Spray greening materials and spray greening methods
A spray greening material with a specific soil erosion preventive agent and fibers forms a cohesive layer to resist runoff and erosion, ensuring effective plant growth and long-term erosion prevention.
Patent Information
- Application Number
- JP2024557080
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2023-06-12
- Filing Date
- 2024-01-17
- Publication Date
- 2024-12-09
- Estimated Expiration
- 2044-01-17
AI Technical Summary
Existing spray greening materials are prone to being washed away or eroded by heavy rainfall before plants can grow, leading to ineffective erosion prevention.
A spray greening material composed of a soil erosion preventive agent with a viscosity of 1000mPa·s ≤ η ≤ 3200mPa·s, mixed with fibers, adhesive, fertilizer, and seeds, forming a cohesive layer that enhances resistance to runoff and erosion without inhibiting plant growth.
The cohesive layer formed by the spray greening material provides improved resistance to runoff and erosion, allowing plants to grow and further strengthen the ground surface, reducing water flow and enhancing erosion prevention.
Smart Images

Figure 0007596007000001 
Figure 0007596007000002 
Figure 0007596007000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a spray greening material and a spray greening method for spraying greening onto ground surfaces such as slopes. [Background technology]
[0002] A spray greening method is known in which spray greening materials are sprayed onto the ground surface such as a slope to green the ground. For example, Patent Document 1 describes how the spray greening method involves spraying a slurry-like mixture of Kurapia cut seedlings, sterile one-year plants, soil dressing, soil erosion prevention material, adhesive, fertilizer, etc., mixed in a mixer, onto the ground surface with a soil dressing sprayer, which causes the sterile one-year plants to cover the ground surface early and form a green area, thereby preventing soil erosion.
[0003] Patent Document 1 also describes the use of, for example, a product name "Crycoat (registered trademark) C-710" containing a synthetic resin emulsion as a main component as a soil erosion inhibitor, and "Crycoat C-402" containing a water-soluble synthetic polymer as a main component as an adhesive, and the use of Kurapia 96 (g / m) as a blending amount per sprayed area of sprayed greening materials. 2 ), soil 12(g / m 2 ), soil erosion prevention material 24(g / m 2 ), adhesive 0.6(g / m 2 ), fertilizer 60 (g / m 2 ), sterile annual plant seeds 15~30 (g / m 2 ) is described as being suitable. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent Publication No. 2021-122265 Summary of the Invention [Problem to be solved by the invention]
[0005] As mentioned above, it is well known that greening is an effective way to prevent erosion. However, in recent years, rainfall caused by abnormal weather such as torrential rains and large typhoons can cause sprayed greening materials to be washed away or eroded before plants can grow. Therefore, an object of the present invention is to provide a spray-applied greening material and a spray-applied greening method which have improved resistance to runoff and erosion caused by rainfall even before plants grow. [Means for solving the problem]
[0006] The spray greening material of the present invention is a spray greening material that is a mixture of a soil erosion inhibitor, fiber, an adhesive, fertilizer, and seeds. The soil erosion inhibitor is mainly composed of a synthetic resin emulsion, has a viscosity η of 1000 mPa s < η ≦ 3200 mPa s, and is mixed in an amount of 1 m2 of spray area. 2 The fiber is mixed in an amount of 60 to 200g per m2 of spray area. 2 It is characterized in that the weight per serving is 80 to 170 g. In addition, in this specification, a numerical range expressed by "to" means a numerical range including the numerical values before and after "to" as the lower limit and upper limit.
[0007] Soil erosion inhibitors, whose main component is a synthetic resin emulsion and whose viscosity η is 1000mPa·s<η≦3200mPa·s, are originally intended to form a strong solidified layer on the bare surface of reclaimed land or developed land to prevent flying sand, dust, and erosion. The solidified layer formed by such soil erosion inhibitors has excellent strength and weather resistance, making it possible to prevent flying sand for a long period of time, but soil erosion inhibitors with a viscosity η of 1000mPa·s<η≦3200mPa·s cannot be used for spray greening because they harden the soil and inhibit plant growth.
[0008] Therefore, in the spray greening material of the present invention, fiber is mixed with the soil erosion prevention agent. Fiber is a fiber (pulp) extracted from wood or grass, and its main component is cellulose. Cellulose has the property of bonding together through hydrogen bonds, and when a soil erosion prevention agent with a viscosity η of 1000 mPa·s<η≦3200 mPa·s is sprayed over an area of 1 m 2Spray 60-200g of fiber onto a 1m2 surface area. 2 By mixing 80 to 170 g per unit, the consolidated layer formed by the soil erosion prevention agent is made more interconnected, and the soil is consolidated in a balanced manner without impeding plant growth.
[0009] The amount of soil erosion inhibitor to be mixed is preferably 80 g or more and 180 g or less, more preferably 160 g or less. 2 If the amount of soil erosion inhibitor is less than 60g per m2, the soil will become weak and some soil may wash away on flat surfaces. Also, there is a problem that runoff will occur more frequently on steep slopes (1:1.0). On the other hand, if the amount of soil erosion inhibitor mixed is more than 1 m2, the soil may become weaker and some soil may wash away on flat surfaces. 2 If the amount is more than 200g per seed, the seed layer may become too strong and may result in poor germination.
[0010] The amount of fiber blended is preferably 100 g or more, or 120 g or more and 160 g or less. 2 If the amount of fiber is less than 80g per m2, the connection to the cohesive layer will be insufficient, resulting in poor balance and poor germination. 2 Above 170g per unit, the balance between solidarity and connectivity becomes poor.
[0011] The adhesive is mixed in an amount of 1 m2 sprayed. 2 The soil erosion inhibitor used in the spray greening material of the present invention has a high viscosity η of 1000 mPa·s<η≦3200 mPa·s, making it difficult to mix and causing the mixture to harden when mixed. 2 By setting the amount at 0.100 to 0.175 g per spray, it is possible to mix the spray greening materials uniformly. Effect of the Invention
[0012] (1) A spray greening material that is a mixture of a soil erosion inhibitor, fiber, adhesive, fertilizer, and seeds, in which the soil erosion inhibitor is mainly composed of a synthetic resin emulsion, has a viscosity η of 1000 mPa s < η ≦ 3200 mPa s, and is mixed in an amount of 1 m2 of spray area. 2 The fiber is mixed in an amount of 60 to 200g per m2 of spray area. 2 Sprayed greening materials at 80 to 170 g per unit area form a well-balanced solidified layer that does not inhibit plant growth, allowing for greening. This improves resistance to runoff and erosion caused by rainfall, and after the plants have grown, the grown plants have a synergistic effect in preventing erosion by reducing the energy of the water flow, resulting in a stronger ground surface.
[0013] (2) The amount of adhesive mixed is 1 m2 of spray area. 2 By keeping the amount at 0.100 to 0.175 g per unit area, the spray greening materials can be mixed uniformly, enabling stable spraying. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] The spray greening material in the embodiment of the present invention is used for greening by spraying it onto the ground surface such as a slope or a flat surface. The spray greening material in the embodiment is a mixture of a soil erosion inhibitor, fiber, an adhesive, fertilizer, and seeds. In the spray greening method in the embodiment, the spray greening material in the embodiment is applied by spraying it onto the ground surface with a spraying machine such as a hydroseeder or a soil spraying machine.
[0015] The main component of the soil erosion inhibitor is a synthetic resin emulsion. The viscosity η of the soil erosion inhibitor is 1000 mPa·s<η≦3200 mPa·s, more preferably 1100 mPa·s or more, and even more preferably 1200 mPa·s or more. As the soil erosion inhibitor, for example, Crycoat (registered trademark) U-228 Green (Kurita Water Industries Ltd.), which is a permeation solidification type blown sand, dust, and erosion inhibitor, can be used.
[0016] The physical properties of Crycoat U-228 Green are as follows: main component: synthetic resin emulsion, appearance: green milky liquid, pH (25°C): 6.0-8.0 (neutral), viscosity η (25°C): 500-2000 mPa·s, specific gravity (25°C): 1.04-1.06. As a soil erosion prevention material, the viscosity η of Crycoat U-228 Green is adjusted to 1000 mPa·s<η≦2000 mPa·s, more preferably 1100 mPa·s≦η≦2000 mPa·s, and even more preferably 1200≦η≦2000 mPa·s. Furthermore, soil erosion prevention materials with a viscosity η exceeding 1000 mPa·s are higher than the viscosity of 200 to 1000 mPa·s (23°C) of Clicoat C-710, a soil erosion prevention agent for slope greening whose main component is a synthetic resin emulsion, and as such will harden the soil and inhibit plant growth, they are not generally used for spray greening.
[0017] The fiber is a fiber (pulp) extracted from wood, grass, etc., and its main component is cellulose. For example, Oji Fiber (product name) and Fujimi Fiber (product name), which are seed spray curing materials, can be used as the fiber.
[0018] The adhesive is mainly composed of a water-soluble synthetic polymer. For example, Kuricoat C-402 (Kurita Water Industries Ltd.), an adhesive for greening work, can be used as the adhesive. The physical properties of Kuricoat C-402 are as follows: main component: water-soluble synthetic polymer, appearance: white granular powder, pH (20°C): 6.8 to 8.0 (0.4% solution), viscosity (30°C): 200 to 500 mPa s (0.4% solution), bulk density 0.65 to 0.85.
[0019] The fertilizer may be a chemical fertilizer. In particular, it is preferable to use an advanced chemical fertilizer in which the total content of the main components, nitrogen, phosphorus, and potassium, exceeds 30%. As an advanced chemical fertilizer, for example, one containing 15% each of nitrogen, phosphorus, and potassium as main components (all 15) may be used.
[0020] In the present embodiment, the spray greening material is prepared by mixing the above-mentioned soil erosion inhibitor, fiber, and adhesive, as well as fertilizer, seeds, water, etc., into a mixer to form a slurry-like mixture. At this time, the amount of the soil erosion inhibitor mixed is adjusted to 100% per 1 m of spray area. 2 The fiber blend amount is set at 60 to 200 g per 1 m2 of spray area. 2 The amount of adhesive to be mixed is 80 to 170 g per 1 m of spray area. 2 The amount of adhesive to be used should be adjusted according to the soil type.
[0021] In addition, in the spray greening material of this embodiment, the amount of seeds mixed is set to 1 m2 of spray area. 2 The amount of fertilizer mixed should be 7.5 to 20.0 g per m2 of spray area, more preferably 10.0 to 17.5 g per m2 of spray area. 2 The spray greening material of this embodiment is preferably applied with color powder per 1 m2 of spray area. 2 The amount of the mixture is preferably 0.300 to 0.750 g, more preferably 0.400 to 0.600 g.
[0022] On the ground surface sprayed with the spray greening material of the present embodiment, a well-balanced consolidated layer is formed so as not to inhibit plant growth, and the ground surface is greened. On this ground surface, even before plants grow, the consolidated layer improves resistance to runoff and erosion caused by rainfall, and after plants grow, the grown plants further inhibit the flow of water, creating a synergistic effect in preventing erosion, resulting in a stronger ground surface. EXAMPLES
[0023] An application experiment was carried out on the spray-on greening material of the above embodiment. Table 1 shows the blending amounts of the spray-on greening material of the present invention that were found to be optimal as a result of the application experiment.
[0024] [Table 1]
[0025] In addition, the range of application of the fiber blend amount of the present invention (spraying area 1 m 2 In order to confirm the mixing ratio (80~170g per unit), construction experiments were carried out using the mix amounts in Table 1 as the standard and a small amount (70g) and a large amount (180g) of fiber alone. Table 2 shows the results.
[0026] [Table 2]
[0027] In addition, the range of application of the fertilizer blend amount of the present invention (spraying area 1 m 2 In order to confirm the effective amount of fertilizer (20 to 50g per application), construction experiments were carried out using the mixture amounts in Table 1 as the standard, with a small amount (10g) and a large amount (60g) of fertilizer alone. Table 3 shows the results.
[0028] [Table 3]
[0029] In addition, the range of application of the soil erosion inhibitor of the present invention (spray area 1 m 2 In order to confirm the effective amount of the soil erosion inhibitor (60 to 200 g per application), construction experiments were carried out using the mixture amounts in Table 1 as the standard, with a small amount (50 g) and a large amount (210 g) of the soil erosion inhibitor alone. Table 4 shows the results.
[0030] [Table 4]
[0031] In addition, the range of application of the amount of the adhesive of the present invention (spray area 1 m 2 To confirm the adhesive strength (0.100~0.175g per unit), construction experiments were carried out using the mixture amounts in Table 1 as the standard, with a small amount (0.075g) and a large amount (0.200g) of adhesive alone. Table 5 shows the results.
[0032] [Table 5]
[0033] In addition, the range of application of the blend amount of color powder of the present invention (spray area 1 m 2 In order to confirm the mixing ratio (0.300~0.750g per unit), application experiments were carried out using the mixture amounts in Table 1 as the standard, with a small amount (0.250g) and a large amount (0.800g) of color powder alone. Table 6 shows the results.
[0034] [Table 6]
[0035] In addition, the range of application of the seed blend amount of the present invention (spraying area 1 m 2 In order to confirm the effective amount of the seedlings (7.5 to 20.0 g per seedling), construction experiments were carried out using the mixture amounts in Table 1 as the standard, with small amounts (5 g) and large amounts (25 g) of seeds alone. Table 7 shows the results.
[0036] [Table 7] [Industrial Applicability]
[0037] The present invention is useful as a spray greening material and a spray greening method for spraying onto ground surfaces such as slopes to greenify them, and is particularly suitable as a spray greening material and a spray greening method that improves resistance to runoff and erosion due to rainfall even before plants grow.
Claims
1. A spray greening material comprising a mixture of a soil erosion prevention agent, a fiber, an adhesive, a fertilizer, and seeds, The soil erosion inhibitor has a synthetic resin emulsion as a main component, a viscosity η of 1000 mPa·s<η≦3200 mPa·s, and a blending amount of the agent per 1 m of spray area. 2 60 to 200 g per serving, The amount of the fiber blended is 1 m 2 Each serving is 80 to 170 g. Sprayed greening materials.
2. The amount of the adhesive to be mixed is 1 m 2 2. The spray greening material according to claim 1, wherein the amount of the spray greening material is 0.100 to 0.175 g per unit area.
3. A spray greening method comprising spraying the spray greening material according to claim 1 or 2 onto a ground surface by a spray machine.
Citation Information
Patent Citations
Greens-planting work for slope
JP1983207419A
Side-slope stabilizing and vegetating material employing refused material
JP1998183632A
Preparation method for porous vegetation bedrock utilizing foaming
JP1999303084A
Spray material and spray technique using it
JP2002249362A
Greening material
JP2005130732A