Radome and preparation method therefor
By using a sandwich structure and hollow design of low dielectric constant materials in the radome, combined with hot pressing molding technology, the problem of high dielectric constant of traditional radomes is solved, the electromagnetic performance is improved and the cost and size are reduced.
Patent Information
- Application Number
- PCT/CN2024/081503
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-31
- Filing Date
- 2024-03-13
- Publication Date
- 2024-10-03
AI Technical Summary
Traditional radomes use high dielectric constant materials, resulting in large electromagnetic wave obstruction and low transmittance, which affects antenna performance, and the edge sealing configuration increases cost and size.
A sandwich structure of low dielectric constant material is used. The core layer is protected by the hollow area and the skin layer to avoid edge sealing. The entire radome is used as a radiation area and the dielectric constant is reduced by hot press molding.
The electromagnetic wave penetration characteristics and mechanical properties of the antenna are improved, the dielectric constant of the radome is reduced, the size and cost are reduced, and the process is simplified.
Smart Images

Figure CN2024081503_03102024_PF_FP_ABST
Abstract
Description
Radome and preparation method thereof
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] The present disclosure is based on Chinese patent application No. 2023103793926 filed on March 31, 2023, entitled “Radome and Method for Preparing the Same”, and claims the priority of the patent application, and all the contents disclosed therein are incorporated into the present disclosure by reference. Technical Field
[0003] The present disclosure relates to the field of communication technology, and in particular to a radome and a preparation method thereof. Background Art
[0004] The radome is a structure that protects the antenna system from external environmental influences. It is required to have good electromagnetic wave penetration characteristics in terms of electrical performance and mechanical properties that can withstand the effects of harsh external environments.
[0005] Traditional communication equipment antenna covers are made of thermoplastic plastics such as PC by injection molding. The properties of this type of material determine that its dielectric constant is relatively large. The high dielectric constant leads to large obstruction to the electromagnetic waves emitted by the antenna and low transmittance, affecting the antenna performance.
[0006] Summary of the Invention
[0007] The main purpose of the present disclosure is to provide a radome and a preparation method thereof, which can effectively reduce the dielectric constant of the radome, utilize the radome body, the first skin layer and the second skin layer to protect the core layer, and there is no need to set edge sealing. The entire radome can be used as a radiation area. Not only does the antenna performance have good, but the setting cost is lower without the need for edge sealing, and the size of the radome is reduced.
[0008] According to a first aspect of the present disclosure, a radome is provided, comprising a radome and a composite panel, wherein the radome is provided with a hollow region, the hollow region having a first opening and a second opening in a first direction, the first direction being a thickness direction of the radome;
[0009] The composite panel comprises:
[0010] a core layer embedded in the hollow area, the core layer having a first side and a second side opposite to each other in the first direction;
[0011] a first skin layer, sealingly attached to a first side of the core layer and covering the first opening;
[0012] a second skin layer, sealingly attached to the second side of the core layer and covering the second opening;
[0013] The core layer is made of a low dielectric constant material, and the periphery of the core layer extends to abut against the inner wall of the hollow area.
[0014] A second aspect of the present disclosure provides a method for preparing a radome, comprising:
[0015] A hollow area is provided on the cover body;
[0016] Cutting the prepreg and the lightweight low dielectric composite material into a preset shape, wherein the prepreg is used to form a first skin layer and a second skin layer, and the lightweight low dielectric composite material is used to form a core layer;
[0017] Laying the first skin layer, the cover body, the core layer, and the second skin layer in sequence in a mold, with the core layer embedded in the hollow area of the cover body, and the first skin layer and the second skin layer respectively attached to opposite sides of the core layer in the thickness direction, with the first skin layer and the second skin layer tightly attached to the mold;
[0018] placing the mold in a molding machine for hot pressing to form the first skin layer, the cover body, the core layer and the second skin layer by hot pressing;
[0019] After the hot pressing is completed, the mold is cooled, opened, and the prepared antenna cover is taken out. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the technical solutions of the embodiments disclosed in the present disclosure, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are some embodiments disclosed in the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.
[0021] FIG1 is a schematic structural diagram of a radome from a first perspective according to an embodiment of the present disclosure;
[0022] FIG2 is a schematic structural diagram of the radome according to an embodiment of the present disclosure from a second perspective;
[0023] FIG3 is an exploded schematic diagram of a radome according to an embodiment of the present disclosure;
[0024] FIG4 is a schematic cross-sectional view of the cover in the width direction according to an embodiment of the present disclosure;
[0025] FIG5 is a flowchart of a method for preparing a radome according to an embodiment of the present disclosure;
[0026] FIG6 is the antenna radiation diagram of Example 1, Comparative Example 1 and Comparative Example 2.
[0027] The figures are marked as follows: 100, antenna cover; 10, cover body; 10a, plate body; 10b, edge; 11, hollow area; 12, first surface; 121, first limiting groove; 13, second surface; 131, second limiting groove; 20, composite panel; 21, core layer; 211, first side; 212, second side; 22, first skin layer; 23, second skin layer. DETAILED DESCRIPTION
[0028] The following will clearly and completely describe the technical solutions in the embodiments of the present disclosure in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present disclosure, not all of them. All other embodiments obtained by ordinary technicians in this field based on the embodiments of the present disclosure without making any creative efforts shall fall within the scope of protection of the present disclosure.
[0029] It should be understood that the terms used in this disclosure are only for the purpose of describing particular embodiments and are not intended to limit the disclosure. As used in this disclosure and the appended claims, the singular forms "a," "an," and "the" are intended to include the plural forms unless the context clearly indicates otherwise.
[0030] It will also be understood that the term "and / or" as used in this disclosure and the appended claims refers to and includes any and all possible combinations of one or more of the associated listed items.
[0031] It should be understood that the specific embodiments described herein are only used to illustrate the present disclosure and are not intended to limit the present disclosure.
[0032] The radome is a structure that protects the antenna system from external environmental influences. It is required to have good electromagnetic wave penetration characteristics in terms of electrical performance and mechanical properties that can withstand the effects of harsh external environments.
[0033] Traditional communication equipment antenna covers are injection-molded using thermoplastics such as PC (polycarbonate). The properties of these materials determine that their dielectric constants are relatively large. The high dielectric constant results in significant obstruction to electromagnetic waves emitted by the antenna and low transmittance, affecting antenna performance.
[0034] Therefore, it is necessary to select low-dielectric constant materials to reduce the dielectric constant of the radome. Among them, the sandwich structure can be applied to the radome because its lightweight, low-dielectric constant core layer can effectively reduce the dielectric constant of the radome. The sandwich structure generally consists of an upper skin, a lower skin, a core layer sandwiched between the upper and lower skins, and edge sealing. If conventional methods are used, such as gluing or screwing with matching sealing strips, to assemble the complete sandwich structure to a traditional radome, the transition area and edge sealing position will occupy the radome space, which not only affects the antenna performance but also increases the size of the radome.
[0035] Therefore, the embodiment of the present disclosure provides a radome and a preparation method thereof, which utilizes a radome body, a first skin layer, and a second skin layer to protect the core layer. There is no need to set edge sealing, and the entire radome can be used as a radiation area. Not only does the antenna performance have good, but the setting cost is lower without the need for edge sealing, and the size of the radome is reduced.
[0036] The following embodiments of the present disclosure are described in detail with reference to the accompanying drawings. In the absence of conflict, the following embodiments and features therein may be combined with each other.
[0037] 1-3 , an embodiment of the present disclosure provides a radome 100, comprising a cover body 10 and a composite panel 20. The cover body 10 is provided with a hollow region 11. The hollow region 11 has a first opening and a second opening in a first direction, where the first direction is the thickness direction of the cover body 10. The composite panel 20 comprises a core layer 21, a first skin layer 22, and a second skin layer 23. The core layer 21 is embedded in the hollow region 11. The core layer 21 has a first side 211 and a second side 212 opposite to each other in the first direction. The first skin layer 22 is sealed against the first side 211 of the core layer 21 and covers the first opening of the hollow region 11. The second skin layer 23 is sealed against the second side 212 of the core layer 21 and covers the second opening of the hollow region 11. The core layer 21 is made of a low dielectric constant material, and the periphery of the core layer 21 extends to abut against the inner wall of the hollow region 11.
[0038] The antenna cover 100 proposed in the embodiment of the present disclosure adopts a low dielectric constant material as the core layer 21, which can effectively reduce the dielectric constant of the antenna cover 100. The core layer 21 does not need to be provided with edge sealing, but is directly connected to the cover body 10. The core layer 21 is protected by the cover body 10, the first skin layer 22 and the second skin layer 23. Without edge sealing, the entire antenna cover 100 can be used as a radiation area. Not only does the antenna performance have good, but the setting cost is lower without the need for edge sealing, and the size of the antenna cover 100 is reduced.
[0039] In some embodiments, since the antenna cover needs to be made to adapt to the shape of the antenna, the structure is relatively complex. If the entire antenna cover adopts a sandwich structure, the molding process is complicated and the cost is high. Therefore, the cover body 10 adopts traditional PC and other thermoplastic plastic injection molding, which has a simple process and low cost. A hollow area 11 is set on the plane part of the cover body 10 to fix the composite panel 20, which can not only effectively reduce the dielectric constant of the antenna cover 100, but also facilitate processing and reduce costs.
[0040] In some embodiments, the thickness of the core layer 21 in the first direction is less than or equal to the thickness of the inner wall of the hollow region 11. For example, the thickness of the core layer 21 can be consistent with the thickness of the inner wall of the hollow region 11, so that the first side 211 and second side 212 surfaces of the core layer 21 are flush with the openings on both sides of the hollow region 11, facilitating close contact between the first skin layer 22 and the second skin layer 23 and the core layer 21, thereby providing better protection. Of course, in other embodiments, the thickness of the core layer 21 can also be less than the thickness of the inner wall of the hollow region 11.
[0041] In some embodiments, as shown in Figures 2 and 3, the cover body 10 has a first surface 12 and a second surface 13 that are opposite to each other in a first direction. The surface of the first skin layer 22 is flush with the first surface 12, and the surface of the second skin layer 23 is flush with the second surface 13. In this embodiment, this arrangement allows the surface of the radome 100 to be smooth, making the overall structure more harmonious and aesthetically pleasing.
[0042] Of course, the first skin layer 22 and the second skin layer 23 are not limited to the above configuration. For example, in other embodiments, the cover body 10 has a first surface 12 and a second surface 13 that are opposite in the first direction, the first skin layer 22 protrudes from the first surface 12 or is embedded in the first surface 12, and the second skin layer 23 protrudes from the second surface 13 or is embedded in the second surface 13. In this embodiment, the first skin layer 22 and the second skin layer 23 can also be configured to be protruding or recessed relative to the surface of the cover body 10, as long as they can protect the core layer 21.
[0043] In some embodiments, as shown in Figures 3 and 4, the first surface 12 is provided with a first limiting groove 121 that is adapted to the first skin layer 22 at the edge of the hollow region 11, and the first skin layer 22 is embedded in the first limiting groove 121. In this embodiment, when the thickness of the core layer 21 is consistent with that of the hollow region 11 of the cover body 10, the first limiting groove 121 can be used to position the first skin layer 22, which is beneficial for the first skin layer 22 to be attached to the first side 211 of the core layer 21. At the same time, it can also facilitate the first skin layer 22 to be flush with the surface of the cover body 10 without protruding outward, making the overall structure more coordinated and beautiful.
[0044] In some embodiments, as shown in FIG5 , the second surface 13 is provided with a second retaining groove 131 at the edge of the hollow region 11, which is adapted to the second skin layer 23. The second skin layer 23 is embedded in the second retaining groove 131. In this embodiment, when the thickness of the core layer 21 is consistent with that of the hollow region 11 of the cover body 10, the provision of the second retaining groove 131 can position the second skin layer 23, facilitating the second skin layer 23 to adhere to the second side 212 of the core layer 21. It also facilitates the second skin layer 23 to be flush with the surface of the cover body 10, preventing it from protruding outward, and providing a more harmonious and aesthetically pleasing overall structure.
[0045] Of course, the antenna cover 100 disclosed in the present invention may also not be provided with the first limiting groove 121 and the second limiting groove 131, so that the first skin layer 22 and the second skin layer 23 can be provided to convex outward, or the cross-sectional dimensions of the first skin layer 22 and the second skin layer 23 can be made consistent with the core layer 21. At this time, the edges of the first skin layer 22 and the second skin layer 23 abut against the inner wall of the hollow area 11, and the sum of the thicknesses of the first skin layer 22, the second skin layer 23 and the core layer 21 is equal to the thickness of the hollow area 11. In this way, the first skin layer 22 and the second skin layer 23 can also be flush with the surface of the cover body 10, and at the same time can protect the core layer 21.
[0046] In some embodiments, to adapt to the usage scenario, the hollow structure can be provided on one side of the cover body 10 in the extension direction, that is, on the left side in the usage state as shown in FIG3 . Of course, in other embodiments, the hollow structure can also be provided on any position of the cover body 10, such as the right side, upper side, lower side, or middle position.
[0047] In some embodiments, as shown in Figures 1-3 , to adapt to the usage scenario, the cover body 10 can be extended along a second direction, and the composite panel 20 can be extended along a third direction, with the second and third directions being located on the same horizontal plane and perpendicular to each other, and both being perpendicular to the first direction. In this embodiment, this arrangement allows the composite panel 20 to be positioned close to the edge of the cover body 10. Of course, in other embodiments, the composite panel 20 can also be arranged in a non-perpendicular direction, such as aligning with the direction of extension of the cover body 10.
[0048] In some embodiments, the first skin layer, the second skin layer, the core layer, and the cover are integrally formed so that the first skin layer, the second skin layer, and the cover are integrally formed and cover the outer surface of the core layer. In this embodiment, this arrangement eliminates the need for additional edge sealing for the radome of the present disclosure, and the cover, the first skin layer, and the second skin layer of the radome are integrally formed to protect the core layer.
[0049] For example, the composite panel 20 and the cover body 10 can be fixed by bonding or heat pressing. In this embodiment, the composite panel 20 and the cover body 10 are fixed and formed by heat pressing, which can ensure the density between the first skin layer 22, the second skin layer 23, the core layer 21 and the cover body 10, improve the connection stability, and reduce the porosity.
[0050] In some embodiments, the cross-sectional dimensions of the hollow area 11 in the horizontal direction are consistent with those of the core layer 21. In this embodiment, the above arrangement facilitates the cover body 10 to provide a protective effect on the core layer 21 while improving the connection stability.
[0051] In some embodiments, the horizontal cross-sectional dimensions of the first skin layer 22 and the second skin layer 23 are consistent. In this embodiment, this arrangement not only balances the opposing sides of the core layer 21, providing consistent protection, but also eliminates the need to distinguish between the first skin layer 22 and the second skin layer 23 during processing, facilitating the processing of the first skin layer 22 and the second skin layer 23.
[0052] In some embodiments, as shown in Figures 1-3, the cover body 10 includes a plate body 10a and a peripheral edge 10b disposed around the periphery of the plate body 10a, with a hollow structure disposed within the plate body 10a. In this embodiment, the plate body 10a has two opposing planar surfaces, and the peripheral edge 10b can extend perpendicularly to the plate body 10a. A hollow region 11 is provided within the flat plate body 10a to facilitate attachment to the composite panel 20.
[0053] In some embodiments, the core layer 21 is composed of aramid honeycombs and micro-foam plastic. In this embodiment, the aramid honeycomb can, on the one hand, limit the flow of the micro-foam plastic during the molding process, preventing the micro-foam plastic from flowing everywhere and causing structural unevenness and uneven height. On the other hand, after molding, the unique honeycomb connection structure of the aramid honeycomb can ensure the tensile and impact resistance of the finished product. Moreover, during the molding process, the aramid honeycomb increases in volume, which can effectively fill the gaps between the parts, making the connection between the parts tighter. At the same time, the enlarged volume of the aramid honeycomb can effectively reduce the mass per unit volume, thereby reducing the weight of the finished product.
[0054] Exemplarily, the aramid honeycomb can be selected to have a structure of at least two layers, and the gaps between the two layers of aramid honeycombs are staggered, so that the staggered gaps further restrict the flow of the micro-foamed plastic. At the same time, the staggered gaps make the honeycomb structure in the finished product appear to have a staggered structure, and the micro-foamed plastic fixed in the honeycomb structure can be interlaced up and down like a textile rope, which is conducive to further improving the tensile strength and impact resistance of the core layer, thereby improving the performance of the antenna cover 100.
[0055] In some embodiments, the micro-foam plastic includes at least one of polymethacrylimide foam and polypropylene foam. In this embodiment, polymethacrylimide foam and polypropylene foam have relatively low dielectric constants and dielectric losses, so that the formed core layer has high transmittance, thereby improving the performance of the radome 100.
[0056] In some embodiments, the density of the micro-foam plastic is 70 kg / m 3 -110 kg / m 3 . In this embodiment, the weight of the core layer is reduced by selecting the micro-foam plastic, thereby reducing the weight of the radome 100 .
[0057] In some embodiments, the dielectric constant of the micro-foam plastic is less than or equal to 1.2. In this embodiment, the micro-foam plastic is selected as described above to form a core layer with high transmittance, thereby improving the performance of the radome 100.
[0058] In some embodiments, the dielectric loss of the micro-cellular plastic is less than or equal to 0.001. In this embodiment, the micro-cellular plastic is selected to form a core layer with high transmittance, thereby improving the performance of the radome 100.
[0059] 4 , the present disclosure also provides a method for preparing a radome 100 , including:
[0060] S1, a hollow area 11 is formed on the cover body 10.
[0061] S2, cutting the prepreg and the lightweight low dielectric composite material into a preset shape, the prepreg is used to cut to form the first skin layer 22 and the second skin layer 23, and the lightweight low dielectric composite material is used to cut to form the core layer 21.
[0062] S3, lay the first skin layer 22, the cover body 10, the core layer 21 and the second skin layer 23 in the mold in sequence, and embed the core layer 21 in the hollow area 11 of the cover body 10, and the first skin layer 22 and the second skin layer 23 are respectively attached to the opposite sides of the core layer 21 in the thickness direction, and the first skin layer 22 and the second skin layer 23 are tightly fitted to the mold.
[0063] S4, placing the mold into a molding machine for hot pressing, so as to hot press the first skin layer 22, the cover body 10, the core layer 21 and the second skin layer 23 into shape.
[0064] S5, after the hot pressing is completed, the mold is cooled, the mold is opened, and the manufactured antenna cover 100 is taken out.
[0065] The preparation method of the antenna cover 100 provided in the embodiment of the present disclosure adopts a lightweight low-dielectric composite material to form the core layer 21, which can effectively reduce the dielectric constant of the antenna cover 100. The protective core layer 21 is formed by hot pressing the cover body 10 of the antenna cover 100 and the first skin layer 22 and the second skin layer 23. There is no need to additionally prepare the edge-sealed protective core layer 21. The entire antenna cover 100 can be used as a radiation area. Not only does it have good antenna performance, but it also has a simple process, low cost, and reduces the size of the antenna cover 100.
[0066] For example, in step S3, the mold surface can be cleaned first. The mold surface can be cleaned by wiping it with a detergent, then drying it and cooling it to room temperature. This process can be repeated several times to ensure that the mold surface is clean and free of oil, droplet agglomeration, and dust.
[0067] Exemplarily, the mold includes an upper mold and a lower mold. The first skin layer 22, the cover body 10, the core layer 21 and the second skin layer 23 are laid in the lower mold in sequence. After laying, the upper mold is covered and the mold is placed in a molding machine. After preheating to the activation temperature of the resin, the pressure is increased, the temperature is increased at the same time, and the heat and pressure are maintained for a period of time.
[0068] For example, the increased pressure may be between 1.5 MPa and 10 MPa, and the heat preservation and pressure holding time may be no less than 0.5 hours.
[0069] For example, after hot pressing is completed, the mold is cooled to the mold opening temperature, and the cooling rate may be 5° C. / min-20° C. / min.
[0070] For example, in step S4, after the upper template is covered, the mold is vibrated while being heated and pressurized to make the material filling in the mold more uniform, thereby reducing the differences in the finished product at different positions. Before covering the upper template, prepreg can also be added to the mold, and the flow of the prepreg can be used to make the surface of the first skin layer 22 smoother. Vibrating the mold can further accelerate the flow of the prepreg. In the case of adding prepreg liquid, the thickness of the raw material is 75%-80% of the mold depth, and the volume of the added prepreg liquid is 1%-2% of the mold volume. The empty space is the expansion space reserved for the raw materials. In order to further ensure the flatness of the outer surface of the first skin layer 22, the mold can be turned upside down for the first 10 minutes of the heat preservation and pressure holding stage, so that the first skin layer 22 is at the bottom, and then turned upside down so that the second skin layer 23 is at the top.
[0071] For example, the composite panel 20 may be machined and / or painted, with the thickness of the paint being approximately 50 μm to 100 μm.
[0072] In some embodiments, the prepreg is a fiber cloth impregnated with a resin system. In this embodiment, the impregnation resin system can enhance the toughness of the material.
[0073] In some embodiments, the weaving form of the fiber cloth is a plain weave. In the present embodiment, the weaving form of the fiber cloth adopts a plain weave with the maximum number of interweaving times, making the fabric strong and wear-resistant.
[0074] In some embodiments, the fiber cloth is one or a combination of glass fiber cloth, quartz fiber cloth, and aramid fiber cloth. In this embodiment, the fiber cloth can be low-dielectric glass fiber cloth, which offers excellent insulation, heat resistance, corrosion resistance, and mechanical strength. Alternatively, quartz fiber cloth can be used, which offers heat resistance, corrosion resistance, and flexibility, high strength retention at high temperatures, dimensional stability, thermal shock resistance, chemical stability, light transmittance, and electrical insulation. Alternatively, aramid fiber cloth can be used, which offers light weight and high breaking strength.
[0075] For example, the glass fiber cloth may be E glass fiber cloth, HL glass fiber cloth or D glass fiber cloth.
[0076] In some embodiments, the resin system used to impregnate the fiber cloth includes one of an epoxy resin system, a vinyl resin system, and a polyurethane resin system. In this embodiment, the epoxy resin exhibits excellent adhesion, heat resistance, chemical resistance, and superior mechanical properties. The vinyl resin blends better with the glass fiber and also exhibits excellent antistatic properties. The polyurethane resin, when heated to form a film, exhibits excellent thermal bonding properties, achieving excellent adhesion to the fiber cloth.
[0077] In some embodiments, the volume fraction of the matrix resin in the resin system used to impregnate the fiber cloth is 30%-42.5%. In this embodiment, by selecting the resin system with the above volume fraction for impregnating the fiber cloth, the formed radome 100 has better performance.
[0078] The preparation method of the antenna cover provided in the embodiment of the present disclosure adopts a lightweight low-dielectric composite material to form a core layer, which can effectively reduce the dielectric constant of the antenna cover. The protective core layer is formed by hot pressing the cover body of the antenna cover and the first skin layer and the second skin layer. There is no need to additionally prepare an edge-sealed protective core layer. The entire antenna cover can be used as a radiation area. Not only does it have good antenna performance, but it also has a simple process, low cost, and reduces the size of the antenna cover.
[0079] Example 1
[0080] An antenna having a radome proposed in an embodiment of the present disclosure is used as Example 1.
[0081] Comparative Example 1
[0082] Since the electromagnetic waves emitted by the antenna may be reflected on the surface of the antenna cover and absorbed in the dielectric layer of the antenna cover, causing power loss, the situation without an antenna cover, that is, the state with minimal interference, is the most ideal state. Therefore, an antenna without an antenna cover is used as comparative example 1.
[0083] Comparative Example 2
[0084] An antenna having an existing antenna cover (the entire antenna cover is made of PC plastic injection molding) is used as comparative example 2.
[0085] The antenna patterns of Example 1, Comparative Example 1, and Comparative Example 2 are shown in Figure 6 . The specific parameters corresponding to Figure 6 are shown in Table 1 . In Figure 6 , the horizontal axis represents angle, and the vertical axis represents antenna gain. As shown in Figure 6 and Table 1, from -90° to 90°, the beam shape of Example 1 is closer to the beam shape of Comparative Example 1 without a radome than that of Comparative Example 2. In particular, between 50° and 90°, the beam deformation of Comparative Example 2 is more severe, while the beam shape of Example 1 is closer to that of Comparative Example 1. This indicates that the radome proposed in the embodiments of the present disclosure has lower power loss when acting on the antenna, causing less interference, thereby improving antenna performance.
[0086] Table 1
[0087] The above embodiments of the present disclosure are for illustrative purposes only and do not represent the advantages or disadvantages of the embodiments. The above are only specific embodiments of the present disclosure, but the scope of protection of the present disclosure is not limited thereto. Any technician familiar with the technical field can easily think of various equivalent modifications or replacements within the technical scope disclosed in the embodiments of the present disclosure, and these modifications or replacements should be included in the scope of protection of the present disclosure. Therefore, the scope of protection of the present disclosure should be based on the scope of protection of the claims.
Claims
1. An antenna cover, comprising a cover body and a composite panel, wherein the cover body is provided with a hollow area, the hollow area has a first opening and a second opening in a first direction, and the first direction is a thickness direction of the cover body; The composite panel include: A core layer, embedded in the hollow area, the core layer having a first side and a second side opposite to each other in the first direction; A first skin layer is sealed and adhered to a first side of the core layer and covers the first opening; A second skin layer is sealed and adhered to the second side of the core layer and covers the second opening; Wherein, the core layer is made of a low dielectric constant material, and the periphery of the core layer extends to abut against the inner wall of the hollow area.
2. The radome according to claim 1, in, In the first direction, the thickness of the core layer is less than or equal to the thickness of the inner wall of the hollow area.
3. The radome according to claim 1, in, The cover body has a first surface and a second surface opposite to each other in the first direction, the surface of the first skin layer is flush with the first surface, and the surface of the second skin layer is flush with the second surface; or, The cover body has a first surface and a second surface opposite to each other in the first direction, the first skin layer protrudes from the first surface or is embedded in the first surface, and the second skin layer protrudes from the second surface or is embedded in the second surface.
4. The radome according to claim 3, in, The first surface is provided with a first limiting groove adapted to the first skin layer at the edge of the hollow area, and the first skin layer is embedded in the first limiting groove; and / or, The second surface is provided with a second limiting groove matched with the second skin layer at the edge of the hollow area, and the second skin layer is embedded in the second limiting groove.
5. The radome according to claim 1, in, The first skin layer, the second skin layer, the core layer and the cover body are integrally formed so that the first skin layer, the second skin layer and the cover body are integrally formed and covered on the outer surface of the core layer.
6. The radome according to any one of claims 1 to 5, in, The core layer is composed of aramid honeycomb and micro-foamed plastic.
7. The radome according to claim 6, in, The micro-foamed plastic comprises at least one of polymethacrylimide foam and polypropylene foam; and / or, The density of the micro-foamed plastic is 70kg / m 3 -110kg / m 3 and / or, The dielectric constant of the micro-foamed plastic is less than or equal to 1.2; and / or, The dielectric loss of the micro-foamed plastic is less than or equal to 0.
001.
8. A method for preparing a radome, include: A hollow area is provided on the cover body; Cutting the prepreg and the lightweight low dielectric composite material into a preset shape, wherein the prepreg is used to cut to form a first skin layer and a second skin layer, and the lightweight low dielectric composite material is used to cut to form a core layer; The first skin layer, the cover body, the core layer and the second skin layer are sequentially laid in a mold, and the core layer is embedded in the hollow area of the cover body, the first skin layer and the second skin layer are respectively attached to two opposite sides of the core layer in the thickness direction, and the first skin layer and the second skin layer are tightly attached to the mold; placing the mold into a molding machine for hot pressing, so as to hot-press the first skin layer, the cover body, the core layer and the second skin layer into shape; After the hot pressing is completed, the mold is cooled, the mold is opened, and the prepared antenna cover is taken out.
9. The preparation method according to claim 8, in, The prepreg is a fiber cloth impregnated with a resin system.
10. The preparation method according to claim 9, in, The weaving form of the fiber cloth is plain weave; and / or, The fiber cloth is one or a combination of glass fiber cloth, quartz fiber cloth, and aramid fiber cloth; and / or, The resin system used for impregnating the fiber cloth comprises one of an epoxy resin system, a vinyl resin system, and a polyurethane resin system; and / or, The volume fraction of the matrix resin in the resin system used for impregnating the fiber cloth is 30%-42.5%.
Citation Information
Patent Citations
Preparation method of high-frequency wave-transparent sandwich structure composite material 5G antenna housing
CN108274879A
Lightweight low-dielectric composite material, 5G millimeter wave antenna housing adopting same and preparation method of antenna housing
CN113823909A
Composite board, antenna housing and manufacturing method of antenna housing
CN114536902A
Hybrid core sandwich radome
US6107976A
Meta-material, de-icing device, and aircraft
WO2021022883A1