Method and apparatus for manufacturing paper binder
The method addresses the environmental and safety concerns of conventional paper binder manufacturing by using heat-reactive molding materials and thermoforming techniques to create a ∩ shaped comb binder, improving productivity and reducing costs while ensuring eco-friendliness and safety.
Patent Information
- Application Number
- PCT/KR2023/007410
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-17
- Filing Date
- 2023-05-31
- Publication Date
- 2024-10-24
AI Technical Summary
Conventional paper binder manufacturing methods using wire or plastic rings face issues such as environmental unfriendliness, safety hazards from sharp edges, complex processes, high costs, and reduced productivity due to the use of liquid adhesives and unnecessary equipment, as well as the need for separate collection and recycling.
A method that eliminates liquid adhesives by using a heat-reactive molding material to bind papers without the need for half cutting or rewinding, and thermoforms a comb-shaped steel ball into a ∩ shape followed by cold molding into a cylindrical shape, reducing manufacturing complexity and waste.
This approach improves productivity, reduces manufacturing costs, and enhances safety by eliminating sharp edges and unnecessary processes, while using eco-friendly biodegradable materials that simplify the production process and maintain the shape of the binder during use.
Smart Images

Figure KR2023007410_24102024_PF_FP_ABST
Abstract
Description
Manufacturing method and manufacturing device for paper binder
[0001] The present invention relates to a method and a manufacturing apparatus for a paper binder for binding through perforated holes, such as a notebook, sketchbook, calendar, or planner.
[0002] In general, there are two types of binding or bookbinding methods through punched holes, such as in conventional notebooks, sketchbooks, calendars, planners, etc.: coil ring and twin ring, and wire or plastic (PVC, PET) rings are used. The binding method using coil rings is a method of binding in a diagonal shape by continuously inserting a row of coil rings into each punched hole, and the binding method using twin rings is a method of binding in the shape of an O ring by inserting two rows of rings into each punched hole and interlocking them with each other.
[0003] Recently, considering the trend / demand for eco-friendliness of products and the issue of separate collection when discarding, products using conventional wire or plastic rings such as the above have had the inconvenience of having to separate the wire and plastic from the paper for recycling when discarding, and there is also the problem that the wire or plastic ring itself is not eco-friendly.
[0004] Furthermore, in the case of office and stationery products such as notebooks, sketchbooks, calendars, planners, and planners bound with wire or plastic rings, there was also a problem that the sharp ends of the wire or plastic protruding from both ends of the coil ring of the product often caused safety accidents such as hands being pricked or cut when using the product.
[0005] Prior art (Patent No. 10-1124063) discloses a product that can replace wire with paper in twin-ring binding. However, the paper product used in twin-ring binding in the prior art suffered from various fundamental problems.
[0006] Hereinafter, the manufacturing process and problems of the twin ring disclosed in the prior art (Patent No. 10-1124063) will be described.
[0007] (1) Liquid adhesive (heat sealing agent)
[0008] In the prior art, a heat sealing agent is applied between papers by dissolving a polymer material in an organic solvent. However, the heat sealing agent, which is a polymer material containing an organic solvent as a solvent, is a major cause of air pollution due to the organic substances that volatilize, and is a material vulnerable to fire hazards because it is harmful to the human body and flammable.
[0009] In addition, after applying a liquid adhesive to the paper surface, long-term or long-term thermal drying is essential to volatilize the organic solvent, which complicates the process and increases installation costs.
[0010] In the prior art, liquid heat sealing agents are not only required in the paper laminating process for laminating papers together, but are also required to heat and re-form the heat sealing agent in a subsequent forming process, and further, they are an adhesive required for thermally bonding the tips of the comb-shaped portions to the comb-joining portions using the heat sealing agent exposed at the tips of the comb-shaped portions in the bookbinding process. In particular, since such heat sealing agents are in a liquid state with low viscosity, they can easily penetrate the paper during the application process to the paper surface, and thus, there is a limit to securing sufficient rigidity due to insufficient film formation of a solid substance, and furthermore, there is a problem in that sufficient rigidity as a binder cannot be secured even when manufacturing thick paper of 1 mm or more.
[0011]
[0012] (2) Unnecessity of half-cutting process and rewinding process
[0013] The prior art is configured to expose the heat sealing agent at the comb-shaped leading edge by cutting the comb-shaped leading edge. As such, the prior art requires a process of cutting the leading edge of the comb-shaped portion to expose the heat sealing agent at the comb-shaped leading edge, and therefore additionally requires an unloading device for unloading comb-shaped laminated paper wound on a bobbin, a half-cutting device for cutting the comb-shaped leading edge of the laminated paper, and a winding device for rewinding the laminated paper unloaded from the half-cutting device onto a bobbin.
[0014] These complex processes are a factor in unnecessary increase in manufacturing costs, and the additional devices required increase the cost of equipment / devices, which also increases the cost.
[0015]
[0016] (3) Complex process and device that divides into two parts and transports them during the molding process.
[0017] In a conventional molding process, a molding device is composed of a first molding section and a second molding section having a table-shaped base frame and a press mechanism, and a plurality of return sections for returning laminated paper from the front and rear of the molding sections on both sides, and is arranged in order as a return section, a first molding section, a return section, a second molding section, and a return section on the upper surface of the base frame.
[0018] In the conventional technology, the molding process is performed by dividing it into a first molding section and a second molding section, so there is a problem in that the return process and device increase unnecessarily.
[0019] That is, since it is divided into two parts and molded, it reduces productivity due to the complex molding process and causes an increase in manufacturing costs due to the need for unnecessary machinery.
[0020]
[0021] (4) Temperature-raising function of multiple jig plates in the forming process
[0022] Since the forming film is not sufficiently formed in the bonding process, it is essential for the forming means to heat the jig plates in the forming process, and as a result, after forming, they must be separated / detached from the jig plate and then go through a cooling process. After separation, the formed shape tends to return to its original shape during cooling, and as a result, the accuracy of the desired forming shape is reduced and sufficient rigidity is not secured.
[0023] In the forming process of a paper binder consisting of cylindrical curved section forming and folded section forming, both the first forming section and the second forming section require a number of jig plates equipped with a temperature raising function, and a cooling device is also required for each.
[0024] Therefore, the temperature rise on the jig plate during molding unnecessarily lengthens the working time, and furthermore, since cooling is required after molding, the manufacturing process takes a lot of time, which reduces productivity and makes accurate molding difficult.
[0025]
[0026] (5) The necessity of a “U” shaped protective paper
[0027] Since the binder according to the prior art is configured such that the heat sealing agent is exposed at the comb-shaped tip, there is a problem that the binder itself may be incorrectly attached by the exposed heat sealing agent when the formed binder is wound on a bobbin during the forming process. Therefore, in the prior art, a process of wrapping the C-shaped binder with paper manufactured in a "U" shape and then winding it is absolutely necessary. Due to these additional paper materials, additional manufacturing processes, and additional winding devices, there was a problem that the manufacturing process and manufacturing device were complicated, resulting in lower productivity and increased manufacturing costs.
[0028] The purpose of the present invention is to improve productivity by not using a liquid adhesive and thus not requiring a long drying period / time for volatilization of an organic solvent, and to eliminate the need for complicated processes such as half-cutting and rewinding processes required to expose a heat sealing agent to the tip of the comb in the prior art, and to enable the binder itself to be wound as it is without the need to separately manufacture and use a “U” shaped protective paper required to prevent incorrect attachment and tangling of the heat sealing agent exposed to the tip of the comb in the prior art, thereby simplifying the production process and reducing unnecessary waste of paper.
[0029] The purpose of the present invention is to make the leading edge cutting process of the prior art unnecessary, so that the thickness of the leading edge of the comb and the connecting portion of the comb teeth are the same, so that the spread shape of the leading edge of the comb teeth can be easily wound on a bobbin without problems such as expansion or contraction, and in particular, the shape is maintained as is during the distribution process, so that the insertion operation is easy in the binding process.
[0030] The purpose of the present invention is to form a comb-shaped spur into a "∩" shape by a thermoforming device, and then to form the comb-shaped spur into a cylindrical shape by cooling the comb-shaped spur, which has been thermoformed into a "∩" shape, in a subsequent cooling device so that the comb-shaped spur ends face the comb-connecting portions, thereby easily forming the comb-shaped spur into a "∩" shape, and to sequentially cool and form the comb-parts and the comb-connecting portions at a fixed position without retransferring, thereby simultaneously cooling the formed finished product, thereby shortening the overall production period and enabling accurate cylindrical forming of a paper binder.
[0031] In order to achieve the above object, a method for manufacturing a paper binder according to one embodiment of the present invention comprises the steps of: thermally bonding inner roll paper and outer roll paper together using a heat-reactive molding material disposed between the inner roll paper and the outer roll paper; slitting the bonded bonded paper to a predetermined width; cutting the slitted bonded paper to have a comb-tooth shape and a comb-tooth connection shape, thereby forming a flat comb-shaped support member; thermally forming the comb-tooth portion of the flat comb-shaped support member into an "∩" shape in a thermal forming device so that the comb-tooth portion corresponds to the comb-tooth connection portion in an "∩" shape; And a step of cooling and forming a comb-shaped sphere formed in the “∩” shape into a cylindrical shape by using a cooling and forming device so that the tip of the comb portion faces the comb connecting portion, wherein the heat-responsive forming material is configured to have a function of causing the inner roll paper and the outer roll paper to be combined by heat, a function of causing the comb-shaped sphere to be pre-formed into a “∩” shape while being heated by the thermal forming device, and a function of cooling and forming the comb-shaped sphere formed in the “∩” shape into a cylindrical shape while being cooled by the cooling and forming device.
[0032] According to the present invention, the following effects are achieved.
[0033] First, since no liquid adhesive is used, there is no need for a long drying period / time for the volatilization of the organic solvent, which improves productivity. In addition, there is no need for complicated processes such as half-cutting and rewinding required to expose the heat sealing agent to the tip of the comb in the conventional technology, which improves productivity and reduces manufacturing costs. In addition, there is no need to separately manufacture and use a “U”-shaped protective paper required to prevent the heat sealing agent exposed to the tip of the comb in the conventional technology from sticking and becoming tangled, and the binder itself can be wound as is, which simplifies the production process and reduces unnecessary waste of paper.
[0034] Second, since the cutting process of the leading edge of the conventional technology is unnecessary, the thickness of the leading edge of the comb and the connecting portion of the comb teeth are the same, and as a result, the comb teeth can be easily wound on a bobbin without problems such as expansion or contraction of the spread shape of the leading edge of the comb teeth, and in particular, the shape is maintained as is during the distribution process, making insertion work easy in the binding process.
[0035] Third, the purpose of the present invention is to provide a method for forming a comb-shaped serpentine into a "∩" shape by a thermoforming device, and then cooling and forming the comb-shaped serpentine into a cylindrical shape by a subsequent cooling and forming device so that the tip of the comb portion faces the comb connection portion, thereby easily forming the comb-shaped serpentine into a "∩" shape, and simultaneously cooling and forming the comb portion and the comb connection portion in a fixed position without retransfer, thereby simultaneously cooling and forming the formed finished product, thereby shortening the overall production period and enabling accurate cylindrical forming of a paper binder.
[0036] Figure 1 is a schematic diagram illustrating a bonding and slitting process according to the present invention.
[0037] Figure 2 illustrates a wound laminated paper and its cross-section after the laminating and slitting process according to the present invention.
[0038] Figure 3 illustrates a flat comb-shaped serration manufactured by cutting slitting paper into a comb-tooth shape and a comb-tooth connecting shape.
[0039] Figure 4 illustrates one embodiment of a press mold used in the cutting process of the present invention.
[0040] Figure 5 is a schematic diagram showing a process of forming a flat comb-shaped burr into a cylindrical comb-shaped burr through a “∩” shape and applying hot melt adhesive to the inner surface of the comb joint of the cylindrical comb-shaped burr.
[0041] Figures 6(a) to 6(c) are schematic diagrams showing sequential forming processes performed in a cooling forming device according to the present invention.
[0042] FIG. 7 illustrates a perspective view and a cross-sectional view of a paper binder formed into a cylindrical shape by a forming device according to one embodiment of the present invention.
[0043] Hereinafter, preferred embodiments of the present invention will be described in more detail with reference to the drawings.
[0044] Figure 1 is a schematic diagram illustrating a slitting and bonding process according to the present invention. Referring to Figure 1, inner roll paper (10), thermal reaction forming material (30a), middle roll paper (40), thermal reaction forming material (30b), and outer roll paper (20) are sequentially supplied while being unwound onto rolls sequentially arranged within a drawing device (100). The inner roll paper (10), heat-responsive molding material film (30a), intermediate roll paper (40), heat-responsive molding material film (30b), and outer roll paper (20) supplied above are first melted in passing through a pair of preheating rollers (200), and then, as they pass through a pair of heat-pressing rollers (300), the inner roll paper (10), intermediate roll paper (40), and outer roll paper (20) are formed into a laminated paper by means of the heat-responsive molding material (30a, 30b) through the close pressure of the pair of heat-pressing rollers (300). The laminated paper is cooled in passing through a pair of cooling pressing rollers (400). That is, the inner roll paper (10), the middle roll paper (40), and the outer roll paper (20) are sequentially passed through a pair of preheating rollers (200), a pair of heat pressing rollers (300), and a pair of cooling pressing rollers (400) arranged in succession, and are laminated to each other by melting and cooling / solidifying the heat reaction forming film (30a, 30b). Then, the laminated paper is slit to a predetermined width by a slitting device (500) and then wound by a winding device (600).
[0045] Additionally, in the schematic diagram shown in Fig. 1, only the inner roll paper (10) and the outer roll paper (20) may be laminated by one heat-reactive molding material in the middle, without the intermediate roll paper (40).
[0046] The above-mentioned heat-reactive molding material (30a, 30b) is preferably a biodegradable film, and may also be a polyethylene film, a soft PVC film, or a heat-liquefied solid film. The coating or film thickness of the heat-reactive molding material is 50 to 200 μm.
[0047] Most preferably, the heat-responsive molding material (30a, 30b) uses an eco-friendly biodegradable material composed only of 100% naturally decomposing biodegradable materials such as corn syrup (PLA), cellulose, and polybutylene terephthalate (PBAT). In this case, when sunlight, temperature, humidity, etc. are under certain conditions (composting conditions such as temperature 58 degrees Celsius and humidity 70% Celsius), primary decomposition occurs, and a secondary decomposition process is carried out by microorganisms (bacteria, mold, etc.), resulting in 100% natural decomposition into water and carbon dioxide within 180 days. Therefore, it is possible to prevent environmental pollution and destruction of the ecosystem, and it can be conveniently disposed of as general waste rather than recycling, and it is also suitable for composting soil that has been landfilled and decomposed, and no carcinogens are emitted at all even when incinerated, and biodegradable vinyl manufactured from biodegradable raw materials (EL724) can also be recycled.
[0048] Preferably, the heat-responsive molding material (30a, 30b) is a heat-responsive molding film, which may be a biodegradable film, polyethylene film, PVC film, hot melt, etc. that reacts at 100 to 220 degrees Celsius, but an environmentally friendly biodegradable film is most preferable.
[0049] The above-mentioned heat-reactive molding material (30a, 30b) is melted by heat and functions to bond the inner roll paper (10), the middle roll paper (40), and the outer roll paper (20).
[0050] FIG. 2(a) and FIG. 2(b) illustrate a wound laminated paper and a cross-section thereof, respectively, after the laminating and slitting processes according to the present invention. The drawing illustrated in FIG. 2(a) illustrates a cross-section in which “inner roll paper (10), a heat-responsive molding material film (30a), an intermediate roll paper (40), a heat-responsive molding material film (30b), and an outer roll paper (20)” are sequentially laminated according to the process illustrated in FIG. 1. The drawing illustrated in FIG. 2(b) illustrates a cross-section in which “inner roll paper (10), a heat-responsive molding material film (30), and an outer roll paper (20)” are sequentially laminated when the intermediate roll paper is not required in FIG. 1. In particular, when manufacturing a paper binder having a large diameter, additional rigidity reinforcement is particularly required. In this case, as illustrated in FIG. 2(a), an intermediate roll paper (40) may be additionally placed between the inner roll paper (10) and the outer roll paper (20), and a heat-reactive molding material film (30a, 30b) may be additionally laminated between the inner roll paper (10) and the intermediate roll paper (40), and between the intermediate roll paper (40) and the outer roll paper (20). Accordingly, depending on the presence or absence and the number of intermediate roll papers (40) added between the inner roll paper (10) and the outer roll paper (20), the binder may be configured as three layers, five layers, or seven layers. For reference, the cross-section illustrated in FIG. 2(a) illustrates a five-layer binder, and the cross-section illustrated in FIG. 2(b) illustrates a three-layer binder.
[0051] Fig. 3 illustrates a flat comb-shaped filing tool manufactured by cutting slit paper into a comb-shaped portion and a comb-shaped connecting portion shape. Referring to Fig. 3, the slit roll paper is cut symmetrically on both sides to have a comb-shaped portion (52) and a comb-shaped connecting portion (54), thereby forming two flat comb-shaped filing tools (50) that are symmetrical on both sides. This cutting process is performed by mounting a mold on a press machine device, and as illustrated in Fig. 3, the comb-shaped portion (52) and the comb-shaped connecting portion (54) are cut symmetrically on both sides on both sides. Preferably, the two flat comb-shaped filing tools in the cut state are separated and wound onto separate bobbins. More preferably, the two flat comb-shaped serrated blades cut symmetrically left and right are separated, and then wound on two bobbins that rotate in opposite directions, so that the comb teeth of the flat comb-shaped serrated blades wound on the two bobbins are aligned in the same direction, and as a result, the comb teeth of the flat comb-shaped serrated blades can be continuously provided to subsequent processes in a state where they are aligned in the same direction.
[0052] FIG. 4 illustrates an embodiment of a press die used in the cutting process of the present invention. Referring to FIG. 4, the press die (60) is a compound die die in which the upper frame (62) and the lower frame (64) intersect to cut symmetrically on both sides, and the comb portion and the comb connection portion on one side fitted into the lower frame are pulled out and transported upward by a slide pad (66) mounted inside the lower frame. The slide pad (66) is configured to move up and down by a spring (68) inside the lower frame. When the upper frame (62) presses the lower frame (64) with strong pressure to symmetrically cut the comb portion and the comb connection portion, the spring (68) inside the lower frame (64) is pushed downward by the upper frame (62), and when the upper frame (62) rises upward, the comb portion and the comb connection portion on one side fitted into the lower frame are pulled out and transported upward by the elastic action of the spring (68) inside the lower frame.
[0053] Figure 5 is a schematic diagram showing a process of forming a flat comb-shaped burr into a cylindrical comb-shaped burr through a “∩” shape and applying hot melt adhesive to the inner surface of the comb joint of the cylindrical comb-shaped burr.
[0054] Referring to Fig. 5, a comb-shaped serrated part wound on a bobbin is unwound by an unwinding device (700) and first supplied to a preheating plate (810) or a preheating zone of a thermal forming device (800). The preheating plate (810) is configured to sufficiently heat up at a low heat so that only the comb portion and the comb connection portion of the flat comb-shaped serrated part, particularly the thermal reactive forming material of the corresponding portion, can be melted immediately before the forming process. For example, it can be configured in the form of a preheating plate controlled and heated by a heater or a preheating zone controlled by hot air.
[0055] As illustrated in FIG. 5, when the flat comb-shaped sphere passes through the preheating plate (810), the heat-reactive molding material inside is melted, and then, as it passes through the first “∩”-shaped molding part (820) and the second “∩”-shaped molding part (830) in succession, the comb portion of the comb-shaped sphere is heat-formed into a “∩” shape corresponding to the comb connecting part. That is, the heat-reactive molding material here functions to cause the comb-shaped sphere to be preliminarily formed into a “∩” shape by the first “∩”-shaped molding part (820) and the second “∩”-shaped molding part (830) while being heated by the heat-forming device (800).
[0056] The first "∩"-shaped forming section (820) is configured as a section in which a flat sphere supplied through a preheating plate (810) is gradually thermally converted into a "∩" shape, while the second "∩"-shaped forming section (830) is configured as a section in which a comb-shaped sphere, which has been finally formed into a "∩" shape through the above-mentioned conversion section, is thermally re-formed by a "∩"-shaped mold.
[0057] Next, the comb-shaped serrated steel ball formed into the above “∩” shape is transferred to a cooling forming device (900), and then cooled and formed into a cylindrical shape by the cooling forming device (900) so that the tip of the comb portion faces the comb connecting portion.
[0058] FIGS. 6(a) to 6(c) are schematic diagrams illustrating sequential forming processes performed in a cooling forming device according to the present invention. Referring to FIG. 6(a), the cooling forming device (900) of the present invention comprises an upper mold (920) that operates downwardly to contact the upper portion of a fixed inner mold (910), and double-sided molds (930a, 930b) that operate simultaneously from both sides toward the inner mold to simultaneously contact both sides of the inner mold, and the upper mold (920) and the double-sided molds (930a, 930b) operate sequentially during the forming process without re-transfer to cool and form the heated "∩"-shaped comb-shaped spherical part, which is placed on the inner mold (910), into a cylindrical shape that is bent outwardly and spread out to face each other.
[0059] Preferably, a cooling means capable of cooling at least one of the inner mold (910), the upper mold (920), and the two side molds (930a, 930b) is further provided, so that cooling can be performed simultaneously with molding by the molding device without separate retransfer. For example, in winter, room temperature cooling is possible, and in summer, at least one cooling device capable of allowing water or air to flow inside each mold may be provided, or cooling can be performed directly by blowing air or cooled air from the outside of the mold.
[0060] In this way, the cooling forming device (900) of the present invention is configured to cool the heated "∩"-shaped comb-shaped sphere and simultaneously form it into a cylindrical shape, thereby eliminating the need for a separate cooling process, thereby saving the time required for the cooling process of the prior art, and as a result, significantly improving productivity and reducing manufacturing costs.
[0061] Referring to FIGS. 6(a) to 6(c), the cooling forming process using the cooling forming device according to the present invention is described as follows.
[0062] First, as illustrated in Fig. 6(a), a comb-shaped sphere having a "∩" shape is placed on the inner mold (910) of the cooling molding device. Then, as illustrated in Fig. 6(b), the upper mold (920) moves downward toward the lower inner mold (910) to pressurize the upper portion of the comb-shaped sphere having a "∩" shape placed on the inner mold (910), thereby forming the upper surface of the placed comb-shaped sphere into a semicircle. Then, as illustrated in Fig. 6(c), by simultaneously pressing both sides of the comb-shaped sphere having a "∩" shape placed on the inner mold (910) while maintaining the sphere as is without a separate re-transfer process, a cylindrical comb-shaped sphere can be formed.
[0063] Referring to Fig. 5, the cylindrical comb-shaped serrated edge formed by cooling and forming by the cooling and forming device (900) is transferred to a hot melt adhesive application device (1100) by a transfer device (1000). The hot melt adhesive application device (1100) applies hot melt adhesive to the inner surface of the comb connection portion facing the comb tooth tip portion of the cooling and forming comb-shaped serrated edge. This application process is performed by applying hot melt adhesive to the inner surface of the comb connection portion by a nozzle configured to be inserted between the comb tooth tip portion of the comb-shaped serrated edge and the comb connection portion.
[0064] FIG. 7(a) and FIG. 7(b) illustrate a perspective view and a cross-sectional view of a paper binder formed into a cylindrical shape by a forming device according to one embodiment of the present invention.
[0065] Preferably, the present invention can additionally cool and form recessed portions at least two places symmetrically on the circular ring portion of the cylindrical comb-shaped burr during cooling and forming by a cooling and forming device.
[0066] When forming a cylindrical comb-shaped holder using a multilayer thick comb-shaped holder made of at least two layers of paper and a heat-responsive molding material (i.e., an adhesive), a temporary external force applied during the forming process may cause structural deformation, resulting in a persistent restoring force that tries to return to a flat state even after the product is formed into a cylindrical comb-shaped holder. As a result, even after the comb-shaped holder is formed into a cylindrical shape, the comb-tooth joints and the tips of the comb teeth may gradually spread apart. In addition, in the cooling forming process, the heat-responsive molding material disposed between the multilayer paper is press-formed into a cylindrical shape in a molten state due to heat, so that the paper may be pushed out during the press-forming process due to the difference in diameter depending on the thickness of the inner and outer papers.
[0067] The inventor of the present invention recognized the above two problems and, in order to solve the above problems, formed at least one pair of concave portions symmetrically on the inner mold that contacts the upper mold in a cooling molding device, or on the inner mold that contacts the two side molds, thereby preventing the phenomenon of the comb teeth tip and the comb teeth connection part from spreading out and the phenomenon of paper creeping in advance.
[0068] While the present invention has been described in detail with reference to specific embodiments with reference to the drawings above, the present invention is not limited to these specific structures. Those skilled in the art will appreciate that various modifications and variations of the present invention can be made without departing from the technical spirit and scope of the invention as set forth in the claims below. However, it should be noted in advance that such simple design material modifications or structural modifications are all clearly within the scope of the present invention.
Claims
1. In the method for manufacturing a paper binder, A step of thermally bonding the inner roll paper and the outer roll paper to each other using a heat-reactive molding material placed between the inner roll paper and the outer roll paper; A step of slitting the above-mentioned combined paper to a predetermined width; A step of cutting the above slit composite paper to have a comb-tooth shape and a comb-tooth connecting shape, thereby forming a flat comb-shaped base; A step of heat forming the comb portion of the flat comb-shaped base into a “∩” shape using a heat forming device so that the comb portion corresponds to the comb connection portion in a “∩” shape; and It includes a step of cooling and forming a cylindrical comb-shaped sphere in a cooling and forming device so that the tip of the comb-shaped portion faces the comb-connecting portion, and A method for manufacturing a paper binder, wherein the above-mentioned heat-responsive molding material has a function of bonding the inner roll paper and the outer roll paper by heat, a function of preforming the comb-shaped serrations into a “∩” shape while being heated by the heat forming device, and a function of cooling and molding the comb-shaped serrations formed into a “∩” shape into a cylindrical shape while being cooled by the cooling forming device.
2. A method for manufacturing a paper binder in which, in the first paragraph, an intermediate roll paper is additionally included between the inner roll paper and the outer roll paper, and a heat-reactive molding material is disposed between the inner roll paper and the intermediate roll paper, and between the intermediate roll paper and the outer roll paper, respectively.
3. A method for producing a paper binder in the second paragraph, wherein the heat-responsive molding material is provided as a heat-responsive molding film.
4. A method for manufacturing a paper binder, further comprising the step of applying a hot melt adhesive to the inner surface of a comb connecting portion facing the tip of the comb portion of the cooled and formed comb-shaped iron tool in the first paragraph.
5. A method for manufacturing a paper binder in which, in the third paragraph, the inner roll paper, the middle roll paper, and the outer roll paper are sequentially passed through a pair of preheating rollers, a pair of heat pressing rollers, and a pair of cooling pressing rollers arranged in succession, and are bonded to each other by the heat reaction forming film.
6. A method for manufacturing a paper binder, wherein in paragraph 1, two flat comb-shaped serrations cut symmetrically on the left and right are separated, and then wound on two bobbins that rotate in opposite directions, so that the comb portions of the flat comb-shaped serrations wound on the two bobbins are in the same direction, so that they can be continuously provided to a subsequent process.
7. A method for manufacturing a paper binder in the first paragraph, wherein the thermal forming device heats the comb-shaped serrated teeth continuously supplied and thermally forms them into a “∩” shape, and the cooling forming device cools and forms the comb-shaped serrated teeth thermally formed into the “∩” shape into a cylindrical shape so that the tip of the comb portion faces the comb connecting portion.
8. In the first paragraph, the cooling forming device is configured with an upper mold that operates downward to contact the upper portion of a fixed inner mold, and two side molds that operate simultaneously toward the inner mold from both sides to contact both sides of the inner mold simultaneously, and the upper mold and the two side molds operate sequentially without retransfer during the forming process to cool and form the heated "∩"-shaped comb-shaped spherical teeth that are seated on the inner mold into a cylindrical, outwardly bent, spread, and facing shape. A method for manufacturing a paper binder.
9. A method for manufacturing a paper binder, wherein in paragraph 8, a cooling means for cooling at least one of the inner mold, the upper mold, and the two side molds is further provided inside or outside the mold, so that cooling is performed simultaneously with molding by the cooling molding device without separate retransfer.
10. A method for manufacturing a paper binder, further comprising the step of applying a hot melt adhesive to the inner surface of the comb-joint portion by a nozzle inserted between the comb-joint portion and the comb-joint portion of the comb-shaped serration tool in the fourth paragraph.
11. In a device for manufacturing a paper binder, A laminated paper generating unit that thermally laminates the inner roll paper and the outer roll paper with each other using a heat-responsive molding material placed between the inner roll paper and the outer roll paper; A slitting unit that slits the above-mentioned combined paper to a predetermined width; A cutting section that cuts the above slit joint paper to have a comb-tooth shape and a comb-tooth connecting shape, thereby forming two flat comb-shaped base plates that are symmetrical on the left and right; A heat forming part that heat forms the comb portion of the above comb-shaped spur into a “∩” shape in a heat forming device so that it corresponds to the comb connecting portion in a “∩” shape; A cooling forming unit is included for cooling and forming a comb-shaped cylindrical shape in a cooling forming device, so that the tip of the comb-shaped portion faces the comb-connecting portion, and the comb-shaped sphere is heat-formed in the shape of "∩". A device for manufacturing a paper binder, wherein the above-mentioned thermal reaction forming material has a function of bonding the inner roll paper and the outer roll paper by heat, a function of preforming the comb-shaped serrations into a “∩” shape while being heated by the thermal forming device, and a function of cooling and forming the comb-shaped serrations formed into a “∩” shape into a cylindrical shape while being cooled by the cooling forming device.
12. A device for manufacturing a paper binder, further comprising a nozzle unit for applying hot melt adhesive to the inner surface of a comb connecting portion facing the tip of the comb portion of the cooled and formed comb-shaped iron tool in accordance with paragraph 11.
Citation Information
Patent Citations
Bookbinding wire and paper clip with biodegradable coatings and a method for their decomposition
EP2291251B1
Books or calendars and its manufacturing method
JP2004017290A
Paper-made binder, and system and device for producing the same
KR101124063B1
The bookbinding device of calendar holder and calendar holder
KR101194080B1
Ring-like paper binder and method of manufacturing the same
KR1020070110826A