Lens unit and camera module
The lens unit design with a plastic lens, hard coat layer, antireflection film, and light shielding member addresses durability issues in camera modules by enhancing adhesion and scratch resistance, ensuring improved durability and weather resistance for outdoor use.
Patent Information
- Application Number
- PCT/JP2024/010435
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-31
- Filing Date
- 2024-03-18
- Publication Date
- 2024-10-03
AI Technical Summary
Existing plastic lens units in camera modules face durability issues due to peeling of the antireflection layer and damage to the hard coat layer, especially when exposed to environmental factors, which reduces their optical performance and longevity.
A lens unit design featuring a plastic lens with an inflection portion, a hard coat layer, and an antireflection film, where the hard coat layer is between the plastic lens and the antireflection film, and a light shielding member shields the bending portion of the plastic lens from light, enhancing adhesion and scratch resistance, and a cylindrical housing member houses the lenses to prevent external damage.
The solution significantly improves the durability and weather resistance of the lens unit by preventing peeling of the antireflection film and damage to the hard coat layer, maintaining optical quality even under harsh conditions, making it suitable for long-term use in outdoor environments.
Smart Images

Figure JP2024010435_03102024_PF_FP_ABST
Abstract
Description
Lens units and camera modules
[0001] The present invention relates to a lens unit and a camera module.
[0002] In order to protect a plastic lens substrate that transmits light, it is known to coat the plastic lens substrate with a hard coat layer that is harder than the plastic lens substrate, and to provide an antireflection layer on the surface of the hard coat layer to prevent reflection of light (see, for example, Patent Document 1).
[0003] Patent Document 1 describes the use of a plastic lens as an eyeglass lens, which has an anti-reflection layer on a hard coat layer covering a plastic lens substrate. In the plastic lens of Patent Document 1, the anti-reflection layer is a multilayer film in which low-refractive-index films made of silicon dioxide (SiO2) and high-refractive-index films made of trisilicon tetranitride (Si3N4) are alternately laminated, and the durability of the plastic lens is improved by setting the low-refractive-index films and high-refractive-index films of the anti-reflection layer to specific film thicknesses.
[0004] Japanese Patent Publication No. 2008-76598
[0005] However, even with the plastic lens of Patent Document 1, there is a risk that the anti-reflection layer may peel off or the hard coat layer may be damaged due to the surrounding environment, resulting in a decrease in the durability of the optical element.
[0006] The present invention has been made in view of the above-mentioned problems, and an object of the present invention is to provide a lens unit and a camera module that can improve durability.
[0007] An exemplary lens unit of the present invention includes a plurality of lenses and a cylindrical housing member that houses the plurality of lenses. The plurality of lenses are arranged in order from the opening of the housing member, and the outermost lens of the plurality of lenses that is located on the opening side of the housing member includes a plastic lens having a surface with an inflection portion, an anti-reflection film disposed on the surface side of the plastic lens, and a hard coat layer disposed between the plastic lens and the anti-reflection film. The lens unit further includes a light-shielding member that shields the inflection portion of the plastic lens.
[0008] An exemplary camera module of the present invention includes the lens unit described above and an image sensor.
[0009] Illustratively, the present invention can provide an optical member and a lens unit that can improve durability.
[0010] Fig. 1A is a schematic diagram of a camera module according to this embodiment. Fig. 1B is a partial enlarged view of Fig. 1A. Fig. 2 is a partial enlarged view of Fig. 1A. Fig. 3A is an exploded view of a camera module according to this embodiment. Fig. 3B is a schematic diagram of a manufacturing process of a camera module according to this embodiment. Fig. 3C is a schematic diagram showing a camera module according to this embodiment.
[0011] The lens unit and camera module according to the embodiments of the present invention will be described below with reference to the drawings. Note that the same or corresponding parts in the drawings are designated by the same reference numerals, and descriptions will not be repeated. The dimensions, shapes, and relative sizes of components in the drawings are not necessarily the same as the actual dimensions, shapes, and relative sizes of components. In particular, the thicknesses of the lens unit, anti-reflection coating, hard coat layer, and plastic lens in the drawings may differ significantly from the actual thicknesses of the lens unit, anti-reflection coating, hard coat layer, and plastic lens. Note that in this specification, the "thickness" of each part of the optical element refers to the length parallel to the optical axis direction of the optical element.
[0012] Hereinafter, a camera module 200 according to this embodiment will be described with reference to Figures 1A and 1B. Figure 1A is a schematic diagram showing an example of a camera module 200 according to this embodiment, and Figure 1B is an enlarged partial view of Figure 1A. The camera module 200 captures an image of its surroundings.
[0013] 1A, the camera module 200 includes the lens unit 100 and an image sensor 210. The image sensor 210 receives light that passes through the lens unit 100 and captures an image of the surroundings.
[0014] The lens unit 100 has an optical axis Lx. Light enters the lens unit 100 in a direction along the optical axis Lx.
[0015] The lens unit 100 includes a plurality of lenses 110. At least one of the plurality of lenses 110 is an optical element 10.
[0016] The plurality of lenses 110 include a first lens 110a, a second lens 110b, a third lens 110c, a fourth lens 110d, and a fifth lens 110e, which are arranged in order from the object side to the image side.
[0017] For example, the first lens 110a is the optical element 10. The optical element 10 has a curved surface shape. Typically, the optical element 10 has a spherical surface shape. The optical element 10 has a spherical surface shape centered on a central axis.
[0018] The optical element 10 has an optical axis Lx. The optical axis Lx passes through the center of the curved surface shape of the optical element 10. The optical element 10 has a symmetric structure with respect to the optical axis Lx. Typically, the optical element 10 has a rotationally symmetric structure with respect to the optical axis Lx. Light is incident on the optical element 10 from a direction along the optical axis Lx.
[0019] The optical element 10 includes a plastic lens 11, a hard coat layer 12, and an anti-reflection film 13. The plastic lens 11, the hard coat layer 12, and the anti-reflection film 13 are laminated in this order. Typically, the plastic lens 11, the hard coat layer 12, and the anti-reflection film 13 are disposed in this order in close contact with each other.
[0020] The plastic lens 11 is made of resin and transmits light. Here, the plastic lens 11 has a curved surface.
[0021] The plastic lens 11 has a front surface 11a and a back surface 11b. A hard coat layer 12 and an anti-reflection film 13 are laminated on the front surface 11a of the plastic lens 11.
[0022] The anti-reflection film 13 is disposed on at least one surface of the plastic lens 11. The anti-reflection film 13 covers the hard coat layer 12. The anti-reflection film 13 suppresses reflection of light incident on the anti-reflection film 13. The anti-reflection film 13 suppresses reflection of at least a portion of light traveling in a direction incident on the plastic lens 11 from the surface side of the plastic lens 11.
[0023] The hard coat layer 12 is located between the plastic lens 11 and the anti-reflection film 13. The hard coat layer 12 covers the plastic lens 11. The hard coat layer 12 has a higher hardness than the plastic lens 11. The hard coat layer 12 imparts scratch resistance to the plastic lens 11 and improves adhesion between the plastic lens 11 and the anti-reflection film 13.
[0024] In the lens unit 100 of this embodiment, an inflection portion 11c is provided in the plastic lens 11. Specifically, the inflection portion 11c is located at the interface between the plastic lens 11 and the hard coat layer 12. In the plastic lens 11, the slope and radius of curvature of the inflection portion 11c are different from the slope and radius of curvature of the surrounding area of the inflection portion 11c.
[0025] In the lens unit 100 of this embodiment, an inflection portion 12c is provided in the hard coat layer 12. Typically, the inflection portion 12c extends in an annular shape. More specifically, the inflection portion 12c is located at the interface between the hard coat layer 12 and the plastic lens 11. In the hard coat layer 12, the slope and radius of curvature of the inflection portion 12c are different from the slope and radius of curvature of the surrounding area of the inflection portion 12c.
[0026] The inflection portion 11c of the plastic lens 11 engages with the inflection portion 12c of the hard coat layer 12. The inflection portion 11c of the plastic lens 11 and the inflection portion 12c of the hard coat layer 12 are located on the periphery of the plastic lens 11 and the hard coat layer 12, respectively.
[0027] Here, the inflection portion 11c in the plastic lens 11 is a concave portion recessed from the surrounding area, and the inflection portion 12c in the hard coat layer 12 is a convex portion protruding from the surrounding area. However, the inflection portion 11c in the plastic lens 11 may be a convex portion, and the inflection portion 12c in the hard coat layer 12 may be a concave portion.
[0028] The lens unit 100 further includes a housing member 120, a filter 130, a sealing member 140, and a light blocking member 150. The housing member 120 is tubular. Typically, the housing member 120 is cylindrical. Note that the inner circumferential surface of the housing member 120 may be provided with irregularities.
[0029] The housing member 120 houses the lenses 110 and the filters 130. The housing member 120 is made of a material that does not transmit light. For example, the housing member 120 is made of a material that does not transmit visible light and ultraviolet light.
[0030] The first lens 110a, the second lens 110b, the third lens 110c, the fourth lens 110d, and the fifth lens 110e are installed in the housing member 120. At least a portion of at least one of the first lens 110a, the second lens 110b, the third lens 110c, the fourth lens 110d, and the fifth lens 110e may be arranged so as to be exposed from the housing member 120. For example, the first lens 110a is arranged so as to be exposed from the housing member 120, and the other lenses, the second lens 110b, the third lens 110c, the fourth lens 110d, and the fifth lens 110e, are arranged within the housing member 120. The first lens 110a is the outermost lens of the multiple lenses 110 located on the opening side of the housing member 120.
[0031] Here, the diameter of the first lens 110a is larger than the diameters of the second lens 110b, the third lens 110c, the fourth lens 110d, and the fifth lens 110e, and the diameter of the fifth lens 110e is larger than the diameters of the second lens 110b, the third lens 110c, and the fourth lens 110d.
[0032] The filter 130 is disk-shaped. The filter 130 selectively transmits incident light. For example, the filter 130 selectively transmits light of a specific wavelength from the incident light. Here, the filter 130 is disposed in the housing member 120. For example, the image sensor 210 is disposed outside the lens unit 100.
[0033] The filter 130 is disposed on the image side relative to the fifth lens 110e. The filter 130 can select the wavelength of light that reaches the image sensor 210. The image sensor 210 is a photoelectric conversion element that converts irradiated light into an electrical signal. The image sensor 210 is, for example, a CMOS image sensor or a CCD image sensor. However, the image sensor 210 is not limited to these. The image sensor 210 captures an image of a subject formed by the multiple lenses 110. Note that the image sensor 210 may be disposed on the image side relative to the filter 130 (lens unit 100).
[0034] The first lens 110a is a negative meniscus lens with a convex surface facing the object side. In this embodiment, the convex surface of the first lens 110a facing the object side is spherical, and the concave surface facing the image side is aspherical.
[0035] The second lens 110b, the third lens 110c, the fourth lens 110d, and the fifth lens 110e may be made of resin (plastic lenses) or glass.
[0036] The second lens 110b, the third lens 110c, the fourth lens 110d, and the fifth lens 110e may be any of a biconvex lens, a plano-convex lens, a convex meniscus lens, and a concave meniscus lens.
[0037] As described above, the lens unit 100 includes a plurality of lenses 110, and at least one of the plurality of lenses 110 is the optical element 10, so that deterioration of the lenses 110 in the lens unit 100 can be suppressed.
[0038] Furthermore, the first lens 110a, which is equipped with the above-mentioned plastic lens 11, hard coat layer 12, and anti-reflection film 13, is positioned exposed from the housing member 120, and the remaining lenses (the second lens 110b, the third lens 110c, the fourth lens 110d, and the fifth lens 110e) are positioned within the housing member 120, thereby suppressing deterioration of lenses other than the highly durable first lens 110a.
[0039] The sealing member 140 deforms between the first lens 110a and the housing member 120 to seal the gap between the first lens 110a and the housing member 120. For example, the sealing member 140 is an annular elastic body. In one example, the sealing member 140 is an O-ring.
[0040] The lens unit 100 is suitable for use as an in-vehicle lens for capturing images of the surroundings of a vehicle. For example, the lens unit 100 is used as an in-vehicle lens for capturing images of the rear or side of a vehicle.
[0041] Since the lens unit 100 includes the sealing member 140, even if water is splashed onto the lens unit 100 from the outside, the water can be prevented from entering the inside of the lens unit 100 (i.e., the inside of the housing member 120).
[0042] The first lens 110a includes the plastic lens 11, the hard coat layer 12, and the anti-reflection film 13, and therefore can effectively suppress ultraviolet rays from entering the housing member 120. As a result, deterioration of the lens in the housing member 120 can be suppressed.
[0043] The light-shielding member 150 shields the first lens 110a from light. Specifically, the light-shielding member 150 shields the inflection portion 11c of the plastic lens 11 and the inflection portion 12c of the hard coat layer 12 in the first lens 110a from light.
[0044] The light-shielding member 150 covers the periphery of the first lens 110a in an annular shape. This blocks light incident on the inflection portion 11c of the plastic lens 11 and the inflection portion 12c of the hard coat layer 12 in the first lens 110a. The light-shielding member 150 extends in a direction perpendicular to the optical axis Lx with respect to the housing member 120. The light-shielding member 150 extends along the periphery of the first lens 110a. The light-shielding member 150 prevents the first lens 110a from detaching from the housing member 120. The light-shielding member 150 may be a single member together with the housing member 120.
[0045] In this embodiment, the lens unit 100 includes the light blocking member 150 , and therefore, the first lens 110 a can be prevented from being detached from the housing member 120 .
[0046] 1B , the plastic lens 11 has a front surface 11a and a back surface 11b. The front surface 11a is located on the object side, and the back surface 11b is located on the image side. The front surface 11a of the plastic lens 11 is provided with an inflection portion 11c. The inflection portion 11c of the plastic lens 11 engages with an inflection portion 12c of the hard coat layer 12. When the plastic lens 11 is provided with the inflection portion 11c, the thickness of the hard coat layer 12 may be relatively small at and near the inflection portion 12c.
[0047] The light-shielding member 150 covers the inflection portion 11c of the plastic lens 11 and the inflection portion 12c of the hard coat layer 12 of the first lens 110a. The light-shielding member 150 covers the periphery of the first lens 110a. The inflection portion 11c of the plastic lens 11 and the inflection portion 12c of the hard coat layer 12 are located at lengths from the outer edges of the plastic lens 11 and the hard coat layer 12 that are 0.5% to 10% of the diameter of the plastic lens 11 and the hard coat layer 12, respectively. The light-shielding member 150 covers the periphery of the first lens 110a over a length that is 0.5% to 10% of the diameter of the first lens 110a. Therefore, the effective diameter Ed of the first lens 110a is smaller than the diameter Ld of the first lens 110a.
[0048] For example, the diameter Ld of the first lens 110a is 1 mm or more and 100 mm or less, and may be 2 mm or more and 50 mm or less. The length Sd of the light blocking member 150 along the direction perpendicular to the optical axis Lx is 0.005 mm or more and 10 mm or less, and may be 0.01 mm or more and 5 mm or less.
[0049] In one example, the diameter Ld of the first lens 110a is 13.70 mm or more and 13.75 mm or less. In one example, the light blocking member 150 covers the periphery of the first lens 110a over a length of 0.1 mm or more and 1.0 mm or less from the outer edge of the first lens 110a. Therefore, the length Sd of the light blocking member 150 along a direction perpendicular to the optical axis Lx is 0.1 mm or more and 1.0 mm or less. Therefore, the effective diameter Ed of the first lens 110a is 11.70 mm or more and 13.55 mm or less.
[0050] As described above, the lens unit 100 includes a plurality of lenses 110 and a cylindrical housing member 120 that houses the plurality of lenses 110. The plurality of lenses 110 are arranged in order from the opening of the housing member 120. The outermost lens of the plurality of lenses 110, which is located on the opening side of the housing member 120, includes a plastic lens 11 having a surface on which an inflection portion 11c is provided, an anti-reflection coating 13 arranged on the surface side of the plastic lens 11, and a hard coat layer 12 located between the plastic lens 11 and the anti-reflection coating 13. The lens unit 100 further includes a light-shielding member 150 that shields the inflection portion 11c of the plastic lens 11 from light.
[0051] The light-shielding member 150 shields the inflection portion 11c of the plastic lens 11, where the thickness of the hard coat layer 12 is likely to become thin, thereby preventing a decrease in adhesion at the interface between the anti-reflection film 13 and the hard coat layer 12 and preventing deterioration of the hard coat layer 12. This improves the weather resistance of the lens unit 100.
[0052] The plastic lens 11 is recessed at the inflection portion 11c. By providing the recessed inflection portion 11c on the surface of the plastic lens 11, the plastic lens 11 can be easily released from the mold.
[0053] The light blocking member 150 is a single member together with the housing member 120. This can prevent an increase in the number of parts required for the light blocking member 150 that blocks light from reaching the inflection portion 11c of the plastic lens 11.
[0054] The camera module 200 includes the lens unit 100 and the image sensor 210. This improves the weather resistance of the camera module 200.
[0055] The lens unit 100 according to this embodiment will be described below with reference to Fig. 2. Fig. 2 is an enlarged view of a portion of Fig. 1A.
[0056] 2, the optical element 10 includes a plastic lens 11, a hard coat layer 12, and an anti-reflection film 13. The plastic lens 11, the hard coat layer 12, and the anti-reflection film 13 are laminated in this order. Typically, the plastic lens 11, the hard coat layer 12, and the anti-reflection film 13 are disposed in this order in close contact with each other.
[0057] [Plastic Lens 11] The plastic lens 11 transmits light. For example, the plastic lens 11 is transparent. Alternatively, the plastic lens 11 may be translucent or translucent.
[0058] Typically, the plastic lens 11 is made of resin. The plastic lens 11 may be composed of a single member. For example, the plastic lens 11 includes a resin having a cyclic imide structure as a ring structure. Examples of such resins include AZP manufactured by Asahi Kasei Corporation, and RM-104, RM-250, and RM-100-Z manufactured by Nippon Shokubai Co., Ltd.
[0059] The plastic lens 11 has a curved shape. Typically, the plastic lens 11 has a spherical shape. At least one surface of the plastic lens 11 may be a convex or concave surface. When the plastic lens 11 has a convex or concave surface, the plastic lens 11 functions as a lens (specifically, for example, a biconvex lens, a plano-convex lens, a convex meniscus lens, or a concave meniscus lens).
[0060] The plastic lens 11 may have a convex surface. For example, the radius of curvature of the plastic lens 11 is equal to or greater than 9 mm and equal to or less than 16 mm.
[0061] The thermal expansion coefficient of the plastic lens 11 is preferably 60 ppm / K or more and 150 ppm / K or less, so that the influence of thermal stress between the plastic lens 11 and the anti-reflection film 13 can be suppressed.
[0062] [Hard Coat Layer 12] The hard coat layer 12 coats the plastic lens 11. For example, the hard coat layer 12 coats one surface (e.g., the air side) of the plastic lens 11 that is located on the object side in the direction in which the optical axis Lx extends. The hard coat layer 12 has a higher hardness than the plastic lens 11. The hard coat layer 12 imparts scratch resistance to the plastic lens 11 and improves adhesion between the plastic lens 11 and the antireflection coating 13.
[0063] The hard coat layer 12 transmits light. For example, the hard coat layer 12 is transparent. Alternatively, the hard coat layer 12 may be semi-transparent or translucent.
[0064] The hard coat layer 12 may have a base layer. Typically, the base layer includes an organic material layer or an organosilicon compound layer. In the hard coat layer 12, metal oxide fine particles may be dispersed in the base layer.
[0065] The elastic modulus of the hard coat layer 12 is preferably 5 GPa or more and 12 GPa or less. When the elastic modulus of the hard coat layer 12 is 5 GPa or more, damage to the plastic lens 11 can be suppressed. Furthermore, when the elastic modulus of the hard coat layer 12 is 12 GPa or less, cracks caused by temperature changes can be suppressed in the hard coat layer 12.
[0066] Typically, the hard coat layer 12 can be formed by drying the component liquids attached to the surface of the plastic lens 11, and then curing the film of the component liquids with electromagnetic waves such as ultraviolet rays or electron beams. The component liquids may be heated when drying them.
[0067] In one example, the hard coat layer 12 may be formed by a spin coating method, in which component liquids of the hard coat layer 12 are ejected onto the plastic lens 11 rotating at a predetermined rotation speed, and the component liquids of the hard coat layer 12 are cured by applying electromagnetic waves such as ultraviolet rays or electron beams to the component liquids.
[0068] Alternatively, the hard coat layer 12 may be formed by a dipping method. In this case, the plastic lens 11 is immersed in a component liquid of the hard coat layer 12, and then the component liquid of the hard coat layer 12 is applied to the plastic lens 11 rotating at a predetermined rotation speed by electromagnetic waves such as ultraviolet rays or an electron beam to harden the component liquid.
[0069] When the hard coat layer 12 is formed on the surface of the plastic lens 11 while the plastic lens 11 is rotated, the thickness of the hard coat layer 12 varies depending on the distance from the optical axis Lx. Typically, the thickness of the hard coat layer 12 decreases as the distance from the optical axis Lx increases.
[0070] [Anti-reflection film 13] The anti-reflection film 13 covers the hard coat layer 12. For example, the anti-reflection film 13 covers the air side of the hard coat layer 12. The anti-reflection film 13 suppresses reflection of light incident on the anti-reflection film 13. The anti-reflection film 13 suppresses reflection of at least a portion of light traveling in a direction incident on the plastic lens 11 from the surface side of the plastic lens 11. For example, the anti-reflection film 13 suppresses reflection of visible light traveling in a direction incident on the plastic lens 11 from the surface side of the plastic lens 11.
[0071] The anti-reflection film 13 transmits light. For example, the anti-reflection film 13 is transparent. Alternatively, the anti-reflection film 13 may be semi-transparent or translucent.
[0072] The thickness of the antireflection film 13 is 100 nm or more and 1000 nm or less. The thickness of the antireflection film 13 may be 200 nm or more and 900 nm or less, or may be 300 nm or more and 800 nm or less.
[0073] The thermal expansion coefficient of the anti-reflection coating 13 is preferably 1 ppm / K or more and 10 ppm / K or less, so that the influence of thermal stress between the plastic lens 11 and the anti-reflection coating 13 can be suppressed.
[0074] The anti-reflection film 13 may have a laminated film structure. For example, in the anti-reflection film 13, layers with different compositions are laminated.
[0075] For example, the anti-reflection film 13 is made of an inorganic oxide. Examples of the inorganic oxide in the anti-reflection film 13 include metal oxides such as silicon oxide, titanium oxide, lanthanum titanate, tantalum oxide, and niobium oxide. For example, the anti-reflection film 13 has layers of multiple types of metal oxides stacked thereon.
[0076] For example, the anti-reflection film 13 has a high refractive index film and a low refractive index film, and is configured so that the high refractive index film and the low refractive index film are alternately stacked.
[0077] The refractive index of the high refractive index film is higher than the refractive index of the low refractive index film, and typically, in the visible range, the refractive index of the high refractive index film is higher than the refractive index of the low refractive index film.
[0078] The high-refractive-index film contains trisilicon tetranitride (Si3N4). The low-refractive-index film contains silicon dioxide (SiO2). In this way, the high-refractive-index film contains trisilicon tetranitride (Si3N4) and the low-refractive-index film contains silicon dioxide (SiO2), thereby improving thermal shock resistance.
[0079] For example, the high refractive index film is 1.9 or more. In one example, the high refractive index film is 1.9 or more and 2.3 or less.
[0080] For example, the refractive index of the low refractive index film is 1.5 or more and 1.8 or less. In one example, the refractive index of the low refractive index film is 1.6 or more and 1.75 or less.
[0081] The thickness of the high-refractive-index film and the low-refractive-index film is 5 nm or more and 200 nm or less. This allows the high-refractive-index film and the low-refractive-index film to be formed uniformly, and allows a plurality of high-refractive-index films and low-refractive-index films to be arranged in the anti-reflection film 13. The thickness of the high-refractive-index film and the low-refractive-index film may be 10 nm or more and 180 nm or less, or may be 20 nm or more and 170 nm or less.
[0082] The anti-reflection film 13 preferably transmits light in the visible range while reflecting light in the ultraviolet range. The average reflectance of the anti-reflection film 13 for visible light wavelengths is preferably lower than the average reflectance for ultraviolet light wavelengths.
[0083] From the viewpoint of further suppressing the influence of thermal stress between the plastic lens 11 and the anti-reflection coating 13, it is preferable that the difference between the thermal expansion coefficient of the plastic lens 11 and the thermal expansion coefficient of the anti-reflection coating 13 is relatively small. For example, it is preferable that the thermal expansion coefficient of the plastic lens 11 is 60 ppm / K or more and 100 ppm / K or less, and the thermal expansion coefficient of the anti-reflection coating 13 is 5 ppm / K or more and 10 ppm / K or less.
[0084] As shown in FIG. 2 , the plastic lens 11 has a curved surface. An inflection portion 11c is provided on the surface 11a of the plastic lens 11. For example, the width Wc of the inflection portion 11c (the length along a direction perpendicular to the optical axis Lx) is greater than the step Dc (the length along a direction parallel to the optical axis Lx). In one example, the step Dc of the inflection portion 11c is 0.05 mm or more and 1 mm or less, or 0.1 mm or more and 0.5 mm or less. Furthermore, the width Wc of the inflection portion 11c is 0.01 mm or more and 1 mm or less, or 0.1 mm or more and 0.5 mm or less.
[0085] Here, one surface (surface 11a) of the plastic lens 11 has a curved surface. The thickness of the plastic lens 11 varies depending on the distance from the optical axis Lx.
[0086] The thickness of the hard coat layer 12 varies depending on the distance from the optical axis Lx. Typically, the thickness of the hard coat layer 12 is greatest at the center of the optical axis Lx. Also, typically, the thickness of the hard coat layer 12 is smallest at the outer edge.
[0087] Typically, the thickness Lx2 of the outer edge of the hard coat layer 12 is smaller than the thickness Lx1 of the hard coat layer 12 on the optical axis Lx.
[0088] If the thickness of the hard coat layer is small, when the optical element is exposed to an outdoor environment and the adhesion at the interface between the hard coat layer and the antireflection coating decreases, the antireflection coating may peel off from the hard coat layer or the hard coat layer may be damaged, resulting in a decrease in the durability of the lens unit. For this reason, within the range of the effective diameter Ed of the plastic lens 11, the minimum thickness of the hard coat layer 12 is preferably 2 μm or more.
[0089] For example, the thickness Lx1e of the portion of the hard coat layer 12 that is not covered with the light-shielding member 150 is 2 μm or more, and the portion of the hard coat layer 12 whose thickness (Lx2s) is less than 2 μm is covered with the light-shielding member 150. This makes it possible to prevent the durability of the optical element 10 from decreasing.
[0090] If the thickness of the hard coat layer along the optical axis Lx is large, optical distortion may occur in the optical element, and the optical characteristics of the lens unit may deteriorate. Furthermore, if the thickness of the hard coat layer along the optical axis Lx becomes even larger, the film state of the hard coat layer may become non-uniform, and cracks may occur in the hard coat layer. Therefore, within the range of the effective diameter Ed of the plastic lens 11, the maximum thickness of the hard coat layer 12 is preferably 20 μm or less. Typically, the thickness Lx1 of the hard coat layer along the optical axis Lx is the maximum thickness of the hard coat layer 12. This makes it possible to suppress deterioration in the optical characteristics of the lens unit 100.
[0091] The lens unit 100 of this embodiment has relatively little optical distortion and exhibits relatively high durability. Therefore, the optical element 10 is suitable for use in a surveillance camera or an in-vehicle camera. The optical element 10 can be used continuously even when the surveillance camera or the in-vehicle camera is used outdoors for a long period of time.
[0092] The lens unit 100 has an optical axis Lx. The thickness of the hard coat layer 12 along the optical axis Lx is 2 μm or more and 20 μm or less. When the thickness of the hard coat layer 12 along the optical axis Lx is 2 μm or more, peeling of the antireflection film 13 along the optical axis Lx, where a high amount of light passes through, can be suppressed. Furthermore, when the thickness of the hard coat layer 12 along the optical axis Lx is 20 μm or less, optical distortion can be suppressed and cracks can be suppressed from occurring in the hard coat layer 12. This makes it possible to provide a lens unit 100 that has excellent weather resistance and is suppressed from deteriorating in optical properties.
[0093] For example, the elastic modulus of the hard coat layer 12 is 5 GPa or more and 12 GPa or less. When the elastic modulus of the hard coat layer 12 is 5 GPa or more, it is possible to prevent scratches on the plastic lens 11. Furthermore, when the elastic modulus of the hard coat layer 12 is 12 GPa or less, it is possible to prevent cracks from occurring in the hard coat layer 12 due to temperature changes.
[0094] For example, the thermal expansion coefficient of the plastic lens 11 is 60 ppm / K or more and 150 ppm / K or less. When the thermal expansion coefficient of the plastic lens 11 is 60 ppm / K or more and 150 ppm / K or less, the influence of thermal stress between the plastic lens 11 and the anti-reflection coating 13 can be reduced.
[0095] For example, the thermal expansion coefficient of the anti-reflection coating 13 is 1 ppm / K or more and 10 ppm / K or less. When the thermal expansion coefficient of the anti-reflection coating 13 is 1 ppm / K or more and 10 ppm / K or less, the influence of thermal stress between the plastic lens 11 and the anti-reflection coating 13 can be reduced.
[0096] For example, the thermal expansion coefficient of the plastic lens 11 is 60 ppm / K or more and 100 ppm / K or less, and the thermal expansion coefficient of the anti-reflection coating 13 is 5 ppm / K or more and 10 ppm / K or less. This makes it possible to further reduce the influence of thermal stress between the plastic lens 11 and the anti-reflection coating 13.
[0097] 1A to 2, the hard coat layer 12 and the anti-reflection film 13 are disposed on one surface of the plastic lens 11, but this embodiment is not limited to this. The hard coat layer 12 and the anti-reflection film 13 may be disposed on both surfaces of the plastic lens 11.
[0098] Next, a camera module 200 according to this embodiment will be described with reference to Figures 1 to 3C. Figure 3A is an exploded view of the camera module 200 according to this embodiment. Figure 3B is a schematic diagram of the manufacturing process of the camera module 200 according to this embodiment. Figure 3C is a schematic diagram showing the camera module 200 according to this embodiment.
[0099] 3A, the housing member 120 can house a plurality of lenses 110. At least one of the plurality of lenses 110 is the optical element 10.
[0100] The accommodation member 120 has a cylindrical shape. Typically, the accommodation member 120 has a cylindrical shape.
[0101] The plurality of lenses 110 include a first lens 110a, a second lens 110b, a third lens 110c, a fourth lens 110d, and a fifth lens 110e. The housing member 120 has housing portions capable of housing the first lens 110a, the second lens 110b, the third lens 110c, the fourth lens 110d, and the fifth lens 110e, respectively.
[0102] Note that here, a protrusion 150a is provided on the outer edge on one side of the housing member 120. Typically, the protrusion 150a is formed from the same material as the housing member 120. The protrusion 150a is a single member together with the housing member 120. The protrusion 150a extends from the housing member 120 parallel to the optical axis Lx.
[0103] 3B , the housing member 120 houses the plurality of lenses 110, the filter 130, and the sealing member 140. Here, the first lens 110a, the second lens 110b, the third lens 110c, and the sealing member 140 are inserted from one side to the other side of the housing member 120. The fourth lens 110d, the fifth lens 110e, and the filter 130 are inserted from the other side to the one side of the housing member 120. The filter 130 is located between the plurality of lenses 110 and the image sensor 210.
[0104] As shown in FIG. 3C , the light-blocking member 150 is formed by bending the protrusion 150a relative to the housing member 120 in a direction perpendicular to the optical axis Lx. The protrusion 150a is pressed in a heated state, causing it to bend relative to the housing member 120 in a direction perpendicular to the optical axis Lx. The light-blocking member 150 blocks the first lens 110a, which is the outermost lens. The light-blocking member 150 prevents light incident on the lens unit 100 from entering the outer edge of the first lens 110a. The light-blocking member 150 also prevents the first lens 110a from detaching from the housing member 120.
[0105] First, the lens unit 100 of the first embodiment will be described.
[0106] A plastic lens 11 was prepared using RM-104 manufactured by Nippon Shokubai Co., Ltd. The plastic lens 11 was a meniscus lens with the convex surface facing the object side, and the outer diameter of the plastic lens 11 was approximately 14 mm. The plastic lens 11 was provided with an inflection portion 11c recessed from the spherical surface of the surface 11a. The step Dc of the inflection portion 11c was 0.2 mm, and the width Wc of the inflection portion 11c was 0.4 mm.
[0107] The surface of the plastic lens 11 was coated with a hard coat layer 12. The hard coat layer 12 was made of a photocurable resin material such as urethane. The hard coat layer 12 was formed by applying a coating liquid to the plastic lens 11 by spin coating, heating and drying the coating film made of the coating liquid, and then photocuring the coating film with electromagnetic waves such as ultraviolet rays or an electron beam. The hard coat layer 12 had an inflection portion 12c protruding from the spherical surface.
[0108] An antireflection film 13 was coated on the surface of the hard coat layer 12. The antireflection film 13 was formed by alternately forming high-refractive index films made of SiN and low-refractive index films made of SiO by sputtering. In this manner, the optical element 10 was fabricated. In the optical element 10, the thickness of the hard coat layer 12 on the optical axis Lx was 2.3 μm, and the thickness of the outer edge of the hard coat layer 12 was 0.5 μm.
[0109] Furthermore, a housing member 120 was prepared, which was provided with a protrusion 150a extending along the optical axis Lx. Thereafter, the optical element 10 was housed in the housing member 120, and the protrusion 150a extending parallel to the optical axis Lx relative to the housing member 120 was bent in a direction perpendicular to the optical axis Lx, thereby forming the light blocking member 150. In this manner, the lens unit 100 of Example 1 was produced.
[0110] Next, the lens unit 100 of Example 1 was subjected to an optical property test and a weather resistance test under the following conditions.
[0111] [Optical Property Test] The lens unit of Example 1 was visually inspected for light distortion using a fluorescent light source.
[0112] [Weathering Test] A weathering test was carried out using a highly accelerated weathering tester, a 7.5 kW super xenon weather meter. In the weathering test, the irradiance was 180 W / m 2 One cycle consisted of 18 minutes of irradiation and rainfall followed by 102 minutes of irradiation alone, and this cycle was repeated 500 times. During and after the weather resistance test, it was checked whether the anti-reflection film 13 had peeled off and whether the hard coat layer 12 had been damaged.
[0113] Table 1 shows the results of the optical property test and weather resistance test of the lens unit 100, along with the thickness at the optical axis and the thickness at the outer edge of the hard coat layer 12 in the lens unit 100 of Example 1. In this specification, a case in which there is no light distortion in a visual inspection under a fluorescent lamp is indicated by "O", and a case in which there is light distortion is indicated by "X". Also in this specification, a case in which there is no peeling of the anti-reflection film or damage to the hard coat layer in a visual inspection under a fluorescent lamp is indicated by "O", and a case in which there is either peeling of the anti-reflection film or damage to the hard coat layer is indicated by "X".
[0114]
[0115] As shown in Table 1, in the lens unit 100 of Example 1, the thickness of the hard coat layer 12 at the optical axis Lx was 2.3 μm, and the inflection portion 11 c of the plastic lens 11 was shielded by the light-shielding member 150. In the lens unit 100 of Example 1, no distortion occurred in the light transmitted through the lens unit 100. Furthermore, even after the weather resistance test, no peeling of the antireflection film 13 or damage to the hard coat layer 12 occurred.
[0116] Lens units of Examples 2 to 4 and Comparative Examples 1 to 4 were fabricated in the same manner as lens unit 100 of Example 1. Optical property tests and weather resistance tests were also carried out on the lens units of Examples 2 to 4 and Comparative Examples 1 to 4 in the same manner as lens unit 100 of Example 1. Table 1 shows the thickness of the hard coat layer on the optical axis, the presence or absence of an inflection portion, the presence or absence of a light-shielding member, and the results of the optical property tests and weather resistance tests for the lens units of Examples 1 to 4 and Comparative Examples 1 to 4.
[0117] In the lens unit 100 of Example 2, the thickness of the hard coat layer 12 at the optical axis was 4.8 μm. The plastic lens 11 and the hard coat layer 12 were provided with inflection portions 11c and 12c, respectively, and the inflection portion 11c of the plastic lens 11 was shielded by a light-shielding member 150. In the lens unit 100 of Example 2, no distortion occurred in the light transmitted through the lens unit 100. Furthermore, even after a weather resistance test, no peeling of the antireflection film 13 or damage to the hard coat layer 12 occurred.
[0118] In the lens unit 100 of Example 3, the thickness of the hard coat layer 12 at the optical axis was 5.4 μm. The plastic lens 11 and the hard coat layer 12 were provided with inflection portions 11c and 12c, respectively, and the inflection portion 11c of the plastic lens 11 was shielded by a light-shielding member 150. In the lens unit 100 of Example 3, no distortion occurred in the light transmitted through the lens unit 100. Furthermore, even after a weather resistance test, no peeling of the antireflection film 13 or damage to the hard coat layer 12 occurred.
[0119] In the lens unit 100 of Example 4, the thickness of the hard coat layer 12 at the optical axis was 15.8 μm. The plastic lens 11 and the hard coat layer 12 were provided with inflection portions 11c and 12c, respectively, and the inflection portion 11c of the plastic lens 11 was shielded by a light-shielding member 150. In the lens unit 100 of Example 4, no distortion occurred in the light transmitted through the lens unit 100. Furthermore, even after a weather resistance test, no peeling of the antireflection film 13 or damage to the hard coat layer 12 occurred.
[0120] In the lens unit of Comparative Example 1, the thickness of the hard coat layer at the optical axis was 2.3 μm. The plastic lens and the hard coat layer each had an inflection portion, and the inflection portion of the plastic lens was not shielded from light. No distortion occurred in the light transmitted through the lens unit of Comparative Example 1. However, after the weather resistance test, either peeling of the anti-reflection film or damage to the hard coat layer occurred.
[0121] In the lens unit of Comparative Example 2, the thickness of the hard coat layer at the optical axis was 4.8 μm. The plastic lens and the hard coat layer each had an inflection portion, and the inflection portion of the plastic lens was not shielded. No distortion occurred in the light transmitted through the lens unit of Comparative Example 2. However, after the weather resistance test, either peeling of the anti-reflection film or damage to the hard coat layer occurred.
[0122] In the lens unit of Comparative Example 3, the thickness of the hard coat layer at the optical axis was 23.5 μm. The plastic lens and the hard coat layer each had an inflection portion, and the inflection portion of the plastic lens was not shielded from light. Distortion occurred in the light transmitted through the lens unit of Comparative Example 3. Furthermore, after the weather resistance test, either peeling of the anti-reflection film or damage to the hard coat layer occurred.
[0123] In the lens unit of Comparative Example 4, the thickness of the hard coat layer at the optical axis was 33.9 μm. The plastic lens and the hard coat layer each had an inflection portion, and the inflection portion of the plastic lens was not shielded from light. Distortion occurred in the light transmitted through the lens unit of Comparative Example 4. Furthermore, after the weather resistance test, either peeling of the anti-reflection film or damage to the hard coat layer occurred.
[0124] Furthermore, lens units of Reference Examples 1 to 4 were produced in the same manner as the lens units of Comparative Examples 1 to 4. In the lens units of Reference Examples 1 to 4, no inflection portion was provided in the plastic lens and the hard coat layer. The lens units of Reference Examples 1 to 4 were also subjected to optical property tests and weather resistance tests in the same manner as lens unit 100 of Example 1. Table 2 shows the thickness of the hard coat layer at the optical axis and the thickness of the outer edge, the presence or absence of an inflection portion, the presence or absence of a light-shielding member, and the results of the optical property tests and weather resistance tests for the lens units of Reference Examples 1 to 4.
[0125]
[0126] In the lens unit of Reference Example 1, the thickness of the hard coat layer at the optical axis and the thickness of the outer edge were 2.3 μm and 0.5 μm, respectively. Neither the plastic lens nor the hard coat layer had an inflection portion, so the lens unit was not light-shielded. No distortion occurred in the light transmitted through the lens unit of Reference Example 1. However, after the weather resistance test, either peeling of the anti-reflection film or damage to the hard coat layer occurred.
[0127] In the lens unit of Reference Example 2, the thickness of the hard coat layer at the optical axis and the thickness of the outer edge were 4.8 μm and 1.4 μm, respectively. Neither the plastic lens nor the hard coat layer had an inflection portion, so the lens unit was not light-shielded. No distortion occurred in the light transmitted through the lens unit of Reference Example 2. However, after the weather resistance test, either peeling of the anti-reflection film or damage to the hard coat layer occurred.
[0128] In the lens unit of Reference Example 3, the thickness of the hard coat layer at the optical axis and the thickness of the outer edge were 23.5 μm and 8.3 μm, respectively. The plastic lens and the hard coat layer did not have an inflection portion, and the lens unit was not light-shielded. Distortion occurred in the light transmitted through the lens unit of Reference Example 3. On the other hand, even after the weather resistance test, peeling of the anti-reflection film and damage to the hard coat layer did not occur.
[0129] In the lens unit of Reference Example 4, the thickness of the hard coat layer at the optical axis and the thickness of the outer edge were 33.9 μm and 10.2 μm, respectively. Neither the plastic lens nor the hard coat layer had an inflection portion, so the lens unit was not light-shielded. Distortion occurred in the light transmitted through the lens unit of Reference Example 4. Furthermore, after the weather resistance test, either peeling of the anti-reflection film or damage to the hard coat layer occurred.
[0130] In the lens units 100 of Examples 1 to 4, there was no optical distortion, and no peeling of the antireflection film 13 or damage to the hard coat layer 12 occurred. In contrast, there was no optical distortion in the lens units of Comparative Examples 1 and 2, but either peeling of the antireflection film or damage to the hard coat layer occurred. In the lens units of Comparative Examples 3 and 4, there was optical distortion, and either peeling of the antireflection film or damage to the hard coat layer occurred.
[0131] Furthermore, in the lens units 100 of Reference Examples 1 and 2, no optical distortion occurred, but either peeling of the antireflection film or damage to the hard coat layer occurred. In contrast, in the lens unit of Reference Example 3, neither peeling of the antireflection film nor damage to the hard coat layer occurred, but optical distortion occurred. In the lens unit of Reference Example 4, optical distortion occurred, and either peeling of the antireflection film or damage to the hard coat layer occurred.
[0132] The present technology may have the following configurations: (1) A lens unit including a plurality of lenses and a cylindrical housing member that houses the plurality of lenses, wherein the plurality of lenses are arranged in order from an opening of the housing member, and an outermost lens of the plurality of lenses that is located on the opening side of the housing member includes: a plastic lens having a surface provided with an inflection portion; an anti-reflection film that is arranged on the surface side of the plastic lens; and a hard coat layer that is located between the plastic lens and the anti-reflection film, and the lens unit further includes a light-shielding member that shields the inflection portion of the plastic lens.
[0133] (2) The lens unit according to (1), wherein the plastic lens is recessed at the inflection portion.
[0134] (3) The lens unit according to (1) or (2), wherein the lens unit has an optical axis, and the thickness of the hard coat layer on the optical axis is 2 μm or more and 20 μm or less.
[0135] (4) The lens unit according to any one of (1) to (3), wherein the hard coat layer has an elastic modulus of 5 GPa or more and 12 GPa or less.
[0136] (5) The lens unit according to any one of (1) to (4), wherein the thermal expansion coefficient of the plastic lens is 60 ppm / K or more and 150 ppm / K or less.
[0137] (6) The lens unit according to any one of (1) to (5), wherein the antireflection film has a thermal expansion coefficient of 1 ppm / K or more and 10 ppm / K or less.
[0138] (7) The lens unit according to any one of (1) to (6), wherein the thermal expansion coefficient of the plastic lens is 60 ppm / K or more and 100 ppm / K or less, and the thermal expansion coefficient of the anti-reflection film is 5 ppm / K or more and 10 ppm / K or less.
[0139] (8) The lens unit according to (3), wherein the difference between the thickness of the hard coat layer on the optical axis and the thickness of the outer edge is 15 μm or less.
[0140] (9) The lens unit according to any one of (1) to (9), wherein the light blocking member is a single member together with the housing member.
[0141] (10) A camera module comprising: the lens unit according to any one of (1) to (9); and an imaging element.
[0142] REFERENCE SIGNS LIST 10 Optical element 11 Plastic lens 12 Hard coat layer 13 Anti-reflection film 100 Lens unit 200 Camera module
Claims
1. A lens unit comprising: a plurality of lenses; and a cylindrical container member that contains the plurality of lenses, wherein the plurality of lenses are arranged in order from an opening of the container member; and an outermost lens of the plurality of lenses that is located on the opening side of the container member includes a plastic lens having a surface with an inflection portion, an anti-reflection film arranged on the surface side of the plastic lens, and a hard coat layer located between the plastic lens and the anti-reflection film, and the lens unit further comprises a light-shielding member that blocks the inflection portion of the plastic lens.
2. The lens unit according to claim 1, wherein said plastic lens is recessed at said inflection portion.
3. The lens unit according to claim 1 or 2, wherein the lens unit has an optical axis, and the thickness of the hard coat layer on the optical axis is 2 μm or more and 20 μm or less.
4. The lens unit according to claim 1 or 2, wherein the hard coat layer has an elastic modulus of 5 GPa or more and 12 GPa or less.
5. The lens unit according to claim 1 or 2, wherein the thermal expansion coefficient of the plastic lens is 60 ppm / K or more and 150 ppm / K or less.
6. The lens unit according to claim 1 or 2, wherein the thermal expansion coefficient of the anti-reflection film is 1 ppm / K or more and 10 ppm / K or less.
7. The lens unit according to claim 1 or 2, wherein the thermal expansion coefficient of said plastic lens is 60 ppm / K or more and 100 ppm / K or less, and the thermal expansion coefficient of said anti-reflection film is 5 ppm / K or more and 10 ppm / K or less.
8. The lens unit according to claim 1 or 2, wherein the light blocking member is a single member together with the housing member.
9. A camera module comprising the lens unit according to claim 1 or 2 and an imaging element.
Citation Information
Patent Citations
Plastic optical member and production thereof
JP1989197701A
Optical element, imaging device, electronic equipment, and method for manufacturing optical element
JP2010072451A
Optical unit and imaging apparatus
JP2014098860A
Substrate with lens, laminated lens structure, camera module, and apparatus and method manufacturing
JP2017032798A
Vehicular camera apparatus
KR1020180046522A