Method for producing dimethyl perhydro-1,4:5,8-dimethanonaphthalene-2,3-dicarboxylate

The crystallization method using specific hydrocarbons in the production of dimethyl perhydro-1,4:5,8-dimethanonaphthalene-2,3-dicarboxylate effectively addresses the challenge of impurity removal, achieving high purity and enhanced blocking resistance in the resulting crystalline composition.

WO2024214665A1PCT designated stage expired Publication Date: 2024-10-17TAOKA CHEM COMPANY
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/014221
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-12
Filing Date
2024-04-08
Publication Date
2024-10-17

AI Technical Summary

Technical Problem

Existing methods struggle to effectively remove low molecular weight impurities, specifically compounds represented by general formula (4), from dimethyl perhydro-1,4:5,8-dimethanonaphthalene-2,3-dicarboxylate due to their similar boiling points with the target compound, making purification challenging.

Method used

A method involving crystallization of dimethyl perhydro-1,4:5,8-dimethanonaphthalene-2,3-dicarboxylate from a solution containing aliphatic or aromatic hydrocarbons, with specific weight ratios, to achieve high purity and reduce residual impurities, including the use of crystallization solvents like n-heptane and aromatic hydrocarbons, and subsequent purification steps.

Benefits of technology

This method significantly reduces the content of low molecular weight impurities, resulting in a crystalline composition with dimethyl perhydro-1,4:5,8-dimethanonaphthalene-2,3-dicarboxylate as the main component, exhibiting excellent blocking resistance and high purity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024014221_17102024_PF_FP_ABST
    Figure JP2024014221_17102024_PF_FP_ABST
Patent Text Reader

Abstract

Provided is a method for producing a compound represented by formula (1), the method comprising a step for crystallizing the compound represented by formula (1) from a crystallization solution, wherein the crystallization solution contains the compound represented by formula (1), at least one compound selected from the group consisting of an aliphatic hydrocarbon having 5-10 carbon atoms and an aromatic hydrocarbon having 6-9 carbon atoms in an amount of 0.5-7 parts by weight per part by weight of the compound represented by formula (1), and a compound represented by formula (2) in a content of 0.3-6% relative to the compound represented by formula (1).
Need to check novelty before this filing date? Find Prior Art

Description

Method for producing dimethyl perhydro-1,4:5,8-dimethanonaphthalene-2,3-dicarboxylate

[0001] The present invention relates to a method for producing dimethyl perhydro-1,4:5,8-dimethanonaphthalene-2,3-dicarboxylate and a crystalline composition obtained by the method.

[0002] The following formula (1):

[0003] Perhydro-1,4:5,8-dimethanonaphthalene-2,3-dicarboxylic acid derivatives such as dimethyl perhydro-1,4:5,8-dimethanonaphthalene-2,3-dicarboxylate represented by the formula (1) are known as raw materials for polyester resins that are excellent in heat resistance, transparency, and dimensional stability (see, for example, Non-Patent Document 1). Furthermore, as a method for industrially producing a compound represented by the formula (1) (hereinafter, a "compound represented by (general) formula (○)" may be referred to as a "compound of formula (○)" (○ represents the formula number)), for example, the method described in Patent Document 1 is known, and this production method is said to be capable of producing a compound of formula (1) of relatively high purity, with the generation of impurities derived from dicyclopentadiene polymers as by-products being suppressed.

[0004] Journal of Polymer Science: Polymer Chemistry Edition, vol. 10, 3191-3204 (1972)

[0005] Japanese Patent Application Laid-Open No. 2021-161067

[0006] By combining the production method described in the above-mentioned patent document with distillation, rectification, or the like as necessary, it is possible to reduce the content of high molecular weight components among the impurities derived from the dicyclopentadiene polymer described above, while reducing the content of low molecular weight impurities, specifically, those represented by the following general formula (4):

[0007] (wherein n is 1 or 2) has a boiling point close to that of the compound of formula (1), and it has been difficult to remove it to a degree greater than that described in the above-mentioned patent documents even after repeated distillation, purification, etc.

[0008] An object of the present invention is to provide a method for producing the compound of formula (1) which can remove or further reduce the compound represented by the above general formula (4).

[0009] As a result of extensive research conducted by the present inventors to solve the above-mentioned problems, they have found that the above-mentioned problems can be solved by a method for producing a compound of formula (1) comprising the steps described below. Specifically, the present invention includes the following inventions.

[0010] [1] The following formula (1):

[0011] The method for producing a compound represented by the formula (1) includes a step of crystallizing the compound represented by the formula (1) from a crystallization solution, wherein the crystallization solution contains the compound represented by the formula (1), at least one compound selected from the group consisting of aliphatic hydrocarbons having 5 to 10 carbon atoms and aromatic hydrocarbons having 6 to 9 carbon atoms, in an amount of 0.5 to 7 parts by weight per part by weight of the compound represented by the formula (1), and a compound represented by the following formula (2):

[0012] The compound represented by formula (1) is contained in an amount of 0.3 to 6% based on the compound represented by formula (1).

[0013] [2] The following formula (1):

[0014] The content of the compound represented by the following formula (3):

[0015] The content of the compound represented by the following general formula (4):

[0016] (wherein n is 1 or 2), wherein the total content of compounds represented by the formula is 0.2% or less.

[0017] [3] The following formula (2):

[0018] The crystalline composition according to [2], wherein the content of the compound represented by the formula (I) is 3% or less.

[0019] According to the present invention, it is possible to provide a method for producing the compound of formula (1) in which the amount of the compound represented by the general formula (4) remaining is significantly reduced.

[0020] Furthermore, the compound of formula (1) obtained by the production method of the present invention contains almost no compound represented by the general formula (4). In addition, the compound represented by the general formula (4) is significantly reduced, and the compound of formula (3):

[0021] It has been found that the crystalline composition of the present invention containing a certain amount of a compound represented by formula (1) has excellent blocking resistance. Therefore, according to the present invention, it is possible to provide a crystalline composition containing the compound of formula (1) as a main component, which has excellent blocking resistance, as needed.

[0022] In the present invention, when a range is expressed as "A to B," it means A or more and B or less, unless otherwise specified. Furthermore, in the present invention, the "content" refers to the area percentage value of a gas chromatograph measured under the conditions described in the Examples section below, unless otherwise specified. Note that, since the correct content of a crystallization solution cannot be calculated from the area percentage value of the gas chromatograph of the solution, the "content relative to the compound of formula (1)" (a value calculated using the area percentage value of the gas chromatograph measured under the conditions described in the Examples section below, and the formula {(area percentage value of the compound of formula (●)) / [(area percentage value of the compound of formula (●)) + (area percentage value of the compound of formula (1))]} × 100 (● represents a formula number other than 1)) is used as the "content."

[0023] <Method for producing the compound of formula (1) of the present invention> The production method of the present invention is characterized by comprising a step of crystallizing the compound of formula (1) from a crystallization solution containing the compound of formula (1), at least one compound selected from the group consisting of aliphatic hydrocarbons having 5 to 10 carbon atoms and aromatic hydrocarbons having 6 to 9 carbon atoms, and the compound of formula (2).

[0024] The compound of formula (1) used in the production method of the present invention can be produced by a known production method. From the viewpoint of providing a crystalline composition containing the compound of formula (1) having excellent blocking resistance, the compound of formula (1) used in the crystallization may further contain the compound of formula (3), and the content of the compound of formula (3) relative to the compound of formula (1) is, for example, 1.5 to 6.5%.

[0025] The aliphatic hydrocarbon having 5 to 10 carbon atoms used in the present invention may be branched or may be an aliphatic hydrocarbon containing a halogen atom. Specific examples include n-pentane, n-hexane, 1-chlorohexane, 1-bromohexane, 3-methylpentane, 2-methylpentane, 2,3-dimethylbutane, cyclohexane, n-heptane, 1-chloroheptane, 1-bromoheptane, 2-methylhexane, 3-ethylpentane, 2,2-dimethylpentane, 2,2,3-trimethylbutane, n-octane, 2-methylheptane, 2,2-dimethylhexane, 2,2,3-trimethylpentane, 2,2,3,3-tetramethylbutane, n-nonane, 2-methyloctane, 2,2-dimethylheptane, 2,2,3-trimethylhexane, 2,2,3,3-tetramethylpentane, n-decane, 2-methylnonane, 2,2-dimethyloctane, 2,2,3-trimethylheptane, 2,2,3,3-tetramethylhexane, 4-propylheptane, and 3,4-diethylhexane. Furthermore, the aromatic hydrocarbon having 6 to 9 carbon atoms used in the present invention may contain a halogen atom, and specific examples thereof include benzene, chlorobenzene, bromobenzene, toluene, o-chlorotoluene, m-chlorotoluene, p-chlorotoluene, o-bromotoluene, m-bromotoluene, p-bromotoluene, o-xylene, m-xylene, p-xylene, α-chloro-p-xylene, 4-chloro-o-xylene, α-bromo-p-xylene, 4-bromo-o-xylene, mesitylene, etc. Among these aliphatic hydrocarbons having 5 to 10 carbon atoms and aromatic hydrocarbons having 6 to 9 carbon atoms, aliphatic hydrocarbons having 5 to 10 carbon atoms are preferred, and n-hexane, n-heptane, cyclohexane, and n-octane are more preferred. The content of at least one compound selected from the group consisting of aliphatic hydrocarbons having 5 to 10 carbon atoms and aromatic hydrocarbons having 6 to 9 carbon atoms in the crystallization solution (when two or more compounds are contained, the total content thereof) is 0.5 to 7 parts by weight, preferably 1 to 6 parts by weight, per part by weight of the compound of formula (1).

[0026] The compound of formula (2) used in the present invention may be contained in the compound of formula (1) used in the present invention, or may be synthesized separately and added to the crystallization solution when carrying out the present invention, but the present invention can be carried out more easily by using one contained in the compound of formula (1) used in the present invention. The compound of formula (1) containing the compound of formula (2) can be produced, for example, by the method of Patent Document 1.

[0027] The content of the compound of formula (2) contained in the crystallization solution must be 0.3 to 6%, preferably 0.5 to 4.5%, relative to the compound of formula (1). If the content of the compound of formula (2) is less than 0.3%, it may not be possible to reduce the compound of formula (4), whereas if it is more than 6%, the yield of the compound of formula (1) may decrease.

[0028] The method for crystallizing the compound of formula (1) can be carried out by a conventional method. Specifically, for example, the compound of formula (1), at least one compound selected from the group consisting of aliphatic hydrocarbons having 5 to 10 carbon atoms and aromatic hydrocarbons having 6 to 9 carbon atoms, and the compound of formula (2) are placed in a reactor, the internal temperature is then increased to 60 to 80°C, the compound of formula (1) is completely dissolved, and the mixture is cooled to -5 to 10°C at a rate of 0.05 to 0.3°C / min to precipitate crystals, and the obtained crystals are filtered at -5 to 10°C.

[0029] The crystallization step may be repeated as necessary. The obtained crystals may be dried as necessary, or may be subjected to conventional purification procedures such as adsorption, steam distillation, and recrystallization.

[0030] <Crystalline composition of the present invention> The crystalline composition of the present invention contains the compound of formula (1) as a main component, the compound of formula (3) as a secondary component, and is almost free of the compound of formula (4). The content of the compound of formula (1) contained in the crystalline composition of the present invention is usually 90% or more, preferably 94% or more. The upper limit is not particularly limited, but is, for example, 99.5% or less, preferably 99% or less.

[0031] The content of the compound of formula (3) contained in the crystalline composition of the present invention must be 0.2 to 5%, preferably 0.5 to 3.5%.

[0032] The content of the compound of formula (4) contained in the crystalline composition of the present invention must be 0.2% or less, and preferably 0.1% or less.

[0033] The content of the compound of formula (2) contained in the crystalline composition of the present invention is not particularly limited, but is typically 3% or less, preferably 2% or less. By reducing the content of the compound of formula (2), a crystalline composition of higher purity can be provided.

[0034] Such a crystalline composition of the present invention is characterized by excellent blocking resistance.

[0035] The present invention will be specifically described below with reference to examples, but the present invention is not limited thereto. The compound of formula (1) used in the following examples was produced based on the method described in Patent Document 1 (JP 2021-161067 A).

[0036] [1] Gas chromatography (GC) analysis Apparatus: Shimadzu Gas Chromatograph GC-2014 or equivalent Column: Agilent DB-5HT (film thickness 0.10 μm × inner diameter 0.25 mm × length 30.0 m) Column temperature: 70°C (1 min) → 10°C / min → 160°C (2 min) → 10°C / min → 210°C (2 min) → 10°C / min → 350°C (2 min) Vaporization chamber temperature: 300°C Detector temperature: 360°C Detector: FID Carrier: N 2 (50 ml / min) Combustion gas: hydrogen (40 ml / min), air (400 ml / min) Injection amount: 1 μL Sample preparation method: Approximately 100 mg of a sample was weighed into a 10 mL volumetric flask and diluted with toluene to obtain a sample liquid. The area percentage values ​​of the gas chromatograph mean the peak area values ​​of the compounds represented by the above formulas (1) to (4) expressed as percentages in the chromatogram obtained by GC analysis, after removing the toluene peak.

[0037] <Blocking Resistance Test> 80 g of a sample was placed in a zippered plastic bag, and a load of 2.0 kPa was uniformly applied thereon, followed by leaving the bag to stand for 5 days in an atmosphere at 60° C. Thereafter, the sample was removed and visually inspected for the presence or absence of blocking, and the blocking resistance was evaluated by assigning a ○ mark to a state where no blocking was observed and an × mark to a state where blocking was observed.

[0038] Example 1 To a four-neck flask equipped with a stirrer and a condenser, 250 g of the compound of formula (1) (purity (content of the compound of formula (1) as a percentage by area on gas chromatography): 94.4%, content of the compound of formula (2): 4.0% (content relative to the compound of formula (1): 4.1%), content of the compound of formula (3): 1.1% (content relative to the compound of formula (1): 1.2%), content of the compound of formula (4): 0.5% (content relative to the compound of formula (1): 0.5%)) and 500 g of n-heptane as a solvent (2 parts by weight relative to 1 part by weight of the compound of formula (1)) were added, and the contents were then heated to 50°C and stirred at the same temperature for 1 hour to completely dissolve the crystals, thereby obtaining a crystallized solution. The obtained crystallized solution was cooled at a rate of 0.2°C / min to 25°C, at which point crystals precipitated. The mixture was then stirred at the same temperature for 1 hour. The mixture was further cooled to 0°C and stirred at the same temperature for 1 hour, then filtered and dried under a reduced pressure of 1.9 kPa at an internal temperature of 45 to 50°C for 4 hours to obtain 198 g of a crystalline composition containing the compound of formula (1). The composition (content of each component) of the obtained crystalline composition is shown in Table 1. The results of the anti-blocking test are shown in Table 2.

[0039] Examples 2 to 10 Crystalline compositions were obtained in the same manner as in Example 1, except that the compound of formula (1) used, the type of solvent added, and the amount of solvent added were changed as shown in Table 1. The compositions (contents of each component) of the obtained crystalline compositions are shown in Table 1. The results of the blocking resistance test are also shown in Table 2.

[0040] Comparative Examples 1 to 4 The same procedures as in Example 1 were carried out, except that the compound of formula (1) used, the type of solvent added, and the amount of solvent added were changed as shown in Table 1. However, no crystals were precipitated even after cooling to 0°C and stirring at the same temperature for 1 hour.

[0041] Reference Examples 1 and 2 The solidified compound of formula (1) was pulverized, and the obtained powder was subjected to a blocking resistance test. The results are shown in Table 2. In Reference Example 1, the compound of formula (1) used in Example 1 was used as the solidified compound of formula (1), and in Reference Example 2, the compound of formula (1) used in Example 6 was used as the solidified compound of formula (1).

[0042]

[0043]

Claims

1. The following formula (1): The present invention relates to a method for producing a compound represented by the formula (1), the method comprising the step of crystallizing a compound represented by the formula (1) from a crystallization solution, the crystallization solution containing 0.5 to 7 parts by weight of at least one compound selected from the group consisting of the compound represented by the formula (1), aliphatic hydrocarbons having 5 to 10 carbon atoms, and aromatic hydrocarbons having 6 to 9 carbon atoms, relative to 1 part by weight of the compound represented by the formula (1), and a compound represented by the following formula (2): The compound represented by the formula (1) is contained in an amount of 0.3 to 6% based on the compound represented by the formula (1).

2. The following formula (1): The content of the compound represented by the following formula (3): The content of the compound represented by the following general formula (4): (wherein n is 1 or 2) A crystalline composition having a total content of compounds represented by the following formula:

3. The following formula (2): The crystalline composition according to claim 2, wherein the content of the compound represented by the formula (I) is 3% or less.

Citation Information

Patent Citations

  • Method of producing alicyclic dicarboxylic acid derivative

    JP2021161067A