Secondary battery diagnostic method, secondary battery diagnostic program, and secondary battery diagnostic device
Patent Information
- Application Number
- JP2025512561
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-03
- Filing Date
- 2024-04-01
- Publication Date
- 2024-10-10
- Estimated Expiration
- 2044-04-01
AI Technical Summary
Existing secondary battery diagnostic methods cannot accurately evaluate the remaining life of lithium-ion batteries based solely on discharge capacity and internal resistance, as the number of usable cycles varies significantly even among batteries with similar characteristics.
A diagnostic method that estimates the electrolyte diffusion coefficient using trained models from input data such as rated capacity, discharge capacity, voltage drop, temperature rise, and electrode area, allowing for the determination of when a battery becomes unsuitable for reuse without disassembly, thereby providing a more accurate assessment of battery life.
This approach enables non-destructive, accurate evaluation of secondary battery life by estimating the electrolyte diffusion coefficient and threshold values, allowing for better prediction of battery longevity and cycle life.
Abstract
Description
Secondary battery diagnostic method, secondary battery diagnostic program, and secondary battery diagnostic device
[0001] The present invention relates to a diagnostic method for a secondary battery, a diagnostic program for a secondary battery, and a diagnostic device for a secondary battery.
[0002] The discharge capacity of secondary batteries such as lithium-ion batteries gradually decreases with repeated charging and discharging. Therefore, it is preferable to diagnose secondary batteries at appropriate times to evaluate their degree of deterioration and determine whether they can be reused or when they should be replaced. Furthermore, since secondary batteries can be reused after diagnosis, it is preferable that the diagnosis be performed non-destructively.
[0003] Japanese Patent Laid-Open Publication No. 2017-97997 describes a method for analyzing the characteristics of a secondary battery, which uses a model equation with the characteristic values of the components constituting the battery as parameters and fits the battery voltage value expressed by the model equation to actual measurement data to estimate the characteristic values of the components. This characteristic analysis method uses the actual measurement data obtained by applying to the battery being analyzed a charge / discharge pattern including an operating period consisting of either a constant current discharge period or a constant current charge period, and a rest period provided following the operating period.
[0004] The publication also describes characteristic values estimated by fitting to actual measurement data, such as the lithium ion diffusion coefficient in the positive electrode active material, the lithium ion diffusion coefficient in the negative electrode active material, the lithium ion diffusion coefficient in the electrolyte (electrolyte diffusion coefficient), the interfacial resistance in the positive electrode active material, the interfacial resistance in the negative electrode active material, and the lithium ion salt concentration in the electrolyte.
[0005] Japanese Patent Application Laid-Open No. 2017-97997
[0006] Conventionally, the degree of deterioration of a secondary battery has been evaluated based on the magnitude of discharge capacity and the magnitude of internal resistance at the time of diagnosis. However, according to research by the present inventors, even if the magnitude of discharge capacity and the magnitude of internal resistance at the time of diagnosis are similar, the number of times the secondary battery can be used thereafter is not necessarily the same. Specifically, even if the magnitude of discharge capacity and the magnitude of internal resistance at the time of diagnosis are similar, there are secondary batteries whose discharge capacity rapidly decreases after a small number of charge / discharge cycles, and those whose discharge capacity does not decrease significantly even after charge / discharge. Therefore, the remaining life of a secondary battery cannot be accurately evaluated simply by measuring the magnitude of discharge capacity and the magnitude of internal resistance at the time of diagnosis.
[0007] The aforementioned Japanese Patent Application Laid-Open No. 2017-97997 describes a method for estimating the characteristic values of components constituting a secondary battery without disassembling the secondary battery. This method estimates the characteristic values of the components constituting the secondary battery through simulation. This simulation requires a certain amount of time and requires proficiency in the software used for the simulation. Therefore, it is preferable to be able to estimate the characteristic values more easily. Furthermore, the publication does not describe a specific method for evaluating the remaining life of a secondary battery from these characteristic values.
[0008] An object of the present invention is to provide a diagnostic method, a diagnostic program, and a diagnostic device for a secondary battery that can easily estimate the electrolyte diffusion coefficient, which is one of the characteristic values (characteristic parameters) of a secondary battery, without disassembling the secondary battery. Another object of the present invention is to provide a diagnostic method, a diagnostic program, and a diagnostic device for a secondary battery that can evaluate the remaining life more accurately than conventional methods.
[0009] A method for diagnosing a secondary battery according to one embodiment of the present invention includes a step of estimating an electrolyte diffusion coefficient Dn of a secondary battery to be diagnosed at the time of diagnosis using a first trained model that estimates the electrolyte diffusion coefficient of the secondary battery from input data including the following (1) to (6): (1) the rated capacity (initial capacity) of the secondary battery; (2) the discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity; (3) the magnitude of the current in the measurements of the following (4) to (6); (4) the amount of voltage drop after a predetermined time has elapsed since the start of discharge (or the amount of voltage rise after a predetermined time has elapsed since the start of charging); (5) the amount of voltage drop at a predetermined SOC; and (6) the amount of temperature rise at a predetermined SOC.
[0010] A method for diagnosing a secondary battery according to one embodiment of the present invention includes a step of estimating the difference ΔD of a secondary battery to be diagnosed using a fifth trained model that estimates the difference ΔD between the electrolyte diffusion coefficient of the secondary battery and a threshold electrolyte diffusion coefficient, which is the value of the electrolyte diffusion coefficient at which the secondary battery becomes unsuitable for reuse, from input data including the following (1) to (8): (1) the rated capacity (initial capacity) of the secondary battery; (2) the discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity; (3) the magnitude of the current in the measurements of (4) to (6) below; (4) the amount of voltage drop after a predetermined time has elapsed since the start of discharge (or the amount of voltage rise after a predetermined time has elapsed since the start of charge); (5) the amount of voltage drop at a predetermined SOC; (6) the amount of temperature rise at a predetermined SOC; (7) the electrode area; and (8) the amount of positive electrode coating.
[0011] A diagnostic program for a secondary battery according to one embodiment of the present invention causes a computer to execute a step of estimating an electrolyte diffusion coefficient Dn of a secondary battery to be diagnosed at the time of diagnosis, using a first trained model that estimates the electrolyte diffusion coefficient of the secondary battery from input data including the following (1) to (6): (1) the rated capacity (initial capacity) of the secondary battery; (2) the discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity; (3) the magnitude of the current in the measurements of the following (4) to (6); (4) the amount of voltage drop after a predetermined time has elapsed since the start of discharge (or the amount of voltage rise after a predetermined time has elapsed since the start of charging); (5) the amount of voltage drop at a predetermined SOC; and (6) the amount of temperature rise at a predetermined SOC.
[0012] A diagnostic program for a secondary battery according to one embodiment of the present invention causes a computer to execute a step of estimating the difference ΔD of a secondary battery to be diagnosed using a fifth trained model that estimates the difference ΔD between the electrolyte diffusion coefficient of the secondary battery and a threshold electrolyte diffusion coefficient value that is the electrolyte diffusion coefficient value at which the secondary battery becomes unsuitable for reuse, from input data including the following (1) to (8): (1) the rated capacity (initial capacity) of the secondary battery; (2) the discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity; (3) the magnitude of the current in the measurements of (4) to (6) below; (4) the amount of voltage drop after a predetermined time has elapsed since the start of discharge (or the amount of voltage rise after a predetermined time has elapsed since the start of charging); (5) the amount of voltage drop at a predetermined SOC; (6) the amount of temperature rise at a predetermined SOC; (7) the electrode area; and (8) the amount of positive electrode coating.
[0013] A diagnostic device for a secondary battery according to one embodiment of the present invention includes an estimation device that estimates an electrolyte diffusion coefficient Dn of a secondary battery to be diagnosed at the time of diagnosis, using a first trained model that estimates the electrolyte diffusion coefficient of the secondary battery from input data including the following (1) to (6): (1) the rated capacity (initial capacity) of the secondary battery; (2) the discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity; (3) the magnitude of the current in the measurements of the following (4) to (6); (4) the amount of voltage drop after a predetermined time has elapsed since the start of discharge (or the amount of voltage rise after a predetermined time has elapsed since the start of charging); (5) the amount of voltage drop at a predetermined SOC; and (6) the amount of temperature rise at a predetermined SOC.
[0014] A diagnostic device for a secondary battery according to one embodiment of the present invention includes an estimation device that estimates the difference ΔD of a secondary battery to be diagnosed using a fifth trained model that estimates the difference ΔD between the electrolyte diffusion coefficient of the secondary battery and a threshold electrolyte diffusion coefficient, which is the value of the electrolyte diffusion coefficient at which the secondary battery becomes unsuitable for reuse, from input data including the following (1) to (8): (1) the rated capacity (initial capacity) of the secondary battery; (2) the discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity; (3) the magnitude of the current in the measurements of (4) to (6) below; (4) the amount of voltage drop after a predetermined time has elapsed since the start of discharge (or the amount of voltage rise after a predetermined time has elapsed since the start of charge); (5) the amount of voltage drop at a predetermined SOC; (6) the amount of temperature rise at a predetermined SOC; (7) the electrode area; and (8) the amount of positive electrode coating.
[0015] According to the present invention, the electrolyte diffusion coefficient can be easily estimated without disassembling the secondary battery, and the remaining life of the secondary battery can be evaluated more accurately than before.
[0016] FIG. 1 is a flow diagram of a secondary battery diagnostic method according to one embodiment of the present invention. FIG. 2 is a flow diagram showing an example of a more specific procedure for estimating characteristic parameters. FIG. 3 is a graph showing an example of the relationship between the electrolyte diffusion coefficient and discharge capacity. FIG. 4 is a diagram showing an example of how to determine the threshold value Dth. FIG. 5 is a flow diagram of a secondary battery diagnostic method according to a first embodiment of the present invention. FIG. 6 is a flow diagram of a secondary battery diagnostic method according to a second embodiment of the present invention. FIG. 7 is a flow diagram of a secondary battery diagnostic method according to a third embodiment of the present invention. FIG. 8 is a flow diagram of a secondary battery diagnostic method according to a fourth embodiment of the present invention. FIG. 9 is a diagram showing the relationship between ΔD obtained by diagnosis and the number of cycles before the onset of a sudden drop. FIG. 10 is a diagram showing the procedure of machine learning. FIG. 11 is a scatter plot in which the predicted value of the electrolyte diffusion coefficient threshold is plotted on the vertical axis and the true value (value obtained by analysis) is plotted on the horizontal axis for training data. FIG. 12 is a scatter plot in which the predicted value of the electrolyte diffusion coefficient threshold is plotted on the vertical axis and the true value (value obtained by analysis) is plotted on the horizontal axis for validation data. FIG. 13 is a scatter plot in which the predicted values of the electrolyte diffusion coefficient threshold are plotted on the vertical axis and the true values (values obtained by analysis) on the horizontal axis for the training data. FIG. 14 is a scatter plot in which the predicted values of the electrolyte diffusion coefficient threshold are plotted on the vertical axis and the true values (values obtained by analysis) on the horizontal axis for the validation data. FIG. 15 is a scatter plot in which the predicted values of electrolyte conductivity are plotted on the vertical axis and the true values (values obtained by analysis) on the horizontal axis for the training data. FIG. 16 is a scatter plot in which the predicted values of electrolyte conductivity are plotted on the vertical axis and the true values (values obtained by analysis) on the horizontal axis for the validation data. FIG. 17 is a scatter plot in which the predicted values of electrolyte diffusion coefficient are plotted on the vertical axis and the true values (values obtained by analysis) on the horizontal axis for the training data. FIG. 18 is a scatter plot in which the predicted values of electrolyte diffusion coefficient are plotted on the vertical axis and the true values (values obtained by analysis) on the horizontal axis for the validation data.
[0017] The present inventors previously developed a diagnostic method for secondary batteries that focuses on the electrolyte diffusion coefficient (PCT / JP2023 / 003516, WO2023 / 149532). In this diagnostic method, characteristic parameters (such as electrolyte diffusion coefficient Dn and electrolyte conductivity) of the secondary battery at the time of diagnosis are estimated based on a predetermined model formula and data obtained by measuring the load characteristics of the secondary battery. Next, the relationship between the electrolyte diffusion coefficient and discharge capacity is determined based on the model formula and the estimated parameters. Based on this "relationship between electrolyte diffusion coefficient and discharge capacity," the value of the electrolyte diffusion coefficient (threshold value) Dth at which the secondary battery becomes unsuitable for reuse is determined. The larger the difference ΔD = Dn - Dth between the electrolyte diffusion coefficient Dn at the time of diagnosis and the threshold value Dth, the more likely it is that the secondary battery to be diagnosed can be used for a long period of time (i.e., has a long remaining life).
[0018] In this secondary battery diagnostic method, in order to determine the threshold Dth, it is necessary to perform a simulation for each secondary battery to be diagnosed to determine the relationship between the electrolyte diffusion coefficient and the discharge capacity. This simulation takes a certain amount of time and requires proficiency in the software used for the simulation. Therefore, in order to more easily diagnose secondary batteries, it is preferable to be able to determine the threshold Dth without performing this simulation.
[0019] The present inventors have also conducted research on this point and developed a method for estimating the threshold Dth using an estimation model (PCT / JP2023 / 027999, WO 2024 / 029501). Specifically, first, the above-mentioned simulation was performed on a plurality of secondary batteries with different types of positive and negative electrode active materials, usage conditions, and degrees of deterioration, etc., to determine the threshold Dth. Furthermore, an estimation model (trained model) was constructed by machine learning using some of the characteristic parameters of the secondary battery as input data (explanatory variables) and the determined threshold Dth as output data (objective variable), and this was used to successfully estimate the threshold Dth of a secondary battery with an unknown threshold Dth. In this case, it was found that the accuracy of the estimation could be improved by including the discharge capacity and electrolyte conductivity of the secondary battery in the input data.
[0020] This method for diagnosing a secondary battery using a trained model can omit simulation when determining the threshold value Dth. However, simulation is required to estimate the electrolyte diffusion coefficient Dn at the time of diagnosis, and at least one simulation must be performed to calculate ΔD = Dn - Dth.
[0021] The inventors further pursued their research and succeeded in constructing a trained model that estimates the electrolyte diffusion coefficient Dn at the time of diagnosis from characteristic parameters that can be obtained without performing simulations (specifically, battery specification data and data that can be obtained by simple measurements). Similarly, they also succeeded in constructing a trained model that estimates the electrolyte conductivity at the time of diagnosis from characteristic parameters that can be obtained without performing simulations. This has made all simulation-based analysis unnecessary, making it possible to calculate ΔD = Dn - Dth from only battery specification data and data that can be obtained by simple measurements.
[0022] The present invention has been completed based on the above findings. Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings.
[0023] [Secondary Battery Diagnosis Method] In the following description, a method for determining ΔD without using an estimation model based on machine learning (hereinafter referred to as a "trained model") will first be described, followed by a method for determining ΔD using the trained model.
[0024] [Method for Determining ΔD Without Using a Trained Model] Figure 1 is a flow diagram of a secondary battery diagnostic method (without using a trained model) according to one embodiment of the present invention. This diagnostic method includes a step of estimating characteristic parameters of a secondary battery to be diagnosed (hereinafter referred to as the "target battery") at the time of diagnosis (step SA1), a step of determining the relationship between the electrolyte diffusion coefficient and the discharge capacity (step SA2), a step of determining a threshold value Dth for the electrolyte diffusion coefficient (step SA3), and a step of determining the difference ΔD between the threshold value Dth and the electrolyte diffusion coefficient Dn at the time of diagnosis (step SA4). Each step will be described in detail below.
[0025] [Step of Estimating Characteristic Parameters] The characteristic parameters of the target battery at the time of diagnosis are estimated (step SA1). More specifically, the characteristic parameters of the target battery at the time of diagnosis, including the electrolyte diffusion coefficient Dn of the target battery at the time of diagnosis, are estimated using a predetermined model formula based on data obtained by measuring the load characteristics of the target battery.
[0026] In this process, the characteristic parameters of the target battery at the time of diagnosis are estimated by fitting data obtained by measuring the load characteristics of the target battery using a predetermined model formula. This analysis (simulation) can be performed using a computer program capable of fluid analysis, such as the software Battery Design Studio manufactured by Siemens.
[0027] The model formula may be one well known in the art, such as the one described in Marc Doyle et al., "Modeling of Galvanostatic Charge and Discharge of the Lithium / Polymer / Insertion Cell," J. Electrochem. Soc., Vol. 140, No. 6, June (1993).
[0028] The target battery is, for example, a lithium ion battery.
[0029] The data obtained by measuring the load characteristics of the target battery may be, for example, a discharge curve obtained by measuring the target battery at multiple discharge rates. This data preferably includes a discharge curve measured at a very low discharge rate (e.g., 0.02 C). This data also preferably includes a discharge curve measured at a discharge rate of 1 C or higher. This data preferably includes discharge curves measured at three or more levels of discharge rate, and more preferably includes discharge curves measured at four or more levels of discharge rate. The data obtained by measuring the load characteristics of the target battery may also be a charge curve obtained by measuring the target battery at multiple charge rates.
[0030] The characteristic parameters estimated in this step (characteristic parameters at the time of diagnosis of the target battery) include at least the electrolyte diffusion coefficient Dn at the time of diagnosis of the target battery. The characteristic parameters may also include, for example, the solid phase diffusion coefficients of the positive and negative electrode active materials, the electrolyte conductivity, etc. Other specific examples of the characteristic parameters will be described later.
[0031] 2 is a flow diagram showing an example of a more specific procedure for the step of estimating the characteristic parameters (step SA1). In this example, the step of estimating the characteristic parameters (step SA1) includes a step of inputting the basic specifications of the target battery (step SA1-1), a step of inputting data obtained by measuring the load characteristics of the target battery (step SA1-2), a step of estimating the static parameters of the target battery (step SA1-3), and a step of estimating the dynamic parameters of the target battery (step SA1-4).
[0032] The basic specifications of the secondary battery to be diagnosed are input into the analysis software (step SA1-1). The basic specifications to be input are not limited to these, but may include, for example, the following: - Electrode composition of positive and negative electrodes (constituent materials, content, particle size, etc.) - Electrode thickness, density, and tortuosity of positive and negative electrodes (= approximately 1.5 in most cases) - Material, thickness, and electrical conductivity of positive and negative current collector foils - Thickness and porosity of separator - Composition of electrolyte (constituent materials, content) - Thermal conductivity and heat capacity of the above constituent materials (basic physical properties specific to the material) - Electrode area
[0033] Since the diagnosis is basically non-destructive, accurate information on the composition of the electrolyte at the time of diagnosis is not available. Therefore, general information on the secondary battery to be diagnosed (or specification information on a new battery) is obtained and input as a parameter. Although some values must be input when actually performing a simulation, the composition of the electrolyte itself does not have a significant impact on the results of the simulation. In the diagnosis method of this embodiment, the composition information on the electrolyte is only used as a reference.
[0034] The densities of the positive and negative electrodes are also expected to have changed due to expansion from the initial state, but accurate values cannot be measured at the time of diagnosis. Therefore, the initial values (standard values, etc.) or values predicted from the initial values are input. If the values are completely unknown, a general value may be input. If necessary, fine adjustments may be made in step SA1-4.
[0035] The data obtained by measuring the load characteristics of the target battery is input into the analysis software (step SA1-2). As described above, the data obtained by measuring the load characteristics of the target battery is a discharge curve obtained by measuring the target battery at multiple discharge rates. Hereinafter, the "data obtained by measuring the load characteristics of the target battery" may be referred to as "actual measurement data."
[0036] The static parameters of the target battery are estimated from the actual measurement data and the model formula (step SA1-3). For example, the static parameters of the target battery are adjusted to fit the shape of the discharge curve measured at a very low discharge rate. The discharge curve measured at a very low discharge rate (for example, 0.02 C) can be considered to roughly match the voltage curve (OCV curve) when no load is connected. The static parameters can include, but are not limited to, the following: Capacity per unit weight of the positive and negative electrode active materials (the discharge capacity of a battery decreases after use); Utilization rates of the positive and negative electrode active materials (they do not use the entire range of each other); Maximum and minimum voltages within the target battery's usage range.
[0037] The dynamic parameters of the target battery are estimated from the actual measurement data and the model formula (step SA1-4). For example, a simulation is performed in which the target battery is discharged at a current value equivalent to the measurement conditions of the actual measurement data, and the results of this simulation are compared with the actual measurement data to adjust the dynamic parameters so that the two match. This simulation can be performed, for example, using the discharge curve prediction function of Battery Design Studio mentioned above. The dynamic parameters can include, but are not limited to, the following: - Electrolyte conductivity - Electrolyte diffusion coefficient - Solid phase diffusion coefficient of positive and negative electrode active materials - Heat capacity of the target battery
[0038] It is preferable to set the environmental temperature during the simulation to match the environmental temperature when the actual measurement data was obtained. For medium-sized or larger product batteries, especially those expected to be used at high rates, it is preferable to consider the influence of heat generation. To this end, it is preferable to perform measurements at least at 1 C and perform fitting with the actual measurement data affected by heat generation. On the other hand, if the target battery is a small cell for desktop testing, it is not necessary to consider the influence of heat generation.
[0039] Through the above steps, it is possible to estimate the characteristic parameters of the target battery at the time of diagnosis, including the electrolyte diffusion coefficient Dn of the target battery at the time of diagnosis.
[0040] [Step of Determining the Relationship Between Electrolyte Diffusion Coefficient and Discharge Capacity] Based on the model formula used in step SA1 and the characteristic parameters estimated in step SA1, the relationship between the electrolyte diffusion coefficient and the discharge capacity is determined (step SA2). More specifically, among the characteristic parameters estimated in step SA1, a discharge simulation is performed while keeping the other characteristic parameters constant and varying only the electrolyte diffusion coefficient, thereby determining the discharge capacity. The discharge rate and environmental temperature during the discharge simulation are preferably set according to the intended reuse application. For example, if the intended application is one in which the battery will be used at an average rate of about 1 C, the discharge rate used to determine the relationship between the electrolyte diffusion coefficient and the discharge capacity is also 1 C. Since it is difficult to precisely match all environments, the simulation may be performed using average values.
[0041] 3 is a graph showing an example of the relationship between the electrolyte diffusion coefficient and the discharge capacity. In this example, the discharge capacity when the environmental temperature is 45° C. and the discharge rate is 0.5 C is calculated by dividing the discharge capacity by the electrolyte diffusion coefficient of 4.8×10 -6 , 4.0 × 10 -6 , 2.95 x 10 -6 , 1.85 × 10 -6 , 1.48 × 10 -6 , and 1.1 × 10 -6 cm 2 / sec.
[0042] As shown in this example, the smaller the electrolyte diffusion coefficient, the smaller the discharge capacity. Furthermore, the relationship between the electrolyte diffusion coefficient and the discharge capacity is not linear, but tends to show a curve in which the smaller the electrolyte diffusion coefficient, the greater the decrease in discharge capacity.
[0043] [Step of Determining the Threshold Dth of the Electrolyte Diffusion Coefficient] The threshold Dth of the electrolyte diffusion coefficient is determined based on the relationship between the electrolyte diffusion coefficient and the discharge capacity obtained in step SA2 (step SA3). More specifically, the value of the electrolyte diffusion coefficient at which the target battery becomes unsuitable for reuse is determined as the threshold Dth by referring to the relationship between the electrolyte diffusion coefficient and the discharge capacity obtained in step SA2. The circumstances under which a battery is determined to be "unsuitable for reuse" vary depending on the intended reuse application of the battery. Therefore, a criterion for determining that a battery is "unsuitable for reuse" is set according to the application.
[0044] For example, when the discharge capacity is equal to or less than a predetermined allowable value, the battery may be determined to be unsuitable for reuse. In this case, the electrolyte diffusion coefficient when the discharge capacity is equal to or less than the predetermined allowable value is determined as the threshold value Dth. For example, in the example of FIG. 3, if the allowable value of the discharge capacity is 36.02 mAh, the threshold value Dth is 1.40×10 -6 cm 2 / sec.
[0045] Alternatively, the battery may be determined to be unsuitable for reuse when the discharge capacity begins to drop sharply. In this case, the electrolyte diffusion coefficient when the discharge capacity begins to drop sharply is determined as the threshold Dth. For example, the electrolyte diffusion coefficient when the slope of the discharge capacity becomes equal to or greater than a predetermined magnitude may be set as the threshold Dth. Furthermore, as shown in FIG. 4, the point where the tangents to the curves before and after the start of the drop in discharge capacity intersect may be set as the threshold Dth.
[0046] [Step of Calculating the Difference ΔD Between the Threshold Value Dth and the Electrolyte Diffusion Coefficient Dn at the Time of Diagnosis] The difference ΔD between the threshold value Dth determined in step SA3 and the electrolyte diffusion coefficient Dn estimated in step SA1 at the time of diagnosis is calculated (step SA4). For example, Dn = 2.22 × 10 -6 cm 2 / sec, Dth = 1.40 × 10 -6 cm2 / sec, ΔD = Dn - Dth = 0.82 × 10 -6 cm 2 / sec.
[0047] This ΔD can be used as an index of the remaining life of the target battery. That is, the larger ΔD, the higher the possibility that the target battery can be used for a long period of time, and the smaller ΔD, the lower the possibility that the target battery can be used for a long period of time. Even if the discharge capacity at the time of diagnosis is approximately the same, ΔD may differ. By using ΔD, the remaining life of the target battery can be evaluated more accurately compared to the conventional method of evaluating the remaining life based on the magnitude of the discharge capacity at the time of diagnosis.
[0048] Note that the lifespan of a secondary battery varies greatly depending on the conditions of use, so "accurate evaluation of remaining life" does not necessarily mean predicting the specific number of charge / discharge cycles until the battery becomes unsuitable for reuse. However, if it is assumed that the target battery will continue to be used under certain conditions, it is also possible to predict the remaining lifespan (number of charge / discharge cycles) of the target battery from ΔD. For example, the relationship between ΔD and remaining lifespan may be measured in advance, and the remaining lifespan of the target battery may be predicted based on this relationship between ΔD and remaining lifespan.
[0049] [Method for Determining ΔD Using Trained Models] [First Embodiment] Fig. 5 is a flow diagram of a secondary battery diagnostic method according to a first embodiment of the present invention. This diagnostic method includes a step (step S1) of estimating the electrolyte diffusion coefficient Dn of the target battery at the time of diagnosis using a first trained model (hereinafter referred to as "trained model A"), a step (step S2) of estimating the threshold value Dth of the electrolyte diffusion coefficient of the target battery using a second trained model (hereinafter referred to as "trained model B"), and a step (step S3) of calculating the difference ΔD between the threshold value Dth and the electrolyte diffusion coefficient Dn at the time of diagnosis. The order of steps S1 and S2 may be reversed.
[0050] [Step of estimating electrolyte diffusion coefficient Dn using trained model A] The electrolyte diffusion coefficient Dn of the target battery at the time of diagnosis is estimated using trained model A (step S1). Trained model A is an estimation model that estimates the electrolyte diffusion coefficient Dn from predetermined input data.
[0051] Specifically, the input data of the trained model A preferably includes (1) the rated capacity (initial capacity) of the secondary battery, (2) the discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity, (3) the magnitude of the current, (4) the amount of voltage drop after a predetermined time has elapsed since the start of discharge (or the amount of voltage increase after a predetermined time has elapsed since the start of charging), (5) the amount of voltage drop at a predetermined SOC, and (6) the amount of temperature increase at a predetermined SOC.
[0052] The rated capacity in (1) above is the capacity of the secondary battery before degradation, i.e., the initial capacity. The rated capacity of a secondary battery is generally measured at a relatively low discharge rate, such as 0.2 C. The discharge capacity in (2) above is the capacity of the secondary battery after degradation, measured at a discharge rate equivalent to that used to measure the rated capacity. The discharge rate used in the measurement in (2) is a current value calculated based on the initial rated capacity.
[0053] The magnitude of the current in (3) above is the magnitude of the current when measuring (4) to (6). This magnitude of current may be set arbitrarily, but is preferably set to the magnitude of the current expected during use of the battery. The magnitude of the current in (3) above can be measured in a relatively short time, and is preferably set to the current at 0.5 C to 1.5 C, and more preferably set to the current at 0.8 C to 1.2 C, based on the initial capacity, as a standard current magnitude used.
[0054] The voltage drop amount after the predetermined time has elapsed (or the voltage increase amount after the predetermined time has elapsed from the start of charging) in (4) above can be obtained from charge data or discharge data (hereinafter referred to as "charge / discharge data"). This "predetermined time" can be determined arbitrarily, but it is preferably a short time (for example, 10 seconds or less) so that it does not take much time to obtain. The charge / discharge data can be substituted with the data used in the measurement in (2) above, but as described in the explanation of (3) above, it is preferable to use data measured at 0.5 to 1.5 C.
[0055] The voltage drop amount at the predetermined SOC in (5) above can also be obtained from the charge / discharge data described above. If the "predetermined SOC" is set to a value that is too small, it may become impossible to measure the secondary battery when it deteriorates. Therefore, the "predetermined SOC" is preferably set to an SOC of 40% to 60%, and more preferably to an SOC of 45% to 55%.
[0056] The temperature rise amount at the predetermined SOC in (6) above can be obtained from the charge / discharge data and the temperature of the secondary battery at that time. It is preferable that the "predetermined SOC" is the same as the SOC set in (5) above.
[0057] The input data of the trained model A may further include one or more selected from (7) the discharge capacity measured at the current of (3) above, (8) the electrode area, (9) the positive electrode mixture layer porosity (or the positive electrode mixture layer density), (10) the negative electrode mixture layer porosity (or the negative electrode mixture layer density), and (11) the heat capacity of the secondary battery.
[0058] The discharge capacity (7) above can be obtained from the charge / discharge data described above. The electrode area (8) above can be, for example, data at the time of manufacture held by the manufacturer. The porosity of the positive electrode mixture layer (9) above and the porosity of the negative electrode mixture layer (10) above can use data at the time of manufacture, or, since a reasonable expansion amount is generally known depending on the type of active material, the maximum value expected after degradation (or the minimum value when density is used) can be used. The heat capacity of the secondary battery (11) above needs to be determined by analysis, but a common value can be used before and after degradation for secondary batteries of the same type.
[0059] In summary, the input data of the trained model A preferably includes the following (1) to (6), and more preferably further includes one or more types selected from the following (7) to (11) in order to further reduce prediction errors. The input data of the trained model A may also include data other than these (e.g., positive electrode coating amount, positive electrode active material type, positive electrode mixture layer thickness, negative electrode coating amount, negative electrode active material type, negative electrode mixture layer thickness, separator thickness, etc.). (1) Rated capacity of the secondary battery (initial capacity) (2) Discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity (3) Current magnitude (4) Voltage drop amount after a predetermined time has elapsed since the start of discharge (or voltage rise amount after a predetermined time has elapsed since the start of charging) (5) Voltage drop amount at a predetermined SOC (6) Temperature rise amount at a predetermined SOC (7) Discharge capacity measured at the current in (3) above (8) Electrode area (9) Porosity of the positive electrode mixture layer (or density of the positive electrode mixture layer) (10) Porosity of the negative electrode mixture layer (or density of the negative electrode mixture layer) (11) Heat capacity of the secondary battery
[0060] The trained model A is obtained by performing machine learning using training data created in advance for a plurality of secondary batteries (hereinafter referred to as "training secondary batteries").
[0061] The training data is preferably created for a plurality of secondary batteries that differ in the type of positive and negative electrode active material, the conditions of use, the degree of deterioration, etc. The greater the number of training secondary batteries (i.e., the greater the amount of training data used in machine learning), the more accurate the trained model that can be obtained.
[0062] 1, a process similar to the process of estimating the characteristic parameters of the target battery at the time of diagnosis (step SA1) is performed for a plurality of learning secondary batteries to estimate the electrolyte diffusion coefficient Dn. This electrolyte diffusion coefficient Dn is used as output data to create training data.
[0063] Using the created training data, an estimation model (trained model) that estimates output data (objective variables) from input data (explanatory variables) is generated by machine learning. The machine learning algorithm is not particularly limited, but nonlinear support vector regression, for example, can be used.
[0064] [Step of estimating the threshold value Dth of the electrolyte diffusion coefficient using the trained model B] The threshold value Dth of the electrolyte diffusion coefficient is estimated (step S2) using the trained model B. The trained model B is an estimation model that estimates the threshold value Dth of the electrolyte diffusion coefficient from predetermined input data.
[0065] Specifically, the input data of the trained model B preferably includes (1) a discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity, (2) the electrolyte conductivity σ or the ohmic resistance converted per unit area of the electrode, (3) the electrode area, (4) the magnitude of the current, and (5) the amount of coating of the positive electrode. Note that the discharge rate during measurement in (1) is a current value calculated based on the initial rated capacity.
[0066] The above (1) "discharge capacity measured at a discharge rate equivalent to the measurement of the rated capacity" is the same as that described for trained model A.
[0067] The electrolyte conductivity σ in (2) above can be obtained by performing a process similar to the process (step SA1) of estimating the characteristic parameters of the target battery at the time of diagnosis, as described in FIG. 1. The ohmic resistance converted to a value per unit electrode area can be obtained by measuring the impedance of the secondary battery. While the ohmic resistance is easy to obtain, it may be less accurate than the electrolyte conductivity σ because it includes the resistance of the electrodes and the contact resistance of components such as tabs.
[0068] The above (3) and (4) are the same as those explained for trained model A. The magnitude of the current in (3) above can be set arbitrarily, but if the magnitude of the current is used as input data, it must be the same as the value used as input data for trained model A. The amount of positive electrode coating in (5) above can use data at the time of manufacture, etc.
[0069] The input data of the trained model B may further include one or more selected from (6) positive electrode active material species, (7) positive electrode mixture layer porosity (or positive electrode mixture layer density), (8) negative electrode mixture layer porosity (or negative electrode mixture layer density), and (9) heat capacity of the secondary battery.
[0070] The above (7) to (9) are the same as those explained in the trained model A. The positive electrode active material type in the above (6) can use data at the time of manufacture, etc.
[0071] In summary, the input data of the trained model B preferably includes the following (1) to (5), and more preferably further includes one or more selected from the following (6) to (9) in order to further reduce prediction errors. The input data of the trained model B may include data other than these. (1) Discharge capacity measured at a discharge rate equivalent to that measured for the rated capacity (2) Electrolyte conductivity σ or ohmic resistance converted per unit area of electrode (3) Electrode area (4) Current magnitude (5) Positive electrode coating amount (6) Positive electrode active material species (7) Porosity of the positive electrode mixture layer (or density of the positive electrode mixture layer) (8) Porosity of the negative electrode mixture layer (or density of the negative electrode mixture layer) (9) Heat capacity of the secondary battery
[0072] Like the trained model A, the trained model B is also obtained by machine learning using training data created in advance for multiple training secondary batteries. Specifically, the same steps as those described in FIG. 1 , namely, the step of estimating characteristic parameters of the target battery at the time of diagnosis (step SA1), the step of determining the relationship between the electrolyte diffusion coefficient and the discharge capacity (step SA2), and the step of determining the threshold value Dth of the electrolyte diffusion coefficient (step SA3), are performed for multiple training secondary batteries to determine the threshold value Dth of the electrolyte diffusion coefficient. Training data is created using this threshold value Dth of the electrolyte diffusion coefficient as output data. Using the created training data, an estimation model (trained model) that estimates output data (objective variable) from input data (explanatory variable) is generated by machine learning.
[0073] [Step of determining the difference ΔD between the threshold value Dth and the electrolyte diffusion coefficient Dn at the time of diagnosis] The difference ΔD = Dn - Dth between the threshold value Dth estimated in step S2 and the electrolyte diffusion coefficient Dn estimated in step S1 at the time of diagnosis is determined (step 3). This ΔD can be used as an index of the remaining life of the target battery. By using ΔD, the remaining life of the target battery can be evaluated more accurately than in the conventional method of evaluating the remaining life based on the magnitude of the discharge capacity at the time of diagnosis.
[0074] Furthermore, according to this embodiment, the electrolyte diffusion coefficient Dn at the time of diagnosis of the target battery can be determined without simulation analysis by using the trained model A. Furthermore, according to this embodiment, the threshold value Dth of the electrolyte diffusion coefficient can be easily determined by using the trained model B.
[0075] 6 is a flowchart of a diagnostic method for a secondary battery according to a second embodiment of the present invention. In addition to the steps of the diagnostic method according to the first embodiment (FIG. 5), this diagnostic method further includes a step (step S4) of estimating the electrolyte conductivity σ of the target battery at the time of diagnosis using a third trained model (hereinafter referred to as “trained model C”).
[0076] The trained model B described above includes the electrolyte conductivity σ or the ohmic resistance converted to a value per unit area of the electrode as input data. To determine the electrolyte conductivity σ at the time of diagnosis, a simulation analysis (step SA1 in FIG. 1) is required. Therefore, when the electrolyte conductivity σ is used as input data, the simulation analysis at the time of diagnosis cannot be completely omitted in the diagnostic method according to the first embodiment ( FIG. 5 ). The ohmic resistance can be determined without the simulation analysis, but the accuracy may be inferior compared to when the electrolyte conductivity σ is used.
[0077] In this embodiment, the electrolyte conductivity σ of the target battery at the time of diagnosis is estimated (step S4) using the trained model C. This makes it possible to omit analysis by simulation at the time of diagnosis while maintaining the accuracy of the estimation.
[0078] Trained model C is an estimation model that estimates the electrolyte conductivity σ from specified input data. The input data for trained model C preferably includes, specifically, (1) a discharge capacity measured at a discharge rate equivalent to the measurement of the rated capacity, (2) the magnitude of the current, (3) the amount of voltage drop after a predetermined time has elapsed since the start of discharge (or the amount of voltage increase after a predetermined time has elapsed since the start of charging), (4) the electrode area, and (5) the amount of positive electrode coating. These are the same as those described for trained model A and trained model B. Note that the discharge rate (1) above is a current value calculated based on the initial rated capacity, and the magnitude of the current (2) above needs to be the same as the value used as the input data for trained model A.
[0079] The input data of the trained model C may further include one or more selected from (6) positive electrode active material species, (7) positive electrode mixture layer porosity (or positive electrode mixture layer density), (8) negative electrode active material species, and (9) negative electrode mixture layer porosity (or negative electrode mixture layer density).
[0080] The above (6) to (7) and (9) are the same as those explained in the trained model B. The negative electrode active material type in the above (8) can use data at the time of manufacture, etc.
[0081] In summary, the input data of the trained model C preferably includes the following (1) to (5), and more preferably further includes one or more selected from the following (6) to (9) in order to further reduce prediction errors. The input data of the trained model C may include data other than these. (1) Discharge capacity measured at a discharge rate equivalent to that measured for the rated capacity (2) Current magnitude (3) Amount of voltage drop after a predetermined time has elapsed since the start of discharge (or amount of voltage increase after a predetermined time has elapsed since the start of charging) (4) Electrode area (5) Positive electrode coating amount (6) Positive electrode active material species (7) Porosity of the positive electrode mixture layer (or density of the positive electrode mixture layer) (8) Negative electrode active material species (9) Porosity of the negative electrode mixture layer (or density of the negative electrode mixture layer)
[0082] Like trained model A, trained model C is obtained by machine learning using training data created in advance for multiple training secondary batteries. Specifically, a process similar to the process of estimating the characteristic parameters of the target battery at the time of diagnosis (step SA1), described in FIG. 1, is performed for multiple training secondary batteries to estimate the electrolyte conductivity σ. Training data is created using this electrolyte conductivity σ as output data. Using the created training data, an estimation model (trained model) that estimates output data (objective variable) from input data (explanatory variable) is generated by machine learning.
[0083] 7 is a flowchart of a diagnostic method for a secondary battery according to a third embodiment of the present invention. This diagnostic method includes a step (step S5) of estimating a threshold value Dth of the electrolyte diffusion coefficient using a fourth trained model (hereinafter referred to as "trained model D"), instead of step S2 of the diagnostic method according to the first embodiment (FIG. 5).
[0084] In the diagnostic method according to the second embodiment described above ( FIG. 6 ), the electrolyte conductivity σ is estimated using the trained model C, and then this electrolyte conductivity σ is used as part of the input data to estimate the threshold Dth of the electrolyte diffusion coefficient using the trained model B. In contrast, in the diagnostic method according to this embodiment, the threshold Dth of the electrolyte diffusion coefficient is estimated directly from predetermined input data using the trained model D without going through the process of estimating the electrolyte conductivity σ.
[0085] The trained model D is an estimation model that estimates the threshold value Dth of the electrolyte diffusion coefficient from predetermined input data. The input data of the trained model D is the union of the input data of the trained model C and the input data of the trained model B excluding the electrolyte conductivity σ.
[0086] That is, the input data of the trained model D preferably includes the following (1) to (5), and more preferably further includes one or more selected from the following (6) to (10) in order to further reduce prediction errors. The input data of the trained model D may include data other than these. (1) Discharge capacity measured at a discharge rate equivalent to that measured for the rated capacity (2) Current magnitude (3) Amount of voltage drop after a predetermined time has elapsed since the start of discharge (or amount of voltage increase after a predetermined time has elapsed since the start of charge) (4) Electrode area (5) Positive electrode coating amount (6) Positive electrode active material species (7) Porosity of the positive electrode mixture layer (or density of the positive electrode mixture layer) (8) Negative electrode active material species (9) Porosity of the negative electrode mixture layer (or density of the negative electrode mixture layer) (10) Heat capacity of the secondary battery
[0087] According to this embodiment, it is also possible to omit the analysis by simulation at the time of diagnosis while maintaining the accuracy of estimation.
[0088] 8 is a flowchart of a method for diagnosing a secondary battery according to a fourth embodiment of the present invention. This method includes a step (step S6) of estimating ΔD = Dn - Dth using a fifth trained model (hereinafter referred to as "trained model E").
[0089] In the diagnostic methods according to the first to third embodiments described above, the electrolyte diffusion coefficient Dn and the electrolyte diffusion coefficient threshold Dth at the time of diagnosis of the target battery are estimated, and ΔD = Dn - Dth is calculated from the difference between them. In contrast, in the diagnostic method according to this embodiment, ΔD = Dn - Dth is estimated directly from predetermined input data using the trained model E.
[0090] Trained model E is an estimation model that estimates ΔD = Dn - Dth from predetermined input data. The input data of trained model E is the union of the input data of trained model A and the input data of trained model D.
[0091] That is, the input data of the trained model E preferably includes the following (1) to (8), and may further include one or more types selected from the following (9) to (14). The input data of the trained model E may include data other than these. (1) Rated capacity (initial capacity) of the secondary battery (2) Discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity (3) Current magnitude (4) Amount of voltage drop after a predetermined time has elapsed since the start of discharge (or amount of voltage increase after a predetermined time has elapsed since the start of charge) (5) Amount of voltage drop at a predetermined SOC (6) Amount of temperature increase at a predetermined SOC (7) Electrode area (8) Positive electrode coating amount (9) Discharge capacity measured at the current of (3) above (10) Positive electrode active material species (11) Porosity of the positive electrode mixture layer (or density of the positive electrode mixture layer) (12) Negative electrode active material species (13) Porosity of the negative electrode mixture layer (or density of the negative electrode mixture layer) (14) Heat capacity of the secondary battery
[0092] According to this embodiment, it is also possible to omit the analysis by simulation at the time of diagnosis while maintaining the accuracy of estimation.
[0093] [Diagnostic Program for Secondary Battery, etc.] The above-described method for diagnosing a secondary battery can also be realized as a computer program. A diagnostic program for a secondary battery according to one embodiment of the present invention causes a computer to execute a step of estimating the electrolyte diffusion coefficient Dn of a secondary battery to be diagnosed at the time of diagnosis, using a trained model A. A diagnostic program for a secondary battery according to another embodiment of the present invention causes a computer to execute a step of estimating ΔD of a secondary battery to be diagnosed, using a trained model E. These computer programs may be recorded on a computer-readable recording medium.
[0094] The above-described secondary battery diagnostic method can also be realized as a computer system. A secondary battery diagnostic system according to one embodiment of the present invention includes a memory and a processor, and the processor executes a step of estimating the electrolyte diffusion coefficient Dn of the secondary battery to be diagnosed at the time of diagnosis using a trained model A in accordance with a program stored in the memory. A secondary battery diagnostic system according to another embodiment of the present invention includes a memory and a processor, and the processor executes a step of estimating ΔD of the secondary battery to be diagnosed using a trained model E in accordance with a program stored in the memory.
[0095] A secondary battery diagnostic device according to one embodiment of the present invention includes an estimation device that estimates the electrolyte diffusion coefficient Dn of the secondary battery to be diagnosed at the time of diagnosis using a trained model A. A secondary battery diagnostic device according to another embodiment of the present invention includes an estimation device that estimates ΔD of the secondary battery to be diagnosed using a trained model E.
[0096] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.
[0097] A plurality of medium-sized laminated cells with a rated capacity of 5 Ah and a plurality of small-sized laminated cells with a rated capacity of 36 mAh were fabricated.
[0098] [Medium-sized laminated cell] <Preparation of positive electrode> LiCoO 2 A positive electrode mixture-containing slurry was prepared by uniformly mixing 93 parts by mass of aluminum foil, 3 parts by mass of carbon black as a conductive additive, and 4 parts by mass of PVDF as a binder using NMP as a solvent. The positive electrode mixture-containing slurry was applied to both sides of a positive electrode current collector made of aluminum foil with a thickness of 15 μm, dried, and then pressure-molded using a roller press. A positive electrode was fabricated by punching out a portion of the positive electrode current collector that was not coated with the positive electrode mixture-containing slurry to form a tab portion.
[0099] <Preparation of Negative Electrode> 97.5 parts by mass of graphite as a negative electrode active material, 1.5 parts by mass of carboxymethyl cellulose as a binder, and 1 part by mass of styrene-butadiene rubber were mixed, and an appropriate amount of water was added and thoroughly mixed to prepare a negative electrode mixture-containing slurry. This negative electrode mixture-containing slurry was applied to both sides of a negative electrode current collector made of copper foil with a thickness of 10 μm, dried, and then pressure-molded using a roller press. A negative electrode was prepared by punching out a portion of the negative electrode current collector that was not coated with the negative electrode mixture-containing slurry to form a tab portion.
[0100] <Preparation of Battery> Seven of the positive electrodes and eight of the negative electrodes were alternately stacked with an 18 μm-thick polyolefin microporous film separator having a three-layer structure including a polyethylene layer as an intermediate layer and two polypropylene layers as outer layers interposed therebetween to form a laminated electrode body.
[0101] Next, the positive electrode tabs of the laminated electrode body and the negative electrode tabs are welded together, and leads are connected to each of them. Then, LiPF is placed in a solution of ethylene carbonate, diethyl carbonate, and methyl ethyl carbonate mixed in a volume ratio of 1:1:1. 6 to a concentration of 1 mol / L, and then vinylene carbonate was further dissolved in an amount of 1 mass % to prepare a nonaqueous electrolyte solution, which was then sealed in an exterior body made of an aluminum laminate film to prepare a nonaqueous electrolyte secondary battery with a rated capacity of 5 Ah.
[0102] [Small laminated cell] <Preparation of positive electrode> LiCoO 2 A positive electrode mixture-containing slurry was prepared by uniformly mixing 94 parts by mass of aluminum foil, 4 parts by mass of carbon black as a conductive additive, and 2 parts by mass of PVDF as a binder using NMP as a solvent. The positive electrode mixture-containing slurry was applied to both sides of a positive electrode current collector made of aluminum foil with a thickness of 15 μm, dried, and then pressure-molded using a roller press. A positive electrode was fabricated by punching out a portion of the positive electrode current collector that was not coated with the positive electrode mixture-containing slurry to form a tab portion.
[0103] <Preparation of negative electrode> 94.5 parts by mass of graphite as a negative electrode active material and 3 parts by mass of SiO particles (D50: 5.0 μm) whose surfaces are coated with carbon were mixed with 1.5 parts by mass of carboxymethyl cellulose as a binder and 1 part by mass of styrene butadiene rubber, and an appropriate amount of water was added and mixed thoroughly to prepare a negative electrode mixture-containing slurry. This negative electrode mixture-containing slurry was applied to both sides of a negative electrode current collector made of copper foil with a thickness of 10 μm, dried, and then pressure-molded using a roller press. A negative electrode was prepared by punching out a portion of the negative electrode current collector that was not coated with the negative electrode mixture-containing slurry to form a tab portion.
[0104] <Fabrication of Battery> The positive electrode and the negative electrode were laminated via a 12 μm-thick polyolefin microporous film separator having a three-layer structure including a polyethylene layer as an intermediate layer and two polypropylene layers as outer layers, to form a laminated electrode body.
[0105] Next, the positive electrode tabs of the laminated electrode body are welded together, and the negative electrode tabs are welded together, and leads are connected to each of them. Then, LiPF is placed in a solution of ethylene carbonate and diethyl carbonate mixed in a volume ratio of 3:7. 6 to a concentration of 1 mol / L, and then vinylene carbonate was further dissolved in an amount of 1 mass % to prepare a nonaqueous electrolyte solution, which was then sealed in an exterior body made of an aluminum laminate film to produce a nonaqueous electrolyte secondary battery with a rated capacity of 36 mAh.
[0106] [Preparation of Degraded Cells] A charge-discharge cycle test was performed on a medium-sized laminated cell with a rated capacity of 5 Ah under multiple conditions, including different charge-discharge rates and ambient temperatures, to produce multiple degraded cells whose discharge capacity had dropped to 4.8 Ah. Similarly, a charge-discharge cycle test was performed on a small-sized laminated cell with a rated capacity of 36 mAh under multiple conditions, including different charge-discharge rates and ambient temperatures, to produce multiple degraded cells whose discharge capacity had dropped to 35 mAh.
[0107] [Measurement of Load Characteristics] The load characteristics of these deteriorated cells were measured. Specifically, discharge curves were measured at discharge rates of 0.02C, 0.2C, 0.5C, and 1C.
[0108] [Diagnosis of Secondary Battery] The secondary battery diagnosis method described in the embodiment was carried out using these deteriorated cells as target batteries. The analysis (simulation) was carried out using the software Battery Design Studio manufactured by Siemens. Among the basic specifications, the solvent ratio and salt concentration were input with the same values as at the time of production (because the values at the time of diagnosis could not be measured).
[0109] After estimating the characteristic parameters at the time of diagnosis, the discharge capacity was calculated at an ambient temperature of 45°C and a discharge rate of 0.5C while changing the electrolyte diffusion coefficient based on the estimated characteristic parameters, and the relationship between the electrolyte diffusion coefficient and the discharge capacity was obtained. The point where the tangents to each curve before and after the discharge capacity started to drop sharply intersect was defined as a threshold Dth, and the difference ΔD between the threshold Dth and the electrolyte diffusion coefficient Dn at the time of diagnosis was calculated.
[0110] [Measurement of remaining life] These deteriorated cells were subjected to charge-discharge cycle tests under the same conditions, and the number of charge-discharge cycles until the discharge capacity suddenly dropped (number of cycles until the sudden drop started) was measured. The relationship between ΔD obtained by the diagnosis and the number of cycles until the sudden drop started is shown in Figure 9.
[0111] As shown in Figure 9, even when the discharge capacity at the time of diagnosis was the same (4.8 Ah or 35 mAh), differences in ΔD were observed. It was also found that the number of cycles at which the rapid drop began changed depending on ΔD, confirming the validity of this diagnostic method.
[0112] [Generation of Trained Model B] Next, secondary batteries were prepared using LCO or NCM as the positive electrode active material and graphite or SiO as the negative electrode active material. The load characteristics of these secondary batteries were measured, and the threshold electrolyte diffusion coefficient was determined using the method described above. These data were used as training data (however, some data was used as validation data rather than training data), and machine learning was performed to generate a trained model (trained model B).
[0113] The following nine variables were used as input data (explanatory variables): (1) Discharge capacity measured at a discharge rate (0.2 C) equivalent to that used to measure the rated capacity; (2) Electrolyte conductivity σ; (3) Electrode area; (4) Current magnitude; (5) Amount of positive electrode coating; (6) Type of positive electrode active material; (7) Porosity of positive electrode mixture layer; (8) Porosity of negative electrode mixture layer; (9) Heat capacity of secondary battery.
[0114] Machine learning was performed using the open source library scikit-learn. The machine learning procedure is shown in Figure 10. The machine learning algorithm used was nonlinear support vector regression (nonlinear SVR).
[0115] First, all data were normalized using the following formula: Xn = (X - Xa) / Xd, where X is the original value, Xn is the normalized value, Xa is the average value of the variable X, and Xd is the standard deviation.
[0116] In the nonlinear SVR, the weighting coefficient w was determined so that the following function was minimized: φ(x): parameter after nonlinear mapping of the original x, w: weighting coefficient for each parameter, c: constant, y: objective variable (threshold value of the electrolyte diffusion coefficient)
[0117] h(y (i) -f(x (i) )) is a function expressed by the following formula: (i) -f(x (i) ))=max(0, |y (i) -f(x (i) ) |−ε) C and ε are so-called hyperparameters.
[0118] 11 and 12 are scatter plots in which the predicted values of the electrolyte diffusion coefficient threshold are plotted on the vertical axis and the true values (values obtained by analysis) are plotted on the horizontal axis. Fig. 11 is for training data (100 data sets used), and Fig. 12 is for validation data (data not used for learning). As shown in Fig. 12, the values obtained by analysis can be predicted with good accuracy even for unlearned data.
[0119] <Contribution of Electrolyte Conductivity to Dth> Using a trained model, the influence of electrolyte conductivity on Dth was examined.
[0120] For a certain secondary battery, if the electrolyte conductivity is reduced from 8.90 (mS / cm) to 1.75 (mS / cm) without changing other parameters, Dth becomes 2.705×10 -6 (cm 2 / sec) to 2.758 × 10 -6 (cm 2 / sec).
[0121] For the same secondary battery, if the heat capacity is halved without changing the electrolyte conductivity, Dth becomes 2.705 × 10 -6 (cm 2 / sec) to 2.643 × 10 -6 (cm 2 / sec).
[0122] Next, consider the case where the heat capacity is halved and the electrolyte conductivity is reduced to 1.75 (mS / cm). From the above results, Dth is 2.643 × 10 -6 (cm 2 / sec), which is expected to increase as the electrolyte conductivity decreases. However, according to the results of the trained model, Dth is 2.643 × 10 -6 (cm 2 / sec) to 2.575 × 10 -6 (cm 2 / sec).
[0123] As described above, the influence of the electrolyte conductivity on Dth is not constant depending on the amount of change in other parameters, and there is a correlation between the parameters. Therefore, it is clear that it is difficult to simply predict.
[0124] For comparison, machine learning was performed excluding electrolyte conductivity from the input data (explanatory variables), and a trained model was created. Figures 13 and 14 are scatter plots with the predicted value of the "electrolyte diffusion coefficient threshold" on the vertical axis and the true value (value obtained by analysis) on the horizontal axis. Figure 13 is for training data, and Figure 14 is for validation data (data not used for learning). As shown in Figure 14, this trained model had inferior prediction accuracy compared to the results of a trained model (Figure 12) that included electrolyte conductivity in the input data.
[0125] This shows that the accuracy of prediction can be improved by including the electrolyte conductivity in the input data.
[0126] [Estimation of Electrolyte Conductivity] Secondary batteries using LCO or NCM as the positive electrode active material and graphite or SiO as the negative electrode active material were prepared. The load characteristics of these secondary batteries were measured, and the electrolyte conductivity was estimated by performing simulation analysis. Using this data as training data, machine learning similar to that used to generate the trained model for estimating the threshold Dth was performed to generate a trained model (trained model C) for estimating the electrolyte conductivity. The following nine variables were used as input data (explanatory variables): (1) Discharge capacity measured at a discharge rate (0.2 C) equivalent to the measurement of the rated capacity; (2) Current magnitude; (3) Amount of voltage drop 1 second after the start of discharge; (4) Electrode area; (5) Amount of positive electrode coating; (6) Type of positive electrode active material; (7) Porosity of the positive electrode mixture layer; (8) Type of negative electrode active material; and (9) Porosity of the negative electrode mixture layer.
[0127] 15 and 16 are scatter plots with predicted values of electrolyte conductivity σ plotted on the vertical axis and true values (values obtained by analysis) plotted on the horizontal axis. FIG. 15 is for training data, and FIG. 16 is for validation data. As shown in FIG. 16, the values obtained by analysis can be predicted with generally good accuracy even for unlearned data. It is expected that accuracy will improve by further accumulating training data.
[0128] [Estimation of Electrolyte Diffusion Coefficient] Secondary batteries were prepared using LCO or NCM as the positive electrode active material and graphite or SiO as the negative electrode active material. The load characteristics of these secondary batteries were measured and analyzed by simulation to estimate the electrolyte diffusion coefficient. Using this data as training data, machine learning was performed in the same way as in the case of generating the trained model for estimating the threshold Dth, and a trained model (trained model A) for estimating the electrolyte diffusion coefficient was generated. The following 11 variables were used as input data (explanatory variables). (1) Rated capacity of the secondary battery (initial capacity) (2) Discharge capacity measured at a discharge rate (0.2C) equivalent to that used to measure the rated capacity (3) Current magnitude (1C) (4) Voltage drop 1 second after the start of discharge (5) Voltage drop at SOC 50% (6) Temperature rise at SOC 50% (7) Discharge capacity measured at the current in (3) above (8) Electrode area (9) Positive electrode mixture layer density (10) Negative electrode mixture layer density (11) Heat capacity of the secondary battery
[0129] 17 and 18 are scatter plots in which the predicted values of the electrolyte diffusion coefficient Dn are plotted on the vertical axis and the true values (values obtained by analysis) are plotted on the horizontal axis. FIG. 17 is for the training data, and FIG. 18 is for the validation data. As shown in FIG. 18, the values obtained by analysis can be predicted with generally good accuracy even for unlearned data. It is expected that accuracy will improve by further accumulating training data.
[0130] Although the embodiments of the present invention have been described above, the present invention is not limited to the above-described embodiments and various modifications are possible within the scope of the invention. For example, in the above-described embodiments, the secondary battery is a single cell, but if the secondary battery is a battery pack, the present invention can be applied not only to each individual cell but also to the entire battery pack as a single battery.
Claims
1. A method for diagnosing a secondary battery, comprising a step of estimating an electrolyte diffusion coefficient Dn of a secondary battery to be diagnosed at the time of diagnosis, using a first trained model that estimates the electrolyte diffusion coefficient of the secondary battery from input data including the following (1) to (6): (1) The rated capacity (initial capacity) of the secondary battery (2) A discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity (3) The magnitude of the current in the measurements of the following (4) to (6) (4) The amount of voltage drop after a predetermined time has elapsed since the start of discharging (or the amount of voltage rise after a predetermined time has elapsed since the start of charging) (5) The amount of voltage drop at a predetermined SOC (6) The amount of temperature rise at a predetermined SOC 2. The method for diagnosing a secondary battery according to claim 1, wherein the input data for the first trained model further includes one or more of the following selected from (7) to (11): (7) Discharge capacity measured at the current of (3) (8) Electrode area (9) Positive electrode mixture layer porosity (or positive electrode mixture layer density) (10) Negative electrode mixture layer porosity (or negative electrode mixture layer density) (11) Heat capacity of the secondary battery 3. A method for diagnosing a secondary battery as described in claim 1 or 2, further comprising the steps of: estimating a threshold electrolyte diffusion coefficient Dth of the secondary battery to be diagnosed using a second trained model that estimates, from predetermined input data, a threshold electrolyte diffusion coefficient which is the value of the electrolyte diffusion coefficient at which the secondary battery becomes unsuitable for reuse; and determining a difference ΔD between the threshold electrolyte diffusion coefficient Dth and the electrolyte diffusion coefficient Dn at the time of diagnosis.
4. A method for diagnosing a secondary battery according to claim 3, wherein the input data of the second trained model includes the following (1) to (5): (1) Discharge capacity measured at a discharge rate equivalent to the measurement of the rated capacity; (2) Electrolyte conductivity σ or ohmic resistance converted per unit area of electrode; (3) Electrode area; (4) The same current magnitude as (3) of the input data of the first trained model; and (5) Amount of coating on the positive electrode.
5. A method for diagnosing a secondary battery as described in claim 4, further comprising a step of estimating the electrolyte conductivity σ of the secondary battery to be diagnosed using a third trained model that estimates the electrolyte conductivity of the secondary battery from specified input data.
6. A method for diagnosing a secondary battery according to claim 5, wherein the input data of the third trained model includes the following (1) to (5): (1) a discharge capacity measured at a discharge rate equivalent to the measurement of the rated capacity; (2) a magnitude of a current the same as that of (3) of the input data of the first trained model; (3) a voltage drop amount after a predetermined time has elapsed since the start of discharging (or a voltage rise amount after a predetermined time has elapsed since the start of charging); (4) an electrode area; and (5) a positive electrode coating amount.
7. A method for diagnosing a secondary battery according to claim 1 or 2, further comprising the steps of: estimating a threshold electrolyte diffusion coefficient Dth of the secondary battery to be diagnosed using a fourth trained model that estimates, from predetermined input data, a threshold electrolyte diffusion coefficient, which is the value of the electrolyte diffusion coefficient when the secondary battery becomes unsuitable for reuse; and calculating a difference ΔD between the threshold electrolyte diffusion coefficient Dth and the electrolyte diffusion coefficient Dn at the time of diagnosis, wherein the input data of the fourth trained model includes the following (1) to (5): (1) Discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity; (2) The same magnitude of current as that of (3) in the input data of the first trained model; (3) Amount of voltage drop after a predetermined time has elapsed since the start of discharge (or amount of voltage rise after a predetermined time has elapsed since the start of charging); (4) Electrode area; and (5) Amount of positive electrode coating.
8. A method for diagnosing a secondary battery, comprising a step of estimating ΔD of a secondary battery to be diagnosed using a fifth trained model that estimates a difference ΔD between the electrolyte diffusion coefficient of the secondary battery and a threshold electrolyte diffusion coefficient that is the value of the electrolyte diffusion coefficient at which the secondary battery becomes unsuitable for reuse, from input data including the following (1) to (8): (1) rated capacity (initial capacity) of the secondary battery (2) discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity (3) magnitude of current in the measurements of the following (4) to (6) (4) amount of voltage drop after a predetermined time has elapsed since the start of discharge (or amount of voltage rise after a predetermined time has elapsed since the start of charging) (5) amount of voltage drop at a predetermined SOC (6) amount of temperature rise at a predetermined SOC (7) electrode area (8) amount of coating on the positive electrode 9. The method for diagnosing a secondary battery according to claim 8, wherein the input data for the fifth trained model further includes one or more of the following (9) to (14): (9) Discharge capacity measured at the current of (3) (10) Positive electrode active material type (11) Positive electrode mixture layer porosity (or positive electrode mixture layer density) (12) Negative electrode active material type (13) Negative electrode mixture layer porosity (or negative electrode mixture layer density) (14) Heat capacity of the secondary battery.
10. A diagnostic program for a secondary battery, which causes a computer to execute a step of estimating an electrolyte diffusion coefficient Dn of a secondary battery to be diagnosed at the time of diagnosis, using a first trained model that estimates the electrolyte diffusion coefficient of the secondary battery from input data including the following (1) to (6): (1) The rated capacity (initial capacity) of the secondary battery; (2) The discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity; (3) The magnitude of the current in the measurements of the following (4) to (6); (4) The amount of voltage drop after a predetermined time has elapsed since the start of discharging (or the amount of voltage rise after a predetermined time has elapsed since the start of charging); (5) The amount of voltage drop at a predetermined SOC; and (6) The amount of temperature rise at a predetermined SOC.
11. A diagnostic program for a secondary battery, which causes a computer to execute a step of estimating ΔD of a secondary battery to be diagnosed, using a fifth trained model that estimates the difference ΔD between the electrolyte diffusion coefficient of the secondary battery and a threshold electrolyte diffusion coefficient that is the value of the electrolyte diffusion coefficient at which the secondary battery becomes unsuitable for reuse, from input data including the following (1) to (8): (1) The rated capacity (initial capacity) of the secondary battery (2) The discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity (3) The magnitude of the current in the measurements of the following (4) to (6) (4) The amount of voltage drop after a predetermined time has elapsed since the start of discharge (or the amount of voltage rise after a predetermined time has elapsed since the start of charging) (5) The amount of voltage drop at a predetermined SOC (6) The amount of temperature rise at a predetermined SOC (7) The electrode area (8) The amount of coating on the positive electrode 12. A diagnostic device for a secondary battery, comprising an estimation device that estimates an electrolyte diffusion coefficient Dn of a secondary battery to be diagnosed at the time of diagnosis, using a first trained model that estimates the electrolyte diffusion coefficient of the secondary battery from input data including the following (1) to (6): (1) The rated capacity (initial capacity) of the secondary battery; (2) A discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity; (3) The magnitude of the current in the measurements of the following (4) to (6); (4) The amount of voltage drop after a predetermined time has elapsed since the start of discharging (or the amount of voltage rise after a predetermined time has elapsed since the start of charging); (5) The amount of voltage drop at a specified SOC; and (6) The amount of temperature rise at a specified SOC.
13. A diagnostic device for a secondary battery, comprising an estimation device that estimates the difference ΔD of a secondary battery to be diagnosed using a fifth trained model that estimates the difference ΔD between the electrolyte diffusion coefficient of the secondary battery and a threshold electrolyte diffusion coefficient that is the value of the electrolyte diffusion coefficient at which the secondary battery becomes unsuitable for reuse, from input data including the following (1) to (8): (1) Rated capacity of the secondary battery (initial capacity) (2) Discharge capacity measured at a discharge rate equivalent to that used to measure the rated capacity (3) The magnitude of the current in the measurements (4) to (6) below (4) The amount of voltage drop after a specified time has elapsed since the start of discharge (or the amount of voltage rise after a specified time has elapsed since the start of charging) (5) The amount of voltage drop at a specified SOC (6) The amount of temperature rise at a specified SOC (7) Electrode area (8) The amount of coating on the positive electrode
Citation Information
Patent Citations
State measuring apparatus for secondary battery
JP2013044580A
Power supply system for vehicle
JP2013046446A
Battery state estimation device
JP2013113625A
System and method for estimating state of health using battery model parameter
US20160131715A1
Device including battery
US20200074297A1