Metal leaching methods

The use of a leaching container with a porous member above the liquid surface in the acidic leaching solution effectively addresses the foaming issue, ensuring efficient metal recovery from lithium-ion battery waste by breaking bubbles and maintaining process stability.

JP7783909B2Active Publication Date: 2025-12-10JX METALS CIRCULAR SOLUTIONS CO LTD JP
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
JP2023566105
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-12-09
Filing Date
2022-10-05
Publication Date
2025-12-10
Estimated Expiration
2042-10-05

AI Technical Summary

Technical Problem

The generation of bubbles in the acidic leaching solution during the metal leaching process of lithium-ion battery waste hinders the smooth operation and efficiency of metal recovery.

Method used

A metal leaching method that involves using a leaching container with a porous member positioned above the liquid surface to break bubbles formed in the acidic leachate, with the porous member having openings of 12 mm or less, effectively suppressing foaming.

Benefits of technology

The method effectively suppresses foaming in the acidic leaching solution, allowing for smooth and efficient metal leaching from lithium-ion battery waste, even under conditions that typically generate significant bubbles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007783909000001
    Figure 0007783909000001
  • Figure 0007783909000002
    Figure 0007783909000002
  • Figure 0007783909000003
    Figure 0007783909000003
Patent Text Reader

Abstract

A metal leaching method includes contacting battery powder of lithium ion battery waste with an acidic leachate 21 inside a leaching container 1 and leaching a metal contained in the battery powder into the acidic leachate 21, wherein the leaching container 1 has a porous member 2 arranged at a position above the liquid surface 22 of the acidic leachate 21 stored inside the container so as to cover the liquid surface 22, and when the metal is leached inside the leaching container 1, gas bubbles Ba generated in the acidic leachate 21 are brought into contact with the porous member 2 and collapsed, the opening of the porous member 2 being 12 mm or less.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Process of defoaming

    JP1986283311A

  • JP1988054405U

  • Foaming preventing apparatus instirring tank

    JP1998309402A

  • Positive electrode active material for lithium secondary battery, manufacturing method for same, positive electrode material for lithium secondary battery using same, positive electrode for lithium secondary battery, and lithium secondary battery

    JP2004342548A

  • Positive electrode for lithium secondary battery and lithium secondary battery including the same

    JP2006310311A