Semiconductor light-receiving element

The semiconductor light-receiving element with a multi-step mesa structure and InGaAs contact layer design addresses the trade-off between sensitivity and speed by reducing light absorption loss and heat generation, enhancing both light-receiving sensitivity and operating speed.

WO2024218941A1PCT designated stage expired Publication Date: 2024-10-24NT T INC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/015784
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-20
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Semiconductor light-receiving elements face a trade-off between light-receiving sensitivity and operating speed due to the thickness of the light-absorbing layer and carrier travel distance, with conventional structures experiencing light absorption loss and heat generation issues, particularly with InGaAs contact layers, which compromise sensitivity and high-speed operation.

Method used

A semiconductor light-receiving element with a multi-step mesa structure and a mirror layer formed within an opening in a contact layer of InGaAs, where the contact layer with a bandgap energy larger than the photon energy does not absorb light, and a metal electrode in ohmic contact with the contact layer, separating the light and carrier paths to reduce absorption loss and heat generation.

Benefits of technology

This configuration enhances light-receiving sensitivity and operating speed by minimizing light absorption loss and heat generation, thereby improving the overall performance of the semiconductor light-receiving element.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023015784_24102024_PF_FP_ABST
    Figure JP2023015784_24102024_PF_FP_ABST
Patent Text Reader

Abstract

This semiconductor light receiving element 100 comprises: a contact layer 102 including p-type InP; a light absorption layer 103 formed on the contact layer 102; a contact layer 104 including n-type InP formed on the light absorption layer 103; a contact layer 105 formed on the contact layer 104 and including n-type InGaAs and having an opening; a metal electrode 107 in ohmic contact with the contact layer 105; and a mirror layer 106 formed on the contact layer 104 in the opening. The contact layer 104 has band gap energy greater than photon energy of incident light, and the contact layer 105 forms ohmic contact with the metal electrode 107 in a more stable manner than the contact layer 104.
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor photodetector

[0001] The present disclosure relates to a semiconductor light receiving element.

[0002] A semiconductor photodiode is an element that converts an optical signal into an electrical signal by utilizing the property of semiconductors that absorbs light and generates carriers (electrons and holes), and is widely used in optical communications as an optical receiver and a terahertz electromagnetic wave source. To improve the performance of semiconductor photodiodes in optical communications systems, the challenge is to achieve both high light sensitivity and high operating speed, but there is a fundamental trade-off between light sensitivity and operating speed.

[0003] The trade-off between the light sensitivity and operating speed of semiconductor light-receiving elements is mainly explained by the film thickness of the light absorption layer and the travel distance of carriers. Increasing the thickness of the light absorption layer increases the amount of incident light absorbed, which increases the number of carriers generated and contributes to current, thereby increasing light sensitivity. However, increasing the thickness of the light absorption layer increases the travel distance of the generated carriers to reach the electrode, thereby decreasing operating speed. As optical communication systems become faster, there is a demand for increased operating speed, but increasing operating speed decreases light sensitivity and shortens the transmission distance.

[0004] A conventional technology that achieves both high operating speed and high light sensitivity is a back-illuminated semiconductor photodetector described in Non-Patent Document 1. The semiconductor photodetector in Non-Patent Document 1 increases the amount of light absorbed by forming a mirror layer to allow incident light to travel back and forth, and then absorbing the incident light twice, on the outward and return paths, in a light absorption layer. This allows for increased light sensitivity without increasing the thickness of the light absorption layer, achieving both improved light sensitivity and operating speed.

[0005] Nada, Masahiro, et al., "Inverted p-down pin photodiodes exceeding 70-GHz bandwidth featuring low operating bias voltage of 2 V," 2020 European Conference on Optical Communications (ECOC), IEEE, 2020Beling, Andreas, et al., "High-power, high-linearity photodiodes," Optica, Vol. 3, Issue 3, 2016, pp. 328-338

[0006] However, in conventional structures, incident light is lost during its round-trip travel, resulting in ineffective utilization of the incident light. Conventional semiconductor photodetectors have a layered structure in which a first contact layer, a light absorption layer, a second contact layer, and a third contact layer are stacked in this order on an InP substrate, with a mirror layer and a metal electrode formed on the third contact layer. Incident light enters the device from the InP substrate side and passes through the absorption layer twice: once on its outward journey and once on its return journey after being reflected by the mirror layer. InP-based semiconductor photodetectors typically use InGaAs for the third contact layer in contact with the mirror layer (Non-Patent Document 2). Because InGaAs absorbs light, the light intensity decreases as the incident light is reflected. Carriers generated by light absorption in the third contact layer are converted into heat and do not contribute to photosensitivity, and an increase in the device's temperature leads to degradation of photosensitivity and high-speed operation.

[0007] InGaAs can achieve a uniform and stable ohmic contact and has high heat resistance at the contact with metal, which prevents deterioration of characteristics due to diffusion of electrode metal material caused by heating during manufacturing. For this reason, it is impossible to avoid using an InGaAs contact layer, which causes light absorption loss, in terms of device operating characteristics.

[0008] The present disclosure has been made in view of the above, and has an object to provide a semiconductor light-receiving element that has higher light-receiving sensitivity and achieves both improved light-receiving sensitivity and improved operating speed.

[0009] A semiconductor light-receiving element according to one aspect of the present disclosure comprises a first semiconductor layer of a first conductivity type, a light absorption layer formed on the first semiconductor layer, a second semiconductor layer of a second conductivity type formed on the light absorption layer, a third semiconductor layer of the second conductivity type formed on the second semiconductor layer and having an opening, a metal electrode in ohmic contact with the third semiconductor layer, and a mirror layer formed on the second semiconductor layer in the opening, wherein the second semiconductor layer has a band gap energy larger than the photon energy of incident light, and the third semiconductor layer forms ohmic contact with the metal electrode more stably than the second semiconductor layer.

[0010] According to the present disclosure, it is possible to provide a semiconductor light-receiving element that has higher light-receiving sensitivity and achieves both improved light-receiving sensitivity and improved operating speed.

[0011] Fig. 1 is a cross-sectional view showing an example of the configuration of a semiconductor light-receiving element of a first embodiment. Fig. 2 is a diagram showing the relationship between a light absorption layer, a contact layer, and optical loss in a conventional semiconductor light-receiving element. Fig. 3 is a cross-sectional view showing an example of the configuration of a semiconductor light-receiving element of a second embodiment. Fig. 4 is a cross-sectional view showing an example of the configuration of a semiconductor light-receiving element of a third embodiment. Fig. 5 is a cross-sectional view showing an example of the configuration of a semiconductor light-receiving element of a fourth embodiment.

[0012] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. In the description, the same components are designated by the same reference numerals and redundant description will be omitted.

[0013] First Embodiment FIG. 1 is a cross-sectional view showing an example of the configuration of a semiconductor light-receiving element (photodiode) according to a first embodiment. The semiconductor light-receiving element 100 shown in FIG. 1 has a layer structure in which a contact layer 102 containing p-type InP, a light-absorbing layer 103 containing undoped InGaAs, a contact layer 104 containing n-type InP, and a contact layer 105 containing n-type InGaAs are sequentially stacked on an InP substrate 101. The layer structure is a multi-step mesa structure in which the contact layers 104 and 105 are processed into the smallest mesa, followed by the light-absorbing layer 103 and contact layer 102, which are then gradually enlarged. The contact layer 105 has an opening that exposes the contact layer 104. The semiconductor light-receiving element 100 also includes a mirror layer 106 formed on the upper surface of the contact layer 104 within the opening, and a metal electrode 107 formed on the upper surface of the contact layer 105 and making ohmic contact with the contact layer 105.

[0014] The contact layer 105 forms an ohmic contact with the metal electrode 107 more stably than the contact layer 104. Carriers generated in the light absorption layer 103 pass through the contact layers 104 and 105 and reach the metal electrode 107. The distance that the carriers travel in the light absorption layer 103 is the same as in the prior art, and therefore the operating speed is not affected.

[0015] The mesa width (element diameter) Wc of the contact layer 104 is preferably 6 μm or more. The smaller the width Wa of the contact layer 105, the greater the effect of suppressing incident light loss, but the width Wa of the contact layer 105 needs to be 1 μm for the manufacturing process. In addition, for high-speed operation, the contact resistance between the contact layer 105 and the metal electrode 107 needs to be about 10 Ω or less. The contact resistivity should be 2×10 -6 Ωcm 2 If the width Wa of the contact layer 105 is 1 μm and the contact layer 105 is annular, then in order to make the contact resistance about 10 Ω or less, the mesa width Wc of the contact layer 104 needs to be 6 μm or more.

[0016] The thickness of the contact layer 105 is preferably 2% or more of the thickness of the light absorption layer 103. However, for stable ohmic contact, the contact layer 105 needs to have a thickness of 10 nm.

[0017] Signal light is incident on the semiconductor photodetector 100 from the bottom (the InP substrate 101 side) in the figure. The incident light is absorbed by the light absorption layer 103. The light that is not absorbed passes through the contact layer 104, is reflected by the mirror layer 106, and is absorbed again by the light absorption layer 103 on the return path. Since the contact layer 104 uses InP, which has a band gap energy larger than the photon energy of the incident light, the contact layer 104 does not absorb light. The contact layer 105 uses InGaAs, which has a band gap energy smaller than the photon energy of the incident light, but since the incident light is reflected by the mirror layer 106 formed in the opening of the contact layer 105, no light absorption loss occurs in the contact layer 105.

[0018] In this embodiment, the path of incident light is separated from the path of carriers responsible for electrical conduction by providing an opening in the contact layer 105 and forming the mirror layer 106 in the opening, thereby realizing both suppression of light absorption loss in the contact layer 105 containing InGaAs and good ohmic contact using the contact layer 105 containing InGaAs.

[0019] The structure of this embodiment suppresses heat generation in the contact layer 105, contributing to suppression of deterioration of characteristics. In conventional structures, carriers generated by light absorbed in the contact layer recombine and are ultimately converted into heat. Since an increase in temperature of the element leads to deterioration of light-receiving sensitivity and high-speed operation, suppressing light absorption in the contact layer can suppress heat generation in the element, which is effective in suppressing deterioration of the element's operating characteristics.

[0020] Next, an example of a method for manufacturing the semiconductor light receiving element 100 of this embodiment will be described.

[0021] First, a contact layer 102 containing p-type InP, a non-doped InGaAs (light absorption layer 103), a contact layer 104 containing n-type InP, and a contact layer 105 containing n-type InGaAs are deposited in this order on an InP substrate 101. Well-known deposition methods such as metalorganic chemical vapor deposition (MOCVD) and molecular beam epitaxy (MBE) can be used.

[0022] Subsequently, a metal electrode 107 is formed on the contact layer 105 by photolithography and an electron beam evaporation apparatus. The metal electrode 107 can be made of a metal having a layer structure of Ti / Pt / Au, for example.

[0023] Next, a resist pattern is formed to open the inside of the metal electrode 107, and the metal electrode 107 and the contact layer 105 are removed by wet etching to form an opening. The opening is not limited to a circular shape as long as it can selectively expose the contact layer 104.

[0024] Subsequently, a mirror layer 106 is formed on the contact layer 104 exposed in the opening. The mirror layer 106 can be formed by evaporating Au, for example.

[0025] Subsequently, the contact layer 104 , the light absorption layer 103 , and the contact layer 102 are processed in order to a desired size by photolithography and wet etching, thereby forming a semiconductor light receiving element on the InP substrate 101 .

[0026] The contact layer 105 does not affect the optical absorption loss, so it can be formed thicker than before. By making the contact layer 105 thicker, it is possible to prevent the contact layer 105 from being lost or degraded during the process, thereby expanding the process margin.

[0027] Next, the effect when there is no contact layer containing InGaAs (hereinafter referred to as an InGaAs contact layer) in the path of incident light will be described.

[0028] 2 is a diagram showing the relationship between the light absorption layer, the InGaAs contact layer, and the optical loss in a conventional semiconductor light receiving element. In FIG. 2, the horizontal axis represents the thickness of the light absorption layer, and the vertical axis represents the optical loss in the InGaAs contact layer. The relationship between the thickness of the light absorption layer and the optical loss in the InGaAs contact layer is shown when the thickness of the InGaAs contact layer is set to 10 nm, 50 nm, 100 nm, and 200 nm. The absorption coefficient of InGaAs is 10 4 / cm. From Figure 2, it can be seen that, for example, when the thickness of the light absorption layer is 500 nm and the thickness of the InGaAs contact layer is 50 nm, 5.8% of the light is absorbed by the InGaAs contact layer. In other words, it is thought that if there is no InGaAs contact layer in the path of the incident light, the loss due to light absorption of 5.8% can be suppressed. Furthermore, when the InGaAs contact layer is 10 nm or more, or when the thickness of the InGaAs contact layer is 2% or more of the thickness of the light absorption layer, the effect of suppressing light absorption by 1% or more can be obtained.

[0029] Second Embodiment A semiconductor light-receiving element 200 according to a second embodiment will be described with reference to FIG.

[0030] 3 has a layer structure in which a contact layer 102 containing p-type InP, a light absorption layer 103 containing undoped InGaAs, a contact layer 104 containing n-type InP, and a contact layer 105 containing n-type InGaAs are stacked in this order on an InP substrate 101. The contact layer 105 has an opening that exposes the contact layer 104. The semiconductor light receiving element 200 also has a mirror layer 106 formed on the upper surface of the contact layer 104 within the opening, and a metal electrode 107 in ohmic contact with the contact layer 105.

[0031] In the second embodiment, the metal electrode 107 is formed on the outer side surface of the contact layer 105. By forming the contact layer 105 so that its height is thicker than its width, the contact area between the contact layer 105 and the metal electrode 107 can be increased, thereby reducing the contact resistance. The metal electrode 107 and the contact layer 104 may or may not be in contact with each other. The other configurations and effects are the same as those of the first embodiment.

[0032] Next, an example of a method for manufacturing the semiconductor light receiving element 200 of this embodiment will be described.

[0033] First, a semiconductor layer structure is grown by crystal growth, as in the first embodiment. In the second embodiment, since the metal electrode 107 is formed on the side surface of the contact layer 105, it is preferable to form the contact layer 105 thicker than in the first embodiment.

[0034] Subsequently, a pattern of the contact layer 105 having a desired width is formed by photolithography and dry etching.

[0035] Next, a resist pattern is formed to open the outer side surface of the contact layer 105, and the metal electrode 107 is formed on the outer side surface of the contact layer 105 by sputtering, and then the metal electrode 107 is formed by lift-off. The metal electrode 107 can be made of a metal having a layer structure of, for example, Ti / Pt / Au.

[0036] Subsequently, a mirror layer 106 is formed on the contact layer 104 exposed in the opening. The mirror layer 106 can be formed by evaporating Au, for example.

[0037] Subsequently, the contact layer 104 , the light absorption layer 103 , and the contact layer 102 are processed in order to a desired size by photolithography and wet etching, thereby forming a semiconductor light receiving element on the InP substrate 101 .

[0038] Third Embodiment A semiconductor light-receiving element 300 according to a third embodiment will be described with reference to FIG.

[0039] 4 has a layer structure in which a contact layer 102 containing p-type InP, a light absorption layer 103 containing undoped InGaAs, a contact layer 104 containing n-type InP, and a contact layer 105 containing n-type InGaAs are stacked in this order on an InP substrate 101. The contact layer 105 has an opening that exposes the contact layer 104. The semiconductor light receiving element 300 also has a mirror layer 106 formed on the upper surface of the contact layer 104 within the opening, and a metal electrode 107 in ohmic contact with the contact layer 105.

[0040] In the third embodiment, the metal electrode 107 is formed on the outer side surface of the contact layer 105 as well as on the top surface of the contact layer 105. The side surface and top surface of the contact layer 105 contact with the metal electrode 107, thereby increasing the contact area and reducing the contact resistance. The metal electrode 107 and the contact layer 104 may or may not contact each other. The other configurations and effects are the same as those of the first embodiment.

[0041] The semiconductor light-receiving element 300 of the third embodiment can be fabricated by the same method as in the second embodiment. To form the metal electrode 107 on the side and top surfaces of the contact layer 105, a resist pattern is formed with openings on the outer side and top surfaces of the contact layer 105, and the metal electrode 107 is deposited by sputtering and then lifted off. The metal electrode 107 can be made of a metal having a layer structure of, for example, Ti / Pt / Au.

[0042] Fourth Embodiment A semiconductor light-receiving element 400 according to a fourth embodiment will be described with reference to FIG.

[0043] 5 has a layer structure in which a contact layer 102 containing p-type InP, a light absorption layer 103 containing undoped InGaAs, a contact layer 104 containing n-type InP, and a contact layer 105 containing n-type InGaAs are stacked in this order on an InP substrate 101. The contact layer 105 has an opening that exposes the contact layer 104. The semiconductor light receiving element 400 also has a mirror layer 106 formed on the upper surface of the contact layer 104 within the opening, and a metal electrode 107 in ohmic contact with the contact layer 105.

[0044] In the fourth embodiment, the metal electrode 107 is formed on the inner side surface, outer side surface, and top surface of the contact layer 105. The side surface and top surface of the contact layer 105 contact the metal electrode 107, thereby increasing the contact area and reducing the contact resistance. The metal electrode 107 and the contact layer 104 may or may not contact each other. The other configurations and effects are the same as those of the first embodiment.

[0045] The semiconductor light-receiving element 400 of the fourth embodiment can be fabricated by the same method as in the second embodiment. To form the metal electrode 107 on the side and top surfaces of the contact layer 105, a resist pattern is formed with openings on the side and top surfaces of the contact layer 105, and the metal electrode 107 is deposited by sputtering and then lifted off. The metal electrode 107 can be made of a metal having a layer structure of, for example, Ti / Pt / Au.

[0046] As described above, according to this embodiment, the semiconductor photodetector 100, 200, 300, 400 includes the contact layer 102 containing p-type InP, the light absorption layer 103 formed on the contact layer 102, the contact layer 104 containing n-type InP formed on the light absorption layer 103, the contact layer 105 containing n-type InGaAs formed on the contact layer 104 and having an opening, the metal electrode 107 in ohmic contact with the contact layer 105, and the mirror layer 106 formed on the contact layer 104 in the opening. The contact layer 104 has a band gap energy larger than the photon energy of incident light, and the contact layer 105 forms an ohmic contact with the metal electrode 107 more stably than the contact layer 104. This separates the path of incident light from the path of carriers responsible for electrical conduction, thereby providing the semiconductor photodetector 100, 200, 300, 400 with higher photosensitivity and improved photosensitivity and operating speed.

[0047] All of the embodiments are applicable to semiconductor light-receiving elements of not only the PIN type but also the avalanche type.

[0048] 100, 200, 300, 400 Semiconductor light receiving element 101 InP substrate 102 Contact layer 103 Light absorption layer 104 Contact layer 105 Contact layer 106 Mirror layer 107 Metal electrode

Claims

1. A semiconductor light-receiving element comprising: a first semiconductor layer of a first conductivity type; a light absorption layer formed on the first semiconductor layer; a second semiconductor layer of a second conductivity type formed on the light absorption layer; a third semiconductor layer of a second conductivity type formed on the second semiconductor layer and having an opening; a metal electrode in ohmic contact with the third semiconductor layer; and a mirror layer formed on the second semiconductor layer in the opening, wherein the second semiconductor layer has a band gap energy larger than the photon energy of incident light, and the third semiconductor layer forms ohmic contact with the metal electrode more stably than the second semiconductor layer.

2. A semiconductor light receiving element according to claim 1, wherein the metal electrode is formed on the upper surface of the third semiconductor layer.

3. A semiconductor light receiving element according to claim 1 or 2, wherein the metal electrode is formed on a side surface of the third semiconductor layer.

4. A semiconductor light receiving element according to claim 1, wherein the film thickness of said third semiconductor layer is 2% or more of the film thickness of said light absorbing layer or 10 nm or more.

5. A semiconductor light receiving element according to claim 1, wherein the second semiconductor layer contains n-type InP, and the third semiconductor layer contains n-type InGaAs.

Citation Information

Patent Citations

  • Photo-semiconductor device

    JP1987062566A

  • Compound semiconductor light receiving element and fabrication thereof

    JP1996204224A

  • Semiconductor Photodiode And Method Of Manufacture Thereof

    US20090242933A1

  • Semiconductor light receiving element

    WO2020209243A1