Laser peening method and laser peening device

The introduction of an expansion jig in laser peening methods allows for stable laminar water film formation over the processing area, addressing uneven processing issues and enhancing design flexibility and treatment consistency on small workpieces.

WO2024202285A1PCT designated stage expired Publication Date: 2024-10-03HAMAMATSU PHOTONICS KK
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/044522
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-28
Filing Date
2023-12-12
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Conventional laser peening methods face challenges in stabilizing the water film formation near the edges of small workpieces, leading to uneven processing due to disturbances in the water film, restricting the design flexibility of the processing area.

Method used

The use of an expansion jig to create an expanded surface outside the workpiece, allowing for the formation of a stable laminar water film over the processing area, which prevents disturbances and enables uniform processing even on small workpieces or across the entire surface.

Benefits of technology

This approach enhances the degree of freedom in designing the processing area, stabilizes the plasma confinement effect, and prevents uneven processing by ensuring a uniform laminar water film, thus improving the peening effect and surface treatment consistency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023044522_03102024_PF_FP_ABST
    Figure JP2023044522_03102024_PF_FP_ABST
Patent Text Reader

Abstract

This laser peening method comprises: an arrangement step for arranging an expansion jig 12 with respect to a workpiece W and forming an expansion surface 15 outside a surface Wa of the workpiece W by the expansion jig 12 in a front view of a processing region K; a formation step for forming a water film P by a laminar flow created by discharge water Pw toward a target position M1 so as to stride at least a portion of the extension surface 15 and an irradiation position M2 of a laser beam L; and a processing step for irradiating the processing region K with the laser beam L through the water film P by scanning over the irradiation position M2 of the laser beam L and the target position M1 of the discharge water Pw on the surface Wa of the workpiece W.
Need to check novelty before this filing date? Find Prior Art

Description

Laser peening method and laser peening device

[0001] The present disclosure relates to a laser peening method and a laser peening apparatus.

[0002] One known technique for processing material surfaces is laser peening, which involves irradiating a workpiece in contact with an interference layer such as water with high-peak pulsed laser light and using shock waves generated by the pressure of plasma generated in the interference layer to create a peening effect (e.g., applying compressive stress) from the surface of the workpiece to a specified depth.

[0003] A conventional technique related to laser peening is described in, for example, Non-Patent Document 1. In this conventional method, a workpiece to be processed is supported by a support substrate, which is further held by a three-axis robot arm. A sacrificial layer made of metal tape or the like is provided on the surface of the workpiece to prevent laser damage to the surface. A nozzle that ejects water is installed near the workpiece. When a laser beam is irradiated toward the workpiece, a water film is formed on the surface of the workpiece by a laminar flow of water ejected from the nozzle.

[0004] J. Kaufman et al., “The effect of laser shock peening with and without protective coating on intergranular corrosion of sensitized AA5083”, Corrosion Science 194 (2022) 109925

[0005] In conventional laser peening techniques such as those described above, when the discharged water hits the workpiece surface near the edge, the water film formed by the discharged water is prone to disturbance, making it difficult to stably form a laminar water film. If a stable laminar water film is not formed at the laser beam irradiation position, the plasma confinement effect of the water film is weakened, potentially resulting in uneven processing. For example, when the workpiece is small in size or when the processing area is near the edge of the workpiece surface, there is insufficient space on the workpiece surface, forcing the target position of the discharged water to be set near the edge of the workpiece surface, potentially resulting in the above-mentioned uneven processing problem. Attempts to avoid such problems may result in limitations on the design of the processing area on the workpiece surface.

[0006] The present disclosure has been made to solve the above-mentioned problems, and aims to provide a laser peening method and a laser peening device that can increase the design freedom of the processing area on the surface of a workpiece.

[0007] A laser peening method according to one aspect of the present disclosure is a laser peening method for peening a processing area set on the surface of a workpiece by irradiating it with laser light, and includes an arrangement step of placing an expansion jig on the workpiece and forming an expanded surface by the expansion jig in an area outside the surface of the workpiece when viewed from the front of the processing area; a formation step of forming a water film by laminar flow using water ejected toward a target position so as to span the irradiation position of the laser light and at least a portion of the expanded surface; and a processing step of irradiating the processing area with laser light through the water film.

[0008] In this laser peening method, an expansion jig is placed on the workpiece, forming an expanded surface by the expansion jig in an area outside the workpiece surface. By forming such an expanded surface, when a laser beam is irradiated onto the processing area through a water film, a laminar water film can be formed across the laser beam irradiation position and at least a portion of the expanded surface. This makes it possible to prevent disturbance of the water film, for example, near the edge of the workpiece surface, even when the workpiece is small in size or the entire workpiece is the processing area. Therefore, this laser peening method can solve the problem of processing unevenness due to the position of the processing area and increase the degree of freedom in designing the processing area on the workpiece surface.

[0009] In the positioning process, the expansion jig may form an expansion surface above the surface of the workpiece when viewed from the front of the machining area. In this case, the target position of the discharged water can be set above the surface of the workpiece, and a water film can be stably formed by laminar flow on the upper edge of the surface of the workpiece. Therefore, it is possible to position the machining area near the upper edge of the surface of the workpiece.

[0010] In the positioning process, the expansion jig may be used to form an expanded surface that surrounds the surface of the workpiece when viewed from the front of the machining area. In this case, the target position of the discharged water can be set around the periphery of the workpiece surface, and a stable laminar water film can be formed around the entire periphery of the workpiece surface. Therefore, it is possible to position the machining area around the entire edge of the workpiece surface.

[0011] In the positioning step, the expansion jig may be positioned relative to the workpiece so that the surface of the workpiece and the expanded surface by the expansion jig are flush with each other. In this case, there is no step between the surface of the workpiece and the expanded surface by the expansion jig, so that a water film can be formed with a more uniform laminar flow in the processing area.

[0012] In the placement process, the expansion jig may be placed in close contact with the workpiece, so that the surface of the workpiece and the expanded surface by the expansion jig are in close contact with each other. In this case, the gap between the surface of the workpiece and the expanded surface by the expansion jig is reduced, so that a water film can be formed in the processing area with a more uniform laminar flow.

[0013] In the placement process, an expansion jig having an expansion surface with an arithmetic mean roughness Ra of 20 μm or less may be used. By reducing the roughness of the expansion surface, it is possible to prevent the discharged water flowing over the expansion surface from becoming turbulent, and to form a water film with a more uniform laminar flow in the processing area.

[0014] In the placement process, a holding jig may be placed to hold the back surface of the workpiece and the back surface of the expansion jig. In this case, the expansion jig can be easily placed on the workpiece. Furthermore, by holding the back surface of the workpiece with the holding jig, deformation of the workpiece during processing can be suppressed. Therefore, the peening effect in the processing area can be improved.

[0015] In the machining process, the irradiation position and the target position may be scanned while maintaining a constant distance between them. This stabilizes the laser light and the discharged water when they strike the surface of the workpiece, and the plasma confinement effect of the water film can be stably generated. This enhances the peening effect in the machining area.

[0016] In the machining process, the irradiation position and the target position may be fixed, and the workpiece may be scanned relative to the irradiation position and the target position. In this case, the irradiation position of the laser light and the target position of the jetted water during machining can be stabilized. Therefore, the peening effect in the machining area can be made uniform.

[0017] The method may further include a protection step of providing a sacrificial layer on the surface of the workpiece over at least the entire processing area. By providing the sacrificial layer in the processing area, the surface of the workpiece is protected from the laser light. This prevents the surface of the workpiece from being roughened, burned, or suffering from unintended effects (such as the application of tensile stress) in the processing area.

[0018] In the protection step, the sacrificial layer may be disposed so as to reach the edge of the surface of the workpiece when viewed from the front of the processing area. In this case, there is no step between the surface of the workpiece and the sacrificial layer, so that a water film can be formed in the processing area with a more uniform laminar flow.

[0019] In the protection step, the sacrificial layer may be disposed so as to reach the surface expanded by the expansion jig. In this case, peeling of the sacrificial layer from the surface of the workpiece can be suitably prevented when the discharged water is applied to the surface of the workpiece.

[0020] A laser peening device according to one aspect of the present disclosure is a laser peening device that performs peening by irradiating a processing area set on the surface of a workpiece with laser light, and includes an expansion jig that is placed relative to the workpiece and forms an expanded surface in an area outside the surface of the workpiece when viewed from the front of the processing area, an ejection unit that ejects water toward a target position to form a laminar water film spanning the laser light irradiation position and at least a portion of the expanded surface, and a light source unit that irradiates the processing area with laser light through the water film.

[0021] In this laser peening device, an expansion jig is placed on the workpiece, forming an expanded surface by the expansion jig in an area outside the workpiece surface. By forming such an expanded surface, a laminar water film can be formed across the laser light irradiation position and at least a portion of the expanded surface. This makes it possible to prevent disturbance of the water film, for example, near the edge of the workpiece surface, even when the workpiece is small in size or when the entire workpiece is the processing area. Therefore, this laser peening device can solve the problem of uneven processing due to the position of the processing area, and increase the degree of freedom in designing the processing area on the workpiece surface.

[0022] The laser peening device may further include an adjustment mechanism for adjusting the positional relationship between the workpiece surface and the expanded surface by the expansion jig. In this case, it is possible to eliminate the step between the workpiece surface and the expanded surface by the expansion jig, or to make the workpiece surface and the expanded surface by the expansion jig closely contact each other. Therefore, a water film can be formed in the processing area with a more uniform laminar flow.

[0023] The extended surface may have an arithmetic mean roughness Ra of 20 μm or less. By reducing the roughness of the extended surface, the discharged water flowing over the extended surface can be prevented from becoming turbulent, and a water film can be formed in the processing region with a more uniform laminar flow.

[0024] According to the present disclosure, it is possible to increase the degree of freedom in designing the machining area on the surface of the workpiece.

[0025] 1 is a schematic diagram showing a laser peening apparatus according to an embodiment of the present disclosure; FIG. 2 is a perspective view showing a state in which a workpiece is processed using the laser peening apparatus shown in FIG. 1; FIG. 3 is an exploded perspective view of the holding jig and the expansion jig shown in FIG. 2; FIG. 4 is a flowchart showing a laser peening method according to an embodiment of the present disclosure; FIG. 5 is a perspective view showing a process subsequent to FIG. 5; FIG. 6 is a perspective view showing a forming process; and FIG. 7 is a front view showing a processing process. (a) to (d) are front views showing modified examples of the placing process. (a) and (b) are front views showing modified examples of the forming process.

[0026] Hereinafter, preferred embodiments of a laser peening method and a laser peening apparatus according to one aspect of the present disclosure will be described in detail with reference to the drawings.

[0027] Fig. 1 is a schematic diagram showing a laser peening apparatus according to an embodiment of the present disclosure. Fig. 2 is a perspective view showing how a workpiece is processed using the laser peening apparatus shown in Fig. 1. The laser peening apparatus 1 shown in Figs. 1 and 2 is an apparatus that irradiates a workpiece W that is in contact with an interference layer such as water (here, a water film P described below) with high-peak pulsed laser light and generates a peening effect (e.g., application of compressive stress) from the surface Wa of the workpiece W to a predetermined depth by utilizing shock waves generated by the pressure of plasma generated in the interference layer.

[0028] The workpiece W is an object made of various metal materials such as copper, aluminum, and iron. In FIGS. 1 and 2 , a rectangular metal plate-shaped member is shown as an example of the workpiece W. The surface Wa of the workpiece W has a size of, for example, 10 mm square. A machining area K is set in advance on the surface Wa of the workpiece W depending on the intended use of the workpiece W. In this embodiment, the entirety of one main surface of the workpiece W, which is a rectangular plate-shaped member, is set as the machining area K. That is, in this embodiment, when viewed from the front of the workpiece W, the machining area K is set to the edges of the four sides of the rectangular surface Wa of the workpiece W.

[0029] As shown in Figures 1 and 2, the laser peening device 1 is configured to include a light source unit 2 that outputs laser light L toward, for example, a workpiece W, a discharge unit 3 that discharges water (hereinafter referred to as "discharged water Pw") that forms a water film P, and a holding unit 4 that holds the workpiece W.

[0030] The light source unit 2 includes a light source device that outputs laser light L. The operation of the light source unit 2 and the output conditions of the laser light L are controlled by a control unit (not shown). The control unit may be configured with an integrated circuit such as an FPGA (Field-programmable gate array). There are no particular restrictions on the type of light source device used in the light source unit 2, and various light sources can be used depending on the material of the workpiece W. The wavelength of the laser light L is selected within a range that is absorbable by the material of the workpiece W. The laser light L is, for example, pulsed light. As an example, the intensity of the laser light L is 0.5 GW / cm 2 ~20 GW / cm 2 The repetition frequency of the laser light L is 1 Hz.

[0031] A light guide optical system (not shown) may be arranged between the light source unit 2 and the holder 4. The light guide optical system may include, for example, a reflecting mirror and a condensing lens. The laser light L emitted from the light source unit 2 is guided along a predetermined optical path by the reflecting mirror, and then focused by the condensing lens before being irradiated onto the surface Wa of the workpiece W (see FIG. 2). The focused diameter of the laser light L is, for example, about 1 mm. The focused shape of the laser light L is usually circular, but may also be elliptical, rectangular, linear, etc.

[0032] The discharge unit 3 includes a nozzle 5 that discharges the discharge water Pw with a predetermined diameter. The operation of the discharge unit 3 and the supply conditions of the discharge water Pw are controlled by the control unit described above. As shown in FIG. 2 , the nozzle 5 is positioned so that, for example, the target position M1 of the discharge water Pw on the surface Wa of the workpiece W is above the irradiation position M2 of the laser light L. In this embodiment, the target position M1 of the discharge water Pw is located approximately 5 mm above the irradiation position M2 of the laser light L. As an example, the discharge rate of the discharge water Pw is 0.1 L / min to 1 L / min, and the diameter of the discharge water Pw at the target position M1 is 1 mm to 5 mm.

[0033] The water Pw discharged from the tip of the nozzle 5 hits the surface Wa of the workpiece W at the target position M1 and spreads to a certain width, forming a laminar water film P below the target position M1 (see FIG. 2). Laminar flow refers to a state in which fluids do not mix with each other and flow regularly along the flow direction. By stably forming the laminar water film P, it is possible to fully generate the plasma confinement effect of the water film P when irradiated with the laser light L, and it is possible to suppress uneven processing in the processing area K.

[0034] The thickness of the water film P is, for example, about 0.1 to 10 mm, and preferably about 1 mm. If the thickness of the water film P is 0.1 mm or more, it is possible to sufficiently generate the plasma confinement effect of the water film P when irradiating the laser light L. If the thickness of the water film P is 10 mm or less, it is possible to suppress attenuation of the intensity of the laser light L by the water film P, even if the laser light L includes a wavelength range that is absorbed by water.

[0035] As shown in Figure 3, the holding unit 4 is configured to include a holding jig 11 and an expansion jig 12 that are placed relative to the workpiece W, and a movable stage 13 (see Figure 1) that holds the holding jig 11 and the expansion jig 12. The holding jig 11 is a member that holds the back side of the workpiece W. In this embodiment, the holding jig 11 is configured from a rectangular plate-shaped member that is slightly larger than the workpiece W. There are no particular restrictions on the material that the holding jig 11 is made of, but it is preferable to use a material that has a hardness that is equal to or greater than the hardness of the workpiece W.

[0036] In this embodiment, the rectangular area in the center of the holding jig 11 is the holding area for the workpiece W, and the holding jig 11 itself is held vertically on the movable stage 13, thereby holding the workpiece W so that the surface Wa of the workpiece W is vertical. With the surface Wa of the workpiece W being vertical, the processing area K is also positioned vertically. Therefore, the water film P on the surface Wa of the workpiece W is also formed by a laminar flow flowing vertically downward.

[0037] The expansion jig 12 is a jig that forms an expansion surface 15 in a region outside the surface Wa of the workpiece W when viewed from the front of the processing area K. In this embodiment, the expansion jig 12 is, for example, a rectangular plate-shaped member having a thickness similar to that of the workpiece W, and one entire main surface of the expansion jig 12 is used as the expansion surface 15. The constituent material of the expansion jig 12 is not particularly limited, but, as with the holding jig 11, it is preferable to use a material having a hardness equal to or greater than that of the workpiece W. The expansion surface 15 is preferably smooth. In this embodiment, the arithmetic mean roughness Ra of the expansion surface 15 is 20 μm or less. Furthermore, considering the intimate contact with the sacrificial layer 20 described below, it is preferable that the arithmetic mean roughness Ra of the expansion surface 15 be 10 μm or less. The smoothness of the expansion surface 15 can be ensured by surface finishing (e.g., mechanical polishing or milling) used for general metal materials.

[0038] In this embodiment, multiple expansion jigs 12 are prepared for the workpiece W. In the example of Figure 3, the expansion jigs 12 are composed of an upper expansion jig 12A, a lower expansion jig 12B, and a pair of side expansion jigs 12C, 12C. The upper expansion jig 12A is a jig that forms an expansion surface 15 above the surface Wa of the workpiece W in a front view of the machining area K, and the lower expansion jig 12B is a jig that forms an expansion surface 15 below the surface Wa of the workpiece W in a front view of the machining area K. The pair of side expansion jigs 12C, 12C are jigs that form expansion surfaces 15 on the left and right sides of the surface Wa of the workpiece W in a front view of the machining area K.

[0039] In the example of Figure 3, the vertical width of each of the upper expansion jig 12A, the lower expansion jig 12B, and the pair of side expansion jigs 12C, 12C is approximately the same as the vertical width of the workpiece W. The horizontal width of the pair of side expansion jigs 12C, 12C is approximately the same as the horizontal width of the workpiece W. The horizontal widths of the upper expansion jig 12A and the lower expansion jig 12B are approximately the same as the sum of the horizontal width of the workpiece W and the horizontal width of the pair of side expansion jigs 12C, 12C. By arranging the upper expansion jig 12A, the lower expansion jig 12, and the pair of side expansion jigs 12C, 12C on the top, bottom, left, and right sides of the workpiece W held in the central holding area of ​​the holding jig 11, an expansion surface 15 is formed by the expansion jig 12 so as to surround the surface Wa of the workpiece W when viewed from the front of the processing area K.

[0040] From the viewpoint of the stability of the water film P due to the laminar flow, it is preferable that the surface Wa of the workpiece W and the expanded surface 15 are flush with each other. By aligning the thickness of the workpiece W with the thickness of the expansion jig 12, the surface Wa of the workpiece W and the expanded surface 15 can be flush with each other. While it is ideal to flush the surface Wa of the workpiece W with the expanded surface 15, slight differences in level may occur due to dimensional tolerances of the workpiece W or the expansion jig 12. In this case, the surface Wa of the workpiece W and the expanded surface 15 may be flush with each other by making the thickness of the expansion jig 12 thicker than the thickness of the workpiece W and appropriately inserting a shim 16 (see Figure 3) of a predetermined thickness between the workpiece W and the holding jig 11. The shim 16 is one of the adjustment mechanisms for adjusting the positional relationship between the surface Wa of the workpiece W and the expanded surface 15 created by the expansion jig 12. Using the shim 16, the positional relationship between the surface Wa of the workpiece W and the expanded surface 15 created by the expansion jig 12 can be adjusted in the thickness direction of the workpiece W. From the viewpoint of the stability of the water film P due to the laminar flow, the step in the thickness direction between the surface Wa of the workpiece W and the extended surface 15 may be, for example, 0.1 mm or less.

[0041] Similarly, from the viewpoint of the stability of the water film P due to the laminar flow, it is preferable that the surface Wa of the workpiece W and the expanded surface 15 are closely spaced in their planar direction. In this context, "closely spaced" means that the surface Wa of the workpiece W and the expanded surface 15 are ideally continuous with no gaps between them. However, slight gaps may occur due to dimensional tolerances of the workpiece W or the expansion jig 12. In this case, the gap is preferably equal to or less than the Rayleigh length of the laser light L (the distance between the irradiation position M2 of the laser light L and the position where the cross-sectional area of ​​the laser light L is twice the cross-sectional area at the irradiation position M2). The gap may be equal to or less than 1 / 100 of the size of the surface Wa of the workpiece W. Furthermore, the gap may be equal to or less than 1 / 10 of the focused diameter of the irradiated laser light L. In this embodiment, the size of the surface Wa of the workpiece W is 10 mm square, and the gap is preferably equal to or less than 0.1 mm.

[0042] In this embodiment, the upper expansion jig 12A is provided integrally with the holding jig 11. The upper expansion jig 12A may be formed by a thick portion of the holding jig 11, or may be formed by joining a separate plate-like member to the holding jig 11 by adhesive bonding, welding, or the like. In addition, in this embodiment, the expansion jig 12 is provided with a screw 17, a long hole 18, and a screw hole 19 as one of the adjustment mechanisms for adjusting the positional relationship between the surface Wa of the workpiece W and the expanded surface 15 by the expansion jig 12. The screw 17 and the long hole 18 allow the positional relationship between the surface Wa of the workpiece W and the expanded surface 15 by the expansion jig 12 to be adjusted in the in-plane direction of the surface Wa of the workpiece W.

[0043] Here, screws 17 are used to fix the lower expansion jig 12 and the pair of side expansion jigs 12C, 12C to the holding jig 11, and the holding jig 11 is provided with a plurality of screw holes 19 corresponding to the elongated holes 18, 18. The lower expansion jig 12 is provided with an elongated hole 18 whose major axis is in the vertical direction, and the pair of side expansion jigs 12C, 12C are provided with an elongated hole 18 whose major axis is in the horizontal direction. The specific fixing directions of the lower expansion jig 12 and the pair of side expansion jigs 12C, 12C will be described later.

[0044] The movable stage 13 is configured, for example, by an XY stage. The operation of the movable stage 13 is controlled by the above-mentioned control unit. As shown in FIG. 1 , the movable stage 13 holds the holding jig 11 to which the workpiece W and the extension jig 12 are fixed so that the surface Wa of the workpiece W is perpendicular to the optical axis of the laser light L, and moves the holding jig 11 vertically and horizontally within the plane of the surface Wa of the workpiece W. As a result, the irradiation position M2 and the target position M1 on the surface Wa of the workpiece W are scanned while maintaining a constant distance between the irradiation position M2 of the laser light L and the target position M1 of the discharged water Pw.

[0045] 2, from the viewpoint of preventing laser damage to the surface Wa of the workpiece W, a sacrificial layer 20 is disposed on the surface of the workpiece W over at least the entire processing region K. The thickness of the sacrificial layer 20 is, for example, about 10 μm to 1000 μm, and preferably about 100 μm. By making the thickness of the sacrificial layer 20 10 μm or more, roughening, burning, and the occurrence of unintended effects (such as the application of tensile stress) on the surface Wa of the workpiece W in the processing region K can be suitably suppressed.

[0046] Although paint, oil, etc. may be used for the sacrificial layer 20, here a metal tape with a thickness of about 100 μm is used. The sacrificial layer 20 has, for example, a rectangular shape, and is arranged so as to reach the edges of the surface Wa of the workpiece W when viewed from the front of the processing area K. In this embodiment, the entire surface Wa of the workpiece W is set as the processing area K, and the sacrificial layer 20 extends to the edges of the four sides of the surface Wa of the workpiece W.

[0047] Furthermore, in this embodiment, the sacrificial layer 20 has a rectangular shape that is slightly larger than the surface Wa of the workpiece W, and extends beyond the edges of the four sides of the surface Wa of the workpiece W to reach the respective expansion surfaces 15 formed by the upper expansion jig 12A, the lower expansion jig 12, and the pair of side expansion jigs 12C, 12C. Because the sacrificial layer 20 extends to reach the expansion surfaces 15, when the irradiation position M2 and the target position M1 on the surface Wa of the workpiece W are scanned, the target position M1 of the ejected water Pw overlaps the sacrificial layer 20. Therefore, the water film P formed by the laminar flow is formed below the target position M1 without being affected by the step between the surface Wa of the workpiece W and the sacrificial layer 20 due to the thickness of the sacrificial layer 20.

[0048] When the sacrificial layer 20 is formed using a metal tape as in this embodiment, it is conceivable that when plasma pressure is generated by irradiation with the laser light L, the plasma pressure will generate a force that stretches the sacrificial layer 20 in an in-plane direction. When this force acts on the edge of the sacrificial layer 20, it is assumed that the sacrificial layer 20 will act in a direction that causes it to peel off from the surface Wa of the workpiece W. Therefore, by arranging the sacrificial layer 20 so that it reaches the expanded surface 15 and by moving the edge of the sacrificial layer 20 away from the irradiation position M2 of the laser light L, it is possible to prevent the sacrificial layer 20 from peeling off due to the action of the above force.

[0049] Next, a laser peening method according to an embodiment of the present disclosure will be described. Fig. 4 is a flowchart showing the laser peening method according to an embodiment of the present disclosure. As shown in Fig. 4, this laser peening method includes a placement step (step S01), a protection step (step S02), a formation step (step S03), and a processing step (step S04). In this embodiment, each step of the laser peening method is performed using the laser peening apparatus 1 described above.

[0050] The placement process is a process of placing the expansion jig 12 on the workpiece W and forming an expansion surface 15 by the expansion jig 12 in an area outside the surface Wa of the workpiece W when viewed from the front of the processing area K. Specifically, in the placement process, first, as shown in Figure 5, the workpiece W is set in the central holding area of ​​the holding jig 11 in the holding unit 4. At this time, if necessary, a shim 16 is placed between the workpiece W and the holding jig 11, and the positional relationship is adjusted so that the surface of the workpiece W and the expansion surface 15 of the expansion jig 12 are flush with each other.

[0051] Next, the workpiece W is positioned relative to the upper expansion jig 12A by abutting the upper surface of the upper expansion jig 12A against the lower surface of the upper expansion jig 12A. This brings the upper edge of the surface Wa of the workpiece W into close contact with the expansion surface 15 of the upper expansion jig 12A. After positioning the workpiece W relative to the upper expansion jig 12A, the upper surface of the lower expansion jig 12 is abutted against the lower surface of the workpiece W, and the lower expansion jig 12 is positioned relative to the workpiece W while sandwiching the workpiece W between the upper expansion jig 12A and the lower expansion jig 12. In this state, by threading the screw 17 into the screw hole 19 of the holding jig 11 through the elongated hole 18, the lower expansion jig 12 is fixed to the holding jig 11 with the lower edge of the surface Wa of the workpiece W and the expansion surface 15 of the lower expansion jig 12 in close contact.

[0052] After the lower expansion jig 12 is fixed, as shown in Figure 6, a pair of side expansion jigs 12C, 12C are arranged so that the workpiece W is sandwiched between the upper expansion jig 12A and the lower expansion jig 12 on the left and right. Then, the sides of the pair of side expansion jigs 12C, 12C are abutted against the left and right sides of the workpiece W, respectively, to position the pair of side expansion jigs 12C, 12C with respect to the workpiece W. In this state, by threading screws 17 into the screw holes 19 of the holding jig 11 through the elongated holes 18, the pair of side expansion jigs 12C, 12C are fixed to the holding jig 11 with the left and right edges of the surface Wa of the workpiece W in close contact with the respective expansion surfaces 15, 15 of the pair of side expansion jigs 12C, 12C.

[0053] The protection process is a process of placing a sacrificial layer 20 over at least the entire processing area K. In this embodiment, as shown in FIG. 7 , the entire surface Wa of the workpiece W is set as the processing area K, and a rectangular sacrificial layer 20 is placed so that it reaches the edges of the four sides of the surface Wa of the workpiece W when viewed from the front of the processing area K. In this embodiment, a rectangular sacrificial layer 20 that is slightly larger than the surface Wa of the workpiece W is used, and the sacrificial layer 20 is placed so that it extends beyond the edges of the four sides of the surface Wa of the workpiece W and reaches the respective expansion surfaces 15 formed by the upper expansion jig 12A, the lower expansion jig 12, and the pair of side expansion jigs 12C, 12C. The amount by which the sacrificial layer 20 protrudes from the edges of the four sides of the surface Wa of the workpiece W onto the expansion surfaces 15 is, for example, approximately 3 mm to 4 mm.

[0054] The forming process is a process in which the water Pw is ejected toward the target position M1 to form a laminar water film P across the irradiation position M2 of the laser light L and at least a portion of the expansion surface 15. In the forming process, the water Pw ejected from the tip of the nozzle 5 is directed toward the surface Wa of the workpiece W at the target position M1, forming a laminar water film P below the target position M1. In the above-mentioned protection process, the sacrificial layer 20 is positioned so that it reaches the respective expansion surfaces 15 formed by the upper expansion jig 12A, the lower expansion jig 12, and the pair of lateral expansion jigs 12C, 12C. For this reason, in this embodiment, the target position M1 of the ejected water Pw overlaps with the sacrificial layer 20, and the ejected water Pw does not directly impinge on the surface Wa of the workpiece W at the target position M1, but rather impinges on the sacrificial layer 20 (see FIG. 2).

[0055] The processing step is a step of irradiating a processing region K with laser light L through a water film P. Irradiation of the laser light L generates plasma in the water film P, which is an interference layer. Shock waves generated by the pressure of the plasma cause a peening effect (e.g., application of compressive stress) from the surface Wa of the workpiece W to a predetermined depth. When irradiating the laser light L, a sacrificial layer 20 is provided on the surface Wa of the workpiece W, thereby preventing laser damage to the surface Wa of the workpiece W.

[0056] In the machining process, as shown in FIG. 8 (the screw 17 and the elongated hole 18 are not shown), the irradiation position M2 and the target position M1 are scanned while maintaining a constant distance between the irradiation position M2 and the target position M1. In this embodiment, the irradiation position M2 and the target position M1 are fixed positions, and the holding jig 11 holding the workpiece W and the extension jig 12 is moved vertically and horizontally by the movable stage 13 to scan the irradiation position M2 and the target position M1 on the surface Wa of the workpiece W. The example of FIG. 8 shows bidirectional horizontal scanning (scanning in one horizontal direction, then scanning vertically, and then scanning in the opposite horizontal direction). The scanning order is not limited to this, and bidirectional vertical scanning (scanning in one vertical direction, then scanning horizontally downward, and then scanning in the opposite vertical direction) may also be used.

[0057] As described above, in the laser peening apparatus 1 and laser peening method, by placing the expansion jig 12 on the workpiece W, the expansion jig 12 forms an expanded surface 15 in a region outside the surface Wa of the workpiece W. By forming such an expanded surface 15, a water film P due to laminar flow can be formed across the irradiation position M2 of the laser light L and at least a portion of the expanded surface 15. This makes it possible to prevent disturbance of the water film P, for example, near the edge of the surface Wa of the workpiece W, even when the size of the workpiece W is small or when the entire surface of the workpiece W is the processing region K. Therefore, the laser peening apparatus 1 and laser peening method can solve the problem of processing unevenness due to the position of the processing region K, and increase the degree of freedom in designing the processing region K on the surface Wa of the workpiece W.

[0058] In the positioning process, the expansion jig 12 forms an expansion surface 15 above the surface Wa of the workpiece W when viewed from the front of the processing area K. This allows the target position M1 of the discharged water Pw to be set above the surface Wa of the workpiece W, and a water film P can be stably formed by laminar flow on the upper edge of the surface of the workpiece W. Therefore, it is possible to position the processing area K near the upper edge of the surface Wa of the workpiece W.

[0059] In the placement process, the expansion jig 12 forms an expanded surface 15 that surrounds the surface Wa of the workpiece W when viewed from the front of the machining area. This allows the target position M1 of the discharged water Pw to be set around the surface Wa of the workpiece W, and a water film P can be stably formed by laminar flow around the entire periphery of the surface Wa of the workpiece W. Therefore, it is possible to position the machining area K over the entire edge of the surface Wa of the workpiece W.

[0060] In the placement process, the expansion jig is placed on the workpiece W so that the surface Wa of the workpiece W and the expanded surface 15 by the expansion jig 12 are flush with each other. This eliminates any step between the surface Wa of the workpiece W and the expanded surface 15 by the expansion jig 12, allowing the water film P to be formed in the processing area K with a more uniform laminar flow.

[0061] In the placement process, the expansion jig 12 is brought into close contact with the workpiece W, so that the surface Wa of the workpiece W and the expanded surface 15 by the expansion jig 12 are in close contact with each other. This reduces the gap between the surface Wa of the workpiece W and the expanded surface 15 by the expansion jig 12, allowing the water film P to be formed in the processing area K with a more uniform laminar flow.

[0062] In the placement process, an expansion jig 12 having an expansion surface 15 with an arithmetic mean roughness Ra of 20 μm or less is used. By reducing the roughness of the expansion surface 15, the discharged water Pw flowing along the expansion surface 15 can be prevented from becoming turbulent, and a water film P can be formed with a more uniform laminar flow in the processing region K. Furthermore, by using an expansion jig 12 having an expansion surface 15 with an arithmetic mean roughness Ra of 10 μm or less, the adhesion of the sacrificial layer 20 to the expansion surface 15 can be sufficiently ensured.

[0063] In the placement process, a holding jig 11 is placed to hold the back surface of the workpiece W and the back surface of the expansion jig 12. This makes it easy to place the expansion jig 12 on the workpiece W. Furthermore, by holding the back surface of the workpiece W with the holding jig 11, deformation of the workpiece W during processing can be suppressed. Therefore, the peening effect in the processing region K can be improved.

[0064] In the machining process, the irradiation position M2 and the target position M1 are scanned while maintaining a constant distance between them. This stabilizes the laser light L and the discharged water Pw when they strike the surface Wa of the workpiece W, and the plasma confinement effect of the water film P can be stably generated. Therefore, the peening effect in the machining region K can be enhanced.

[0065] In the machining process, the irradiation position M2 and the target position M1 are fixed, and the workpiece W is scanned relative to the irradiation position M2 and the target position M1. In this case, by fixing the light guiding optical system of the laser light L and the nozzle 5 of the discharged water Pw, the irradiation position M2 of the laser light L and the target position M1 of the discharged water Pw can be stabilized during machining. Therefore, the peening effect in the machining region K can be made uniform.

[0066] In the protection step, a sacrificial layer 20 is placed on the surface Wa of the workpiece W over at least the entire processing region K. By placing the sacrificial layer 20 in the processing region K, the surface Wa of the workpiece W is protected from the laser light L. This makes it possible to prevent the surface Wa of the workpiece W in the processing region K from becoming rough, burning, or having unintended effects (for example, the application of tensile stress).

[0067] In the protection process, the sacrificial layer 20 is arranged so that it reaches the edge of the surface Wa of the workpiece W when viewed from the front of the processing area K. This eliminates any step between the surface Wa of the workpiece W and the sacrificial layer 20, allowing a water film to be formed with a more uniform laminar flow in the processing area K. Furthermore, in the protection process, the sacrificial layer 20 is arranged so that it reaches the expanded surface 15 created by the expansion jig 12. This makes it possible to suitably prevent the sacrificial layer 20 from peeling off from the surface Wa of the workpiece W when the discharged water Pw is applied to the surface Wa of the workpiece W.

[0068] The laser peening device 1 is provided with an adjustment mechanism (shim 16, screw 17, elongated hole 18, and screw hole 19) for adjusting the positional relationship between the surface Wa of the workpiece W and the expanded surface 15 by the expansion jig 12. By introducing such an adjustment mechanism, it is possible to eliminate the step between the surface Wa of the workpiece W and the expanded surface 15 by the expansion jig 12, or to make the surface Wa of the workpiece W and the expanded surface 15 by the expansion jig 12 closely contact each other. Therefore, a water film P can be formed in the processing region K with a more uniform laminar flow.

[0069] Furthermore, in the laser peening apparatus 1, the arithmetic mean roughness Ra of the expansion surface 15 of the expansion jig 12 is 20 μm or less. By suppressing the roughness of the expansion surface 15, it is possible to prevent the discharged water Pw flowing on the expansion surface 15 from becoming turbulent, and it is possible to form the water film P in the processing region K with a more uniform laminar flow.

[0070] The present disclosure is not limited to the above-described embodiment. For example, in the above-described embodiment, the entire surface Wa of the workpiece W is set as the processing area K, but the setting of the processing area K is arbitrary, and a part of the surface Wa of the workpiece W may be set as the processing area K. The processing area K may be set in a linear shape or in a dotted shape. A dotted processing area refers to, for example, an area that is processed by irradiating the laser light L once without scanning the surface Wa of the workpiece W with the laser light L. In other words, a dotted processing area is, for example, an area that corresponds to the focused diameter of the laser light L.

[0071] In the above embodiment, when scanning the irradiation position M2 and the target position M1, the sacrificial layer 20 protruding onto the expansion surface 15 is included in the target position M1 of the discharged water Pw, but the expansion surface 15 itself may also be included in the target position M1. In the above embodiment, the irradiation position M2 and the target position M1 are fixed positions, and the workpiece W is scanned with respect to the irradiation position M2 and the target position M1, but an embodiment in which the workpiece W is fixed position and the irradiation position M2 and the target position M1 are scanned with respect to the workpiece W may also be adopted.

[0072] In the above embodiment, the expansion jigs 12 form expansion surfaces 15 on the top, bottom, left, and right sides of the surface Wa of the workpiece W so as to surround the surface Wa. However, the formation of the expansion surfaces 15 is not limited to this, and various modifications are possible depending on the setting of the machining area K. For example, as shown in FIG. 9( a), the expansion surfaces 15 may be formed on the top and bottom sides of the surface Wa of the workpiece W using only the upper expansion jig 12A and the lower expansion jig 12. As shown in FIG. 9( b), the expansion surface 15 may be formed only on the top side of the surface Wa of the workpiece W using only the upper expansion jig 12A. As shown in FIG. 9( c), the expansion surfaces 15 may be formed on the left and right sides of the surface Wa of the workpiece W using only a pair of side expansion jigs 12C, 12C. As shown in FIG. 9( d), the expansion surface 15 may be formed only on the bottom side of the surface Wa of the workpiece W using only the lower expansion jig 12. As a further modification of FIG. 9C, an extended surface 15 may be formed on either the left or right side of the surface Wa of the workpiece W using only one of the pair of side extension jigs 12C, 12C.

[0073] In the above embodiment, the sacrificial layer 20 extends beyond the edges of the four sides of the surface Wa of the workpiece W to reach the respective expansion surfaces 15 formed by the upper expansion jig 12A, the lower expansion jig 12, and the pair of side expansion jigs 12C, 12C. However, the arrangement of the sacrificial layer 20 is not limited to this and various modifications are possible depending on the setting of the processing area K. For example, as shown in FIG. 10( a), the sacrificial layer 20 may be arranged so as to align with the edges of the four sides of the surface Wa of the workpiece W. As shown in FIG. 10( b), the sacrificial layer 20 may be arranged so as to reach only the upper expansion surface 15 of the surface Wa of the workpiece W. Although not shown, the sacrificial layer 20 may also be arranged so as to reach one or more expansion surfaces 15 of the surface Wa of the workpiece W in any direction.

[0074] In this embodiment, a rectangle is exemplified as the shape of the surface Wa of the workpiece W (the shape of the workpiece W when viewed from the front), but the shape of the surface Wa of the workpiece W may be other shapes such as a circle, an ellipse, a polygon, etc. The shape of the expansion surface 15 of the expansion jig 12 may also be a shape other than a rectangle depending on the shape of the surface Wa of the workpiece W.

[0075] In this embodiment, the surface Wa of the workpiece W and the expanded surface 15 are flush with each other, but they do not necessarily have to be flush with each other as long as a water film P due to laminar flow is formed so as to straddle the irradiation position M2 of the laser light L and at least a portion of the expanded surface 15. In other words, a step may be formed between the surface Wa and the expanded surface 15 as long as the water film P due to laminar flow is formed so as to straddle the irradiation position M2 of the laser light L and at least a portion of the expanded surface 15. Such a step may be greater than 0.1 mm, for example.

[0076] In addition, in this embodiment, the surface Wa of the workpiece W and the expanded surface 15 are in close contact with each other in the planar direction, but a gap may be formed in the planar direction between the surface Wa of the workpiece W and the expanded surface 15 as long as the gap is within a range in which a water film P is formed by laminar flow so as to span the irradiation position M2 of the laser light L and at least a part of the expanded surface 15. Such a gap may be larger than 0.1 mm, for example.

[0077] 1...laser peening device, 2...light source unit, 3...discharge unit, 11...holding jig, 12...expansion jig, 15...expansion surface, shim 16 (adjustment mechanism), screw 17 (adjustment mechanism), long hole 18 (adjustment mechanism), screw hole 19 (adjustment mechanism), 20...sacrificial layer, W...workpiece, Wa...surface, K...processing area, L...laser light, M1...target position, M2...irradiation position, P...water film, Pw...discharged water.

Claims

1. A laser peening method for peening a processing area set on the surface of a workpiece by irradiating it with laser light, comprising: a positioning step of placing an expansion tool on the workpiece and forming an expanded surface by the expansion tool in an area outside the surface of the workpiece when viewed from the front of the processing area; a formation step of forming a water film by laminar flow using water ejected toward a target position so as to span the irradiation position of the laser light and at least a portion of the expanded surface; and a processing step of irradiating the processing area with the laser light through the water film.

2. A laser peening method according to claim 1, wherein in the positioning step, an expanded surface is formed by the expansion jig above the surface of the workpiece when viewed from the front of the processing area.

3. A laser peening method according to claim 1 or 2, wherein in the positioning step, an extended surface is formed by the extension jig so as to surround the surface of the workpiece when viewed from the front of the processing area.

4. A laser peening method according to any one of claims 1 to 3, wherein in the positioning step, the expansion jig is positioned relative to the workpiece so that the surface of the workpiece and the expanded surface by the expansion jig are flush with each other.

5. A laser peening method according to any one of claims 1 to 4, wherein in the positioning process, the expansion jig is brought into close contact with the workpiece, and the surface of the workpiece and the expanded surface by the expansion jig are brought into close contact with each other.

6. A laser peening method according to any one of claims 1 to 5, wherein in the positioning step, an expansion jig having an arithmetic mean roughness Ra of the expansion surface of 20 μm or less is used.

7. A laser peening method according to any one of claims 1 to 6, wherein the positioning step includes positioning a holding jig for holding the back surface of the workpiece and the back surface of the expansion jig.

8. A laser peening method according to any one of claims 1 to 7, wherein in the processing step, the irradiation position and the target position are scanned while maintaining a constant distance between the irradiation position and the target position.

9. A laser peening method according to any one of claims 1 to 8, wherein in the processing step, the irradiation position and the target position are fixed positions, and the workpiece is scanned relative to the irradiation position and the target position.

10. A laser peening method according to any one of claims 1 to 9, further comprising a protection step of disposing a sacrificial layer on the surface of the workpiece over at least the entire processing area.

11. A laser peening method according to claim 10, wherein in the protection step, the sacrificial layer is disposed so as to extend to the edge of the surface of the workpiece when viewed from the front of the processing area.

12. A laser peening method according to claim 10 or 11, wherein in the protection step, the sacrificial layer is disposed so as to reach the surface expanded by the expansion jig.

13. A laser peening device that performs peening by irradiating a processing area set on the surface of a workpiece with laser light, comprising: an expansion jig that is arranged with respect to the workpiece and forms an expanded surface in an area outer than the surface of the workpiece when viewed from the front of the processing area; a discharge unit that discharges water toward a target position to form a water film by laminar flow so as to span the irradiation position of the laser light and at least a part of the expanded surface; and a light source unit that irradiates the laser light to the processing area through the water film.

14. The laser peening apparatus according to claim 13, further comprising an adjustment mechanism for adjusting the positional relationship between the surface of the workpiece and the surface expanded by the expansion jig.

15. A laser peening apparatus according to claim 13 or 14, wherein the arithmetic mean roughness Ra of the extended surface is 20 μm or less.

Citation Information

Patent Citations

  • Laser shock peening system with time-of-flight monitoring

    JP2007152434A

  • A system and method for performing laser shock peening on a target having a fluid flow path sandwiched between a solid medium transparent to laser light and the target

    JP2016515475A

  • Overlay control for laser peening

    US20030213788A1

  • Mechanical gauges for quality assurance of laser peening

    US6483578B1

  • Laser processing device, and laser processing method

    WO2020166670A1