Recycled Cowhide Fiber Eco-Friendly Leather, Production Line, and Manufacturing Process
The recycled cowhide fiber eco-friendly leather with a double-suede base fabric and thermosensitive hydrogel fibers addresses shape and color limitations of traditional leather, enhancing bonding strength and breathability, achieving customizable and durable products.
Patent Information
- Application Number
- US19/375203
- Authority / Receiving Office
- US · United States
- Patent Type
- Applications(United States)
- Current Assignee / Owner
- Priority Date
- 2025-05-09
- Filing Date
- 2025-10-30
- Publication Date
- 2026-11-12
AI Technical Summary
Traditional genuine leather is irregular in shape and size, contains natural defects, and has fixed color and grain patterns, limiting its utilization and customization, while conventional recycled leather processes face issues with weak bonding strength and low hydroentanglement density.
A recycled cowhide fiber eco-friendly leather with a structure comprising a cowhide fiber surface layer, a double-suede base fabric layer with fleece on both surfaces, and a cowhide fiber bottom layer, using a binding warp double-layer weave and island-in-the-sea yarns for enhanced interlacing and crosslinking, along with thermosensitive hydrogel fibers for adaptive breathability.
The leather achieves customizable lengths and colors, improved interlayer bonding strength, and enhanced durability with adaptive breathability, addressing the limitations of traditional leather and conventional recycled leather processes.
Smart Images

Figure US20260357509A1-D00000_ABST
Abstract
Description
CROSS-REFERENCE TO RELATED APPLICATIONS
[0001] This application is a continuation of International Application No. PCT / CN2025 / 113810, filed on Aug. 11, 2025, which claims foreign priority of Chinese Patent Application No. 202510596979.1, filed on May 9, 2025 in the China National Intellectual Property Administration (CNIPA), the entire contents of which are hereby incorporated by reference in their entireties.TECHNICAL FIELD
[0002] The present invention relates to the field of fabric technology, and more particularly to a recycled cowhide fiber eco-friendly leather, as well as its production line and manufacturing process.BACKGROUND OF THE INVENTION
[0003] In the field of leather manufacturing, traditional genuine leather has long been widely used across various industries due to its superior texture and performance. However, since genuine leather is primarily derived from animal hides, it faces numerous limitations. On one hand, genuine leather is irregular in shape and size, and its surface often contains natural defects such as scars, resulting in a relatively low utilization rate. On the other hand, the color and grain pattern of genuine leather are relatively fixed, making it difficult to customize according to diverse customer needs, thereby restricting its range of applications to some extent. To address these issues associated with traditional genuine leather, recycled leather technologies have been developed. In commonly used recycled leather processes, cowhide waste materials are often subjected to simple processes such as buffing and fiber separation, followed by compounding with other fibers or materials. Meanwhile, in terms of base fabric selection and application, conventional woven base fabrics are typically employed. These base fabrics mainly rely on simple physical adhesion or limited chemical crosslinking when combined with cowhide fibers. Additionally, such base fabrics usually adopt a single-yarn structure, with relatively simple interlacing and bonding between yarns, making it difficult to achieve strong adhesion with cowhide fibers during compounding. The density of hydroentanglement crosslinking is often low, which in turn affects the bonding strength between the layers of the leather and its overall performance. In view of the foregoing, the present invention has been developed.SUMMARY OF THE INVENTION
[0004] One objective of the present invention is to provide a recycled cowhide fiber eco-friendly leather, along with its production line and manufacturing process, to solve at least the aforementioned problems.
[0005] To achieve the above objectives, the technical solution adopted by the present invention is as follows: The recycled cowhide fiber eco-friendly leather comprises, from top to bottom, a cowhide fiber surface layer, a double-suede base fabric layer, and a cowhide fiber bottom layer. Both the upper and lower surfaces of the double-suede base fabric layer are provided with fleece. The cowhide fibers of the surface layer and bottom layer are crosslinked with the yarn fibers and fleece fibers of the double-suede base fabric layer.
[0006] Preferably, the fabric structure of the double-suede base fabric layer is a binding warp double-layer structure, wherein the fabric surface layer is formed by interweaving surface warps and surface wefts, and the fabric inner layer is formed by interweaving inner warps and inner wefts. The binding warps are interwoven with both the surface and inner wefts, thereby connecting the surface and inner layers of the base fabric to one another.
[0007] Preferably, in the binding warp double-layer structure, the surface fabric adopts a 2-over-2-under right-hand twill weave, and the inner fabric adopts a 1-over-3-under right-hand twill weave. The warp yarn arrangement sequence is one surface warp, one inner warp, and one binding warp, while the weft yarn arrangement sequence is one surface weft and one inner weft.
[0008] Preferably, the surface and inner warps are island-in-the-sea yarns, which are composite yarns formed by network processing of island-in-the-sea fibers and high-shrinkage fibers. The island-in-the-sea fibers are produced by composite spinning of a sea component encapsulating an island component, wherein the sea component is low-viscosity PET, the island component is a PBT / IPA copolymer, and the high-shrinkage fiber is modified PET. The binding warp is a high-strength PA66 filament, and the surface and inner wefts are modified PA6 staple fiber yarns.
[0009] Preferably, the raw materials of the island-in-the-sea yarns comprise, by parts by weight, the following components: 65-70 parts of low-viscosity PET, 35-40 parts of PBT / IPA copolymer, 30-35 parts of modified PET, and 0.6-0.8 parts of network oiling agent.
[0010] Preferably, the slurry composition for the cowhide fiber surface layer and the cowhide fiber bottom layer comprises, by parts by weight, the following components: 90-100 parts of recycled cowhide fiber, 5-8 parts of plant fiber, 8-10 parts of thermosensitive hydrogel fiber, 3-5 parts of nanocellulose whiskers, and 5-8 parts of waterborne polyurethane.
[0011] The production line for the above-described recycled cowhide fiber eco-friendly leather comprises an inclined wire paper-making machine, a base fabric unwinding machine, a base fabric conveyor, a composite conveyor, a hydroentanglement device, and a drying device. Two inclined wire paper-making machines are provided. The base fabric unwinding machine is positioned at the front end of the base fabric conveyor. The hydroentanglement device and the drying device are sequentially arranged at the rear end of the composite conveyor. A carding machine is arranged at the end of the base fabric conveyor, and the carding machine is provided with oppositely arranged upper and lower carding rollers. Downstream of the carding machine are oppositely arranged upper air knives and lower suction rollers, followed by oppositely arranged upper and lower ionizing air bars.
[0012] The production process for the above-described recycled cowhide fiber eco-friendly leather comprises the following steps:
[0013] Step a: Preparing a double-suede base fabric.
[0014] Step b: Forming a cowhide fiber slurry sheet using the inclined wire paper-making machine.
[0015] Step c: Unwinding the pre-prepared double-suede base fabric using the base fabric unwinding machine.
[0016] Step d: Conveying the double-suede base fabric through the base fabric conveyor, wherein the base fabric is sandwiched between cowhide fiber slurry sheets formed by the two inclined wire paper-making machines, and the resulting layers are superposed on the composite conveyor to form a sandwich-structured fabric.
[0017] Step e: Feeding the fabric into the hydroentanglement device, where the cowhide fiber surface layer, double-suede base fabric layer, and cowhide fiber bottom layer are subjected to hydroentanglement bonding.
[0018] Step f: Passing the hydroentangled composite substrate sequentially through dewatering, cylindrical drying, harmful substance removal, and mesh-cylinder drying processes, followed by final winding into rolls.
[0019] Preferably, the preparation process of the double-suede base fabric comprises the following steps:
[0020] Step a: Preparation of island-in-the-sea yarns.
[0021] Step b: Weaving the base fabric having a double-layer structural organization.
[0022] Step c: Alkali treatment: Treating the woven base fabric with a 10% NaOH solution at a temperature of 90 °C for 30 minutes.
[0023] Step d: Double-sided sueding: Using a ceramic abrasive disk for double-sided sueding at a rotation speed of 1500 rpm and a pressure of 0.15 MPa.
[0024] Preferably, the preparation process of the island-in-the-sea yarn comprises the following steps: after melting sea-component chips and island-component chips, extruding the melt through an island-in-the-sea spinneret to form an island-in-the-sea fiber with a 16-island structure; combining the island-in-the-sea fiber and high-shrinkage fiber in a predetermined ratio to form the island-in-the-sea yarn through network processing, followed by treatment with a polyether-based network oiling agent.
[0025] From the foregoing description, it can be understood that the recycled cowhide fiber eco-friendly leather, as well as its production line and manufacturing process provided by the present invention, offer the following advantages: Cowhide waste is subjected to buffing and fiber separation to obtain recycled cowhide fibers. The recycled cowhide fiber serves as the primary component of both the cowhide fiber surface layer and bottom layer, thereby enabling the resulting eco-friendly leather to possess a hand feel similar to genuine leather, along with excellent tear resistance and tensile strength. This effectively addresses the low utilization rate of traditional genuine leather caused by irregular shape, limited sheet size, and natural defects such as surface scars. The recycled leather can be manufactured in customizable lengths according to product requirements, and various colors and grain patterns can be tailored to meet customer preferences, overcoming the limitations of natural leather in terms of color and texture. The inclusion of thermosensitive hydrogel fibers allows the inter-fiber spacing within the material to self-adjust in response to ambient humidity, thereby imparting adaptive breathability to the material. Moreover, the base fabric layer is provided with evenly distributed fleece on both upper and lower surfaces. This uniform fleece structure significantly enhances the degree of interlacing between the base fabric and cowhide fibers during hydroentanglement, thereby improving the interlayer bonding strength of the composite fabric. The double-suede base fabric layer combines the tensile strength of woven fabrics with the high interlacing density of nonwoven fabrics, resulting in recycled cowhide fiber eco-friendly leather with superior transverse tensile strength and longitudinal adhesion. Consequently, the durability of the recycled cowhide fiber eco-friendly leather is greatly improved.BRIEF DESCRIPTION OF DRAWINGS
[0026] FIG. 1 is a schematic structural diagram of the recycled cowhide fiber eco-friendly leather.
[0027] FIG. 2 is a fabric structural diagram of the double-suede base fabric layer.
[0028] FIG. 3 is a longitudinal sectional view of the double-suede base fabric layer.
[0029] FIG. 4 is a schematic structural diagram of the production line for the recycled cowhide fiber eco-friendly leather.
[0030] FIG. 5 is a schematic structural diagram of the carding machine.DETAILED DESCRIPTION OF THE INVENTION
[0031] The present invention is further described below through specific embodiments.
[0032] To facilitate a clearer understanding of the technical means, innovative features, objectives, and advantages achieved by the present invention, the following detailed embodiments are provided in conjunction with the accompanying drawings.
[0033] As shown in FIG. 1, the recycled cowhide fiber eco-friendly leather of the present invention comprises, from top to bottom, a cowhide fiber surface layer 10, a double-suede base fabric layer 20, and a cowhide fiber bottom layer 30. Both the upper and lower surfaces of the double-suede base fabric layer 20 are provided with fleece. The cowhide fibers of the surface layer 10 and bottom layer 30 are crosslinked with the yarn fibers and fleece fibers of the double-suede base fabric layer 20. In the present invention, the incorporation of a base fabric with fleece distributed on both sides significantly enhances the degree of interlacing between the base fabric layer and cowhide fibers during hydroentanglement. The uniformly distributed fleece structure markedly improves the bonding strength between the composite fabric layers. The double-suede base fabric layer 20 combines the tensile strength of woven fabrics with the high crosslinking characteristics of nonwoven fabrics, thereby providing the recycled cowhide fiber eco-friendly leather with both excellent transverse tensile strength and longitudinal adhesion, resulting in improved overall durability.
[0034] The fabric structure of the double-suede base fabric layer 20 is a binding warp double-layer structure. In this structure, the surface fabric layer is formed by interweaving surface warps and surface wefts, while the inner fabric layer is formed by interweaving inner warps and inner wefts. The binding warps are interwoven simultaneously with both the surface and inner wefts, thereby connecting the surface and inner layers of the base fabric. By employing this dual-layer structural design, the double-suede base fabric layer 20 achieves a dual-surfaced pile texture while maintaining sufficient tensile strength. Since the binding warp fibers are composed of materials different from those of the surface and inner warps, they are resistant to alkali dissolution. Moreover, the binding warps are embedded between the surface and inner layers, effectively connecting the two layers together. During the sueding process, no physical deformation occurs in the binding warps, thereby ensuring consistent connection strength between the surface and inner layers.
[0035] In the binding warp double-layer structure, the surface fabric adopts a 2-over-2-under right-hand twill weave, while the inner fabric adopts a 1-over-3-under right-hand twill weave. The warp yarns are arranged in the sequence of one surface warp, one inner warp, and one binding warp, and the weft yarns are arranged in the sequence of one surface weft and one inner weft. As shown in FIG. 2, which illustrates the weaving draft of the fabric structure, the Chinese numerals “1, 2, 3, 4” represent the surface warps and surface wefts, the Roman numerals “I, II, III, IV” represent the inner warps and inner wefts, and the letters “a, b, c, d” denote the binding warps. The intersections of surface warps and surface wefts are marked with the surface weave symbol “★”, the intersections of inner warps and inner wefts are marked with the inner weave symbol “☆”, the binding points are indicated by “Δ”, the lifting heddles by “O”, and “□” represents the positions where the surface warp is not lifted during the insertion of the inner weft. As shown in FIG. 3, which depicts the longitudinal cross-sectional view, the binding warp “a” interlaces respectively with the surface weft “1” and the inner weft “III”. The structure comprises two sets of yarn systems, wherein the binding warp is embedded between the surface and inner layers, effectively joining the two layers together. This design ensures structural stability and enhances fabric durability. After the alkali treatment and sueding processes, fleece fibers are formed along the floating lines of both the outer and inner warps.
[0036] The surface warps and inner warps are island-in-the-sea yarns, which are composite yarns formed by network processing of island-in-the-sea fibers and high-shrinkage fibers. The island-in-the-sea fibers are produced by composite spinning in which the sea component encapsulates the island component. The sea component is low-viscosity PET, the island component is a PBT / IPA copolymer, and the high-shrinkage fiber is modified PET. The binding warp is a high-strength PA66 filament, and the surface and inner wefts are modified PA6 staple fiber yarns. The low-viscosity PET used as the sea component possesses excellent alkali solubility, with an intrinsic viscosity of 0.60 dL / g. Acting as the continuous phase surrounding the island component, it dissolves during alkali treatment to form fleece gaps, achieving a dissolution rate of ≥98% under conditions of 10% NaOH at 90 °C for 30 minutes. The PBT / IPA copolymer used as the island component is resistant to alkali hydrolysis, with a strength retention rate of ≥95% after alkali treatment. It forms 16 radially distributed ultrafine fibers with diameters of 1-2 μm and a specific surface area of 6-8 m2 / g, thereby enhancing hydroentanglement anchoring points. The high-shrinkage fiber, made of modified PET, preferably comprises a copolymerized polyethylene terephthalate with 8% isophthalic acid as a comonomer to improve shrinkage performance. Additionally, 0.5% triphenyl phosphite is added as a thermal stabilizer to suppress thermo-oxidative degradation during high-temperature shrinkage processing, and 1% nano-silica is incorporated as an alkali-resistant additive dispersed within the PET matrix, forming an alkali-resistant barrier that enhances chemical durability. After copolymerization modification, the fibers are immersed in a 0.3% fluorocarbon resin solution to form an alkali-resistant coating, reducing alkali absorption by 40%. All the percentages described herein are by weight. The monofilament fineness is 75 dtex / 36 f, with a circular cross-section and a boiling-water shrinkage rate of 38%. During shrinkage, the high-shrinkage fibers exert mechanical tension on the floating yarns of the island-in-the-sea structure, inducing curvature that facilitates fleece formation while maintaining excellent alkali stability. The island-in-the-sea yarns float along both the upper and lower surfaces of the base fabric. After alkali treatment, the fixed state of the high-shrinkage fibers is disrupted, causing them to contract. Meanwhile, the sea component dissolves as the continuous phase, leaving the island microfibers in a relaxed, entangled configuration around the high-shrinkage fibers. These island microfibers consist of ultrafine filaments with extremely small diameters that fracture during the sueding process, forming numerous fine and uniformly distributed fleece clusters on both the inner and outer surfaces of the base fabric. These fleece clusters significantly enhance the bonding strength with the cowhide fibers. Testing results show that the recycled cowhide fiber eco-friendly leather prepared with the double-suede base fabric exhibits a fleece density of 3,000fibers / cm2. Compared with recycled cowhide fiber leather made using conventional base fabrics such as plain weave or twill weave structures, the hydroentanglement anchoring points are substantially increased. Scanning Electron Microscope (SEM) observations of cross-sections indicate that the hydroentanglement depth is doubled, and the interlayer peel strength increases by 30-40%, reaching ≥80 N / cm. The binding warps are embedded between the dual fabric layers, minimizing exposure to alkali. Both the high-strength PA66 filaments and the modified PA6 staple fiber yarns are coated with a fluorocarbon resin layer, which reduces alkali absorption and improves alkali resistance.
[0037] The raw materials of the island-in-the-sea yarns comprise, by parts by weight, the following components: 65-70 parts low-viscosity PET, 35-40 parts PBT / IPA copolymer, 30-35 parts modified PET, and 0.6-0.8 parts network oiling agent. The network oiling agent is a polyether-based network agent with a molecular weight of 5,000 and a friction coefficient ≤0.25, which enhances the cohesion between the island-in-the-sea fibers and the high-shrinkage fibers, prevents fiber slippage during sueding, and provides antistatic properties.
[0038] The slurry compositions of the cowhide fiber surface layer 10 and the cowhide fiber bottom layer 30 comprise, in parts by weight, the following components: 90-100 parts recycled cowhide fiber, 5-8 parts plant fiber, 8-10 parts thermosensitive hydrogel fiber, 3-5 parts nanocellulose whiskers, and 5-8 parts waterborne polyurethane. Among these components, cowhide waste is subjected to buffing and fiber separation to obtain recycled cowhide fibers. The recycled cowhide fiber serves as the principal component of both the surface layer 10 and the bottom layer 30, enabling the produced eco-friendly leather to possess a hand feel similar to genuine leather, along with excellent tear strength and tensile performance. This addresses the low utilization rate of natural leather caused by irregularity, limited sheet size, and surface defects. The recycled leather can be produced in customizable lengths and colors and can be patterned according to client requirements, overcoming the limitations of genuine leather in terms of color and texture. The plant fiber used is bamboo pulp fiber, which enhances flexibility and breathability. The nanocellulose whiskers improve crosslinking density and tear resistance. The waterborne polyurethane enhances interlayer adhesion. The thermosensitive hydrogel fiber comprises, by parts by weight, the following raw materials: 80-90 parts N-isopropylacrylamide (NIPAM), 1-3 parts crosslinking agent, 5-10 parts hydrophilic modifying monomer, and 0.5-2 parts dispersant. NIPAM contains both hydrophobic (isopropyl) and hydrophilic (amide) groups, allowing it to swell or contract in response to changes in ambient humidity, thereby adjusting the porosity of the fiber layer. The crosslinking agent is N,N′-methylenebisacrylamide (MBA), which forms a three-dimensional network structure to enhance mechanical strength and shape stability. The hydrophilic modifying monomer is acrylamide (AM) or 2-hydroxyethyl methacrylate (HEMA), which adjusts moisture absorption and improves hydrophilicity and swelling capacity. The dispersant is polyvinyl alcohol (PVA). The thermosensitive hydrogel fiber is produced by polymerizing the above raw materials to form a PNIPAM prepolymer, wherein poly(N-isopropylacrylamide) (PNIPAM) constitutes the main polymer chain. The prepolymer is then processed by wet spinning or electrospinning, coagulated in a bath such as an ethanol-water solution, and subsequently stretched and dried to form the thermosensitive hydrogel fiber. The addition of thermosensitive hydrogel fibers enables automatic adjustment of the fiber-layer spacing in response to environmental humidity, imparting self-regulating breathability and dynamic responsiveness to the composite layer. Owing to their swelling-contraction properties, the fibers can achieve a 200% range of air permeability regulation. At low humidity (<40% RH), the hydrophobic groups of the PNIPAM molecular chain dominate, causing fiber contraction with a volume reduction of 25-30%, reducing the fiber-layer porosity from 60% to 30% and increasing air resistance. At high humidity (>60% RH), water molecules form hydrogen bonds with the hydrophilic groups (—CONH—) of PNIPAM, causing swelling with a volume increase of 40-50%, raising porosity to 70-80%, and significantly improving air permeability. Furthermore, the fleece clusters formed on the surface of the double-suede base fabric create three-dimensional air-guiding channels, which amplify the spacing variation effect of the thermosensitive fibers, thereby enhancing the overall air permeability adjustment performance.
[0039] As shown in FIG. 4, the production line of the recycled cowhide fiber eco-friendly leather comprises an inclined wire paper-making machine 1, a base fabric unwinding machine 2, a base fabric conveyor 3, a composite conveyor 4, a hydroentanglement device, and a drying device. Two inclined wire paper-making machines 1 are provided. The base fabric unwinding machine 2 is located at the front end of the base fabric conveyor 3, while the hydroentanglement and drying devices are sequentially arranged at the rear end of the composite conveyor 4. A carding machine 5 is installed at the terminal end of the base fabric conveyor 3. The base fabric, after being processed by the carding machine 5, merges with the cowhide fiber slurry produced by the two inclined wire paper-making machines 1 and then enters the composite conveyor 4. The carding machine 5 is equipped with oppositely arranged upper carding roller 51 and lower carding roller 52, followed by oppositely arranged upper air knife 53 and lower suction roller 54, and finally oppositely arranged upper ionizing air bar 55 and lower ionizing air bar 56. During operation, the base fabric sequentially passes through the gaps between the upper and lower carding rollers 51, 52, the upper air knife and lower suction roller 53, 54, and the upper and lower ionizing air bars 55, 56. The upper and lower carding rollers 51, 52 comb the fleece, dispersing clustered fibers into individual filaments; the upper air knife 53 blows the surface fleece open, while the lower suction roller 54 straightens and aligns the lower fleece. This process forms a symmetrical three-dimensional fleece structure on both sides of the fabric. The upper and lower ionizing air bars 55, 56 eliminate static electricity from the fleece, preventing fiber agglomeration caused by static charges. By incorporating a three-stage treatment system-consisting of dual-sided carding rollers, dual airflow dispersion, and electrostatic activation-at the rear end of the base fabric conveyor 3, the system achieves high-efficiency dispersion and orientation of fleece fibers on both surfaces of the double-suede base fabric. This effectively resolves issues of fleece clustering and low penetration, while significantly enhancing the density of hydroentanglement crosslinking.
[0040] The production process of the recycled cowhide fiber eco-friendly leather comprises the following steps:
[0041] Step a: Preparing the double-suede base fabric.
[0042] Step b: Forming a cowhide fiber slurry sheet using the inclined wire paper-making machine 1.
[0043] Step c: Unwinding the pre-fabricated double-suede base fabric by means of the base fabric unwinding machine 2.
[0044] Step d: Conveying the double-suede base fabric through the base fabric conveyor 3, wherein the base fabric is sandwiched between cowhide fiber slurry sheets generated by the two inclined wire paper-making machines 1, and the layers are superimposed on the composite conveyor 4 to form a sandwich-structured fabric.
[0045] Step e: Feeding the fabric into the hydroentanglement device, where the cowhide fiber surface layer 10, double-suede base fabric layer 20, and cowhide fiber bottom layer 30 are subjected to hydroentanglement bonding to form an integrated composite.
[0046] Step f: Sequentially passing the hydroentangled composite substrate through dewatering, cylindrical drying, harmful substance removal, and mesh-cylinder drying processes, followed by final winding into rolls.
[0047] The preparation process of the double-suede base fabric comprises the following steps:
[0048] Step a: Preparation of island-in-the-sea yarns.
[0049] Step b: Weaving of a base fabric with a double-layer structural weave.
[0050] Step c: Alkali treatment: Treating the woven fabric in a 10% NaOH solution at 90 °C for 30 minutes.
[0051] Step d: Double-sided sueding: Using ceramic abrasive disks for double-sided sueding at a rotation speed of 1500 rpm and pressure of 0.15 MPa.
[0052] The preparation process of the island-in-the-sea yarn is as follows: after melting the sea-component and island-component chips, the melt is extruded through an island-in-the-sea spinneret to form island-in-the-sea fibers with a 16-island structure. The island-in-the-sea fibers are then networked and combined with high-shrinkage fibers in a predetermined ratio to form the island-in-the-sea yarns, followed by treatment with a polyether-type network oiling agent. The nozzle pressure during network processing is 0.6 MPa, the polyether oiling agent concentration is 0.8%, and the dipping speed is 20 m / min, ensuring that the fiber surface friction coefficient is ≤0.25.
[0053] The foregoing embodiments are merely illustrative of specific implementations of the present invention, and are not intended to limit its scope. Any non-substantial modifications or variations made based on the design concept of this invention shall fall within the scope of protection of the present invention.
Claims
1. A recycled cowhide fiber eco-friendly leather, characterized in that it comprises, from top to bottom, a cowhide fiber surface layer, a double-suede base fabric layer, and a cowhide fiber bottom layer; wherein both the upper and lower surfaces of the double-suede base fabric layer are provided with fleece; the cowhide fibers of the surface layer and the bottom layer are crosslinked with the yarn fibers and fleece fibers of the double-suede base fabric layer;the fabric structure of the double-suede base fabric layer is a binding warp double-layer structure, wherein the surface fabric layer is formed by interweaving surface warps and surface wefts, the inner fabric layer is formed by interweaving inner warps and inner wefts, and the binding warps are interwoven with both the surface and inner wefts to connect the surface and inner layers of the base fabric;the surface warps and inner warps are island-in-the-sea yarns formed by network processing and compounding of island-in-the-sea fibers and high-shrinkage fibers, wherein the island-in-the-sea fibers are composite-spun fibers comprising a sea component encapsulating an island component; the sea component is low-viscosity PET, the island component is a PBT / IPA copolymer, and the high-shrinkage fiber is modified PET;the binding warp is a high-strength PA66 filament, and the surface and inner wefts are modified PA6 staple fiber yarns;the raw materials of the island-in-the-sea yarns comprise, by parts by weight: 65-70 parts low-viscosity PET, 35-40 parts PBT / IPA copolymer, 30-35 parts modified PET, and 0.6-0.8 parts network oiling agent;the slurry compositions of the cowhide fiber surface layer and cowhide fiber bottom layer comprise, by parts by weight: 90-100 parts recycled cowhide fiber, 5-8 parts plant fiber, 8-10 parts thermosensitive hydrogel fiber, 3-5 parts nanocellulose whiskers, and 5-8 parts waterborne polyurethane.
2. The recycled cowhide fiber eco-friendly leather according to claim 1, wherein, in the binding warp double-layer structure, the surface fabric adopts a 2-over-2-under right-hand twill weave, the inner fabric adopts a 1-over-3-under right-hand twill weave, the warp yarns are arranged in the order of one surface warp, one inner warp, and one binding warp, and the weft yarns are arranged in the order of one surface weft and one inner weft.
3. The recycled cowhide fiber eco-friendly leather according to claim 1, wherein the production line of the recycled cowhide fiber eco-friendly leather comprises an inclined wire paper-making machine, a base fabric unwinding machine, a base fabric conveyor, a composite conveyor, a hydroentanglement device, and a drying device;two inclined wire paper-making machines are provided; the base fabric unwinding machine is located at the front end of the base fabric conveyor; the hydroentanglement device and drying device are sequentially arranged at the rear end of the composite conveyor;a carding machine is provided at the end of the base fabric conveyor, and the carding machine is equipped with oppositely arranged upper and lower carding rollers, followed by oppositely arranged upper air knife and lower suction roller, and finally oppositely arranged upper and lower ionizing air bars.
4. A production process for the recycled cowhide fiber eco-friendly leather according to claim 1, comprising the following steps:Step a: preparing the double-suede base fabric;Step b: forming cowhide fiber slurry sheets using the inclined wire paper-making machine;Step c: unwinding the pre-fabricated double-suede base fabric using the base fabric unwinding machine;Step d: conveying the double-suede base fabric through the base fabric conveyor, sandwiching it between the cowhide fiber slurry sheets produced by the two inclined wire paper-making machines, and superimposing the layers on the composite conveyor to form a sandwich-structured fabric;Step e: feeding the fabric into the hydroentanglement device, where the cowhide fiber surface layer, double-suede base fabric layer, and cowhide fiber bottom layer undergo hydroentanglement bonding;Step f: sequentially subjecting the hydroentangled composite substrate to dewatering, cylindrical drying, harmful substance removal, and mesh-cylinder drying, followed by final winding.
5. The production process according to claim 4, wherein the preparation process of the double-suede base fabric comprises the following steps:Step a: preparing island-in-the-sea yarns;Step b: weaving a base fabric having a double-layer structural weave;Step c: performing alkali treatment with a 10% NaOH solution at 90 °C for 30 minutes;Step d: conducting double-sided sueding using ceramic abrasive disks at a rotation speed of 1500 rpm and pressure of 0.15 MPa.
6. The production process according to claim 4, wherein the preparation process of the island-in-the-sea yarns comprises the following steps: melting sea-component and island-component chips, extruding the melt through an island-in-the-sea spinneret to form island-in-the-sea fibers having a 16-island structure; networking and combining the island-in-the-sea fibers with high-shrinkage fibers in a predetermined ratio to form island-in-the-sea yarns, and treating them with a polyether-type network oiling agent.