Circuit board, manufacturing method thereof, and inspection method thereof
The ceramic substrate with partition lines and through holes enables precise detection of defects, ensuring high-yield production of reliable circuit boards by accurately identifying and excluding defective parts, thus enhancing insulation properties and yield.
Patent Information
- Application Number
- JP2021526883
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-06-28
- Filing Date
- 2020-06-18
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2040-06-18
AI Technical Summary
Power module circuit boards require high insulation properties, but ceramic substrates are prone to defects that impair insulation, leading to reduced yield and reliability if not accurately detected and discarded.
A ceramic substrate with partition lines and through holes allows for precise detection of defects, enabling high-yield production of reliable circuit boards by excluding defective parts.
The method ensures high reliability and yield of circuit boards by accurately identifying and excluding defective ceramic substrates, reducing manufacturing costs and improving insulation inspection efficiency.
Smart Images

Figure 0007588071000002 
Figure 0007588071000003 
Figure 0007588071000004
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a ceramic substrate and a manufacturing method thereof, a composite substrate, a circuit substrate and a manufacturing method thereof, and a method for inspecting a circuit substrate. [Background technology]
[0002] Power modules that control large currents are used in fields such as automobiles, electric railways, industrial equipment, and power generation. The circuit board mounted on the power module has an insulating ceramic substrate. The following technology, as described in Patent Document 1, is known as a method for manufacturing a circuit board. That is, a composite substrate is formed by bonding metal layers to both sides of a ceramic substrate having a scribe line formed on its surface. Then, the metal layer on the surface of the composite substrate is processed into a circuit pattern by etching. After that, the composite substrate is divided along the scribe lines to manufacture a plurality of circuit substrates.
[0003] Circuit boards, as insulating boards, are required to have voltage resistance characteristics. As a method for testing voltage resistance characteristics, for example, a method of testing in liquid such as insulating oil to avoid discharge into the atmosphere is known. Patent Document 2 proposes a technology for testing voltage resistance in a fluorine-based inert liquid. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2007-324301 A [Patent Document 2] JP 2016-183923 A Summary of the Invention [Problem to be solved by the invention]
[0005] Circuit boards for power modules are required to have excellent insulation properties. Here, if there are defects such as scratches in the ceramic substrate that is responsible for the insulation properties of the circuit board, the insulation properties will be impaired, so it is necessary to eliminate the defects as much as possible. On the other hand, since ceramic substrates are more prone to defects than other materials, it is difficult to completely eliminate defects. For this reason, it is necessary to inspect the presence or absence of defects by an inspection before forming the circuit board, and to reject ceramic substrates in which defects are found. On the other hand, if a ceramic substrate with even one defect is discarded as a defective product, the yield will decrease. For this reason, it is believed that a technology that can eliminate defective parts with high accuracy, even when a ceramic substrate with defects is used, can greatly contribute to improving the reliability of the circuit board.
[0006] In view of the above, the present disclosure provides a ceramic substrate and a manufacturing method thereof that can provide a highly reliable circuit board. It also provides a composite substrate and a highly reliable circuit board. It also provides a highly reliable circuit board and a manufacturing method thereof. It also provides a method for inspecting a circuit board that can improve the reliability of the circuit board. [Means for solving the problem]
[0007] A ceramic substrate according to one aspect of the present disclosure is a ceramic substrate having a surface divided into a plurality of sections by partition lines, and at least one of the partitions defined by the partition lines has a defect and a through hole.
[0008] Since such a ceramic substrate has a defect and a through hole in one partition, the partition having a defect can be detected with high accuracy even after processing into a circuit board. Therefore, the partition having a defect can be removed with high accuracy. Therefore, even if a ceramic substrate having a defect is used, a circuit board having high reliability can be obtained. Although this ceramic substrate has a defect, it can be used to manufacture a circuit board, so that the circuit board can be manufactured with a high yield. In other words, the above-mentioned ceramic substrate makes it possible to manufacture a circuit board having high reliability with a high yield.
[0009] The opening area of the through hole on the surface of the above-mentioned ceramic substrate is 1200 μm 2 This makes it possible to detect sections having defects with even higher accuracy, thereby further reducing the manufacturing costs of the circuit board and the workload involved in the insulation inspection.
[0010] At least a portion of the through hole may be tapered, which makes it easier for the brazing material to be filled from the surface side having the larger opening, thereby further improving the accuracy of detecting defects.
[0011] At least a part of the through hole may be filled with a brazing material. This can further improve the detection accuracy of the partition having the defect and the through hole. Note that the "through hole" in this disclosure does not necessarily have to be a cavity, and may be filled with a material different from the material constituting the ceramic substrate.
[0012] A composite substrate according to one aspect of the present disclosure includes a pair of metal substrates arranged to face each other, and any one of the ceramic substrates described above between the pair of metal substrates. Since the composite substrate includes the ceramic substrate described above, it is possible to manufacture highly reliable circuit substrates with a high yield.
[0013] A circuit board according to one aspect of the present disclosure includes any one of the ceramic substrates described above and conductor portions arranged to face each other across the ceramic substrate, the conductor portions being provided independently for each partition portion.
[0014] Such a circuit board has high reliability and can be manufactured with a high yield because it includes the above-mentioned ceramic substrate.
[0015] A method for manufacturing a ceramic substrate according to one aspect of the present disclosure includes a step of irradiating a surface of a base material made of ceramic with laser light to form partition lines that divide the surface into multiple sections, and a step of providing a through hole in at least one of the partition sections defined by the partition lines, the partition section having a defect, to obtain a ceramic substrate.
[0016] In the above manufacturing method, since a through hole is provided in at least one partition having a defect, the partition can be detected with high accuracy. Therefore, the partition having a defect can be removed with high accuracy. Therefore, even if a ceramic substrate having a defect is used for manufacturing a circuit substrate, a highly reliable circuit substrate can be obtained. Since the ceramic substrate obtained by this manufacturing method can be used for manufacturing a circuit substrate even if it has a defect, the circuit substrate can be manufactured with a high yield. In other words, the above-mentioned manufacturing method of a ceramic substrate makes it possible to manufacture a highly reliable circuit substrate with a high yield.
[0017] A method for manufacturing a circuit board according to one aspect of the present disclosure includes the steps of stacking a pair of metal substrates so as to sandwich the ceramic substrate obtained by the above-described manufacturing method to obtain a composite substrate, removing portions of the metal substrates in the composite substrate to form independent conductor portions for each partition portion, and applying a voltage between the pair of conductor portions sandwiching the ceramic substrate to measure the current.
[0018] In the above manufacturing method, a voltage is applied between a pair of conductors sandwiching a ceramic substrate having a through hole in at least one partition having a defect, and a current is measured. Therefore, the defective portion of the ceramic substrate and the partition having a through hole can be detected with high accuracy. Therefore, the partition having a defective portion can be removed with high accuracy. Therefore, even if a ceramic substrate having a defective portion is used for manufacturing a circuit substrate, a circuit substrate having high reliability can be manufactured. In this manufacturing method, since a ceramic substrate having a defective portion can be used for manufacturing a circuit substrate, the circuit substrate can be manufactured with a high yield. In other words, this manufacturing method for a circuit substrate makes it possible to manufacture a circuit substrate having high reliability with a high yield.
[0019] A method for inspecting a circuit board according to one aspect of the present disclosure is the above-mentioned method for inspecting a circuit board, and includes a step of applying a voltage between at least a pair of conductor parts sandwiching a ceramic board and measuring a current. Since the ceramic board has a through hole in at least one partition part having a defect, the partition part having a defect can be detected with high accuracy. Therefore, a circuit board having high reliability can be obtained. Furthermore, since the ceramic board can be used to manufacture a circuit board even if it has a defect, the circuit board can be manufactured with a high yield. In other words, the above-mentioned method for inspecting a circuit board makes it possible to manufacture a circuit board having high reliability with a high yield.
[0020] A method for inspecting a circuit board relating to another aspect of the present disclosure is a method for inspecting a circuit board including a ceramic substrate having a surface divided into a plurality of sections by dividing lines, and conductor portions arranged opposite each other across the ceramic substrate and provided independently for each divided section defined by the dividing lines, the method including a step of applying a voltage between a pair of conductor portions sandwiching the ceramic substrate and measuring a current for each divided section.
[0021] This inspection method makes it possible to easily and quickly inspect each partition for the presence or absence of defects. By carrying out such inspection, highly reliable circuit boards can be obtained with high productivity. Effect of the Invention
[0022] According to the present disclosure, it is possible to provide a ceramic substrate capable of obtaining a highly reliable circuit board and a manufacturing method thereof. It is also possible to provide a composite substrate capable of obtaining a highly reliable circuit board. It is also possible to provide a highly reliable circuit board and a manufacturing method thereof. It is also possible to provide a method for inspecting a circuit board capable of improving the reliability of the circuit board. [Brief description of the drawings]
[0023] [Figure 1] FIG. 1 is a perspective view of a ceramic substrate according to one embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along line II-II in FIG. [Diagram 3] FIG. 3 is a cross-sectional view taken along line III-III in FIG. [Figure 4] FIG. 4 is a perspective view of a composite substrate according to an embodiment. [Diagram 5] FIG. 5 is a perspective view of a circuit board according to an embodiment. [Figure 6] FIG. 6 is a perspective view showing an example of a ceramic substrate to which a brazing material is applied. [Figure 7] FIG. 7 is a perspective view showing an example of a composite substrate having a resist pattern formed on the surface thereof. [Figure 8] FIG. 8 is a diagram showing an example of an inspection device for measuring leakage current of a circuit board. [Figure 9] FIG. 9 is a photograph of an optical microscope image showing the surface and through holes of the ceramic substrate of Experimental Example 3. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] Hereinafter, an embodiment of the present disclosure will be described with reference to the drawings as needed. However, the following embodiment is an example for explaining the present disclosure, and is not intended to limit the present disclosure to the following content. In the description, the same reference numerals are used for the same elements or elements having the same functions, and redundant descriptions are omitted as needed. Furthermore, positional relationships such as up, down, left, and right are based on the positional relationships shown in the drawings, unless otherwise specified. Furthermore, the dimensional ratios of each element are not limited to the ratios shown in the drawings.
[0025] FIG. 1 is a perspective view of a ceramic substrate according to one embodiment. The ceramic substrate 100 in FIG. 1 has a flat plate shape. A surface 100A of the ceramic substrate 100 is divided into a plurality of sections by division lines. The surface 100A is provided with a plurality of division lines L1 extending along a first direction and arranged at equal intervals, and a plurality of division lines L2 extending along a second direction perpendicular to the first direction and arranged at equal intervals. The division lines L1 and L2 are perpendicular to each other.
[0026] The dividing lines L1, L2 may be, for example, a plurality of depressions arranged in a straight line, or may be linear grooves. Specifically, they may be scribe lines formed by laser light. Examples of the laser source include a carbon dioxide laser and a YAG laser. The scribe lines can be formed by intermittently irradiating the laser light from such a laser source. The dividing lines L1, L2 do not have to be arranged at equal intervals, and are not limited to being perpendicular to each other. Moreover, they may be curved or bent instead of straight.
[0027] Fig. 2 is a cross-sectional view taken along line II-II in Fig. 1, and Fig. 3 is a cross-sectional view taken along line III-III in Fig. 1. As shown in Figs. 1, 2, and 3, the partition 10 is a three-dimensional area surrounded by a region of the front surface 100A surrounded by partition lines L1 and L2, a region of the back surface 100B corresponding to the region, and virtual lines VL1 and VL2 drawn parallel to the thickness direction of the ceramic substrate 100 from the partition lines L1 and L2. That is, the ceramic substrate 100 has a plurality of partitions 10 defined by the partition lines L1 and L2. Among the plurality of partitions 10, the partition 10a has a defect portion 11 and a through hole 12.
[0028] The through-holes 12 penetrate the ceramic substrate 100 in the thickness direction, and are formed, for example, by using a laser beam or a drill. The through-holes 12 may be hollowed out in a cylindrical shape. However, the shape is not limited to a cylindrical shape. The opening area of the through-holes 12 on the front surface 100A and the back surface 100B is, for example, 1200 μm 2 It may be 5000 μm or more. 2 It may be 7000 μm or more. 2 In this way, by having the opening areas on the front surface 100A and the back surface 100B have a predetermined size, the partitions 10a having the defects 11 can be detected with higher accuracy. From the viewpoint of reducing the time required to form the through holes 12, the opening area of the through holes 12 is set to 0.5 mm 2 It may be the following:
[0029] For example, the through hole 12 may be tapered in part so as to be narrowed along the thickness direction of the ceramic substrate 100. That is, the through hole 12 may have a tapered portion whose hole diameter changes along the thickness direction of the ceramic substrate 100. The entire through hole 12 may be tapered. When the opening areas of the through hole 12 on the front surface 100A and the back surface 100B are different, the brazing material can be smoothly filled by applying the brazing material from the side of the through hole 12 with the larger opening area. If the brazing material is filled in the through hole 12, the defective portion 11 can be detected with higher accuracy.
[0030] The defect 11 refers to a cause of leakage current when the substrate is made into a circuit board, and examples of the defect include cracks, holes, scratches, and other dents. The defect 11 is different from the through hole 12, and in this embodiment, the defect 11 appears on the front surface 100A. However, the shape is not limited to this, and the defect may be, for example, a crack that reaches the rear surface 100B from the front surface 100A on the opposite side. That is, the defect may be exposed on the front surface 100A or the rear surface 100B, or may not be exposed. A defect that is not exposed can be detected, for example, by non-destructive testing. From the viewpoint of ease of detection by visual inspection, the defect may be exposed on the front surface 100A and / or the rear surface 100B of the ceramic substrate 100.
[0031] 1, 2, and 3 show an example in which the division lines L1 and L2 are formed only on one side, the front surface 100A, of the ceramic substrate 100, but the present invention is not limited thereto. That is, the division lines L1 and L2 may also be formed on the back surface 100B opposite to the front surface 100A of the ceramic substrate 100. In addition, the defect portion 11 and the division lines L1 and L2 do not need to coexist on the front surface 100A. For example, the defect portion 11 may be exposed only on the back surface 100B, or may be present inside the ceramic substrate 100.
[0032] In this embodiment, among the multiple partitions 10, only the partition 10a has the defect 11 and the through hole 12, but this is not limited thereto. In some modified examples, the ceramic substrate may have two or more partitions having a defect and a through hole. In addition, it is not necessary to provide a through hole in all partitions having a defect, and for example, a through hole may be provided only in partitions having a defect that is visually detected on the front surface 100A and the back surface 100B.
[0033] Since the ceramic substrate 100 has the defective portion 11 and the through hole 12 in the partition portion 10a, the partition portion 10a having the defective portion 11 can be detected with high accuracy even after processing into a circuit board. Therefore, the partition portion 10a having the defective portion 11 can be removed with high accuracy. Therefore, even if the ceramic substrate 100 having the defective portion 11 is used for manufacturing a circuit board, the occurrence of defective products is suppressed, and a circuit board having high reliability can be obtained. In this way, the ceramic substrate 100 can be used for manufacturing a circuit board despite having a defective portion, so that a circuit board having high reliability can be manufactured with a high yield. In other words, the ceramic substrate 100 makes it possible to manufacture a circuit board having high reliability with a high yield.
[0034] FIG. 4 is a perspective view of a composite substrate according to an embodiment. The composite substrate 200 includes a pair of metal substrates 110 arranged to face each other, and a ceramic substrate 100 between the pair of metal substrates 110. An example of the metal substrate 110 is a copper plate. The ceramic substrate 100 and the metal substrate 110 may have the same shape and size or may have different shapes and sizes. The metal substrate 110 and the ceramic substrate 100 may be joined by, for example, a brazing material. Since the composite substrate 200 includes the ceramic substrate 100, it is possible to manufacture a highly reliable circuit substrate with a high yield.
[0035] An example of composite substrate 200 is one in which ceramic substrate 100 is made of aluminum nitride and metal substrate 110 is made of aluminum.
[0036] 5 is a perspective view of a circuit board according to one embodiment. The circuit board 300 includes a ceramic substrate 100 and conductors 20 arranged to face each other with the ceramic substrate 100 in between. The conductors 20 are provided on the front surface 100A and the back surface 100B independently for each partition 10. That is, a pair of conductors 20 arranged to face each other is provided for each partition 10. The defect portions 11 and the through holes 12 of the ceramic substrate 100 may be covered with the conductors 20.
[0037] Since the partitions 10a having the defects 11 are provided with the through holes 12, the partitions 10a can be detected with high accuracy even if the defects 11 are minute. After dividing the circuit board 300 into divided boards for each partition 10, the divided boards including the defects 11 can be removed to obtain divided boards that do not include the defects 11. In this way, the ceramic substrate 100 having the defects 11 can be used to manufacture the circuit board, and high reliability can be ensured. Therefore, the highly reliable circuit boards can be obtained with a high yield.
[0038] An example of the circuit board 300 is one in which the ceramic substrate 100 is made of aluminum nitride and the conductor portion 20 is made of aluminum.
[0039] As a method for manufacturing a ceramic substrate according to one embodiment, a method for manufacturing a ceramic substrate 100 will be described. The method for manufacturing the ceramic substrate 100 includes a step of irradiating a surface of a base material made of ceramic with a laser beam to form partition lines L1, L2 that partition the surface into a plurality of sections, and a step of providing a through hole 12 in a partition portion 10a having a defect portion 11 among partition portions 10 defined by the partition lines L1, L2 to obtain the ceramic substrate 100.
[0040] As the substrate made of ceramics, a flat ceramic substrate having an outer shape as shown in Fig. 1 is used. There is no particular limitation on the type of ceramic, and examples thereof include carbides, oxides, and nitrides. Specific examples include silicon carbide, alumina, silicon nitride, aluminum nitride, and boron nitride.
[0041] Examples of the laser light irradiated onto the surface of the base material include a carbon dioxide laser and a YAG laser. By intermittently irradiating the laser light from such a laser source, scribe lines that become the division lines L1 and L2 are formed. The division lines L1 and L2 become cutting lines when dividing the circuit board 300 in a later process.
[0042] Next, among the partitions 10 defined by the partition lines L1 and L2, a through hole 12 is provided in the partition 10a having the defect 11. The through hole 12 is formed using a laser, a drill, or the like. The size and shape of the through hole 12 are as described above. The defect 11 in the ceramic substrate 100 may be detected visually or by non-destructive testing such as ultrasonic flaw detection and infrared testing. If the defect 11 is not detected, the through hole 12 does not need to be provided. In this manner, the ceramic substrate 100 shown in Figures 1, 2, and 3 is obtained.
[0043] The manufacturing method of the composite substrate according to one embodiment uses the above-mentioned ceramic substrate 100. That is, this manufacturing method includes a step of stacking a pair of metal substrates 110 so as to sandwich the ceramic substrate 100 to obtain the composite substrate. The metal substrate 110 may have a flat plate shape similar to the ceramic substrate 100. The pair of metal substrates 110 are bonded to the front surface 100A and the back surface 100B of the ceramic substrate 100, respectively, via a brazing material.
[0044] Specifically, first, a paste-like brazing material is applied to the front surface 100A and the back surface 100B of the ceramic substrate 100 by a method such as a roll coater method, a screen printing method, or a transfer method. The brazing material contains, for example, metal components such as silver and titanium, an organic solvent, and a binder. The viscosity of the brazing material may be, for example, 5 to 20 Pa·s. The content of the organic solvent in the brazing material may be, for example, 5 to 25 mass %, and the content of the binder may be, for example, 2 to 15 mass %.
[0045] FIG. 6 is a perspective view showing a ceramic substrate 100 coated with a brazing material 40. Although FIG. 6 shows only the front surface 100A side, the brazing material 40 may be similarly coated on the back surface 100B side. A metal substrate 110 is bonded to the front surface 100A and the back surface 100B of the ceramic substrate 100 coated with the brazing material 40 in this manner to obtain a bonded body. Thereafter, the bonded body is heated in a heating furnace to sufficiently bond the ceramic substrate 100 and the metal substrate 110 to obtain a composite substrate 200 shown in FIG. 4. The heating temperature may be, for example, 700 to 900° C. The atmosphere in the furnace may be an inert gas such as nitrogen. The bonded body may be heated under reduced pressure below atmospheric pressure or under vacuum. The heating furnace may be a continuous type in which a plurality of bonded bodies are continuously supplied and heated, or may be a type in which one or a plurality of bonded bodies are heated in a batch manner. The bonded body may be heated while pressing the bonded body in the stacking direction.
[0046] In the method for manufacturing a circuit board according to an embodiment, following the above-mentioned method for manufacturing a composite substrate, a step is performed in which a part of the metal substrate 110 in the composite substrate 200 is removed to form an independent conductor portion 20 for each partition portion 10. This step may be performed by, for example, photolithography. Specifically, first, as shown in FIG. 7, a photosensitive resist is printed on the surface 200A of the composite substrate 200. Then, an exposure device is used to form a resist pattern having a predetermined shape. The resist may be negative or positive. Uncured resist is removed by, for example, washing.
[0047] Fig. 7 is a perspective view showing a composite substrate 200 having a resist pattern 30 formed on a front surface 200A. Although Fig. 7 shows only the front surface 200A side, a similar resist pattern is also formed on the back surface 200B side. The resist pattern 30 is formed in regions on the front surface 200A and the back surface 200B that correspond to each partition portion 10 of the ceramic substrate 100.
[0048] After forming the resist pattern 30, the portions of the metal substrate 110 that are not covered by the resist pattern 30 are removed by etching. This exposes the front surface 100A and the back surface 100B of the ceramic substrate 100 in the portions. Thereafter, the resist pattern 30 is removed to form an independent conductor portion 20 for each partition portion 10. The conductor portions 20 are formed in pairs for each partition portion 10, sandwiching the ceramic substrate 100 therebetween, as shown in FIG. 5.
[0049] Through the above steps, a circuit board 300 as shown in Fig. 5 is obtained. Next, a step (inspection step) of applying a voltage between the pair of conductors 20 sandwiching the ceramic substrate 100 and measuring the current is performed. Specifically, a voltage is applied between the pair of conductors 20 sandwiching the ceramic substrate 100 and the current is measured. This measurement may be performed for each partition 10. As a result, the partitions 10a having the defective parts 11 and the through holes 12 are detected.
[0050] FIG. 8 is a diagram showing a schematic diagram of an example of an inspection device that measures leakage current of a circuit board 300 to inspect for dielectric breakdown. The inspection device 400 includes an AC power source 60 and a voltage endurance tester 50 connected to the AC power source 60. One terminal of the voltage endurance tester 50 is electrically connected to a conductive support 72a that contacts one of a pair of conductors 20 formed in the partition 10. The other terminal of the voltage endurance tester 50 is electrically connected to a conductive support 72b that contacts the other of the pair of conductors 20 through an electrode 70 disposed in an insulating solvent tank 77 that stores a solvent 76. That is, the pair of conductors 20 that face each other across the ceramic substrate 100 in the partition 10 where the current is measured are in contact with the conductive support 72a and the conductive support 72b, respectively.
[0051] The electrode 70 is disposed along the bottom surface and one side surface of the insulating solvent tank 77. As shown in FIG. 8, the electrode 70 has an L-shape when viewed in vertical cross section. Two insulating supports 74 are provided adjacent to the conductive support 72b on the electrode 70. The two insulating supports 74 are in contact with two conductors 20 disposed adjacent to the conductor 20 electrically connected to the conductive support 72b, respectively, and support the circuit board 300 in the solvent 76.
[0052] The electrode 70 and the conductive support parts 72a, 72b may be made of, for example, oxygen-free copper. The solvent 76 may be, for example, a fluorine-based inert liquid. The voltage endurance tester 50 may be a commercially available one. The positions of the insulating support part 74 and the conductive support part 72b are configured to be interchangeable depending on the position of the partition part 10 to be measured. The position of the conductive support part 72a is also configured to be movable in accordance with the position of the conductive support part 72b. By using such an inspection device 400, a voltage can be applied to a pair of conductor parts 20 for each partition part 10 to measure the leakage current.
[0053] The inspection device 400 applies a voltage of, for example, 1500 to 6000 V between a pair of conductors 20 sandwiching the ceramic substrate 100, and a withstand voltage tester 50 measures the presence or absence of leakage current. Since the partition 10a having the defect 11 has the through hole 12, leakage current occurs even at a low voltage. Therefore, the partition 10a can be detected with high accuracy by an inspection method that detects the presence or absence of leakage current at a predetermined voltage.
[0054] Using such an inspection device 400, an inspection method can be performed that includes a step of applying a voltage between a pair of conductors 20 that sandwich the ceramic substrate 100 and measuring a current for each partition 10. The inspection device is not limited to the configuration shown in Fig. 8, and any inspection device can be used without particular limitations as long as it is capable of measuring a current flowing between a pair of conductors that are arranged opposite to each other in at least one partition when a voltage is applied between the conductors.
[0055] The inspection device 400 is not limited to inspection of the circuit board 300 including the ceramic substrate 100 having the through hole 12 formed therein, but can be used to inspect various circuit boards including independent conductors for each partition. An inspection method using such an inspection device 400 can easily detect partitions having defects included in a ceramic substrate with high accuracy. This can improve the reliability and productivity of the circuit board 300.
[0056] The inspected circuit board 300 is cut along the dividing lines L1, L2 and divided into a plurality of divided boards. If the divided boards having through holes are eliminated and the divided boards having no through holes are manufactured or semi-manufactured as components to be used in, for example, a power module, it is possible to avoid using the divided boards having defects as components and to increase the reliability of the components. For example, electronic components are mounted on the conductor portions 20 of the divided boards.
[0057] Although several embodiments of the present disclosure have been described above, the present disclosure is not limited to the above-mentioned embodiments. For example, the shapes of the conductors 20 provided in each partition 10 do not need to be the same, and each partition 10 may have a different shape. Also, for example, the voltage application to the conductors 20 that are paired with the ceramic substrate 100 and that are sandwiched between them and the current measurement may be performed simultaneously for multiple pairs, rather than performing the measurement for each pair.
[0058] Any surface treatment may be applied to the conductor portion 20 in the circuit board 300. For example, a part of the surface of the conductor portion 20 may be covered with a protective layer such as a solder resist, and the other part of the surface of the conductor portion 20 may be plated. Such surface treatment may be performed before or after the inspection using the inspection device 400. EXAMPLES
[0059] (Experimental Examples 1 to 3) A laser beam was irradiated onto the surface of a silicon nitride ceramic substrate to form partition lines, and the substrate was divided into three sections along the vertical and horizontal directions. Thus, a ceramic substrate having a total of nine partitions was prepared. This ceramic substrate had an outer periphery with a width of 5 mm outside the nine partitions. The size of each partition was length x width x thickness = 41 mm x 41 mm x 0.32 mm. A through hole was formed in the partition in the center of the ceramic substrate using a fiber laser (wavelength: 1064 nm). By changing the area to be irradiated with the laser beam, five ceramic substrates each having through holes of different sizes were produced. The opening shape of the through hole on the front and back surfaces of each ceramic substrate was circular, and the size (diameter) was as shown in Table 1. FIG. 9 is a photograph of an optical microscope image showing the surface and through hole of the ceramic substrate of Experimental Example 3.
[0060] A brazing filler metal containing Ag as a main component was applied to the front and back surfaces of the ceramic substrate by screen printing. The copper plate and the ceramic substrate were laminated so that each ceramic substrate was sandwiched between two copper plates (thickness 0.8 mm). In this way, a joint body including a copper plate, a ceramic substrate, and a copper plate in this order was produced.
[0061] Five sets of bonded bodies were stacked in a vacuum bonding furnace to form a laminate. A copper plate was placed on top of the laminate, and a pressure of 5 g / cm was applied. 2 The copper plate and the ceramic substrate were then heated at 810°C for 20 minutes while applying pressure at 100°C to bond the copper plate and the ceramic substrate together. -3 The substrate was heated under a reduced pressure of less than 1 Pa. In this manner, a composite substrate was prepared which included a pair of copper plates and a ceramic substrate therebetween.
[0062] Using an inspection device as shown in FIG. 8, a withstand voltage test was performed on each composite substrate manufactured in accordance with JIS C2110-1:2010 (n=5). For this test, an AC20kV withstand voltage tester (model: 7473) manufactured by Keisoku Gijutsu Kenkyusho Co., Ltd. was used. Perfluorocarbon (manufactured by 3M Japan Ltd., product name: Fluorinert, model number: FC-3283) was used as the solvent. Inspection jigs manufactured by Onishi Electronics Co., Ltd. were used as the insulating solvent tank 77, the electrode 70, the conductive support parts 72a and 72b, and the insulating support part 74. The electrode 70 was made of oxygen-free copper, and the conductive support parts 72a and 72b were made of carbon tool steel material (SK material) plated with rhodium.
[0063] With the composite board set in the inspection device, the voltage was increased to 4.2 kV at a rate of 0.12 kV / sec. The contact current threshold was set to 9.99 mA, and a current above this threshold was judged to have been a dielectric breakdown. The voltage at which a dielectric breakdown was judged to have occurred is shown in the "Voltage Withstand Test Results" column in Table 1.
[0064] [Table 1]
[0065] The through-hole in Experimental Example 1 had a cylindrical shape. On the other hand, the through-holes in Experimental Examples 2 and 3 had a tapered portion inside the ceramic substrate, the hole diameter of which changed along the thickness direction of the ceramic substrate. In Table 1, "<0 kV" indicates that the leakage current value reached or exceeded the above-mentioned predetermined value immediately after the start of voltage application. In Experimental Example 1 No. 3, the ceramic substrate experienced dielectric breakdown at the voltage listed in Table 1. In all of the experimental examples, the leakage current value reached or exceeded the above-mentioned predetermined value before the voltage reached 4.2 kV. From these results, it was confirmed that by forming a through-hole, a substrate (partition portion) having a defect can be detected with high accuracy. [Industrial Applicability]
[0066] According to the present disclosure, a ceramic substrate capable of obtaining a highly reliable circuit board and a manufacturing method thereof are provided. Also, a composite substrate capable of obtaining a highly reliable circuit board is provided. Also, a highly reliable circuit board and a manufacturing method thereof are provided. Also, a circuit board inspection method capable of improving the reliability of the circuit board is provided. [Explanation of symbols]
[0067] 10,10a...partition portion, 11...defective portion, 12...through hole, 20...conductor portion, 30...resist pattern, 50...voltage resistance tester, 60...AC power source, 70...electrode, 72a,72b...conductive support portion, 74...insulating support portion, 76...solvent, 77...insulating solvent tank, 100...ceramic substrate, 110...metal substrate, 100A...surface, 100B...rear surface, 110...metal substrate, 200...composite substrate, 200A...surface, 200B...rear surface, 300...circuit substrate, 400...inspection device.
Claims
1. A ceramic substrate having a surface divided into a plurality of sections by dividing lines; and conductor portions arranged to face each other across the ceramic substrate, the ceramic substrate has a through hole covered by the conductor portion only in at least one partition portion having a defect portion among a plurality of partition portions defined by the partition lines; The conductor portion is a circuit board provided independently for each of the partition portions.
2. The circuit board according to claim 1, wherein the opening area of the through hole on the surface is 1200 μm 2 or more.
3. A circuit board as described in claim 1 or 2, wherein at least a portion of the through hole is formed in a tapered shape.
4. A circuit board described in any one of claims 1 to 3, wherein at least a portion of the through hole is filled with solder material.
5. A circuit board described in any one of claims 1 to 4, having through holes in all partitions having the defective portion.
6. A process of irradiating a surface of a substrate made of ceramics with laser light to form partition lines that partition the surface into a plurality of sections; providing a through hole only in at least one of the partitions, which has a defect in the base material made of the ceramic, among the plurality of partitions defined by the partition lines, to obtain a ceramic substrate; laminating a pair of metal substrates so as to sandwich the ceramic substrate therebetween to obtain a composite substrate; removing a portion of the metal substrate in the composite substrate to form an independent conductor portion for each partition portion; and applying a voltage between the pair of conductors that sandwich the ceramic substrate and measuring a current.
7. A step of irradiating a surface of a substrate made of ceramic with laser light to form partition lines that partition the surface into a plurality of sections; providing a through hole in at least one of the partitions defined by the partition lines, the through hole having a defect, to obtain a ceramic substrate; laminating a pair of metal substrates so as to sandwich the ceramic substrate therebetween to obtain a composite substrate; removing a portion of the metal substrate in the composite substrate to form an independent conductor portion for each partition portion; and applying a voltage between the pair of conductors that sandwich the ceramic substrate and measuring a current.
8. The method for inspecting a circuit board according to any one of claims 1 to 5, The method for inspecting a circuit board includes a step of applying a voltage between at least a pair of the conductor portions sandwiching the ceramic substrate therebetween and measuring a current.
Citation Information
Patent Citations
Method for detecting defect of electronic component module
JP2001358432A
Substrate inspection method, inspection device therefor and method for manufacturing product for electronic machinery
JP2003014654A
Method and device for detecting defect in through hole
JP2005337900A
Method for manufacturing nitride ceramics circuit board
JP2007324301A
Wiring circuit board aggregate sheet and method for manufacturing the same
JP2011176075A