COATINGS, ARTICLES, AND METHODS FOR PROTECTING CERAMIC SUBSTRATES - Patent application

A composite coating system with a bond coat, top coat, and intermediate layer addresses the challenges of high-temperature, corrosive, and oxidizing conditions in gas turbine engines by forming stable silicates, improving oxidative stability and mechanical integrity.

JP7591084B2Active Publication Date: 2024-11-27RTX CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023059893
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-04-01
Filing Date
2023-04-03
Publication Date
2024-11-27
Estimated Expiration
2043-04-03

AI Technical Summary

Technical Problem

Gas turbine engine components face challenges due to exposure to high temperatures, corrosive and oxidizing conditions, and high stress levels, necessitating improved thermal and oxidative stability.

Method used

A composite coating system comprising a bond coat with gettering and diffusing particles, a top coat, and an intermediate layer with non-silicate oxide particles dispersed in a matrix, which reacts with oxidants to form protective silicates, mitigating the formation of undesirable oxide phases and enhancing mechanical integrity.

Benefits of technology

The coating system effectively protects underlying substrates by limiting oxygen and moisture exposure, improving oxidative stability and mechanical integrity through the formation of stable silicates, thereby enhancing the durability and performance of gas turbine engine components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007591084000001
    Figure 0007591084000001
  • Figure 0007591084000002
    Figure 0007591084000002
Patent Text Reader

Abstract

To provide an environmental barrier coating.SOLUTION: A coating according to an exemplary embodiment of this disclosure, among other possible things, includes a bond coat including gettering particles and diffusive particles dispersed in a matrix, a top coat disposed over the bond coat, and an intermediate layer between the bond coat and the top coat. The intermediate layer includes non-silicate oxide particles dispersed in a matrix. An article and a method of protecting a ceramic-based substrate are also disclosed.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to environmental barrier coatings. [Background technology]

[0002] A gas turbine engine typically includes a fan section, a compressor section, a combustor section, and a turbine section. Air entering the compressor section is compressed and delivered to the combustor section where it is mixed with fuel and ignited to generate a high energy exhaust gas stream. The high energy exhaust gas stream expands through the turbine section to drive the compressor section and the fan section. The compressor section typically includes low and high pressure compressors, and the turbine section includes low and high pressure turbines. Summary of the Invention [Problem to be solved by the invention]

[0003] The present disclosure relates to composite articles, such as those used in gas turbine engines. Components, such as gas turbine engine components, may be exposed to high temperatures, corrosive and oxidative conditions, and high stress levels. To improve thermal and / or oxidative stability, the components may include a protective barrier coating. [Means for solving the problem]

[0004] A coating according to an exemplary embodiment of the present disclosure includes, among other possibilities, a bond coat including gettering and diffusing particles dispersed in a matrix, a top coat disposed on the bond coat, and an intermediate layer between the bond coat and the top coat, the intermediate layer including non-silicate oxide particles dispersed in a matrix.

[0005] In a further example of the foregoing, the matrix of the intermediate layer is the same as the matrix of the bond coat.

[0006] In further examples of any of the foregoing, the non-silicate oxide particles comprise about 25 to about 50 volume percent of the intermediate layer.

[0007] In a further example of any of the foregoing, the non-silicate oxide particles have an average diameter between about 10 and about 25 microns (about 0.5 and about 1 mil).

[0008] In a further example of any of the foregoing, the non-silicate oxide particles have an average diameter that is about the same as an average diameter of the gettering particles.

[0009] In a further example of any of the foregoing, the non-silicate oxide particles are hafnium dioxide particles.

[0010] In a further example of any of the foregoing, the topcoat includes hafnium silicate.

[0011] In a further example of any of the foregoing, the gettering particles include molybdenum disilicide particles.

[0012] In further examples of any of the foregoing, the gettering particles further include silicon carbide particles and silicon oxycarbide particles.

[0013] In a further example of any of the foregoing, the intermediate layer includes particles of the topcoat material.

[0014] In a further example of any of the foregoing, the intermediate layer includes a region of diffusing particle material.

[0015] An article according to an exemplary embodiment of the present disclosure includes, among other possibilities, a ceramic-based substrate and a coating disposed on the ceramic-based substrate, the coating including a bond coat including gettering particles and diffusing particles dispersed in a matrix, a top coat disposed on the bond coat, and an intermediate layer between the bond coat and the top coat, the intermediate layer including non-silicate oxide particles dispersed in a matrix.

[0016] In a further example of the foregoing, the intermediate layer comprises a silicate reaction product.

[0017] In a further example of any of the foregoing, the silicate reaction product is the same material as the topcoat.

[0018] In a further example of any of the foregoing, the intermediate layer includes a region of diffusing particle material.

[0019] In a further example of any of the foregoing, the non-silicate oxide particles are hafnium dioxide and the topcoat and the silicate reaction product are hafnium silicate.

[0020] In a further example of any of the foregoing, the gettering particles include molybdenum disilicide particles.

[0021] A method of protecting a ceramic-based substrate according to an exemplary embodiment of the present disclosure includes, among other possibilities, a bond coat including gettering particles and diffusing particles dispersed in a matrix, a top coat disposed on the bond coat, and an intermediate layer between the bond coat and the top coat. The intermediate layer includes silicate oxide particles dispersed in a matrix. The gettering particles react with an oxidant to form oxidation products. The non-silicate oxide particles react with the oxidation products to form silicates in the intermediate layer.

[0022] In a further example of the foregoing, the non-silicate oxide particles are hafnium dioxide and the silicate is hafnium silicate.

[0023] In a further example of any of the foregoing, the gettering particles include molybdenum disilicide particles. [Brief description of the drawings]

[0024] [Figure 1] 1 is a schematic diagram of an exemplary gas turbine engine. [Diagram 2] 2 illustrates the gas turbine engine article of claim 1 having a coating. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0025] FIG. 1 illustrates a schematic of a gas turbine engine 20. The gas turbine engine 20 is disclosed herein generally as a two-spool turbofan incorporating a fan section 22, a compressor section 24, a combustor section 26, and a turbine section 28. The fan section 22 drives air along a bypass flowpath B in a bypass duct defined in a housing 15, such as a fan case or nacelle, and drives air along a core flowpath C for compression and communication to the combustor section 26 and then expansion through the turbine section 28. Although shown in the disclosed non-limiting embodiment as a two-spool turbofan gas turbine engine, it should be understood that the concepts described herein are not limited to use with a two-spool turbofan, as the present teachings may also be applied to other types of turbine engines, including three-spool configurations.

[0026] The exemplary engine 20 generally includes a low speed spool 30 and a high speed spool 32 mounted for rotation about a central longitudinal axis A of the engine relative to an engine static structure 36 via a number of bearing systems 38. It will be appreciated that different bearing systems 38 may alternatively or additionally be provided at different locations and the locations of the bearing systems 38 may vary as appropriate depending on the application.

[0027] The low speed spool 30 generally includes an inner shaft 40 that interconnects a first (or low pressure) compressor 44 and a first (or low pressure) turbine 46. The inner shaft 40 is connected to the fan 42 via a speed change mechanism, shown in the exemplary gas turbine engine 20 as a gear arrangement 48, for driving the fan 42 at a lower speed than the low speed spool 30. The high speed spool 32 includes an outer shaft 50 that interconnects a second (or high pressure) compressor 52 and a second (or high pressure) turbine 54. A combustor 56 is disposed in the exemplary gas turbine 20 between the high pressure compressor 52 and the high pressure turbine 54. A mid-turbine frame 57 of the engine static structure 36 may generally be disposed between the high pressure turbine 54 and the low pressure turbine 46. The mid-turbine frame 57 further supports a bearing system 38 within the turbine section 28. The inner shaft 40 and the outer shaft 50 are concentric and rotate about a central longitudinal axis A of the engine, collinear with its longitudinal axis, via the bearing system 38.

[0028] The core airflow is compressed by the low pressure compressor 44, then the high pressure compressor 52, mixed with fuel and combusted in the combustor 56, and then expanded through the high pressure turbine 54 and the low pressure turbine 46. A mid-turbine frame 57 includes an airfoil 59 located within the core airflowpath C. The turbines 46, 54 rotate the respective low speed spool 30 and high speed spool 32 in response to the expansion. It will be appreciated that the locations of each of the fan section 22, compressor section 24, combustor section 26, turbine section 28, and fan drive gear system 48 may be varied. For example, the gear system 48 may be located aft of the low pressure compressor, or aft of the combustor section 26, or even aft of the turbine section 28, and the fan 42 may be located forward or aft of the location of the gear system 48.

[0029] In one example, the engine 20 is a high bypass gear aircraft engine. In a further example, the bypass ratio of the engine 20 can be greater than about 6, and in an exemplary embodiment, greater than about 10, and can be less than or equal to about 18.0, or more specifically, less than or equal to 16.0. The gear structure 48 is a planetary gear train, such as a planetary gear system or other gear system, having a gear reduction ratio greater than about 2.3. The gear reduction ratio can be less than or equal to 4.0. The low pressure turbine 46 has a pressure ratio greater than about 5. The low pressure turbine pressure ratio can be less than or equal to 13.0, or more specifically, less than or equal to 12.0. In one disclosed embodiment, the bypass ratio of the engine 20 is greater than about 10 (10:1), the diameter of the fan is significantly larger than the diameter of the low pressure compressor 44, and the pressure ratio of the low pressure turbine 46 is greater than about 5 (5:1). The pressure ratio of the low pressure turbine 46 is the pressure measured in front of the inlet of the low pressure turbine 46 relative to the pressure at the outlet of the low pressure turbine 46 in front of the exhaust nozzle. The gear structure 48 may be a planetary gear train, such as an epicyclic gear system or other gear system having a gear reduction ratio greater than about 2.3:1 and less than about 5:1. However, it should be understood that the above parameters are merely exemplary of one embodiment of a gear structure engine, and that the present invention is applicable to other gas turbine engines, including direct drive turbofans.

[0030] Due to the high bypass ratio, a significant amount of thrust is provided by the bypass flow B. The fan section 22 of the engine 20 is designed to cruise at certain flight conditions, typically at about Mach 0.8 and about 35,000 feet (10,668 meters). At flight conditions of Mach 0.8 and 35,000 feet (10,668 meters), when the engine is at its highest fuel consumption (also referred to as "bucket cruise thrust specific fuel consumption ('TSFC')"), is the industry standard parameter of lbm of fuel burned divided by the lbf of thrust the engine produces at its minimum point. The engine parameters described above and in this paragraph are measured at this condition unless otherwise specified. The "low fan pressure ratio" is the overall pressure ratio of the fan blades alone without the use of a fan exit guide vane ("FEGV") system. According to one non-limiting embodiment, the low fan pressure ratio disclosed herein is less than about 1.45, or more specifically, greater than or equal to 1.25. "Low corrected fan tip speed" is the speed at the actual fan tip divided by an industry standard temperature correction value of [(Tram°R) / (518.7°R)]0.5. According to one non-limiting embodiment, the "low corrected fan tip speed" disclosed herein is less than about 1150.0 ft / sec (350.5 m / sec) and may be greater than or equal to 1000.0 ft / sec (304.8 m / sec).

[0031] 2 illustrates a schematic representation of a representative portion of an exemplary article 100 for a gas turbine engine 20, including a composite bond coat 102 that functions as a barrier layer. The article 100 may be, for example, an airfoil such as a blade or vane in the compressor section 24 or turbine section 28, a combustor liner panel in the combustor section 26, a blade outer air seal, or other components that would benefit from the examples herein. In this example, the bond coat 102 is used as an environmental barrier layer to protect an underlying substrate 104 from environmental and thermal conditions. As will be appreciated, the bond coat 102 may be used as a standalone barrier layer, as an outermost / topcoat with additional underlayers, or in combination with other coating underlayers or overlayers, such as, but not limited to, ceramic-based topcoats.

[0032] The bond coat 102 includes a matrix 106, a dispersion of "gettering" particles 108, and a dispersion of diffusing particles 110. In one example, the matrix 106 may be silicon dioxide (SiO2). In one example, the gettering particles 108 are silicon oxycarbide particles (SiOC) or molybdenum disilicide (MoSi2) particles 108, although other examples are contemplated. The gettering particles 108 may be, for example, molybdenum disilicide particles, other silicides, silicon oxycarbide particles, silicon carbide (SiC) particles, silicon nitride (Si3N4) particles, silicon oxycarbonitride (SiOCN) particles, silicon aluminum oxynitride (SiAlON) particles, silicon boron oxycarbonitride (SiBOCN) particles, or combinations thereof. The diffusing particles 110 can be, for example, barium magnesium aluminosilicate (BMAS) particles, barium strontium aluminum silicate particles, magnesium silicate particles, calcium aluminosilicate particles (CAS), alkaline earth aluminum silicate particles, yttrium aluminum silicate particles, ytterbium aluminum silicate particles, other rare earth metal aluminum silicate particles, borosilicate particles, or combinations thereof.

[0033] In a particular example, the gettering particles 108 include a combination of silicon carbide particles, silicon oxycarbide particles, and molybdenum disilicide particles, in this example, the bond coat 102 includes at least about 50% by volume of silicon carbide and silicon oxycarbide together prior to oxidation of the gettering particles.

[0034] The bond coat 102 protects the underlying substrate 104 from oxygen and moisture. For example, the substrate 104 can be a ceramic-based substrate, such as a silicon-containing ceramic material. One example is silicon carbide. Another non-limiting example is silicon carbide fibers in a silicon carbide matrix. The gettering particles 108 and the diffusing particles 110 act as oxygen and moisture diffusion barriers that limit exposure of the underlying substrate 104 to oxygen and / or moisture from the surrounding environment. Without being bound to a particular theory, the diffusing particles 110, such as the BMAS particles 110, enhance oxidation and moisture protection by diffusing to the outer surface of the barrier layer opposite the substrate 104 and forming a sealing layer that seals the underlying substrate 104 from exposure to oxygen / moisture. Additionally, the cationic metal species of the diffusing particles 110 (e.g., BMAS particles, barium, magnesium, and aluminum) can diffuse into the gettering particles 108 to enhance the oxidation stability of the gettering material. Additionally, the diffusion behavior of the diffusing particles 110 may act to seal any microcracks that may form in the barrier layer. Sealing the microcracks may prevent oxygen from penetrating the barrier layer, further improving the oxidation resistance of the barrier layer. The gettering particles 108 may react with oxidant species, such as oxygen and water, that may diffuse into the bond coat 102. In this manner, the gettering particles may reduce the likelihood of these oxidant species reaching and oxidizing the substrate 104.

[0035] The ceramic-based topcoat 114 is in contact with the bond coat 102. By way of example, the ceramic-based topcoat 114 can include one or more layers of an oxide-based material. The oxide-based material can be, for example, but is not limited to, a hafnium-based oxide or a yttrium-based oxide (such as hafnia, hafnium silicate, yttrium silicate, yttria-stabilized zirconia, or gadolinia-stabilized zirconia), or a combination thereof.

[0036] Together, the topcoat 114 and the bond coat 102 form a barrier coating 116 for the substrate 104 .

[0037] When the gettering particles 108 react with the oxidant in the protective mechanism described above, oxidation products of the gettering particles 108 accumulate in the bond coat 102. The reaction products accumulate primarily between the outermost surface of the bond coat 102 near the top coat 114. For example, the reaction products can be or include silicon dioxide. However, silicon dioxide can have an undesirable microstructure due in part to the high temperatures at which oxidation reactions occur during operation of, for example, a gas turbine engine 20 including the article 100. In certain instances, the silicon dioxide is in the cristobalite phase, which is relatively unstable and exhibits reduced mechanical properties compared to the matrix 106. The cristobalite phase forms in planar layers and is prone to cracking. Thus, accumulation of these oxidation products in the coating 116 can compromise the protective properties and mechanical integrity of the coating 116.

[0038] To mitigate the effects of the reaction products, an intermediate layer 118 is provided in the coating 116 between the top coat 114 and the bond coat 102. The intermediate layer 118 includes a matrix 106 loaded with non-silicate oxide particles 120, such as hafnium dioxide, zirconium dioxide, titanium dioxide, or other rare earth metal non-silicate oxides. The non-silicate oxide particles 120 consume the oxide reaction products from the oxidation of the gettering particles 108 described above by reacting with the silicon-containing oxide reaction products to form silicates. Thus, the non-silicate oxide particles 120 prevent the formation of large pockets of undesirable oxide phases as described above, minimizing the chance of cracking, thereby improving the effectiveness and integrity of the coating 116. Additionally, silicates have relatively low thermal conductivity and are generally crystalline, which may provide thermal protection and improve the mechanical stability of the coating 116.

[0039] The intermediate layer 118 has a thickness T1, and the bond coat 102 has a thickness T2. In some examples, the ratio of thickness T2 to T1 is at least about 3. In particular examples, the ratio is between about 3 and about 4. For example, thickness T1 is about 50 microns (2 mils) and thickness T2 is between about 150 and about 200 microns (about 6 and about 8 mils).

[0040] During the life of the article 100, various components of the topcoat 114 and / or bond coat 102 may diffuse into the coating 116. For example, material of the topcoat 114 may diffuse into the intermediate layer 118 and / or components of the coating 102 may diffuse into the intermediate layer 118. Thus, the intermediate layer 118 may include particles 122 of the topcoat 114 material. The intermediate layer 118 may also include amorphous regions 124 of the diffusing particle 110 material and / or borosilicate glass.

[0041] In other examples, the intermediate layer 118 can be formed to include particles of the topcoat 114 material and / or the diffusing particles 110 material.

[0042] In some particular examples, the silicate product of the reaction between the non-silicate oxide particles 120 and the reaction products of the oxidation of the gettering particles 108 is the same material as the material of the topcoat 114. For example, the topcoat 114 is hafnium silicate and the non-silicate oxide particles 120 are hafnium dioxide. The hafnium dioxide reacts with the silicon-containing reaction products of the oxidation of the gettering particles 108 to form hafnium silicate.

[0043] In general, the greater the surface area of ​​the non-silicate oxide particles 120, the more favorable the reactions involving the non-silicate oxide particles 120. Thus, the size of the non-silicate oxide particles 120 is selected to provide the desired reaction kinetics to consume the undesirable phases discussed above and improve the properties of the coating 116. The non-silicate oxide particles 120 may have an average diameter between about 10 and about 25 microns (about 0.5 and about 1 mil) in some examples. In some particular examples, the non-silicate oxide particles 120 have an average diameter that is approximately the same as the average diameter of the gettering particles 108 before the gettering particles 108 react with the oxidant.

[0044] The non-silicate oxide particles 120 may comprise about 25 to about 50 volume percent of the intermediate layer 118 before reacting with other components of the coating 116 as described above. The amount of non-silicate oxide particles 120 in the intermediate layer is balanced with the size of the non-silicate oxide particles 120 in consideration of the desired thermal and mechanical properties of the coating 116 as well as the desired reaction kinetics described above.

[0045] In a particular example, the gettering particles 108 include molybdenum disilicide particles. The non-silicate oxide particles 120 are hafnium dioxide particles. The topcoat 114 is hafnium silicate.

[0046] The coating 116 can be applied to the part 100 by any known method, such as a slurry-based method. For example, a slurry containing the bond coat 102 components can be applied to the part 100 and then cured or hardened by any known method, such as heat treatment. A similar slurry application and curing / hardening method can be repeated for the intermediate layer 118. The topcoat 114 can be applied by a similar method or other methods known in the art, such as spray coating.

[0047] The term "about" as used herein has its typical meaning in the art, however, in certain instances, "about" can mean up to a 10% deviation from the values ​​set forth herein.

[0048] Although different examples are described as having particular components, the examples of the disclosure are not limited to those particular combinations, and some of the components or features from any of the embodiments can be used in combination with features or components from any of the other embodiments.

[0049] The foregoing description should be interpreted as illustrative and not in any limiting sense. Those skilled in the art will appreciate that certain modifications may fall within the scope of the present disclosure. For these reasons, the following claims should be studied to determine the true scope and content of the present disclosure.

Claims

1. a bond coat including gettering particles and diffusing particles dispersed in a matrix; a topcoat disposed on the bond coat; an intermediate layer between the bond coat and the top coat, the intermediate layer comprising non-silicate oxide particles dispersed in a matrix; Equipped with the non-silicate oxide particles include at least one of hafnium dioxide particles, zirconium dioxide particles, or titanium dioxide particles; the topcoat comprises hafnium silicate; the gettering particles include molybdenum disilicide particles; The coating, wherein the gettering particles further comprise silicon carbide particles and silicon oxycarbide particles.

2. The coating of claim 1 , wherein the matrix of the intermediate layer is the same as the matrix of the bond coat.

3. The coating of claim 1 , wherein the non-silicate oxide particles comprise 25-50 volume percent of the intermediate layer.

4. The coating of claim 1, wherein the non-silicate oxide particles have an average diameter of 10 to 25 microns (0.5 to 1 mil).

5. The coating of claim 1 , wherein the non-silicate oxide particles have an average diameter about the same as an average diameter of the gettering particles.

6. The coating of claim 1 , wherein the intermediate layer comprises particles of the material of the topcoat.

7. The coating of claim 1 , wherein the intermediate layer comprises a region of the material of the diffusing particles.

8. A ceramic base material; A coating disposed on the ceramic-based substrate, a bond coat including gettering particles and diffusing particles dispersed in a matrix; a topcoat disposed on the bond coat; an intermediate layer between the bond coat and the top coat, the intermediate layer comprising non-silicate oxide particles dispersed in a matrix; the coating comprising: Equipped with the non-silicate oxide particles include at least one of hafnium dioxide particles, zirconium dioxide particles, or titanium dioxide particles; the topcoat comprises hafnium silicate; the gettering particles include molybdenum disilicide particles; The article, wherein the gettering particles further comprise silicon carbide particles and silicon oxycarbide particles.

9. The article of claim 8 , wherein the intermediate layer comprises a silicate reaction product.

10. The article of claim 9 , wherein the silicate reaction product is the same material as the topcoat.

11. The article of claim 9 , wherein the intermediate layer comprises a region of the diffusing particle material.

12. 10. The article of claim 9, wherein said non-silicate oxide particles are hafnium dioxide and said topcoat and said silicate reaction product are hafnium silicate.

13. The article of claim 8 , wherein the gettering particles comprise molybdenum disilicide particles.

14. 1. A method for protecting a ceramic substrate, comprising: providing a coating on the ceramic-based substrate, a bond coat including gettering particles and diffusing particles dispersed in a matrix; a topcoat disposed on the bond coat; an intermediate layer between the bond coat and the top coat, the intermediate layer comprising non-silicate oxide particles dispersed in a matrix; providing the coating comprising: Including, the non-silicate oxide particles include at least one of hafnium dioxide particles, zirconium dioxide particles, or titanium dioxide particles; the topcoat comprises hafnium silicate; the gettering particles include molybdenum disilicide particles; the gettering particles further include silicon carbide particles and silicon oxycarbide particles; the gettering particles react with an oxidant to form an oxidation product, and the non-silicate oxide particles react with the oxidation product to form a silicate in the intermediate layer. The method.

15. 15. The method of claim 14, wherein the non-silicate oxide particles are hafnium dioxide and the silicate is hafnium silicate.

16. The method of claim 14 , wherein the gettering particles comprise molybdenum disilicide particles.

Citation Information

Patent Citations

  • Environmentally resistant film material, film structure and ceramic structure using the same

    JP2005200226A

  • Article comprising substrate and top barrier layer and method of preparing it

    JP2005325014A

  • High-density protective coating, method for manufacturing the same and coated article

    JP2007229704A

  • Ebc with mullite bondcoat that includes oxygen getter phase

    JP2020100545A

  • Environmental barrier coating

    US20210246082A1