Electronic component
Patent Information
- Application Number
- JP2024552827
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-07-03
- Filing Date
- 2023-07-03
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2043-07-03
AI Technical Summary
Electronic components face limitations in flux resistance due to high melting point conductive pastes containing silica powder, which can lead to cracking and restrict the use of silica powder concentration, necessitating an alternative to enhance flux resistance without increasing silica powder content.
A glass film with a base portion containing oxides of alkali or alkaline earth metals and silicon oxide, and a specific portion with a lower metal oxide content, is applied over the electronic component, creating an interface that impedes the penetration of water-soluble flux, thereby improving flux resistance.
The interface in the glass film effectively prevents deeper penetration of water-soluble flux, enhancing the component's resistance to erosion and allowing for improved flux resistance without increasing silica powder concentration.
Abstract
Description
Electronic Components
[0001] The present invention relates to electronic components.
[0002] Patent Document 1 describes an electronic component. The electronic component includes an element body and external electrodes laminated on the surface of the element body. The external electrodes are formed by firing a conductive paste. The conductive paste contains conductive powder, borosilicate glass, silica powder, and an organic vehicle.
[0003] Patent No. 5765041
[0004] The electronic component described in Patent Document 1 contains silica powder in the external electrodes. This can improve resistance to water-soluble flux, a surface treatment agent used during soldering, or so-called flux resistance. On the other hand, the electronic component described in Patent Document 1 has a high melting point because the conductive paste contains a high concentration of silica powder. This makes it more likely that cracks will occur in the element body when the conductive paste is fired. Therefore, there is a limit to how much silica powder can be added. Therefore, a technology that can improve flux resistance, separate from the addition of silica powder, is needed.
[0005] In order to solve the above-described problems, one aspect of the present disclosure is an electronic component comprising: an element body; a glass film covering an outer surface of the element body; and an external electrode provided on the outer surface of the glass film and having at least a base electrode, wherein the glass film has a base portion containing, in addition to silicon oxide, an oxide of one or more metal elements selected from alkali metals and alkaline earth metals; and a specific portion containing, in addition to silicon oxide, an oxide of the same metal element as in the base portion, wherein the content of the metal element in the specific portion is lower than the content of the metal element in the base portion.
[0006] According to the above configuration, an interface between the base portion and the specific portion can be present in the glass film. If an interface is present in the glass film, even if the water-soluble flux penetrates the glass film, the water-soluble flux will spread along the interface but will not penetrate deeper. This can better prevent external corrosion of the element body.
[0007] Flux resistance can be improved.
[0008] FIG. 1 is a perspective view of an electronic component according to an embodiment. FIG. 2 is a side view of the electronic component according to an embodiment. FIG. 3 is a cross-sectional view taken along line 3-3 in FIG. 2. FIG. 4 is an enlarged cross-sectional view of a portion including a glass film in FIG. 3. FIG. 5 is a flowchart illustrating a method for manufacturing an electronic component. FIG. 6 is an explanatory diagram illustrating a method for manufacturing an electronic component. FIG. 7 is an explanatory diagram illustrating a method for manufacturing an electronic component. FIG. 8 is an explanatory diagram illustrating a method for manufacturing an electronic component. FIG. 9 is an explanatory diagram illustrating a method for manufacturing an electronic component. FIG. 10 is an explanatory diagram illustrating a method for manufacturing an electronic component. FIG. 11 is an explanatory diagram illustrating a method for manufacturing an electronic component. FIG. 12 is an enlarged cross-sectional view of a portion including a glass film of an electronic component according to a modified example.
[0009] An embodiment of an electronic component will be described below with reference to the drawings. The drawings may show components enlarged to facilitate understanding. The dimensional proportions of the components may differ from those in the actual drawings or from those in other drawings.
[0010] 1, the electronic component 10 is, for example, a surface-mount type negative temperature coefficient thermistor component mounted on a circuit board, etc. Note that a negative temperature coefficient thermistor component has the characteristic that its resistance value decreases as the temperature increases.
[0011] The electronic component 10 includes an element body 20. The element body 20 is generally rectangular prism-shaped and has a central axis CA. In the following description, an axis extending along the central axis CA is referred to as a first axis X. One of the axes perpendicular to the first axis X is referred to as a second axis Y. An axis perpendicular to the first axis X and the second axis Y is referred to as a third axis Z. One of the directions along the first axis X is referred to as a first positive direction X1, and the direction along the first axis X that is opposite to the first positive direction X1 is referred to as a first negative direction X2. One of the directions along the second axis Y is referred to as a second positive direction Y1, and the direction along the second axis Y that is opposite to the second positive direction Y1 is referred to as a second negative direction Y2. One of the directions along the third axis Z is referred to as a third positive direction Z1, and the direction along the third axis Z that is opposite to the third positive direction Z1 is referred to as a third negative direction Z2.
[0012] The outer surface 21 of the element body 20 has six flat surfaces 22. The term "surface" of the element body 20 as used herein refers to a surface that can be observed when the entire element body 20 is observed. In other words, even if there are minute irregularities or steps that are not visible unless a portion of the element body 20 is magnified and observed using a microscope, the surface is still referred to as a flat or curved surface. The six flat surfaces 22 extend in different directions. The six flat surfaces 22 are broadly divided into a first end surface 22A facing the first positive direction X1, a second end surface 22B facing the first negative direction X2, and four side surfaces 22C. The four side surfaces 22C are, respectively, a surface facing the third positive direction Z1, a surface facing the third negative direction Z2, a surface facing the second positive direction Y1, and a surface facing the second negative direction Y2.
[0013] The outer surface 21 of the element body 20 has 12 boundary surfaces 23. The boundary surfaces 23 include curved surfaces that exist at the boundaries between adjacent flat surfaces 22. That is, the boundary surfaces 23 include curved surfaces that are formed by, for example, R-chamfering the corners that form the adjacent flat surfaces 22.
[0014] The outer surface 21 of the element body 20 also has eight spherical corner surfaces 24. The corner surfaces 24 are boundary portions between three adjacent flat surfaces 22. In other words, the corner surfaces 24 include curved surfaces at the intersections of the three boundary surfaces 23. That is, the corner surfaces 24 include curved surfaces formed by, for example, R-chamfering the corners formed by the three adjacent flat surfaces 22.
[0015] 1 and 2, the surface of a glass film 50 (described later) is identified with the outer surface 21 of the element body 20 and is designated by a reference symbol. As shown in Fig. 2, the element body 20 has a larger dimension along the first axis X than along the third axis Z. As shown in Fig. 1, the element body 20 has a larger dimension along the first axis X than along the second axis Y. The material of the element body 20 is a ceramic obtained by firing a metal oxide containing at least one of Mn, Fe, Ni, Co, Ti, Ba, Al, and Zn.
[0016] 3 , the electronic component 10 includes two first internal electrodes 41 and two second internal electrodes 42. The first internal electrodes 41 and the second internal electrodes 42 are embedded inside the element body 20.
[0017] The first internal electrode 41 is made of a conductive material. For example, the first internal electrode 41 is made of silver and palladium. The second internal electrode 42 is made of the same material as the first internal electrode 41, that is, silver and palladium.
[0018] The first internal electrode 41 has a rectangular plate shape. The main surface of the first internal electrode 41 is perpendicular to the second axis Y. The second internal electrode 42 has the same rectangular plate shape as the first internal electrode 41. The main surface of the second internal electrode 42 is perpendicular to the second axis Y, similar to the first internal electrode 41.
[0019] The dimension of the first internal electrode 41 in the direction along the first axis X is smaller than the dimension of the element body 20 in the direction along the first axis X. Also, as shown in Fig. 1 , the dimension of the first internal electrode 41 in the direction along the third axis Z is approximately two-thirds of the dimension of the element body 20 in the direction along the third axis Z. The dimensions of the second internal electrode 42 in each direction are the same as those of the first internal electrode 41.
[0020] 3, the first internal electrodes 41 and the second internal electrodes 42 are positioned alternately in the direction along the second axis Y. That is, the first internal electrode 41, the second internal electrode 42, the first internal electrode 41, and the second internal electrode 42 are arranged in this order from the side surface 22C facing the second positive direction Y1 to the second negative direction Y2. In this embodiment, the distances between the internal electrodes in the direction along the second axis Y are equal.
[0021] 1, the two first internal electrodes 41 and the two second internal electrodes 42 are both located at the center of the element body 20 in the direction along the third axis Z. On the other hand, as shown in Fig. 3, the first internal electrodes 41 are located closer to the first positive direction X1, and the second internal electrodes 42 are located closer to the first negative direction X2.
[0022] Specifically, the end of the first internal electrode 41 on the first positive direction X1 side coincides with the end of the element body 20 on the first positive direction X1 side. The end of the first internal electrode 41 on the first negative direction X2 side is located inside the element body 20 and does not reach the end of the element body 20 on the first negative direction X2 side. On the other hand, the end of the second internal electrode 42 on the first negative direction X2 side coincides with the end of the element body 20 on the first negative direction X2 side. The end of the second internal electrode 42 on the first positive direction X1 side is located inside the element body 20 and does not reach the end of the element body 20 on the first positive direction X1 side.
[0023] The electronic component 10 includes a glass film 50. The glass film 50 covers the outer surface 21 of the element body 20. In this embodiment, the glass film 50 covers substantially the entire area of the outer surface 21 of the element body 20. The main material of the glass film 50 is insulating glass. Therefore, the glass film 50 contains silicon oxide, specifically silicon dioxide.
[0024] 3 , the electronic component 10 includes a first external electrode 61 and a second external electrode 62. The first external electrode 61 includes a first base electrode 61A and a first metal layer 61B. The first base electrode 61A is laminated on the glass film 50 in a portion of the outer surface 21 of the element body 20, including the first end face 22A. Specifically, the first base electrode 61A is a five-sided electrode that covers the first end face 22A of the element body 20 and portions of the four side faces 22C facing the first positive direction X1. In this embodiment, the first base electrode 61A is made of copper.
[0025] The first metal layer 61B covers the first base electrode 61A from the outside. Therefore, the first metal layer 61B is laminated on the first base electrode 61A. Specifically, as shown in FIG. 4, the first metal layer 61B has a two-layer structure of a nickel layer 61C and a tin layer 61D. Furthermore, as shown in FIG. 3, the outer edge of the first metal layer 61B is located outside the outer edge of the first base electrode 61A. The outer edge of the first metal layer 61B is located on the surface of the glass film 50. Therefore, a portion of the first metal layer 61B is located on the surface of the glass film 50.
[0026] 3 , the second external electrode 62 has a second base electrode 62A and a second metal layer 62B. The second base electrode 62A is laminated on the glass film 50 in a portion of the outer surface 21 of the element body 20, including the second end face 22B. Specifically, the second base electrode 62A is a five-sided electrode that covers the second end face 22B of the element body 20 and portions of the four side faces 22C facing the first negative direction X2. In this embodiment, the material of the second base electrode 62A is the same as the material of the first external electrode 61, that is, copper.
[0027] The second metal layer 62B covers the second base electrode 62A from the outside. Therefore, the second metal layer 62B is laminated on the second base electrode 62A. Specifically, like the first metal layer 61B, the second metal layer 62B has a two-layer structure of a nickel layer and a tin layer (not shown). Furthermore, as shown in FIG. 3 , the outer edge of the second metal layer 62B is located outside the outer edge of the second base electrode 62A. The outer edge of the second metal layer 62B is located on the surface of the glass film 50. Therefore, a portion of the second metal layer 62B is located on the surface of the glass film 50.
[0028] The second external electrode 62 does not reach the first external electrode 61 on the side surface 22C, and is spaced apart from the first external electrode 61 in the direction along the first axis X. In addition, the first external electrode 61 and the second external electrode 62 are not stacked in the central portion of the side surface 22C of the element body 20 in the direction along the first axis X, and the glass film 50 is exposed. Note that in Figures 1 to 3, the first external electrode 61 and the second external electrode 62 are shown by two-dot chain lines.
[0029] 3 , the first external electrode 61 and the end of the first internal electrode 41 on the first positive direction X1 side are connected via a first through portion 71 that penetrates the glass film 50. Note that, as will be described in detail later, the first through portion 71 is formed during the manufacturing process of the electronic component 10 when the silver and palladium that constitute the first internal electrode 41 extend toward the first external electrode 61.
[0030] The second external electrode 62 and the end of the second internal electrode 42 on the first negative direction X2 side are connected via a second through portion 72 that penetrates the glass film 50. Similar to the first through portion 71, the second through portion 72 is formed by the silver and palladium constituting the second internal electrode 42 extending toward the second external electrode 62 during the manufacturing process of the electronic component 10. Note that while FIG. 3 illustrates the first internal electrode 41 and the first through portion 71 as separate components with a boundary, in reality, there is no clear boundary between them. The same applies to the second through portion 72. The first through portion 71 and the second through portion 72 are not shown in FIGS. 1 and 2 .
[0031] <Regarding the Glass Film> The portions of the glass film 50 that are not covered by either the first base electrode 61A or the second base electrode 62A are made of a generally uniform glass layer of silicon dioxide. On the other hand, the portions of the glass film 50 that are covered by either the first base electrode 61A or the second base electrode 62A are made of a mixture of two types of glass layers with different compositions.
[0032] Specifically, as shown in FIG. 4 , the glass film 50 has a base portion 51 and a specific portion 52. Most of the base portion 51 and the specific portion 52 are located in the glass film 50 between the first base electrode 61A and the outer surface 21 of the element body 20, and between the second base electrode 62A and the outer surface 21 of the element body 20. The base portion 51 contains, in addition to silicon oxide, an oxide of one or more metal elements selected from alkali metals and alkaline earth metals. In this embodiment, the metal element is barium. In this embodiment, the base portion 51 contains an oxide of barium and calcium, which are alkaline earth metals. The base portion 51 also contains zinc oxide. Furthermore, the base portion 51 contains an oxide of aluminum.
[0033] The specific portion 52 has a flat layer shape when viewed in cross section. The specific portion 52 contains an oxide of the same metal element as the base portion 51, in addition to an oxide of silicon. That is, in this embodiment, the specific portion 52 contains an oxide of barium, which is an alkaline earth metal. On the other hand, the specific portion 52 does not contain an oxide of calcium. Furthermore, the specific portion 52 contains an oxide of zinc. On the other hand, the specific portion 52 does not contain an oxide of aluminum.
[0034] The content of barium, which is a metal element, in the specific portion 52 is smaller than the content of barium, which is a metal element, in the base portion 51. The content of silicon in the specific portion 52 is larger than the content of silicon in the base portion 51. The content of zinc in the specific portion 52 is larger than the content of zinc in the base portion 51.
[0035] <Method for Manufacturing Electronic Component> Next, a method for manufacturing electronic component 10 will be described. As shown in Fig. 5, the method for manufacturing electronic component 10 includes a laminate preparation step S11, an R-chamfering step S12, a solvent introduction step S13, a catalyst introduction step S14, an element introduction step S15, a polymer introduction step S16, and a metal alkoxide introduction step S17. The method for manufacturing electronic component 10 also includes a film formation step S18, a drying step S19, a baking step S20, a conductor application step S21, a curing step S22, and a plating step S23.
[0036] First, in forming the element body 20, in the laminate preparation step S11, a laminate is prepared, which is the element body 20 that does not have boundary surfaces 23 and corner surfaces 24. That is, the laminate is in a state before R-chamfering and has a rectangular parallelepiped shape with six flat surfaces 22. For example, first, a plurality of ceramic sheets that will become the element body 20 are prepared. The sheets are thin plate-like. A conductive paste that will become the first internal electrode 41 is laminated on the sheets. A ceramic sheet that will become the element body 20 is laminated on the laminating paste. A conductive paste that will become the second internal electrode 42 is laminated on the sheet. In this manner, the ceramic sheets and the conductive paste are laminated. Then, the laminate is cut to a predetermined size to form an unfired laminate. The unfired laminate is then fired at a high temperature to prepare the laminate.
[0037] Next, an R-chamfering process S12 is performed. In the R-chamfering process S12, a boundary surface 23 and a corner surface 24 are formed on the laminate prepared in the laminate preparation process S11. For example, the corners of the laminate are R-chamfered by barrel polishing, thereby forming the curved boundary surface 23 and the curved corner surface 24. In this way, the element body 20 is formed.
[0038] Next, a solvent introduction step S13 is performed. As shown in Fig. 6, in the solvent introduction step S13, 2-propanol is introduced into a reaction vessel 81 as a solvent 82. Next, as shown in Fig. 5, a catalyst introduction step S14 is performed. As shown in Fig. 7, in the catalyst introduction step S14, first, stirring of the solvent 82 in the reaction vessel 81 is started. Then, ammonia water is introduced into the reaction vessel 81 as an aqueous solution 83 containing a catalyst. The catalyst in this embodiment is hydroxide ions, which function as a catalyst for promoting hydrolysis of a metal alkoxide 85, which will be described later.
[0039] Next, an element body introduction step S15 is performed as shown in Fig. 5. As shown in Fig. 8, in the element body introduction step S15, a plurality of element bodies 20 formed in advance in the R-chamfering step S12 as described above are introduced into a reaction vessel 81.
[0040] Next, a polymer introduction step S16 is performed as shown in Fig. 5. As shown in Fig. 9, in the polymer introduction step S16, polyvinylpyrrolidone is introduced as a polymer 84 into the reaction vessel 81. As a result, the polymer 84 introduced into the reaction vessel 81 is adsorbed onto the outer surface 21 of the element body 20.
[0041] Next, as shown in FIG. 5 , a metal alkoxide introduction step S17 is performed. As shown in FIG. 10 , in the metal alkoxide introduction step S17, liquid tetraethyl orthosilicate is introduced into the reaction vessel 81 as the metal alkoxide 85. Note that tetraethyl orthosilicate is also sometimes referred to as tetraethoxysilane. In this embodiment, the amount of metal alkoxide 85 introduced in the metal alkoxide introduction step S17 is calculated based on the area of the outer surface 21 of the element bodies 20 introduced in the element introduction step S15. Specifically, the amount of metal alkoxide 85 is calculated by multiplying the amount of metal alkoxide 85 per element body 20 required to form a pre-diffusion glass film 50A covering the outer surface 21 of the element body 20 by the number of element bodies 20. The pre-diffusion glass film 50A is a film in a state before diffusion of metal elements contained in the glass of the conductive paste occurs, as described below. In other words, the pre-diffusion glass film 50A does not contain metal elements derived from the conductive paste.
[0042] Next, as shown in Fig. 5, a film-forming step S18 is performed. As shown in Fig. 11, in the film-forming step S18, the stirring of the solvent 82, which was started in the solvent-adding step S13 described above, is continued for a predetermined time after the metal alkoxide 85 is added to the reaction vessel 81 in the metal alkoxide-adding step S17. In the film-forming step S18, a pre-diffusion glass film 50A is formed by a liquid-phase reaction in the reaction vessel 81.
[0043] 5, a drying step S19 is performed. In the drying step S19, after stirring is continued for a predetermined time in the film-forming step S18, the element body 20 is removed from the reaction vessel 81 and dried. As a result, the sol-state pre-diffusion glass film 50A is dried and becomes a gel-state pre-diffusion glass film 50A.
[0044] Next, a firing step S20 is performed. In the firing step S20, the element body 20 covered with the gel-like pre-diffusion glass film 50A is heated. This causes the water and polymer 84 to evaporate from the gel-like pre-diffusion glass film 50A. As a result, a pre-diffusion glass film 50A made of silicon dioxide is formed.
[0045] Next, a conductor application step S21 is performed. In the conductor application step S21, a conductor paste is applied to two portions of the surface of the pre-diffusion glass film 50A: a portion covering the first end face 22A of the element body 20 and a portion covering the second end face 22B of the element body 20. Specifically, the conductor paste is applied to cover the entire first end face 22A and portions of the four side faces 22C of the glass film 50. The conductor paste is also applied to cover the entire second end face 22B and portions of the four side faces 22C of the pre-diffusion glass film 50A. The conductor paste contains copper powder, glass, and an organic medium. The copper powder in the conductor paste becomes the first base electrode 61A and the second base electrode 62A in a subsequent curing step S22. The glass in the conductor paste contains an additive containing one or more metal elements selected from alkali metals and alkaline earth metals. More specifically, the metal element is barium, and the conductive paste further contains calcium, aluminum, and zinc as additives.
[0046] Next, a curing step S22 is performed. Specifically, in the curing step S22, the pre-diffusion glass film 50A and the element body 20 to which the conductive paste has been applied are heated. This causes the organic medium in the conductive paste to evaporate. The copper powder in the conductive paste then combines to form the first base electrode 61A and the second base electrode 62A. In other words, the first base electrode 61A and the second base electrode 62A are made of copper. Note that the first base electrode 61A and the second base electrode 62A may contain impurities.
[0047] At the same time, the glass in the conductive paste melts and becomes integrated with a portion of the pre-diffusion glass film 50A. However, at the start of the curing step S22, the pre-diffusion glass film 50A is composed almost entirely of silicon oxide. Therefore, the pre-diffusion glass film 50A has a high melting point. Therefore, a portion of the pre-diffusion glass film 50A remains without being integrated with the glass of the conductive paste. However, at this time, metal elements contained in the glass additive in the conductive paste diffuse into the pre-diffusion glass film 50A made of silicon dioxide. As a result, the metal elements penetrate into the pre-diffusion glass film 50A covering the outer surface 21 of the element body 20. When the element body 20 is then fired, the mixture of the glass derived from the conductive paste and the pre-diffusion glass film 50A becomes the base portion 51. Meanwhile, the remaining pre-diffusion glass film 50A that has not been integrated with the glass of the conductive paste becomes the specific portion 52. As described above, metal elements also diffuse into the remaining pre-diffusion glass film 50A that has not been integrated with the glass of the conductive paste. Therefore, the specific portion 52 contains a metal element, although the amount is smaller than that of the base portion 51 .
[0048] In addition, the diffusion of metal elements as described above is unlikely to occur in the portions of the pre-diffusion glass film 50A that are not covered with the conductive paste, and therefore, the portions of the pre-diffusion glass film 50A that are not covered with the conductive paste become a generally uniform glass layer without distinction between the base portion 51 and the specific portion 52.
[0049] In this embodiment, during heating in the curing step S22, the Kirkendall effect, which arises from the difference in diffusion rate between the first internal electrode 41 and the first base electrode 61A, attracts silver and palladium contained in the first internal electrode 41 toward the first base electrode 61A, which is copper. As a result, the first through-hole 71 extends from the first internal electrode 41 toward the first base electrode 61A, penetrating the glass film 50, thereby connecting the first internal electrode 41 and the first base electrode 61A. The same applies to the second through-hole 72 connecting the second internal electrode 42 and the second base electrode 62A.
[0050] Next, a plating step S23 is performed. In the plating step S23, electroplating is performed on the first base electrode 61A and the second base electrode 62A. As a result, a first metal layer 61B is formed on the surface of the first base electrode 61A. Furthermore, a second metal layer 62B is formed on the surface of the second base electrode 62A. As shown in FIG. 4 , the first metal layer 61B is electroplated with two types of metal, nickel and tin, to form a two-layer structure of a nickel layer 61C and a tin layer 61D. Although not shown, similar to the first metal layer 61B, the second metal layer 62B is electroplated with two types of metal, nickel and tin, in sequence to form a two-layer structure of a nickel layer and a tin layer. In this manner, the electronic component 10 is formed.
[0051] (Operation of the embodiment) When the electronic component 10 of the above embodiment is solder-mounted on a substrate, etc., it is surface-treated using a water-soluble flux. At this time, the water-soluble flux may penetrate into the glass film 50 from the interface between the first external electrode 61 and the glass film 50, and further into the element body 20.
[0052] Effects of the Embodiments (1) According to the above embodiment, the glass film 50 has a base portion 51 and a specific portion 52. The specific portion 52 contains silicon oxide and an oxide of a metal element. The content of the metal element in the specific portion 52 is lower than the content of the metal element in the base portion 51. Therefore, an interface between the base portion 51 and the specific portion 52 can be present in the glass film 50. If an interface is present in the glass film 50, even if water-soluble flux penetrates the glass film 50, the water-soluble flux will spread along the interface. Therefore, the penetrated water-soluble flux is less likely to penetrate deeper than the interface between the base portion 51 and the specific portion 52. This effectively prevents external erosion of the element body 20. As described above, according to the above embodiment, flux resistance can be improved without necessarily requiring the addition of silica powder.
[0053] (2) According to the above embodiment, the silicon content of the specific portion 52 is greater than the silicon content of the base portion 51. In this manner, the composition of the specific portion 52 is different from the composition of the base portion 51. Therefore, the interface between the base portion 51 and the specific portion 52 becomes clearer.
[0054] (3) According to the above embodiment, the metal element is barium, which is an alkaline earth metal. Barium is relatively easy to obtain among alkaline earth metals. Therefore, there is no need to prepare an element that is difficult to obtain.
[0055] (4) According to the above embodiment, the specific portion 52 contains zinc oxide. Therefore, the inclusion of zinc makes it easier to obtain a stable composition containing barium, an alkaline earth metal. (5) According to the above embodiment, the zinc content of the specific portion 52 is greater than the zinc content of the base portion 51. Therefore, the composition of the specific portion 52 is different from the composition of the base portion 51. Therefore, the interface between the base portion 51 and the specific portion 52 becomes clearer.
[0056] (6) According to the above embodiment, the first external electrode 61 includes the first metal layer 61B. Therefore, the electronic component 10 is likely to be used by being mounted on a substrate or the like by soldering. In other words, the electronic component 10 is likely to be exposed to water-soluble flux. Therefore, the effect of preventing the penetration of water-soluble flux is very significant.
[0057] (7) According to the above embodiment, the first metal layer 61B extends over a wider area than the first base electrode 61A. Therefore, a portion of the first metal layer 61B is also located on the surface of the glass film 50. Therefore, when the outer edge of the first metal layer 61B is located outside the outer edge of the first base electrode 61A, it is possible to prevent a gap from being formed between the first external electrode 61 and the glass film 50. Preventing such a gap from being formed makes it easier to prevent the intrusion of water-soluble flux between the first external electrode 61 and the glass film 50.
[0058] (Other Embodiments) The above embodiment can be modified as follows: The above embodiment and the following modifications can be combined and implemented within the scope of technical compatibility.
[0059] In the above embodiment, the electronic component 10 is not limited to a negative temperature coefficient thermistor component. For example, the electronic component 10 may be a thermistor component other than a negative temperature coefficient thermistor component, a multilayer capacitor component, or an inductor component, as long as it has some kind of wiring inside the element body 20.
[0060] The material of the element body 20 is not limited to the example of the above embodiment. The material of the element body 20 may be a composite body of resin and metal powder. The shape of the element body 20 is not limited to the example of the above embodiment. For example, the element body 20 may be a polygonal columnar shape other than a quadrangular columnar shape having a central axis CA. The element body 20 may also be the core of a wire-wound inductor component. For example, the core may have a so-called drum core shape. Specifically, the core may have a columnar winding core portion and flange portions provided at each end of the winding core portion.
[0061] The outer surface 21 of the element body 20 does not have to have boundary surfaces 23 and corner surfaces 24. For example, if the boundary between adjacent flat surfaces 22 on the outer surface 21 of the element body 20 is not chamfered, there is no curved surface at the boundary. Therefore, in such a case, the boundary surfaces 23 and corner surfaces 24 may not exist.
[0062] In the above embodiment, the shapes of the first internal electrodes 41 and the second internal electrodes 42 are not important as long as they can ensure electrical conduction with the corresponding first external electrodes 61 and second external electrodes 62. Furthermore, the number of first internal electrodes 41 and second internal electrodes 42 is not important, and the number of internal electrodes may be one, or three or more.
[0063] The configuration of the first external electrode 61 is not limited to the example of the above embodiment. For example, the first external electrode 61 may be composed of only the first base electrode 61A, or the first metal layer 61B may not have a two-layer structure. The same applies to the second external electrode 62.
[0064] In the above embodiment, the combination of materials for the first internal electrode 41 and the first base electrode 61A is not limited to a combination of copper on one side and silver and palladium on the other side. For example, combinations of palladium and silver, copper and nickel, copper and silver, copper and palladium, silver and gold, nickel and cobalt, or nickel and gold are also possible. Also, for example, a combination of copper on one side and copper and nickel on the other side may be used. Also, for example, a combination of nickel on one side and copper and nickel on the other side may be used. Also, for example, a combination of gold on one side and silver and palladium on the other side may be used.
[0065] Depending on the combination of the first internal electrode 41 and the first base electrode 61A, the Kirkendall effect may not be achieved. In this case, the first internal electrode 41 may be exposed prior to the external electrode formation process. For example, the first end surface 22A side of the element body 20 may be polished to physically remove a portion of the glass film 50. The base electrode formation process may then be performed to connect the first internal electrode 41 and the first base electrode 61A. Alternatively, for example, after forming the first base electrode 61A, the glass film 50 may be formed on the surface of the first base electrode 61A as well, and the glass film 50 covering the surface of the first base electrode 61A may then be removed. This also applies to the combination of materials for the second internal electrode 42 and the second base electrode 62A.
[0066] The location of the first external electrode 61 is not limited to the example in the above embodiment. For example, the first external electrode 61 may be disposed only on the first end surface 22A and one side surface 22C. The same applies to the second external electrode 62.
[0067] <Regarding the Glass Film> The glass film 50 does not have to cover the entire area of the outer surface 21 of the element body 20. The area covered by the glass film 50 may be changed as appropriate depending on the shape of the element body 20, the positions of the first external electrode 61 and the second external electrode 62, etc.
[0068] The metal element contained in the glass film 50 may be an alkali metal. The metal element contained in the glass film 50 may also be any of the alkali metals lithium, sodium, and potassium. Among alkali metals, lithium, sodium, and potassium are relatively easy to obtain. Therefore, there is no need to prepare an element that is difficult to obtain.
[0069] The metal element contained in the glass film 50 may be calcium, which is an alkaline earth metal. Alternatively, the metal contained in the glass film 50 may be another alkaline earth metal.
[0070] The specifying portion 52 may contain aluminum oxide. The specifying portion 52 may contain zinc oxide. The base portion 51 and the specifying portion 52 may contain additives of other elements. Depending on the content ratio of the other elements, the silicon content ratio of the specifying portion 52 may be equal to or lower than the silicon content ratio of the base portion 51.
[0071] The base portion 51 may not contain aluminum oxide. The base portion 51 may not contain zinc oxide. Furthermore, the zinc content of the specific portion 52 may be equal to or less than the zinc content of the base portion 51.
[0072] The material of the glass film 50 is not limited to the example of the above embodiment. For example, the glass is not limited to silicon dioxide, but may be a multi-component oxide containing Si, such as B-Si, Si-Zn, Zr-Si, or Al-Si oxides. Furthermore, the glass may be a multi-component oxide containing an alkali metal and Si, such as Al-Si, Na-Si, K-Si, or Li-Si oxides. Furthermore, the glass may be a multi-component oxide containing an alkaline earth metal and Si, such as Mg-Si, Ca-Si, Ba-Si, or Sr-Si. Furthermore, the glass may not contain Si, or may be a mixture thereof. If the material of the glass film 50 contains boron, the specific portion 52 may contain boron oxide. In this case, the base portion 51 may also contain boron oxide.
[0073] The material of the glass film 50 may contain, in addition to glass, a pigment, a silicone-based flame retardant, a surface treatment agent such as a silane coupling agent or a titanate coupling agent, or an antistatic agent.
[0074] More specifically, the glass film 50 may contain, in addition to glass, additives such as fine particles and nanoparticles of organic acid salts, oxides, inorganic salts, organic salts, and other metal oxides. Examples of organic acid salts include salts of oxoacids such as soda ash, sodium carbonate, sodium hydrogencarbonate, sodium percarbonate, sodium sulfite, sodium hydrogensulfite, sodium sulfate, sodium thiosulfate, sodium nitrate, and sodium sulfite, and halogen compounds such as sodium fluoride, sodium chloride, sodium bromide, and sodium iodide.
[0075] Examples of oxides include sodium peroxide, examples of hydroxides include sodium hydroxide, and examples of inorganic salts include sodium hydride, sodium sulfide, sodium hydrogen sulfide, sodium silicate, trisodium phosphate, sodium borate, sodium borohydride, sodium cyanide, sodium cyanate, and sodium tetrachloroaurate.
[0076] Examples of inorganic salts include calcium peroxide, calcium hydroxide, calcium fluoride, calcium chloride, calcium bromide, calcium iodide, calcium hydride, calcium carbide, and calcium phosphide.
[0077] The additive may be an oxoacid salt such as calcium carbonate, calcium bicarbonate, calcium nitrate, calcium sulfate, calcium sulfite, calcium silicate, calcium phosphate, calcium pyrophosphate, calcium hypochlorite, calcium chlorate, calcium perchlorate, calcium bromate, calcium iodate, calcium arsenite, calcium chromate, calcium tungstate, calcium molybdate, calcium magnesium carbonate, or hydroxyapatite. Examples of the additive include calcium acetate, calcium gluconate, calcium citrate, calcium malate, calcium lactate, calcium benzoate, calcium stearate, and calcium aspartate.
[0078] Furthermore, for example, the additive may be lithium carbonate, lithium chloride, lithium titanate, lithium nitride, lithium peroxide, lithium citrate, lithium fluoride, lithium hexafluorophosphate, lithium acetate, lithium iodide, lithium hypochlorite, lithium tetraborate, lithium bromide, lithium nitrate, lithium hydroxide, lithium aluminum hydride, lithium triethylborohydride, lithium hydride, lithium amide, lithium imide, lithium diisopropylamide, lithium tetramethylpiperidide, lithium sulfide, lithium sulfate, lithium thiophenolate, or lithium phenoxide.
[0079] Also for example, the additive may be boron triiodide, sodium cyanoborohydride, sodium borohydride, tetrafluoroboric acid, triethylborane, borax, or boric acid.
[0080] Further, for example, the additives include potassium arsenide, potassium bromide, potassium carbonate, potassium chloride, potassium fluoride, potassium hydride, potassium iodide, potassium triiodide, potassium azide, potassium nitride, potassium superoxide, potassium ozonate, potassium peroxide, potassium phosphide, potassium sulfide, potassium selenide, potassium telluride, potassium tetrafluoroaluminate, potassium tetrafluoroborate, potassium tetrahydroborate, potassium methanide, potassium cyanide, potassium formate, potassium hydrogen fluoride, tetramercury iodide ( Potassium tetrachloroplatinate (II), potassium hydrogen sulfide, potassium octachlorodimolybdate (II), potassium amide, potassium hydroxide, potassium hexafluorophosphate, potassium carbonate, potassium tetrachloroplatinate (II), potassium hexachloroplatinate (IV), potassium nonahydrido rhenate (VII), potassium sulfate, potassium acetate, potassium cyanideaurate (I), potassium hexanitrocobaltate (III), potassium hexacyanoferrate (III), potassium hexacyanoferrate (II), potassium methoxide, potassium ethoxide thoxide, potassium tert-butoxide, potassium cyanate, potassium fulminate, potassium thiocyanate, potassium aluminum sulfate, potassium aluminate, potassium arsenate, potassium bromate, potassium hypochlorite, potassium chlorite, potassium chlorate, potassium perchlorate, potassium carbonate, potassium chromate, potassium dichromate, potassium tetrakis(peroxo)chromate(V), potassium cuprate(III), potassium ferrate, potassium iodate, potassium periodate, potassium permanganate, potassium manganate, manganese hypochlorite The salt may be potassium phosphate, potassium molybdate, potassium nitrite, potassium nitrate, tripotassium phosphate, potassium perrhenate, potassium selenate, potassium silicate, potassium sulfite, potassium sulfate, potassium thiosulfate, potassium disulfite, potassium dithionate, potassium disulfate, potassium peroxodisulfate, potassium dihydrogen arsenate, dipotassium hydrogen arsenate, potassium hydrogen carbonate, potassium dihydrogen phosphate, dipotassium hydrogen phosphate, potassium hydrogen selenate, potassium hydrogen sulfite, potassium hydrogen sulfate, or potassium hydrogen peroxosulfate.
[0081] For example, the additive may be barium sulfite, barium chloride, barium chlorate, barium perchlorate, barium peroxide, barium chromate, barium acetate, barium cyanide, barium bromide, barium oxalate, barium nitrate, barium hydroxide, barium hydride, barium carbonate, barium iodide, barium sulfide, barium sulfate, or sodium acetate or sodium citrate.
[0082] The additive may also be fine particles or nanoparticles of a metal oxide, such as sodium oxide, calcium oxide, lithium oxide, boron oxide, potassium oxide, barium oxide, silicon oxide, titanium oxide, zirconium oxide, aluminum oxide, zinc oxide, and magnesium oxide.
[0083] The specific portion 52 is not limited to one layer. The number of specific portions 52 may be multiple. The shape of the specific portions 52 does not have to be layered. For example, in the modified example shown in FIG. 12 , the glass film 50 has multiple specific portions 52. When viewed in cross section on a plane perpendicular to the outer surface 21 of the element body 20, the major axis of each specific portion 52 is three or more times the minor axis. The major axis is the longest length of a line segment that passes through the geometric center of one specific portion 52 and can be drawn from outer edge to outer edge when viewed in cross section. The minor axis is the length of a line segment that passes through the geometric center of the same specific portion 52, is perpendicular to the major axis, and can be drawn from outer edge to outer edge when viewed in cross section. In other words, according to the modified example shown in FIG. 12 , the multiple specific portions 52 increase the number of interfaces between the base portion 51 and the specific portions 52. The major axis of each specific portion 52 is three or more times the minor axis, i.e., the specific portion 52 has a plate-like or needle-like shape when viewed in cross section. This makes it possible to make the path from the outside of the glass film 50 to the element body 20 through the base portion 51 more complex. Also, it is possible to increase the likelihood that more interfaces will be aligned in the direction perpendicular to the outer surface 21 of the element body 20.
[0084] In the method for manufacturing the electronic component 10, the metal alkoxide 85 may be, for example, sodium methoxide, sodium ethoxide, calcium diethoxide, lithium isopropoxide, lithium ethoxide, lithium tert-butoxide, lithium methoxide, boron alkoxide, potassium t-butoxide, tetraethyl orthosilicate, allyltrimethoxysilane, isobutyl(trimethoxy)silane, tetrapropyl orthosilicate, tetramethyl orthosilicate, [3-(diethylamino)propyl]trimethoxide, silane, triethoxy(octyl)silane, triethoxyvinylsilane, triethoxyphenylsilane, trimethoxyphenylsilane, trimethoxymethylsilane, butyltrichlorosilane, n-propyltriethoxysilane, methyltrichlorosilane, dimethoxy(methyl)octylsilane, dimethoxydimethylsilane, tris(tert-butoxy)silanol, tris(tert-pentoxy)silanol, hexadecyltrimethoxysilane, tris(1,2-benzenediolate-O,O')silane dipotassium orthosilicate, tetrabutyl orthosilicate, aluminum silicate, calcium silicate, tetramethylammonium silicate solution, titanium(IV) chloroisopropoxide, titanium(IV) isopropoxide, titanium(IV) 2-ethylhexyl oxide, titanium(IV) ethoxide, titanium(IV) butoxide, titanium(IV) tert-butoxide, titanium(IV) propoxide, titanium(IV) methoxide, zirconium(IV) bis(diethylcitrate)dipropoxide, zirconium(IV) dibutoxide oxide (bis-2,4-pentanedionate), zirconium(IV) 2-ethylhexanoate, zirconium(IV) isopropoxide isopropanol complex, zirconium(IV) ethoxide, zirconium(IV) butoxide, zirconium(IV) tert-butoxide, zirconium(IV) propoxide, aluminum tert-butoxide, aluminum isopropoxide, aluminum ethoxide, aluminum-tri-sec-butoxide, aluminum phenoxide.
[0085] In the manufacturing method of electronic component 10, metal alkoxide 85 may be replaced with a metal complex or acetate, which is a precursor of metal alkoxide 85. In this case, in metal alkoxide introduction step S17, a metal complex or acetate, which is a metal alkoxide precursor, may be introduced. Examples of metal complexes include acetylacetonates such as lithium acetylacetonate, titanium(IV) oxyacetylacetonate, titanium diisopropoxide bis(acetylacetonate), zirconium(IV) trifluoroacetylacetonate, zirconium(IV) acetylacetonate, aluminum acetylacetonate, aluminum(III) acetylacetonate, calcium(II) acetylacetonate, and zinc(II) acetylacetonate. Examples of acetates include zirconium acetate, zirconium(IV) hydroxide acetate, and basic aluminum acetate.
[0086] The method for manufacturing electronic component 10 is not limited to the example of the above embodiment. For example, solvent introduction step S13 may be performed after catalyst introduction step S14 or element introduction step S15. Furthermore, solvent 82 is not limited to 2-propanol. Solvent 82 may be changed as appropriate as long as it can sufficiently disperse metal alkoxide 85.
[0087] The technical concepts that can be derived from the above embodiments and modifications are described below. <1> An electronic component comprising: an element body, a glass film covering an outer surface of the element body, and an external electrode laminated on the outer surface of the glass film and having at least a base electrode, wherein the glass film has a base portion containing, in addition to silicon oxide, an oxide of one or more metal elements selected from alkali metals and alkaline earth metals, and a specific portion containing, in addition to silicon oxide, an oxide of the same metal element as in the base portion, and wherein the content of the metal element in the specific portion is lower than the content of the metal element in the base portion.
[0088] <2> The electronic component according to <1>, wherein the specific portion has a silicon content greater than the silicon content of the base portion.
[0089] <3> The electronic component according to <1> or <2>, wherein the metal element is any one of lithium, sodium, and potassium, which are alkali metals.
[0090] <4> The electronic component according to <1> or <2>, wherein the metal element is either calcium or barium, which are alkaline earth metals.
[0091] <5> The electronic component according to any one of <1> to <4>, wherein the specific portion contains an oxide of any one of zinc, boron, and aluminum.
[0092] <6> The electronic component according to <5>, wherein the base portion contains zinc oxide, the specific portion contains zinc oxide, and a zinc content in the specific portion is higher than a zinc content in the base portion.
[0093] <7> The electronic component according to any one of <1> to <6>, wherein the glass film has a plurality of the specific portions, and when viewed in cross section, a major axis is defined as the maximum length of a line segment that passes through a geometric center of the specific portion and can be drawn from outer edge to outer edge, and when a minor axis is defined as the length of a line segment that passes through a geometric center of the specific portion, is perpendicular to the major axis, and can be drawn from outer edge to outer edge, the major axis is three times or more of the minor axis.
[0094] <8> The electronic component according to any one of <1> to <7>, wherein the external electrodes further include a metal layer, and the metal layer is provided on a surface of the base electrode.
[0095] <9> The electronic component according to <8>, wherein a portion of the metal layer is located on a surface of the glass film.
[0096] REFERENCE SIGNS LIST 10... Electronic component 20... Body 21... Outer surface 50... Glass film 51... Base portion 52... Specific portion 61... First external electrode 61A... First base electrode 61B... First metal layer
Claims
1. The body and a glass film covering an outer surface of the element; an external electrode laminated on an outer surface of the glass film and having at least a base electrode; the glass film has a base portion including, in addition to silicon oxide, an oxide of one or more metal elements selected from alkali metals and alkaline earth metals, and a specific portion including, in addition to silicon oxide, an oxide of the same metal element as that in the base portion; The content ratio of the metal element in the specific portion is smaller than the content ratio of the metal element in the base portion. Electronic components.
2. The specific portion has a silicon content greater than the silicon content of the base portion. The electronic component according to claim 1 .
3. The metal element is any one of the alkali metals lithium, sodium, and potassium. The electronic component according to claim 1 .
4. The metal element is either calcium or barium, which is an alkaline earth metal. The electronic component according to claim 1 .
5. The specific portion contains an oxide of any one of zinc, boron, and aluminum. The electronic component according to claim 1 .
6. the base portion includes zinc oxide; The specific portion contains zinc oxide, The zinc content of the specific portion is greater than the zinc content of the base portion. The electronic component according to claim 5 .
7. The glass film has a plurality of the specific portions, When viewed in cross section, the longest length of a line segment that passes through the geometric center of the specific portion and can be drawn from one outer edge to the other is defined as the major axis; When viewed in cross section, the length of a line segment that passes through the geometric center of the specific portion, is perpendicular to the major axis, and can be drawn from one outer edge to the other outer edge is defined as the minor axis. The major axis is three times or more larger than the minor axis. The electronic component according to claim 1 .
8. The external electrode further includes a metal layer, The metal layer is provided on a surface of the base electrode. The electronic component according to claim 1 .
9. A portion of the metal layer is located on the surface of the glass film. The electronic component according to claim 8.