Method for manufacturing resolution-enhancing mask for x-ray projection lithography
The laminated structure with a convex-to-concave curvature transformation addresses X-ray lithography's focusing and diffraction challenges, achieving high-resolution pattern formation in semiconductor devices.
Patent Information
- Application Number
- KR1020250144597
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2025-10-02
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2045-10-02
AI Technical Summary
Conventional X-ray lithography masks face limitations in focusing and diffraction control due to X-rays' refractive index less than 1, leading to degraded precision and resolution in semiconductor device fabrication.
A method involving a laminated structure with a convex curvature structure formed on a photoreactive polymer layer, followed by an X-ray shielding layer and a transmitting layer, which is then inverted to create a concave curvature structure for precise diffraction control and focusing.
Enables high-resolution and high-precision pattern formation in X-ray projection lithography by controlling diffraction angles and focusing X-rays to a target point, enhancing the precision and resolution of semiconductor device fabrication.
Smart Images

Figure 112025112637843-PAT00004_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a high-resolution lithography technology using X-rays, and more specifically, to a method for manufacturing a projection X-ray exposure mask capable of focusing or controlling X-rays by utilizing curvature-based optical properties. Background Technology
[0002] The following descriptions are intended to aid in understanding the technical significance of the invention and are not based on the premise that they were publicly known prior to the filing. Therefore, the fact that a description is included in the background technology of the invention should not be regarded as publicly known technology in itself.
[0003] In the manufacturing process of semiconductor devices, photolithography is a process used to form circuit patterns on a wafer. This process proceeds by irradiating light onto a wafer coated with photoresist to transfer a pattern of the desired shape; for this purpose, a mask or reticle formed with a fine pattern corresponding to the semiconductor circuit is essential. In particular, diffraction occurs as light passing through the mask focuses onto the wafer via an optical system, and this is influenced by the wavelength of the light source, the shape of the mask, and aberrations of the optical system. As the linewidth of semiconductor circuits becomes finer, securing precision and resolution in this lithography process becomes increasingly critical; consequently, active technological development for high-resolution exposure is underway.
[0004] Conventionally, photolithography processes using ultraviolet (UV) or deep ultraviolet (DUV) light sources have been widely used for forming fine patterns in semiconductor devices; however, with the continuous improvement in integration density, next-generation lithography technologies utilizing light sources with shorter wavelengths have been researched. Among these, X-ray lithography has been proposed, and since X-rays have short wavelengths of less than a few nanometers, it is possible to form patterns with higher resolution than UV-based technologies. For this reason, X-ray lithography has attracted attention from academia and industry as a promising candidate technology capable of overcoming the resolution limitations of conventional photolithography. In conventional technology, a planar mask is fabricated by patterning X-ray absorbing materials such as gold (Au), tungsten (W), and bismuth (Bi) onto a substrate with high X-ray transmittance, such as polyimide (PI) film or beryllium (Be), and a method has been used to transfer a desired image onto a wafer surface coated with photoresist using the transmission and shielding regions of this mask. These masks generally have a multilayer structure combining a transmitting layer and an absorbing layer, thereby aiming to selectively control the path of X-rays.
[0005] However, unlike ultraviolet or visible light, X-rays have a refractive index less than 1 and exhibit the opposite direction of refraction at material boundaries, making it difficult to apply conventional convex lens-based focusing methods. Consequently, there are fundamental limitations to X-ray focusing and diffraction control, and planar mask structures cannot actively control the diffraction angle or have very limited functionality. As a result, diffracted light passing through the mask spreads out at large angles as it passes through the projection optical system, leading to a problem where the precision and resolution of the pattern transferred onto the wafer are degraded. Furthermore, if the mask pattern is miniaturized to achieve high resolution, process deviations occurring during deposition and etching processes reduce the pattern precision and process stability of the mask, which can ultimately lead to a degradation of mask quality.
[0006] These issues act as structural limiting factors for the resolution of projection-type X-ray lithography systems, hindering the formation of ultrafine patterns essential for the fabrication of highly integrated semiconductor devices. Therefore, a new concept of mask structure design that fundamentally considers the refraction and diffraction characteristics of X-rays is required. The problem to be solved
[0007] The present invention aims to provide a manufacturing technology for a metal-based mask that enables the formation of high-resolution and high-precision patterns required in X-ray projection lithography.
[0008] However, the technical problem that this embodiment aims to solve is not limited to the technical problem described above, and other technical problems may exist. means of solving the problem
[0009] A method for manufacturing a projection type X-ray exposure mask according to one embodiment of the present invention may include the steps of: forming a photoreactive polymer layer on a first film substrate; placing an inversion pattern mask having an inversion shape of a target pattern on the photoreactive polymer layer and irradiating X-rays through the inversion pattern mask to form a convex curvature structure corresponding to the target pattern on the surface of the photoreactive polymer layer; laminating an X-ray shielding layer on the surface on which the convex curvature structure is formed; laminating an X-ray transmitting material and a second film substrate in sequence on the X-ray shielding layer to form a laminated structure; and removing the first film substrate and the photoreactive polymer layer on which the convex curvature structure is formed to form a mask having a concave curvature structure.
[0010] According to one embodiment, the X-ray shielding layer is characterized by being composed of at least one of lead (Pb), tungsten (W), gold (Au), bismuth (Bi), tantalum (Ta), hafnium (Hf), iridium (Ir), or barium (Ba).
[0011] According to one embodiment, the X-ray transmitting material is characterized by being composed of at least one of beryllium (Be), aluminum (Al), silicon (Si), or diamond (C).
[0012] According to one embodiment, the step of forming a mask is characterized by inverting the laminated structure, removing a first film substrate located at the outermost edge of the laminated structure, and removing a photoreactive polymer layer having a convex curvature structure located below the first film substrate using X-rays.
[0013] According to one embodiment, the radius of curvature of a convex curvature structure is controlled based on at least one of the irradiation distance, irradiation time, and irradiation intensity of X-ray irradiation in the step of forming a mask.
[0014] According to one embodiment, the mask is characterized by being a lens structure configured to focus incident X-rays to a target point within a predetermined focal length through a concave curvature structure.
[0015] According to one embodiment, the concave curvature structure is characterized by being formed such that the deviation in radius of curvature relative to the target pattern is maintained within ±5%. Effects of the invention
[0016] According to the present invention, the invention can provide a manufacturing technology for a metal-based mask that enables the formation of high-resolution and high-precision patterns required in X-ray projection lithography.
[0017] However, the effects obtainable through the present invention are not limited to those described above, and other unmentioned technical effects will be clearly understood by a person skilled in the art from the description of the invention below. Brief explanation of the drawing
[0018] Figure 1a is a diagram showing a convex curvature structure formed on a PI film. Figure 1b is a diagram showing a structure in which a shielding layer is formed on a convex curvature structure. FIG. 1c is a drawing showing a stacked structure in which a shielding layer and a transparent layer are stacked. Figure 1d is a diagram showing the final structure of a mask with the PMMA layer removed. Specific details for implementing the invention
[0019] The present invention is susceptible to various modifications and may have various embodiments, and specific embodiments are illustrated and described in the drawings. However, this is not intended to limit the invention to specific embodiments, and it should be understood that the invention includes all modifications, equivalents, and substitutions that fall within the spirit and scope of the invention. That is, expressions such as "for example" or "exemplarily" used in this specification are intended to describe specific embodiments and should not be interpreted as limiting the scope of the invention.
[0020] The technical concept of the present invention is not limited to the embodiments described and can be implemented in various different forms. Within the scope of the technical concept of the present invention, one or more of the components of the embodiments may be selectively combined or substituted, and it should be understood that new embodiments combining various embodiments are also included in this disclosure. Each component described as an integral may be implemented by dividing it into multiple elements, and likewise, components described as multiple elements may also be implemented as an integral form.
[0021] It should be noted that the drawings are schematic and not drawn to scale. Relative dimensions and proportions of parts in the drawings may be exaggerated or reduced in size for clarity and convenience, and arbitrary dimensions are merely illustrative and not limiting. Additionally, the same reference numerals are used whenever possible to denote similar features for the same structure, element, or part appearing in two or more drawings.
[0022] In addition, terms used in the embodiments of the present invention (including technical and scientific terms) shall be interpreted in a meaning generally understood by those skilled in the art to which the present invention pertains, unless explicitly and specifically defined otherwise. Commonly used terms, such as those defined in a dictionary, shall be interpreted in consideration of their contextual meaning as described in the present invention. If a commonly used term defined in a dictionary does not match the meaning it has in the context according to the description of the present invention, it shall be interpreted in accordance with the meaning it has in the context according to the description of the present invention. Furthermore, even if not explicitly defined in this application, it shall not be interpreted in an overly formal sense based on the description of the present invention.
[0023] Furthermore, the terms used in the embodiments of the present invention are for describing the embodiments and are not intended to limit the present invention. In some embodiments, well-known process steps, well-known device structures, or well-known techniques are not specifically described to avoid the present invention being interpreted ambiguously. Additionally, in this specification, the singular form may include the plural form unless specifically stated otherwise in the text.
[0024] Terms containing ordinal numbers, such as "first," "second," etc., may be used to describe various components, but the meaning of the components is not limited by the ordinal numbers. Terms containing ordinal numbers are used solely for the purpose of distinguishing one component from another and are not limited by the essence, order, or sequence of the corresponding component. For example, without departing from the scope of the present invention, the second component may be named the first component, and similarly, the first component may be named the second component. Furthermore, if the meaning of the component does not depart from the scope of the present invention even without ordinal numbers such as "first" and "second," the component may be referred to by excluding the ordinal number.
[0025] The expression 'and / or' is interpreted to mean that it may include one or more or all of the listed components, and for example, 'A and / or B' should be understood to include cases where A alone, B alone, or both A and B are included.
[0026] In this specification, terms such as 'comprising,' 'provided,' 'having,' and 'consisting of' are intended to indicate the existence of the features, numbers, steps, actions, components, parts, or combinations thereof described in the specification, and should not be interpreted as precluding the existence or addition of one or more other features, numbers, steps, actions, components, parts, or combinations thereof.
[0027] The embodiments describe the relationship of one element or feature depicted in the drawings to other elements or features using spatial relative terms such as 'top', 'bottom', 'left', and 'right'. In addition to the orientations depicted in the drawings, spatial terms imply different orientations in the use or operation of the device. For example, if the device in the drawing is inverted, an element located 'below' another element or feature is described as being located 'above' another element or feature. Thus, the exemplary term 'bottom' may include both top and bottom.
[0028] Furthermore, when described as being formed or placed 'above or below' each component, 'above or below' includes not only cases where two components are in direct contact with each other, but also cases where one or more other components are formed or placed between the two components. Additionally, when expressed as 'above or below,' it may include the meaning of a downward direction as well as an upward direction relative to a single component.
[0029] Additionally, the meaning that Configuration A is positioned between Configuration B and Configuration C may mean that Configuration A is located in the horizontal space between Configuration B and Configuration C, and / or in the vertical space between Configuration B and Configuration C. Furthermore, the meaning that Configuration A is positioned between Configuration B and Configuration C may include the meaning that Configuration A is positioned such that at least a portion of it overlaps with Configuration B and Configuration C in the vertical and / or horizontal directions. Unless otherwise noted, Configuration C may also be included in the meaning that Configuration A is positioned between Configuration A and Configuration B even if Configuration C is located between a virtual line extending vertically and / or horizontally from Configuration A and a virtual line extending vertically and / or horizontally from Configuration B.
[0030] Furthermore, the meaning that Configuration A is exposed from Configuration B should not be limited to Configuration A being exposed from the entire product, but should be understood as meaning that Configuration A is exposed from Configuration B; unless there are special circumstances, it should not be understood as necessarily meaning that the entire Configuration A is covered by Configuration B. In other words, when Configuration A is described as being exposed from Configuration B, it should be understood to encompass the case where another Configuration C, other than Configurations A and B, covers Configuration A exposed from Configuration B.
[0031] Additionally, where it is stated that a component is 'connected,' 'combined,' 'connected,' or 'contacted' with another component, this may include not only cases where the component is directly connected, combined, or connected to the other component, but also cases where it is 'connected,' 'combined,' 'connected,' or 'contacted' due to another component located between the component and the other component. Accordingly, if component A is to be understood only as being directly 'connected,' 'combined,' 'connected,' or 'contacted' with component B, it is described as being 'directly connected,' 'directly combined,' 'directly connected,' or 'directly contacted.'
[0032] In addition, when described as 'flat' or 'located on the same plane,' it should not be interpreted according to the dictionary definition, but rather understood by a person with ordinary knowledge in the relevant technical field to the extent that process deviations are taken into account.
[0033] Additionally, throughout the specification, 'planar' or 'when viewed in a planar view' means when the subject part is viewed from above or below, and 'cross-sectional' or 'when viewed in a cross-sectional view' may mean when the cross-section obtained by vertically cutting the subject part is viewed from the side.
[0034] In this specification and drawings, the same reference numerals represent the same or substantially the same components, and the reference numerals are not limited to a specific drawing and may be used identically in other drawings. Accordingly, the reference numerals described in this specification should be understood as referring to parts that perform the same or similar functions throughout the entire specification.
[0035] A method for manufacturing a projection type X-ray exposure mask according to embodiments of the present invention will be described below with reference to the drawings.
[0036] FIG. 1a is a drawing showing a convex curvature structure formed on a PI film, FIG. 1b is a drawing showing a structure in which a shielding layer is formed on a convex curvature structure, FIG. 1c is a drawing showing a laminated structure in which a shielding layer and a transparent layer are laminated, and FIG. 1d is a drawing showing the final structure of a mask with the PMMA layer removed.
[0037] First, FIG. 1a is an initial step for manufacturing a mask structure for X-ray exposure that includes a curvature structure, wherein a PMMA layer (120), which is a curvature-reactive polymer material, is formed on a polyimide film (110), an inversion pattern mask is aligned on the upper surface, and then X-rays are irradiated to form a curved pattern.
[0038] The polyimide film (110) is a flexible polymer material that serves as a substrate and is a structure that maintains mechanical stability even at high temperatures and has a low coefficient of thermal expansion and excellent chemical resistance. The polyimide film (110) is configured to be used alone or laminated with a dry film resist (DFR) as needed to ensure ease of subsequent peeling processes and shape transfer precision. The polyimide film (110) must simultaneously satisfy the functions of maintaining the flatness of the substrate, minimizing distortion in the optical path, and supporting the structure, and may perform surface cleaning or primer treatment in advance to ensure adhesion with the spin-coated polymer layer.
[0039] The PMMA layer (120) is an acrylate-based polymer material, and is formed by using polymethyl methacrylate produced by radical polymerization of methyl methacrylate (MMA) monomers as a starting material. This is applied to a polyimide film (110) by dispensing or spin coating, and then the solvent is removed through a baking process for several tens of minutes in the range of 80 to 120 degrees. The formed PMMA layer (120) has a thickness of 1 to 200 μm, and the region irradiated by X-rays can be selectively removed during the development process due to molecular weight reduction and weakening of mechanical strength, and forms a structure suitable for precise implementation of a curved shape pattern.
[0040] Additionally, the PMMA layer (120) has a relatively low thermal conductivity and local change in volume density upon radiation, which can induce a difference in expansion rate and stress distribution between the irradiated area and the non-irradiated area. In another embodiment, a photosensitive polymer material such as SU-8 can also be used to form the same structure based on X-ray reactivity and process compatibility.
[0041] The inversion pattern mask includes a negative structure of the target shape and is made based on metals such as gold (Au), chromium (Cr), or tungsten (W), or is composed of an X-ray shielding mask based on graphite or a composite absorption layer. The inversion pattern mask has a transmitting portion and a shielding portion arranged two-dimensionally and is placed in close contact with the upper surface of the PMMA layer (120) through a precision alignment device. The inversion pattern mask can be manufactured using the same principle as a photomask for photoresist exposure used in conventional photolithography processes, and is manufactured by irradiating a light source onto a substrate coated with a positive photoresist and performing an exposure and development process. The photoresist used at this time can be composed of polymers with various resolutions, such as PMMA, AZ series, and SU-8, and can be selected according to the X-ray wavelength and process resolution.
[0042] X-rays are selectively irradiated onto the upper surface of the PMMA layer (120) through the opening of the inversion pattern mask. In the irradiated area, bonds within the polymer chains are cleaved due to the absorption of high-energy photons, resulting in the formation of radicals. The formed radicals induce instability in adjacent bonds, causing a chain reaction of main chain cleavage and a decrease in average molecular weight. Consequently, the mechanical strength and density of the irradiated area are significantly reduced compared to the non-irradiated area, and dissolution becomes easier during the subsequent development process. As a result, the irradiated area is selectively removed, making it possible to form a fine pattern.
[0043] Unlike a step-based stepped structure, the curvature has a continuous curved phase delay distribution and provides a structure suitable for controlling phase errors in diffraction phenomena. The radius of curvature, shape precision, and curved slope are determined according to conditions such as irradiation intensity, irradiation time, and irradiation distance, which directly affect the shape precision of the subsequent X-ray shielding layer (130) transfer process.
[0044] The convex curvature structure included in the PMMA layer (120) formed in this manner and the polyimide film (110) mechanically supporting it function as a curvature mold for transferring the curvature shape to the X-ray shielding layer (130) in a subsequent step. The curvature mold can physically and optically control the diffraction angle of X-rays incident within the mask and has a structure that determines the focus formation range and image resolution on the wafer in an X-ray exposure system.
[0045] FIG. 1b illustrates a process of forming an X-ray shielding layer (130) that performs diffraction control and light blocking functions within a mask by depositing a metal material having X-ray absorption characteristics on the upper surface of a PMMA layer having a curved structure. The X-ray shielding layer (130) is deposited on the surface of the PMMA layer having a curved structure, and after being formed over the entire curved surface, the curved structure is exposed through an etching process that selectively reacts only with the metal layer. The X-ray shielding layer (130) subsequently serves as a basis for forming a concave curved structure of the final mask and affects the diffraction angle and focusing range of the light rays.
[0046] The metal material used to form the X-ray shielding layer (130) is limited to a high-density metal with a high mass absorption coefficient for X-rays, and one or more metals among lead (Pb), tungsten (W), gold (Au), bismuth (Bi), tantalum (Ta), hafnium (Hf), iridium (Ir), and barium (Ba) may be used. These high-density metals have physical properties that allow them to effectively block X-rays even with a single layer, and can secure a sufficient absorption rate even with a thin metal film with a thickness of less than a micrometer. Since X-rays have a short wavelength and strong penetration power through materials, if the thickness of the shielding layer (130) is insufficient, back-side transmission of diffracted light may occur, which may affect the exposure precision; therefore, an appropriate material is selected based on the density, absorption coefficient, crystal structure, etc. of the metal.
[0047] The X-ray shielding layer (130) can be formed by vapor deposition, sputtering, or electroplating. Preferably, a vapor deposition-based process may be applied as a uniform metal coating is required on a curved surface with a curved structure. For example, a vapor deposition method in which a metal target is vaporized at a high temperature under vacuum and condensed onto a surface can ensure excellent adhesion even on a curved shape in the case of metal materials with high condensation strength, such as tungsten or gold. At this time, it is desirable to select low-temperature deposition conditions so that delamination does not occur due to the difference in the coefficient of thermal expansion between the curvature-reactive polymer layer and the metal.
[0048] The thickness of the X-ray shielding layer (130) is generally formed to a level of several hundred nanometers to several micrometers, and if thickness uniformity is not ensured, the resolution of the curvature structure may be degraded or optically distorted phase information may be transferred. Since the detailed shape of the curvature structure directly affects the fine adjustment of the diffraction angle and the position control of the focal plane, all parameters such as the thickness variation of the X-ray shielding layer (130), surface roughness, particle size, and internal stress have a sensitive effect on the exposure resolution and linewidth variation. In particular, according to diffraction theory, the profile slope of the metal structure is a factor that controls the side lobes of the saturated diffraction region, so density control and tapered structure management in the metal deposition process are required to implement a high-resolution mask.
[0049] After the X-ray shielding layer (130) is uniformly deposited over the entire curved surface, the underlying convex curvature structure can be selectively exposed by removing a portion of the metal layer using an etching solution that reacts selectively only with the metal layer and not with the curvature-reactive polymer layer. For example, in the case of gold (Au), an etching solution of the series containing potassium iodide (KI) and iodine (I2) can be used. Through such a selective etching process, only the metal layer on the curvature structure can be removed, while the metal layer in the relatively flat region can be maintained. This method can be applied as an effective process for implementing stable X-ray shielding layer (130) patterning on a curvature structure polymer layer such as PMMA or SU-8. Furthermore, the metal structure formed after selective etching can be maintained as a concave curvature structure even after the stacked structure is inverted, and can function as a diffraction structure that controls the path of incident X-rays. In particular, the structure affects the diffraction pattern after mask transmission, which can improve the resolution limit of the exposure system and enhance image clarity on the wafer.
[0050] The design of the X-ray shielding layer (130) is carried out in correspondence with the wavelength of the incident X-ray, and, for example, based on an X-ray of 0.1 nm, a metal structure having a curvature period of about 1 to 5 μm must be formed. To achieve this, the curvature shape induced in the curvature-reactive polymer layer must be maintained without loss, and process stability must be ensured so that no warping due to thermal deformation or surface stress occurs during the metal deposition step.
[0051] FIG. 1c is a step of completing a laminated structure by laminating a material having X-ray transmission properties on top of an X-ray shielding layer (130) and a curvature structure, and additionally laminating a second polyimide film (150) that functions as a mechanical support structure on top thereof. More specifically, after the X-ray shielding layer (130) is uniformly deposited over the entire curved surface, the curvature structure is exposed by removing the metal portion corresponding to the curvature structure using an etching solution that selectively reacts only with the metal layer. After this selective etching process, a material having X-ray transmission properties is laminated on top of the X-ray shielding layer (130) and the curvature structure.
[0052] The X-ray transmission layer (140) is formed on the upper surface of the X-ray shielding layer (130) and is composed of a material that has a very low X-ray absorption coefficient and simultaneously possesses high mechanical stability and thermal conductivity, such as beryllium (Be), aluminum (Al), silicon (Si), and diamond (C). This X-ray transmission material must transmit X-rays incident from the top of the structure to the concave curvature structure of the X-ray shielding layer (130) with almost no loss, and at the same time, it also performs the role of protecting the upper part of the entire mask and maintaining the structure rigidly. Beryllium has the lowest X-ray absorption rate, and while diamond has excellent hardness and thermal conductivity, it is difficult to process and expensive. Aluminum has excellent processability and deposition properties, and silicon has excellent process compatibility, so an appropriate transmission material can be selected according to the mask specifications for actual application.
[0053] The formation of the X-ray transmission layer (140) is generally carried out by vapor deposition, sputtering, or atomic layer deposition (ALD), and since it must be continuously deposited on the curvature shape of the X-ray shielding layer (130), surface conformability of the thin film formation process is important. In particular, since the fine curvature shape of the X-ray shielding layer (130) functions as a lens that optically transmits phase information, the thickness uniformity and surface adhesion of the X-ray transmission layer (140) must be designed so that the curvature information is maintained without phase distortion. For example, the atomic layer deposition process can form a thin film with a very uniform thickness even on a curved surface, which is advantageous for maintaining curvature precision. Since the formed X-ray transmission layer (140) is used as the main path for the exposure light to be incident after the first mask is removed in a subsequent step, internal pores, interfacial defects, thickness non-uniformity, etc., must be prevented, and it is a structure that determines the optical reliability of the entire mask.
[0054] A second polyimide film (150), which is a polyimide-based polymer support layer, is laminated on top of the X-ray transmission layer (140). The second polyimide film (150) acts as a base layer that physically supports the mask at the bottom after the structure inversion, and can provide structural stability against external mechanical stress, thermal stress, handling deformation, etc. during subsequent processes. The second polyimide film (150) is selected within a thickness range of about 25 to 125 μm and can also be used as a flexible base material for substrate replacement. The second polyimide film (150) must maintain excellent flatness and tensile strength during processing, and at the same time provide sufficient mechanical rigidity to prevent alignment and pattern position deviation within the laminated structure.
[0055] The second polyimide film (150) is laminated onto the upper surface of the X-ray transmission layer (140) by adhesion or lamination rather than deposition, and the interface with the film is fixed through a thermosetting or UV-curing adhesive. Since this structure constitutes the mechanical frame of the mask structure that is finally formed, the film material, type of adhesive, difference in coefficient of thermal expansion, chemical resistance, etc., must be comprehensively considered. In particular, when the first mask is removed after the inversion process, the interfacial stability of the second polyimide film (150) plays a decisive role in maintaining the curvature structure, so the lamination quality at this stage affects the overall yield of the mask.
[0056] When the X-ray shielding layer (130), X-ray transparent layer (140), and second polyimide film (150), in which the curvature structure is exposed in this manner, are stacked in sequence, a multilayer laminated structure having a curvature structure is completed.
[0057] FIG. 1d illustrates a process of forming a concave curvature shape on the underside of an X-ray shielding layer (130) by inverting a multilayer laminated structure including a curvature structure and then removing the PMMA layer (120) that was used as a curvature mold.
[0058] Inversion of the multilayer laminated structure refers to the process of mechanically flipping the entire laminate based on the second polyimide film (150) so that the PMMA layer (120), which was the original lower structure, is exposed as the top layer. In the inverted state, the PMMA layer (120) is selectively removed based on the interface with the X-ray shielding layer (130), and the removal method is selected by considering the material properties of the PMMA layer (120) and the corrosion resistance and heat resistance of the X-ray shielding layer (130). The generally used methods are oxygen plasma etching or wet dissolution using an organic solvent, and in some cases, both methods may be performed in combination.
[0059] In the case of plasma etching, oxygen (O2) plasma is generated to cut the main chain and ester side chain bonds of the PMMA layer (120) and convert the generated low-molecular-weight compounds into volatile byproducts for removal. This method has the advantage of enabling anisotropic etching and fine-tuning. However, since excessive etching can damage the surface of the X-ray shielding layer (130), the etching time, pressure, RF power, etc., must be precisely controlled.
[0060] On the other hand, the wet dissolution method proceeds by using organic solvents with high solubility for PMMA, such as acetone, tetrahydrofuran (THF), and chloroform, to swell and dissolve the PMMA, and then remove it. This method has the advantage of not causing damage by plasma and reducing surface roughness, but additional processes are required to remove solvent residue and clean the metal surface after removal.
[0061] In addition, the PMMA layer (120) can be removed using an X-ray irradiation method. When using an X-ray irradiation method, ion bombardment and sputtering damage to the metal shielding layer (130) that may occur during oxygen plasma etching can be prevented, and solvent residue problems that occur during wet removal using an organic solvent can also be minimized.
[0062] When the PMMA layer (120) is removed, a curvature structure is directly exposed at the bottom of the X-ray shielding layer (130), and this curvature structure is formed into a concave curvature structure in which the original convex shape is inverted. The concave curvature structure performs a diffracted light control function using phase delay, and controls the distribution of the angle of incidence and the angle of diffraction when X-rays pass through this structure to focus the light rays to a specific focal point. In particular, since X-rays have a refractive index less than 1 unlike visible light, the convergence of the light rays can be induced through a concave lens shape rather than a conventional convex lens, and this structure forms a micro-scale concave metal curvature structure reflecting this characteristic.
[0063] The X-ray shielding layer (130) must preserve its internal curvature shape even after the removal process and maintain structural integrity without shape distortion or peeling damage. To this end, the X-ray shielding layer (130) must have sufficient thickness and density and must not have any pores or stress concentrations inside. Since the X-ray transmission layer (140) is continuously stacked on top of the X-ray shielding layer (130), X-rays diffracted through the concave curvature structure are radiated outward through the transmission layer, and scattering or multiple reflection of the light rays is suppressed during this process.
[0064] Additionally, the second polyimide film (150) located on top of the X-ray transmission layer (140) serves to support the entire lens structure as a substructure after the mask is inverted, and provides structural stability during mechanical handling and subsequent alignment processes. Based on thermal stability and flexibility, the second polyimide film (150) prevents twisting or deformation during the alignment, clamping, and transfer processes of the mask and maintains the structural flatness of the entire mask.
[0065] Finally, the structure illustrated in FIG. 1d is a multilayer structure composed of an X-ray shielding layer (130) having a concave curvature, an X-ray transmission layer (140) stacked on top of it, and a second polyimide film (150) located at the outermost edge, which is used directly as a microlens mask in a projection X-ray exposure process. This mask is a structure equipped with a diffraction lens function and is designed to focus X-rays within a specific focal length to precisely transfer a high-resolution pattern image onto a photosensitive film on a wafer.
[0066] Although the embodiments have been described above with reference to limited embodiments and drawings, those skilled in the art can make various modifications and variations from the description above. For example, appropriate results can be achieved even if the described techniques are performed in a different order than described, and / or the components of the described system, structure, device, circuit, etc. are combined or assembled in a form different from described, or replaced or substituted by other components or equivalents.
[0067] Therefore, other implementations, other embodiments, and equivalents to the claims also fall within the scope of the claims set forth below. Explanation of the symbols
[0068] 110: 1st PI film 120: PMMA layer 130: X-ray shielding layer 140: X-ray transmission layer 150: 2nd PI film
Claims
Claim 1 A method for manufacturing a projection-type X-ray exposure mask comprises: a step of forming a photoreactive polymer layer on a first film substrate; a step of placing an inversion pattern mask having an inversion shape of a target pattern on the photoreactive polymer layer and irradiating X-rays through the inversion pattern mask to form a convex curvature structure having a three-dimensional structure corresponding to the target pattern on the surface of the photoreactive polymer layer; a step of laminating an X-ray shielding layer on the surface where the convex curvature structure is formed so that the curved profile of the convex curvature structure is transferred to the X-ray shielding layer; a step of laminating an X-ray transmitting material on the X-ray shielding layer to form an X-ray transmitting layer after partial etching, and laminating a second film substrate on the X-ray transmitting layer by an adhesive or lamination method to form a laminated structure in which the second film substrate functions as a support film that supports the mask after a subsequent inversion process. A method for manufacturing a mask comprising the step of inverting the laminated structure based on the second film substrate and then removing the first film substrate and the photoreactive polymer layer having the convex curvature structure formed thereon, thereby forming an X-ray transmission layer having a concave curvature structure corresponding to the convex curvature structure at the bottom of the X-ray shielding layer, and forming a mask having a concave curvature structure formed thereon that controls the diffraction angle or focal position of the incident X-ray, wherein the concave curvature structure is formed to operate as a diffraction structure that controls the path of the X-ray passing through the mask. Claim 2 A method for manufacturing a mask according to claim 1, wherein the X-ray shielding layer is composed of at least one of lead (Pb), tungsten (W), gold (Au), bismuth (Bi), tantalum (Ta), hafnium (Hf), iridium (Ir), or barium (Ba). Claim 3 A method for manufacturing a mask according to claim 1, wherein the X-ray transmitting material is composed of at least one of beryllium (Be), aluminum (Al), silicon (Si), or diamond (C). Claim 4 delete Claim 5 A method for manufacturing a mask according to claim 1, characterized in that, in the step of forming the convex curvature structure, the radius of curvature of the convex curvature structure is controlled based on at least one of the irradiation distance, irradiation time, and irradiation intensity of the X-ray irradiation. Claim 6 A method for manufacturing a mask according to claim 1, wherein the mask is formed as a diffraction lens structure configured to focus incident X-rays to a target point within a predetermined focal length through the concave curvature structure. Claim 7 A method for manufacturing a mask according to claim 1, wherein the concave curvature structure formed in the mask is formed such that the deviation of the radius of curvature relative to the radius of curvature corresponding to the target pattern is maintained within ±5%.
Citation Information
Patent Citations
Mask for x-ray lithography, manufacturing method thereof, manufacturing method of light reflection prevention structure using the same, forming body using light reflection prevention structure, and manufacturing method of glass object to be formed or resin object to be formed
JP2007220732A
Dustproof film manufacturing method
JP2013257373A
mask
JP2015507213A
particle, x-ray and gamma-ray quantum beam controllers
JP3090471B2
Micro-lens array and manufacturing method thereof
KR1020050033987A