Radiation refrigeration coating having high sunlight reflectivity, and preparation method therefor and use thereof

By using a pigment combination with specific particle size and bandgap width, combined with a film-forming agent with high hemispheric emissivity, the solar reflection and infrared emission performance of the coating are improved, the problem of insufficient reflectance of the existing coating is solved, and efficient The radiant cooling effect reduces the energy consumption of buildings and facilities.

WO2024216664A1PCT designated stage expired Publication Date: 2024-10-24SHIJIAZHUANG CHANGAN YUCAI BUILDING MATERIALS +1

Patent Information

Application Number
PCT/CN2023/091045
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-19
Filing Date
2023-04-27
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Existing commercially available heat-reflective insulation coatings have insufficient solar reflectance, resulting in a large amount of light and heat being absorbed under direct sunlight, causing buildings and open-air facilities to heat up. Moreover, existing radiant cooling technology uses expensive materials and may be difficult to promote on a large scale. .

Method used

Use pigments and fillers with a particle size of 300 nm - 2000 nm, a volume concentration of ≥50%, and a band gap greater than 4.13 eV. Alumina, magnesium oxide, boron nitride, barium sulfate, calcium carbonate and other materials are used as pigments, combined with high hemispheric emission High-efficiency film-forming agent, which reduces heat absorption by efficiently scattering or reflecting sunlight.

Benefits of technology

It achieves high solar reflectance (≥90%) and high infrared emissivity (≥90%), effectively reducing the temperature of the coated object and reducing the cooling energy consumption of buildings and facilities.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_-APPB-I100001
    Figure SMS_-APPB-I100001
  • Figure 00000013_0000
    Figure 00000013_0000
Patent Text Reader

Abstract

The present disclosure provides a radiation refrigeration coating having high sunlight reflectivity, and a preparation method therefor and the use thereof. The radiation refrigeration coating having high sunlight reflectivity is prepared from raw materials comprising a color filler, a film-forming agent, an auxiliary agent and water, wherein the median particle size of the color filler is 300-2000 nm. The radiation refrigeration coating having high sunlight reflectivity of the present disclosure can efficiently scatter or reflect sunlight radiation, such that the temperature of a coated object is lower than the ambient temperature. When the radiation refrigeration coating having high sunlight reflectivity of the present disclosure is used for coating the surface of buildings or other outdoor facilities, the energy consumption for refrigeration of commercial and residential buildings and other outdoor facilities can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Radiative cooling coating with high solar reflectance, preparation method and application thereof

[0001] This disclosure claims priority to a patent application filed with the Patent Office of China on April 19, 2023, with application number 2023104218071, entitled “Radiative cooling coating with high solar reflectance, preparation method and application thereof,” the entire contents of which are incorporated herein by reference. Technical Field

[0002] The present disclosure relates to the field of coatings, and in particular to a radiant cooling coating with high solar reflectance. The present disclosure also relates to a preparation method and application of the radiant cooling coating with high solar reflectance. Background Art

[0003] Buildings and other outdoor structures often heat up to unacceptable levels when exposed to direct sunlight. The most widely used and proven technology currently uses air conditioning for cooling, but active cooling consumes significant amounts of electricity, and the refrigerants also pose an environmental risk of increasing greenhouse gas emissions. In contrast, passive radiative cooling utilizes a radiation-transparent window into the atmosphere to release surface heat into the extremely cold outer space, eliminating the need for external energy input. This reduces the energy consumption for cooling commercial and residential buildings and other outdoor structures.

[0004] Existing commercially available heat-reflective insulation coatings typically contain heat-reflective pigments to reduce solar heat absorption, while also using low-thermal conductivity components to slow heat transfer into the building. However, these coatings lack sufficient solar reflectance and still absorb significant amounts of heat, causing temperature rise.

[0005] On the other hand, the radiative cooling technology that has emerged in recent years either uses expensive metal materials, special polymer materials, and complex metamaterial structures obtained by precision processing of semiconductor equipment, which is difficult to promote on a large scale; or uses titanium dioxide as a pigment component that strongly absorbs the ultraviolet band of sunlight. The insufficient sunlight reflectance seriously limits the cooling effect. Summary of the Invention

[0006] In view of this, the present disclosure proposes a radiant cooling coating with high solar reflectance to efficiently scatter or reflect radiation from the sun, effectively reducing the heat absorption of sunlight by the coated facilities.

[0007] To achieve the above objectives, the technical solution of the present disclosure is implemented as follows:

[0008] A radiant cooling paint with high solar reflectance, wherein the raw materials for preparing the radiant cooling paint with high solar reflectance include pigments, fillers, film-forming agents, additives, and water; the median particle size of the pigments and fillers is 300 nm to 2000 nm.

[0009] Furthermore, the volume concentration of the pigment and filler is ≥50%.

[0010] Furthermore, the band gap of the pigment is greater than 4.13 eV.

[0011] Furthermore, the pigment filler includes at least one of aluminum oxide, magnesium oxide, boron nitride, barium sulfate, calcium carbonate, and calcium hydroxide.

[0012] Furthermore, the film-forming agent includes a resin emulsion or a solid resin.

[0013] Furthermore, the resin emulsion includes pure acrylic emulsion, styrene acrylic emulsion or fluorocarbon emulsion; and the solid resin includes acrylic resin or fluorocarbon resin.

[0014] Furthermore, the auxiliary agent includes at least one of a dispersant, a wetting agent, a defoaming agent, a leveling agent, a film-forming aid, a thickener, an anti-settling agent, a preservative, a pH regulator, and an antifreeze agent.

[0015] The present disclosure also provides a method for preparing a radiative cooling coating with high solar reflectance, the method comprising the following steps:

[0016] First, some additives such as wetting agents, dispersants, defoaming agents, and pH regulators are fully mixed in water, then pigments and fillers are added and ground and dispersed at high speed, and finally the remaining additives such as film-forming agents, leveling agents, defoaming agents, thickeners and film-forming agents are added and stirred evenly at low speed to obtain a radiant cooling coating with high solar reflectance.

[0017] The present disclosure further proposes an application of a radiant cooling paint with high solar reflectance, wherein the radiant cooling paint with high solar reflectance is used to coat the exterior surfaces of buildings or other outdoor facilities.

[0018] The high solar reflectance radiant cooling coating disclosed herein can efficiently scatter or reflect solar radiation across the entire wavelength range by controlling the median particle size of the pigments and fillers within the size range of 300 nm to 2000 nm. Furthermore, increasing the pigment dosage to a volume concentration of ≥50%, and incorporating pigment compounds with a bandgap greater than 4.13 eV, can further enhance the scattering or reflection of sunlight. Furthermore, the film-forming polymer used in the high solar reflectance radiant cooling coating disclosed herein has a high hemispherical emissivity, efficiently radiating heat in the form of infrared rays, keeping the temperature of the coated object below the ambient temperature. Applying the high solar reflectance radiant cooling coating disclosed herein to the surfaces of buildings or other outdoor facilities can reduce energy consumption for cooling commercial and residential buildings and other outdoor facilities. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The accompanying drawings, which constitute part of this disclosure, are used to provide a further understanding of the disclosure. The exemplary embodiments of the disclosure and their descriptions are used to explain the disclosure and do not constitute an improper limitation of the disclosure. In the accompanying drawings:

[0020] FIG1 is a diagram showing the refrigeration performance of different embodiment and comparative example coatings over time. DETAILED DESCRIPTION

[0021] It should be noted that, unless there is any conflict, the embodiments and features in the embodiments of the present disclosure may be combined with each other.

[0022] The experimental methods in the following examples, unless otherwise specified, are conventional methods. The experimental materials used in the following examples, unless otherwise specified, were purchased from conventional biochemical reagent stores. Furthermore, unless otherwise specified in this example, the terms and processes involved in this example should be understood in accordance with general knowledge and conventional methods in the prior art.

[0023] A radiant cooling paint with high solar reflectance, wherein the raw materials for preparing the radiant cooling paint with high solar reflectance include pigments, fillers, film-forming agents, additives and water; the median particle size of the pigments and fillers is 300 nm to 2000 nm.

[0024] Pigments and fillers are essential components of coatings and cannot form films on their own. They are typically in the form of fine powders. They are uniformly dispersed in the film-forming agent and its solution through processes such as stirring, grinding, and high-speed dispersion during the coating production process. After the film-forming agent forms a coating film, the pigments and fillers are evenly dispersed in the coating film, becoming functional components that scatter or reflect sunlight. To ensure high solar reflectance, the pigments and fillers selected in this disclosure have a median particle size of 300 nm to 2000 nm, a volume concentration preferably ≥50%, and a band gap preferably >4.13 eV. The pigment and filler compound components can preferably include at least one of aluminum oxide, magnesium oxide, boron nitride, barium sulfate, calcium carbonate, and calcium hydroxide.

[0025] The present invention is meticulously designed to improve the solar reflectance of radiative cooling coatings. First, the median particle size of the pigments and fillers is controlled within a range of 300 nm to 2000 nm. Particles within this size range produce strong Mie scattering of sunlight across the entire wavelength range of 0.3-2.5 μm in the ultraviolet, visible, and near-infrared regions. Furthermore, the pigment dosage is increased to a volume concentration of ≥50%. This achieves a well-balanced volume of pigment particles relative to the volume of the resin in the coating. The close packing of the pigment particles creates some pores, and the air in these pores significantly increases the scattering of incident light. Furthermore, by using pigments with a band gap greater than 4.13 eV, their energy band structure cannot absorb light wavelengths greater than 0.3 μm, thus avoiding the UV-band heat absorption associated with titanium dioxide used in conventional coatings. The various features of the present invention are combined to efficiently scatter or reflect sunlight across the entire wavelength range, resulting in a high solar reflectance (≥90%) after drying, potentially exceeding 95%.

[0026] The film-forming agent in the high solar reflectance radiant cooling coating disclosed herein primarily serves to bond the other components together and firmly adhere to the surface of the base material, forming a complete, tough protective film. The polymer film-forming agent component employed in this disclosure has high infrared emissivity, effectively radiating heat to the outside world via infrared rays. Preferably, the film-forming agent comprises a resin emulsion or solid resin. The resin emulsion includes pure acrylic emulsion, styrene acrylic emulsion, or fluorocarbon emulsion, while the solid resin includes acrylic resin or fluorocarbon resin.

[0027] The film-forming agent exhibits high infrared emissivity within the 8-13 μm atmospheric radiation window wavelength range, and a hemispherical emissivity of ≥90% at the coating's thermal radiation wavelength, preferably exceeding 95%. Heat from the surface of an object coated with the coating can be radiated directly into outer space in the form of infrared radiation within this wavelength range under suitable weather conditions, lowering the temperature of the coated object to below ambient temperature.

[0028] The additives may be selected according to the actual usage scenario and include one or more of dispersants, wetting agents, defoaming agents, leveling agents, film-forming aids, thickeners, anti-settling agents, preservatives, pH regulators, and antifreeze agents.

[0029] Dispersants are surfactants with opposing properties, both lipophilic and hydrophilic, within their molecules. They can uniformly disperse solid and liquid particles of inorganic and organic pigments that are difficult to dissolve in liquids, reducing the time and energy required for the dispersion process. They also prevent particle sedimentation and aggregation, stabilize the pigment dispersion, modify the surface properties of the pigment particles, and adjust their mobility to form a stable suspension. Commercially available dispersants such as BYK 111, Digo 755W, Dow Corning DC-51, and Sandingjia SDJ8012 can be used as the dispersant of the present disclosure.

[0030] Wetting agents reduce the surface tension or interfacial tension of the substrate being wetted. Adding them to a coating can improve the blending of pigments, fillers, and liquid materials. Alternatively, they can help the coating spread across or even penetrate the substrate, effectively improving the coating's surface leveling. The wetting agent in this embodiment is preferably a polyether siloxane wetting agent, such as Dow CF-10, which reduces surface tension, controls surface flow, and provides excellent slip, anti-cratering, and anti-blocking properties.

[0031] Defoamers easily spread across the surface of the solution and automatically expand across the foam, entraining a layer of solution adjacent to the surface. This can cause the liquid film to thin locally, reaching a critical thickness, causing the film to rupture and the foam to break. The faster the defoamer spreads across the solution, the thinner the film becomes, accelerating the foam's destruction and enhancing its defoaming effect. Therefore, defoaming occurs, in part, due to its ease of spreading. Adsorbed defoamer molecules displace foaming agent molecules, forming a weaker film. Furthermore, the spreading process can also entrain a portion of the solution adjacent to the surface, thinning the foam film and reducing its stability, making it more susceptible to breakage.

[0032] The defoaming agent disclosed herein can preferably be an organosilicon defoaming agent. Organosilicon defoaming agents have three functions: breaking bubbles, removing bubbles, and suppressing bubbles. They also have excellent chemical stability. Due to the relatively stable Si-O bond, silicone oil has high chemical stability and is difficult to react chemically with other substances. Organosilicon defoaming agents can not only effectively break up already generated foam, but also significantly suppress foam and prevent its formation. The organosilicon defoaming agents disclosed herein can be selected from commercially available products such as Evonik TEGO 825, Maier Chemical HY-037, and Nopco NXZ.

[0033] The leveling agent disclosed in the present invention migrates to the surface of the paint film through limited compatibility, affects the surface properties of the paint film such as the interfacial tension, and enables the paint film to obtain good leveling. According to the different chemical structures of the leveling agents, there are three main categories commonly used: acrylic, silicone and fluorocarbon compounds. The leveling agent disclosed in the present invention is preferably at least one of silicone rheological additives and acrylic rheological additives. When an acrylic rheological additive is selected, a surface flow control agent such as commercially available polyacrylates such as BYK333, BYK354, Qingtian DH3170, and silicone-modified polyacrylates containing hydroxyl functional groups such as BYK3700 can be used. When a silicone rheological additive is selected, a commercially available polyether-modified polydimethylsiloxane such as Sandingjia SDJ3007 and a polyester-modified polyorganosiloxane such as Siloke 313 can be used. The compatibility of polyether- and polyester-modified silicones with resins has been greatly improved, and the surface tension can be reduced, and the ability to control surface flow, increase slip, resist shrinkage, and resist adhesion are also very good. However, polyether-modified polysiloxanes have poor thermal stability.

[0034] Film-forming aids, also known as coagulants or coalescing agents, are typically high-boiling-point solvents. They act as a temporary plasticizer, lowering the polymer's glass transition temperature (Tg). Once particle deformation and film formation are complete, the film-forming aid evaporates from the coating, restoring the polymer's Tg to its initial value. While water-based acrylic emulsions can form films normally, the addition of a film-forming aid promotes film drying and solidification. Commercially available alcohol esters may be used as the film-forming aid in this disclosure.

[0035] Thickeners can increase the viscosity of water-based paints, maintaining a uniform and stable state, and can increase the viscosity of the paint solution, facilitating construction. The thickener can preferably be an associative polyurethane thickener. Associative polyurethane thickeners are typically water-soluble polyurethanes with relatively low molecular weights. Their molecular structure contains both hydrophilic and lipophilic parts, exhibiting a certain degree of surface activity, maintaining a good coating state and excellent anti-sagging properties. The thickener disclosed herein can be selected from commercially available options such as Dow RM-8W.

[0036] The anti-settling agent added to the coating can prevent fillers or pigments from agglomerating and settling to the bottom, while also imparting thixotropy to the coating and significantly increasing its viscosity. The anti-settling agent is at least one of polyamide-modified hydrogenated castor oil, polyurea, polyamide, and organobentonite. The amide-modified hydrogenated castor oil exhibits excellent storage stability, excellent coating performance, and anti-sagging properties, with long-term storage having no significant effect on the coating gloss. The modified polyurea in N-methylpyrrolidone (BYK-410) is a rheological additive suitable for solvent-based and solvent-free coatings. This additive works by being "diluted" with a solvent or liquid resin. BYK-410 is selectively incompatible with the coating system, producing small, needle-shaped crystals at appropriate stirring speeds. The bonding forces between the crystals form a three-dimensional network structure, thereby providing the system with strong thixotropy and superior anti-settling and anti-sagging properties.

[0037] Polyamide is mostly prepared by emulsifying fatty acid amide in natural paraffin to produce polarity, and then putting it into xylene to swell and form a paste thixotropic agent in advance. Its swelling structure is network-shaped, has very good strength and heat resistance, good storage stability, has excellent anti-settling effect in coating systems, and can improve the thixotropy of coatings. Organic bentonite is mainly hectorite, which is a natural montmorillonite, and is reacted with onium salts (such as quaternary ammonium salts) to form. In coatings, organic bentonite is generally used as an anti-settling agent and thickening agent. The mechanism of its prevention of precipitation is to change the rheological properties of the system, so that it has thixotropy, thereby preventing pigment sedimentation. The anti-settling agent of the present disclosure can be selected from commercially available ones such as Arkema's MT, LV, Deqian 908, Qingtian DH6900, Disi Baron 6900-2X, Nuoyi NY-200, etc.

[0038] The use of preservatives is to prevent the coating from deteriorating during storage due to the action of microorganisms and enzymes. The preservative disclosed herein can be Acticide-RSC from Lanxess.

[0039] The present disclosure further adds a pH regulator to make the coating alkaline to a certain extent, so as to improve the compatibility of the coating with the working surface and improve the corrosion resistance of the working surface. The pH regulator of the present disclosure preferably includes at least one of 25% concentration ammonia water and AMP-95.

[0040] During storage and transportation, the produced coating may sometimes be subjected to high and low temperature fluctuations, especially in cold places such as the north. Adding antifreeze can improve the freeze-thaw stability of the coating. The antifreeze disclosed in the present invention is preferably ethylene glycol or propylene glycol.

[0041] The present disclosure also provides a method for preparing a radiative cooling coating with high solar reflectance, the method comprising the following steps:

[0042] First, some additives such as wetting agents, dispersants, defoaming agents, and pH regulators are fully mixed in water, then pigments and fillers are added and ground and dispersed at high speed, and finally the remaining additives such as film-forming agents, leveling agents, defoaming agents, thickeners and film-forming agents are added and stirred evenly at low speed to obtain a radiant cooling coating with high solar reflectance.

[0043] The present disclosure further proposes the application of a radiant cooling coating with a high solar reflectance, which is applied to the surface of buildings or other outdoor facilities, such as the exterior surfaces of buildings, grain storage warehouses, freezers, communication base stations, power facilities, etc., by roller coating, brushing, spraying, etc., to reduce the energy consumption for cooling commercial and residential buildings and other outdoor facilities.

[0044] The specific implementation scheme of the present disclosure is described in detail below. Example 1

[0045] First, 0.7 kg of dispersant, 0.1 kg of pH adjuster, 0.2 kg of defoamer, 0.2 kg of wetting agent, and 0.3 kg of anti-settling agent were weighed and thoroughly mixed in 26 kg of deionized water. Then, 38 kg of aluminum oxide with a particle size of 300 nm and 13 kg of barium sulfate with a particle size of 700 nm were added and ground and dispersed using a high-speed disperser at 1500 RPM. Finally, 0.6 kg of leveling agent, 0.7 kg of thickener, 0.2 kg of defoamer, and 20 kg of polystyrene acrylic emulsion were added and stirred at a low speed of 400 RPM. The volume concentration of the pigments and fillers in this example was 61.2%.

[0046] The radiant cooling coating obtained in this example was applied to the roof of an industrial plant by roller coating. Example 2

[0047] First, 0.5 kg of dispersant, 0.2 kg of defoamer, and 0.1 kg of preservative were weighed and thoroughly mixed in 22.3 kg of deionized water. Then, 30 kg of magnesium oxide with a particle size of 400 nm and 8 kg of calcium carbonate with a particle size of 1000 nm were added and dispersed using a high-speed disperser at 1500 RPM. Finally, 2.7 kg of pH adjuster, 22.8 kg of deionized water, 0.7 kg of thickener, 0.2 kg of defoamer, 1.5 kg of antifreeze, 1 kg of film-forming aid, and 10 kg of water-based solid acrylic resin were added and stirred at 500 RPM until uniform. The volume concentration of the pigment and filler in this example was 57.6%.

[0048] The radiant cooling coating obtained in this example was applied to the roof and exterior walls of a grain storage warehouse by brushing. Example 3

[0049] First, 0.4 kg of dispersant and 0.2 kg of defoamer were weighed and thoroughly mixed in 28.7 kg of deionized water. Then, 25 kg of 500 nm boron nitride and 8 kg of 2000 nm calcium hydroxide were added and dispersed using a high-speed disperser at 1500 RPM. Finally, 0.8 kg of film-forming aid, 0.7 kg of thickener, 0.2 kg of defoamer, and 36 kg of fluorocarbon emulsion were added and stirred at 400 RPM until uniform. The volume concentration of the pigment and filler in this example was 52.2%.

[0050] The radiant cooling coating obtained in this example was applied to the roof of an industrial plant by spraying.

[0051] Comparative Example 1

[0052] Commercially available Jiangsu Chenguang exterior wall paint was applied to the roof of the industrial plant by roller coating.

[0053] Comparative Example 2

[0054] The raw materials and preparation process of this comparative example are basically the same as those of Example 1, except that the particle sizes of aluminum oxide and barium sulfate in this comparative example are 10 μm and 5 μm, respectively.

[0055] Comparative Example 3

[0056] The raw materials and preparation process of this comparative example are basically the same as those of Example 2, except that the amounts of magnesium oxide and calcium carbonate used in this comparative example are 18 kg and 5 kg, respectively, and the volume concentration of the pigments and fillers in this comparative example is 45.1%.

[0057] The coatings of the above embodiments and comparative examples were subjected to performance tests, and the test data are shown in Table 1 and FIG1 .

[0058] Table 1 Performance test results of coatings of different embodiments and comparative examples

[0059]

[0060] The above test results show that the high solar reflectance radiant cooling coating disclosed herein achieves coating performance of high solar reflectance (≥90%) and high hemispherical emissivity (≥90%) by preferably using pigment and filler components with a particle size of 300 nm to 2000 nm and a pigment and filler volume concentration of more than 50%, thereby significantly reducing the temperature of the coated object.

[0061] The preferred embodiments of the present disclosure are described in detail above. However, the present disclosure is not limited to the specific details of the above embodiments. Within the technical concept of the present disclosure, various simple modifications can be made to the technical solutions of the present disclosure, and these simple modifications all fall within the scope of protection of the present disclosure.

[0062] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any appropriate manner without contradiction. In order to avoid unnecessary repetition, the present disclosure will not further describe various possible combinations.

Claims

1. A radiant cooling coating with high solar reflectance, characterized in that: The raw materials for preparing the radiation cooling coating with high solar reflectance include pigments, fillers, film-forming agents, additives and water; The median particle size of the pigment and filler is 300 nm - 2000 nm.

2. The radiant cooling coating with high solar reflectance according to claim 1, characterized in that: The volume concentration of the pigment and filler is ≥50%.

3. The radiant cooling coating with high solar reflectance according to claim 1, characterized in that: The bandgap width of the pigment is greater than 4.13 eV.

4. The radiant cooling coating with high solar reflectance according to claim 1, characterized in that: The pigment filler includes at least one of aluminum oxide, magnesium oxide, boron nitride, barium sulfate, calcium carbonate and calcium hydroxide.

5. The radiant cooling coating with high solar reflectance according to claim 1, characterized in that: The film former includes a resin emulsion or a solid resin.

6. The radiant cooling coating with high solar reflectance according to claim 5, characterized in that: The resin emulsion includes pure acrylic emulsion, styrene acrylic emulsion or fluorocarbon emulsion; the solid resin includes acrylic resin or fluorocarbon resin.

7. The radiant cooling coating with high solar reflectance according to claim 1, characterized in that: The auxiliary agent includes at least one of a dispersant, a wetting agent, a defoamer, a leveling agent, a film-forming aid, a thickener, an anti-settling agent, a preservative, a pH adjuster, and an antifreeze agent.

8. A method for preparing a radiant cooling coating with high solar reflectance, characterized in that: The method comprises the following steps: First, some additives such as wetting agent, dispersant, defoamer, and pH adjuster are fully mixed in water, then pigments and fillers are added and ground and dispersed at high speed, and finally the remaining additives such as film-forming agent, leveling agent, defoamer, thickener and film-forming agent are added and stirred evenly at low speed to obtain a radiant cooling coating with high solar reflectance.

9. Application of a radiant cooling coating with high solar reflectance, characterized in that: The radiation cooling paint with high solar reflectance is used for coating on the surface of buildings or other open-air facilities.

Citation Information

Patent Citations

  • Radiation cooling coating as well as preparation method and application thereof

    CN109988467A

  • Selective radiation refrigeration coating and composite material and application method thereof

    CN110317521A

  • Radiation refrigeration coating material and applications thereof

    CN110684463A

  • Radiation refrigeration coating and preparation method thereof

    CN115449252A

  • MgO coating for radiation cooling and preparation process thereof

    CN115651460A

Cited By

  • Layered environment-friendly water-based radiation refrigeration coating composition

    CN122356912A