Method for manufacturing polishing pad
The method enhances polishing pad production by using precise hole formation and adhesive alignment to support terminal detection windows, improving durability and accuracy in chemical mechanical polishing processes.
Patent Information
- Application Number
- JP2021051702
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-25
- Publication Date
- 2025-01-31
- Estimated Expiration
- 2041-03-25
AI Technical Summary
Existing methods for producing polishing pads with terminal detection windows are prone to damage the polishing layer and affect polishing performance due to the need for large openings or positioning notches, leading to inaccurate end point detection in chemical mechanical polishing processes.
A method involving precise location information acquisition and alignment processes using imaging or laser techniques to form holes smaller than the terminal detection windows, supported by adhesive sheets, ensuring accurate placement and improved durability.
Facilitates the production of polishing pads with enhanced durability and improved accuracy for end point detection, reducing the risk of damage and maintaining polishing performance.
Smart Images

Figure 0007624858000001 
Figure 0007624858000002 
Figure 0007624858000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a polishing pad. [Background technology]
[0002] In the semiconductor manufacturing process, chemical mechanical polishing (CMP) is used for planarization after insulating film deposition and for forming metal wiring. One of the important technologies required for chemical mechanical polishing is the polishing end point detection to detect whether the polishing process is complete. For example, over-polishing or under-polishing with respect to the target polishing end point directly leads to product defects. Therefore, in chemical mechanical polishing, it is necessary to strictly control the amount of polishing by detecting the polishing end point.
[0003] Chemical mechanical polishing is a complex process, and the polishing speed (polishing rate) changes depending on the operating conditions of the polishing equipment, the quality of consumables (slurry, polishing pads, dressers, etc.), and the influence of variations in conditions over time during the polishing process. Furthermore, in recent years, the accuracy of the remaining film thickness and the uniformity of the surface are becoming increasingly strict in the semiconductor manufacturing process. For these reasons, it is becoming more difficult to detect the polishing end point with sufficient accuracy.
[0004] The main methods for detecting the polishing endpoint include the optical endpoint detection method, the torque endpoint detection method, and the eddy current endpoint detection method. In the optical endpoint detection method, the endpoint is detected by irradiating the wafer with light through a transparent window member provided on the polishing pad and monitoring the reflected light.
[0005] As a method for manufacturing a polishing pad using such an optical end point detection method, for example, Patent Document 1 discloses a method for manufacturing a laminated polishing pad including a step of forming an opening by removing a support layer and a peelable protective member in a portion corresponding to a light transmitting region. Patent Document 2 discloses providing an alignment notch for aligning the openings with each other in a polishing pad having a transparent sheet in the opening. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2013-219276 A [Patent Document 2] JP 2001-291686 A Summary of the Invention [Problem to be solved by the invention]
[0007] The invention of Patent Document 1 is a method of forming an opening after laminating each layer, in which the portion corresponding to the light transmitting region is protected with a peelable protective member to prevent the portion from being scratched or foreign matter from adhering to the portion. However, in order to remove the peelable protective member after forming the opening, it is necessary to form the opening larger than the peelable protective member. As a result, when forming the opening, the portion where the peelable protective member does not exist is cut, so there is a risk of damaging the polishing layer and the end point detection window, which is a concern as it may cause a decrease in the strength of the polishing pad and a decrease in the optical properties required for end point detection. In addition, in the method of providing an alignment notch as in Patent Document 2, the alignment notch is present at the end of the polishing layer, and even if the size of the alignment notch is limited, there is a risk of adversely affecting the polishing performance.
[0008] The present invention has been made in consideration of the above problems, and an object of the present invention is to provide a method for more easily producing a polishing pad having an endpoint detection window. [Means for solving the problem]
[0009] That is, the present invention is as follows. [1] a first acquisition step of acquiring position information of an end point detection window provided in an opening of the resin sheet; a first hole forming step of forming a hole in a portion of the adhesive sheet corresponding to a position where the end point detection window is to be installed based on the position information; a first bonding step of aligning the end point detection window with the hole and bonding the resin sheet to the adhesive surface of the adhesive sheet; A method for manufacturing a polishing pad. [2] The position information is based on image information obtained by an imaging device, or information obtained by receiving, by a laser receiver, the laser light that is irradiated on the resin sheet and that has passed through an end point detection window. A method for producing the polishing pad described in [1]. [3] In the first hole forming step, the hole is formed to be smaller than the end point detection window. A method for producing a polishing pad according to [1] or [2]. [4] the position information includes information regarding a center position of the end point detection window, In the first hole forming step, the hole is formed so that a center position of the end point detection window and a center position of the hole coincide with each other. A method for producing a polishing pad according to any one of [1] to [3]. [5] The resin sheet has a plurality of the end point detection windows. A method for producing a polishing pad according to any one of [1] to [4]. [6] The pressure-sensitive adhesive sheet is a double-sided tape or a laminate of a double-sided tape and another layer. A method for producing a polishing pad according to any one of [1] to [5]. [7] When the pressure-sensitive adhesive sheet is the double-sided tape, a second acquisition step of acquiring position information of holes formed in the double-sided tape on the resin sheet; a second hole forming step of forming a hole in a portion of the other layer corresponding to the installation position of the endpoint detection window based on the position information; and a second bonding step of aligning the hole in the double-sided tape with the hole in the other layer, and bonding the double-sided tape on the resin sheet to the other layer. A method for producing the polishing pad described in [6]. Effect of the Invention
[0010] According to the present invention, it is possible to provide a manufacturing method that can more easily manufacture a polishing pad having an endpoint detection window. [Brief description of the drawings]
[0011] [Figure 1] 3A to 3C are schematic cross-sectional views showing an embodiment of a first obtaining step, a first hole forming step, and a first bonding step in the method for producing a polishing pad of the present embodiment. [Diagram 2] 3A to 3C are schematic cross-sectional views showing an embodiment of a second obtaining step, a second hole forming step, and a second bonding step in the method for producing a polishing pad of the present embodiment. [Diagram 3] FIG. 2 is a top view showing one aspect of the resin sheet of the present embodiment. [Figure 4] 1 is a schematic perspective view of a polishing pad according to an embodiment of the present invention. [Diagram 5] 3 is a schematic cross-sectional view of an end point detection window portion of the polishing pad of the present embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, an embodiment of the present invention (hereinafter referred to as "the present embodiment") will be described in detail with reference to the drawings as necessary, but the present invention is not limited to this, and various modifications are possible without departing from the gist of the present invention. In the drawings, the same elements are given the same symbols, and duplicated explanations will be omitted. Furthermore, positional relationships such as up, down, left, and right are based on the positional relationships shown in the drawings, unless otherwise specified. Furthermore, the dimensional ratios of the drawings are not limited to those shown in the drawings.
[0013] 1. Manufacturing method of polishing pad The manufacturing method of the polishing pad of this embodiment includes a first acquisition process for acquiring position information of an end point detection window provided in an opening of a resin sheet, a first hole formation process for forming a hole in a portion of the adhesive sheet corresponding to the installation position of the end point detection window based on the position information, and a first bonding process for aligning the end point detection window and the hole and bonding the adhesive surface of the resin sheet and the adhesive sheet together.
[0014] In addition, the manufacturing method of the polishing pad of this embodiment may further include a second acquisition step of acquiring position information of a hole formed in the double-sided tape on the resin sheet when the adhesive sheet is a double-sided tape, a second hole formation step of forming a hole in a portion corresponding to the installation position of the end point detection window on the other layer based on the position information, and a second bonding step of aligning the hole in the double-sided tape with the hole in the other layer and bonding the double-sided tape on the resin sheet to the other layer. Here, the "other layer" may be a cushion layer.
[0015] Each step will be described in detail below with reference to FIGS. 1 and 2, which are schematic cross-sectional views of each step.
[0016] 1.1.Cutting process The method for manufacturing the polishing pad may include, before the first obtaining step, a cutting step for adjusting the outer shape of the resin sheet 11 having the embedded end point detection windows 12. In the cutting step, a center position O that is equidistant from each of the end point detection windows 12 is identified from the positions of the multiple end point detection windows 12, and the resin sheet 11 may be cut into a predetermined square shape with the center at that position.
[0017] This makes it possible to obtain a resin sheet 11 having a standardized outer shape based on the center position O specified by the end point detection window 12. Then, by subjecting the resin sheet 11 having such a fixed shape to each process described later, each process can be performed with greater accuracy.
[0018] The resin sheet 11 provided in the first obtaining step and thereafter may be one after being punched into a circle, or may be one before being punched into a circle as a rectangle as shown in FIG. 3, which shows a top view of one embodiment of the resin sheet 11. Among these, a rectangle is preferable for carrying out each step related to the subsequent alignment, such as regulating the orientation of the resin sheet 11 during transportation. When carrying out each step with the resin sheet 11 in a rectangular state, in the final stage after each step, the resin sheet 11 may be further punched into a circle based on the center position O specified by the end point detection window 12 to obtain a polishing pad.
[0019] 1.2.First acquisition process The first acquisition step is a step of acquiring position information of the end point detection window 12 provided in the opening of the resin sheet 11. The resin sheet may have a plurality of end point detection windows.
[0020] In FIG. 1, the first manufacturing apparatus 100 includes a conveying mechanism 110 such as a belt conveyor that conveys a resin sheet 11 having an end point detection window 12, an imaging device 120 that acquires position information of the end point detection window 12 provided in the opening of the resin sheet 11, a roller 141 that feeds out an adhesive sheet 21 with a release sheet 22 attached, a hole forming device 130 that forms an opening in the fed adhesive sheet 21, a roller 142 that peels off the release sheet 22 from the adhesive sheet 21 in which the hole has been formed, and a roller 143 that bonds the resin sheet 11 and the adhesive sheet 21 together while aligning the hole in the adhesive sheet 21 from which the release sheet 22 has been peeled off with the end point detection window 12 of the resin sheet 11.
[0021] Here, the transport mechanism 110, the imaging device 120, the hole forming device 130, and the rollers 141, 142, and 143 may be connected to a control unit (not shown) that controls them by wire or wirelessly. The control unit can be configured as an information processing device such as a personal computer. Drive control of the transport mechanism 110, the imaging device 120, the hole forming device 130, and the rollers 141, 142, and 143 and information transmission can be performed via this control unit.
[0022] The method for acquiring the position information of the end point detection window 12 is not particularly limited, but for example, the position information can be acquired from image information captured when the resin sheet 11 transported in the direction of the arrow F by the transport mechanism 110 passes directly below the imaging device 120. At this time, the transport mechanism 110 may be driven so that the resin sheet 11 pauses directly below the imaging device 120 for imaging.
[0023] The method of extracting the position information of the end point detection window 12 from the image information acquired in this manner is not particularly limited, but examples include a method of identifying the end point detection window 12 based on differences in the color shades, etc., of the resin sheet 11 and the end point detection window 12 in the image information and identifying its contour; and a method of identifying the end point detection window 12 from the image information by image processing such as edge detection and identifying its contour.
[0024] Also, a laser receiver may be used instead of the imaging device 120. For example, the position of the end point detection window 12 may be specified based on information obtained by receiving, by the laser receiver, the laser light that is irradiated on the resin sheet 11 and that has passed through the end point detection window 12.
[0025] At this time, the conveying mechanism 110 may be driven to temporarily stop the resin sheet 11 directly below the laser oscillator and the laser receiver, and the laser oscillator and the laser receiver may be scanned across the resin sheet 11, or the laser oscillator and the laser receiver may be fixed midway along the conveying mechanism 110, and the conveying mechanism 110 may be kept moving at a constant speed, so that the laser oscillator and the laser receiver scan the resin sheet 11 relatively to identify the position of the end point detection window 12.
[0026] Furthermore, the control unit may calculate the center position of the end point detection window 12 based on the information related to the contour of the end point detection window 12 thus obtained from the image information. The position information such as the contour and center position of the end point detection window 12 thus obtained may be transmitted to the hole forming device 130 via the control unit.
[0027] 1.3.First hole formation process The first hole forming step is a step of forming a hole in a portion of the adhesive sheet corresponding to the installation position of the end point detection window based on the position information. Here, the adhesive sheet may be a double-sided tape or a laminate of the double-sided tape and another layer such as a cushion layer.
[0028] Specifically, the control unit drives and controls the roller 141 to feed out the adhesive sheet 21, and transmits position information of the end point detection window 12 to the hole forming device 130, and the hole forming device 130 forms a hole in a portion of the fed adhesive sheet 21 that corresponds to the installation position of the end point detection window. When the hole forming device 130 forms a hole, the roller 141 may be temporarily stopped.
[0029] At this time, the hole forming device 130 may form a hole smaller than the end point detection window 12. More specifically, the control unit transmits position information including information on the contour of the end point detection window 12 and its center position to the hole forming device 130, and the hole forming device 130 can form a hole smaller than the contour while aligning the center position of the end point detection window 12 so that it coincides with the center position of the hole to be formed.
[0030] This allows the adhesive sheet 21, in which a hole smaller than the end point detection window 12 is formed, to be attached to the resin sheet 11 while aligning the center position of the formed hole with the center position of the end point detection window 12. In this way, by making the hole in the adhesive sheet 21 to be attached smaller than the end point detection window 12, the end point detection window 12 can be supported from the back side of the resin sheet 11 by the adhesive sheet 21. This further improves the durability of the resulting polishing pad.
[0031] 1.4.First lamination process The first lamination step is a step of laminating the adhesive surface of the adhesive sheet to the resin sheet by aligning the end point detection window with the hole. After lamination, the adhesive sheet may be cut to fit the size of the resin sheet.
[0032] Specifically, the control unit drives and controls roller 141 to further feed adhesive sheet 21 with holes formed therein, and drives and controls roller 142 to take up the release sheet attached to the adhesive surface of adhesive sheet 21. At the same time, the control unit drives conveying mechanism 110 to further feed resin sheet 11 in the direction of arrow F, aligns end point detection window 12 with the holes, and attaches resin sheet 11 to the adhesive surface of adhesive sheet 21.
[0033] At this time, the control unit can drive and control the rollers 143 and the conveying mechanism 110 while calculating the positional relationship between the adhesive sheet 21 sent out by the rollers 141 and the resin sheet 11 conveyed by the conveying mechanism 110. Furthermore, in the drive control, based on information on the center position of the hole formed in the adhesive sheet 21 and information on the center position of the end point detection window 12 of the resin sheet 11, the moving distances of the resin sheet 11 and the adhesive sheet 21 may be controlled so that the center positions of these sheets overlap, and they are bonded together.
[0034] This allows the end point detection window 12 and the hole formed in the adhesive sheet 21 to be attached in a state where they overlap concentrically. Therefore, for example, as shown in Fig. 5 which shows a cross-sectional view of the periphery of the end point detection window 12, when the hole formed in the adhesive sheet 21 is smaller than the end point detection window 12, the end point detection window 12 can be supported from the back side of the resin sheet 11 by the adhesive sheet 21. This further improves the durability of the resulting polishing pad.
[0035] 1.5.Second acquisition process The second obtaining step is a step of obtaining position information of holes in the double-sided tape that has been adhered to the resin sheet 11 in the first adhering step.
[0036] In FIG. 2, the second manufacturing apparatus 200 includes a conveying mechanism 210 that conveys the resin sheet 11, an imaging device 220 that acquires positional information of holes in the double-sided tape, a roller 241 that feeds out the other layer 31, a hole forming device 230 that forms openings in the fed out other layer 31, and a roller 242 that bonds the resin sheet 11 and the other layer 31 together while aligning the holes in the other layer 31 with the holes in the double-sided tape of the resin sheet 11.
[0037] Here, the transport mechanism 210, the imaging device 220, the hole forming device 230, and the rollers 241, 242 may be connected by wire or wirelessly to a second control unit (not shown) that controls them. The second control unit can be configured as an information processing device such as a personal computer. Drive control of the transport mechanism 210, the imaging device 220, the hole forming device 230, and the rollers 241, 242 and information transmission can be performed via this second control unit.
[0038] The method for acquiring the position information of the holes in the double-sided tape attached to the resin sheet 11 is not particularly limited, but examples thereof include a method using an imaging device or a method using a laser receiver, as described in the first acquisition process above.
[0039] 1.6.Second hole formation process The second hole forming step is a step of forming a hole in a portion of the other layer corresponding to the installation position of the end point detection window based on the position information acquired in the second acquisition step. Here, the other layer may be a cushion layer or a cushion layer with a double-sided tape attached thereto.
[0040] Specifically, the control unit controls the driving of the roller 241 to feed out the other layer 31, and transmits position information of holes in the double-sided tape to the hole forming device 230, and the hole forming device 230 forms holes in the portions of the other layer 31 that correspond to the installation positions of the double-sided tape. When the hole forming device 230 forms holes, the roller 241 may be temporarily stopped.
[0041] 1.7.Second lamination process The second lamination step is a step of laminating the double-sided tape on the resin sheet to the other layer by aligning the holes in the double-sided tape with the holes in the other layer. The other layer after lamination may be cut to fit the size of the resin sheet.
[0042] Specifically, the second control unit drives and controls roller 242 to further feed adhesive sheet 21 with holes formed therein, and drives conveying mechanism 210 to further feed resin sheet 11 in the direction of arrow F, aligning the holes in the double-sided tape with the holes in the other layer, and bonding the adhesive surface of resin sheet 11 (adhesive sheet 21) to the other layer 31.
[0043] Even in this case, the transport mechanism 210 and the roller 242 may be driven and controlled so that the central positions of the hole formed in the other layer 31 and the hole in the double-sided tape of the resin sheet 11 overlap, based on information on the central position of the hole formed in the other layer 31 and the central position of the hole in the double-sided tape of the resin sheet 11. This allows the holes formed in the other layer 31 and the holes in the double-sided tape of the resin sheet 11 to be bonded together in a state where they overlap concentrically, thereby further improving the durability of the resulting polishing pad.
[0044] Furthermore, the resin sheet 11 to which the other layer 31 has been attached as described above can be punched out into a circular shape in a subsequent process and used as a polishing pad.
[0045] 2. Polishing pad A schematic perspective view of the polishing pad of this embodiment is shown in Fig. 4. As shown in Fig. 4, the polishing pad 10 of this embodiment has a polishing layer made of a resin sheet 11 and a plurality of end point detection windows 12, and may have another layer 31 such as a cushion layer 13 on the side opposite to the polishing surface 11a, if necessary.
[0046] Fig. 5 shows a cross-sectional view of the periphery of the end point detection window 12 in Fig. 4. As shown in Fig. 5, an adhesive layer 14 (adhesive sheet 21) may be provided between the polishing layer (resin sheet 11) and the cushion layer 13 (other layer 31), and an adhesive layer 15 may be provided on the surface of the cushion layer 13 (other layer 31). The polishing surface 11a of the polishing pad of this embodiment may be flat, or may be uneven with grooves 16 formed therein, as shown in Fig. 5. [Industrial Applicability]
[0047] The method for producing a polishing pad of the present invention has industrial applicability as a method for efficiently producing a polishing pad that can be suitably used in an optical endpoint detection method. [Explanation of symbols]
[0048] 10...polishing pad, 11...resin sheet, 11a...polishing surface, 12...end point detection window, 13...cushion layer, 14, 15...adhesive layer, 16...groove, 21...adhesive sheet, 22...release sheet, 31...other layer, 100...first manufacturing device, 110...transport mechanism, 120...imaging device, 130...hole forming device, 141, 142, 143...rollers, 200...second manufacturing device, 210...transport mechanism, 220...imaging device, 230...hole forming device, 241, 242...rollers
Claims
1. a first acquisition step of acquiring position information of an end point detection window provided in an opening of the resin sheet; a first hole forming step of forming a hole in a portion of the adhesive sheet corresponding to a position where the end point detection window is to be installed based on the position information; a first bonding step of aligning the end point detection window with the hole and bonding the resin sheet to the adhesive surface of the adhesive sheet; A method for manufacturing a polishing pad.
2. The position information is based on image information obtained by an imaging device, or information obtained by receiving, by a laser receiver, the laser light that is irradiated on the resin sheet and that has passed through an end point detection window. A method for producing the polishing pad according to claim 1 .
3. In the first hole forming step, the hole is formed to be smaller than the end point detection window. The method for producing the polishing pad according to claim 1 or 2.
4. the position information includes information regarding a center position of the end point detection window, In the first hole forming step, the hole is formed so that a center position of the end point detection window coincides with a center position of the hole. The method for producing a polishing pad according to any one of claims 1 to 3.
5. The resin sheet has a plurality of the end point detection windows. The method for producing the polishing pad according to any one of claims 1 to 4.
6. The pressure-sensitive adhesive sheet is a double-sided tape or a laminate of a double-sided tape and another layer. The method for producing a polishing pad according to any one of claims 1 to 5.
7. When the pressure-sensitive adhesive sheet is the double-sided tape, a second acquisition step of acquiring position information of holes formed in the double-sided tape on the resin sheet; a second hole forming step of forming a hole in a portion of the other layer corresponding to the installation position of the endpoint detection window based on the position information; and a second bonding step of aligning the hole in the double-sided tape with the hole in the other layer, and bonding the double-sided tape on the resin sheet to the other layer. The method for producing the polishing pad according to claim 6 .
Citation Information
Patent Citations
Polishing pad for chemical-mechanical polishing apparatus having leak-preventive transparent window
JP2001291686A
Method of forming laminated polishing pad
JP2005260222A
Method of manufacturing polishing pad
JP2007283459A
Manufacturing method of polishing pad
JP2008296333A
Processing of the polishing pad window
JP2012524672A