Coating liquid composition, production method therefor, and liquid containing low-temperature-damage inhibitor

A stable and effective coating liquid composition using sugar-based surfactants and rapid cooling addresses the limitations of existing food freshness maintenance methods by providing enhanced low-temperature damage prevention and improved coating properties for fruits and vegetables.

WO2024204849A1PCT designated stage expired Publication Date: 2024-10-03MITSUBISHI CHEM CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/013515
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2024-03-27
Filing Date
2024-04-01
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Current methods for maintaining food freshness, particularly in packaging and coatings for fruits and vegetables, face issues such as instability of coating liquids, low effectiveness in preventing low-temperature damage, and unsatisfactory safety and appearance of applied coatings, with existing surfactants like sucrose fatty acid esters having limitations in dispersion and concentration.

Method used

A coating liquid composition containing a surfactant with high dispersibility and stability, using sugar-based surfactants like sugar fatty acid esters and glycerin fatty acid esters, and a manufacturing process that includes rapid cooling to enhance dispersibility and prevent aggregation, resulting in a stable and effective low-temperature damage inhibitor.

Benefits of technology

The composition achieves high stability and effectiveness in preventing low-temperature damage to fruits and vegetables, maintaining freshness, and ensuring a safe and aesthetically pleasing coating, with improved dispersibility and long-term stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JPOXMLDOC01-APPB-M000001
    Figure JPOXMLDOC01-APPB-M000001
  • Figure JPOXMLDOC01-APPB-M000002
    Figure JPOXMLDOC01-APPB-M000002
  • Figure JPOXMLDOC01-APPB-T000003
    Figure JPOXMLDOC01-APPB-T000003
Patent Text Reader

Abstract

Provided is a coating liquid composition containing a surfactant in which the transmittance of light having a wavelength of 875 nm as measured under specific conditions using a multisample dispersion analyzer is 60% or higher at the time of production and the amount of change in the transmittance after being left at 20°C for 18 days relative to the transmittance at the time of production is no higher than 10%. The present invention makes it possible to provide a coating liquid composition having extremely high stability, a production method for the coating liquid composition, a method for maintaining food freshness, and a liquid containing a low-temperature-damage inhibitor.
Need to check novelty before this filing date? Find Prior Art

Description

Coating liquid composition, its method of manufacture, and liquid containing agent for suppressing low-temperature damage

[0001] The present invention relates to a coating liquid composition, a method for producing the same, and a liquid containing an agent for suppressing low-temperature damage.

[0002] In recent years, packaging materials capable of preserving the freshness of food during distribution or storage, such as modified atmosphere (MA) packaging, have been attracting attention. For example, a technology has been proposed in which a layer having a freshness-preserving effect is provided on a film for packaging food to preserve the freshness of food (see Patent Document 1). Another technology has also been proposed in which a quality-preserving agent is directly applied to food such as fruits and vegetables to preserve the freshness of food (see Patent Documents 2, 3, and 4).

[0003] As a liquid agent for maintaining the freshness of food, Patent Document 5 discloses an agent for preventing damage to fruit and vegetables peels, the active ingredient of which is a surfactant with an HLB of 5 or less. Since the lipophilic surfactant used in Patent Document 5 is difficult to disperse or dissolve in water, Patent Document 5 discloses a method of spraying an emulsion emulsified with a hydrophilic emulsifier onto fruit and vegetables, or a method of immersing the fruit and vegetables in the emulsion to attach the surfactant with an HLB of 5 or less to the surface of the fruit and vegetables.

[0004] Furthermore, Patent Document 6 describes an agent for preventing chilling damage to fruits and vegetables, which contains a sucrose fatty acid ester and has a monoester content of 40% by weight or more.

[0005] Furthermore, Patent Document 7 describes an aqueous dispersion of a sucrose fatty acid ester, which contains a sucrose fatty acid ester, an anionic surfactant, and water, wherein the anionic surfactant is a fatty acid metal salt, and the content of the anionic surfactant is 0.1 to 50% by weight based on the sucrose fatty acid ester.

[0006] JP 2001-171058 JP 2018-134115 JP 2005-530502 JP JP 2018-529627 JP 8-56564 JP 1-206947 JP 2022-100297

[0007] In the technology disclosed in Patent Document 1, food may come into contact with the packaging film during distribution or storage, so it is preferable that the layer with freshness-preserving properties be highly safe for humans. Another issue is reducing the amount of packaging film itself from the perspective of waste. The methods disclosed in Patent Documents 2 and 3 have short freshness-preserving periods and are not necessarily sufficient to achieve freshness-preserving properties. Furthermore, there are also issues, such as the materials used being compositions that are not gentle on the human body. On the other hand, as disclosed in Patent Document 4, a method is known for maintaining the freshness of agricultural produce by using a protective coating derived from monoacylglycerides to cover the produce. However, agricultural produce comes in a variety of shapes and types, and it is considered that a protective coating cannot necessarily be applied to the entire surface of the produce depending on the coating method.

[0008] The liquid formulation disclosed in Patent Document 5 has insufficient liquid stability, and gelation may occur during preparation of the liquid formulation or over time. Furthermore, when the liquid formulation disclosed in Patent Document 5 is applied to foods such as fruits and vegetables, it takes a long time to dry, which may result in poor productivity. In addition, traces of application may be visible, or the surface of the applied food may become white, resulting in poor appearance of the coating film.

[0009] The agent for preventing damage to fruit and vegetables peels disclosed in Patent Document 6 is emulsified because it is difficult to disperse and dissolve in water, but the upper limit of the concentration is 1.0% by weight, and there is still room for improvement in terms of the effect on fruit and vegetables.

[0010] The sucrose fatty acid ester aqueous dispersion disclosed in Patent Document 7 is described as being useful as an additive for foods, cosmetics, pharmaceuticals, etc., or as a coating agent, but there is room for further optimization before it can be applied to fruits and vegetables.

[0011] In response to the above-mentioned problems, the present applicant proposed in Japanese Patent Application No. 2021-169055 a composition comprising a sugar-based surfactant and an aqueous solvent, wherein the sugar-based surfactant is primarily a sugar fatty acid ester, and the sugar fatty acid ester comprises 50 to 98% by mass of a sugar fatty acid ester having three or fewer fatty acid ester groups, and 2 to 50% by mass of a sugar fatty acid ester having five or more fatty acid ester groups, out of 100% by mass of the sugar fatty acid ester. The composition described in this application has good liquid stability, and by applying it to food, sufficient freshness retention can be ensured. However, while it is preferable to use, for example, sucrose fatty acid ester, a food surfactant, as a raw material for the coating liquid, it is not dissolved in the aqueous solvent but forms a dispersed structure as an emulsion, making it difficult to maintain a uniform dispersion in a low-viscosity liquid such as an aqueous solvent.

[0012] On the other hand, the mechanism of chilling injury, which is one of the indicators for evaluating the freshness of agricultural products, has not been elucidated, and it cannot be assumed that chilling injury can be prevented or suppressed even if an agent that suppresses weight loss and ripening during storage is used. In contrast, Patent Document 6 uses sucrose fatty acid esters to prevent chilling injury in fruits and vegetables, but the concentration when applied to fruits and vegetables is low, and it is believed that there is still room for further study on the preparation and effectiveness of the chilling injury inhibitor. Therefore, the present applicant aims to provide a coating liquid composition and a method for producing a coating liquid composition that are extremely stable, aiming for further liquid stability and chilling injury suppression effect, and to provide a solution containing a chilling injury inhibitor that is highly stable and highly effective, aiming for further liquid stability and chilling injury suppression effect.

[0013] The present inventors focused on the manufacturing process of a surfactant-containing coating liquid composition and a surfactant-containing solution containing a chilling injury inhibitor. Specifically, they discovered that by controlling the manufacturing conditions, the stability of the surfactant-containing coating liquid composition and the surfactant-containing solution containing a chilling injury inhibitor can be maintained at an extremely high level. Furthermore, they discovered that fruits and vegetables to which the chilling injury inhibitor was added by applying the resulting chilling injury inhibitor-containing solution exhibited excellent chilling injury inhibitory effects. The present invention was completed based on the above findings.

[0014] That is, the present invention has the following aspects. [1] A coating liquid composition containing a surfactant, and for which evaluation of dispersibility in multiple samples during preparation using a particle size distribution analyzer under the following conditions shows a transmittance of 60% or more at a wavelength of 875 nm, and the change in transmittance after standing at 20°C for 18 days relative to the transmittance at the time of preparation is 10% or less. [Measurement conditions] Cell optical path length: 2 mm, liquid volume: 0.4 ml, cell internal cross-sectional area: 16 mm 2 , Measurement position: Multiple specimens / dispersibility evaluation, distance from the rotation center of the particle size distribution measurement device: 120 mm, rotation speed: 4000 rpm, rotation time: 30 minutes [2] The coating liquid composition according to the above [1], wherein the surfactant comprises a sugar-based surfactant. [3] The coating liquid composition according to the above [1] or [2], wherein the surfactant comprises a glycerin fatty acid ester. [4] The coating liquid composition according to the above [2] or [3], wherein the sugar-based surfactant comprises a sugar fatty acid ester. [5] The coating liquid composition according to any one of the above [1] to [4], wherein the concentration of non-volatile components is 1 to 20% by mass. [6] The coating liquid composition according to the above [5], wherein the content of surfactant in the non-volatile components is 60% by mass or more. [7] Shear rate 1 s -1 [8] The coating liquid composition according to any one of the above [1] to [6], wherein the shear viscosity at 1000 kJ / cm2 is 0.1 to 900 mPa·s in differential scanning calorimetry at a measurement temperature range of −80° C. or higher. 3 The total area A of the endothermic peaks between 0 ° C and 80 ° C 2

[10] A method for preserving the freshness of food, using the coating liquid composition according to any one of [1] to [8] above.

[11] A low-temperature damage inhibitor containing a surfactant, which has a transmittance of 60% or more at a wavelength of 875 nm and a non-volatile component concentration of 0.5% by mass or more, as measured under the following conditions using a particle size distribution analyzer for multi-sample / dispersibility evaluation during preparation. [Measurement conditions] Cell optical path length: 2 mm, liquid volume: 0.4 ml, cell internal cross-sectional area: 16 mm 2, Measurement position: Multiple sample / dispersibility evaluation, distance from the rotation center of the particle size distribution analyzer: 120 mm, rotation speed: 4000 rpm, rotation time: 30 minutes

[12] The agent for preventing low-temperature damage according to

[11] , wherein the change in transmittance after standing at 20°C for 18 days relative to the transmittance at the time of preparation is 10% or less.

[13] A method for applying the agent for preventing low-temperature damage according to

[11] or

[12] above.

[14] A method for preventing low-temperature damage in fruits and vegetables, using the agent for preventing low-temperature damage according to

[11] or

[12] above.

[15] A method for producing a coating liquid composition containing a surfactant, the method comprising heating the coating liquid composition to 50 to 90°C and then cooling it to 25°C within 60 minutes.

[16] A method for producing the coating liquid composition according to

[15] above, wherein the surfactant comprises a sugar-based surfactant.

[17] A method for producing the coating liquid composition according to

[15] or

[16] above, wherein the surfactant comprises a glycerin fatty acid ester.

[18] A method for producing a coating liquid composition according to the above

[16] or

[17] , wherein the sugar-based surfactant is a sugar fatty acid ester.

[19] A method for producing a coating liquid composition according to any one of the above

[15] to

[18] , wherein the concentration of non-volatile components in the coating liquid composition is 1 to 20 mass %.

[20] A method for producing a coating liquid composition according to the above

[19] , wherein the content of surfactant in the non-volatile components is 60 mass % or more.

[0015] According to the present invention, it is possible to provide a coating liquid composition having extremely high stability, a method for producing a coating liquid composition, and a highly stable liquid containing an agent for suppressing low-temperature damage.

[0016] The present invention will be described in detail below, but the present invention is not limited to specific embodiments.

[0017] [Coating Liquid Composition] The coating liquid composition of the present invention contains a surfactant and is characterized in that, after 30 minutes at 4000 rpm using an analytical centrifuge for a particle size distribution measurement device for multiple specimens and dispersibility evaluation (LUMiSizer (registered trademark), manufactured by Nippon Luft Co., Ltd.), the transmittance of light with a wavelength of 875 nm at a measurement position 120 mm from the center of rotation of the particle size distribution measurement device for multiple specimens and dispersibility evaluation is 60% or more. Light with a wavelength of 875 nm is called near-infrared light, and a transmittance of 60% or more for light of this wavelength indicates high dispersibility of the surfactant. From the above perspectives, the transmittance in this wavelength range is preferably 65% ​​or more, more preferably 70% or more, and even more preferably 75% or more. Note that the transmittance here refers to the transmittance immediately after preparation of the coating liquid composition. Furthermore, a coating liquid is used to cover the surface of a substance with a coating or layer formed of a substance other than the substance. When a sugar fatty acid ester or a glycerin fatty acid ester, which will be described later, is used as the surfactant contained in the coating liquid, the coating liquid composition can be suitably used for food and fruit and vegetables. The coating liquid composition of the present invention can also be used for preventing low-temperature damage. In this case, the coating liquid composition for preventing low-temperature damage can be applied to foods such as fruits and vegetables. This can also suppress low-temperature damage in foods such as fruits and vegetables.

[0018] In the present invention, when measuring the coating liquid composition, it is assumed that the coating liquid composition is free of precipitation. The absence of precipitation refers to a state in which the coating liquid composition is homogenized by stirring before sampling, then part or all of it is quickly transferred to a transparent container, and after leaving it at room temperature for 30 minutes, it can be visually confirmed that no precipitation has occurred at the bottom. This standard also applies when performing measurements other than the particle size distribution measurement for multiple sample dispersibility evaluation.

[0019] [Low-temperature damage inhibitor-containing liquid] The low-temperature damage inhibitor-containing liquid of the present invention contains a surfactant and a solvent, has a non-volatile component concentration of 0.5% by mass or more, and is characterized in that, after 30 minutes at 4000 rpm using an analytical centrifuge for multi-analyte / dispersibility evaluation particle size distribution measurement (LUMiSizer (registered trademark), manufactured by Nippon Luft Co., Ltd.), the transmittance of light with a wavelength of 875 nm at a measurement position 120 mm away from the center of rotation of the multi-analyte / dispersibility evaluation particle size distribution measurement device is 60% or more. The low-temperature damage inhibitor-containing liquid of the present invention may contain the above-mentioned coating liquid composition. Hereinafter, when the "coating liquid composition" of the present invention is referred to as the "low-temperature damage inhibitor-containing liquid" of the present invention, it is also intended to include the "low-temperature damage inhibitor-containing liquid" of the present invention in cases where the combinations of components overlap. In other words, when the "coating liquid composition" of the present invention is referred to as the "low-temperature damage inhibitor-containing liquid," it can also be used as the "low-temperature damage inhibitor-containing liquid" of the present invention, and the preferred composition, manufacturing method, and usage method may be the same.

[0020] The coating liquid composition of the present invention also has a high transmittance after standing for 18 days, and the change in transmittance after standing for 18 days at 20°C relative to the transmittance at the time of preparation (change amount) is preferably 10% or less (10% pt or less). The transmittance at the time of preparation and the transmittance after standing for 18 days at 20°C are each expressed as a percentage, and the difference between them is also referred to as % pt. This index indicates that the surfactant has high dispersibility immediately after preparation and that this high dispersibility is maintained even after 18 days have passed. From the above perspectives, the change in transmittance after standing for 18 days at 20°C is more preferably 8% (8% pt) or less, and particularly preferably 7% (7% pt) or less. The change in transmittance after standing for 18 days at 20°C relative to the transmittance at the time of preparation is calculated by subtracting the transmittance at the time of preparation from the transmittance after standing for 18 days at 20°C.

[0021] Incidentally, coating liquid compositions containing conventional surfactants exhibit low transmittance values ​​immediately after preparation, while the transmittance may increase after 18 days (after standing still). This indicates that immediately after preparation, there is a dispersion that does not precipitate even after centrifugation, and that the particle size is small. Dispersions with small particle sizes have a large surface area and poor stability, so aggregation and sedimentation are likely to occur. The increase in transmittance after 18 days means that the amount of dispersions with small particle sizes has decreased. In other words, this means that the dispersion state has changed during the 18-day standing period, and this means that the degree of dispersion of the surfactant is low.

[0022] On the other hand, if the value falls within the range of the present invention, the change in transmittance after standing for 18 days is small. This means that the number of low-stability microparticles is small, there is little change in state, and the liquid state is highly stable. While the change in transmittance may be negative, taking into account measurement variability, a value between -10% pt and +10% pt indicates high liquid stability. Preferably, the value is between -8% pt and +8% pt, and more preferably between -7% pt and +7% pt. While the liquid stability can be partially estimated from the particle size of the dispersion, it is extremely difficult to evaluate it while taking into account scientific properties such as shape, particle size distribution, and surface potential. However, the method used in the present invention makes it possible to evaluate the liquid stability without having to go to the trouble of understanding the properties of such dispersions.

[0023] [Evaluation of Stability of Coating Liquid Composition] The stability of the coating liquid composition is evaluated immediately after preparation and after standing at 20°C for 18 days using the following device under the following conditions: Device: Dispersion Stability Analyzer "LUMiSizer (registered trademark)" (Nippon Luft Co., Ltd.) Measurement cell: LUM 2 mm PA (polyamide) (optical path length 2 mm) Rotation speed: 4000 rpm Measurement temperature: 25°C Measurement time: 30 minutes <Evaluation criteria> ○: The transmittance at a measurement position of 120 mm is 60% or more, and the change in transmittance between immediately after preparation and after standing is 10% or less. ×: The transmittance at a measurement position of 120 mm is less than 60%, and the change in transmittance between immediately after preparation and after standing is 10% or more.

[0024] <Surfactant> The coating liquid composition of the present invention contains a surfactant. By including a surfactant, the coating liquid composition has high wettability and can improve the coating properties on target foods such as vegetables and fruits. Two or more surfactants may be used in combination. A surfactant is a substance that exhibits interfacial activity that reduces the surface tension of a solution in which it is dissolved, and is used in practical applications.

[0025] The surfactant has a hydrophilic group and a lipophilic group. Examples of the hydrophilic group include a hydroxyl group, a carboxylic acid group, a sulfate group, a phosphate group, an amine, and a quaternary ammonium group. The carboxylic acid group, the sulfate group, the phosphate group, the amino group, and the quaternary ammonium group may be in the form of a salt. Examples of the hydrophobic group include a hydrocarbon group, a fluorine group, and an organosilicon group. When a fatty acid is used as a compound for forming a lipophilic group in synthesizing the surfactant, the fatty acid is preferably an edible oil or fat.

[0026] The number of carbon atoms in the fatty acid is not particularly limited, but is preferably from 12 to 22, more preferably from 12 to 18, and even more preferably from 14 to 18. When the number of carbon atoms is within the above range, the stickiness of the resulting coating can be suppressed.

[0027] The fatty acid may be saturated or unsaturated, but saturated fatty acids are preferred from the viewpoint of readily solidifying at room temperature (20-25°C) and reducing the stickiness of the resulting coating. More specifically, examples include lauric acid, myristic acid, pentadecylic acid, palmitic acid, palmitoleic acid, margaric acid, stearic acid, and oleic acid. Among these, saturated fatty acids having 12 to 18 carbon atoms, such as lauric acid, myristic acid, palmitic acid, and stearic acid, are preferred, and saturated fatty acids having 14 to 18 carbon atoms, such as myristic acid, palmitic acid, and stearic acid, are more preferred. These saturated fatty acids may be used alone or in combination. Furthermore, the fatty acids do not all need to be the same; it is sufficient that 60% by mass or more of the fatty acids constituting the surfactant are the above-mentioned suitable constituent fatty acids. From the viewpoint of reducing the stickiness of the resulting coating, this ratio is preferably 70% by mass or more, more preferably 80% by mass or more, and even more preferably 90% by mass or more. The upper limit is not particularly limited, but may be 100% by mass or less. The composition of fatty acids constituting the surfactant can be measured by isolating the surfactant from the composition, derivatizing it, and then analyzing it by gas chromatography.

[0028] As surfactants used in the coating liquid composition of the present invention, ester-type and ether-type surfactants are preferred from the viewpoint of biodegradability. As ester-type surfactants, glycerin fatty acid esters and sugar fatty acid esters are preferred from the viewpoint of being approved as food additives. As ether-type surfactants, alkyl glycosides are preferred from the viewpoint of being approved as food additives. Among these, glycerin fatty acid esters and sugar fatty acid esters are preferred from the viewpoint of easily adjusting hydrophilicity and hydrophobicity, and sugar fatty acid esters are preferred from the viewpoint of being highly water-soluble and being usable by dissolving in a solvent whose main component is water. Hereinafter, sugar fatty acid esters and alkyl glycosides will be collectively referred to as sugar-based surfactants.

[0029] The HLB of the surfactant is not particularly limited, but from the viewpoint of being able to form a coating film using an aqueous solvent described below, it is preferably 5 or more, more preferably 7 or more, and even more preferably 9 or more. The upper limit of the HLB is usually 20, and more preferably 18 or less.

[0030] (Sugar-based surfactants) Sugar-based surfactants are surfactants that contain sugar as a hydrophilic group, and examples thereof include sugar fatty acid esters formed by an ester bond between a sugar and a fatty acid, and alkyl glycosides formed by a glycosidic bond between a sugar and a higher alcohol. Of these, sugar fatty acid esters are preferred from the viewpoint of film-forming properties.

[0031] The sugar-based surfactant is preferably crystalline from the viewpoint of suppressing stickiness of the resulting coating and enhancing the water vapor barrier property and oxygen barrier property. Furthermore, from the viewpoint of suppressing stickiness of the resulting coating, the sugar-based surfactant preferably contains 60% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, and even more preferably 90% by mass or more of a component that becomes solid at room temperature (20-25°C). The sugar-based surfactant may be composed solely of components that become solid at room temperature (20-25°C), and therefore, the above ratio may be 100% by mass or less.

[0032] The HLB of the sugar-based surfactant is not particularly limited, but from the viewpoint of being able to form a coating using an aqueous solvent described below, it is preferably 5 or more, more preferably 7 or more, and even more preferably 9 or more. The upper limit of the HLB is usually 20, and more preferably 18 or less.

[0033] <Sugar fatty acid ester> A sugar fatty acid ester is an ester bond between a sugar and a fatty acid.

[0034] The sugar in the sugar fatty acid ester may be any of monosaccharides, disaccharides, trisaccharides, tetrasaccharides, polysaccharides, sugar alcohols, and other oligosaccharides. Monosaccharides include pentoses such as ribulose, xylulose, ribose, arabinose, xylose, lyxose, and deoxyribose; and hexoses such as psicose, fructose, sorbose, tagatose, allose, altrose, glucose, mannose, gulose, idose, galactose, talose, fucose, fuculose, and rhamnose. Disaccharides include sucrose (cane sugar), lactose, maltose, trehalose, turanose, and cellobiose. Trisaccharides include raffinose, melezitose, and maltotriose. Tetrasaccharides include acarbose and stachyose. Examples of polysaccharides include glycogen, starch, cellulose, dextrin, glucan, fructan, chitin, etc. Examples of sugar alcohols include sorbitol, erythritol, xylitol, maltitol, lactitol, mannitol, glycerin, etc., and may be condensates of these sugar alcohols. Examples of other oligosaccharides include fructooligosaccharides, galactooligosaccharides, mannanoligosaccharides, lactosucrose, etc.

[0035] The constituent fatty acid of the sugar fatty acid ester is preferably an edible oil or fat. The number of carbon atoms of the constituent fatty acid of the sugar fatty acid ester is not particularly limited, but is preferably 12 to 22, more preferably 12 to 18, and even more preferably 14 to 18. Having a carbon number within the above range reduces the stickiness of the resulting coating. The constituent fatty acid of the sugar fatty acid ester may be a saturated or unsaturated fatty acid, but saturated fatty acids are preferred because they tend to solidify at room temperature (20 to 25°C) and reduce the stickiness of the resulting coating. More specific examples include lauric acid, myristic acid, pentadecylic acid, palmitic acid, palmitoleic acid, margaric acid, stearic acid, and oleic acid. Of these, saturated fatty acids having 12 to 18 carbon atoms, such as lauric acid, myristic acid, palmitic acid, and stearic acid, are preferred, and saturated fatty acids having 14 to 18 carbon atoms, such as myristic acid, palmitic acid, and stearic acid, are more preferred. These saturated fatty acids may be used alone or in combination. It is not necessary for all of the constituent fatty acids of the sugar fatty acid ester to be the same, as long as 60% by mass or more of the constituent fatty acids in the sugar fatty acid ester are the above-mentioned suitable constituent fatty acids. From the viewpoint of suppressing stickiness of the resulting coating, this ratio is preferably 70% by mass or more, more preferably 80% by mass or more, and even more preferably 90% by mass or more. There is no particular upper limit, but it is sufficient as long as it is 100% by mass or less. The constituent fatty acid composition of the sugar fatty acid ester can be measured by isolating the sugar fatty acid ester from the composition, derivatizing it, and then analyzing it by gas chromatography.

[0036] The number of fatty acid ester groups in a sugar fatty acid ester varies depending on the number of ester-bondable hydroxyl groups in the molecular structure of the sugar, which is the hydrophilic group; for example, 1 to 8 for sucrose fatty acid esters and 1 to 4 for sorbitan fatty acid esters. From the viewpoint of being dispersible or soluble in aqueous solvents, the sugar-based surfactant preferably contains 50% by mass or more of sugar fatty acid esters (monoesters, diesters, or triesters) having three or fewer fatty acid ester groups, when the total amount of the sugar-based surfactant is taken as 100% by mass, more preferably 60% by mass or more, and even more preferably 70% by mass or more. The upper limit is not particularly limited, but it is sufficient as long as it is 100% by mass or less. From the same viewpoint, the sugar-based surfactant preferably contains 30% by mass or less of sugar fatty acid esters (hexaesters, heptaesters, octaesters, or more) having six or more fatty acid ester groups, when the total amount of the sugar-based surfactant is taken as 100% by mass, more preferably 20% by mass or less, and even more preferably 10% by mass or less. The sugar fatty acid ester having six or more fatty acid ester groups may not be contained, and its content may be 0% by mass or more.

[0037] The content ratio by number of fatty acid ester groups can be measured after isolating the sugar fatty acid ester from the composition according to the method of assay described in the Residue Monograph prepared by the meeting of the Joint FAO / WHO Expert Committee on Food Additives (JECFA), 84th meeting 2017, "Sucrose Esters of Fatty Acids," and in the FAO JECFA Monographs 7 (2009), "Sucrose Oligoesters Type I" and "Sucrose Oligoesters Type II," prepared at the 71st JECFA meeting (2009) and published in FAO JECFA Monographs 7 (2009).

[0038] <<Measurement of Monoesters to Triesters and Tetraesters or Higher>> A sample is dissolved in a certain amount of tetrahydrofuran (stabilized GPC or industrial grade), and the insoluble matter is removed using a 0.5 μm membrane filter. This solution is used as a measurement sample and subjected to high performance liquid chromatography under the following conditions. The composition ratio is calculated by individually calculating the peak areas of the monoesters to triesters and the combined peak area of ​​tetraesters or higher, and then calculating the ratio to the total peak area of ​​all peaks detected up to 43 minutes. The peak area is the area from the start point (rising point) to the end point (falling point) of each peak. If two or more peaks are adjacent and the start and end points are unknown, the points where the data between the peaks is smallest are used as the start and end points, respectively, to calculate the area.

[0039] <Measurement conditions: monoesters to triesters and tetraesters and above> Apparatus: HLC-8320GPC Detector: differential refractometer (manufactured by Tosoh Corporation) Column: TSK-gel G1000HXL, G2000HXL, G3000HXL, G4000HXL (manufactured by Tosoh Corporation) Column temperature: 40°C Detector temperature: 40°C Eluent: tetrahydrofuran (stabilizer-containing GPC or industrial grade) Flow rate: 0.8 ml / min Injection volume: 80 μl Measurement time: 50 minutes (area ratio is calculated based on all peaks detected up to 43 minutes)

[0040] <<Measurement of Tetraesters to Octaesters>> A sample is dissolved in a fixed amount of methanol (special reagent grade) / tetrahydrofuran (stabilizer-free HPLC grade) = 20 / 80 (vol / vol), and the solution is used as the measurement sample after removing insoluble matter with a 0.45 μm membrane filter. High-performance liquid chromatography is performed under the following conditions. The composition ratio of tetraesters to octaesters is calculated by calculating the peak areas of each tetraester to octaester individually, calculating the ratio to the total peak area of ​​tetraesters to octaesters, and then proportionally dividing the area ratio of tetraesters and higher peaks obtained in <<Measurement of Monoesters to Triesters and Tetraesters and Higher>> by the area ratio of tetraesters to octaesters.>> The peak area is the area from the start point (rising point) to the end point (falling point) of each peak. If two or more peaks are adjacent and the start and end points are unknown, the points with the smallest data between the peaks are used as the start and end points to calculate the area.

[0041] <Measurement conditions: tetraester to octaester> Equipment Degasser: DGU-20A (Shimadzu Corporation) Pump: LC-20AD (Shimadzu Corporation) Oven: CTO-20A (Shimadzu Corporation) Detector: RID-20A differential refractometer (Shimadzu Corporation) Column: 150 mm x 4.6 mm i.d.; ODS-2 (GL Sciences) Column temperature: 40°C Detector temperature: 40°C Eluent: methanol (special reagent grade) / tetrahydrofuran (stabilizer-free HPLC grade) = 70 / 30 to 50 / 50 (vol / vol) Flow rate: 0.8 ml / min Injection volume: 20 μl Measurement time: 16 minutes

[0042] The sugar fatty acid ester is not particularly limited as long as it is usable for food products, but examples include sucrose fatty acid esters, sorbitan fatty acid esters, glucose esters, etc., with sucrose fatty acid esters being preferred from the viewpoint of easy availability. It is not necessary to use only one sugar-based surfactant; two or more types may be used in combination. When two or more types are combined, it is preferable that 60% by mass or more of the sucrose fatty acid esters account for 100% by mass of the total amount of sugar-based surfactants. This ratio is more preferably 70% by mass or more, even more preferably 80% by mass or more, and particularly preferably 90% by mass or more, from the viewpoint of suppressing stickiness of the resulting coating and enhancing the water vapor barrier property and oxygen barrier property. The sugar-based surfactant may be sucrose fatty acid ester alone, and therefore the above ratio may be 100% by mass or less.

[0043] <Glycerin fatty acid ester> Glycerin fatty acid ester is an ester bond between glycerin and a fatty acid. Examples of fatty acids constituting glycerin fatty acid esters include the same fatty acids as those constituting sucrose fatty acid esters. However, since glycerin fatty acid esters have a small number of hydroxyl groups and are relatively low in hydrophilicity, the number of carbon atoms of the fatty acid used in the hydrophobic portion is preferably in a relatively small range. From this viewpoint, the number of carbon atoms of the fatty acid is preferably 4 or more, more preferably 6 or more, and more preferably 8 or more. The number of carbon atoms of the fatty acid is preferably 24 or less, more preferably 22 or less, even more preferably 20 or less, particularly preferably 18 or less, and most preferably 16 or less.

[0044] The content of glycerin fatty acid ester (monoester) having one fatty acid ester group is usually 5% by mass or more when the total amount of glycerin fatty acid ester is taken as 100% by mass, from the viewpoints of dispersibility in aqueous solvents, viscosity of the composition, and handling. 10% by mass or more is preferred, 20% by mass or more is more preferred, 30% by mass or more is even more preferred, and 40% by mass or more is particularly preferred. 50% by mass or more is preferred, 60% by mass or more is more preferred, 70% by mass or more is even more preferred, and 80% by mass or more is particularly preferred. There is no particular upper limit, but it is sufficient as long as it is 100% by mass or less.

[0045] The content of the glycerin fatty acid ester (diester) having two fatty acid ester groups depends on the content of the monoester and triester, and is not particularly limited.

[0046] From the viewpoints of dispersibility in aqueous solvents, viscosity of the composition, and ease of handling, the content of glycerin fatty acid esters (triesters) having three fatty acid ester groups is preferably 50% by mass or less, more preferably 40% by mass or less, even more preferably 30% by mass or less, particularly preferably 20% by mass or less, and most preferably 10% by mass or less, when the total amount of glycerin fatty acid esters is taken as 100% by mass. The lower limit is not particularly limited, but it may not be contained (0% by mass), or may contain less than 1% by mass as an impurity, or may be 0.5% by mass or more.

[0047] From the viewpoints of dispersibility in aqueous solvents, viscosity of the composition, and ease of handling, when the total amount of glycerin fatty acid esters is taken as 100% by mass, the total amount of glycerin fatty acid esters (monoesters) having one fatty acid ester group and fatty acid esters (diesters) having two fatty acid ester groups is preferably 50% by mass or more, more preferably 60% by mass or more, and even more preferably 70% by mass or more. There are no particular limitations on the upper limit, but it is sufficient that it is 100% by mass or less. Of these, the proportion of monoesters when the monoesters and diesters are combined is preferably 20% by mass or more, more preferably 40% by mass or more, even more preferably 50% by mass or more, particularly preferably 60% by mass or more, and most preferably 80% by mass. There are no particular limitations on the upper limit, but it is sufficient that it is 100% by mass or less.

[0048] The types and amounts of fatty acids can be analyzed by column chromatography, gas chromatography, thin layer chromatography, high performance liquid chromatography, colorimetric analysis, or the like.

[0049] <Mass Ratio> The mass ratio (solids content) of the sucrose fatty acid ester to the total mass of the sucrose fatty acid ester and the glycerin fatty acid ester is preferably 1% or more, more preferably 5% or more, even more preferably 10% or more, and particularly preferably 20% or more. Furthermore, this ratio is less than 100%. Within this range, the composition exhibits good applicability, resulting in a good coating appearance after application to fruits and vegetables. From the above viewpoints, the mass ratio of the sucrose fatty acid ester to the glycerin fatty acid ester is preferably 1 / 99 to 99 / 1, more preferably 5 / 95 to 99 / 1, even more preferably 10 / 90 to 98 / 2, particularly preferably 20 / 80 to 97 / 3, and most preferably 20 / 80 to 80 / 20.

[0050] The coating liquid composition of the present invention provides a coating film formed using the coating liquid composition, which exhibits water vapor barrier properties and oxygen barrier properties. Furthermore, since the coating liquid composition contains a surfactant, it is also preferable from the viewpoint of safety when used for food. The surfactant is as described above. One surfactant may be used alone, or two or more surfactants may be used in combination.

[0051] <Solvent> From the viewpoint of coating efficiency, the coating liquid composition of the present invention preferably contains a solvent. The solvent contained in the coating liquid composition is preferably an aqueous solvent. The aqueous solvent is water or a mixed solvent of one or more water-soluble organic solvents and water. Examples of the water-soluble organic solvent include alcohols such as ethanol, isopropanol, ethylene glycol, and glycerin. From the viewpoint of being able to be applied to food, water is preferred, but from the viewpoint of stability and coatability, an organic solvent such as the above-mentioned alcohol may be contained as the solvent in addition to water. The content of the water-soluble organic solvent in the aqueous solvent is preferably 30% by mass or less, more preferably 20% by mass or less, even more preferably 10% by mass or less, and particularly preferably 5% by mass or less.

[0052] <Other Components> The coating liquid composition of the present invention may contain other components to the extent that the effects of the present invention are not impaired. Examples of other components include a pH adjuster. Examples of pH adjusters that can be used include acetic acid, lactic acid, citric acid, and ammonia.

[0053] <Non-volatile component concentration> The non-volatile component concentration in the coating liquid composition of the present invention is not particularly limited, but is preferably 0.1% by mass or more, more preferably 0.5% by mass or more, more preferably 1% by mass or more, even more preferably 1.5% by mass or more, particularly preferably 2% by mass or more, and most preferably 3% by mass or more. On the other hand, it is preferably 20% by mass or less, more preferably 15% by mass or less, even more preferably 10% by mass or less, particularly preferably 9% by mass or less, and most preferably 8% by mass or less. By setting the non-volatile component concentration within the above range, the surfactant can be appropriately dissolved in the solvent, the stability of the dispersion is improved, and a uniform coating liquid composition can be obtained, making it easier to form a uniform film. It also makes it easier to form a coating with a suitable film thickness. On the other hand, if the concentration is high, the distance between the dispersions becomes closer, increasing the opportunity for contact, which increases the risk of aggregation and reduces the stability of the liquid. The "non-volatile component concentration" in the present invention refers to the concentration of non-volatile components excluding the solvent contained in the composition, more specifically, the concentration of non-volatile components excluding components that volatilize at normal pressure and 105°C or lower. Alternatively, it can be calculated as the proportion of non-volatile components in the blended composition.

[0054] <Surfactant Content> The surfactant content in the coating liquid composition of the present invention is preferably 60% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, and particularly preferably 90% by mass or more, of the non-volatile components in the coating liquid composition, with 100% by mass as the upper limit, from the viewpoint of improving the water vapor barrier property and oxygen barrier property of the resulting coating film, and from the viewpoint of improving the effect of suppressing low-temperature damage of fruits and vegetables to which the low-temperature damage inhibitor is attached when the coating liquid composition is used as a low-temperature damage inhibitor-containing liquid. Since the coating film formed by the coating liquid composition of the present invention is obtained by volatilizing the solvent from the composition, the suitable content of the surfactant in the coating is the same as above. Furthermore, when the coating liquid composition of the present invention is used as a low-temperature damage inhibitor-containing liquid, the low-temperature damage inhibitor of the present invention is solidified by an operation such as volatilizing the solvent from the low-temperature damage inhibitor-containing liquid, and therefore the suitable content of the surfactant in the low-temperature damage inhibitor is the same as above.

[0055] <pH of Coating Liquid Composition> The pH of the coating liquid composition of the present invention is preferably 4 or more and 10 or less, more preferably 4 or more and 8 or less, from the viewpoint of safe application to food.

[0056] <Shear Viscosity of Coating Liquid Composition> The coating liquid composition of the present invention preferably has a shear viscosity measured under the following conditions of 0.1 (mPa·s) or more, more preferably 0.2 (mPa·s) or more, even more preferably 0.5 (mPa·s) or more, and particularly preferably 1 (mPa·s) or more. On the other hand, it is preferably 900 (mPa·s) or less, more preferably 800 (mPa·s) or less, even more preferably 700 (mPa·s) or less, and particularly preferably 500 (mPa·s) or less. By having the viscosity within the above range, the coating can be performed without damaging the appearance of the object to be coated.

[0057] [Shear Viscosity Measurement] Immediately after preparation of the liquid containing the agent for suppressing low-temperature damage, it was evaluated using the following device. Device: Rotational rheometer (model: Kinexus pro+) Measurement mode: Shear rate dispersion of shear viscosity Measurement temperature: 25°C Plate: Cone-plate type, diameter 40 mm, cone angle 2 degrees Shear viscosity: Shear rate was adjusted to 0 (s -1 ) to 1000 (s -1 ) and then 1000 (s -1 ) to 0.1 (s -1 In the measurement where the shear rate is reduced to 1 (s -1 ) shear viscosity at

[0058] <Differential Scanning Calorimetry at 0°C or Higher> The coating composition of the present invention has a total endothermic peak area A in the range of 0°C to 40°C in differential scanning calorimetry at a measurement temperature range of 0°C or higher. 1 The total area A of the endothermic peaks between 0 ° C and 80 ° C 2 The ratio of the coating composition to the total amount of the raw material may be 50% or less. The ratio is preferably 40% or less, more preferably 30% or less, and even more preferably 20% or less. The ratio may be 0%. By being within this range, the phase change rate of the film formed on the coating composition is reduced within the practical temperature range for storing, transporting, and selling fruits and vegetables that are not stored frozen, and no phase change that affects the properties of the film occurs. For example, freshness-preserving functions such as water vapor barrier properties and oxygen barrier properties, which will be described later, can be maintained. The peak area is the area from the start point (rising point) to the end point (falling point) of each peak. In addition, A 1The temperature range when calculating is preferably 0°C or higher and 35°C or lower, more preferably 0°C or higher and 30°C or lower, and even more preferably 0°C or higher and 25°C or lower. This indicates that it is within the temperature range that is preferable for practical use as described above. By setting the measurement temperature range to 0°C or higher, it becomes possible to reflect the properties of the coating in the practical temperature range in which fruits and vegetables that are not stored frozen are stored, transported, and sold. For example, for a compound with a melting point of less than 0°C, setting the measurement range to less than 0°C makes it possible to perform measurements that reflect behaviors such as the phase change from liquid to solid, crystallization of uncrystallized components, and melting of solids. However, these behaviors are not exhibited within the practical temperature range described above, and it is difficult to say that the measurements reflect practical behavior. A 1 and A 2 Regarding the total area, there may be cases where multiple peaks exist within each temperature range for which the total area is calculated, or where only a portion of a peak falls within that temperature range. In such cases, for all peaks present within that temperature range, the total area of ​​only the portion that falls within that temperature range is calculated. For example, if one broad peak exists between 0 and 50°C, only the portion between 0 and 40°C is used as A. 1 It is considered that the surfactant used in the coating composition of the present invention has almost no peak in the temperature range exceeding 80°C. 2 Regarding the temperature range above 80°C, it is not considered necessary to consider the temperature range above 80°C.

[0059] Differential scanning calorimetry, with a measurement temperature range of 0°C or higher, is performed under the following conditions: Measurement device: differential scanning calorimeter Measurement method: heat flux method Temperature: 25°C → 0°C → 100°C Temperature increase / decrease rate: 10°C / min Atmosphere: nitrogen Sample preparation: The coating composition is placed in an empty aluminum pan so that the dry solid content is 1 mg, and the pan is left to dry at room temperature. It is confirmed that the weight change from the previous day is 1% or less, and a measurement sample is obtained. Reference: aluminum pan Note that for a sample in which no peak is observed when the temperature is increased or decreased below 0°C, the temperature may be decreased from 25°C to below 0°C, and then increased to 100°C for measurement.

[0060] <Differential Scanning Calorimetry at −80° C. or Higher> The coating composition of the present invention has a total exothermic peak area A 3 The total area A of the endothermic peaks between 0 ° C and 80 ° C 2 The ratio of the coating composition to the total surface area of ​​the coating composition may be 50% or less. By being within this range, the stickiness of the coating formed from the coating composition can be reduced within the temperature range in which fruits and vegetables that are not stored frozen are stored, transported, and sold, improving handleability, and further improving freshness-retaining properties such as water vapor barrier property and oxygen barrier property, which will be described later. The peak area is the area from the start point (rising point) to the end point (falling point) of each peak. The exothermic peak is thought to indicate the phase change behavior in which a component that was not solid becomes solid, or the crystallization behavior of a component that was not crystallized. On the other hand, the endothermic peak observed at 0°C or higher is thought to be a peak resulting from the phase change behavior of all components in the coating formed from the coating composition that can become solid, for example, the behavior in which all crystallizable components of the coating crystallize. Therefore, the total exothermic peak area A 3 The total area A of the endothermic peaks between 0 ° C and 80 ° C 2 The ratio of A to B is considered to indicate the ratio of components in the coating film formed from the coating composition that are not solid at temperatures above 0°C, e.g., not crystallized. From the viewpoint of enhancing the above-mentioned effect, this ratio is preferably 40% or less, more preferably 30% or less, and even more preferably 20% or less. Note that the exothermic peak observed by the measurement method described below may be observed during temperature rise. This is considered to indicate the behavior of components that have been in a supercooled state becoming solid, e.g., crystallizing. A 2 and A 3 Regarding the temperature ranges for which the total area is calculated, there may be cases where multiple peaks exist within the respective temperature ranges. In such cases, the total area of ​​only the parts of all peaks within the temperature range is calculated. Although unlikely, it is also possible that one peak exists within a temperature range that includes 0°C. In such cases, the peak area is calculated as A depending on whether it is an endothermic peak or an exothermic peak.2 and A 3 It is considered that the surfactant used in the coating composition of the present invention has almost no peaks in the temperature range below -80°C or above 80°C. 2 and A 3 Regarding the temperature range, it is not considered necessary to consider the range below -80°C and above 80°C.

[0061] Differential scanning calorimetry with a measurement temperature range of -80°C or higher is carried out under the following conditions. Measurement device: differential scanning calorimeter Measurement method: heat flux method Temperature: 25°C → -80°C → 100°C Temperature increase / decrease rate: 10°C / min Atmosphere: nitrogen Sample preparation: The coating composition is placed in an empty aluminum pan so that the dry solid content is 1 mg, and the pan is left to dry at room temperature. It is confirmed that the weight change from the previous day is 1% or less, and a measurement sample is obtained. Reference: aluminum pan

[0062] [Method for Producing a Coating Liquid Composition] The method for producing a coating liquid composition of the present invention is characterized by heating the composition to 50 to 90°C and then cooling it to 25°C within 60 minutes. Rapid cooling to 25°C within 60 minutes can improve the dispersibility of the surfactant in the coating liquid composition during production and prevent precipitation or aggregation of the surfactant even after long-term storage. From the above perspectives, the cooling time to 25°C is preferably within 50 minutes, and more preferably within 40 minutes. The rapid cooling method is not particularly limited, and includes, for example, cooling in an ice bath or cooling by exposure to cold air. After heating to 50 to 90°C, the composition may be held for a certain period of time before cooling. The holding time is preferably 15 minutes or more, more preferably 20 minutes or more, and even more preferably 25 minutes or more. It is preferably 2 hours or less, more preferably 1 hour or less, and even more preferably 45 minutes or less. By keeping the holding time within the above range, the uniformity of the surfactant in the coating liquid composition can be improved. When multiple solvents are used, some of them may be added at a predetermined timing, for example, before heating or before cooling after heating. In addition to the above-mentioned production method, the uniformity of the coating liquid composition can be improved by using a sugar fatty acid ester and a glycerin fatty acid ester in combination.

[0063] [Coating] The coating formed by the coating liquid composition of the present invention has water vapor barrier properties and / or oxygen barrier properties. Since the coating is applied to foods such as vegetables, it is preferably edible in consideration of safety when used in food. The surfactant used in the coating liquid composition of the present invention may be used alone or in combination of two or more. The coating liquid composition of the present invention contains a surfactant, but may also contain polysaccharides, polyvinyl alcohol, clay, etc. in addition to the surfactant. These materials preferably account for 60% by mass or more of the coating, with the upper limit being 100% by mass, more preferably 70% by mass or more, even more preferably 80% by mass or more, and even more preferably 90% by mass or more. The coating may be formed by solventless application or may be formed from a composition containing a solvent. In the present invention, from the viewpoint of safety when used in food, it is preferable to have a coating formed from a coating composition containing a sugar-based surfactant and an aqueous solvent. The coating formed by such a coating liquid composition inhibits respiration and moisture evaporation of vegetables, etc., thereby preserving the freshness of vegetables, etc.

[0064] [Cold Damage Inhibitor] When the coating liquid composition of the present invention is used as a liquid containing a cold damage inhibitor, the coating formed by the coating liquid composition of the present invention serves as a cold damage inhibitor. The cold damage inhibitor of the present invention can exhibit a cold damage inhibitory effect. It can also simultaneously exhibit water vapor barrier properties and / or oxygen barrier properties. Since it is applied to fruits and vegetables, it is preferable that it be edible, taking into consideration safety when used in food. The surfactant contained in the cold damage inhibitor of the present invention may be used alone or in combination with two or more. The cold damage inhibitor of the present invention contains a surfactant, but may also contain polysaccharides, polyvinyl alcohol, clay, etc. in addition to the surfactant. The surfactant content of the cold damage inhibitor is preferably 60% by mass or more, with the upper limit being 100% by mass, more preferably 70% by mass or more, even more preferably 80% by mass or more, and particularly preferably 90% by mass or more. The cold damage inhibitor can be conveniently applied to fruits and vegetables using a cold damage inhibitor-containing liquid containing a solvent. From the viewpoint of safety when used for food, the chilling injury inhibitor of the present invention is preferably applied to fruits and vegetables by applying a chilling injury inhibitor-containing solution containing a sugar-based surfactant and an aqueous solvent. By applying such a chilling injury inhibitor, the chilling injury inhibitor effect is exerted. At the same time, respiration and transpiration of vegetables and the like are suppressed, thereby maintaining the freshness of vegetables and the like.

[0065] <Water Vapor Barrier Properties> The coating film formed by the coating liquid composition of the present invention has a water vapor permeability of 0.1 g / (m 2 ·day·atm) or more, and 2 ·day·atm) or more, and 1.0 g / (m 2 ·day·atm) or more is more preferable. 2 ·day·atm) or less, and 2 ·day·atm) or less, and 2 ·day·atm) or less, and more preferably 40 g / (m 2 ·day·atm) or less is particularly preferable.2 ·day·atm) or less, and 2 ·day·atm) or less, and more preferably 15 g / (m 2 It is even more preferable that the water vapor transmission rate is equal to or less than 1 / 2 day / atm. When the water vapor transmission rate is within the above range, evaporation from vegetables or fruits can be suppressed, enabling freshness to be maintained. The water vapor transmission rate (WVTR) can be measured by a differential pressure method using a water vapor transmission rate measuring device DELTAPERM in accordance with JIS K7129-5. More specifically, the water vapor transmission rate measured when the film is coated on a polyethylene terephthalate film with a thickness of 50 μm under conditions of 30°C and 80% RH is converted into transmission rate per μm using the following formula:

[0066]

[0067] <Oxygen Barrier Property> The coating film formed by the coating liquid composition of the present invention has an oxygen permeability per 1 μm at 25° C. and 50% RH of 0.1 cc / (m 2 ·day·atm) or more is preferable, and 0.5 cc / (m 2 ·day·atm) or more is more preferable, and 1.0 cc / (m 2 ·day·atm) or more is more preferable. 2 ·day·atm) or less, and 300cc / (m 2 ·day·atm) or less is more preferable, and 250cc / (m 2 ·day·atm) or less is more preferable, and 200 cc / (m 2 ·day·atm) or less is particularly preferable. 2 ·day·atm) or less is more preferable, and 90cc / (m 2 ·day·atm) or less is more preferable, and 50 cc / (m 2·day·atm) or less is particularly preferred. When the oxygen permeability is within the above range, aging of vegetables or fruits due to respiration can be suppressed, and freshness can be better maintained. The oxygen permeability (OTR) can be measured by the isobaric method using an oxygen permeability measuring device OX-TRAN 2 / 21 (manufactured by MOCON) based on JIS K7126-2. More specifically, the measured oxygen permeability when coated on a polyethylene terephthalate film with a thickness of 50 μm under conditions of 25°C and 50% RH is converted into permeability per μm using the following formula.

[0068]

[0069] <Edibility> The coating film formed by the coating liquid composition of the present invention is preferably edible. Edible means that it can be used as food. From the viewpoint of safety, it is preferable to make the coating film edible by using a compound approved as a food additive in a dosage that satisfies the required amount.

[0070] <Average Film Thickness> The average film thickness of the coating formed by the coating liquid composition of the present invention is preferably 0.1 μm or more and 10 μm or less, more preferably 0.5 μm or more and 5 μm or less. An average film thickness of 0.1 μm or more results in good water vapor barrier properties and oxygen barrier properties. Furthermore, when used as a low-temperature damage inhibitor, the low-temperature damage inhibitory effect is good. On the other hand, an average film thickness of 10 μm or less allows the coating to be formed while maintaining the texture of the food. In the present invention, the thickness of the coating does not need to be uniform over the entire food. The average film thickness of the coating can be determined by removing the coating from the surface of the coated food, observing the cross section of the coating and the peeled portion with an electron microscope or metallurgical microscope, and measuring the thickness at 10 or more randomly selected points.

[0071] [Method for preserving food freshness] The method for preserving food freshness using the coating liquid composition of the present invention includes a step of covering food such as vegetables or fruits with the coating liquid composition. The step of covering with the coating liquid composition of the present invention is not particularly limited as long as it is a step of covering food with the coating liquid composition of the present invention, and examples thereof include direct application methods such as brush coating and curtain coating; immersion methods such as impregnation coating; and spraying methods such as spray coating. Of these, the immersion method or spraying method is preferred from the viewpoint of being able to relatively uniformly coat food having a three-dimensional shape and from the viewpoint of productivity. Note that the coating liquid composition may be solvent-free as long as it can be applied to food.

[0072] [Method for Suppressing Low-Temperature Injury in Fruits and Vegetables] When the coating film formed by the coating liquid composition of the present invention is used as an agent for suppressing low-temperature injury in fruits and vegetables, the method for suppressing low-temperature injury in fruits and vegetables includes a step of applying the agent for suppressing low-temperature injury to foods such as vegetables or fruits. The step of applying the agent for suppressing low-temperature injury in fruits and vegetables can be the same as the method for preserving the freshness of foods described above.

[0073] The coating liquid composition of the present invention may be applied to only a portion of a food product or the entire food product. From the viewpoint of shortening the drying time of the coating liquid composition and increasing the efficiency of the coating film formation process, it is preferable to apply the coating liquid composition to only a portion of the food product. In this case, the application area is preferably 10% or more of the surface area of ​​the food product, more preferably 25% or more, even more preferably 40% or more, and even more preferably 50% or more. A portion of the applied coating liquid composition may also be removed. While the removal method is not particularly limited, examples include removal by wind pressure using an air dryer. Removing excess coating liquid composition from the surface of the food product can prevent poor drying of the excess coating liquid composition. Examples of application methods include "Coating Methods" (published by Maki Shoten, 1979, by Harasaki Yuji).

[0074] [Fruits and vegetables] Fruits and vegetables that are susceptible to chilling damage include kidney beans, okra, pumpkin, cucumber, watermelon, melon, sweet potato, tomato, eggplant, bell pepper, avocado, plum, and olive; citrus fruits such as orange, grapefruit, lemon, hassaku, Natsumikan, Sudachi, and Kabosu; banana, pineapple, passion fruit, papaya, mango, and apple.

[0075] [Drying] After the coating liquid composition is applied to the food, the coating may be dried for the purpose of removing the aqueous solvent, etc. Examples of drying methods include static drying, air drying, and heat drying, but from the viewpoint of preserving the freshness of vegetables, etc., a method of drying by static drying at room temperature (20 to 25°C) or a method of air drying at room temperature is preferred.

[0076] Next, the present invention will be described in more detail with reference to examples. However, the present invention is not limited to the examples described below. Furthermore, when measuring the coating liquid composition, it is assumed that the coating liquid composition does not have any precipitate. "No precipitate" means that the coating liquid composition is stirred to a homogeneous state before sampling, and then a part or all of it is quickly transferred to a transparent container, and after leaving it at room temperature for 30 minutes, it can be visually confirmed that no precipitate has formed at the bottom.

[0077] [Evaluation of Stability of Coating Liquid Composition] The stability of the coating liquid compositions prepared in the examples and comparative examples was evaluated using the following device for transmittance immediately after preparation and after standing at 20°C for 18 days. For the following measurement results, the results of this measurement are referred to as transmittance. Device: Dispersion stability analyzer "LUMiSizer" (Nihon Luft Co., Ltd.) Measurement cell: LUM 2mm PA (polyamide) (optical path length 2mm) Rotation speed: 4000 rpm Measurement temperature: 25°C Measurement time: 30 minutes <Evaluation criteria> ○: The transmittance at a measurement position of 120mm is 60% or more, and the change in transmittance between immediately after preparation and after standing is 10%pt or less. ×: The transmittance at a measurement position of 120mm is less than 60%, and the change in transmittance between immediately after preparation and after standing is 10%pt or more.

[0078] [Viscosity Measurement] Immediately after preparation of the coating liquid composition, the viscosity was evaluated using the following device. Device: Rotational rheometer (model: Kinexus pro+) Measurement mode: Shear rate dispersion of shear viscosity Measurement temperature: 25°C Plate: Cone-plate type, diameter 40 mm, cone angle 2 degrees Shear viscosity: When the shear rate was 0 (s -1 ) to 1000 (s -1 ) and then 1000 (s -1 ) to 0.1 (s -1 In the measurement where the shear rate is reduced to 1 (s -1 ) shear viscosity at

[0079] <Differential scanning calorimetry at temperatures above 0°C> Differential scanning calorimetry was carried out under the following conditions. If no peak is observed below 0°C, the temperature may be changed from 25°C to -80°C to 100°C. Measuring device: NETZSCH DSC 204F1 Measurement method: heat flux method Temperature: 25°C → 0°C → 100°C Temperature increase / decrease rate: 10°C / min Atmosphere: nitrogen Sample preparation: The coating composition was placed in an empty aluminum pan so that the dry solid content was 1 mg, and the pan was left to dry at room temperature. It was confirmed that the weight change from the previous day was 1% or less, and a measurement sample was obtained. Reference: aluminum pan

[0080] <Differential scanning calorimetry at -80°C or higher> Differential scanning calorimetry with a measurement temperature range of -80°C or higher was carried out under the following conditions. Measurement device: NETZSCH DSC 204F1 Measurement method: heat flux method Temperature: 25°C → -80°C → 100°C Temperature increase / decrease rate: 10°C / min Atmosphere: nitrogen Sample preparation: The coating composition was placed in an empty aluminum pan so that the dry solid content was 1 mg, and the pan was left to dry at room temperature. It was confirmed that the weight change from the previous day was 1% or less, and a measurement sample was obtained. Reference: aluminum pan

[0081] [Incidence of chilling injury] Tomato fruits (variety: Momotaro (registered trademark)) were harvested at the peach ripe stage, and individuals with damage were excluded. They were then randomly divided into 20 fruits for each test. The tomato fruits were immersed in a predetermined coating solution and then dried at room temperature for 60 minutes to prepare tomato fruits treated with a chilling injury inhibitor. 20 tomato fruits were stored at 5°C and observed on days 7, 14, 21, and 28. Individuals with confirmed skin discoloration, spotted depressions, or softened flesh were counted as chilling-injured fruits, and the number of these fruits was evaluated as a percentage of the total number of 20 fruits.

[0082] [Coating Appearance] Ten cherry tomatoes were immersed in the solution containing the chilling injury inhibitor immediately after preparation, and then dried at room temperature overnight to impart the chilling injury inhibitor. The stems of the tomatoes were checked with the naked eye to see if the dried coating solution had solidified or turned white. If four or more tomatoes had solidified or turned white, they were evaluated as ×, and otherwise they were evaluated as ○.

[0083] Evaluation of Freshness Retention Avocados were used as fruits and vegetables, and the coating solutions prepared in each of the Examples and Comparative Examples were applied to them by dipping, and the coating appearance, weight retention rate, and skin color were evaluated.

[0084] (Coating Appearance) The coating solution prepared in each Example and Comparative Example was applied to an avocado by dipping, and after drying, the coating solution remaining on the avocado skin was visually evaluated for appearance defects resulting from the coating solution, according to the following criteria: <Evaluation Criteria> A: The area with poor appearance was less than 5% of the avocado skin surface, B: The area with poor appearance was 5% or more but less than 50% of the avocado skin surface, C: The area with poor appearance was 50% or more but less than 100% of the avocado skin surface.

[0085] (Weight Retention Rate) Using the weight of the avocado before storage (day 0) as the reference, the weight retention rate after 4 days of storage at 25°C and 50% RH ((weight after storage / weight on day 0) x 100(%)) was calculated. (Weight Loss Rate) Using the weight of the avocado before storage (day 0) as the reference, the weight loss rate after 4 days of storage at 25°C and 50% RH was calculated (100 - (weight after storage / weight on day 0) x 100(%)).

[0086] (Skin Color) As avocados ripen, their skin color changes from green to dark purple. This change is easy to see, and consumers commonly evaluate the freshness of avocados by their color. Therefore, a coating was formed on the surface of each avocado, and the freshness-preserving effect was confirmed by the color change. Five avocados were prepared, and the color change was evaluated according to the following criteria. The color change was evaluated according to the following criteria before storage (day 0) and after four days of storage at 25°C and 50% RH. <Evaluation Criteria> A: Either none (0%) or less than 50% of the samples had a completely dark purple surface. B: 50% or more but less than 100% of the samples had a completely dark purple surface. C: All samples had a completely dark purple surface (100%).

[0087] (Fruit Firmness) The load (N) was measured when a cylindrical plunger with a diameter of 5 mm was pressed 3 mm into an avocado at a speed of 60 mm / min. Three avocados stored at 25°C and 50% RH for 4 days were used for the measurement, and measurements were taken at three different locations near the equator for each avocado. The arithmetic mean of the obtained values ​​was taken as the fruit firmness.

[0088] The materials used are as follows: S-1670: sucrose stearate, manufactured by Mitsubishi Chemical Corporation, "Ryoto (registered trademark) Sugar Ester S-1670", HLB: 16, mono- to triester content: 97% or more, tetraester to octaester content: less than 3% S-370: sucrose stearate, manufactured by Mitsubishi Chemical Corporation, "Ryoto (registered trademark) Sugar Ester S-370", HLB: approximately 3, monoester content: approximately 20%, di-, tri-, and polyester content: approximately 80% S-570: sucrose stearate, manufactured by Mitsubishi Chemical Corporation, "Ryoto (registered trademark) Sugar Ester S-570", HLB: approximately 5, mono- to triester content: 86% or more S-1170: sucrose stearate, manufactured by Mitsubishi Chemical Corporation, "Ryoto (registered trademark) Sugar Ester S-1170", HLB: approximately 11, mono- to triester content: 94% or more S-1670: sucrose stearate, Mitsubishi Chemical Corporation "Ryoto (registered trademark) Sugar Ester S-1670", HLB: approximately 16, monoester content: approximately 75%, bound fatty acid purity: approximately 70% F-110: sucrose stearate, Dai-ichi Kogyo Seiyaku Co., Ltd. "DK Ester (registered trademark) F-110", HLB: 11 M-100: glycerin monocaprylate, Riken Vitamin Co., Ltd. "Poem (registered trademark) M-100", HLB: 7.0 Sodium behenate: NS-7, Nitto Kasei Kogyo Co., Ltd. Sodium stearate: Fujifilm Wako Pure Chemical Industries, Ltd. Sodium laurate: Fujifilm Wako Pure Chemical Industries, Ltd. Sodium octanoate: Fujifilm Wako Pure Chemical Industries, Ltd.

[0089] Example 1 A coating liquid composition was prepared by dispersing sucrose fatty acid ester (S-1670) in an aqueous solvent consisting of ethanol and water at 73°C for 30 minutes, and then rapidly cooling to 25°C using ice water. It took 30 minutes to cool to 25°C. The mass ratio of sucrose fatty acid ester / ethanol / water was 5 / 5 / 90. The stability of the coating liquid composition was evaluated by the above method, and the results are shown in Table 1.

[0090] Comparative Example 1 In Example 1, instead of rapid cooling, the produced coating liquid composition was cooled to 25° C. by air cooling. It took 3 hours to cool to 25° C. The stability of the coating liquid composition was evaluated by the above-mentioned method, and the results are shown in Table 1.

[0091] Example 2 A coating liquid composition (low-temperature damage inhibitor) was prepared by dispersing sucrose fatty acid ester (S-1170) in an aqueous solvent consisting of ethanol and water at 73°C for 30 minutes and then rapidly cooling to 25°C using ice water. It took 30 minutes to cool to 25°C. The mass ratio of sucrose fatty acid ester / ethanol / water was 5 / 5 / 90. The results of evaluation using the above method are shown in Table 1.

[0092] Example 3 In Example 2, instead of rapid cooling, the produced coating liquid composition (low-temperature damage inhibitor) was cooled to 25°C by air cooling. It took 3 hours to cool to 25°C. In addition, the coating liquid composition excluding ethanol was dispersed at 73°C for 30 minutes, and then ethanol was added, followed by cooling to prepare a coating liquid composition. The results of evaluation using the above method are shown in Table 1.

[0093] Comparative Example 2 A coating liquid composition (low-temperature damage inhibitor) was prepared by dispersing sucrose fatty acid ester (S-1170) in an aqueous solvent consisting of ethanol and water at 60°C for 30 minutes and then rapidly cooling to 25°C using ice water. It took 30 minutes to cool to 25°C. The mass ratio of sucrose fatty acid ester / ethanol / water was 0.35 / 0 / 99.65. The results of evaluation using the above method are shown in Table 1.

[0094] Test Example 1 The incidence of low-temperature damage and the appearance of the coating were evaluated by the above-mentioned method under the same conditions except that the coating liquid composition (low-temperature damage inhibitor) was not applied. The results are shown in Table 1.

[0095]

[0096] The results of Example 1 show that the coating liquid composition of the present invention, which uses rapid cooling as the cooling method, has high transmittance immediately after preparation and also after standing for 18 days, indicating high stability. On the other hand, the coating liquid composition of Comparative Example 1, which uses air cooling as the cooling method, has low transmittance immediately after preparation and the transmittance after standing for 18 days changes significantly compared to immediately after preparation, indicating that the coating liquid composition is less stable. Thus, it has become clear that a highly stable coating liquid composition can be obtained according to the present invention.

[0097] The results of Example 2 show that coating liquid compositions (chilling injury inhibitors) with a viscosity of 900 mPa·s or less provide good coating appearance. On the other hand, in Example 3, coating liquid compositions (chilling injury inhibitors) with a viscosity higher than 900 mPa·s caused some cherry tomato stems to have an unnatural appearance due to the coating, but no significant unnaturalness was observed in the fruit itself. The results of Example 2 clearly demonstrate that a highly stable coating liquid composition (chilling injury inhibitor) can be obtained that can be applied to fine areas such as cherry tomato stems with a good appearance. In other words, a viscosity of 900 mPa·s or less ensures smooth coating and a good appearance. The results of Example 2 show that the incidence of chilling injury is low when a coating liquid composition (chilling injury inhibitor) with a nonvolatile component concentration of 0.5% by mass or more is used. On the other hand, the results of Comparative Example 3 show that when the concentration of nonvolatile components in the solution containing a low-temperature damage inhibitor is lower than 0.5 mass%, the incidence of low-temperature damage is high, and compared with Test Example 1, in which no low-temperature damage inhibitor is added, the low-temperature damage inhibitor effect is about the same, but low-temperature damage is not sufficiently suppressed. Thus, it has become clear that the present invention can provide a solution containing a low-temperature damage inhibitor that can effectively suppress low-temperature damage.

[0098] Comparative Example 3: Sucrose fatty acid ester (S-1670) and sodium behenate were dispersed in water at 73°C for 30 minutes, and then the produced coating liquid composition was cooled to 25°C in an ice bath, requiring 30 minutes. The mass ratio of sucrose fatty acid ester S-1670 / sodium behenate / water was 9.8 / 0.2 / 90. The stability of the coating liquid composition was evaluated by the above method, and the results are shown in Table 2.

[0099] Comparative Example 4 Sucrose fatty acid ester (S-1670) and sodium stearate were dispersed in water at 73°C for 30 minutes, and then the produced coating liquid composition was cooled to 25°C in an ice bath, requiring 30 minutes. The mass ratio of sucrose fatty acid ester S-1670 / sodium stearate / water was 9.8 / 0.2 / 90. The stability of the coating liquid composition was evaluated by the above method, and the results are shown in Table 2.

[0100] Comparative Example 5: Sucrose fatty acid ester (S-1670) and sodium laurate were dispersed in water at 73°C for 30 minutes, and then the produced coating liquid composition was cooled to 25°C in an ice bath, requiring 30 minutes. The mass ratio of sucrose fatty acid ester S-1670 / sodium laurate / water was 9.8 / 0.2 / 90. The stability of the coating liquid composition was evaluated by the above method, and the results are shown in Table 2.

[0101] Comparative Example 6: Sucrose fatty acid ester (S-1670) and sodium octanoate were dispersed in water at 73°C for 30 minutes, and then the produced coating liquid composition was cooled to 25°C in an ice bath, requiring 30 minutes. The mass ratio of sucrose fatty acid ester S-1670 / sodium octanoate / water was 9.8 / 0.2 / 90. The stability of the coating liquid composition was evaluated by the above method, and the results are shown in Table 2.

[0102] Comparative Example 7 Sucrose fatty acid ester (S-1170) and sodium stearate were dispersed in water at 73°C for 30 minutes, and then the produced coating liquid composition was cooled to 25°C in an ice bath, requiring 30 minutes. The mass ratio of sucrose fatty acid ester S-1170 / sodium stearate / water was 8 / 2 / 90. The stability of the coating liquid composition was evaluated by the above method, and the results are shown in Table 2.

[0103] Comparative Example 8 Sucrose fatty acid ester (S-370) and sodium stearate were dispersed in water at 73°C for 30 minutes, and then the produced coating liquid composition was cooled to 25°C in an ice bath, requiring 30 minutes. The mass ratio of sucrose fatty acid ester S-370 / sodium stearate / water was 8 / 2 / 90. The stability of the coating liquid composition was evaluated by the above method, and the results are shown in Table 2.

[0104] From the results of Comparative Examples 3 to 8, it can be seen that when the coating composition contains 10.0 mass% of nonvolatile components, the change in transmittance immediately after preparation, the transmittance after standing for 18 days, or the transmittance from immediately after preparation to after standing for 18 days is large, and the stability of the coating liquid composition is low.

[0105]

[0106] Example 4 Sucrose fatty acid ester (S-1170) and glycerin fatty acid ester (M-100) were dispersed in water at 73°C for 30 minutes, and the resulting coating liquid composition was then cooled to 25°C by air cooling. It took 1 hour to cool to 25°C. The composition ratio of the coating liquid composition and the results of the evaluation using the above method are shown in Table 3. Differential scanning calorimetry at temperatures above -80°C for the coating liquid composition in Example 3, in which S-1170 was replaced with the equivalent F-110, showed one exothermic peak of 17.48 J / g with a peak top at -29.7°C in the range of -28°C to -33°C during cooling, and one exothermic peak of 19.86 J / g with a peak top at -26.0°C in the range of -32°C to -20°C during heating. In addition, there was an endothermic peak of 59.87 J / g with a peak top at 20.8°C in the range of 3°C to 24°C, and an endothermic peak of 15.98 J / g with a peak top at 27.0°C in the range of 24°C to 32°C. 3 / A 2 =49%.

[0107] Example 5 Sucrose fatty acid ester (S-1670) and glycerin fatty acid ester (M-100) were dispersed in water at 73°C for 30 minutes, and the resulting coating liquid composition was then cooled to 25°C by air cooling. It took 1 hour to cool to 25°C. The compositional ratio of the coating liquid composition and the results of evaluation using the above method are shown in Table 3. Differential scanning calorimetry at temperatures above -80°C showed an exothermic peak of 4.885 J / g with a peak top at 1.1°C in the range of 2°C to -1°C during cooling, two exothermic peaks of 32.9 J / g with a peak top at -29.6°C in the range of -29°C to -32°C, and an exothermic peak of 32.07 J / g with a peak top at -27.1°C during heating in the range of -27°C to -25°C. In addition, there was an endothermic peak of 59.91 J / g with a peak top at 20.8°C in the range of 5°C to 24°C, and an endothermic peak of 25.2 J / g with a peak top at 27.6°C in the range of 24°C to 30°C. 3 / A 2 =82%.

[0108] Example 6 Sucrose fatty acid esters (S-570 and S-1670) and glycerin fatty acid ester (M-100) were dispersed in water at 73°C for 30 minutes, and the resulting coating liquid composition was then cooled to 25°C by air cooling. It took 1 hour to cool to 25°C. The compositional ratio of the coating liquid composition and the results of evaluation using the above method are shown in Table 3. Differential scanning calorimetry at temperatures above -80°C showed an exothermic peak of 4.358 J / g with a peak top at 1.8°C in the range of 2°C to -2°C during cooling, and two exothermic peaks of 30.58 J / g with a peak top at -29.7°C in the range of -29°C to -32°C during heating, and an exothermic peak of 28.11 J / g with a peak top at -26.4°C in the range of -29°C to -24°C during heating. In addition, there was an endothermic peak of 57.56 J / g with a peak top at 21.0° C. in the range of 2° C. to 24° C., and an endothermic peak of 23.3 J / g with a peak top at 27.2° C. in the range of 24° C. to 30° C. In this case, A3 / A2=78%.

[0109] Test Example 2 The results of evaluation by the above method under the same conditions except that the coating liquid composition was not applied are shown in Table 3.

[0110]

[0111] The results shown in Table 3 demonstrate that the coating composition of the present invention is highly stable. It was also found that the coating compositions of Examples 5 and 6 allowed for stable coating treatment and provided good coating appearance. Furthermore, the avocados coated with the coating composition of the present invention showed better results in weight retention, skin color, and fruit firmness after 4 days of storage than those of Test Example 2, which was not coated with a coating composition. In other words, the results of Examples 4 to 6 and Test Example 2 demonstrate that even when a mixture of sugar fatty acid ester and glycerin fatty acid ester is used, the coating liquid composition is highly stable and can adequately maintain the freshness of the avocado. Furthermore, the A obtained from the differential scanning calorimetry results at temperatures above -80°C shows that the A 3 / A 2 It was found that the smaller the value, the higher the freshness preservation effect. 3 / A 2 Example 5, in which the percentage of the weight loss was 82.1%, was found to suppress weight loss, changes in skin color, and softening of the fruit compared to Test Example 2, which was not subjected to coating treatment. 3 / A 2 In Example 6, where A = 78.0%, the change in skin color and softening of the fruit were further suppressed. 3 / A 2 In Example 4, where the solubility was 49.2%, the results showed further suppression of changes in skin color and softening of the fruit. This is because, in differential scanning calorimetry, an exothermic peak appears when a liquid component changes to a solid component upon temperature change. Therefore, the ratio of the exothermic peak to the endothermic peak is considered to be one aspect that indicates the amount of liquid component. The film formed on the fruit surface inhibits the permeation of oxygen gas and water vapor, thereby suppressing the progression of ripening and weight loss. As the liquid component in the film component increases, the amount of gas component permeation increases. Therefore, from the perspective of maintaining freshness, a smaller ratio of the exothermic peak to the endothermic peak, which represents the liquid component, is considered more desirable. From the above, it has been demonstrated that the coating composition of the present invention is particularly suitable for use on fruits and vegetables.

[0112] According to the present invention, simply by changing the cooling method from air cooling to rapid cooling, the dispersibility of the coating liquid composition can be dramatically improved, and the dispersibility can be maintained for a long period of time. Therefore, it can be used as a coating composition for food. Furthermore, according to the present invention, a coating liquid composition (low-temperature injury inhibitor) can be obtained that exhibits a high low-temperature injury inhibitory effect on fruits and vegetables to which it is applied. Therefore, it can be used as a liquid containing an inhibitor for low-temperature injury in fruits and vegetables, and is a technology of great industrial value.

Claims

1. A coating liquid composition containing a surfactant, and having a transmittance of 60% or more for light of wavelength 875 nm measured under the following conditions using a particle size distribution measuring device for multi-sample / dispersibility evaluation at the time of preparation, and having a change in transmittance of 10% pt or less after standing at 20°C for 18 days compared to the transmittance at the time of preparation. [Measurement conditions] Cell optical path length: 2 mm, liquid volume: 0.4 ml, cell internal cross-sectional area: 16 mm 2 Measurement position: Distance from the rotation center of the particle size distribution measurement device for multiple samples and dispersibility evaluation: 120 mm; Rotation speed: 4000 rpm; Rotation time: 30 minutes 2. The coating liquid composition according to claim 1, wherein the surfactant comprises a sugar-based surfactant.

3. The coating liquid composition according to claim 1, wherein the surfactant comprises a glycerin fatty acid ester.

4. The coating liquid composition according to claim 2, wherein the sugar-based surfactant comprises a sugar fatty acid ester.

5. The coating liquid composition according to claim 1, wherein the concentration of the non-volatile components is 1 to 20% by mass.

6. The coating liquid composition according to claim 5, wherein the content of the surfactant in the non-volatile components is 60 mass % or more.

7. Shear rate 1s -1 5. The coating liquid composition according to claim 4, wherein the shear viscosity at 200° C. is 0.1 to 900 mPa·s.

8. In differential scanning calorimetry with a measurement temperature range of -80°C or higher, the total area A of exothermic peaks 3 The total area A of endothermic peaks at 0°C to 80°C 2 The coating liquid composition according to claim 4 or 7, wherein the ratio of 9. A method for applying the coating liquid composition according to claim 4.

10. A method for preserving the freshness of food, which comprises using the coating liquid composition according to claim 4.

11. A liquid containing a surfactant and a low temperature damage inhibitor, the transmittance of light at a wavelength of 875 nm is 60% or more, and the concentration of non-volatile components is 0.5% by mass or more, as measured under the following conditions using a particle size distribution measuring device. [Measurement conditions] Cell optical path length: 2 mm, liquid volume: 0.4 ml, cell internal cross-sectional area: 16 mm 2 Measurement position: Distance from the rotation center of the particle size distribution measurement device for multiple samples and dispersibility evaluation: 120 mm; Rotation speed: 4000 rpm; Rotation time: 30 minutes 12. A solution containing an agent for suppressing low temperature damage according to claim 11, in which the change in transmittance after standing at 20° C. for 18 days is 10% or less compared to the transmittance at the time of preparation.

13. A method for applying the liquid containing the agent for suppressing low temperature damage according to claim 11.

14. A method for suppressing chilling damage in fruits and vegetables, which comprises using a liquid containing the chilling damage suppressant according to claim 11.

15. A method for producing a coating liquid composition containing a surfactant, comprising heating the composition to 50 to 90°C and then cooling the composition to 25°C within 60 minutes.

16. The method for producing a coating liquid composition according to claim 15, wherein the surfactant comprises a sugar-based surfactant.

17. The method for producing a coating liquid composition according to claim 16, wherein the surfactant comprises a glycerin fatty acid ester.

18. The method for producing a coating liquid composition according to claim 15, wherein the sugar-based surfactant is a sugar fatty acid ester.

19. The method for producing a coating liquid composition according to claim 17, wherein the concentration of non-volatile components in the coating liquid composition is 1 to 20 mass %.

20. The method for producing a coating liquid composition according to claim 19, wherein the content of the surfactant in the non-volatile components is 60 mass % or more.

Citation Information

Patent Citations

  • Anti-fogging surface-treatment agent and Anti-fogging resin sheet

    JP2010037387A

  • Food Coating

    JP2020506988A

  • Coated agricultural products and corresponding methods

    WO2021178553A1

  • Composition, coated food product, coated food product manufacturing method, coating formation method, and food product shipping method

    WO2022080444A1