Electrically conductive sheet, resin molded article, and manufacturing method for same

The conductive sheet configuration with a protective sheet and controlled expansion settings addresses the peeling and disconnection issues of wires in three-dimensional shapes, ensuring stability and successful molding of conductive sheet products.

WO2024219110A1PCT designated stage expired Publication Date: 2024-10-24NISSHA PRINTING CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/009317
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-17
Filing Date
2024-03-11
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Conductive sheets with embedded wires face peeling and disconnection issues when formed into three-dimensional shapes due to differences in elongation between the film and wire, leading to structural instability and potential breakage.

Method used

A conductive sheet configuration featuring a base sheet with a conductive pattern, a protective sheet covering the pattern, and a bending area where the wire crosses, with linear expansion settings to absorb expansion differences, ensuring the protective sheet adheres to the base sheet and prevents peeling, even when bent.

Benefits of technology

This configuration effectively prevents wire peeling and disconnection during bending, allowing for stable formation of three-dimensional shapes and successful injection molding of resin molded products without wire failure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024009317_24102024_PF_FP_ABST
    Figure JP2024009317_24102024_PF_FP_ABST
Patent Text Reader

Abstract

[Problem] The purpose of the present invention is to provide an electrically conductive sheet, a resin molded article, and a manufacturing method for the same, wherein peeling or severing of a wire that occurs due to configuring the electrically conductive sheet as a three-dimensional shape is prevented. [Solution] A film heater 10 that is an electrically conductive sheet comprises: a base sheet 11 that has a rectangular shape in planar view; an electrically conductive pattern 13 that is formed by an electrically conductive wire 12 which has been fixed on the base sheet 11; and a protective sheet 21 that is formed on the base sheet 11 so as to cover the electrically conductive pattern 13. The film heater 10 is, for example, incorporated into an emblem or a bumper of an automobile and used for melting snow. In an end section of the base sheet 11, there is a bending region A that extends in a belt shape in the short direction of the base sheet 11. The electrically conductive pattern 13 is a meander-shaped pattern that is formed in a single continuous line so as to repeatedly make U-turns, which are aligned at a fixed width, to the left and right in the short direction of the base sheet 11, and such that the intervals in the long direction are equal. This pattern constitutes a heater part 14.
Need to check novelty before this filing date? Find Prior Art

Description

Conductive sheet, resin molded product, and manufacturing method thereof

[0001] There is a film heater, which is a conductive sheet having a conductive pattern made of conductive wires formed on one surface of the base sheet. The conductive wires are embedded in the surface of the base sheet over their entire length by ultrasonic welding (see, for example, Patent Document 1).

[0002] Conventionally, a conductive sheet having a conductive pattern on a base sheet has been proposed.

[0003] When a conventional conductive sheet such as that described above is formed into a three-dimensional shape, the elongation of the film and the elongation of the wire are different, which can cause the wire to peel off from the base sheet at the bent portion or cause the wire to break.

[0004] The present invention has been made to solve the above-mentioned problems, and aims to provide a conductive sheet, a resin molded product, and a manufacturing method thereof that prevent wire peeling and breakage that occur when the product is formed into a three-dimensional shape.

[0005] In order to achieve the above object, the first invention comprises a base sheet having a bending region, a conductive pattern formed by conductive wires fixed onto the base sheet, and a protective sheet formed on the base sheet so as to cover the conductive pattern, wherein a portion of the wires crosses the bending region and is set so that when the base sheet and the protective sheet are bent in the bending region, the linear expansion of the outer sheet is greater than the linear expansion of the inner sheet.

[0006] By configuring it in this manner, the difference in expansion and contraction between the outer and inner sheets when the conductive sheet is bent is absorbed, so that even when the conductive sheet is bent, the protective sheet adheres to the base sheet, preventing the wire from peeling off.

[0007] In the second invention, when the conductive sheet is bent in the bending region, the length of the outer surface of the sheet that is on the inside is set to be equal to the length of the inner surface of the sheet that is on the outside.

[0008] With this configuration, stress caused by the difference in expansion between the protective sheet and the base sheet is less likely to be applied to the contact surface between them, so peeling of the wire can be reliably prevented.

[0009] The third invention is a configuration of the first invention, in which the linear expansion of the base sheet is A1, the linear expansion of the protective sheet is A2, the thickness of the conductive sheet is d, the bent portion of the base sheet when the conductive sheet is bent in the bending region is regarded as an arc with its radius R, the forming temperature when the conductive sheet is bent in the bending region is T1, and the room temperature at that time is T2, are set to have the relationship of the following formula (1) or (2): (1) When A1<A2 (2) When A1>A2

[0010] When configured in this manner, if there is a difference in expansion between the base sheet and the protective sheet when the conductive sheet is bent, the conductive sheet will warp toward the sheet with the smaller linear expansion, and this warping can be used to assist in forming the conductive sheet into a three-dimensional shape.

[0011] A fourth aspect of the present invention is the structure of the first aspect of the present invention, wherein the conductive pattern is made of a single continuous wire and includes a heater portion and a connection terminal portion.

[0012] With this configuration, the wires are protected by the protective sheet and adhere closely to the base sheet, so that the wires will not come off even if the conductive sheet is bent.

[0013] A fifth invention is a resin molded product comprising a preform body in which the conductive sheet of the first invention is bent in a bending region, and a resin molded body laminated on the front surface, back surface, or both surfaces of the preform body.

[0014] With this configuration, the preform body from which the wires are not peeled is laminated on the resin molded body, resulting in a resin molded product from which the wires are not peeled.

[0015] The sixth invention is a method for manufacturing a resin molded product, comprising the steps of: placing the conductive sheet described in claim 1 on one of the cavity surfaces of an injection molding mold having a fixed mold and a movable mold that forms a cavity between the fixed mold and the movable mold by clamping; clamping the injection molding mold; injecting molten resin into the cavity to form a resin molded product while simultaneously fixing the conductive sheet to the surface of the resin molded product; and opening the injection molding mold and removing the resin molded product.

[0016] With this configuration, the wires are protected by the protective sheet and adhere to the base sheet even when the conductive sheet is bent during injection molding, so that a resin molded product can be injection molded in which the wires do not peel off.

[0017] A seventh aspect of the present invention is a method for producing a resin molded product according to the sixth aspect of the present invention, which is a preform obtained by bending the conductive sheet according to the first aspect of the present invention at a bending region.

[0018] With this configuration, a preform body with no peeled wires is inserted into the injection molding die, so that a resin molded product with no peeled wires can be obtained.

[0019] An eighth invention is a method for manufacturing a resin molded product, comprising the steps of: preparing a preform body in which the conductive sheet of the first invention is bent at a bending region; and adhering a resin molded body having a surface shape corresponding to the shape of the front, back, or both surfaces of the preform body to the front, back, or both surfaces of the preform body.

[0020] With this configuration, the preform with no broken wires is laminated onto the resin molded product, so that a resin molded product with no broken wires can be obtained.

[0021] According to this invention, when the conductive sheet is formed into a three-dimensional shape, the conductive wires fixed to the conductive sheet can be prevented from peeling off or breaking.

[0022] 1 is a schematic plan view showing a film heater according to a first embodiment and a second embodiment of the present invention. FIG. 2 is a schematic cross-sectional view taken along the line II-II shown in FIG. 1. FIG. 2(1) is a schematic cross-sectional view taken along the line II-II when the film heater shown in FIG. 1 according to the first embodiment of the present invention is bent in a bending region, and FIG. 2(2) is a schematic cross-sectional view taken along the line II-II when the film heater shown in FIG. 1 according to the second embodiment of the present invention is bent in a bending region. FIG. 3 is a diagram showing a process for producing a film heater molded product. FIG. 4 is a diagram showing another process for producing a film heater molded product.

[0023] Next, an embodiment of the present invention will be described with reference to the drawings.

[0024] Referring to FIG. 1 , a film heater 10, which is a conductive sheet according to a first embodiment of the present invention, includes a base sheet 11 having a rectangular shape in a plan view, a conductive pattern 13 formed by conductive wires 12 fixed to the base sheet 11, and a protective sheet 21 formed on the base sheet 11 so as to cover the conductive pattern 13. The film heater 10 is used, for example, in an automobile emblem or bumper for snow melting. An end of the base sheet 11 has a curved region A extending in a strip shape in the lateral direction of the base sheet 11. The conductive pattern 13 is a meandering pattern formed in a single stroke with repeated U-turns aligned at a constant width on both sides of the lateral direction of the base sheet 11 and equidistantly spaced apart in the longitudinal direction. This pattern constitutes a heater section 14. A portion of the wire 12 crosses the curved region A, and both ends of the wire 12 meet at a single point in the pattern, extending outward from the outer edge of the corner of the base sheet 11 in parallel with a constant distance. This portion constitutes the connection terminal portion 15. Depending on the product to which the film heater 10 is applied, a decorative layer, a transfer layer, an adhesive layer, or other functional layers may be laminated on the front and back surfaces of the film heater 10. The base sheet 11 has a rectangular shape, but may have other shapes, such as an irregular shape, that match the shape of the final product.

[0025] Referring to FIG. 2 , the wire 12 is fixed onto the base sheet 11 so that a portion of its cross section is embedded in the base sheet 11. A protective sheet 21 is superimposed on the base sheet 11 so as to cover the wire 12. The wire 12 is sandwiched between the base sheet 11 and the protective sheet 21. A preferred method for embedding the wire 12 into the base sheet 11 is, for example, a method that utilizes the principle of ultrasonic fusion to embed the wire 12 into the base sheet 11. When performing ultrasonic fusion, a wiring drawing device can be used that can melt the surface of the base sheet 11 made of a thermoplastic resin while unwinding the wire 12, thereby embedding the wire 12 into the base sheet 11. By embedding the wire 12 into the base sheet 11, the conductive pattern 13 is positioned on the base sheet 11.

[0026] 3A is a schematic cross-sectional view taken along line II-II of the film heater 10 according to the first embodiment of the present invention, in which the protective sheet 21 is bent downward at the bending region A with the protective sheet 21 facing upward. The base sheet 11 is stretched by the bending, and the length of the outer surface 30 of the base sheet 11 after bending is longer than the length of the outer surface 30 of the base sheet 11 before bending.

[0027] The film heater 10 according to the first embodiment of the present invention can be configured so that when it is bent by applying heat in the bending region A, the length of the outer surface 30 of the base sheet 11 on the inside and the length of the inner surface 41 of the protective sheet 21 on the outside become equal. Specifically, they expand due to thermal expansion between room temperature and the glass transition point, and this expansion difference is used to make the lengths equal. Furthermore, when exposed to a temperature exceeding the glass transition point, the molecular arrangement changes and the shape is maintained.

[0028] With this configuration, stress caused by the difference in expansion between the protective sheet 21 and the base sheet 11 is less likely to be applied to the contact surface between them, so peeling of the wire 12 can be reliably prevented.

[0029] In the first embodiment of the present invention, the linear expansion of the base sheet 11 is A1, the linear expansion of the protective sheet 21 is A2, the thickness of the film heater 10 is d, the bent portion of the base sheet 11 when the film heater 10 is bent is considered to be an arc with a radius of R (see FIG. 3(1)), the forming temperature when bent in the bent region is T1, and the room temperature at that time is T2, so that the relationship of the following formula (1) can be satisfied. (1)

[0030] By setting it in this way, when the film heater 10 is bent, the difference in expansion between the base sheet 11 and the protective sheet 21 causes the film heater 10 to warp toward the base sheet 11, which has a smaller linear expansion, and this warping can be used to assist in forming the conductive sheet into a three-dimensional shape.

[0031] A thermoplastic resin sheet such as polycarbonate, acrylic resin, or ABS resin is used for the base sheet 11. For example, if a thermoplastic resin sheet made of the same type as that of the resin molded body 17 is used, it becomes easier to adhere the base sheet 11 to the resin molded body 17. In particular, it is preferable to use a thermoplastic resin sheet that has excellent formability, mechanical strength, flexibility, and weather resistance.

[0032] The thickness of the base sheet 11 is preferably three to four times the diameter of the wire 12. If the thickness is less than three times the diameter of the wire 12, the embedding of the wire 12 into the base sheet 11 will result in the shape of the wire 12 being visible on the side of the base sheet 11 opposite the side on which the wire 12 is embedded, which may cause cracks in the decorative layer laminated on that side or may result in a poor appearance when that side becomes the exterior of a molded product. If the thickness is more than four times the diameter of the wire 12, it will be difficult to form the film heater 10 into a three-dimensional shape. For example, for a wire 12 with a diameter of 0.2 mm, the thickness of the base sheet 11 is preferably 0.6 mm to 0.8 mm.

[0033] A thermoplastic resin sheet such as polyethylene terephthalate, polyethylene, or polypropylene is used for the protective sheet 21. For example, if a thermoplastic resin sheet of the same type as that of the resin molded body 17 is used, it becomes easier to adhere the protective sheet 21 to the resin molded body 17. In particular, it is preferable to use a thermoplastic resin sheet that has excellent formability, mechanical strength, flexibility, and weather resistance.

[0034] The thickness of the protective sheet 21 is preferably 1 to 2 times the diameter of the wire 12. If the thickness is less than 1 time the diameter of the wire 12, the shape of the wire 12 will be visible when the protective sheet 21 covers the wire 12 fixed on the base sheet 11, which may cause cracks in the decorative layer laminated on the protective sheet 21 or may result in a poor appearance when the protective sheet 21 forms the exterior of a molded product. If the thickness is more than twice the diameter of the wire 12, it will be difficult to mold the film heater 10 into a three-dimensional shape. For example, in the case of a wire 12 with a diameter of 0.2 mm, the thickness of the protective sheet 21 is preferably 0.2 mm to 0.4 mm.

[0035] Various conductive metal materials can be selected for the wire 12 depending on the intended use and purpose of the molded product to be manufactured. Examples include pure copper and copper alloys containing copper with or without silver, lead, tin, aluminum, nickel, beryllium, zirconium, etc. In particular, pure copper with low resistance and alloys with excellent mechanical strength are preferable.

[0036] The diameter of the wire 12 is preferably 0.05 mm to 0.2 mm, and more preferably 0.15 mm to 0.2 mm. If it is thinner than 0.05 mm, the resistance value will be high, which will reduce heater performance, and there is a risk of wire breakage when forming into a three-dimensional shape. If it is thicker than 0.2 mm, it will be difficult to form the film heater 10 into a three-dimensional shape. The length of the wire 12 can be determined according to the pattern shape of the conductive pattern 13, etc.

[0037] The embedding depth of the wire 12 into the base sheet 11 is 1 / 3 of the thickness of the base sheet 11 and is about 2 / 5 to 4 / 5 of the diameter of the wire 12, preferably 1 / 2 to 3 / 4.

[0038] A material having properties suited to the intended use and purpose of the molded product to be manufactured is used for the resin molded body 17. Examples include polycarbonate, acrylonitrile butadiene styrene, and PC-ABS alloy.

[0039] When the film heater 10 according to the first embodiment of the present invention is used in an automobile emblem or bumper, it is suitable to use polycarbonate for the base sheet 11, polyethylene terephthalate for the protective sheet 21, a silver-containing copper alloy for the wire 12, and polycarbonate for the resin molded body 17 if the part requires light transmission, or PC-ABS if the part requires strength.

[0040] Next, a second embodiment of the present invention will be described with reference to the drawings, focusing on the differences from the previous embodiment.

[0041] The film heater 10, which is a conductive sheet according to the second embodiment of the present invention, is the same as the film heater 10 according to the first embodiment except for the relationship between the linear expansion of the base sheet 11 and the protective sheet 21 and the material of the protective sheet 21.

[0042] 3(2) is a schematic cross-sectional view taken along line II-II of the film heater 10 according to the second embodiment of the present invention, in which the base sheet 11 is bent downward at the bending region A with the base sheet 11 facing upward. The base sheet 11 is stretched by bending, and the length of the outer surface of the base sheet 11 after bending is longer than the length of the outer surface of the base sheet 11 before bending.

[0043] The film heater 10 according to the second embodiment of the present invention can be configured so that when it is bent at the bending region A, the length of the outer surface of the protective sheet 21 on the inside and the length of the inner surface of the base sheet 11 on the outside are equal to each other.

[0044] With this configuration, stress caused by the difference in expansion between the protective sheet 21 and the base sheet 11 is less likely to be applied to the contact surface between them, so peeling of the wire 12 can be reliably prevented.

[0045] In the second embodiment of the present invention, the linear expansion of the base sheet 11 is A1, the linear expansion of the protective sheet 21 is A2, the thickness of the film heater 10 is d, the bent portion of the base sheet 11 when the film heater 10 is bent is considered to be an arc with a radius of R (see FIG. 3 (2)), the forming temperature when bent in the bent region is T1, and the room temperature at that time is T2, and the relationship of the following formula (2) can be satisfied. (2)

[0046] By setting it in this way, when the film heater 10 is bent, the difference in expansion between the base sheet 11 and the protective sheet 21 causes the film heater 10 to warp toward the protective sheet 21, which has a smaller linear expansion, and this warping can be used to assist in forming the conductive sheet into a three-dimensional shape.

[0047] An inorganic resin sheet containing a negative thermal expansion filler or the like is used for the protective sheet 21. In particular, it is preferable to use an inorganic resin sheet that has excellent formability, mechanical strength, flexibility, and weather resistance.

[0048] The thickness of the protective sheet 21 is preferably 1 to 2 times the diameter of the wire 12. If the thickness is less than 1 time the diameter of the wire 12, the shape of the wire 12 will be visible when the protective sheet 21 covers the wire 12 fixed on the base sheet 11, which may cause cracks in the decorative layer laminated on the protective sheet 21 or may result in a poor appearance when the protective sheet 21 forms the exterior of a molded product. If the thickness is more than twice the diameter of the wire 12, it will be difficult to mold the film heater 10 into a three-dimensional shape. For example, in the case of a wire 12 with a diameter of 0.2 mm, the thickness of the protective sheet 21 is preferably 0.2 mm to 0.4 mm.

[0049] Next, a process for manufacturing the film heater molded product 18, which is a resin molded product, will be described.

[0050] 4(1), the injection molding die 22 includes a movable die 23 and a fixed die 24. In this embodiment, the die on the left side of the injection molding die 22 is the movable die 23, and the die on the right side is the fixed die 24. The movable die 23 moves horizontally (left and right on the plane of the paper in FIG. 4(1)) to approach or move away from the fixed die 24. The movable die 23 includes a cavity line surface 26 that corresponds to the shape of the preform 16 obtained by bending the film heater 10 in the bending region A, and the fixed die 24 includes a resin flow path 25 for injecting molten resin 28. With the injection molding die 22 open to the left and right, the preform 16 is placed on the cavity line surface 26 of the movable die 23.

[0051] 4(2), the fixed mold 24 and the movable mold 23 are clamped together to form a cavity 27 between the fixed mold 24 and the movable mold 23. Molten resin 28 is injected into the cavity 27 from the resin flow path 25 of the fixed mold 24 to form the resin molded body 17, and at the same time, the film heater molded product 18 is molded. The molded film heater molded product 18 is cooled and solidified while still clamped together.

[0052] 4(3), the injection mold 22 is opened to remove the film heater molded product 18. In this manner, the film heater molded product 18 is produced in which the preform body 16 and the resin molded body 17 are molded simultaneously by injection molding.

[0053] 5, a resin molded body 17 corresponding to the shape of the outer sheet surface of the bent preform body 16 is laminated onto the bent outer sheet surface of the preform body 16. If necessary, an adhesive layer may be interposed between the preform body 16 and the resin molded body 17 to bond them together. For the adhesive layer, for example, an acrylic, urethane, epoxy, rubber, polyester, cellulose, emulsion, or other adhesive may be used. In this manner, a film heater molded product 18 is produced.

[0054] As described above, in the film heater 10 configured as above, when the film heater 10 is formed into a three-dimensional shape, the wire 12 adheres closely to the base sheet 11, thereby preventing peeling or breakage of the wire 12 due to bending. Furthermore, the method for manufacturing a molded film heater product 18 using the film heater 10 configured as above makes it possible to manufacture a molded film heater product 18 in which the wire 12 is not broken.

[0055] In the first and second embodiments of the present invention, the wire 12 is embedded directly in the base sheet 11, but another layer, such as an adhesive layer, may be formed on the base sheet 11 and the wire 12 may be fixed to that layer.

[0056] Furthermore, in the first and second embodiments of the present invention, the protective sheet 21 is directly adhered to the base sheet 11, but another layer, such as an adhesive layer, may be formed on the base sheet 11, and the protective sheet 21 may be adhered to that layer.

[0057] Furthermore, in the first and second embodiments of the present invention, one conductive pattern 13 is provided on the base sheet 11 by one wire 12, but as long as the wire 12 is configured to cross the bending region, the number of wires and the number and shape of the patterns are not limited to those of the above embodiments.

[0058] Furthermore, in the first and second embodiments of the present invention, a bent region is provided at the end of the film heater 10, but the wire 12 may be located elsewhere on the base sheet 11 as long as a portion of the wire 12 crosses the bent region.

[0059] Furthermore, in the first and second embodiments of the present invention, in another process for producing the film heater molded product 18, the resin molded body 17 is laminated on the bent outer sheet surface of the preform body 16, but the resin molded body 17 can be laminated on the front surface, back surface, or both surfaces of the preform body 16.

[0060] REFERENCE SIGNS LIST 10 Film heater 11 Base sheet 12 Wire 13 Conductive pattern 14 Heater portion 15 Connection terminal portion 16 Preform body 17 Resin molded body 18 Film heater molded product 21 Protective sheet 22 Injection molding mold 23 Movable mold 24 Fixed mold 26 Cavity surface 27 Cavity 30, 40 Outer surface 31, 41 Inner surface A Bending region

Claims

1. A conductive sheet comprising: a base sheet having a bending region; a conductive pattern formed by conductive wires fixed onto the base sheet; and a protective sheet formed on the base sheet so as to cover the conductive pattern, wherein a portion of the wires crosses the bending region, and when the conductive sheet is bent at the bending region, the linear expansion of the outermost sheet of the base sheet and the protective sheet is set to be larger than the linear expansion of the innermost sheet.

2. A conductive sheet as claimed in claim 1, in which the length of the outer surface of the sheet that is on the inside when the conductive sheet as claimed in claim 1 is bent in the bending region is set to be equal to the length of the inner surface of the sheet that is on the outside.

3. The conductive sheet according to claim 1, wherein the linear expansion of the base sheet is A1, the linear expansion of the protective sheet is A2, the thickness of the conductive sheet according to claim 1 is d, the bent portion of the base sheet when the conductive sheet is bent in the bending region is regarded as a circular arc with a radius of R, the forming temperature when the conductive sheet is bent in the bending region is T1, and the room temperature at that time is T2, are set to have the relationship of the following formula (1) or (2): (1) When A1<A2 (2) When A1>A2 4. The conductive sheet according to claim 1, wherein the conductive pattern is made of a single continuous wire and includes a heater portion and a connection terminal portion.

5. A resin molded product comprising a preform obtained by bending the conductive sheet according to claim 1 at the bending region, and a resin molded body laminated on the front surface, back surface, or both surfaces of the preform.

6. A method for manufacturing a resin molded product, comprising the steps of: placing the conductive sheet according to claim 1 on any cavity surface of an injection molding die having a fixed die and a movable die which forms a cavity between the fixed die and the movable die by clamping; clamping the injection molding die; injecting molten resin into the cavity to form a resin molded body while simultaneously adhering the conductive sheet to a surface of the resin molded body; and opening the injection molding die and removing the resin molded body.

7. The method for producing a resin molded product according to claim 6, wherein the conductive sheet is a preform that is bent at the bending region.

8. A method for manufacturing a resin molded product, comprising the steps of: preparing a preform by bending the conductive sheet according to claim 1 at the bending region; and adhering a resin molded product having a surface shape corresponding to the shape of the front, back or both surfaces of the preform.

Citation Information

Patent Citations

  • Spiral-pipe-shaped heater and manufacture thereof

    JP1999074066A

  • Planar heater for signal light and ice or snow adhesion prevention method using the same

    JP2017004918A

  • Film heater

    JP2019169417A

  • Conductive circuit sheet integrated molded product and manufacturing method of the same