Laminated film for diaphragm and method for manufacturing same
A three-layer laminated film with ester-based and styrene-based thermoplastic elastomer layers addresses the balance of rigidity, internal loss, and heat resistance in speaker diaphragms, ensuring durable and high-quality sound performance.
Patent Information
- Application Number
- PCT/JP2024/007488
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-27
- Filing Date
- 2024-02-29
- Publication Date
- 2024-10-03
AI Technical Summary
Speaker diaphragms face challenges in achieving a balance between high rigidity, moderate internal loss, and light weight, with existing materials often failing to maintain sound quality over long-term use due to temperature-related changes.
A three-layer laminated film structure comprising ester-based thermoplastic elastomer outer layers and a styrene-based thermoplastic elastomer intermediate layer, with specific thickness ratios and materials like polystyrene-poly(ethylene-butylene)-polystyrene copolymer, providing enhanced heat resistance and internal loss.
The laminated film achieves a suitable balance of internal loss and heat resistance, ensuring durable and high-quality sound performance even under prolonged use and varying temperatures.
Smart Images

Figure JP2024007488_03102024_PF_FP_ABST
Abstract
Description
Laminated film for diaphragm and method for manufacturing same
[0001] The present invention relates to a laminated film made of synthetic resin for use as a diaphragm for a speaker.
[0002] Speaker diaphragms are required to be highly rigid, have adequate internal loss, and be lightweight. Various materials are used for diaphragms, but synthetic resins are often used for small speakers used in mobile devices, earphones, etc. Furthermore, since a single material often cannot achieve both lightweight, high rigidity, and adequate internal loss, diaphragms with a laminated structure are often used to improve these balances.
[0003] For example, Patent Document 1 describes a speaker diaphragm including two surface layers made of thermoplastic polyester elastomer films and an intermediate layer that is an adhesive layer. Patent Document 2 describes a diaphragm for an acoustic transducer including a base body having a polyester elastomer and a vibration-damping layer. Patent Document 2 also describes that when a small speaker device or the like is driven for a long period of time, the temperature of the diaphragm itself increases, which changes the characteristics of the diaphragm and may result in a deterioration in sound quality.
[0004] Patent Publication No. 2021-527995 International Publication No. 2009 / 118940
[0005] The present invention has been made in consideration of the above, and its object is to provide a synthetic resin laminated film that can be used as a new diaphragm having a moderately large internal loss and excellent heat resistance, or as a material for such a diaphragm.
[0006] The laminated film for diaphragms of the present invention has a three-layer structure in which first and second outer layers are made of an ester-based thermoplastic elastomer and an intermediate layer is made of a styrene-based thermoplastic elastomer, the thickness ratio of the first outer layer to the second outer layer is in the range of 0.5:1.5 to 1.5:0.5, and the ratio of the total thickness of the first outer layer and the second outer layer to the thickness of the intermediate layer is in the range of 2:3 to 2:8. Preferably, the styrene-based thermoplastic elastomer is a polystyrene-poly(ethylene-butylene)-polystyrene copolymer.
[0007] The manufacturing method of the laminated film for diaphragms of the present invention includes the steps of kneading and melting an ester-based thermoplastic elastomer, kneading and melting a styrene-based thermoplastic elastomer, and co-extruding the molten ester-based thermoplastic elastomer as two outer layers and the molten styrene-based thermoplastic elastomer as an intermediate layer.
[0008] According to the laminated film for diaphragms or the manufacturing method thereof of the present invention, a moderately large internal loss and required heat resistance can be obtained.
[0009] 1 is a diagram illustrating a layer structure of a laminated film for a diaphragm according to an embodiment of the present invention, and is a diagram illustrating the temperature dependence of a loss factor of the laminated film for a diaphragm.
[0010] Referring to Figure 1, a laminate film 10 for a diaphragm according to one embodiment has a three-layer structure consisting of a first outer layer 11, a second outer layer 12, and an intermediate layer 13, which constitute both surfaces of the laminate film 10. The laminate film 10 for a diaphragm is processed into a required shape, or is laminated with other films and then processed into a required shape, and is used as a diaphragm for a speaker. Hereinafter, the laminate film for a diaphragm will be simply referred to as a laminate film.
[0011] The first outer layer 11 and the second outer layer 12 are made of a thermoplastic ester elastomer (TPC). TPC is a block copolymer in which the hard segment is an aromatic polyester and the soft segment is a polyether or polyester. TPC has higher rigidity and excellent heat resistance than general rubber. The melting point of TPC is preferably 180°C or higher and 220°C or lower. If the melting point of TPC is too low, the laminate film 10 will not have sufficient heat resistance, and if the melting point of TPC is too high, the cold resistance will be poor, leading to a decrease in physical properties in the negative temperature range.
[0012] The hard segment of the TPC is preferably heat-resistant polybutylene terephthalate (PBT). This allows the laminate film 10 to have superior heat resistance and mechanical strength. The TPC can be a polyester-polyether type elastomer (TPC-ET) in which the soft segment has an ether bond, a polyester-polyester type elastomer (TPC-ES) in which the soft segment has an ester bond, or a polyester-poly(ether-ester) type elastomer (TPC-EE) in which the soft segment has both ether and ester bonds. Various commercially available TPCs can be used. Ester-based thermoplastic elastomers are sometimes abbreviated as TPEE in this technical field.
[0013] The TPC may contain additives such as a heat stabilizer and an antioxidant, preferably in an amount of 5% by mass or less, as long as the properties of the laminate film 10 are not impaired.
[0014] The TPC constituting the first outer layer 11 and the second outer layer 12 may be a mixture of two or more different TPCs. The first outer layer and the second outer layer may be made of different types or components of TPC, but preferably are made of the same TPC.
[0015] Although there are no particular limitations on the thickness ratio of the first outer layer 11 to the second outer layer 12, from the viewpoint of ease of production, it is preferable that the thicknesses of the first outer layer 11 and the second outer layer 12 are approximately the same. Specifically, the thickness ratio of the first outer layer to the second outer layer is preferably in the range of 0.5:1.5 to 1.5:0.5, and more preferably in the range of 0.9:1.1 to 1.1:0.9.
[0016] The intermediate layer 13 is made of a styrene-based thermoplastic elastomer (TPS). TPS is a block copolymer consisting of a hard segment of polystyrene and a soft segment of polydiene or hydrogenated polydiene. TPS has a larger internal loss (loss factor, tan δ) than TPC, and by using TPS as an intermediate layer, the internal loss of the laminated film 10 can be increased.
[0017] It is preferable to use a hydrogenated TPS. This improves the heat resistance of the TPS and prevents unexpected reactions from occurring during the film-forming process, which is carried out at high temperatures. As the hydrogenated TPS, various copolymers with different soft segments can be used, such as polystyrene-poly(ethylene-butylene)-polystyrene (TPS-SEBS), polystyrene-poly(ethylene-propylene)-polystyrene (TPS-SEPS), polystyrene-poly(ethylene-ethylene-propylene)-polystyrene (TPS-SEEPS), and polystyrene-poly(ethylene-propylene)-polystyrene (TPS-SEP). Of these, it is particularly preferable to use TPS-SEBS, whose soft segment is made of poly(ethylene-butylene). This is because the loss factor peak is high and the position of the peak is close to the temperature range normally used in speakers, etc.
[0018] The TPS may contain additives such as a heat stabilizer and an antioxidant, preferably in an amount of 5% by mass or less, to the extent that the properties of the laminate film 10 are not impaired.
[0019] Various commercially available TPSs can be used, and the TPS may be a mixture of two or more different TPSs.
[0020] The thickness of the intermediate layer 13 is preferably such that the ratio of the total thickness of the first outer layer 11 and the second outer layer 12 to the thickness of the intermediate layer is in the range of 2:3 to 2:8. If the intermediate layer is too thin compared to the outer layers, the loss factor of the laminated film 10 will not be sufficiently large. On the other hand, if the intermediate layer is too thick compared to the outer layers, the rigidity and heat resistance of the laminated film 10 will be impaired.
[0021] The thickness of the laminated film 10 is preferably 5 to 120 μm, more preferably 10 to 100 μm, and even more preferably 20 to 50 μm.
[0022] The internal loss of the laminated film 10 is determined by dynamic mechanical analysis (DMA) as the loss factor tan δ=M" / M', which is the ratio of the loss modulus M" to the storage modulus M'. Referring to FIG. 2, when the loss factor of the laminated film 10 is measured while increasing the temperature from a low temperature, it peaks at a certain temperature (A in FIG. 2), maintains an almost constant value after passing the peak (B in FIG. 2), and rises sharply as the softening point is approached (C in FIG. 2), becoming unmeasurable. The magnitude of the loss factor in the region B in FIG. 2 correlates with the height of the peak A in FIG. 2.
[0023] The internal loss of the laminated film 10 preferably has a peak loss factor in the range of -10°C to 15°C, and the maximum value is preferably 0.30 or more, more preferably 0.35 or more, thereby achieving a moderately large internal loss in the temperature range in which the speaker is normally used.
[0024] The heat resistance of the laminate film 10 can be evaluated based on the temperature (heat resistance temperature) before the loss factor starts to increase sharply in Fig. 2. The heat resistance temperature of the laminate film 10 is preferably 130°C or higher, and more preferably 160°C or higher.
[0025] The diaphragm laminate film 10 of this embodiment can be manufactured by co-extrusion of the outer layer TPC and the middle layer TPS. Forming a laminate structure by co-extrusion strengthens the adhesion between the layers, improving the integrity of the diaphragm and providing pure sound quality and durability that can withstand long-term use.
[0026] The laminated film 10 for a diaphragm of the present embodiment will be described in more detail with reference to examples and comparative examples.
[0027] The following resins were used in the examples and comparative examples: TPC1: TPC-ET, melting point 208°C, hardness 55D TPC2: TPC-ES, melting point 203°C, hardness 50D TPS1: TPS-SEBS, glass transition point 5°C TPS2: TPS-SEBS, glass transition point 17°C TPS3: TPS-SEBS, glass transition point -14°C TPS4: A blend of TPS1 and TPS2 in a mass ratio of 7:3
[0028] The laminated films of Examples and Comparative Examples 1 to 8 were produced by adding additives as needed to the TPC used in the outer layers and the TPS used in the intermediate layer, kneading and melting them, co-extruding the TPS layer from a multilayer T-die so that the TPC layers sandwiched the TPS layer from both sides, and passing the extrusion through a pair of cooling rolls. The film of Comparative Example 9 was produced by kneading, melting, extruding, and cooling only the TPC to produce a single-layer film.
[0029] The produced laminated film and the monolayer film of Comparative Example 9 were evaluated by a tensile vibration method in accordance with JIS K 7244-4 using a DMA measuring device (TA Instruments, DMA850). Specifically, the film was cut into a 6 mm wide strip, held at a clamp distance of 20 mm, and under a preload (static tensile force) of 0.01 N, a maximum strain of 0.1% was applied at a frequency of 1 Hz, and the loss factor was measured at a temperature increase from -40°C at a rate of 5°C / min up to a maximum temperature of 240°C.
[0030] Table 1 shows the production conditions and evaluation results of the films of Examples and Comparative Examples. The loss coefficients in Table 1 are the maximum values of the peaks, and the peaks were in the range of -10°C to 15°C for all samples. Heat resistance was indicated by ○, △, and × according to the following criteria: ○: Heat resistant temperature is 160°C or higher △: Heat resistant temperature is 130°C or higher but less than 160°C ×: Heat resistant temperature is less than 130°C
[0031] From Table 1, it was confirmed that the laminated films of the examples had a large peak value of the loss factor and excellent heat resistance.
[0032]
[0033] The present invention is not limited to the above-described embodiments and examples, and various modifications are possible within the scope of the technical concept thereof.
[0034] 10: Laminated film for diaphragm 11: First outer layer 12: Second outer layer 13: Intermediate layer
Claims
1. A laminated film for diaphragms, having a three-layer structure in which a first outer layer and a second outer layer are made of an ester-based thermoplastic elastomer and an intermediate layer is made of a styrene-based thermoplastic elastomer, the thickness ratio of the first outer layer to the second outer layer is in the range of 0.5:1.5 to 1.5:0.5, and the ratio of the sum of the thicknesses of the first outer layer and the second outer layer to the thickness of the intermediate layer is in the range of 2:3 to 2:
8.
2. The laminated film for diaphragms according to claim 1, wherein the styrene-based thermoplastic elastomer is a polystyrene-poly(ethylene-butylene)-polystyrene copolymer.
3. The laminated film for diaphragms according to claim 1 or 2, wherein the loss factor peak is in the range of -10°C to 15°C, the maximum value of said peak is 0.30 or more, and the heat resistance temperature is 130°C or more.
4. A method for manufacturing a laminated film for diaphragms, comprising the steps of: kneading and melting an ester-based thermoplastic elastomer; kneading and melting a styrene-based thermoplastic elastomer; and co-extruding the molten ester-based thermoplastic elastomer as two outer layers and the molten styrene-based thermoplastic elastomer as an intermediate layer.
Citation Information
Patent Citations
Heat shrinkable laminated film, molded product using it, heat shrinkable label and container
JP2006159905A
Intermediate film for glass laminate and glass laminate
JP2016108222A
Method for producing a film for a diaphragm of a loudspeaker or a diaphragm of a microphone
JP2016534685A
Acoustic converter diaphragm, and acoustic converter
WO2009118940A1