Lithium silicate glass ceramic with easy machinability
A lithium silicate glass ceramic with lithium metasilicate as the major phase addresses the challenge of rapid machining and conversion into high-strength dental products with excellent properties, facilitating single-session dental restoration production.
Patent Information
- Application Number
- KR1020220104854
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-08-23
- Filing Date
- 2022-08-22
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2042-08-22
AI Technical Summary
Existing lithium silicate glass ceramics used in dentistry are difficult to machine quickly and efficiently, leading to tool wear and limitations in providing dental restorations in a single treatment session, while maintaining high mechanical and optical properties.
A lithium silicate glass ceramic with lithium metasilicate as the major crystalline phase, containing specific compositions and crystal sizes, allowing for easy and rapid machining into complex shapes, followed by heat treatment to achieve high mechanical and optical properties.
The glass ceramic enables rapid machining with reduced tool wear, converting into high-strength dental products with excellent mechanical and optical properties, suitable for single-session dental restoration production.
Smart Images

Figure 112022087650419-PAT00001 
Figure 112022087650419-PAT00002 
Figure 112022087650419-PAT00003
Abstract
Description
Technology Field
[0001] The present invention relates to a lithium silicate glass ceramic suitable for use in dentistry, particularly suitable for the manufacture of dental restorations, and a precursor for the manufacture of the glass ceramic. Background Technology
[0002] Lithium silicate glass ceramics have generally been used for some time in the dental field, mainly for the fabrication of dental crowns and small dental bridges, because they are characterized by very excellent mechanical properties.
[0003] WO 95 / 32678 A2 describes lithium disilicate glass ceramics that are processed into dental restorations by compression in a viscous state. However, processing is very complex because the use of a deformable crucible is essential.
[0004] EP 0 827 941 A1 and EP 0 916 625 A1 disclose lithium disilicate glass ceramics that can be shaped into desired dental restorations by pressing or machining.
[0005] EP 1 505 041 A1 and EP 1 688 398 A1 describe a process for producing dental restorations of lithium disilicate glass ceramics. In this process, a glass ceramic having lithium metasilicate as the major crystalline phase is first produced as a precursor, which can be machined, for example, through a CAD / CAM process. This precursor is then further heat-treated to form a desired high-strength lithium disilicate glass ceramic.
[0006] Machining conventional lithium disilicate glass ceramics is difficult due to their high strength, leading to frequent wear on the tools used. Machining lithium metasilicate glass ceramics is fundamentally easier and may result in less tool wear. However, known lithium metasilicate glass ceramics can only be machined relatively slowly, for example, by grinding tools on standard CAD / CAM machines. This is a particular issue regarding the frequent and desirable provision of dental restorations to patients in a single treatment session (so-called chairside treatment).
[0007] Therefore, there is a need for lithium silicate glass ceramics that can be machined more quickly than known lithium metasilicate glass ceramics and subsequently converted into high-strength dental products exhibiting high chemical resistance and excellent optical properties.
[0008] This problem is solved by the lithium silicate glass ceramic according to claims 1 to 10 and 12. The subject matter of the present invention is also the starting glass according to claims 11 and 12, the method according to claims 13 and 14, the use according to claims 15 to 17, and the method according to claim 18.
[0009] The lithium silicate glass ceramic according to the present invention is characterized by having lithium metasilicate as a major crystalline phase and containing 30 weight percent or less of lithium metasilicate crystals.
[0010] Surprisingly, the glass ceramic according to the present invention has been shown to possess a combination of highly desirable mechanical and optical properties, particularly required for dental restorative materials. Although this glass ceramic has low strength and toughness, allowing for easy and rapid machining into complex dental restoration shapes, it can be converted into a glass ceramic product with excellent mechanical properties, excellent optical properties, and excellent chemical stability through heat treatment following such machining.
[0011] The term "major crystalline phase" is used to describe the crystalline phase with the highest mass proportion among all crystalline phases present in glass ceramics. The mass of the crystalline phase is determined specifically using the Rietveld method. Appropriate procedures for the quantitative analysis of the crystalline phase by the Rietveld method are described, for example, in the paper by M. Dittmer ["Glaeser und Glaskeramiken im System MgO-Al2O3-SiO2mit ZrO2als Keimbildner", University of Jena 2011].
[0012] Preferably, the glass ceramic according to the present invention comprises 28 weight% or less, preferably 26 weight% or less, and particularly preferably 22 weight% or less of lithium metasilicate crystals. Particularly preferably, the glass ceramic comprises 10 to 30 weight%, preferably 12 to 28 weight%, more preferably 15 to 26 weight%, and most preferably 18 to 22 weight% of lithium metasilicate crystals.
[0013] It is more preferable that the average size of the lithium metasilicate crystals in the glass ceramic according to the present invention is in the range of 5 to 80 nm, particularly in the range of 10 to 50 nm, preferably in the range of 15 to 45 nm, and particularly preferably in the range of 25 to 35 nm.
[0014] The average size of lithium metasilicate crystals can be determined by X-ray diffraction of glass-ceramic powders, particularly using CuKα radiation. To this end, the obtained X-ray diffraction pattern can be evaluated according to the Rietveld method, and the average size of the lithium metasilicate crystals can be calculated from the full width at half maximum of the lithium metasilicate peaks according to the Scherrer equation. This evaluation can preferably be performed with software support, for example, Bruker’s TOPAS 5.0 software.
[0015] The lithium silicate glass ceramic according to the present invention comprises SiO2 in the amount of 71.0 to 82.0, preferably 73.1 to 80.0, and particularly preferably 74.0 to 78.0 weight%, particularly 74.0 to 78.0 weight%.
[0016] It is more preferable that the glass ceramic contains 6.0 to 14.0, preferably 7.0 to 12.9, and particularly preferably 8.0 to 12.0 weight% of Li2O. Li2O is believed to lower the viscosity of the glass matrix and promote the crystallization of the desired phase.
[0017] In another preferred embodiment, the glass ceramic contains 4.0 to 15.0, preferably 5.1 to 10.0, particularly preferably 5.5 to 7.0 weight% of an additional oxide Me of a monovalent element. I Includes 2O, where Me I 2O is selected from Na2O, K2O, Rb2O, Cs2O and mixtures thereof, preferably K2O.
[0018] Particularly preferably, the glass ceramic contains additional oxide Me of a monovalent element in the amount indicated below. I Includes at least one of 2O, in particular all:
[0019] Component weight %
[0020] Na2O 0 to 2.0
[0021] K2O 0 to 10.0
[0022] Rb2O 0 to 13.0
[0023] Cs2O 0 to 13.0.
[0024] In a particularly preferred embodiment, the glass ceramic according to the present invention contains 2.0 to 10.0, preferably 5.1 to 9.0, and particularly preferably 5.5 to 7.0 weight% of K2O.
[0025] It is also desirable that the glass ceramic contains 2.0 to 10.0, preferably 4.0 to 7.0, and particularly preferably 5.1 to 6.5 weight% of Al2O3.
[0026] In another preferred embodiment, the glass ceramic comprises 0.5 to 7.0, preferably 1.0 to 4.0, particularly preferably 1.2 to 2.6, and most preferably 1.5 to 2.5 weight% of P2O5. P2O5 is believed to act as a nucleating agent.
[0027] Glass ceramics are oxides of divalent elements Me selected from the group consisting of MgO, CaO, SrO, ZnO, and mixtures thereof. II It is more preferable to include 1.0 to 9.0, preferably 2.0 to 8.0, and particularly preferably 3.0 to 7.0 weight% of O.
[0028] In another preferred embodiment, the glass ceramic contains less than 2.0 weight percent of BaO. In particular, the glass ceramic substantially does not contain BaO.
[0029] Preferably, the glass ceramic is an oxide of a divalent element Me in the amount indicated below. II Includes at least one of O, in particular all of them:
[0030] Component weight %
[0031] MgO 0 to 4.0
[0032] CaO 0 to 4.0
[0033] SrO 0 to 7.0
[0034] ZnO 0 to 5.0.
[0035] In a particularly preferred embodiment, the glass ceramic contains 0.1 to 4.0, preferably 0.5 to 3.0, and particularly preferably 1.0 to 2.0 weight% of MgO.
[0036] In another particularly preferred embodiment, the glass ceramic contains 0.1 to 7.0, preferably 1.0 to 6.0, particularly preferably 2.0 to 5.0, most preferably 3.0 to 4.0 weight% of SrO.
[0037] In addition, additional oxide Me of a trivalent element selected from the group consisting of B2O3, Y2O3, La2O3, Ga2O3, In2O3, and mixtures thereof. III A glass ceramic containing 0 to 8.0, preferably 1.0 to 7.0, and particularly preferably 2.0 to 6.0 weight% of 2O3 is preferred.
[0038] Particularly preferably, the glass ceramic contains additional oxide of a trivalent element Me in the amount indicated below. III Includes at least one of 2O3, in particular all:
[0039] Component weight %
[0040] B2O30 to 4.0
[0041] Y2O30 to 5.0
[0042] La2O30 to 5.0
[0043] Ga2O30 to 3.0
[0044] In2O30 to 5.0.
[0045] In addition, oxides of tetravalent elements Me selected from the group of TiO2, ZrO2, GeO2, SnO2, CeO2, and mixtures thereof. IV A glass ceramic containing 0 to 10.0, preferably 1.0 to 8.0, and particularly preferably 2.0 to 6.0 weight% of O2 is preferred.
[0046] Particularly preferably, the glass ceramic contains the oxide of a tetravalent element Me in the amount indicated below. IV Includes at least one of O2, in particular all of them:
[0047] Component weight %
[0048] TiO2O to 4.0
[0049] ZrO2 to 3.0
[0050] GeO20 to 9.0
[0051] SnO2O to 3.0
[0052] CeO2 to 4.0.
[0053] In another embodiment, the glass ceramic is an additional oxide Me of a pentavalent element selected from the group consisting of V2O5, Nb2O5, Ta2O5, and mixtures thereof. V It contains 0 to 8.0, preferably 1.0 to 7.0, and particularly preferably 2.0 to 6.0 weight% of 2O5.
[0054] Particularly preferably, the glass ceramic contains additional oxide of the pentavalent element Me in the amount indicated below. V Includes at least one of 2O5, in particular all:
[0055] Component weight %
[0056] V2O50 to 2.0
[0057] Nb2O50 to 5.0
[0058] Ta2O50 to 5.0.
[0059] In another embodiment, the glass ceramic is an oxide of a hexavalent element Me selected from the group consisting of MoO3, WO3, and mixtures thereof. VI It contains 0 to 5.0, preferably 1.0 to 4.0, and particularly preferably 2.0 to 3.0 weight% of O3.
[0060] Particularly preferably, the glass ceramic contains the amount of oxide Me indicated below. VI Includes at least one of O3, in particular all of them:
[0061] Component weight %
[0062] MoO30 to 3.0
[0063] WO30 to 3.0.
[0064] In a further embodiment, the glass ceramic according to the present invention comprises 0 to 1.0, particularly 0 to 0.5 weight percent of fluorine.
[0065] Glass ceramics comprising at least one, preferably all, of the components indicated in the amounts below are particularly preferred:
[0066] Component weight %
[0067] SiO2 3.1 to 80.0
[0068] Li2O 7.0 to 12.9
[0069] Me I 2O 4.0 to 15.0, particularly 5.1 to 10.0
[0070] Al2O3 4.0 to 10.0
[0071] P2O5 1.2 to 2.6
[0072] Me II O 0 to 9.0
[0073] Me III 2030 to 8.0
[0074] Me IV 20 to 10.0
[0075] Me V 2050 to 8.0
[0076] Me VI O30 to 5.0
[0077] Fluorine 0 to 1.0
[0078] Here, Me I 2O, Me II 0, Me III 2O3, Me IV O2, Me V 2O5 and Me VI O3 has the meaning given above.
[0079] In another particularly preferred embodiment, the glass ceramic comprises at least one, preferably all, of the following components in amounts indicated below:
[0080] Component weight %
[0081] SiO2 3.1 to 80.0
[0082] Li2O 7.0 to 12.9
[0083] Al2O3 4.0 to 10.0
[0084] P2O5 1.2 to 2.6
[0085] Na2O 0 to 2.0
[0086] K2O 0 to 10.0
[0087] Rb2O 0 to 13.0
[0088] Cs2O 0 to 13.0
[0089] MgO 0 to 4.0
[0090] CaO 0 to 4.0
[0091] SrO 0 to 7.0
[0092] ZnO 0 to 5.0
[0093] B2O30 to 4.0
[0094] Y2O30 to 5.0
[0095] La2O30 to 5.0
[0096] Ga2O30 to 3.0
[0097] In2O30 to 5.0
[0098] TiO2O to 4.0
[0099] ZrO2 to 3.0
[0100] GeO20 to 9.0
[0101] SnO2O to 3.0
[0102] CeO2 to 4.0
[0103] V2O50 to 2.0
[0104] Nb2O50 to 5.0
[0105] Ta2O50 to 5.0
[0106] MoO30 to 3.0
[0107] WO30 to 3.0
[0108] Fluorine 0 to 1.0.
[0109] Some of the above components may act as coloring agents and / or fluorescent agents. The glass ceramic according to the present invention may further include additional coloring agents and / or fluorescent agents. These may be selected, for example, from Bi2O3 or Bi2O5, in particular from additional inorganic pigments and / or oxides of d and f elements, for example, oxides of Mn, Fe, Co, Pr, Nd, Tb, Er, Dy, Eu, and Yb. With these coloring agents and fluorescent agents, it is possible to easily color the glass ceramic to mimic the desired optical properties of natural dental materials in particular.
[0110] In a preferred embodiment of the glass ceramic, the molar ratio of SiO2 to Li2O is in the range of 2.5 to 5.0, preferably in the range of 2.9 to 4.6, and particularly preferably in the range of 3.3 to 4.4. Despite this high molar excess of SiO2 to Li2O, it is not surprising that the glass ceramic of the present invention can be formed to have lithium metasilicate as the major crystalline phase.
[0111] In addition to lithium metasilicate, the glass ceramic according to the present invention may comprise additional crystalline phases such as quartz, particularly low quartz, apatite, cesium aluminosilicate, and particularly lithium phosphate. However, the amount of cristobalite should be as small as possible, particularly less than 1.0 weight%. It is particularly preferable that the glass ceramic according to the present invention is substantially free of cristobalite.
[0112] The type and, in particular, the amount of the crystalline phase formed can be controlled by the composition of the starting glass and the heat treatment applied to produce glass ceramics from the starting glass. Examples illustrate this by varying the composition of the starting glass and the heat treatment applied.
[0113] The biaxial fracture strength of the glass ceramic is preferably at least 80 MPa, particularly preferably 100 to 200 MPa. The biaxial fracture strength was determined according to ISO 6872 (2008) (piston-on-three-ball test).
[0114] The glass ceramic according to the present invention is preferably 9.5 to 14.0·10 -6 K -1 It has a coefficient of thermal expansion CTE (measured in the range of 100 to 500°C). The CTE is determined according to ISO 6872 (2008). The coefficient of thermal expansion is adjusted to a desired value, particularly by the type and amount of crystalline phase present in the glass ceramic and the chemical composition of the glass ceramic.
[0115] The transparency of the glass ceramic was determined in terms of the contrast value (CR value) according to British Standard BS 5612, and this contrast value was preferably 40 to 92.
[0116] The present invention also relates to various precursors of corresponding compositions to which lithium silicate glass ceramics according to the present invention can be produced by heat treatment. These precursors are starting glasses with corresponding compositions and starting glasses having correspondingly composed nuclei. The term "corresponding composition" means that these precursors contain the same components in the same amount as the glass ceramics, wherein the components are calculated as oxides excluding fluorine, as is customary for glass and glass ceramics.
[0117] Accordingly, the present invention also relates to a starting glass comprising a component of a lithium silicate glass ceramic according to the present invention.
[0118] Accordingly, the starting glass according to the present invention comprises appropriate amounts of SiO2 and Li2O necessary to form the glass ceramic according to the present invention, particularly having lithium metasilicate as the major crystalline phase. Additionally, the starting glass may also comprise other components as indicated above for the lithium silicate glass ceramic according to the present invention. All such embodiments are preferred for the components of the starting glass that are also indicated as preferred for the components of the lithium silicate glass ceramic according to the present invention.
[0119] The present invention also relates to such starting glass comprising a nucleus for the formation of lithium metasilicate crystals.
[0120] The lithium silicate glass ceramic according to the present invention and the starting glass according to the present invention exist particularly in the form of powder, granules, or blanks of any shape and size, for example, monolithic blanks such as plates, cubes, or cylinders, or powder compacts in the form of non-sintered, partially sintered, or densely sintered forms. These can be easily further processed in these forms. However, they may also be in the form of dental restorations such as inlays, onlays, crowns, veneers, facets, or abutments.
[0121] The procedure for manufacturing starting glass involves melting a mixture of suitable starting materials, particularly carbonates, oxides, phosphates, and fluorides, at a temperature of 1300 to 1600°C for 2 to 10 hours. In particular, to achieve high homogeneity, the resulting glass melt is poured into water to form glass granules, and then the resulting granules are melted again.
[0122] Then, the molten material can be poured into a mold to produce a blank of starting glass, a so-called solid glass blank or monolithic blank.
[0123] It is also possible to introduce the molten material back into water to produce granules. After grinding, and if necessary, after adding additional ingredients such as coloring agents and fluorescent agents, these granules can be compressed into blanks, so-called powder compacts.
[0124] Finally, the starting glass may be processed into powder after granulation.
[0125] Next, at least one heat treatment is performed on a starting glass in the form of, for example, a solid glass blank, a powder compact, or a powder. It is preferable to perform a first heat treatment initially to produce a starting glass according to the present invention having a nucleus for the formation of lithium metasilicate crystals. Then, at least one additional heat treatment is typically performed on the starting glass having the nucleus at a higher temperature to crystallize the lithium metasilicate and produce a lithium silicate glass ceramic according to the present invention.
[0126] Accordingly, the present invention also relates to a method for manufacturing a lithium silicate glass ceramic according to the present invention, wherein at least one heat treatment is performed on a starting glass or a starting glass having a nucleus at a temperature of 450 to 750°C for a duration of particularly 1 to 120 minutes, preferably 5 to 120 minutes, particularly preferably 10 to 60 minutes.
[0127] At least one heat treatment performed in the method according to the present invention may also be performed during the high-temperature pressing or sintering process of the starting glass according to the present invention or the starting glass having a nucleus according to the present invention.
[0128] To produce a starting glass having nuclei for the crystallization of lithium metasilicate, it is preferable to heat-treat the starting glass at a temperature of 450 to 600°C, preferably 480 to 580°C, particularly preferably 480 to 520°C, for a duration of particularly 1 to 120 minutes, preferably 10 to 60 minutes.
[0129] To manufacture lithium silicate glass ceramics, it is more preferable to heat-treat a starting glass having a nucleus at a temperature of 550 to 750°C, preferably 580 to 700°C, particularly preferably 590 to 630°C for a duration of 1 to 120 minutes, preferably 5 to 60 minutes, particularly preferably 10 to 30 minutes.
[0130] In a preferred embodiment, the method for manufacturing a lithium silicate glass ceramic according to the present invention
[0131] (a) a step of heat-treating a starting glass at a temperature of 450 to 600°C, preferably 480 to 580°C, particularly preferably 480 to 520°C for a duration of particularly 1 to 120 minutes, preferably 10 to 60 minutes, to form a starting glass having a nucleus, and
[0132] (b) a step of forming a glass ceramic by heat-treating a starting glass having a nucleus at a temperature of 550 to 750°C, preferably 580 to 700°C, particularly preferably 590 to 630°C for a duration of particularly 1 to 120 minutes, preferably 5 to 60 minutes, particularly preferably 10 to 30 minutes.
[0133] Includes
[0134] Due to the aforementioned properties of the glass ceramic according to the present invention and the glass according to the present invention, they are particularly suitable for use in dentistry. Accordingly, the object of the present invention is also to use the glass ceramic according to the present invention or the glass according to the present invention as a dental material, particularly for the manufacture of dental restorations or as a coating material for dental restorations.
[0135] In particular, the glass ceramic according to the present invention and the glass according to the present invention can be used to manufacture dental restorations such as bridges, inlays, onlays, veneers, abutments, partial crowns, crowns, or facets. Accordingly, the present invention also relates to the use of the glass ceramic according to the present invention or the glass according to the present invention for the manufacture of dental restorations. In this context, it is desirable that the glass ceramic or the glass be imparted with the desired shape of the dental restoration by pressing or machining.
[0136] The present invention also relates to a method for manufacturing a dental restoration in which a desired shape of the dental restoration is imparted to the glass ceramic or glass according to the present invention by pressing or machining.
[0137] Compression is generally performed at increased pressure and increased temperature. It is preferable to perform compression at a temperature of 700 to 1200°C. It is even more preferable to perform compression at a pressure of 2 to 10 bar. During compression, the desired shape change is achieved by the viscous flow of the material used. Starting glass according to the present invention, in particular starting glass having a nucleus according to the present invention, and lithium silicate glass ceramic according to the present invention can be used for compression. The glass and glass ceramic according to the present invention can be used particularly in the form of blanks of any shape and size, for example, as solid blanks, or as powder compacts in the form of, for example, unsintered, partially sintered, or densely sintered forms.
[0138] Machining is generally performed by material removal processes, particularly milling and / or grinding. It is particularly desirable to perform machining as part of a CAD / CAM process. Starting glass according to the present invention, starting glass having a nucleus according to the present invention, and lithium silicate glass ceramic according to the present invention can be used for machining. The glass and glass ceramic according to the present invention can be used particularly in blank form, e.g., solid blank, or as powder compacts in the form of, e.g., unsintered, partially sintered, or densely sintered. Preferably, the lithium silicate glass ceramic according to the present invention is used for machining.
[0139] Surprisingly, it was found that the lithium silicate glass ceramic according to the present invention can be machined faster than known lithium silicate glass ceramics when the same force is applied. To explain this characteristic, the removal rate can be determined, in particular, for a sample body of the glass ceramic. To do this, a plate is cut from the sample body and weighed. The plate is then attached to a holder and ground under water cooling using an automatic grinding machine, such as one available from Struers, using, for example, a diamond grinding wheel with a grain size of 20 μm. The pressure of the grinding machine is selected so that the same force, for example, 15 N, is applied to each plate. After grinding the plate for 1 minute, it is dried and weighed again. The removal rate is calculated according to the following formula:
[0140] Removal rate [weight% · min -1 ] = 100 ×(1-(m 그라인딩 :m 언그라인딩 ))
[0141] Furthermore, it was revealed that lithium silicate glass ceramics with easy machinability, having lithium metasilicate as the major crystalline phase, can be converted into glass ceramics having lithium disilicate as the major crystalline phase through additional heat treatment. This glass ceramic not only exhibits excellent mechanical properties such as high strength but also other properties required for dental restorative materials.
[0142] After the glass ceramic obtains the desired shape of the dental restoration, additional heat treatment may be performed to convert the lithium metasilicate crystals into lithium disilicate crystals. Preferably, the glass ceramic is heat-treated at a temperature of 750 to 950°C, preferably 820 to 890°C, particularly preferably 840 to 870°C, for a duration of particularly 1 to 60 minutes, preferably 5 to 30 minutes, more preferably 5 to 15 minutes, and even more preferably 5 to 10 minutes. Suitable conditions for a given glass ceramic can be determined, for example, by performing X-ray diffraction analysis at various temperatures.
[0143] In addition, the transformation into lithium disilicate glass ceramics was found to be associated with only a very small linear shrinkage of about 0.2 to 0.3%, which is almost negligible compared to the linear shrinkage of up to 30% when sintering ceramics.
[0144] However, the glass ceramic according to the present invention and the glass according to the present invention are also suitable as coating materials for, for example, ceramics and glass ceramics. Accordingly, the present invention also relates to the use of the glass or glass ceramic according to the present invention for coating ceramics, glass ceramics, and in particular dental restorations.
[0145] The present invention also relates to a coating method for ceramics, metals, metal alloys, and glass ceramics in which glass ceramics or glass according to the present invention is applied to ceramics, metals, metal alloys, or glass ceramics and performed at an increased temperature.
[0146] This can be accomplished, particularly by sintering or by combining an overlay produced by CAD-CAM with a suitable glass solder or adhesive, preferably by pressing. In the case of sintering, the glass ceramic or glass is applied in a conventional manner, for example as a powder, to a material to be coated, such as ceramic or glass ceramic, and then sintered at an elevated temperature. In a preferred pressing process, the glass ceramic or glass according to the present invention, for example in the form of a powder compact or monolithic blank, is pressed at an increased temperature, for example, of 700 to 1200°C, and a pressure, for example, of 2 to 10 bar, is applied. In particular, the process described in EP 231 773 and the pressing furnace disclosed herein may be used for this purpose. A suitable furnace is, for example, the Programat EP 5000 of Ivoclar Vivadent AG in Liechtenstein.
[0147] After the coating process is completed, it is desirable for such glass ceramics to be present because they possess particularly excellent properties.
[0148] The present invention will be described in more detail below with reference to non-limiting embodiments. Specific details for implementing the invention
[0149] Examples
[0150] A total of 28 glasses were prepared according to the examples of the present invention and comparative examples having the compositions given in Table I below. The glasses were crystallized into glass ceramics according to Table II below. The following meanings apply.
[0151] Tg Glass transition temperature determined by DSC
[0152] T S and t S Temperature and time applied to melting
[0153] T Kb and t Kb Temperature and time applied to nucleation
[0154] T C1 and t C1 Temperature and time applied for primary crystallization
[0155] T C2 and t C2 Temperature and time applied for secondary crystallization
[0156] In the examples, the starting glass having the composition given in Table I below is t S Temperature T during the duration S In general, the raw material was first melted in a scale of 100 to 200 g, and melting was very well possible without the formation of bubbles or streaks. The glass frit was prepared by pouring the starting glass into water and then melting it again at 1500°C or 1400°C for 1 hour for homogenization. Subsequently, the resulting melt of the starting glass was poured into a graphite mold to produce a solid glass block.
[0157] t Kb Temperature T during the duration Kb The first heat treatment of the glass monolith obtained from induced the formation of nucleated glass. This nucleated glass, as determined by X-ray diffraction analysis at room temperature, t C1 Temperature T during the duration C1 It is crystallized by additional heat treatment to form a glass ceramic having lithium metasilicate as the main crystalline phase.
[0158] The amount of the crystalline phase and the average size of the lithium metasilicate crystals were determined by X-ray diffraction. For this purpose, powders of each glass ceramic were prepared by grinding and sieving (< 45 μm), and an internal standard, Al2O3 (Alfa Aesar, product number 42571), was mixed in a ratio of 80 wt% glass ceramic to 20 wt% Al2O3. This mixture was slurried with acetone to achieve the best possible mixing. Subsequently, the mixture was dried at approximately 80°C. Then, diffraction patterns were recorded using a Bruker D8 Advance diffractometer in the range of 10 to 100° 2θ using CuKα radiation and a step size of 0.014° 2θ. These diffraction patterns were analyzed using Bruker's TOPAS 5.0 software according to the Rietveld method. The phase fractions were determined by comparing the peak intensities of lithium metasilicate and Al2O3, respectively. The average size of the lithium metasilicate crystals was determined from the full width at half maximum of the lithium metasilicate peak according to the Scheret equation.
[0159] To measure the machinability of the glass-ceramic blocks obtained in this way, each with an area of 170 mm 2 ± 10 mm 2 Two small plates measuring approximately 12.5 mm x 13.8 mm with a thickness of 4.0 ± 0.5 mm were cut and weighed under precise balance. The plates were then bonded to a holder and ground under water cooling using an automatic grinding machine (LdaboForche-100, Struers) with a diamond grinding wheel having a grain size of 20 μm. The pressure of the grinding machine was selected to apply a force of 15 N to each plate. The rotational direction of the turntable equipped with the diamond grinding wheel and the grinding machine head equipped with the holder holding the specimen were identical. The turntable speed was set to 300 revolutions per minute. -1 The slicing plate was ground for 1 minute, dried, and weighed. The removal rate was calculated according to the following formula:
[0160] Removal rate [weight% · min -1 ] = 100 × (1-(m 그라인딩 :m 언그라인딩 ))
[0161] As can be seen from Table II below, the removal rates of Examples 1 to 28 according to the present invention were consistently higher than those of the comparative example. This indicates that the lithium silicate glass ceramic according to the present invention can be machined faster than known lithium silicate glass ceramics when the same force is applied.
[0162] The remaining glass ceramic blocks are t C2 Temperature T during the duration C2 Further heat treatment was performed. As a result, a glass ceramic having lithium disilicate as the main phase was formed. In the case of lithium phosphate and Example 27, lithium strontium phosphate was found as a trace phase.
[0163] [Table I]
[0164]
[0165]
[0166]
[0167] [Table II]
[0168]
[0169]
[0170]
Claims
Claim 1 A lithium silicate glass ceramic comprising lithium metasilicate as the main crystalline phase and 30 weight% or less of lithium metasilicate crystals, wherein the molar ratio of SiO2 to Li2O is in the range of 2.9 to 5.
0. Claim 2 A glass ceramic according to claim 1, comprising 28 wt% or less, 26 wt% or less, 22 wt% or less, 10 to 30 wt%, 12 to 28 wt%, 15 to 26 wt%, or 18 to 22 wt% of lithium metasilicate crystals. Claim 3 A glass ceramic according to claim 1, wherein the average size of the lithium metasilicate crystals is in the range of 5 to 80 nm, 10 to 50 nm, 15 to 45 nm, or 25 to 35 nm. Claim 4 A glass ceramic according to claim 1, comprising 71.0 to 82.0 weight%, 73.1 to 80.0 weight%, or 74.0 to 78.0 weight% of SiO2. Claim 5 A glass ceramic according to claim 1, comprising 6.0 to 14.0 weight%, 7.0 to 12.9 weight%, or 8.0 to 12.0 weight% of Li2O. Claim 6 In claim 1, additional oxide Me of a monovalent element in an amount of 4.0 to 13.0 wt%, 5.1 to 10.0 wt%, or 5.5 to 7.0 wt%. I Includes 2O, where Me I 2O is a glass ceramic selected from Na2O, K2O, Rb2O, Cs2O and mixtures thereof. Claim 7 A glass ceramic according to claim 1, comprising 2.0 to 10.0 weight%, 4.0 to 7.0 weight%, or 5.1 to 6.5 weight% of Al2O3. Claim 8 A glass ceramic according to claim 1, comprising 0.5 to 7.0 weight%, 1.0 to 4.0 weight%, 1.2 to 2.6 weight%, or 1.5 to 2.5 weight% of P2O5. Claim 9 In claim 1, the glass ceramic comprising at least one or all of the components in the amounts indicated below: component weight% SiO2 7.1 to 80.0 Li2O 7.0 to 12.9 Me I 2O 4.0 to 10.0 Al2O3 4.0 to 10.0 P2O5 1.2 to 2.6 Me II O 0 to 9.0Me III 2030 to 8.0Me IV O20 to 10.0Me V 2050 to 8.0Me VI O30 to 5.0 fluorine 0 to 1.0, where, Me I 2O is selected from Na2O, K2O, Rb2O, Cs2O and mixtures thereof, and Me II O is selected from MgO, CaO, SrO, ZnO and mixtures thereof, and Me III 2O3 is selected from B2O3, Y2O3, La2O3, Ga2O3, In2O3 and mixtures thereof, and Me IV O2 is selected from TiO2, ZrO2, GeO2, SnO2, CeO2 and mixtures thereof, and Me V 2O5 is selected from V2O5, Nb2O5, Ta2O5 and mixtures thereof; Me VI O3 is selected from MoO3, WO3, and mixtures thereof. Claim 10 A glass ceramic according to claim 1, wherein the molar ratio of SiO2 to Li2O is in the range of 2.9 to 4.6 or 3.3 to 4.
4. Claim 11 A starting glass comprising a glass ceramic component according to any one of claims 1 to 10, or comprising a glass ceramic component according to any one of claims 1 to 10 and a nucleus for forming a lithium metasilicate crystal. Claim 12 In any one of claims 1 to 10, the glass ceramic is a glass ceramic in the form of powder, granules, blanks, or dental restorations. Claim 13 A method for manufacturing a glass ceramic according to any one of claims 1 to 10, wherein at least one heat treatment is performed in the range of 450 to 750°C on a starting glass containing the components of the glass ceramic according to any one of claims 1 to 10. Claim 14 A manufacturing method according to claim 13, wherein (a) a starting glass is heat-treated at a temperature of 450 to 600°C to form a starting glass having a nucleus, and (b) the starting glass having a nucleus is heat-treated at a temperature of 550 to 750°C to form a glass ceramic. Claim 15 Glass ceramic according to any one of claims 1 to 10, for use as a dental material, for coating a dental restoration, or for manufacturing a dental restoration. Claim 16 In paragraph 15, glass ceramic for the manufacture of dental restorations, wherein the dental restoration is selected from the group consisting of bridges, inlays, onlays, veneers, abutments, partial crowns, crowns, and facets. Claim 17 A method for manufacturing a dental restoration, wherein a starting glass comprising a glass ceramic according to any one of claims 1 to 10 or a component of a glass ceramic according to any one of claims 1 to 10 is formed into a desired shape of the dental restoration by pressing or machining, or by a CAD / CAM process. Claim 18 A manufacturing method according to claim 17, wherein the glass ceramic is heat-treated at a temperature of 750 to 950°C, 820 to 890°C, or 840 to 870°C.
Citation Information
Patent Citations
Inorganic composition for information recording medium
EP1772440A1
Inorganic composition article
JP2008254984A
Inorganic composition
KR1020070038908A
Method for manufacturing a multi-color dental restorations
WO2021136726A1
Glass-ceramics or Lithium silicate glass for Zirconia overlaying materials and preparation method thereof
KR1020150043633A