conditioner
The conditioner's multi-layer structure addresses thermal stress-induced warpage and cracking by balancing thermal stresses, ensuring uniform abrasive particle distribution and reducing manufacturing complexity and costs.
Patent Information
- Application Number
- US19/564219
- Authority / Receiving Office
- US · United States
- Patent Type
- Applications(United States)
- Current Assignee / Owner
- Priority Date
- 2025-03-14
- Filing Date
- 2026-03-12
- Publication Date
- 2026-11-12
AI Technical Summary
Conventional conditioners used in chemical-mechanical polishing processes suffer from warpage and cracking due to uneven thermal stress distribution during high-temperature brazing, leading to instability and difficulty in controlling abrasive particle distribution and flatness.
A conditioner with a multi-layer structural design, featuring a supporting structural layer, abrasive particles bonded via high-temperature brazing layers, and a composite layer bonded to a base through a low-temperature adhesive, dispersing thermal stresses and ensuring uniform abrasive particle distribution.
The multi-layer design effectively reduces warpage and cracking, maintains abrasive particle flatness, and simplifies the manufacturing process while reducing production costs.
Smart Images

Figure US20260355899A1-D00000_ABST
Abstract
Description
CROSS-REFERENCE TO RELATED PATENT APPLICATION
[0001] This application claims the benefit of priority to China Patent Application No. 202510300743.9, filed on Mar. 14, 2025, in the People's Republic of China. The entire content of the above identified application is incorporated herein by reference.
[0002] Some references, which may include patents, patent applications and various publications, may be cited and discussed in the description of this disclosure. The citation and / or discussion of such references is provided merely to clarify the description of the present disclosure and is not an admission that any such reference is “prior art” to the disclosure described herein. All references cited and discussed in this specification are incorporated herein by reference in their entireties and to the same extent as if each reference was individually incorporated by reference.FIELD OF THE DISCLOSURE
[0003] The present disclosure relates to a conditioner, and more particularly to a conditioner suitable for dressing a polishing pad.BACKGROUND OF THE DISCLOSURE
[0004] In a chemical-mechanical polishing (CMP) process or a high-precision polishing process, a polishing pad is typically used in combination with a polishing slurry to polish surfaces of workpieces such as semiconductor wafers, optical components, or glass. Generally, a conditioner is used to dress a surface of the polishing pad. The conditioner uses its abrasive layer to remove waste material remaining on the polishing pad during polishing, and restores surface roughness of the polishing pad so as to maintain stability of polishing quality.
[0005] In the related art, a brazing process is used to directly fix abrasive particles (e.g., diamond abrasive particles) onto a base of the conditioner. However, during the brazing process in which the abrasive particles are bonded from a high-temperature stage to a cooling stage, a cooling rate at a central region of the base differs from a cooling rate at an edge region of the base, and coefficients of thermal expansion of the brazing filler and the base made of metal are also different. As a result, the conditioner (i.e., a structure composed of the base, the brazing filler, and the abrasive particles) is prone to warpage or bending, and an amount of the warpage is difficult to control, thereby adversely affecting subsequent processing.
[0006] In addition, another conventional technique involves forming a grinding sheet (i.e., a structure composed of a grinding layer, brazing filler, and abrasive particles) through a pre-sintering process, and then attaching the grinding sheet to a metal base. Since the pre-sintered grinding sheet has relatively high rigidity, when the amount of warpage is excessively large, external pressure may be applied to force the bent brazed sheet, which is formed after the brazing filler cools and solidifies, to be flattened and bonded to the base of the conditioner. As a result, the brazed sheet structure may crack, thereby causing detachment of the abrasive particles.SUMMARY OF THE DISCLOSURE
[0007] In response to the above-referenced technical inadequacies, the present disclosure provides a conditioner that can prevent deformation of the conditioner caused by high-temperature thermal stress, effectively control a grinding structural member to achieve a desired warpage direction and an expected warpage magnitude, and address surface cracking issues resulting from welding thermal stress.
[0008] In order to solve the above-mentioned problems, one of the technical aspects adopted by the present disclosure is to provide a conditioner, which includes a base and a grinding structural member disposed on the base. The grinding structural member includes a supporting structural layer, a first bonding layer, a plurality of abrasive particles, a second bonding layer, and an infiltrated composite layer. The supporting structural layer has a first surface and a second surface opposite to each other. The first bonding layer is disposed on the first surface. The plurality of abrasive particles are disposed on the first surface in a single-layer arrangement and are bonded to the supporting structural layer through the first bonding layer. The second bonding layer is disposed on the second surface. The infiltrated composite layer is disposed on the second surface and is bonded to the supporting structural layer through the second bonding layer. A third bonding layer is disposed between the base and the infiltrated composite layer so as to bond the grinding structural member to the base.
[0009] Therefore, the conditioner provided by the present disclosure adopts a multi-layer structural design. Specifically, two sides of the supporting structural layer are respectively provided with high-temperature brazing bonding layers, with one side bonded to the abrasive particles and another side bonded to a porous structural layer. Accordingly, during a high-temperature manufacturing process, thermal stresses can be effectively dispersed and balanced, thereby significantly reducing warpage deformation caused by thermal stress and improving dimensional stability of the product. In addition, through a layered bonding design that combines brazing and a low-temperature adhesive, the base and the grinding structural member are prevented from undergoing high-temperature sintering together, thereby further reducing overall deformation while simplifying the manufacturing process and lowering production costs.
[0010] These and other aspects of the present disclosure will become apparent from the following description of the embodiment taken in conjunction with the following drawings and their captions, although variations and modifications therein may be effected without departing from the spirit and scope of the novel concepts of the disclosure.BRIEF DESCRIPTION OF THE DRAWINGS
[0011] The described embodiments may be better understood by reference to the following description and the accompanying drawings, in which:
[0012] FIG. 1 is a schematic cross-sectional view of a conditioner according to a first embodiment of the present disclosure;
[0013] FIG. 2 is a schematic view of step S1 of a manufacturing method of the conditioner according to the first embodiment of the present disclosure;
[0014] FIG. 3 is a schematic view of step S2 and step S3 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure;
[0015] FIG. 4 is a schematic view of steps S4, S41 and S43 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure;
[0016] FIG. 5 is a schematic view of step S5 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure;
[0017] FIG. 6 is a schematic view of step S6 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure;
[0018] FIG. 7 is a schematic view of step S7 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure;
[0019] FIG. 8 is a schematic cross-sectional view of another implementation of a base of the conditioner according to the first embodiment of the present disclosure;
[0020] FIG. 9 is a schematic cross-sectional view of a conditioner according to a second embodiment of the present disclosure; and
[0021] FIG. 10 is a schematic top view of a distribution of abrasive particles on a grinding surface of the conditioner according to the present disclosure.DETAILED DESCRIPTION OF THE EXEMPLARY EMBODIMENTS
[0022] The present disclosure is more particularly described in the following embodiments and examples that are intended as illustrative only since numerous modifications and variations therein will be apparent to those skilled in the art. Like numbers in the drawings indicate like components throughout the views. As used in the description herein and throughout the claims that follow, unless the context clearly dictates otherwise, the meaning of “a,”“an” and “the” includes plural reference, and the meaning of “in” includes “in” and “on.” Titles or subtitles can be used herein for the convenience of a reader, which shall have no influence on the scope of the present disclosure.
[0023] The terms used herein generally have their ordinary meanings in the art. In the case of conflict, the present document, including any definitions given herein, will prevail. The same thing can be expressed in more than one way. Alternative language and synonyms can be used for any term(s) discussed herein, and no special significance is to be placed upon whether a term is elaborated or discussed herein. A recital of one or more synonyms does not exclude the use of other synonyms. The use of examples anywhere in this specification including examples of any terms is illustrative only, and in no way limits the scope and meaning of the present disclosure or of any exemplified term. Likewise, the present disclosure is not limited to various embodiments given herein. Numbering terms such as “first,”“second” or “third” can be used to describe various components, signals or the like, which are for distinguishing one component / signal from another one only, and are not intended to, nor should be construed to impose any substantive limitations on the components, signals or the like.Embodiments
[0024] Reference is made to FIG. 1. FIG. 1 is a schematic cross-sectional view of a conditioner according to a first embodiment of the present disclosure. In the first embodiment, the present disclosure provides a conditioner D, which includes a base 1 and a grinding structural member 2. The grinding structural member 2 is disposed on the base 1.
[0025] The grinding structural member 2 includes a supporting structural layer 21, a plurality of abrasive particles 23, and an infiltrated composite layer 25. Moreover, the grinding structural member 2 further includes a first bonding layer 22 and a second bonding layer 24. The first bonding layer 22 is disposed between the supporting structural layer 21 and the plurality of abrasive particles 23. The second bonding layer 24 is disposed between the supporting structural layer 21 and the infiltrated composite layer 25. The supporting structural layer 21 has a first surface 211 and a second surface 212 opposite to each other. The plurality of abrasive particles 23 are disposed on the first surface 211 in a single-layer arrangement (i.e., the plurality of abrasive particles 23 form a single-layer structure), and the plurality of abrasive particles 23 are bonded to the supporting structural layer 21 through the first bonding layer 22 disposed on the first surface 211. More specifically, each of the abrasive particles 23 is partially covered by the first bonding layer 22 and partially exposed. The infiltrated composite layer 25 is disposed on the second surface 212, and the infiltrated composite layer 25 is bonded to the supporting structural layer 21 through the second bonding layer 24 disposed on the second surface 212.
[0026] It should be noted that, in the embodiments of the present disclosure, the first bonding layer 22 and the second bonding layer 24 are made of a same material and are both formed of a metal brazing filler having a melting point of at least 900 °C. In addition, a third bonding layer 3 is disposed on a side of the infiltrated composite layer 25 that is away from the supporting structural layer 21, and the infiltrated composite layer 25 is bonded to the base 1 through the third bonding layer 3. In other words, the grinding structural member 2 can be fixed to the base 1 through the third bonding layer 3.
[0027] In the first embodiment, the supporting structural layer 21 is formed as a metal plate. Specifically, a thickness of the metal plate (e.g., SUS316L) ranges from 0.03 mm to 2 mm. When the thickness of the metal plate is excessively large (e.g., greater than 2 mm), planarization after a brazing or bonding process becomes difficult. Conversely, when the thickness of the metal plate is excessively small (e.g., less than 0.03 mm), the critical buckling stress thereof is significantly reduced, such that wrinkles or wave-like deformation are likely to occur during the manufacturing process, thereby making it difficult to satisfy practical application requirements.
[0028] A manufacturing process of the conditioner D of the first embodiment will be described below with reference to the above structural configuration. Reference is made to FIGS. 2 to 7. FIGS. 2 to 7 illustrate steps S1 to S7 of a manufacturing method of the conditioner according to the first embodiment.
[0029] Initially, reference is made to FIG. 2, and FIG. 2 is a schematic view of step S1 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure. In step S1, a supporting structural layer 21 formed as a metal plate is provided, and a first metal brazing filler B1 and a second metal brazing filler B2 are respectively disposed on the first surface 211 and the second surface 212 of the supporting structural layer 21. The first metal brazing filler B1 and the second metal brazing filler B2 can be made of the same material and have a melting point ranging from 900 °C to 1100 °C. For example, the materials of the first metal brazing filler B1 and the second metal brazing filler B2 can include a metal alloy, preferably a nickel-based alloy (BNi-2). In addition, the metal brazing filler (i.e., the first metal brazing filler B1 and the second metal brazing filler B2) can be in the form of a brazing foil, brazing paste, brazing powder, or a mixture of brazing powder and resin, and the present disclosure is not limited thereto.
[0030] Then, reference is made to FIG. 3, and FIG. 3 is a schematic view of step S2 and step S3 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure. In step S2, a plurality of abrasive particles 23 are provided so that the plurality of abrasive particles 23 form a single-layer grinding structure. The plurality of abrasive particles 23 are disposed on the first surface 211 and are in contact with the first metal brazing filler B1. Moreover, in step S3, a metal porous layer M is provided and disposed on the second surface 212 so as to contact the second metal brazing filler B2.
[0031] The abrasive particles 23 can include, but are not limited to, single-crystal diamond, polycrystalline diamond, polycrystalline diamond compact (PCD), CVD diamond, diamond, cubic boron nitride (cBN) particles, silicon carbide particles, or any combination thereof. The metal porous layer M is a metal porous structure having a plurality of pores distributed on its interior and surface. The material of the metal porous layer M can include, but is not limited to, nickel, iron, copper, titanium, molybdenum, cobalt, chromium, stainless steel, nickel alloys, iron alloys, copper alloys, or titanium alloys.
[0032] In addition, the metal porous layer M can have, but is not limited to, a mesh structure, a foamed structure, or a fibrous structure. In a preferred embodiment, the metal porous layer M can be formed of foamed nickel or an alloy thereof, such as nickel foam. In other embodiments, the metal porous layer M can be formed of foamed titanium, foamed stainless steel, or nickel fibers. Furthermore, for example, the metal porous layer M can be fabricated by powder metallurgy, hot extrusion, molten metal processing, electroplating, electrochemical deposition, or casting processes.
[0033] Then, FIG. 4 is a schematic view of step S4, step S41, and step S43 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure. In step S4, a stacked structure composed of the abrasive particles 23, the supporting structural layer 21, and the metal porous layer M is placed into a vacuum brazing furnace C to perform a brazing process. The first metal brazing filler B1 and the second metal brazing filler B2 are heated to a high temperature (e.g., above 900 °C) in the vacuum brazing furnace C so as to melt into a molten state.
[0034] During the melting process, the first metal brazing filler B1 bonds the plurality of abrasive particles 23 to the supporting structural layer 21 and, after cooling and solidification, forms the first bonding layer 22. On the other hand, when the second metal brazing filler B2 melts, a portion of the second metal brazing filler B2 infiltrates into the pores of the metal porous layer M and cooperates with the metal porous layer M to form the infiltrated composite layer 25. The remaining portion of the second metal brazing filler B2 that does not infiltrate into the metal porous layer M cools and solidifies to form the second bonding layer 24. Accordingly, the first bonding layer 22 and the second bonding layer 24 bond the supporting structural layer 21, the plurality of abrasive particles 23, and the infiltrated composite layer 25 together as an integral structure, thereby forming the grinding structural member 2.
[0035] It should be noted that when the second metal brazing filler B2 infiltrates into the metal porous layer M, the metal porous layer M maintains its initial thickness and is not compressed. Therefore, the second metal brazing filler B2 only infiltrates and fills an upper portion of the metal porous layer M, while a lower portion of the metal porous layer M is not filled by the second metal brazing filler B2.
[0036] Reference is further made to FIG. 4. Step S4 cam further include step S41 and step S43. When the stacked structure composed of the abrasive particles 23, the supporting structural layer 21, and the metal porous layer M is placed on a platform E1 in the vacuum brazing furnace C to perform the brazing process, a pressing plate P1 is provided and disposed above the stacked structure. The pressing plate P1 is mainly configured to hold the abrasive particles 23 in position during the brazing process. By applying downward pressure through the pressing plate P1, displacement of the abrasive particles 23 during the brazing process can be suppressed, thereby stabilizing the sintering process of the grinding structural member 2.
[0037] In the brazing process shown in FIG. 4, the grinding structural member 2 is disposed on the platform E1 with the metal porous layer M facing downward, wherein the metal porous layer M is converted into the infiltrated composite layer 25 after brazing. However, the present disclosure is not limited thereto. In another embodiment, the grinding structural member 2 can also be inverted, such that the grinding structural member 2 is placed on the platform E1 inside the vacuum brazing furnace C, with the side provided with the abrasive particles 23 facing downward.
[0038] Then, reference is made to FIGS. 5 and 6. FIG. 5 is a schematic view of step S5 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure, and FIG. 6 is a schematic view of step S6 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure. In step S5, an adhesive B3 is disposed on a side of the grinding structural member 2 that faces away from the supporting structural layer 21 (i.e., a surface of the metal porous layer M that does not contact the second metal brazing filler B2). In step S6, a base 1 is provided, the grinding structural member 2 is disposed on the base 1, and the adhesive B3 is in contact with a bonding surface 11 of the base 1 so that the adhesive B3 bonds the base 1 and the grinding structural member 2. For example, the adhesive B3 can include, but is not limited to, low-temperature metal brazing filler, polymer binder, epoxy resin, polymethyl methacrylate (PMMA), or phenolic resin, and the melting point of the adhesive B3 is lower than 400 °C.
[0039] Then, reference is made to FIG. 7. FIG. 7 is a schematic view of step S7 of the manufacturing method of the conditioner according to the first embodiment of the present disclosure. In step S7, a low-temperature (for example, below 400 °C) and high-pressure bonding process can be performed. During the bonding process, the grinding structural member 2 and the base 1 are placed on a platform E2, and a pressing plate P2 is provided to apply downward pressure to the grinding structural member 2 and the base 1. The pressing plate P2 has a rigid and planar pressing surface, such that the plurality of abrasive particles 23 on the grinding structural member 2 are subjected to uniform pressing during the pressing process, thereby causing the tip heights of the abrasive particles 23 to become substantially consistent and forming an abrasive particle layer having equal heights and uniform distribution. In other words, the flatness of the pressing plate P2 affects the flatness of the abrasive layer formed by the abrasive particles 23. Subsequently, a portion of the adhesive B3 infiltrates into the infiltrated composite layer 25, and another portion of the adhesive B3 solidifies to form the third bonding layer 3, thereby firmly bonding the grinding structural member 2 to the base 1 and forming the conditioner D.
[0040] Specifically, the infiltrated composite layer 25 includes an upper layer portion 251 and a lower layer portion 252. The upper layer portion 251 is a portion of the metal porous layer M that has been infiltrated by the second metal brazing filler B2, and the lower layer portion 252 is a portion of the metal porous layer M that has not been infiltrated by the second metal brazing filler B2. Since the lower layer portion 252 has not been infiltrated by the second metal brazing filler B2, the lower layer portion 252 forms a compressible elastic layer. When the pressing plate P2 applies downward pressure, the lower layer portion 252 is compressed to reduce its thickness, while the upper layer portion 251 maintains its initial thickness because it is filled with the second metal brazing filler B2.
[0041] Since the upper layer portion 251 and the lower layer portion 252 are compressed to different extents, the porosity within the infiltrated composite layer 25 is different between the upper and lower portions. Specifically, the porosity of the upper layer portion 251 is greater than the porosity of the lower layer portion 252. For example, the porosity of the upper layer portion 251 is greater than 50%, and the porosity of the lower layer portion 252 is less than 50%. It should be noted that porosity is defined as the ratio of a total volume of pores in a material (or structure) to an overall volume of the material.
[0042] It should be noted that in the bonding process shown in FIG. 7, the conditioner D is disposed on the platform E2 with the base 1 facing downward. However, the present disclosure is not limited thereto. In another embodiment, the conditioner D can also be inverted, such that the side of the grinding structural member 2 on which the abrasive particles 23 are disposed faces downward and is placed on the platform E2. In other words, in the bonding process, the placement orientation or order of the conditioner D on the platform E2 is not limited in the present disclosure. Regardless of whether the base 1 or the grinding structural member 2 faces downward as the lower support, the downward pressing action of the pressing plate P2 uniformly presses the plurality of abrasive particles 23, thereby achieving height leveling. Accordingly, the flatness of the finally formed abrasive particle layer and the bonding quality and performance of the conditioner D are not affected.
[0043] Referring to FIG. 8, FIG. 8 is a schematic cross-sectional view of another implementation of a base of the conditioner according to the first embodiment of the present disclosure. In other embodiments, a retaining wall 12 can be provided along a periphery of the bonding surface 11 of the base 1. The retaining wall 12 and the bonding surface 11 jointly define an accommodating cavity. The grinding structural member 2 is disposed within the accommodating cavity and fixed on the base 1 through the third bonding layer 3, thereby preventing displacement during the bonding process and avoiding adhesive overflow.
[0044] Reference is made to FIG. 9. FIG. 9 is a schematic cross-sectional view of a conditioner according to a second embodiment of the present disclosure. The conditioner D of the second embodiment has a structure and manufacturing process similar to those of the first embodiment, and the similarities will not be reiterated herein. The main difference between the second embodiment and the first embodiment lies in that, in the second embodiment, the supporting structural layer 21 is a compressed metal porous structure having a porosity less than 50%. Specifically, when the grinding structural member 2 undergoes the brazing process in the vacuum brazing furnace C and is formed by compression, a portion of the molten first metal brazing filler B1 infiltrates into pores on the first surface 211 of the supporting structural layer 21, while the remaining portion of the first metal brazing filler B1 that does not infiltrate into the supporting structural layer 21 cools and solidifies to form the first bonding layer 22. Similarly, a portion of the molten second metal brazing filler B2 infiltrates into pores on the second surface 212 of the supporting structural layer 21, while the remaining portion of the second metal brazing filler B2 that does not infiltrate into the supporting structural layer 21 cools and solidifies to form the second bonding layer 24.
[0045] Reference is made to FIG. 10. FIG. 10 is a schematic top view of a distribution of abrasive particles on a grinding surface of the conditioner according to the present disclosure. For example, an effective measurement region A1 is defined on a grinding surface G of the conditioner D, wherein the measurement region excludes an innermost ring region A2 of the grinding surface (e.g., a region extending outward from a center point of the grinding surface by a radius of 2 mm) and an outermost ring region A3 (e.g., a region extending inward from an edge of the grinding surface G by 2 mm), so as to avoid interference caused by edge structures. Then, the effective measurement region A1 is radially divided into an outer ring region A11 and an inner ring region A12, and the height distribution of the tips of the abrasive particles 23 can be measured using a 3D surface scanner or a platform equipped with a dial gauge. Subsequently, ten of the abrasive particles 23 having the greatest heights are selected from each of the outer ring region A11 and the inner ring region A12 as effective contact points. A best-fit plane is then calculated using height data of the tips of the ten abrasive particles 23. Based on the best-fit plane, height deviation values of the tips of the abrasive particles 23 relative to the best-fit plane are obtained (in units of μm), wherein a maximum height deviation value is defined as Hmax and a minimum height deviation value is defined as Hmin. Finally, a flatness of the conditioner D is defined as a difference between the maximum height deviation value and the minimum height deviation value, and the calculation formula is as follows: Flatness=Hmax−Hmin.
[0046] Through the above measurement method, flatness values corresponding to the plurality of abrasive particles 23 located in the outer ring region A11 and the inner ring region A12 on the grinding surface G of the conditioner D can be obtained respectively, and a difference between the flatness values of the outer ring region A11 and the inner ring region A12 is less than 0.05 mm.
[0047] However, it should be noted that the above inner-ring and outer-ring measurement method is not limited in the present disclosure. In another embodiment, flatness of the grinding surface G of the conditioner D can be measured using a nine-grid measurement method. Specifically, with the geometric center of the grinding surface G as a reference, the grinding surface G is divided into a plurality of measurement regions, which are equally spaced to form nine subregions arranged in three rows and three columns.
[0048] Then, within each of the subregions, the height distribution of the tips of a plurality of abrasive particles located in the subregion is measured using a 3D surface scanner or a platform equipped with a dial gauge. A plurality of abrasive particles having relatively greater heights are then selected from each subregion as effective contact points. Subsequently, based on tip height data of the effective contact points in each subregion, a best-fit plane is calculated to obtain a maximum height deviation value and a minimum height deviation value, thereby determining a flatness value for each subregion. By comparing the flatness values of the subregions, height uniformity of the grinding surface G of the conditioner D at different positions can be evaluated.Beneficial Effects of the Embodiments
[0049] Conventional conditioners or grinding structural members generally directly braze abrasive particles onto a metal sheet using a high-temperature brazing filler, or further subject the abrasive particles, the metal sheet, and the base to an overall high-temperature sintering process. However, in such structural designs, significant differences in material properties (e.g., coefficients of thermal expansion) exist among the abrasive particles, the metal sheet, the brazing layer, and the base. As a result, non-uniform thermal stress distribution is likely to occur during high-temperature sintering and subsequent cooling processes. Consequently, the grinding structural member may exhibit central bulging, warpage, or wave-like deformation. For example, when the thickness of the metal sheet is relatively small, compressive stress tends to be generated in a central region during cooling of the brazing filler, while tensile stress tends to be generated in edge regions, thereby making the warpage of the overall structure more pronounced. Consequently, a subsequent bonding process with the base is adversely affected, and it is also difficult to effectively control flatness and equal-height distribution of the abrasive particles. In addition, some conventional techniques attempt to address the above problems by adopting multi-layer abrasive structures or overall high-temperature sintering processes. However, such approaches involve complicated manufacturing processes and high costs, and still cannot simultaneously satisfy requirements for stress control and planar adjustment.
[0050] In contrast to the above conventional techniques, the conditioner provided by the present disclosure effectively improve problems of thermal stress concentration and warpage deformation through a multi-layer structural design. Specifically, a first bonding layer 22 and a second bonding layer 24 formed of metal brazing filler are respectively disposed on two opposite sides of the supporting structural layer 21 (e.g., a metal plate). During a high-temperature brazing process, the plurality of abrasive particles 23 and the metal porous layer M are respectively bonded to upper and lower sides of the supporting structural layer 21, such that the abrasive particles 23, the supporting structural layer 21, and the metal porous layer M form a vertically symmetrical layered structure having a stress-balancing effect. As a result, warpage caused by differences in coefficients of thermal expansion among different materials is significantly reduced.
[0051] Furthermore, in a subsequent low-temperature bonding process of the present disclosure, the infiltrated composite layer 25 formed jointly by the metal porous layer M and the metal brazing filler therein is bonded to the base 1 through the third bonding layer 3 formed of an adhesive. Accordingly, the infiltrated composite layer 25 can function as a compressible buffer layer during the bonding stage. The infiltrated composite layer 25 cooperates with a rigid and planar pressing plate P2 to perform downward pressing and planarization, thereby effectively adjusting and controlling the equal-height distribution and flatness of the abrasive particles 23. Furthermore, the base 1 and the grinding structural member 2 are prevented from undergoing the high-temperature brazing process together, thereby further reducing overall deformation.
[0052] The foregoing description of the exemplary embodiments of the disclosure has been presented only for the purposes of illustration and description and is not intended to be exhaustive or to limit the disclosure to the precise forms disclosed. Many modifications and variations are possible in light of the above teaching.
[0053] The embodiments were chosen and described in order to explain the principles of the disclosure and their practical application so as to enable others skilled in the art to utilize the disclosure and various embodiments and with various modifications as are suited to the particular use contemplated. Alternative embodiments will become apparent to those skilled in the art to which the present disclosure pertains without departing from its spirit and scope.
Claims
1. A conditioner, comprising:a base; anda grinding structural member disposed on the base, the grinding structural member including:a supporting structural layer having a first surface and a second surface opposite to the first surface;a first bonding layer disposed on the first surface;a plurality of abrasive particles disposed on the first surface in a single-layer arrangement and bonded to the supporting structural layer through the first bonding layer;a second bonding layer disposed on the second surface; andan infiltrated composite layer disposed on the second surface and bonded to the supporting structural layer through the second bonding layer; anda third bonding layer disposed on a side of the infiltrated composite layer that is away from the supporting structural layer and configured to bond the infiltrated composite layer to the base.
2. The conditioner according to claim 1, wherein the supporting structural layer is a metal plate.
3. The conditioner according to claim 1, wherein the first bonding layer and the second bonding layer are made of a same material and are both formed of a metal brazing filler having a melting point of at least 900 °C.
4. The conditioner according to claim 3, wherein the supporting structural layer is a compressed metal porous structure.
5. The conditioner according to claim 4, wherein a porosity of the compressed metal porous structure is less than 50%.
6. The conditioner according to claim 4, wherein, when the metal brazing filler forming the first bonding layer is in a molten state, a portion of the metal brazing filler infiltrates into pores of the metal porous structure, and a remaining portion that does not infiltrate forms the first bonding layer.
7. The conditioner according to claim 1, wherein the infiltrated composite layer is formed by infiltration of a portion of a metal brazing filler into a metal porous layer, and a remaining portion of the metal brazing filler forms the second bonding layer.
8. The conditioner according to claim 7, wherein the third bonding layer is formed of an adhesive, and when the adhesive is used to bond the grinding structural member to the base, a portion of the adhesive infiltrates into the infiltrated composite layer; and wherein the infiltrated composite layer includes an upper layer portion and a lower layer portion, the upper layer portion is a portion infiltrated by the metal brazing filler, and the lower layer portion is a portion infiltrated by the adhesive.
9. The conditioner according to claim 8, wherein the infiltrated composite layer is a multi-layer porous composite layer, and a porosity of the upper layer portion of the infiltrated composite layer is greater than a porosity of the lower layer portion.
10. The conditioner according to claim 8, wherein the adhesive includes a polymer binder, epoxy resin, polymethyl methacrylate (PMMA), phenolic resin, or a metal solder, and a melting point of the adhesive is lower than 400 °C.
11. The conditioner according to claim 1, wherein a grinding surface defined by the plurality of abrasive particles of the grinding structural member defines an effective measurement area, the effective measurement area is radially divided into an outer ring region and an inner ring region, and a difference between a flatness of the outer ring region and a flatness of the inner ring region is less than 0.05 mm.