member 43 is disposed at the intersection of three tire components including two fiber members, specifically, the carcass ply 23, the steel belt 26, and the shoulder pad 38.
[0054] At this time, since the covering rubber of the carcass ply 23, the covering rubber of the steel belt 26, and the shoulder pad 38 are in a state of raw rubber before vulcanization, their adhesiveness may be utilized to attach these components to the protective member 43 covered by the protective member 43. Alternatively, in cases where the adhesiveness is low, an adhesive or the like may be used for attachment.
[0055] In this manner, the rubber components constituting the tire are assembled to form a green tire. Thereafter, the raw tire to which each component part including the RFID tag 40 is assembled is vulcanized in a vulcanization process to manufacture a tire.
[0056] In this manner, in this embodiment, the RFID tag 40 covered with the protective member 43 can be attached to the covering rubber of the carcass ply 23 in a raw rubber state during tire manufacturing, which facilitates the installation of the RFID tag 40 during the tire manufacturing process. In particular, the carcass ply 23 has a certain degree of rigidity, which facilitates the installation of the RFID tag 40 covered with the protective member 43.
[0057] Furthermore, if the protective member 43 is formed of two covering rubber sheets 431, 432, the RFID tag 40 including the protective member 43 can be formed thin, which is suitable for embedding in the tire 1. Furthermore, when assembling the RFID tag 40 to a component of the tire 1 before vulcanization, the RFID tag 40 covered by the covering rubber sheets can be attached very easily. For example, the RFID tag 40 covered by the covering rubber sheets 431, 432 can be appropriately attached to a desired position of a member, such as a boundary between multiple rubber members before vulcanization, by utilizing the adhesiveness of raw rubber. Also, by using the covering rubber sheets 431, 432 as raw rubber before vulcanization, the adhesiveness of the covering rubber sheets themselves can be utilized to more easily attach the RFID tag 40.
[0058] However, the protective member 43 is not limited to being constituted by two covering rubber sheets, and various other configurations can be adopted. For example, as long as the covering rubber sheet constituting the protective member covers at least a part of the RFID tag 40, it is possible to obtain effects such as improved workability and stress relief in the manufacturing process. Therefore, a configuration in which only one side of the RFID tag 40 is covered by one covering rubber sheet 431 as the protective member may be adopted. Also, for example, a configuration in which one rubber sheet is wrapped around the entire circumference of the RFID tag 40, or a configuration in which a protective member in the form of a highly viscous potting agent is attached to the entire circumference of the RFID tag 40 may be used. Even with such a configuration using a covering rubber, the RFID tag 40 can be adequately protected.
[0059] The RFID tag 40 covered by the protective member 43 is embedded in the tire 1 so that the direction in which the antenna extends, i.e., the longitudinal direction, is, for example, a tangential direction to the circumferential direction of the tire 1, i.e., a direction perpendicular to the paper surface in the cross-sectional views of FIGS. 1 and 2. The covering rubber sheets 431, 432 are embedded in the tire 1 so as to be aligned in the tire radial direction. That is, in the manufacturing process, one surface of either one of the covering rubber sheets 431, 432 is attached to a component of the tire 1 before vulcanization, such as the carcass ply 23. The RFID tag 40 covered by the protective member 43 is disposed between the carcass ply 23 and the steel belt 26. By adopting such an embodiment, even when the tire 1 is deformed, stress is unlikely to be applied to the RFID tag 40. Furthermore, the task of attaching the RFID tag 40 covered with the protective member 43 in the manufacturing process is simplified.
[0060] It is preferable to place the RFID tag 40 at the intersection of the carcass ply 23, the steel belt 26, and the shoulder pad 38 while covered with the protective member 43 as described above, but it may also be placed directly at the intersection of the carcass ply 23, the steel belt 26, and the shoulder pad 38 without being covered with the protective member 43. If the uncoated RFID tag 40 is placed directly at the intersection of the carcass ply 23, the steel belt 26, and the shoulder pad 38, the variation in thickness of the rubber material where the RFID tag 40 is placed is reduced, improving tire uniformity. Also, in the work of embedding the RFID tag 40 in such a position, the volume of the embedded object is small, making it easier to remove air. Also, by eliminating the process of covering the RFID tag 40 with a protective material, the work time is reduced.
[0061] In this embodiment, an RFID tag 40 is embedded in the tire as an electronic component, but the electronic component embedded in the tire is not limited to an RFID tag. For example, it may be various electronic components such as a sensor that performs wireless communication. In addition, since electronic components handle electrical information such as transmitting and receiving electrical signals, the presence of metal components in the vicinity may cause a decrease in performance. In addition, electronic components may be damaged by excessive stress. Therefore, the effect of the present invention can be obtained even when various electronic components are embedded in a tire. For example, the electronic components may be piezoelectric elements or strain sensors.
[0062] The tire 1 of the present embodiment provides the following advantages.
[0063] (1) The tire 1 according to this embodiment includes a plurality of tire components that constitute the tire, and an RFID tag 40 as an electronic component. The plurality of tire components include a rubber component and a fiber component, and the RFID tag 40 is disposed at a position where at least three tire components, each including at least one fiber component, intersect. This effectively prevents the movement of the RFID tag 40 when the tire deforms, and appropriately protects the RFID tag 40. Also, by using the intersection point of the three members as the reference for the placement position of the RFID tag 40, variation in the placement position of the RFID tag 40 is reduced. This also reduces the possibility that the RFID tag 40 will be mistakenly placed in an undesirable position, and the function of the RFID tag 40 can be properly maintained.
[0064] (2) Each of the three tire constituent members including one fiber member of the tire 1 according to the present embodiment is an annular member formed in an annular shape. In this way, even if the three tire constituent members are annular members that constitute the tire 1 having an annular shape, the above-mentioned effects can be obtained.
[0065] (3) The RFID tag 40 of the tire 1 according to this embodiment is disposed at a position where at least three tire constituent members, including at least two fiber members, intersect. This makes it possible for the RFID tag to be securely protected by the two fiber members.
[0066] (4) The fiber member of the tire 1 in this embodiment includes a carcass ply 23 and a steel belt 26 arranged radially outward of the carcass ply 23, and the rubber member includes a shoulder pad 38 arranged between the carcass ply 23 and the steel belt 26 on the outer portion in the tire width direction, and an RFID tag 40 is arranged at the position where the carcass ply 23, the steel belt 26, and the shoulder pad 38 intersect. With this configuration, the RFID tag 40 is strongly protected by two fiber components, the carcass ply 23 and the steel belt 26, while the shoulder pad 38, which is a rubber component, can mitigate any stress that may occur.
[0067] (5) The RFID tag 40 of the tire 1 according to this embodiment is at least partially covered by the covering rubber sheets 431, 432, and the covering rubber sheets 431, 432 covering the RFID tag 40 are arranged at positions where at least three tire components, including at least one fibrous member, intersect. This allows the RFID tag 40 to be easily attached to a constituent member of the tire 1 before vulcanization.
[0068] (6) The RFID tag 40 of the tire 1 according to this embodiment is disposed at a position where at least three tire constituent members, including at least one fiber member and at least one rubber member, intersect. This makes it possible to firmly protect the RFID tag 40 with the fiber member, while the rubber member can mitigate any stress that may occur.
[0069] <Second embodiment> Next, a tire according to a second embodiment will be described with reference to the drawings. In the following description, the same components as those in the first embodiment are given the same reference numerals, and detailed description thereof will be omitted.
[0070] FIG. 4 is an enlarged cross-sectional view showing the periphery of the embedded portion of the RFID tag 40 in the tire 1 of the present embodiment. 4, the RFID tag 40 (including a state where it is at least partially covered by a protective member 43) is disposed at a position where three tire constituent members, including one fiber member, intersect. More specifically, the tire 1 of this embodiment includes the carcass ply 23 as a fiber member, the shoulder pad 38 as a rubber member disposed on the tire outer surface side of the carcass ply 23, and the sidewall rubber 30 as a rubber member disposed on the tire outer surface side of the carcass ply 23 and the shoulder pad 38, and the RFID tag 40 is disposed at a position where the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30 intersect.
[0071] Also in this embodiment, more preferably, the RFID tag 40 is covered with a protective member 43 made of a covering rubber sheet, and the protective member 43 is disposed at a position where three tire constituent members including one fiber member intersect. Specifically, the protective member 43 is disposed at the boundary between the carcass ply 23 and the shoulder pad 38 so as to straddle the boundary between the carcass ply 23 and the shoulder pad 38. That is, the protective member 43 is attached so as to press the tire radial direction inner end 38B of the shoulder pad 38, the end of which is tapered in a tire width direction cross section (see FIG. 4). The tire outer surface side of the protective member 43 is covered by the sidewall rubber 30.
[0072] Here, the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30 are each annular tire constituent members that constitute the annular tire 1. A protection member 43 that holds an RFID tag 40 is disposed so as to be in surface contact with the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30.
[0073] Even if the RFID tag 40 is placed in such a position, the RFID tag 40 is surrounded by the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30, so that the movement of the RFID tag 40 during tire deformation is effectively suppressed and the RFID tag 40 can be suitably protected. In addition, in this embodiment, the RFID tag 40 is held by the carcass ply 23 and in contact with the shoulder pad 38 and the sidewall rubber 30, so that the movement of the RFID tag 40 is effectively suppressed by the fiber member, and the generated stress can be alleviated by the presence of the shoulder pad 38 and the sidewall rubber 30, which are rubber members in contact with the RFID tag 40. Then, the boundary between a plurality of tire constituent members, in this embodiment, the boundary B between the carcass ply 23 and the shoulder pad 38, is used as the reference for the placement position of the RFID tag 40, so that the variation in the placement position of the RFID tag 40 is reduced. This reduces the possibility that the RFID tag 40 is erroneously placed in an unfavorable position in terms of stress, distortion, etc., and the function of the RFID tag 40 can be properly maintained.
[0074] Furthermore, by arranging the RFID tag 40 in the shoulder portion, i.e., near the outer side in the tire radial direction of the sidewall, the RFID tag 40 can be arranged at a position sufficiently away from the metallic bead core 21, which may adversely affect communication. Here, the bead core 21 is formed into an annular shape by laminating and winding metallic bead wires, and is therefore a metallic member that is particularly likely to adversely affect communication. Also, in consideration of communication quality, it is preferable to place the RFID tag 40 as close as possible to the outer surface of the tire 1. If the RFID tag 40 is placed on the inner cavity side of the carcass ply 23, the communication quality will decrease because it will be far from the outer surface of the tire 1. Furthermore, if the carcass ply 23 is made of metal, placing the RFID tag 40 on the inner cavity side of the carcass ply 23 will significantly decrease the communication quality. Considering these points, the position where the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30 intersect is a suitable position for embedding the RFID tag 40.
[0075] In addition, in consideration of embedding the RFID tag 40 during the tire manufacturing process, it is preferable to place the RFID tag 40 at a position where three tire constituent members constituting the tire intersect. For example, when the RFID tag 40 is sandwiched between layers of wound ribbon-shaped rubber members, the timing of attaching the RFID tag 40 to the ribbon-shaped rubber member becomes complicated. In addition, when the RFID tag 40 is simply placed between two rubber members, it is difficult to set a reference for the placement position, and the placement position of the electric component may vary. On the other hand, if the RFID tag 40 is placed at a position where three tire constituent members intersect as in the present embodiment, the RFID tag 40 can be attached with high accuracy to the boundary between the first tire constituent member (in this embodiment, the carcass ply 23) made of a fiber member and the second tire constituent member (in this embodiment, the shoulder pad 38) made of a rubber member in the tire molding process, and then the third tire constituent member (in this embodiment, the sidewall rubber 30) can be overlapped thereon to sandwich the RFID tag 40. Considering these points, the position where the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30 intersect is a suitable position for embedding the RFID tag 40.
[0076] The shoulder pad 38 has cushioning properties, so that if the RFID tag 40 is placed on this portion, distortion occurring around the RFID tag 40 can be absorbed. In addition, the shoulder pad has low heat generation properties, so the RFID tag 40 provided in such a position is less susceptible to heat generated by the rubber during use. Considering these points, the position where the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30 intersect is a suitable position for embedding the RFID tag 40.
[0077] Furthermore, if the RFID tag 40 is disposed at the intersection of the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30, the RFID tag 40 will not be removed even in the case of retreading. In other words, since the portion of the tread rubber 28 that is removed during retreading is at least on the outer side of the steel belt 26 in the tire radial direction, if the RFID tag 40 is disposed at the intersection of the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30, the RFID tag 40 will not be removed and can continue to be used. In this respect, too, the intersection of the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30 is a suitable position for embedding the RFID tag 40.
[0078] Next, a manufacturing process of the tire 1 will be described. Figure 5A is a diagram of the peripheral portion of the protective member 43 during the manufacturing process as viewed from the outside in the tire width direction, and shows the protective member 43 covering the RFID tag 40 attached to the boundary B between the carcass ply 23 and the shoulder pad 38.
[0079] The RFID tag 40 covered with the protective member 43 is attached before the vulcanization step in the tire manufacturing process. 5A, in the manufacturing process of the tire 1 in this embodiment, the protective member 43 covering the RFID tag 40 is attached to the boundary portion B between the carcass ply 23 and the shoulder pad 38 so as to straddle the carcass ply 23 and the shoulder pad 38. That is, the protective member 43 is attached so as to press the tire radially inner end 38B of the shoulder pad 38, the end of which has a tapered shape in a cross section in the tire width direction (see FIG. 4). By attaching the protective member 43 to such a position, it is possible to partially assist the joining between tire constituent members, specifically, the joining between the carcass ply 23 and the shoulder pad 38.
[0080] Furthermore, by using the boundary between multiple rubber members, in this embodiment, the boundary B between the carcass ply 23 and the shoulder pad 38 as the reference for the placement position of the RFID tag 40, variation in the placement position of the RFID tag 40 is reduced. This reduces the possibility that the RFID tag 40 will be mistakenly placed in an undesirable position in terms of stress, distortion, etc., and allows the RFID tag 40 to maintain its proper function.
[0081] 5A (see FIG. 4), is attached so as to cover the protective member 43 attached to the boundary portion B between the carcass ply 23 and the shoulder pad 38. As a result, the RFID tag 40 covered with the protective member 43 is disposed at the intersection of at least three tire constituent members that constitute the tire 1, in this embodiment, at the intersection of the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30.
[0082] At this time, since the covering rubber of the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30 are in the state of raw rubber before vulcanization, the protective member 43 covered by the protective member 43 may be attached to these members by utilizing their adhesiveness. Alternatively, when the adhesiveness is low, the protective member 43 may be attached using an adhesive or the like.
[0083] In this manner, the rubber components constituting the tire are assembled to form a green tire. Thereafter, the raw tire to which each component part including the RFID tag 40 is assembled is vulcanized in a vulcanization process to manufacture a tire.
[0084] In this manner, in this embodiment, the RFID tag 40 covered with the protective member 43 can be affixed to the covering rubber of the carcass ply 23 in a raw rubber state and to the shoulder pad 38 during tire manufacturing, which facilitates the installation of the RFID tag 40 during the tire manufacturing process. In particular, the carcass ply 23 has a certain degree of rigidity, which facilitates the installation of the RFID tag 40 covered with the protective member 43.
[0085] As a modified example of the manufacturing process of the tire 1, the following manufacturing process may be adopted. That is, the protective member 43 covered by the RFID tag 40 is attached to the sidewall rubber 30, and then the sidewall rubber 30 to which the protective member 43 is attached is attached to the carcass ply 23 and the shoulder pad 38. Here, the protective member 43 is attached to the sidewall rubber 30 so that the protective member 43 is positioned at the boundary portion B between the carcass ply 23 and the shoulder pad 38 when the sidewall rubber 30 is attached to the carcass ply 23 and the shoulder pad 38. Even when such a process is adopted, the RFID tag 40 covered with the protective member 43 is disposed at a position where at least three tire constituent members constituting the tire 1 intersect, that is, at a position where the carcass ply 23, the shoulder pad 38, and the sidewall rubber 30 intersect. Therefore, the movement of the RFID tag 40 during tire deformation can be effectively suppressed, and the RFID tag 40 can be suitably protected.
[0086] The RFID tag 40 covered with the protective member 43 is embedded in the tire 1 so that the direction in which the antenna extends, i.e., the longitudinal direction, is, for example, tangent to the circumferential direction of the tire 1, i.e., perpendicular to the paper surface in the cross-sectional view of Figure 4. Here, in the process of attaching the RFID tag 40, the boundary between multiple rubber members, in this embodiment, the circumferential shape of boundary B between the carcass ply 23 and the shoulder pad 38 (the inner circumferential shape of the tire radially inner end 38B of the shoulder pad 38) shown in Fig. 5A is used as a reference, so that the RFID tag 40 covered by the protective member 43 can be easily arranged in the above-mentioned direction. That is, as shown in Fig. 5A, the circumferential shape of boundary B is used as a reference, and the covering rubber sheets 431, 432 covering the RFID tag 40 may be attached so that the longitudinal direction thereof approximately coincides with the tangent direction of the circumferential shape of boundary B.
[0087] 5B is a diagram showing a modified example of the manufacturing process, and shows a case where the covering rubber sheets 431, 432 covering the RFID tag 40 are attached while being bent so as to follow the circumferential shape of the boundary part B between the carcass ply 23 and the shoulder pad 38. At this time, the covering rubber sheets 431, 432 made of raw rubber can also be attached while being deformed so as to follow the circumferential direction of the boundary part B. A flexible coil-shaped spring antenna or the like may be used as the antenna of the RFID tag 40, so that the antenna also deforms following the deformation of the covering rubber sheets 431, 432. By using these methods, the RFID tag 40 covered with the protective member 43 can be easily and accurately arranged in the above-mentioned direction without the need for any special marking.
[0088] 5C is a diagram showing an annular rubber sheet 50 as a modified example of the protective member. For example, the protective member is configured by sandwiching the RFID tag 40 between two annular covering rubber sheets. In this case, it is preferable that the entire circumference of the boundary portion B between the carcass ply 23 and the shoulder pad 38 is covered by the annular rubber sheet 50. This can generally assist in the joining between the rubber members, specifically, the joining between the carcass ply 23 and the shoulder pad 38.
[0089] FIG. 6 shows a modified example of the tire 1 of the present embodiment. In the first modified example shown in FIG. 6, the protective member 43 covering the RFID tag 40 is disposed at a position where the carcass ply 23, the second pad 36, and the sidewall rubber 30 intersect. In this modified example, the protective member 43 covering the RFID tag 40 is disposed so as to straddle the carcass ply 23 and the second pad 36 at the boundary between the carcass ply 23 and the second pad 36. That is, the protective member 43 is attached so as to press the tire radial direction outer end 36A of the second pad 36, the end of which is tapered in a tire width direction cross section (FIG. 6), from the tire outer surface side. The tire outer surface side of the protective member 43 is covered by the sidewall rubber 30. Even if the RFID tag 40 is placed in such a position, the RFID tag 40 is surrounded by a plurality of tire components, specifically, the carcass ply 23, the second pad 36, and the sidewall rubber 30, so that the movement of the RFID tag 40 during tire deformation is effectively suppressed and the RFID tag 40 can be suitably protected. Furthermore, by using the boundary between a plurality of tire components, in this modified example, the boundary between the carcass ply 23 and the second pad 36 as the reference for the placement position of the RFID tag 40, the variation in the placement position of the RFID tag 40 is reduced. This reduces the possibility that the RFID tag 40 will be erroneously placed in an undesirable position in terms of stress, strain, and the like, and the function of the RFID tag 40 can be properly maintained.
[0090] In addition to the above advantages (1) to (5), the tire 1 of the present embodiment has the following advantages.
[0091] (7) The three tire components of tire 1 according to this embodiment include a carcass ply 23 as a first tire component made of a fibrous member, a shoulder pad 38 or a second pad 36 as a second tire component made of a rubber member having a tapered end in a cross-sectional view in the tire width direction and arranged so as to cover a portion of the first tire component, and a sidewall rubber 30 as a third tire component covering at least the boundary between the fibrous member and the rubber member, and the covering rubber sheet is arranged so as to straddle the first tire component and the second tire component at the boundary between the first tire component and the second tire component and is covered by the third tire component. This can assist in joining the first tire component and the second tire component, in this embodiment, the joining of the carcass ply 23 as the first tire component and the shoulder pad 38 or the second pad 36 as the second tire component.
[0092] (8) A manufacturing method for producing tire 1 according to this embodiment includes a step of attaching covering rubber sheets 431, 432 at the boundary between the first tire component and the second tire component so as to straddle the first tire component and the second tire component, and a step of attaching a third tire component so as to cover covering rubber sheets 431, 432 attached to the boundary between the first tire component and the second tire component. This can assist in joining the first tire component and the second tire component, in this embodiment, the joining of the carcass ply 23 as the first tire component and the shoulder pad 38 or the second pad 36 as the second tire component.
[0093] (9) The RFID tag 40 of the tire 1 according to this embodiment is disposed at a position where at least three tire constituent members, including one fiber member and two rubber members, intersect. As a result, the movement of the RFID tag 40 is effectively restricted by the fiber member, while the generated stress can be alleviated by the presence of the two rubber members.
[0094] (10) In the tire 1 according to this embodiment, an RFID tag 40 is disposed at a position where the carcass ply 23 as a fibrous member, the shoulder pad 38 as a rubber member, and the sidewall rubber 30 as a rubber member intersect. As a result, the movement of the RFID tag 40 is effectively suppressed by the fiber member, while the generated stress can be alleviated by the presence of the contacting rubber members, the shoulder pad 38 and the sidewall rubber 30. By using the boundary part B between the carcass ply 23 and the shoulder pad 38 as the reference for the position of the RFID tag 40, the variation in the position of the RFID tag 40 is reduced.
[0095] (11) In the tire 1 according to this embodiment, an RFID tag 40 is disposed at a position where the carcass ply 23 as a fibrous member, the second pad 36 as a rubber member, and the sidewall rubber 30 as a rubber member intersect. As a result, the movement of the RFID tag 40 is effectively suppressed by the fiber member, while the generated stress can be alleviated by the presence of the rubber members, the second pad 36, and the sidewall rubber 30. By using the boundary part B between the carcass ply 23 and the second pad 36 as the reference for the position of the RFID tag 40, the variation in the position of the RFID tag 40 is reduced.
[0096] (12) In the tire 1 of this embodiment, the RFID tag 40 is covered with an annular rubber sheet 50, and the annular rubber sheet 50 covers the entire circumference of the boundary between the annular first tire component and the annular second tire component. This can generally assist in joining between the first tire constituent member and the second tire constituent member, for example, in joining between the carcass ply 23 as the first tire constituent member and the shoulder pad 38 or the second pad 36 as the second tire constituent member.
[0097] <Third embodiment> Next, a tire according to a third embodiment will be described with reference to the drawings. In the following description, the same components as those in the first and second embodiments are given the same reference numerals, and detailed description thereof will be omitted.
[0098] FIG. 7 is an enlarged cross-sectional view showing the periphery of the embedded portion of the RFID tag 40 in the tire 1 of the present embodiment. 7, the RFID tag 40 (including a state where at least a part of it is covered by a protective member 43) is disposed at a position where three tire constituent members including one fiber member intersect. For example, the tire 1 of this embodiment includes the carcass ply 23 as a fiber member, the second bead filler 222 as a rubber member disposed on the tire outer surface side of the carcass ply 23, and the second pad 36 as a rubber member disposed on the tire outer surface side of the carcass ply 23 and the second bead filler 222, and the RFID tag 40 is disposed at a position where the carcass ply 23, the second bead filler 222, and the second pad 36 intersect.
[0099] Also in this embodiment, more preferably, the RFID tag 40 is covered with a protective member 43 made of a covering rubber sheet, and the protective member 43 is disposed at a position where three tire constituent members including one fiber member intersect. Specifically, the protective member 43 is disposed so as to straddle the boundary between the carcass ply 23 and the second bead filler 222 at the boundary between the carcass ply 23 and the second bead filler 222. That is, the protective member 43 is attached so as to press the tire radial direction outer end 22A of the second bead filler 222 having a tapered end in a tire width direction cross section (see FIG. 7). The tire outer surface side of the protective member 43 is covered by the second pad 36.
[0100] Here, the carcass ply 23, the second bead filler 222, and the second pad 36 are each annular tire constituent members that constitute the annular tire 1. The protective member 43 that holds the RFID tag 40 is disposed so as to be in surface contact with the carcass ply 23, the second bead filler 222, and the second pad 36.
[0101] Even if the RFID tag 40 is disposed in such a position, the RFID tag 40 is surrounded by the carcass ply 23, the second bead filler 222, and the second pad 36, so that the movement of the RFID tag 40 during tire deformation is effectively suppressed and the RFID tag 40 can be suitably protected. In the present embodiment, the RFID tag 40 is held by the carcass ply 23 and in contact with the second bead filler 222 and the second pad 36, so that the movement of the RFID tag 40 is effectively suppressed by the fiber member, and the generated stress can be alleviated by the presence of the second bead filler 222 and the second pad 36, which are rubber members in contact with the RFID tag 40. The boundary between a plurality of tire constituent members, in this embodiment, the boundary between the carcass ply 23 and the second bead filler 222, is used as the reference for the position of the RFID tag 40, so that the variation in the position of the RFID tag 40 is reduced. This also reduces the chance of the RFID tag 40 being accidentally placed in an undesirable location, and helps ensure that the RFID tag 40 continues to function properly.
[0102] In addition, when the modulus of the second pad 36 is taken as a standard, the sidewall rubber 30 preferably has a modulus 0.4 to 0.6 times that of the second pad 36. In addition, the first pad 35 preferably has a modulus 1.1 to 1.2 times that of the second pad 36. In addition, the second bead filler 222 preferably has a modulus 0.7 to 0.8 times that of the second pad. In addition, when the modulus of the second pad 36 is taken as a standard, the rim strip rubber 32 preferably has a modulus 0.8 to 1 times that of the second pad 36. In addition, the rubber sheet 37 preferably has a modulus 1.1 to 1.2 times that of the second pad 36. In other words, the modulus of the rubber sheet 37 is preferably approximately equal to the modulus of at least the portion (first pad 35) of the pad member 34 that covers the folded end 25A of the carcass ply 23. By setting the modulus in this range, a balance between the flexibility of the tire and the rigidity in the vicinity of the bead 11 can be maintained. The modulus refers to the 100% elongation modulus (M100) measured in an atmosphere of 23° C. in accordance with “3.7 Stress at a given elongation, S” of JIS K6251:2010.
[0103] 7, the RFID tag 40 may be placed at the position of the end 32B on the inner side in the tire width direction of the rim strip rubber 32, that is, at the position where the carcass ply 23, the rim strip rubber 32, and the inner liner 29 intersect. Even in this case, the RFID tag 40 is placed at the position where three tire constituent members including one fiber member intersect. This makes it possible to obtain the above-mentioned effects of suitably protecting the RFID tag 40 and reducing the variation in the placement position of the RFID tag 40.
[0104] 7, the RFID tag 40 may be disposed at the position of the tire radial direction inner end 36B of the second pad 36, that is, at the position where the carcass ply 23, the second pad 36, and the rim strip rubber 32 intersect. In this case, too, the RFID tag 40 is disposed at the position where three tire constituent members including one fiber member intersect. Therefore, the above-mentioned effects of suitably protecting the RFID tag 40 and reducing the variation in the placement position of the RFID tag 40 can be obtained.
[0105] In addition to the above advantages (1) to (2), (5), (7) to (9), and (12), the tire 1 of the present embodiment has the following advantages.
[0106] (13) In the tire 1 according to this embodiment, the RFID tag 40 is disposed at a position where the carcass ply 23 as a fiber member, the second bead filler 222 as a rubber member, and the second pad 36 as a rubber member intersect. This makes it possible to effectively suppress the movement of the RFID tag 40 by the fiber member, while the generated stress can be alleviated by the rubber member. In addition, there is also an effect of reducing the variation in the arrangement position of the RFID tag 40.
[0107] (14) In the tire 1 according to this embodiment, the RFID tag 40 is disposed at a position where the carcass ply 23 as a fiber member, the rim strip rubber 32 as a rubber member, and the inner liner 29 as a rubber member intersect. This makes it possible to effectively suppress the movement of the RFID tag 40 by the fiber member, while the generated stress can be alleviated by the rubber member. In addition, there is also an effect of reducing the variation in the arrangement position of the RFID tag 40.
[0108] (15) In the tire 1 according to this embodiment, the RFID tag 40 is disposed at a position where the carcass ply 23 as a fiber member, the second pad 36 as a rubber member, and the rim strip rubber 32 as a rubber member intersect. This makes it possible to effectively suppress the movement of the RFID tag 40 by the fiber member, while the generated stress can be alleviated by the rubber member. In addition, there is also an effect of reducing the variation in the arrangement position of the RFID tag 40.
[0109] <Fourth embodiment> Next, a tire according to a fourth embodiment will be described with reference to the drawings. In the following description, the same components as those in the first to third embodiments are given the same reference numerals, and detailed description thereof will be omitted.
[0110] FIG. 8 is an enlarged cross-sectional view showing the periphery of the embedded portion of the RFID tag 40 in the tire 1 of the present embodiment. 8, the RFID tag 40 (including a state where at least a part of it is covered by a protective member 43) is disposed at a position where three tire constituent members including two fiber members intersect. For example, the tire 1 of this embodiment includes a carcass ply 23 as a fiber member, a steel chafer 31 as a fiber member, and an inner liner 29 as a rubber member, and the RFID tag 40 is disposed at a position where the carcass ply 23, the steel chafer 31, and the inner liner 29 intersect in such a manner that the RFID tag 40 comes into contact with an end 31B of the steel chafer 31 on the inner side in the tire width direction.
[0111] Also in this embodiment, more preferably, the RFID tag 40 is covered with a protective member 43 made of a covering rubber sheet, and this protective member 43 is placed at the intersection of three tire constituent members including two fiber members.
[0112] Here, the carcass ply 23, the steel chafer 31, and the inner liner 29 are each annular tire constituent members that constitute the annular tire 1. The protective member 43 that holds the RFID tag 40 is disposed so as to be in contact with the carcass ply 23, the steel chafer 31, and the inner liner 29.
[0113] Even if the RFID tag 40 is placed in such a position, the RFID tag 40 is surrounded by three tire constituent members including two fiber members, so that the movement of the RFID tag 40 during tire deformation is effectively suppressed and the RFID tag 40 can be suitably protected. Furthermore, by using the boundary portion between multiple tire constituent members as the reference for the placement position of the RFID tag 40, the variation in the placement position of the RFID tag 40 is reduced. This reduces the possibility that the RFID tag 40 is mistakenly placed in an undesirable position, and the function of the RFID tag 40 can be maintained appropriately.
[0114] As shown by the dotted line in Fig. 8, the RFID tag 40 may be disposed at the intersection of the carcass ply 23, the steel chafer 31, and the first pad 35 in such a manner that the RFID tag 40 contacts the outer end 31A of the steel chafer 31 in the tire width direction. Even in this case, the RFID tag 40 is disposed at the intersection of three tire constituent members including two fiber members. Therefore, the above-mentioned effects of suitably protecting the RFID tag 40 and reducing the variation in the arrangement position of the RFID tag 40 can be obtained.
[0115] In addition to the above advantages (1) to (3), (5) to (6), and (12), the tire 1 of the present embodiment has the following advantages.
[0116] (16) In the tire 1 according to the present embodiment, the RFID tag 40 is disposed at a position where the carcass ply 23 as a fibrous member, the steel chafer 31 as a fibrous member, and the inner liner 29 as a rubber member intersect. This makes it possible to effectively suppress the movement of the RFID tag 40 by the fiber member, while the generated stress can be alleviated by the rubber member. In addition, there is also an effect of reducing the variation in the arrangement position of the RFID tag 40.
[0117] (17) In the tire 1 according to the present embodiment, the RFID tag 40 is disposed at a position where the carcass ply 23 as a fibrous member, the steel chafer 31 as a fibrous member, and the first pad 35 as a rubber member intersect. This makes it possible to effectively suppress the movement of the RFID tag 40 by the fiber member, while the generated stress can be alleviated by the rubber member. In addition, there is also an effect of reducing the variation in the arrangement position of the RFID tag 40.
[0118] <Fifth embodiment> Next, a tire according to a fifth embodiment will be described with reference to the drawings. In the following description, the same components as those in the first to third embodiments are given the same reference numerals, and detailed description thereof will be omitted.
[0119] FIG. 9 is an enlarged cross-sectional view showing the periphery of the embedded portion of the RFID tag 40 in the tire 1 of the present embodiment. 9, the RFID tag 40 (including a state where at least a part of it is covered by a protective member 43) is disposed at a position where three tire constituent members, including one fiber member, intersect. More specifically, the tire 1 of this embodiment includes a carcass ply 23 as a fiber member, a rubber sheet 37 as a rubber member, and a second bead filler 222 as a rubber member, and the RFID tag 40 is disposed at a position where the carcass ply 23, the rubber sheet 37, and the second bead filler 222 intersect such that the RFID tag 40 comes into contact with an inner end 37B of the rubber sheet 37 in the tire radial direction.
[0120] Also in this embodiment, more preferably, the RFID tag 40 is covered with a protective member 43 made of a covering rubber sheet, and this protective member 43 is placed at a position where three tire constituent members including one fiber member intersect.
[0121] Here, the carcass ply 23, the rubber sheet 37, and the second bead filler 222 are each annular tire constituent members that constitute the annular tire 1. The protective member 43 that holds the RFID tag 40 is disposed so as to be in contact with the carcass ply 23, the rubber sheet 37, and the second bead filler 222.
[0122] Even if the RFID tag 40 is placed in such a position, the RFID tag 40 is surrounded by three tire constituent members including one fiber member, so that movement of the RFID tag 40 during tire deformation is effectively suppressed and the RFID tag 40 can be suitably protected. Furthermore, by using the boundary between multiple tire constituent members as the reference for the placement position of the RFID tag 40, variation in the placement position of the RFID tag 40 is reduced. This reduces the possibility that the RFID tag 40 will be mistakenly placed in an undesirable position, and the function of the RFID tag 40 can be maintained appropriately.
[0123] 9, the RFID tag 40 may be disposed at the intersection of the steel chafer 31, the first pad 35, and the second pad 36 in such a manner that the RFID tag 40 comes into contact with the tire radial direction inner end 35B of the first pad 35. In this case as well, the RFID tag 40 is disposed at the intersection of three tire constituent members including one fiber member. Therefore, the above-mentioned effects of suitably protecting the RFID tag 40 and reducing the variation in the arrangement position of the RFID tag 40 can be obtained.
[0124] In addition to the above advantages (1) to (2), (5), (9) and (12), the tire 1 of the present embodiment has the following advantages.
[0125] (18) In the tire 1 according to the present embodiment, the RFID tag 40 is disposed at a position where the carcass ply 23 as a fibrous member, the rubber sheet 37 as a rubber member, and the second bead filler 222 as a rubber member intersect. This makes it possible to effectively suppress the movement of the RFID tag 40 by the fiber member, while the generated stress can be alleviated by the rubber member. In addition, there is also an effect of reducing the variation in the arrangement position of the RFID tag 40. (19) In the tire 1 according to this embodiment, the RFID tag 40 is disposed at the intersection of the steel chafer 31 as a fiber member, the first pad 35 as a rubber member, and the second pad 36 as a rubber member. This makes it possible to effectively suppress the movement of the RFID tag 40 by the fiber member, while the generated stress can be alleviated by the rubber member. In addition, there is also an effect of reducing the variation in the arrangement position of the RFID tag 40.
[0126] Sixth Embodiment Next, a tire according to a sixth embodiment will be described with reference to the drawings. In the following description, the same components as those in the first to third embodiments are given the same reference numerals, and detailed description thereof will be omitted.
[0127] FIG. 10 is an enlarged cross-sectional view showing the periphery of the embedded portion of the RFID tag 40 in the tire 1 of the present embodiment. 10, the RFID tag 40 (including a state where at least a part of it is covered by a protective member 43) is disposed at a position where three tire constituent members including one fiber member intersect. More specifically, the tire 1 of this embodiment includes a carcass ply 23 as a fiber member, a second bead filler 222 as a rubber member, and a first bead filler 221 as a rubber member, and the RFID tag 40 is disposed at a position 22B on the inner side in the tire width direction, which is a position where the carcass ply 23, the second bead filler 222, and the first bead filler 221 intersect.
[0128] Also in this embodiment, more preferably, the RFID tag 40 is covered with a protective member 43 made of a covering rubber sheet, and this protective member 43 is placed at a position where three tire constituent members including one fiber member intersect.
[0129] Here, the carcass ply 23, the second bead filler 222, and the first bead filler 221 are each annular tire constituent members that constitute the annular tire 1. The protective member 43 that holds the RFID tag 40 is disposed so as to be in contact with the carcass ply 23, the second bead filler 222, and the first bead filler 221.
[0130] Even if the RFID tag 40 is placed in such a position, the RFID tag 40 is surrounded by three tire constituent members including one fiber member, so that movement of the RFID tag 40 during tire deformation is effectively suppressed and the RFID tag 40 can be suitably protected. Furthermore, by using the boundary between multiple tire constituent members as the reference for the placement position of the RFID tag 40, variation in the placement position of the RFID tag 40 is reduced. This reduces the possibility that the RFID tag 40 will be mistakenly placed in an undesirable position, and the function of the RFID tag 40 can be maintained appropriately. 10, the RFID tag 40 may be disposed at a position 22C on the outer side in the tire width direction, which is a position where the carcass ply 23, the second bead filler 222, and the first bead filler 221 intersect. Even in this case, the RFID tag 40 is disposed at a position where three tire constituent members including one fiber member intersect. Therefore, the above-mentioned effects of suitably protecting the RFID tag 40 and reducing the variation in the position where the RFID tag 40 is disposed can be obtained.
[0131] In addition to the above advantages (1) to (2), (5), (7) to (9), and (12), the tire 1 of the present embodiment has the following advantages.
[0132] (20) In the tire 1 according to the present embodiment, the RFID tag 40 is disposed at a position where the carcass ply 23 as a fiber member, the second bead filler 222 as a rubber member, and the first bead filler 221 as a rubber member intersect. This makes it possible to effectively suppress the movement of the RFID tag 40 by the fiber member, while the generated stress can be alleviated by the rubber member. In addition, there is also an effect of reducing the variation in the arrangement position of the RFID tag 40.
[0133] Seventh embodiment Next, a tire according to a seventh embodiment will be described with reference to Figures 11 to 17. In the following description, the same components as those in the first to third embodiments are given the same reference numerals, and detailed description thereof will be omitted. This embodiment is particularly suitable when the antenna of the RFID tag 40 is a coil spring antenna.
[0134] The RFID tag 40 of this embodiment uses a coil-shaped spring antenna 421 with high communication performance and flexibility as an antenna. The spring antenna 421 is set to an antenna length optimized according to the frequency band to be used, etc.
[0135] In this embodiment, rubber is placed inside the spring antenna 421 before the RFID tag 40 is sandwiched between the two covering rubber sheets 431, 432 constituting the protective member 43. More preferably, the rubber is filled inside the spring antenna so that as little air as possible remains. The process and the reason for adopting the process will be described with reference to Figures 11 to 17.
[0136] 11 to 13, a state around the RFID tag 40 when no rubber is filled in the spring antenna 421 will be described as a reference example. Fig. 11 is a diagram showing cross sections of the spring antenna 421 and the covering rubber sheets 431 and 432 before the RFID tag 40 is sandwiched between the covering rubber sheets 431 and 432. Fig. 12 is a diagram showing cross sections of the spring antenna 421 and the covering rubber sheets 431 and 432 after the RFID tag 40 has been sandwiched between the covering rubber sheets 431 and 432.
[0137] 12, in this reference example, since rubber is not filled in spring antenna 421 beforehand, a certain amount of air 45 may remain in spring antenna 421 after it is sandwiched between covering rubber sheets 431, 432. If air remains in this way, the integrity between covering rubber sheets 431, 432 and spring antenna 421 will be insufficient, and spring antenna 421 will not follow the movement of the rubber when the tire deforms, which may damage RFID tag 40 having spring antenna 421.
[0138] In this example, raw rubber before vulcanization is used as the covering rubber sheets 431, 432. Therefore, by pressing the covering rubber sheets 431, 432 from both sides, the covering rubber sheets 431, 432 are embedded to a certain extent into the spring antenna, as shown in Fig. 12. However, it takes a great deal of time and effort to embed the covering rubber sheets 431, 432 until they are completely embedded inside the spring antenna.
[0139] Even if the rubber sheet is driven in over a long period of time until it is completely filled in the spring antenna, the distance L between the outer periphery of spring antenna 421 and the outer surfaces of covering rubber sheets 431 and 432 becomes very short as shown in Fig. 13. It is also difficult to stabilize the distance L, and localized thin portions may occur. This results in insufficient protection of RFID tag 40 by covering rubber sheets 431 and 432, and there is a possibility that covering rubber sheets 431 and 432 may be damaged during vulcanization.
[0140] Therefore, in this embodiment, as shown in Figures 14 to 17, rubber is placed inside spring antenna 421 before RFID tag 40 is sandwiched between covering rubber sheets 431, 432. More preferably, rubber is filled inside spring antenna 421 so that as little air as possible remains. The drawings on the right side of Figures 14 to 17 are cross-sectional views of spring antenna 421 and its surroundings.
[0141] FIG. 14 is a diagram showing the state before the rubber 46 is filled inside the spring antenna 421, and FIG. 15 is a diagram showing the state after the rubber 46 is filled inside the spring antenna 421. Rubber 46 is embedded so as to have approximately the same outer diameter as the outer circumferential surface of spring antenna 421. If rubber 46 protrudes beyond the outer circumferential surface of spring antenna 421, it is preferable to wipe off the protruding portion. In other words, it is preferable that the outer circumferential surface of rubber 46 is molded so as to be approximately flush with the outer circumferential surface of spring antenna 421. It is also possible to fill the inside of the spring antenna 421 with rubber 46 and to wrap the outer periphery of the spring antenna 421 thinly with rubber 46. On the other hand, wrapping the spring antenna 421 thickly with rubber 46 is not preferable because it reduces the flexibility of the spring antenna 421 and increases the width dimension formed by the covering rubber sheets 431 and 432 after the RFID tag 40 is sandwiched therebetween. The rubber 46 may be embedded so that its outer diameter is approximately the same as the inner circumferential surface of the spring antenna 421. It is desirable that the outer circumferential portion of the rubber 46 is located within the range from the inner circumferential surface to the outer circumferential surface of the spring antenna 421.
[0142] Here, in order to ensure the flexibility of spring antenna 421, a flexible rubber is used as rubber 46. However, in consideration of workability and the like, it is preferable to use a rubber with a higher modulus than covering rubber sheets 431 and 432 as rubber 46. Incidentally, unvulcanized rubber is preferably used as the rubber 46 disposed inside the spring antenna 421. By making the rubber 46 and the covering rubber sheets 431 and 432 unvulcanized rubber and vulcanizing them simultaneously, the integrity of the rubber 46, the covering rubber sheets 431 and 432, and the spring antenna 421 is improved. Also, it is more preferable that the rubber 46 and the covering rubber sheets 431 and 432 are made of the same type of rubber. In addition, in consideration of the flexibility of the spring antenna 421, rubber 46 may have a lower modulus than the covering rubber sheets 431 and 432. Also, rubber of approximately the same modulus or rubber of the same material may be used. Note that vulcanized rubber may be used as the rubber 46 disposed inside the spring antenna 421. It is also possible to use a rubber adhesive, a rubber filler, or the like. Various rubber materials can be used while ensuring flexibility and taking into consideration the need to minimize the amount of air remaining inside the spring antenna 421. Various methods can be used for arranging the rubber 46, but for example, it is also possible to inject the rubber into the spring antenna 421 using a syringe. In this case, a set appropriate amount of the rubber 46 may be filled using the syringe. Also, after filling a larger amount of the rubber 46, the portion protruding from the outer periphery of the spring antenna 421 may be wiped off.
[0143] FIG. 16 shows the RFID tag 40 having the spring antenna 421 filled with rubber 46 before it is sandwiched between the covering rubber sheets 431 and 432, and FIG. 17 shows the RFID tag 40 after it is sandwiched between the covering rubber sheets 431 and 432.
[0144] 17, according to this embodiment, since the rubber 46 is filled in advance inside the spring antenna 421, no air pocket exists between the covering rubber sheets 431 and 432. Therefore, since there is no need to worry about air pockets, the process of sandwiching the RFID tag 40 between the covering rubber sheets 431 and 432 is simplified. In addition, by disposing the rubber 46 inside the spring antenna 421, the integrity of the spring antenna 421, the rubber 46, and the covering rubber sheets 431 and 432 is improved, and when the tire deforms, the spring antenna 421 follows the movement of the rubber. Therefore, the durability of the RFID tag 40 having the spring antenna 421 is also improved.
[0145] Moreover, according to this embodiment, the distance L between the outer periphery of the spring antenna 421 and the outer surfaces of the covering rubber sheets 431 and 432 is stable. That is, the distance L is generally secured to be close to the thickness of the covering rubber sheets 431 and 432. Therefore, the RFID tag 40 is sufficiently protected by the covering rubber sheets 431 and 432. In this embodiment, the RFID tag 40 sandwiched between the covering rubber sheets 431, 432 is disposed between the tire constituent members, and then the green tire is vulcanized.
[0146] In this embodiment, the RFID tag 40, in which the spring antenna 421 is filled with rubber 46 in advance, is covered with covering rubber sheets 431 and 432, and then is placed between the tire constituent members. However, the RFID tag 40 in which the rubber 46 has been filled in advance inside the spring antenna 421 may be disposed between the tire constituent members without being covered with the covering rubber sheets 431 and 432 . In this way, by disposing the uncoated RFID tag 40 directly between tire constituent members, the variation in thickness of the rubber member where the RFID tag 40 is sandwiched is reduced, improving the uniformity of the tire 1. In addition, since the rubber 46 is filled in advance inside the spring antenna 421, the rubber sheet 37 will not be excessively embedded in the spring antenna.
[0147] In addition to the above advantages (1) to (20), the tire according to this embodiment has the following advantages.
[0148] (21) In this embodiment, the RFID tag 40 as an electronic component with communication function has a spring antenna 421, and a step of placing rubber 46 within the spring antenna 421 is provided prior to the step of attaching the RFID tag 40 to a tire constituent member. This makes it possible to easily assemble the RFID tag 40 without having to worry about air pockets during the process of sandwiching the spring antenna 421 of the RFID tag 40 between rubber members. (22) In this embodiment, the method includes a step of placing rubber 46 inside spring antenna 421 of RFID tag 40, which is an electronic component having communication function; a step of sandwiching RFID tag 40 having spring antenna 421 with rubber 46 placed therein, between covering rubber sheets 431, 432; and a step of disposing RFID tag 40 sandwiched between covering rubber sheets 431, 432 between tire constituent members. This prevents air 45 from remaining inside the spring antenna 421. In addition, since there is no need to worry about air pockets, the task of sandwiching the RFID tag 40 between the covering rubber sheets 431 and 432 is also simplified. Furthermore, since the distance L between the outer periphery of the spring antenna 421 and the outer surfaces of the covering rubber sheets 431 and 432 is stable, the RFID tag 40 is sufficiently protected by the covering rubber sheets 431 and 432 .
[0149] (23) This embodiment includes a step of placing rubber 46 within the spring antenna 421 of the RFID tag 40, which is an electronic component having communication function, and a step of attaching a rubber sheet 37 to the bead filler 22 so as to sandwich the uncoated RFID tag 40 between the tire constituent components. In this way, by sandwiching the uncoated electronic component directly between tire constituent members, the variation in thickness of the rubber member in the portion where the RFID tag 40 is sandwiched is reduced, improving the uniformity of the tire 1. In addition, since the rubber 46 is filled in advance inside the spring antenna 421, the rubber sheet 37 will not be excessively embedded in the spring antenna.
[0150] The tire of the present invention can be used as various tires for passenger cars, light trucks, trucks, buses, etc., and is particularly suitable as a tire for trucks, buses, etc. The present invention is not limited to the above-described embodiment, and even if modifications and improvements are made within the scope of the present invention, they will still be included in the scope of the present invention. [Explanation of symbols]
[0151] 1. Tires 11...Bead 12…Tread 13…Sidewall 21…Bead core 22…Bead filler 22A…Tire radial outer end 221…First bead filler 222…Second bead filler 23…Carcass ply 24…Ply body 25…Ply turn-up section 26…Steel belt 28...Tread rubber 28B…Tire radial inner end 29…Inner liner 30...Sidewall rubber 31…Steel Chaher 32…Rim strip rubber 32B...end 34...Pad member 35…First pad 36…Second pad 36A…Tire radial outer end 36B…Tire radial inner end 37…Rubber sheet 38…Shoulder pads 38A…Inner end in the tire width direction 38B…Tire radial inner end 40…RFID tag 41…RFID chip 42…Antenna 421...Spring antenna 43...Protective material 431, 432...Rubber sheet 46…Rubber
Claims
1. The tire includes a plurality of tire constituent members that constitute a tire, and an electronic component, The plurality of tire constituent members include a rubber member and a fiber member, the fiber member includes a carcass ply, the rubber member includes a bead filler disposed on a tire outer surface side of the carcass ply, and a pad member disposed on the tire outer surface side of the carcass ply and the bead filler, The tire, wherein the electronic component is disposed at a position where the carcass ply, the bead filler, and the pad member intersect.
2. A tire as described in claim 1, wherein the carcass ply, the bead filler and the pad member as the tire constituent members are each annular members formed in a circular ring shape.
3. 3. The tire according to claim 1, wherein at least a portion of the electronic component is covered by a covering rubber sheet, and the covering rubber sheet covering the electronic component is disposed at a position where the carcass ply, the bead filler, and the pad member intersect.
4. 4. The tire according to claim 3, wherein the covering rubber sheet is arranged at a boundary between the carcass ply as a first tire component and the bead filler as a second tire component, so as to straddle the first tire component and the second tire component, and is covered by the pad member as a third tire component.
5. A method for producing the tire according to claim 4, comprising the steps of: a step of attaching the covering rubber sheet to a boundary portion between the carcass ply as the first tire component member and the bead filler as the second tire component member so as to straddle the first tire component member and the second tire component member; and attaching the pad member as the third tire component so as to cover the covering rubber sheet attached to the boundary portion between the first tire component and the second tire component.
Citation Information
Patent Citations
Pneumatic tire provided with electronic component and method for manufacturing same
JP2015223918A
tire
JP2016037236A
tire
JP2016049920A
Pneumatic tire
JP2017222294A