Composition for living body
A composition of α-monoalkyl glyceryl ether, phospholipids, and alcohols or polyalkylene oxides addresses the inadequacy of existing pain relief compositions by forming a durable film with enhanced elastic modulus and strain resistance, effectively suppressing pain in mucous membranes and skin.
Patent Information
- Application Number
- PCT/JP2024/014935
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-21
- Filing Date
- 2024-04-15
- Publication Date
- 2024-10-24
AI Technical Summary
Existing compositions for suppressing pain in mucous membranes and skin, such as those used for stomatitis, fail to form a durable film when exposed to water, lacking sufficient elastic modulus and strain resistance, leading to inadequate pain relief.
A composition comprising α-monoalkyl glyceryl ether, phospholipids, and alcohols or polyalkylene oxides, with specific mass ratios and content percentages, forms a film with excellent elastic modulus and strain resistance when contacted with water, enhancing bioadhesion and pain relief.
The composition effectively forms a durable film with improved elastic modulus and strain resistance, providing sustained pain relief on mucous membranes and skin, even when exposed to water-containing environments.
Smart Images

Figure JPOXMLDOC01-APPB-T000001 
Figure JPOXMLDOC01-APPB-T000002
Abstract
Description
Biocomposition
[0001] The present invention relates to a composition for biological use.
[0002] Conventionally, there has been a need to suppress pain caused by inflammation in mucous membranes and skin. For example, cancer patients are prone to developing stomatitis due to cancer treatment affecting the oral mucosa. Stomatitis is inevitable when anti-cancer drug treatment involves the administration of drugs that are likely to cause stomatitis, or when radiation therapy for head and neck cancer (cancer in the area from the head to the neck) involves direct exposure of the oral mucosa to radiation. The pain of stomatitis can be so severe that it can be difficult to eat.
[0003] Symptomatic treatment for stomatitis involves applying patches directly to the affected area (e.g., Afterseal (R) 25 μg, Taisho Toyama Pharmaceutical Co., Ltd.; active ingredient: triamcinolone acetonide), ointments to be applied to the affected area (e.g., Dexaltin Oral Ointment, Nippon Kayaku Co., Ltd.; active ingredient: dexamethasone), and sprays to be sprayed on the affected area (e.g., Sulcoat (R) Examples include capsules for external use 50 μg, manufactured by Teijin Pharma Limited; active ingredient: beclomethasone propionate.
[0004] However, when eating a meal, the patch attached to the affected area may come off or the ointment or spray applied to the affected area may be lost, making it impossible to sufficiently suppress the pain of stomatitis.
[0005] Patent Document 1 discloses, as a composition capable of exerting anti-inflammatory effects and the like, an alkyl glyceryl ether-blended composition comprising (A) one or more alkyl glyceryl ethers selected from the group consisting of chimyl alcohol, batyl alcohol, and selachyl alcohol, (B) lecithin, (C) a nonionic surfactant, and (D) a polyhydric alcohol, wherein (A) / (B)=10 / 1 to 10 / 10, [(A)+(B)] / (C)=10 / 1 to 10 / 10, and [(A)+(B)] / (D)=10 / 5 to 10 / 100, and the blending amount of (A) in the composition is 5 to 50 mass%.
[0006] JP 2010-059066 A
[0007] Materials used in living organisms are often used in environments where they come into contact with water-containing aqueous fluids such as atmospheric water and body fluids. As described above, such materials are required to be resistant to removal from the surface of living organisms in such environments. To achieve such performance, specifically, the film formed by contacting the composition for living organisms with water must have excellent elastic modulus and strain resistance. The present inventors have studied the composition described in Patent Document 1 and found that the elastic modulus and strain resistance of the film do not meet the desired levels, and further improvement is required.
[0008] Therefore, an object of the present invention is to provide a composition for use in living organisms that can form a film when it comes into contact with water, and that the film formed has excellent elastic modulus and strain resistance.
[0009] As a result of extensive research into solving the above problems, the present inventors have found that the problems can be solved by the following configuration.
[0010] [1] A composition for living organisms comprising: a compound X selected from the group consisting of α-monoalkyl glyceryl ethers and α-monoalkenyl glyceryl ethers; a phospholipid; and a compound Y selected from the group consisting of an alcohol having 4 or less carbon atoms and a polyalkylene oxide, wherein the content of compound Y is 1 to 10% by mass relative to the total mass of compound X and the phospholipid. [2] The composition for living organisms according to [1], wherein compound X is selected from the group consisting of selachyl alcohol, batyl alcohol, and chimyl alcohol. [3] The composition for living organisms according to [1] or [2], wherein compound X is selachyl alcohol. [4] The composition for living organisms according to any one of [1] to [3], wherein the mass ratio of the content of compound X to the content of the phospholipid is 70 / 30 to 50 / 50. [5] The composition for living organisms according to any one of [1] to [4], wherein the content of water is 0 to 10% by mass relative to the total mass of the composition for living organisms. [6] The composition for living organisms according to any one of [1] to [5], wherein the content of the compound X is 50% by mass or more relative to the total mass of the composition for living organisms. [7] The composition for living organisms according to any one of [1] to [6], which forms an inverted hexagonal columnar phase upon water or moisture absorption. [8] The composition for living organisms according to any one of [1] to [7], which is for use on the skin or mucous membrane.
[0011] According to the present invention, it is possible to provide a composition for use in a living body, which can form a film when it comes into contact with water, and the film formed has excellent elastic modulus and strain resistance.
[0012] The present invention will be described in detail below. The following description of the components may be based on representative embodiments of the present invention, but the present invention is not limited to such embodiments.
[0013] In this specification, a numerical range expressed using "to" means a range that includes the numerical values written before and after "to" as the lower and upper limits. Furthermore, in this specification, when two or more types of a component are present, the "content" of that component means the total content of those two or more components. In this specification, in a numerical range described in stages, the upper or lower limit value described in a certain numerical range may be replaced with the upper or lower limit value of another numerical range described in stages. Furthermore, in a numerical range described in this specification, the upper or lower limit value described in a certain numerical range may be replaced with a value shown in the Examples. In this specification, a combination of two or more preferred embodiments is a more preferred embodiment.
[0014] [Composition for Biological Use] The composition for biological use of the present invention is described in detail below. The composition for biological use of the present invention comprises a compound X selected from the group consisting of α-monoalkyl glyceryl ethers and α-monoalkenyl glyceryl ethers, a phospholipid, and a compound Y selected from the group consisting of an alcohol having 4 or less carbon atoms and a polyalkylene oxide, wherein the content of compound Y is 1 to 10% by mass based on the total mass of compound X and the phospholipid.
[0015] While the reason why the composition for living bodies having the above-described configuration can solve the problems of the present invention is not entirely clear, the inventors speculate as follows. The following speculation does not limit the mechanism by which the effect is achieved. In other words, mechanisms other than those described below are also within the scope of the present invention. The composition for living bodies of the present invention contains a compound X selected from the group consisting of α-monoalkyl glyceryl ethers and α-monoalkenyl glyceryl ethers, and a compound Y selected from the group consisting of phospholipids, alcohols having 4 or fewer carbon atoms, and polyalkylene oxides. This allows the composition for living bodies to form a film (preferably a film exhibiting a liquid crystal phase) that exhibits excellent bioadhesion and strength (e.g., elastic modulus and strain resistance) upon contact with water. In particular, it is speculated that the composition for living bodies of the present invention contains the above components in a specific content ratio, resulting in an excellent elastic modulus and strain resistance of the formed film. Hereinafter, a film that is excellent in at least one of the elastic modulus and strain resistance of the formed film upon contact with water is also referred to as having "excellent effects of the present invention." Below, each component that the composition for living bodies of the present invention may contain is described in detail.
[0016] [Compound X Selected from the Group Consisting of α-Monoalkyl Glyceryl Ethers and α-Monoalkenyl Glyceryl Ethers] The composition for living organisms of the present invention comprises compound X selected from the group consisting of α-monoalkyl glyceryl ethers and α-monoalkenyl glyceryl ethers. The number of carbon atoms in the alkyl group in the α-monoalkyl glyceryl ether is preferably 6 to 32, more preferably 10 to 24, and even more preferably 16 to 18. The number of carbon atoms in the alkenyl group in the α-monoalkenyl glyceryl ether is preferably 6 to 32, more preferably 10 to 24, and even more preferably 16 to 18. The number of double bonds in the alkenyl group is not particularly limited as long as it is one or more, but is preferably 1 to 3, and more preferably 1. The alkyl group and alkenyl group may each be linear or branched, but linear groups are preferred. Examples of the alkyl and alkenyl groups include oleyl, stearyl, cetyl, lauryl, tridecyl, myristyl, pentadecyl, and monoisostearyl groups. Compound X is also preferably an α-monoalkenyl glyceryl ether.
[0017] Examples of compound X include selachyl alcohol (α-monooleyl glyceryl ether), batyl alcohol (α-monostearyl glyceryl ether), chimyl alcohol (α-monocetyl glyceryl ether), α-monolauryl glyceryl ether, α-monotridecyl glyceryl ether, α-monomyristyl glyceryl ether, α-monopentadecyl glyceryl ether, and α-monoisostearyl glyceryl ether. Selachyl alcohol, batyl alcohol, or chimyl alcohol is preferred, and selachyl alcohol is more preferred. Of these, compound X is preferably selected from the group consisting of selachyl alcohol, batyl alcohol, and chimyl alcohol, and selachyl alcohol is more preferred.
[0018] Compound X may be used alone or in combination of two or more. Compound X may be a combination of an α-monoalkyl glyceryl ether and an α-monoalkenyl glyceryl ether. From the viewpoint of superior strain resistance and liquid viscosity, the content of compound X is preferably 30% by mass or more, more preferably 45% by mass or more, and even more preferably 50% by mass or more, relative to the total mass of the composition for biological use. Furthermore, from the viewpoint of superior elastic modulus, strain resistance, and film formation rate, the content of compound X is preferably 90% by mass or less, more preferably 80% by mass, even more preferably 70% by mass or less, and particularly preferably 65% by mass or less, relative to the total mass of the composition for biological use. The content of compound X refers to the total content of the α-monoalkyl glyceryl ether and the α-monoalkenyl glyceryl ether contained in the composition for biological use. The liquid viscosity is the viscosity of the composition for biological use before contact with water. A low liquid viscosity is preferable from the viewpoint of ease of application and excellent usability. In terms of use, it is also preferable that the composition for living organisms of the present invention has a high film formation rate. The above film formation rate may also correspond to the formation rate of a liquid crystal film (a film containing a liquid crystal phase), i.e., the formation rate of a liquid crystal phase.
[0019] [Phospholipid] The composition for living bodies of the present invention contains a phospholipid. The phospholipid is not particularly limited as long as it is a lipid having a phosphate ester structure in its molecular structure, but representative examples include glycerophospholipids having a glycerin skeleton and sphingophospholipids having a sphingosine skeleton. Both glycerophospholipids and sphingophospholipids have an acyl group derived from a fatty acid in the molecule.
[0020] The number of carbon atoms in the acyl group of the phospholipid is not particularly limited, but is preferably 12 to 22, and more preferably 16 to 18. The hydrocarbon group excluding the carbonyl group of the acyl group is preferably a saturated or unsaturated chain hydrocarbon group having 11 to 21 carbon atoms, and more preferably a saturated or unsaturated chain hydrocarbon group having 15 to 17 carbon atoms. Specific examples of the hydrocarbon group include CH 3 (CH 2 ) 14 -, CH 3 (CH 2 )7 CH=CH(CH 2 ) 7 - and CH 3 (CH 2 ) 4 (CH=CHCH 2 ) 2 (CH 2 ) 6 When a phospholipid has two or more acyl groups in the molecule, the acyl groups may be the same as or different from one another.
[0021] Examples of phospholipids include phosphatidylcholine, lysophosphatidylcholine, phosphatidylethanolamine, phosphatidylinositol, phosphatidic acid, phosphatidylglycerol, sphingomyelin, and sphingoethanolamine.
[0022] The phospholipid preferably contains an ionic phospholipid, since this improves the water absorption rate of the composition for living bodies of the present invention and facilitates the formation of a columnar layer with a large domain size. The water absorption rate refers to the rate at which the composition for living bodies of the present invention absorbs water or moisture. A fast water absorption rate is preferable, since it improves the film formation rate and the effects of the present invention. Examples of ionic phospholipids include phospholipids having a cationic moiety and an anionic moiety in one molecule, and specific examples include phosphatidylcholine. Phosphatidylcholine has N-type cations derived from choline as the cationic moiety. + and P—O derived from phosphoric acid as the anion moiety. - The acyl group of phosphatidylcholine is palmitic acid (CH 3 (CH 2 ) 14 COOH), oleic acid (CH 3 (CH 2 ) 7 CH=CH(CH 2 ) 7 COOH), or linoleic acid (CH 3 (CH 2 ) 4 (CH=CHCH 2 ) 2(CH 2 ) 6 COOH) are preferred.
[0023] Specific examples of phosphatidylcholine include PO phosphatidylcholine (phosphatidylcholine having an acyl group derived from palmitic acid at position 1 (α-position), an acyl group derived from oleic acid at position 2 (β-position), and choline at position 3 (γ-position)), DL phosphatidylcholine (phosphatidylcholine having an acyl group derived from linoleic acid at position 1 (α-position), an acyl group derived from linoleic acid at position 2 (β-position), and choline at position 3 (γ-position)), and dipalmitoylphosphatidylcholine.
[0024] The phospholipid preferably contains phosphatidylcholine. When the phospholipid contains phosphatidylcholine, the content of phosphatidylcholine is preferably 50% by mass or more, more preferably 75% by mass or more, and even more preferably 90% by mass or more, based on the total mass of the phospholipid. The upper limit of the content of phosphatidylcholine relative to the total mass of the phospholipid is not particularly limited, and may be 100% by mass, or in many cases, 99% by mass or less. In addition, a composition containing phospholipid may be used in the preparation of a composition for living organisms, and specifically, for example, a composition containing phosphatidylcholine may be used. The content of phosphatidylcholine in the composition containing phosphatidylcholine is preferably 75% by mass or more, more preferably 90% by mass or more, based on the total mass of the composition containing phosphatidylcholine.
[0025] The phospholipid may be used alone or in combination of two or more. In terms of achieving superior effects of the present invention, the mass ratio of the content of compound X to the content of phospholipid (compound X / phospholipid) is preferably 95 / 5 to 20 / 80, more preferably 80 / 20 to 40 / 60, even more preferably 70 / 30 to 50 / 50, and particularly preferably 65 / 35 to 55 / 45. In terms of achieving superior effects of the present invention, the content of phospholipid is preferably 5 to 80% by mass, more preferably 20 to 50% by mass, and even more preferably 30 to 45% by mass, relative to the total mass of the composition for living organisms.
[0026] [Compound Y Selected from the Group Consisting of Alcohols Having 4 or Less Carbon Amounts and Polyalkylene Oxides] The composition for living organisms of the present invention contains compound Y selected from the group consisting of alcohols having 4 or less carbon atoms and polyalkylene oxides. The alcohols having 4 or less carbon atoms and polyalkylene oxides can function as solvents for compound X and phospholipids. The alcohols having 4 or less carbon atoms and polyalkylene oxides are preferably biocompatible.
[0027] <Alcohols with 4 or less carbon atoms> Alcohols with 4 or less carbon atoms are compounds in which at least one hydroxy group is bonded to an aliphatic hydrocarbon group with 4 or less carbon atoms. If the alcohol has 5 or more carbon atoms, its function as a solvent for compound X and phospholipids decreases, resulting in insufficient solubility, which is undesirable. The aliphatic hydrocarbon group with 4 or less carbon atoms may be linear, branched, or cyclic, but linear or branched is preferred. The number of carbon atoms in the alcohol with 4 or less carbon atoms is not particularly limited as long as it is 4 or less, but 3 or less is preferred. The lower limit of the number of carbon atoms in the alcohol with 4 or less carbon atoms is 1 or more, preferably 2 or more, and more preferably 3 or more. The number of hydroxy groups in the alcohol with 4 or less carbon atoms is not particularly limited as long as it is 1 or more, but 1 or 2 is preferred.
[0028] Examples of alcohols having 4 or less carbon atoms include monoalcohols such as ethanol, propanol, isopropanol, and butanol; glycols (dialcohols) such as ethylene glycol, propylene glycol, butylene glycol, and 1,3-butylene glycol; and glycerol. Ethanol, isopropanol, ethylene glycol, 1,3-butylene glycol, or propylene glycol is preferred, and ethanol, 1,3-butylene glycol, or propylene glycol is more preferred.
[0029] <Polyalkylene Oxide> Polyalkylene oxide is a polymer having oxyalkylene groups as repeating units. The terminal of the polyalkylene oxide may be either an alkyl group or a hydroxy group. The polyalkylene oxide may have a hydroxy group, and the number of hydroxy groups is not particularly limited. The number of carbon atoms in the alkylene group of the polyalkylene oxide is not particularly limited, but 1 to 4 is preferable. Examples of oxyalkylene groups include oxyethylene groups and oxypropylene groups. The polyalkylene oxide may be either linear or branched. The multiple oxyalkylene groups in the polyalkylene oxide may be the same or different. For example, the polyalkylene oxide may be a polymer having both oxyethylene groups and oxypropylene groups as repeating units. Examples of polyalkylene oxides include polyoxyethylene polyols, polyoxypropylene polyols, and polyoxyethyleneoxypropylene polyols.
[0030] Compound Y may be used alone or in combination of two or more. Compound Y may be a combination of an alcohol having 4 or less carbon atoms and a polyalkylene oxide. The content of compound Y is 1 to 10% by mass relative to the total mass of compound X and phospholipid. A content of compound Y of less than 1% by mass relative to the total mass of compound X and phospholipid is undesirable because the composition is not homogenized and a film cannot be formed. A content of compound Y of more than 10% by mass is undesirable because strain resistance deteriorates. The content of compound Y refers to the total content of an alcohol having 4 or less carbon atoms and a polyalkylene oxide contained in the composition for living organisms. Therefore, when a composition for living organisms contains an alcohol having 4 or less carbon atoms and a polyalkylene oxide, the total content of both satisfies the above requirements. In terms of better strain resistance and film formation rate, the content of compound Y is preferably 3 to 8% by mass relative to the total mass of compound X and phospholipid. The content of compound Y is preferably 1 to 9 mass %, more preferably 3 to 8 mass %, based on the total mass of the composition for living organisms.
[0031] [Water] The composition for a living body of the present invention may contain water. In order to prevent the composition for a living body from being easily removed when the composition for a living body of the present invention is applied to the skin or mucous membrane, the content of water is preferably 0 to 10% by mass, more preferably 0 to 5% by mass, even more preferably 0 to 1% by mass, and particularly preferably 0% by mass, relative to the total mass of the composition for a living body.
[0032] [Quaternary Ammonium Salt] The composition for living organisms of the present invention may further contain a quaternary ammonium salt (excluding phosphatidylcholine).
[0033] Quaternary ammonium salts have the molecular formula NR 4 + Preferred are ionic compounds comprising a positively charged polyatomic ion (quaternary ammonium cation) represented by the formula (I) and an anion. Each R independently represents an alkyl group which may have a substituent, an alkenyl group which may have a substituent, or an aryl group, and multiple Rs may be the same or different. Examples of the substituents that the alkyl and alkenyl groups may have include a hydroxyl group, an acyloxy group, an acyl group, an alkoxy group, an alkenyloxy group, and an aryl group. The hydrocarbon group of the acyloxy group and acyl group is preferably a long-chain alkyl group (an alkyl group having 8 or more carbon atoms) or a long-chain alkenyl group (an alkenyl group having 8 or more carbon atoms). The anion is not particularly limited, and examples thereof include an acid anion, a halide ion, and a hydroxide ion.
[0034] The quaternary ammonium salt is preferably a di-long-chain alkyl quaternary ammonium salt or a di-long-chain alkenyl quaternary ammonium salt. The di-long-chain alkyl quaternary ammonium salt and the di-long-chain alkenyl quaternary ammonium salt are each represented by the molecular formula NR 4 +In the quaternary ammonium cation represented by the formula (I), two of the R groups are long-chain alkyl groups (alkyl groups having 8 or more carbon atoms) or long-chain alkenyl groups (alkenyl groups having 8 or more carbon atoms). The other two R groups are each independently a short-chain alkyl group (alkyl groups having 1 to 7 carbon atoms) or an aryl group. The long-chain alkyl group and long-chain alkenyl group preferably have 12 to 22 carbon atoms, more preferably 16 to 18 carbon atoms. The two long-chain alkyl groups may be the same or different types, and the two long-chain alkenyl groups may be the same or different types.
[0035] Examples of quaternary ammonium salts include dioleoyloxytrimethylammonium propane chloride (DOTAP, N-[1-(2,3-dioleoyloxy)propyl]-N,N,N-trimethylammonium chloride), dioctadecenyltrimethylammonium propane chloride (DOTMA, N-[1-(2,3-dioleyloxy)propyl]-N,N,N-trimethylammonium chloride), didecyldimethylammonium chloride, didecyldimethylammonium bromide, dilauryldimethylammonium chloride, dicetyldimethylammonium chloride, dicetyldimethylammonium bromide, distearyldimethylammonium chloride, distearyldimethylammonium bromide, dioleyldimethylammonium chloride, dibehenyldimethylammonium chloride, dibehenyldimethylammonium bromide, dipalmitoylethylhydroxyethylmonium methosulfate, and distearoylethylhydroxyethylmonium methosulfate.
[0036] [Liquid Crystal Phase] The composition for biological use of the present invention preferably forms a liquid crystal phase by coming into contact with water and absorbing water or moisture. Due to the formation of a liquid crystal phase, the film formed by the composition for biological use of the present invention exhibits excellent elastic modulus and strain resistance. In this specification, moisture absorption refers to the absorption of moisture. Examples of moisture include water in the atmosphere and water in exhaled breath. In this specification, moisture absorption refers to the absorption of water (excluding moisture). The thickness of the film formed by the composition for biological use of the present invention is not particularly limited, but is, for example, 0.1 μm to 1 mm, and preferably 1 to 100 μm.
[0037] Examples of water that may come into contact with the composition for biological use of the present invention include water (humidity) in the atmosphere, water (humidity) in exhaled breath, pure water, and water contained in aqueous fluids other than water. Examples of aqueous fluids other than water include saliva, interstitial fluid, blood, and lymph. When using the composition for biological use of the present invention, the amount of water to be brought into contact with the composition for biological use of the present invention is not particularly limited, but is preferably 1000% by mass or less, more preferably 500% by mass or less, based on the total mass of the composition for biological use of the present invention. The lower limit of the amount of water used when contacting the composition for biological use of the present invention with the composition for biological use of the present invention, based on the total mass of the composition for biological use of the present invention, is not particularly limited, but may be, for example, more than 1% by mass. The temperature when the composition for biological use of the present invention is brought into contact with water is not particularly limited, but is preferably 20 to 40°C, more preferably 35 to 40°C.
[0038] The liquid crystal phase that can be formed by contacting the composition for living bodies of the present invention with water is not particularly limited, but is often any one selected from the group consisting of a reverse hexagonal columnar (H2) phase (W / O hexagonal columnar phase), a hexagonal columnar (H1) phase (O / W hexagonal columnar phase), a lamellar (La) phase, a sponge (V2) phase, a bicontinuous cubic (L3) phase, and a mixture of two or more of these. The liquid crystal phase preferably has a reverse hexagonal columnar (H2) phase or a hexagonal columnar (H1) phase.
[0039] In particular, the composition for living organisms of the present invention preferably forms an inverted hexagonal columnar (H2) phase upon water or moisture absorption, and more preferably forms an inverted hexagonal columnar (H2) phase upon moisture absorption.
[0040] The composition for living bodies of the present invention may undergo a phase transition of the liquid crystal phase upon further water absorption after absorbing moisture. Examples of such phase transitions include a phase transition from an inverted hexagonal columnar (H2) phase to a hexagonal columnar (H1) phase. Specifically, as described above, after forming a liquid crystal phase (e.g., an inverted hexagonal columnar (H2) phase) by absorbing a small amount of water (moisture) such as atmospheric water or water in exhaled breath, the liquid crystal phase may transition to another liquid crystal phase (e.g., a hexagonal columnar (H1) phase) upon further absorbing a larger amount of water (moisture) than that in the atmosphere, such as water sprayed by a sprayer, artificial saliva, aqueous fluids, skin exudates, or water from eating and drinking.
[0041] [Method for producing a composition for living organisms] As a method for producing the composition for living organisms of the present invention, for example, a method of mixing compound X, phospholipid, compound Y, and, if necessary, optional components at a predetermined mixing ratio can be used. The mixing method is not particularly limited, and a conventionally known method can be used.
[0042] [Uses of the composition for living bodies] The composition for living bodies of the present invention can be used in living bodies. The composition for living bodies of the present invention can be used for the purpose of supporting or repairing parts of living bodies that have lost their original functions due to injury or illness (e.g., objects such as skin, hair, and mucous membranes; the same applies hereinafter to "parts") and parts with reduced function. In particular, the composition for living bodies of the present invention can be preferably used for skin or mucous membranes (particularly for protecting oral mucosa and digestive tract).
[0043] [Method of using the composition for living bodies] Methods of using the composition for living bodies of the present invention include, for example, placing the composition for living bodies of the present invention on an area having symptoms such as those described above, and then contacting the composition for living bodies of the present invention with water.
[0044] When the composition for living bodies of the present invention is used on the skin, for example, the composition for living bodies of the present invention may be applied to the skin in the atmosphere, and water or a solution containing water may be added to the composition for living bodies of the present invention as needed. The composition for living bodies of the present invention on the skin can form a film (preferably a liquid crystal film) by contacting, for example, water in the atmosphere, water sprayed by a spray, the above-mentioned aqueous fluid, or exudate from the skin.
[0045] When the composition for living bodies of the present invention is applied to a mucous membrane, the composition for living bodies of the present invention is placed on the mucous membrane, and water or a solution containing water is added to the composition for living bodies of the present invention as needed. The composition for living bodies of the present invention on the mucous membrane can form a film (preferably a liquid crystal film) by contact with, for example, water in the atmosphere, water in breath, water sprayed by a sprayer, the above-mentioned aqueous fluids, and water from eating and drinking. In particular, when the composition for living bodies of the present invention is applied to the oral mucosa, the composition for living bodies of the present invention is simply attached (applied) to the oral mucosa, and a film is formed by contact with water in the atmosphere, water in breath, or water in saliva, making it easy to handle. Furthermore, if the amount of saliva is low, water can be supplied by applying the composition for living bodies of the present invention to the oral mucosa and then spraying water or artificial saliva.
[0046] The present invention will be described in more detail below with reference to the following examples. The materials, amounts used, ratios, treatment details, and treatment procedures shown in the following examples can be changed as appropriate without departing from the spirit of the present invention. Therefore, the scope of the present invention should not be construed as being limited by the following examples.
[0047] [Evaluation] [Preparation of Composition for Biological Use] Compositions for biological use in each Example and Comparative Example were prepared by mixing the following raw materials so that each component shown in Tables 1 and 2 was in the amount (parts by mass) shown in the tables. Details of the raw materials for each component in Tables 1 and 2 are as follows: Selachyl alcohol (NIKKOL Selachyl Alcohol V, manufactured by Nikko Chemicals): Compound X Phospholipid (LIPOID P100: manufactured by Lipoid, containing 90% or more by mass of phosphatidylcholine) Propylene glycol (manufactured by Fujifilm Wako Pure Chemical Industries): Compound Y Ethanol (manufactured by Fujifilm Wako Pure Chemical Industries): Compound Y 1,3-Butylene glycol (manufactured by Fujifilm Wako Pure Chemical Industries): Compound Y 1-Pentanol (manufactured by Fujifilm Wako Pure Chemical Industries)
[0048] [Elastic Modulus] The elastic modulus of the film formed by the biocomposition was measured using a rheometer (MCR302) and a measuring jig PP25 according to the following procedure. Using a stainless steel jig with a hole 25 mm in diameter and 200 μm in thickness, a 25 mm diameter, 200 μm thick layer of the biocomposition was applied to a base, and the base was then set in the rheometer. The applied biocomposition was sprayed with water three times (0.3 mL per spray) using a Trusco finger sprayer (TFSB-20) and allowed to stand for 1 minute. After 1 minute, strain dispersion measurements were performed in the range of 0.001 to 1000% at a measurement temperature of 25°C, 50% rh (relative humidity), a gap of 200 μm, a frequency of 1 Hz, and Nf = 1 N. The elastic modulus of the film formed by the biocomposition was evaluated from the obtained storage modulus G' at a shear strain of 0.1% according to the following evaluation criteria. The elastic modulus is preferably rated B or higher.
[0049] A: Storage modulus G' at a shear strain of 0.1% is 30,000 Pa or more. B: Storage modulus G' at a shear strain of 0.1% is 1,000 Pa or more and less than 30,000 Pa. C: Storage modulus G' at a shear strain of 0.1% is less than 1,000 Pa.
[0050] [Strain Tolerance] The storage modulus G' and loss modulus G'' obtained by strain dispersion measurement in the above-mentioned [Elastic Modulus] were evaluated for strain tolerance according to the following evaluation criteria from the shear strain (%) at which G' = G'' (i.e., the shear strain at the intersection of the storage modulus G' and the loss modulus G'' when a graph is prepared with shear strain on the horizontal axis and elastic modulus on the vertical axis). The strain tolerance is preferably rated C or higher.
[0051] A: The shear strain (%) at which G' = G'' is 30% or more. B: The shear strain (%) at which G' = G'' is 10% or more and less than 30%. C: The shear strain (%) at which G' = G'' is 5% or more and less than 10%. D: The shear strain (%) at which G' = G'' is less than 5%.
[0052] [Liquid Viscosity] The liquid viscosity of the composition for biomedical use was evaluated using a rheometer (MCR302) and a measuring jig PP25. The composition for biomedical use was set on the base of the device, and the liquid viscosity of the composition for biomedical use was measured under conditions of a measurement temperature of 25°C, 50% rh (relative humidity), a gap of 1 mm, and a shear rate of 0.1 to 1000 (1 / s). The liquid viscosity was evaluated according to the following evaluation criteria using the viscosity at a shear rate of 0.1 (1 / s).
[0053] A: Viscosity at a shear rate of 0.1 (1 / s) is less than 10,000 cPs. B: Viscosity at a shear rate of 0.1 (1 / s) is 10,000 cPs or more but less than 100,000 cPs. C: Viscosity at a shear rate of 0.1 (1 / s) is 100,000 cPs or more.
[0054] [Film formation rate] Each composition for biomedical use was applied to a glass slide at a thickness of 200 μm under conditions of 25°C and 50% rh (relative humidity). After application, the composition for biomedical use on the glass slide was observed under a polarizing microscope 1 minute, 30 minutes, 1 hour, and 24 hours later. The time required for the composition for biomedical use on the glass slide to form a liquid crystal phase (the time required for the field of view of the polarizing microscope to change from dark field to bright field) was recorded. When the composition for biomedical use formed a liquid crystal phase, the field of view of the polarizing microscope changed to bright field. The film formation rate was evaluated from the time required for the liquid crystal phase to be formed under the above observation.
[0055] A: A liquid crystal phase was formed within 1 minute. B: A liquid crystal phase was formed in more than 1 minute and within 1 hour. C: A liquid crystal phase was formed in more than 1 hour and within 24 hours. D: A liquid crystal phase was not formed even after 24 hours.
[0056] [Liquid Crystal Phase] Each composition for biological use was applied to a glass slide to a thickness of 200 μm, and the glass slide was left to stand for 24 hours or more under conditions of 25°C and 50% rh (relative humidity). Using the sample, SAXS (small-angle X-ray scattering diffraction) measurement was performed to determine the liquid crystal structure. For the SAXS measurement, a Rigaku Nanopix small-angle X-ray scattering measurement device (Cu Ka, 40 kV / 30 mA) was used. The results of the SAXS measurement were expressed as the scattering vector length (q / nm -1 The scattering vector length (q / nm) was calculated for each peak on the scattering curve. -1 The ratio of the scattering vector lengths of the three peaks was measured to identify the liquid crystal structure. When at least three peaks were observed on the scattering curve and the ratio of the scattering vector lengths of the peaks was approximately 1:√3:√4, the liquid crystal phase was determined to be an inverted hexagonal columnar (H2) phase. The ratio of the scattering vector lengths of the three peaks being 1:√3:√4 is characteristic of an inverted hexagonal columnar (H2) phase.
[0057] [Results] The composition and evaluation results of each composition for biological use are shown in Tables 1 and 2. In the evaluation column of the tables, if the above evaluation could not be performed due to the properties of the composition, it was marked "N.D." In the evaluation of the liquid crystal phase, if the liquid crystal phase was a reverse hexagonal columnar phase, it was marked "H2," and if no liquid crystal phase was formed, it was marked "N.D."
[0058]
[0059]
[0060] The composition of Comparative Example 1, in which the content of compound Y was more than 10% by mass relative to the total mass of compound X and phospholipid, did not meet the desired level of strain resistance. The composition of Comparative Example 2, which did not contain phospholipid, was unable to form a film, and the elastic modulus and strain resistance did not meet the desired levels. The composition of Comparative Example 3, in which the content of compound Y was less than 1% by mass relative to the total mass of compound X and phospholipid, was inhomogeneous and unable to form a film, making it impossible to perform any evaluation and not exhibiting the desired properties. The composition of Comparative Example 4, in which an alcohol having 5 or more carbon atoms was used, did not dissolve the components and unable to form a film, making it impossible to perform any evaluation and not exhibiting the desired properties. In contrast to the above, it was confirmed that the composition for living bodies of the present invention can form a film when contacted with water, and the formed film has excellent elastic modulus and strain resistance.
[0061] A comparison of Examples 1 to 7 confirmed that when the mass ratio of the compound X content to the phospholipid content was 70 / 30 to 50 / 50, the liquid viscosity and film formation rate were superior, and when it was 65 / 35 to 55 / 45, the effects of the present invention were even superior. A comparison of Examples 1 to 7 confirmed that when the compound X content was 45% by mass or more, relative to the total mass of the composition for living bodies, the liquid viscosity was superior, and when it was 50% by mass or more, the strain resistance and liquid viscosity were even superior. Furthermore, it was confirmed that when the compound X content was 80% by mass or less, relative to the total mass of the composition for living bodies, the elastic modulus was superior, when it was 70% by mass or less, the strain resistance and film formation rate were even superior, and when it was 65% by mass or less, the film formation rate was particularly superior. A comparison of Examples 4 and 8 confirmed that when the compound Y content was 3 to 8% by mass, relative to the total mass of compound X and phospholipid, the strain resistance and film formation rate were superior.
Claims
1. A composition for use in a living body, comprising: a compound X selected from the group consisting of an α-monoalkyl glyceryl ether and an α-monoalkenyl glyceryl ether; a phospholipid; and a compound Y selected from the group consisting of an alcohol having 4 or less carbon atoms and a polyalkylene oxide, wherein the content of compound Y is 1 to 10% by mass based on the total mass of compound X and the phospholipid.
2. The biological composition according to claim 1, wherein the compound X is selected from the group consisting of selachyl alcohol, batyl alcohol, and chimyl alcohol.
3. The biological composition according to claim 1, wherein the compound X is selachyl alcohol.
4. The composition for living organisms according to claim 1, wherein the mass ratio of the content of said compound X to the content of said phospholipid is 70 / 30 to 50 / 50.
5. The composition for living organisms according to claim 1, wherein the water content is 0 to 10% by mass based on the total mass of the composition for living organisms.
6. The composition for living organisms according to claim 1, wherein the content of said compound X is 50 mass % or more based on the total mass of said composition for living organisms.
7. The biological composition according to claim 1, which forms an inverted hexagonal columnar phase upon absorption of water or moisture.
8. A biological composition according to any one of claims 1 to 7, which is for use on the skin or mucous membrane.
Citation Information
Patent Citations
Alkyl glyceryl ether-mixed composition and cosmetic or skin care preparation containing the same
JP2010059066A
Oil-in-water type emulsified composition incorporated with ascorbic acid derivative
JP2013209319A
Translucent to transparent composition
JP2013227294A
Emulsified composition
JP2014237595A
Biomaterial
WO2020059543A1