Graphitization furnace and battery production system
By optimizing the electrode distance and size in the graphitization furnace to form a uniform electric field, the problem of inconsistent quality of graphitized products in the existing technology is solved, and the quality of graphitized products and the performance of battery negative electrode materials are improved.
Patent Information
- Application Number
- PCT/CN2023/099779
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-28
- Filing Date
- 2023-06-13
- Publication Date
- 2024-10-31
AI Technical Summary
When existing graphitization furnaces generate graphitized products, the uneven distribution of electric field intensity results in inconsistent quality of graphitized products, which affects the performance of battery anode materials.
Design a graphitization furnace in which a first electrode and a ring electrode are arranged in the furnace body. By adjusting the distance and size of the electrodes, an electric field with a relatively uniform electric field intensity distribution is formed to uniformly heat the material and improve the quality of the graphitized product. Specific measures include setting the distance H1 between the end face of the first electrode and the annular electrode part and the inner diameter D1 of the annular electrode to satisfy 0.5≤H1/D1≤5, and the outer diameter D2 and inner diameter D1 of the annular electrode satisfying 1.17≤ D2/D1≤3, the diameter D3 of the first electrode and the inner diameter D1 of the annular electrode satisfy 1≤D1/D3≤3.4, and the contact area of the diversion electrode part and the annular electrode part satisfy 1.5≤S4/S3≤8.
Through uniform electric field heating, the consistency and quality of graphitized products are improved, meeting the standard requirements of battery anode materials, reducing the chance of material blocking, and extending the service life of the graphitization furnace.
Smart Images

Figure CN2023099779_31102024_PF_FP_ABST
Abstract
Description
Graphitization furnace and battery production system
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to Chinese patent application No. 202310484921.9, filed on April 28, 2023, entitled “Graphitization Furnace and Battery Production System,” the entire contents of which are incorporated herein by reference. Technical Field
[0003] The present application relates to the technical field of industrial equipment, and in particular to a graphitization furnace and a battery production system. Background Art
[0004] With the rapid development of energy technology, batteries have become an indispensable part of human life. Currently, carbon materials are widely used in battery negative electrode materials. Among them, graphitized carbon materials (also known as graphite materials) have been widely commercialized due to their long service life, stable structure and low cost.
[0005] A graphitization furnace is a device that produces graphite. The quality of the resulting graphitized product is crucial for battery manufacturing. Therefore, improving the quality of graphitized products is a pressing technical challenge.
[0006] Summary of the Invention
[0007] The embodiments of the present application provide a graphitization furnace and a battery production system, which can improve the quality of graphitized products.
[0008] In a first aspect, a graphitization furnace is provided, comprising: a furnace body, wherein a material channel is provided within the furnace body; a first electrode, wherein at least a portion of the first electrode is located within the material channel; a second electrode having a polarity opposite to that of the first electrode, comprising an annular electrode portion, wherein the annular electrode portion is protruded from the inner wall of the material channel along the radial direction of the material channel and surrounds a partial channel section of the material channel; along the extension direction of the material channel, a distance between an end surface of the first electrode facing the second electrode and a first plane is H1, an inner diameter of the annular electrode portion is D1, and H1 and D1 satisfy: 0.4≤H1 / D1≤5; wherein the first plane is a plane where a surface of the annular electrode portion facing the first electrode is located.
[0009] Through the technical solution of the embodiment of the present application, the distance H1 between the end face of the first electrode 220 and the first plane and the inner diameter D1 of the annular electrode portion satisfy 0.5≤H1 / D1≤5, so that an electric field with a relatively uniform electric field intensity distribution can be formed between the end face 221 of the first electrode 220 and the surface of the annular electrode portion 231 facing the end face 221 of the first electrode 220, so as to uniformly heat the material passing through the electric field, which is beneficial to improving the consistency of the graphitized product and thus improving the quality of the graphitized product.
[0010] In some possible implementations, H1 and D1 satisfy: 0.8≤H1 / D1≤1.5.
[0011] After a large number of experimental verifications, it was found that when H1 and D1 satisfy 0.8≤H1 / D1≤1.5, the quality of graphitized products can be further improved.
[0012] In some possible implementations, the value range of H1 is 350-3000 mm.
[0013] After a large number of experimental verifications, H1 in the range of 350 ~ 3000mm is conducive to the formation of a more concentrated electric field and is not prone to blockage.
[0014] In some possible implementations, the value range of D1 is 430-2400 mm.
[0015] After a large number of experimental verifications, it was found that D1 in the range of 430 to 2400 mm is conducive to forming a more concentrated electric field and is less likely to cause material blockage.
[0016] In some possible implementations, the outer diameter of the annular electrode portion is D2, and D1 and D2 satisfy: 1.17≤D2 / D1≤3.
[0017] In the above embodiment, the outer diameter D2 and the inner diameter D1 of the annular electrode portion satisfy 1.17≤D2 / D1≤3, which can not only make the electric field reach the temperature required for the graphitization process, but also make the graphitization path length moderate. The material is heated for a sufficient time, and the pores of the graphitized product can be repaired to an acceptable level, thereby improving the quality of the graphitized product.
[0018] In some possible implementations, D1 and D2 satisfy: 1.24≤D2 / D1≤2.51.
[0019] After a large number of experimental verifications, it was found that when D1 and D2 satisfy 1.24≤D2 / D1≤2.51, the quality of graphitized products can be further improved.
[0020] In some possible implementations, the value range of D2 is 580-2750 mm.
[0021] After a large number of experimental verifications, it was found that D2 in the range of 580 to 2750 mm is conducive to the formation of a more concentrated electric field.
[0022] In some possible implementations, along the radial direction of the material channel, the thickness dimension of the annular electrode portion is T, and H1 and T satisfy: 0.6≤H1 / T≤7.4.
[0023] In the above embodiment, the thickness T of the annular electrode portion and the distance H1 between the end face of the first electrode and the first plane satisfy 0.6 ≤ H1 / T ≤ 7.4. This allows the electric field to reach the temperature required for the graphitization process, and the graphitization path length to be moderate. The material is heated for a sufficient time, and the pores of the graphitized product can be repaired to an acceptable level, thereby improving the quality of the graphitized product. Furthermore, the probability of material blockage can be reduced.
[0024] In some possible implementations, H1 and T satisfy: 0.81≤H1 / T≤5.
[0025] After a large number of experimental verifications, it was found that when H1 and T satisfy 0.81≤H1 / T≤5, the quality of graphitized products can be further improved.
[0026] In some possible implementations, the value range of T is 130 to 1500 mm.
[0027] After a large number of experimental verifications, it is found that when T is in the range of 130 to 1500 mm, it is conducive to forming a more concentrated electric field.
[0028] In some possible implementations, the first electrode is a cylindrical electrode, the diameter of the first electrode is D3, and D3 and D1 satisfy: 1≤D1 / D3≤3.4.
[0029] In the above embodiment, the diameter D3 of the first electrode and the inner diameter D1 of the annular electrode portion satisfy 1≤D1 / D3≤3.4. This not only forms an electric field with a relatively uniform electric field intensity distribution, but also allows the temperature of all regions within the electric field to reach the temperature required for the graphitization process as much as possible, thereby uniformly and effectively heating the material, thereby improving the quality of the graphitized product. It also facilitates the uniform flow of the material in the material channel and reduces the probability of material blockage.
[0030] In some possible implementations, D1 and D3 satisfy: 1≤D1 / D3≤2.
[0031] After a large number of experimental verifications, it was found that when D1 and D3 satisfy 1≤D1 / D3≤2, the quality of graphitized products can be further improved.
[0032] In some possible implementations, the value range of D3 is 350-1200 mm.
[0033] After a large number of experimental verifications, it was found that D3 in the range of 350 to 1200 mm is conducive to the formation of a more concentrated electric field.
[0034] In some possible implementations, the first electrode is a cylindrical electrode, the diameter of the first electrode is D3, and D3 and H1 satisfy: 0.7≤H1 / D3≤4.7.
[0035] In the above embodiment, the diameter D3 of the first electrode and the distance H1 between the end face of the first electrode and the first plane satisfy 0.7≤H1 / D3≤4.7. This not only forms an electric field with a relatively uniform electric field intensity distribution, but also allows the temperature required for the graphitization process to be reached within the electric field, thereby uniformly and effectively heating the material passing through the electric field, thereby improving the quality of the graphitized product.
[0036] In some possible implementations, D3 and H1 satisfy: 0.7≤H1 / D3≤2.
[0037] After a large number of experimental verifications, it was found that when D3 and H1 satisfy 0.7≤H1 / D3≤2, the quality of graphitized products can be further improved.
[0038] In some possible implementations, along the radial direction of the material channel, the cross-sectional area of the first electrode is S1, the cross-sectional area of the annular electrode portion is S2, and S1 and S2 satisfy: 0.8≤S2 / S1≤18.
[0039] In the above embodiment, the cross-sectional area S1 of the first electrode and the cross-sectional area S2 of the annular electrode portion along the radial direction of the material channel satisfy 0.8≤S2 / S1≤18, so that the temperature required for the graphitization process can be reached in the electric field, and the material can be heated for a sufficient time to repair the pores of the graphitized product to an acceptable level, thereby improving the quality of the graphitized product.
[0040] In some possible implementations, S1 and S2 satisfy: 1.2≤S2 / S1≤12.
[0041] After a large number of experimental verifications, it was found that when S1 and S2 satisfy 1.2≤S2 / S1≤12, the quality of graphitized products can be further improved.
[0042] In some possible implementations, the value range of S1 is 0.12 to 1.2 m 2 .
[0043] After a lot of experimental verification, S1 is between 0.12 and 1.2 m 2 range, which is conducive to forming a more concentrated electric field.
[0044] In some possible implementations, the value range of S2 is 0.15 to 2.5 m 2 .
[0045] After a lot of experimental verification, S2 is between 0.15 and 2.5m 2 range, which is conducive to forming a more concentrated electric field.
[0046] In some possible embodiments, the second electrode further includes a current-conducting electrode portion; one end of the current-conducting electrode portion is connected to the annular electrode portion, and the other end is connected to a power supply; the contact surface area between the current-conducting electrode portion and the annular electrode portion is S3, and the outer surface area of the annular electrode portion is S4, and S3 and S4 satisfy: 1.5≤S4 / S3≤8.
[0047] In the above embodiment, the outer side surface area S4 of the annular electrode portion and the contact surface area S3 between the guide electrode portion and the annular electrode portion satisfy 1.5≤S4 / S3≤8, so that the contact surface area S3 can meet the current density requirement and reduce the current deviation phenomenon, thereby making the temperature required for the graphitization process reach in the electric field, thereby improving the quality of the graphitized product.
[0048] In some possible implementations, S3 and S4 satisfy: 3≤S4 / S3≤5.
[0049] After a large number of experimental verifications, it was found that when S3 and S4 satisfy 3≤S4 / S3≤5, the quality of graphitized products can be further improved.
[0050] In some possible implementations, the value range of S3 is 0.15 to 1.1 m 2 .
[0051] After a lot of experimental verification, S3 is between 0.15 and 1.1 m 2 Within this range, it is beneficial for a large current to pass through the contact surface between the annular electrode portion and the guide electrode portion, so that there is sufficient current density in the electric field.
[0052] In some possible implementations, the value range of S4 is 0.5 to 7 m 2 .
[0053] After a lot of experimental verification, S3 is between 0.15 and 1.1 m 2 Within this range, the annular electrode portion is conducive to receiving a larger current density, thereby ensuring sufficient current density in the electric field.
[0054] In some possible embodiments, along the radial direction of the material channel, the bottom surface of the guide electrode portion is flush with the bottom surface of the annular electrode portion; along the extension direction of the material channel, the height dimension of the annular electrode portion is H2, and the height dimension of the guide electrode portion is H3, and H2 and H3 satisfy: 1≤H2 / H3≤4.
[0055] The above embodiment enables the height dimension H2 of the annular electrode portion and the height dimension H3 of the guide electrode portion to satisfy 1≤H2 / H3≤4, which not only takes into account the manufacturing cost of the annular electrode portion, but also forms a more concentrated electric field to centrally heat the material, thereby improving the quality of the graphitized product.
[0056] In some possible implementations, H2 and H3 satisfy: 1≤H2 / H3≤1.8.
[0057] After a large number of experimental verifications, S3 and S4 satisfy 1≤H2 / H3≤1.8, which can further improve the quality of graphitized products.
[0058] In some possible implementations, the value range of H2 is 400-2000 mm.
[0059] After a large number of experimental verifications, it was found that H2 in the range of 400 to 2000 mm is conducive to the formation of an umbrella-shaped electric field.
[0060] In some possible implementations, the value range of H3 is 300-1200 mm.
[0061] After a large number of experimental verifications, it was found that H2 in the range of 400 to 2000 mm is conducive to the formation of an umbrella-shaped electric field.
[0062] In some possible implementations, the graphitization furnace further includes a first thermal insulation layer, which is disposed at the innermost side of the furnace body and forms a partial channel section of the material channel.
[0063] In the above embodiment, by providing the first insulation layer, the temperature of the heating zone formed between the first electrode and the second electrode can be insulated, so that the heating zone is maintained in a high temperature range, the degree of graphitization of the material is uniform, and the consistency of the graphitized product can be improved.
[0064] In some possible implementations, the thermal conductivity of the first thermal insulation layer is 0.05 to 5 w / mk; or the compressive strength of the first thermal insulation layer is 0.1 to 40 MPa; or the temperature resistance of the first thermal insulation layer is 1800 to 3200°C.
[0065] In the above embodiment, by setting the thermal conductivity of the first thermal insulation layer, the first thermal insulation layer can reduce heat loss in the graphitization furnace under this thermal conductivity, thereby improving energy utilization. By setting the compressive strength of the first thermal insulation layer, the first thermal insulation layer can have a higher degree of heat resistance. By setting the temperature resistance of the first thermal insulation layer, the first thermal insulation layer can have a higher degree of heat resistance, thereby improving the service life of the graphitization furnace.
[0066] In some possible implementations, the graphitization furnace further includes a second thermal insulation layer disposed on a side of the first thermal insulation layer facing the outside of the furnace body.
[0067] In the above embodiment, by providing a second insulation layer outside the first insulation layer, the temperature of the heating zone formed between the first electrode and the second electrode can be further insulated, so that the heating zone is maintained in a high temperature range, the degree of graphitization of the material is uniform, and the consistency of the graphitized products can be further improved.
[0068] In some possible embodiments, the thermal conductivity of the second insulation layer is 0.1 to 20 w / mk; or the compressive strength of the second insulation layer is 20 to 60 MPa; or the temperature resistance of the second insulation layer is 1500 to 3200° C.; or the ash content of the second insulation layer is 0.1% to 10%.
[0069] In the above embodiment, by setting the thermal conductivity of the second insulation layer, the second insulation layer can reduce heat loss in the graphitization furnace under this thermal conductivity, thereby improving energy utilization. By setting the compressive strength of the second insulation layer, the second insulation layer can have a high-strength supporting effect. By setting the temperature resistance of the second insulation layer, the second insulation layer can have a high-strength heat resistance effect. By setting the ash content of the second insulation layer, the effect of excessive ash content on the quality of the second insulation layer can be reduced, thereby improving the service life of the graphitization furnace.
[0070] In some possible implementations, the graphitization furnace further includes a third thermal insulation layer disposed on a side of the second thermal insulation layer facing the outside of the furnace body.
[0071] In the above embodiment, by providing the third insulation layer outside the second insulation layer, the energy loss of the first insulation layer and the second insulation layer can be reduced, and the energy utilization rate and insulation effect can be improved.
[0072] In some possible implementations, the third thermal insulation layer contains more than 30% alumina; or the compressive strength of the third thermal insulation layer is 1 to 60 MPa; or the temperature resistance of the third thermal insulation layer is 1000 to 2000°C.
[0073] In the above embodiment, by setting alumina material in the third thermal insulation layer, the third thermal insulation layer can have a certain anti-oxidation function; by setting the compressive strength of the third thermal insulation layer, the third thermal insulation layer can have a higher strength supporting effect; by setting the temperature resistance of the third thermal insulation layer, the third thermal insulation layer can have a higher strength heat resistance effect, thereby improving the service life of the graphitization furnace.
[0074] In a second aspect, a battery production system is provided, comprising: a graphitization furnace according to the first aspect or any possible embodiment of the first aspect, wherein the graphitization furnace is used to produce negative electrode graphite material for a battery. BRIEF DESCRIPTION OF THE DRAWINGS
[0075] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the following is a brief introduction to the drawings required for use in the embodiments of the present application. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on the drawings without creative work.
[0076] FIG1 is a schematic structural diagram of a graphitization furnace;
[0077] FIG2 is a front cross-sectional view of a graphitization furnace provided in an embodiment of the present application;
[0078] FIG3 is a top cross-sectional view of a graphitization furnace provided in an embodiment of the present application;
[0079] FIG4 is a front cross-sectional view of a graphitization furnace provided in an embodiment of the present application;
[0080] FIG5 is a top cross-sectional view of a graphitization furnace provided in an embodiment of the present application;
[0081] FIG6 is a front cross-sectional view of another graphitization furnace provided in an embodiment of the present application;
[0082] FIG7 is a front cross-sectional view of another graphitization furnace provided in an embodiment of the present application.
[0083] In the drawings, the drawings are not drawn to scale. DETAILED DESCRIPTION
[0084] The following detailed description of the embodiments of the present application is provided in conjunction with the accompanying drawings and examples. The following detailed description of the embodiments and the accompanying drawings are used to illustrate the principles of the present application, but are not intended to limit the scope of the present application, that is, the present application is not limited to the described embodiments.
[0085] In the description of this application, it should be noted that, unless otherwise specified, "multiple" means more than two; the terms "upper", "lower", "left", "right", "inside", "outside", etc., indicating directions or positional relationships, are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on this application. In addition, the terms "first", "second", "third", etc. are only used for descriptive purposes and cannot be understood as indicating or implying relative importance. "Vertical" is not strictly perpendicular, but is within the allowable error range. "Parallel" is not strictly parallel, but is within the allowable error range.
[0086] The directional words appearing in the following description are all directions shown in the figures, and do not limit the specific structure of this application. In the description of this application, it should also be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to the specific circumstances.
[0087] This application relates to a graphitization furnace, which can transform carbon materials from irregularly arranged carbon atoms into an ordered graphite crystal structure through heating, thereby achieving graphitization of the carbon materials. Graphitization is intended to improve the thermal and electrical conductivity of carbon materials, enhance their thermal shock resistance and chemical stability, impart lubricity and wear resistance to carbon materials, increase their purity, reduce their hardness, and facilitate machining.
[0088] Currently, graphitization furnaces are primarily used for high-temperature processing, including the sintering and graphitization of carbon materials, graphitization of polyimide (PI) films, graphitization of thermally conductive materials, sintering of carbon fiber ropes, sintering and graphitizing of carbon fiber filaments, graphite purification, and other materials that can be graphitized in a carbon environment. In some specific applications, graphite treated in a graphitization furnace can be used to form the negative electrode material of batteries. For example, graphite is currently a major negative electrode material in lithium batteries.
[0089] In this application, a battery refers to a physical module that includes one or more battery cells to provide electrical energy. A battery generally includes a casing for encapsulating one or more battery cells. Optionally, the battery cells may include, but are not limited to, lithium-ion secondary batteries, lithium-ion primary batteries, lithium-sulfur batteries, sodium-lithium-ion batteries, sodium-ion batteries, or magnesium-ion batteries. Among them, graphite can be used as the negative electrode active material of the battery cell, and is combined with the positive electrode active material of the battery cell (for example, lithium cobalt oxide, lithium iron phosphate, ternary lithium or lithium manganese oxide, etc.) to realize the movement of metal ions to form an electric current.
[0090] In some graphitization furnace designs, a positive electrode and a negative electrode are installed within the furnace. One end of the positive electrode and one end of the negative electrode are both connected to a DC or AC power source. The other end of the positive electrode and the other end of the negative electrode are positioned opposite each other, forming an electric field between them. When carbon material entering the graphitization furnace passes through this electric field, it energizes the carbon material, causing it to reach the graphitization temperature through self-resistive heating, thereby achieving graphitization.
[0091] As an example, in some specific implementations, the positive electrode is a columnar electrode placed vertically in the material channel, and the negative electrode is a ring electrode located in the lower part of the furnace body and placed horizontally. An umbrella-shaped electric field is formed between the lower surface of the positive electrode and the upper surface of the negative electrode facing the positive electrode. When the material (carbon material) passes through the umbrella-shaped electric field, Joule heat is generated based on its own resistance, thereby enabling graphitization of the material. Under this embodiment, the electric field intensity distribution in the umbrella-shaped electric field is uneven, especially when the distance between the positive electrode and the negative electrode is too long, the difference in electric field intensity in different areas of the electric field is more obvious. When the electric field intensity distribution in different areas is uneven, the current density in different areas is not equal, which will cause the Joule heat generated by the material passing through different areas of the electric field to be unequal, thereby affecting the consistency of the graphitized product and reducing the quality of the graphitized product.
[0092] In view of this, the present application provides a graphitization furnace, which includes a furnace body, a first electrode, and a second electrode with opposite polarity to the first electrode. A material channel is provided in the furnace body, at least a portion of the first electrode is located in the material channel, and the second electrode includes an annular electrode portion. Along the radial direction of the material channel, the annular electrode portion is protruded from the inner wall of the material channel and surrounds a portion of the material channel. Along the extension direction of the material channel, the distance H1 between the end face of the first electrode and the first plane and the inner diameter D1 of the annular electrode portion meet certain numerical conditions. The first plane is the plane where the surface of the annular electrode portion facing the first electrode is located. An electric field with a relatively uniform electric field intensity distribution can be formed between the first electrode and the second electrode to uniformly heat the material passing through the electric field, which is conducive to improving the consistency of the graphitized product, thereby improving the quality of the graphitized product.
[0093] The graphitization furnace involved in this application can be applied to any graphite production system, for example, sintering and graphitization system of carbon materials, PI film graphitization system, thermal conductive material graphitization system, carbon fiber rope / carbon fiber filament sintering graphitization system, graphite purification system, etc. The specific application scenarios of the graphitization furnace in this application include but are not limited to the above application scenarios.
[0094] As an example, in some practical applications, the graphitized product (graphite material) produced by the graphitization furnace described in this application can be used as the negative electrode material of a battery. In other words, in this application, the graphitization furnace can be used in a battery production system. The graphitization furnace can serve as a type of process equipment in a battery production line.
[0095] Figure 1 shows a front view of a graphitization furnace 100. As shown in Figure 1, the main body of the graphitization furnace 100 is arranged vertically and mainly includes a furnace body 1 and various functional units disposed in the furnace body 1. Specifically, as shown in Figure 1, the graphitization furnace can include a loading unit, a DC power supply unit, and a cooling and discharging unit.
[0096] The loading unit primarily comprises a silo 2 and a feed pipe 3. The silo 2 is positioned above the furnace body 1 and connected to the feed port on the furnace body via the feed pipe 3. Optionally, a material shut-off valve 4 may be provided at the junction of the silo 2 and the feed pipe 3 to control the flow of material within the material channel 12.
[0097] Optionally, the material entering the graphitization furnace 100 is a graphitizable carbonaceous material, such as petroleum coke, coal coke, and asphalt. After entering the graphitization furnace, the material undergoes four stages of preheating, calcination, graphitization, and cooling to complete the graphitization process, such as obtaining a negative electrode material product, and volatile tail gas escapes during the process.
[0098] Optionally, the number of the silos 2 can be 2, 4 or more, and they are evenly distributed above the furnace body 1 .
[0099] The DC power supply unit may include a positive electrode 5, a negative electrode 6, and a DC transformer 7. As shown in FIG1 , the positive electrode 5 may extend into the furnace through an opening above the furnace body 1 and be suspended in the material passage 12. The negative electrode 6 may be disposed in the lower middle portion of the furnace body 1. The negative electrode 6 may extend through the furnace body 1.
[0100] The DC transformer 7 supplies power to the furnace body 1, with a power supply controllable between 600 and 1500 kW. The positive and negative electrodes 5 and 6 apply voltage to the material passing between them. DC current flows from the positive electrode of the DC transformer 7 through the material, generating Joule heat due to its own electrical resistance, raising the furnace core temperature to approximately 3000°C or higher. This creates a stable temperature field between the positive and negative electrodes 5 and 6. The current flowing through the material then returns from the negative electrode 6 to the negative electrode of the DC transformer 7, completing a current loop.
[0101] Optionally, the DC power supply unit may further include a fixed brake 8, a conductive member 9, a cable 10, and a copper busbar 11. The positive electrode 5 is held securely in place directly above the furnace body 1 by the fixed brake. The conductive member 9 is secured below the fixed brake 8 and conducts current to the positive electrode 5. The cable 10 connects to the copper busbar 11, which in turn connects to the positive and negative terminals of the DC transformer 7.
[0102] Alternatively, the positive electrode 5 and the negative electrode 6 may be graphite electrodes.
[0103] The cooling and discharging unit is mainly used to cool the graphitized material. Specifically, as shown in Figure 1, the cooling and discharging unit can include a low-temperature cooling section 13, which can be a water-cooling jacket. The low-temperature cooling section 13 can also be provided with a water inlet 14 and a water outlet 15. The cooling medium can be circulating water.
[0104] Optionally, the graphitization furnace 100 may further include a furnace heating unit (not shown). For example, a furnace cover and a furnace lining. The furnace cover can be placed on the upper portion of the furnace body 1 to provide insulation, while the furnace lining surrounds the inner wall of the furnace body 1 to provide insulation against the high temperature of the furnace core.
[0105] Figures 2 to 6 respectively illustrate the structure of a graphitization furnace 200 provided in an embodiment of the present application, with Figures 2, 4, and 6 being front cross-sectional views, and Figures 3 and 5 being top cross-sectional views. As shown in Figures 2 to 5, the graphitization furnace 200 may include a furnace body 210, a first electrode 220, and a second electrode 230 having a polarity opposite to that of the first electrode 220. The furnace body 210 is provided with a material channel 211. At least a portion of the first electrode 220 is located within the material channel 211. The second electrode 230 includes an annular electrode portion 231 that protrudes from the inner wall 2111 of the material channel 211 along the radial direction of the material channel 211 and surrounds a portion of the material channel 211. Along the extension direction of the material channel 211, the distance between the end surface 221 of the first electrode 220 facing the second electrode 230 and the first plane is H1, and the inner diameter of the annular electrode portion 231 is D1. H1 and D1 satisfy the following relationship: 0.4≤H1 / D1≤5. The first plane is the plane where the surface 2311 of the annular electrode portion 231 facing the first electrode 220 is located.
[0106] A cavity is formed inside the furnace body 210 , and a material channel 211 may be formed in the cavity. The material for generating the graphite material may flow in the material channel 211 and be graphitized under the action of high temperature.
[0107] Optionally, as shown in FIG. 2 , the material channel 211 may penetrate the wall of the furnace body 210 , and after the material passing through the material channel 211 is converted into graphite material, the graphite material may be output to the outside of the furnace body 210 through the material channel 211 .
[0108] Optionally, the material channel 211 may extend in a direction parallel to the direction of gravity, and the material entering the material channel 211 may flow in the material channel 211 under the action of gravity. Alternatively, in other alternative embodiments, the material channel 211 may extend in other directions. In such embodiments, other auxiliary components may be provided inside the furnace body 210 to drive the carbonaceous material to flow in the material channel 211.
[0109] The first electrode 220 and the second electrode 230 can be the positive electrode and negative electrode, respectively, of the graphitization furnace 200. The first electrode 220 can be fixedly mounted at the opening of the furnace body 210 via a fixing device. At least a portion of the first electrode 220 can be located within the material channel 211, i.e., within the furnace body 210, while another portion of the first electrode 220 can be located outside the furnace body 210. The second electrode 230 can be disposed through the wall of the furnace body 210, with at least a portion of the second electrode 230 located outside the furnace body 210. The portions of the first electrode 220 and the second electrode 230 located outside the furnace body 210 can be connected to a power source via electrical connectors, thereby forming an electric field between the portions of the first electrode 220 and the second electrode 230 located inside the furnace body 210, thereby heating the material passing through the material channel 211.
[0110] Optionally, the first electrode 220 and the second electrode 230 may be graphite electrodes. In some embodiments, the first electrode 220 may be a positive electrode, having a current density of 18 to 26 A / cm², a current load of 50,000 to 75,000 A, and a resistivity of less than 6 micro-ohms. The second electrode 230 may be a negative electrode, having a current density of 10 to 20 A / cm², a current load of 20,000 to 30,000 A, and a resistivity of less than 8 micro-ohms.
[0111] Continuing with Figure 2 , the annular electrode portion 231 of the second electrode 230 protrudes from the inner wall 2111 of the material channel 211 along the radial direction of the material channel 211. This creates an umbrella-shaped electric field between the end surface 221 of the first electrode 220 and the surface 2311 of the annular electrode portion 231 facing the first electrode 220. The portion of the material channel 211 where the second electrode 230 surrounds the electrode wall of the second electrode 230 can be understood as the electrode wall of the second electrode 230 serving as the channel wall for a portion of the material channel 211. Thus, after entering the material channel 211 and being heated by the umbrella-shaped electric field, the material flows out of the hollow portion of the annular electrode portion 231 and then out of the furnace body 210, resulting in a graphitized product.
[0112] It should be noted that, in the embodiment of the present application, the end surface 221 of the first electrode 220 refers to the surface of one end of the first electrode 220 facing the second electrode 230 along the extension direction of the material channel 211 .
[0113] In one embodiment, in order to support the annular electrode portion 231 and prevent it from falling, the discharge section 212 of the material channel 211 can be flush with the inner diameter of the annular electrode portion 231 along the radial direction of the material channel 211 .
[0114] Continuing with Figure 2 , along the extension direction of the material channel 211, the distance between the end surface 221 of the first electrode 220 and the first plane is H1, and the inner diameter of the annular electrode portion is D1. The first plane is the plane where the surface 2311 of the annular electrode portion 231 facing the first electrode 220 lies. In this embodiment of the present application, H1 and D1 satisfy the following relationship: 0.5 ≤ H1 / D1 ≤ 5.
[0115] Optionally, in some embodiments, the value range of H1 may be 350 to 3000 mm.
[0116] After a large number of experimental verifications, H1 in the range of 350 ~ 3000mm is conducive to the formation of a more concentrated electric field and is not prone to blockage.
[0117] Optionally, in some embodiments, the value range of D1 may be 430 to 2400 mm.
[0118] After a large number of experimental verifications, it was found that D1 in the range of 430 to 2400 mm is conducive to forming a more concentrated electric field and is less likely to cause material blockage.
[0119] Optionally, in some embodiments, the outer diameter D2 of the annular electrode portion 231 may range from 580 to 2750 mm.
[0120] After a large number of experimental verifications, it was found that D2 in the range of 580 to 2750 mm is conducive to the formation of a more concentrated electric field.
[0121] Optionally, in some embodiments, the thickness T of the annular electrode portion 231 may be in the range of 130 to 1500 mm.
[0122] After a large number of experimental verifications, it is found that when T is in the range of 130 to 1500 mm, it is conducive to forming a more concentrated electric field.
[0123] It should be understood that the thickness T is the difference between the outer diameter D2 and the inner diameter D1 , ie, T= D2 − D1 .
[0124] Optionally, as shown in FIG6 , the height H2 of the annular electrode portion 231 may be in the range of 400 to 2000 mm.
[0125] After a large number of experimental verifications, it was found that H2 in the range of 400 to 2000 mm is conducive to the formation of an umbrella-shaped electric field.
[0126] Optionally, as shown in Figures 5 and 6 , the second electrode 230 includes, in addition to the annular electrode portion 231, a current-conducting electrode portion 232. One end of the current-conducting electrode portion 232 is connected to the annular electrode portion 231, and the other end is connected to a power source. The bottom surface of the current-conducting electrode portion 232 can be flush with the bottom surface of the annular electrode portion 231. The height H3 of the current-conducting electrode portion 232 ranges from 300 to 1200 mm.
[0127] After a large number of experimental verifications, it was found that H2 in the range of 400 to 2000 mm is conducive to the formation of an umbrella-shaped electric field.
[0128] Alternatively, in some embodiments, the first electrode 220 may be a cylindrical electrode.
[0129] Optionally, in some embodiments, the diameter D3 of the first electrode 220 may be in the range of 350 to 1200 mm.
[0130] After a large number of experimental verifications, it was found that D3 in the range of 350 to 1200 mm is conducive to the formation of a more concentrated electric field.
[0131] It should be understood that an umbrella-shaped electric field is formed between the end surface 221 of the first electrode 220 and the surface of the annular electrode portion 231 facing the first electrode 220. For example, where the first electrode 220 is a positive electrode and the second electrode 230 is a negative electrode, the electric field intensity near the end surface 221 of the first electrode 220 is generally greater than the electric field intensity in other areas of the electric field. When the ratio of H1 to D1 is too large, the height of the electric field coverage area increases, and thus the difference in electric field intensity between different areas of the electric field increases. After the material enters the electric field, it passes through different electric field areas with different electric field strengths, resulting in poor consistency of the graphitized product, thereby reducing the quality of the graphitized product.
[0132] In the embodiment of the present application, H1 and D1 are set to satisfy 0.5≤H1 / D1≤5, so that an electric field with a relatively uniform electric field intensity distribution can be formed between the end surface 221 of the first electrode 220 and the surface of the end surface 221 of the annular electrode portion 231 facing the first electrode 220, so as to uniformly heat the material passing through the electric field, which is beneficial to improving the consistency of the graphitized product and thus improving the quality of the graphitized product.
[0133] In order to verify whether the above-mentioned numerical range of H1 / D1 can improve the quality of graphitized products, relevant evaluation parameters of graphitized products corresponding to different H1 / D1 ratios are measured below.
[0134] In the embodiments of the present application, the relevant evaluation parameters of the graphitized product include the degree of graphitization. The degree of graphitization is the main indicator for evaluating graphitized products. The degree of graphitization is an indicator that measures the degree to which carbon atoms in the graphitized product form a close-packed hexagonal graphite crystal structure. The closer the lattice size is to the lattice constant of ideal graphite, the higher the degree of graphitization. Generally, a degree of graphitization of 90% is used as the qualification standard for graphitized products. As an example and not a limitation, the degree of graphitization of the graphitized product can be measured by X-ray diffraction analysis, which is a common method used by those skilled in the art to measure the degree of graphitization and will not be described in detail here.
[0135] It should be understood that the examples described below are illustrative and intended only to explain the present application, and should not be construed as limiting the present application. Where specific techniques or conditions are not specified in the examples, the techniques or conditions described in the literature in the art or in the product specifications were used. Materials or instruments used without manufacturer designation are commercially available conventional products.
[0136] Test Process 1: With the first electrode 220 as the positive electrode and the second electrode 230 as the negative electrode, the power supply during the closed loop control was 1200 kW, the outer diameter D2 of the annular electrode portion 231 of the second electrode 230 was 1350 mm, the diameter D3 of the first electrode 220 was 600 mm, the height H2 of the annular electrode portion 231 was 910 mm, and the height H3 of the guide electrode portion 232 was 700 mm. The graphitization degree of the graphitized product produced by the graphitization furnace 200 was recorded at different H1 / D1 ratios. The H1 / D1 ratio and test results are shown in Table 1. The graphitization degree of the graphitized product can be calculated using the peak value measured using an X-ray diffractometer.
[0137] Table 1
[0138] It can be seen from Table 1 that when H1 and D1 meet 0.5≤H1 / D1≤5, the graphitization degree of the graphitized product is above 90%, which meets the standard quality requirements of graphitized products. However, when H1 and D1 do not meet 0.5≤H1 / D1≤5, the graphitization degree of the graphitized product is less than 90%, which does not meet the standard quality requirements of graphitized products.
[0139] Therefore, as verified by the above tests, the above numerical range of H1 / D1 can make the graphitized products meet the standard quality requirements, thereby reducing the probability of unqualified graphitized products and improving the quality of graphitized products.
[0140] In some possible implementations, H1 and D1 satisfy 0.8≤H1 / D1≤1.5.
[0141] It can also be seen from the experimental data in Table 1 above that when H1 and D1 satisfy 0.8≤H1 / D1≤1.5, the graphitization degree of the graphitized product can exceed 93.5%, which can further improve the quality of the graphitized product.
[0142] In some possible implementations, with continued reference to FIG. 2 and FIG. 3 , the inner diameter D1 and the outer diameter D2 of the annular electrode portion 231 satisfy the following: 1.17≤D2 / D1≤3.
[0143] It should be understood that the electric field is formed between the end surface 221 of the first electrode 220 and the surface 2311 of the annular electrode portion 231 facing the first electrode 220. When the ratio of the outer diameter D2 to the inner diameter D1 of the annular electrode portion 231 is too large, that is, the wall of the annular electrode portion 231 is too thick and the surface 2311 of the annular electrode portion 231 facing the first electrode 220 is too large, the electric field covers a large area and the electric field intensity is low. The temperature required for the graphitization process may not be reached, resulting in a low degree of graphitization of the graphitized product. When the ratio of phase D2 to phase D1 is too small, that is, the wall of the annular electrode portion 231 is too thin, the electric field thickness is too thin along the radial direction of the material channel 211, resulting in a shorter graphitization path for the material, insufficient heating time, and inability to complete the graphitization process. As a result, the pores of the graphitized product cannot be repaired to an acceptable level.
[0144] It should be understood that specific surface area is an important indicator of whether the pores of the graphitized product have been repaired to an acceptable level. The better the pore repair of the graphitized product, such as the more regular the crystal structure of the graphitized product surface and the fewer defects, the closer the specific surface area is to the acceptable range.
[0145] Specific surface area refers to the surface area per gram of solid material. When graphite material is used as the negative electrode material of lithium-ion batteries, the specific surface area is a very important parameter of lithium-ion battery materials. If the specific surface area of the graphite material is too large, it will cause excessive initial capacity loss. The specific surface area of the graphite material is related to the shape and surface structure of the graphite particles. For example, artificial graphite has a special microporous structure and a large specific surface area. It contains more active sites, increases the reaction area, and improves the utilization rate of the active material, showing high capacity and high rate performance. However, during the first charge and discharge process, the electrolyte consumed by the formation of the SEI film is relatively large, resulting in a large proportion of irreversible capacity. If the specific surface area of the graphite particles is too small, the dynamic performance of the battery will deteriorate. Therefore, only graphite materials need to have a suitable specific surface area. Usually, the specific surface area is set between 1.1 and 1.3 m 2 / g of graphite material is considered to be a qualified battery negative electrode material. As an example and not limitation, the specific surface area can be measured by volumetric adsorption method, gravimetric adsorption method, flow adsorption method, permeability method, gas adhesion method, etc. These methods are commonly used by those skilled in the art for measuring specific surface area and will not be repeated here.
[0146] It should be noted that the graphitization degree of the graphitized product is positively correlated with the specific surface area.
[0147] In the embodiment of the present application, the outer diameter D2 and the inner diameter D1 of the annular electrode portion 231 satisfy 1.17≤D2 / D1≤3, which can not only make the electric field reach the temperature required for the graphitization process, but also make the graphitization path length moderate. The material is heated for a sufficient time, and the channels of the graphitized product can be repaired to an acceptable level, thereby improving the quality of the graphitized product.
[0148] In some possible implementations, D1 and D2 satisfy 1.24≤D2 / D1≤2.51.
[0149] A large amount of experimental data shows that when D1 and D2 satisfy 1.24≤D2 / D1≤2.51, the pores of the graphitized product can be further repaired, thereby further improving the quality of the graphitized product.
[0150] In some possible implementations, as shown in FIG. 4 , along the radial direction of the material channel 211 , the thickness dimension of the annular electrode portion 231 is T, and T and H1 satisfy: 0.6≤H1 / T≤7.4.
[0151] When the ratio of H1 to T is too large, for example, when the distance H1 is large and T is small, the uneven distribution of electric field strength becomes more pronounced, which can easily affect the consistency of the graphitized product. Furthermore, if the thickness of the electric field is too thin along the radial direction of the material channel 211, the graphitization path of the material will be short, resulting in insufficient heating time and an inability to complete the graphitization process, which in turn causes the pores of the graphitized product to be unable to be repaired to an acceptable level. When the ratio of H1 to T is too small, for example, when H1 is small and T is large, material blockage may occur, reducing the efficiency of graphitization. Furthermore, if the wall of the annular electrode portion 231 is too thick, the electric field strength in the area near the annular electrode portion 231 is low, which may not reach the temperature required for the graphitization process, resulting in a low degree of graphitization in the graphitized product.
[0152] In the embodiment of the present application, the thickness T of the annular electrode portion 231 and the distance H1 between the end surface 221 of the first electrode 220 and the first plane satisfy 0.6≤H1 / T≤7.4. This allows the electric field to reach the temperature required for the graphitization process, and the graphitization path length to be moderate. The material is heated for a sufficient time, and the pores of the graphitized product can be repaired to an acceptable level, thereby improving the quality of the graphitized product. Furthermore, the probability of material blockage can be reduced.
[0153] In some possible implementations, H1 and T satisfy 0.81≤H1 / T≤5.
[0154] A large amount of experimental data shows that when H1 and T satisfy 0.81≤H1 / T≤5, the quality of graphitized products can be further improved.
[0155] In order to verify whether the above numerical ranges of D2 / D1 and H1 / T can improve the quality of graphitized products, the specific surface areas of graphitized products corresponding to different D2 / D1 and H1 / T ratios were measured.
[0156] Test Process 2: Unlike Test Process 1, this test used H1 of 1100 mm and D3 of 600 mm. The specific surface area of the graphitized product produced by the graphitization furnace was recorded for different D2 / D1 and H1 / T ratios. The D2 / D1 and H1 / T ratios and specific surface area test results are shown in Table 2. The specific surface area of the graphitized product can be directly measured using a specific surface area analyzer.
[0157] Table 2
[0158] It can be seen from Table 2 above that the outer diameter D2 and the inner diameter D1 of the annular electrode portion 231 satisfy 1.17≤D2 / D1≤3, and the specific surface area of the graphitized product is 1.1~1.3m 2 When the outer diameter D2 and the inner diameter D1 of the annular electrode portion 231 do not satisfy 1.17≤D2 / D1≤3, such as D2 / D1=1.14, the specific surface area of the graphitized product is not within the range of 1.1 to 1.3 m 2 / g range, which does not meet the requirements for battery negative electrode materials.
[0159] In addition, it can be seen from Table 2 above that when D2 and D1 satisfy 1.24≤D2 / D1≤2.51, the specific surface area of the graphitized product is far away from the specific surface area boundary value of 1.1m 2 / g and 1.3m 2 / g, the quality of graphitized products is more stable, and the quality of graphitized products can be further improved.
[0160] It can be seen from Table 2 above that H1 and T satisfy 0.6≤H1 / T≤7.4, and the specific surface area of the graphitized product is 1.1~1.3m 2 / g range, which meets the requirements for battery negative electrode materials. When H1 and T do not meet 0.6≤H1 / T≤7.4, such as H1 / T=8.46, the specific surface area of the graphitized product is not within the range of 1.1~1.3m 2 / g range, which does not meet the requirements for battery negative electrode materials.
[0161] In addition, it can be seen from Table 2 above that when H1 and T satisfy 0.81≤H1 / T≤5, the specific surface area of the graphitized product is far away from the specific surface area boundary value of 1.1m2 / g and 1.3m 2 / g, the quality of graphitized products is more stable, and the quality of graphitized products can be further improved.
[0162] In some possible embodiments, with continued reference to FIG. 2 to FIG. 4 , the first electrode 220 may be a cylindrical electrode with a diameter of D3 . D3 and the inner diameter D1 of the annular electrode portion 231 satisfy the following relationship: 1≤D1 / D3≤5.
[0163] Optionally, the first electrode 220 can be coaxially arranged with the material channel 211, that is, along the radial direction of the material channel 211, the first electrode 220 can be arranged at the center of the material channel 211. Of course, the first electrode 220 can also be arranged not coaxially with the material channel 211.
[0164] It should be understood that an umbrella-shaped electric field can be formed between the end surface 221 of the first electrode 220 and the surface of the annular electrode portion 231 facing the first electrode 220. When the ratio of the inner diameter D1 of the annular electrode portion 231 to the diameter D3 of the first electrode 220 is large, for example, when the inner diameter D1 is large and D3 is small, the uneven distribution of electric field intensity in the electric field becomes more pronounced, and the temperature of some areas within the electric field may not reach the temperature required for the graphitization process, thereby resulting in a low degree of graphitization of the graphitized product. When the ratio of the inner diameter D1 of the annular electrode portion 231 to the diameter D3 of the first electrode 220 is small, for example, when the inner diameter D1 is small and D3 is large, the shape of the electric field may change, i.e., it will not be umbrella-shaped, which can easily result in the electric field failing to centrally heat the material and failing to reach the temperature required for the graphitization process. This can result in a low degree of graphitization of the graphitized product, thereby reducing the quality of the graphitized product. Furthermore, the material is prone to clogging in the material channel 211, reducing the efficiency of graphitization.
[0165] In the embodiment of the present application, the diameter D3 of the first electrode 220 and the inner diameter D1 of the annular electrode portion 231 satisfy 1≤D1 / D3≤3.4. This not only forms an electric field with a relatively uniform electric field intensity distribution, but also allows the temperature of all regions within the electric field to reach the temperature required for the graphitization process as much as possible, thereby uniformly and effectively heating the material, thereby improving the quality of the graphitized product. It also facilitates the uniform flow of the material in the material channel 211, reducing the probability of material blockage.
[0166] In order to verify whether the numerical range of D1 / D3 can improve the quality of graphitized products, the graphitization degrees of graphitized products corresponding to different D1 / D3 ratios were measured.
[0167] Test Process 3: Unlike Test Process 1, this test used an H1 of 1100 mm, a D3 of 600 mm, and an outer diameter D2 of the annular electrode portion 231 of 1350 mm. The graphitization degree of the graphitized product produced by the graphitization furnace 200 was recorded at different D1 / D3 ratios. The D1 / D3 ratio and test results are shown in Table 3.
[0168] Table 3
[0169] As can be seen from Table 3 above, when the diameter D3 of the first electrode 220 and the inner diameter D1 of the annular electrode portion 231 satisfy 1≤D1 / D3≤3.4, the graphitization rate of the graphitized product is above 94%, far exceeding the qualified standard (90%), which can improve the quality of the graphitized product.
[0170] In some possible implementations, D1 and D3 satisfy 1≤D1 / D3≤2.
[0171] It can also be seen from Table 3 above that the diameter D3 of the first electrode 220 and the inner diameter D1 of the annular electrode portion 231 satisfy 1≤D1 / D3≤2, and the graphitization rate exceeds 95%, which can further improve the quality of the graphitized product.
[0172] In some possible implementations, with continued reference to FIG. 4 , the diameter D3 of the first electrode and the distance H1 between the end surface 221 of the first electrode 220 and the first plane may satisfy: 0.7≤H1 / D3≤4.7.
[0173] It should be understood that an umbrella-shaped electric field is formed between the end face 221 of the first electrode and the surface 2311 of the annular electrode portion 231. The electric field intensity near the end face 221 of the first electrode in the umbrella-shaped electric field is relatively high. In other words, the temperature in this area is higher than in other areas. If the ratio of H1 to D3 is too large, for example, H1 is large and D3 is small, the difference in electric field intensity between different areas in the electric field is greater, and the temperature difference is also greater. The temperature in some areas may not even reach the temperature required for the graphitization process, resulting in the material passing through this area having a substandard degree of graphitization. If the ratio of H1 to D3 is too small, for example, H1 is small and D3 is large, the electric field intensity in the electric field is low, and it may not be possible to reach the temperature required for the graphitization process, resulting in a substandard degree of graphitization.
[0174] In the embodiment of the present application, the diameter D3 of the first electrode 220 and the distance H1 between the end surface 221 of the first electrode 220 and the first plane satisfy 0.7≤H1 / D3≤4.7. This not only allows an electric field with a relatively uniform electric field intensity distribution to be formed between the end surface 221 of the first electrode 220 and the surface of the annular electrode portion 231 facing the end surface 221 of the first electrode 220, but also allows the temperature required for the graphitization process to be reached within the electric field, thereby uniformly and effectively heating the material passing through the electric field, thereby improving the quality of the graphitized product.
[0175] In order to verify whether the above numerical range of H1 / D3 can improve the quality of graphitized products, the graphitization degrees of graphitized products corresponding to different H1 / D3 ratios were measured.
[0176] Test Process 4: Unlike Test Process 1, this test used an H1 of 600 mm and a D1 of 900 mm. The graphitization degree of the graphitized product produced by the graphitization furnace 200 was recorded at different H1 / D3 ratios. The H1 / D3 ratio and test results are shown in Table 4.
[0177] Table 4
[0178] It can be seen from Table 4 above that when H1 and D3 satisfy 0.7≤H1 / D3≤4.7, the graphitization rate of the graphitized product is above 94%, which can improve the quality of the graphitized product.
[0179] In some possible implementations, H1 and D3 satisfy 0.7≤H1 / D3≤2.
[0180] It can also be seen from Table 4 above that when H1 and D3 satisfy 0.7≤H1 / D3≤2, the degree of graphitization exceeds 95%, which can further improve the quality of the graphitized product.
[0181] As shown in Figure 5, S1 is the cross-sectional area of the first electrode 220 along the radial direction of the material channel 211. S2 is the cross-sectional area of the annular electrode portion 231 along the radial direction of the material channel 211. It should be understood that S1 can be calculated based on the diameter D3 of the first electrode 220. S2 can be calculated based on the inner diameter D1 and outer diameter D2 of the annular electrode portion 231.
[0182] In some possible implementations, along the radial direction of the material channel 211 , the cross-sectional area S1 of the first electrode 220 and the cross-sectional area S2 of the annular electrode portion 231 satisfy: 0.8≤S2 / S1≤18.
[0183] Optionally, in some embodiments, the value range of S1 is 0.12 to 1.2 m 2 .
[0184] After a lot of experimental verification, S1 is between 0.12 and 1.2 m 2 range, which is conducive to forming a more concentrated electric field.
[0185] Optionally, in some embodiments, the value range of S2 is 0.15 to 2.5 m 2 .
[0186] After a lot of experimental verification, S2 is between 0.15 and 2.5m 2 range, which is conducive to forming a more concentrated electric field.
[0187] It should be understood that the size of the umbrella-shaped electric field region is related to the cross-sectional area S1 of the first electrode 220 along the radial direction of the material channel 211, and the cross-sectional area S2 of the annular electrode portion 231 along the radial direction of the material channel 211. When S2 / S1 is too large, for example, S2 is large and S1 is small, the electric field intensity in the area near the first electrode 220 is low, and the temperature required for the graphitization process may not be reached, resulting in a low degree of graphitization of the graphitized product and the inability to repair the pores of the graphitized product to an acceptable level. When S2 / S1 is too small, for example, S2 is small and S1 is large, the graphitization path of the material in the electric field is short, and the heating time is insufficient, resulting in the inability to repair the pores of the graphitized product to an acceptable level.
[0188] In the embodiment of the present application, the cross-sectional area S1 of the first electrode 220 and the cross-sectional area S2 of the annular electrode portion 221 along the radial direction of the material channel 211 satisfy 0.8≤S2 / S1≤18. This allows the temperature required for the graphitization process to be reached within the electric field, and allows the material to be heated for a sufficient time so that the pores of the graphitized product are repaired to an acceptable level, thereby improving the quality of the graphitized product.
[0189] In order to verify whether the above-mentioned numerical range of S2 / S1 can improve the quality of graphitized products, the specific surface areas of graphitized products corresponding to different S2 / S1 ratios were measured.
[0190] Test Procedure 5: Unlike Test Procedure 1, this test used an H1 of 1100 mm and a D1 of 900 mm. The specific surface area of the graphitized product was recorded for different S2 / S1 ratios. The S2 / S1 ratios and test results are shown in Table 5.
[0191] Table 5
[0192] It can be seen from Table 5 above that when S1 and S2 satisfy 0.8≤S2 / S1≤18, the specific surface area of the graphitized product is 1.1~1.3m 2 / g range, which meets the requirements for battery negative electrode materials.
[0193] In some possible implementations, S1 and S2 satisfy 1.2≤S2 / S1≤12.
[0194] It can also be seen from Table 5 above that when S1 and S2 satisfy 1.2≤S2 / S1≤12, the specific surface area of the graphitized product is far away from the specific surface area boundary value of 1.1m 2 / g and 1.3m 2 / g, that is, the quality of graphitized products is more stable and better, which can further improve the quality of graphitized products.
[0195] In some possible implementations, with continued reference to FIG. 5 , the contact surface area between the guide electrode portion 232 and the annular electrode portion 231 is S3 , the outer surface area of the annular electrode portion 231 is S4 , and S3 and S4 satisfy: 1.5≤S4 / S3≤8.
[0196] Optionally, the shape of the current-guiding electrode portion 232 may include but is not limited to a columnar shape, a rectangular parallelepiped, and the like.
[0197] Optionally, the guide electrode portion 232 and the annular electrode portion 231 may be an integrated structure, or the two may be independent structures connected to each other.
[0198] One end of the current-conducting electrode portion 232 connected to the power supply is located outside the furnace body and can be connected to the power supply via a connector. At least a portion of the current-conducting electrode portion 232 passes through the furnace body 210 to connect to the annular electrode portion 231 .
[0199] In the embodiment of the present application, the contact surface area S3 between the guiding electrode portion 232 and the annular electrode portion 231 is positively correlated with the cross-sectional area of the guiding electrode portion 232 along the extension direction of the material channel 211, that is, the thicker the guiding electrode portion 232, the larger S3, and the thinner the guiding electrode portion 232, the smaller S3.
[0200] Optionally, in some embodiments, the value range of S3 is 0.15 to 1.1 m 2 .
[0201] After a lot of experimental verification, S3 is between 0.15 and 1.1 m 2 Within this range, it is beneficial for a large current to pass through the contact surface between the annular electrode portion and the guide electrode portion, so that there is sufficient current density in the electric field.
[0202] Optionally, in some embodiments, the value range of S4 is 0.5 to 7 m 2 .
[0203] After a lot of experimental verification, S4 is between 0.5 and 7m 2 Within this range, the annular electrode portion is conducive to receiving a larger current density, thereby ensuring sufficient current density in the electric field.
[0204] When S4 / S3 is too large, for example, S4 is large and S3 is small, the current density passing through the contact surface S3 is small, and thus the current density in the electric field is small, resulting in the inability to reach the temperature required for the graphitization process in the electric field, and the quality of the graphitized product is reduced. When S4 / S3 is too small, the current is prone to bias flow, and the temperature difference between different areas in the electric field is obvious, resulting in poor consistency of the graphitized product, thereby reducing the quality of the graphitized product.
[0205] In the embodiment of the present application, the outer surface area S4 of the annular electrode portion 231 and the contact surface area S3 between the guide electrode portion 232 and the annular electrode portion 231 satisfy 1.5≤S4 / S3≤8, so that the contact surface area S3 can meet the current density requirement and reduce the current deviation phenomenon, thereby allowing the temperature required for the graphitization process to be reached in the electric field, thereby improving the quality of the graphitized product.
[0206] In order to verify whether the above numerical range can improve the quality of graphitized products, relevant evaluation parameters of graphitized products corresponding to different S4 / S3 ratios were measured.
[0207] Test Process 6: Unlike Test Process 1, this test used D2 = 1350 mm and H1 = 1100 mm, and recorded the graphitization degree of the graphitized products produced by the graphitization furnace at different S4 / S3 ratios. The S4 / S3 ratios and test results are shown in Table 6.
[0208] Table 6
[0209] It can be seen from Table 6 above that when S3 and S4 satisfy 1.5≤S4 / S3≤8, the graphitization rate of the graphitized product is above 94%, which can improve the quality of the graphitized product and far exceeds the standard value of graphitization degree.
[0210] In some possible implementations, S3 and S4 satisfy 3≤S4 / S3≤5.
[0211] It can be seen from Table 6 above that when S4 and S3 satisfy 3≤S4 / S3≤5, the graphitization rate exceeds 95%, which can further improve the quality of the graphitized product.
[0212] In some possible embodiments, with continued reference to FIG. 6 , along the radial direction of the material channel 211 , the bottom surface of the guide electrode portion 232 may be flush with the bottom surface of the annular electrode portion 231 , and along the extension direction of the material channel 211 , the height dimension of the annular electrode portion 231 is H2, and the height dimension of the guide electrode portion 232 is H3, and H2 and H3 satisfy: 1≤H2 / H3≤4.
[0213] It should be understood that when the material channel 211 is in an inverted trapezoidal shape, as shown in FIG6 , because the furnace body 210 is not completely insulated, an electric field can be generated between the first electrode 220 and the annular electrode portion 231, as well as between the first electrode 220 and the conductive electrode portion 232. To further concentrate the electric field and thereby centrally heat the material, the height dimension H2 of the annular electrode portion 231 can be made greater than the height dimension H3 of the conductive electrode portion 232. This allows the electric field to be generated as little as possible between the first electrode 220 and the annular electrode portion 231. If H2 is less than H3, that is, the annular electrode portion 231 is lower than the conductive electrode portion 232, an electric field may form between the side surfaces of the first electrode 220 and the conductive electrode portion 232, resulting in a larger electric field coverage area and lower current density, which is not conducive to centralized heating of the material and affects the quality of the graphitized product. However, H2 / H3 cannot be too large, that is, the annular electrode portion 231 cannot be too high compared to the conducting electrode portion 232. Although the annular electrode portion 231 is higher than the conducting electrode portion 232, it is beneficial for the electric field to be formed between the first electrode 220 and the annular electrode portion 231, but being too high will increase the manufacturing cost of the annular electrode portion 231.
[0214] In the embodiment of the present application, the height dimension H2 of the annular electrode portion 231 and the height dimension H3 of the guide electrode portion 232 satisfy 1≤H2 / H3≤4. This not only takes into account the manufacturing cost of the annular electrode portion 231, but also forms a more concentrated electric field to centrally heat the material, thereby improving the quality of the graphitized product.
[0215] In some possible implementations, H2 and H3 satisfy: 1≤H2 / H3≤1.8.
[0216] A large amount of experimental data shows that the height dimension H2 of the annular electrode portion 231 and the height dimension H3 of the guide electrode portion 232 satisfy 1≤H2 / H3≤1.8, and the graphitization rate can reach more than 93.5%, which can further improve the quality of the graphitized product.
[0217] In some possible implementations, as shown in FIG. 7 , the graphitization furnace 200 may further include a first thermal insulation layer 240 . The thermal insulation layer 240 is disposed at the innermost side of the furnace body 210 and forms a partial channel section of the material channel 211 .
[0218] The first thermal insulation layer 240 is an insulating thermal insulation layer, and its resistivity is much greater than that of graphite.
[0219] In the above embodiment, by providing the first insulation layer 240, the temperature of the heating zone formed between the first electrode 220 and the second electrode 230 can be insulated, so that the heating zone is maintained in a high temperature range, the degree of graphitization of the material is uniform, and the consistency of the graphitized product can be improved.
[0220] In some possible implementations, the thermal conductivity of the first insulation layer 240 is 0.05-5 w / mk.
[0221] The greater the thermal conductivity of the material, the better the thermal conductivity and the worse the heat preservation effect. The above embodiment makes the thermal conductivity lower, which can reduce the heat loss of the graphitization furnace 200, thereby improving energy utilization.
[0222] In some possible implementations, the compressive strength of the first thermal insulation layer 240 is 0.1-40 MPa.
[0223] The higher the compressive strength, the less likely the object is to crack or pulverize. By setting the compressive strength of the first insulation layer 240, the first insulation layer 240 can have a higher strength support function, thereby increasing the service life of the graphitization furnace 200.
[0224] In some possible implementations, the first thermal insulation layer 240 has a temperature resistance of 1800-3200°C.
[0225] Temperature resistance refers to the ability of an object to withstand changes in external temperature without being damaged or significantly reduced in its usability. By ensuring the temperature resistance of the first insulation layer 240, the first insulation layer 240 can have a higher degree of heat resistance, thereby increasing the service life of the graphitization furnace.
[0226] In some possible implementations, as shown in FIG. 7 , the graphitization furnace 200 may further include a second thermal insulation layer 250 , which is disposed on a side of the first thermal insulation layer 240 facing the outside of the furnace body 210 .
[0227] The second insulation layer 250 is a carbon insulation layer. By arranging the second insulation layer 250 outside the first insulation layer 240, the temperature of the heating zone formed between the first electrode 220 and the second electrode 230 can be further insulated, so that the heating zone is maintained in a high temperature range, the degree of graphitization of the material is uniform, and the consistency of the graphitized product can be further improved.
[0228] In some possible implementations, the thermal conductivity of the second insulation layer 250 is 0.1-20 W / mK. A lower thermal conductivity can reduce heat loss in the graphitization furnace 200, thereby improving energy utilization.
[0229] In some possible implementations, the compressive strength of the second thermal insulation layer 250 is 20-60 MPa.
[0230] In the above embodiment, by setting the compressive strength of the second thermal insulation layer 250 , the second thermal insulation layer 250 can have a high-strength supporting effect, thereby increasing the service life of the graphitization furnace 200 .
[0231] In some possible implementations, the second thermal insulation layer 250 has a temperature resistance of 1500-3200°C.
[0232] In the above embodiment, by setting the temperature resistance of the second thermal insulation layer 250 , the second thermal insulation layer 250 can have a higher intensity of temperature resistance, thereby increasing the service life of the graphitization furnace 200 .
[0233] In some possible implementations, the ash content of the second thermal insulation layer 250 is 0.1% to 10%.
[0234] Ash content refers to the amount of solid elements other than carbon and graphite in an object. Excessive ash content can affect the object's quality. By adjusting the ash content of the second insulation layer 250, the impact of excessive ash content on the quality of the second insulation layer 250 can be reduced, thereby increasing the service life of the graphitization furnace 200.
[0235] In some possible implementations, as shown in FIG. 7 , the graphitization furnace further includes a third thermal insulation layer 260 , which is disposed on a side of the second thermal insulation layer 250 facing the outside of the furnace body 210 .
[0236] By providing the third thermal insulation layer 260 outside the second thermal insulation layer 250 , the energy loss of the first thermal insulation layer 240 and the second thermal insulation layer 250 can be reduced, thereby improving energy utilization and thermal insulation effect.
[0237] In some possible embodiments, the third insulation layer 260 contains more than 30% alumina. In the above embodiment, by providing the third insulation layer 260 with alumina, the third insulation layer 260 can have a certain anti-oxidation function, thereby improving the service life of the graphitization furnace 200.
[0238] In some possible implementations, the compressive strength of the third thermal insulation layer 260 is 5 to 60 MPa.
[0239] In the above embodiment, by setting the compressive strength of the third thermal insulation layer 260 , the third thermal insulation layer 260 can have a higher strength supporting effect, thereby increasing the service life of the graphitization furnace.
[0240] In some possible implementations, the third insulation layer 260 has a temperature resistance of 1000-2000° C. In the above implementations, by setting the temperature resistance of the third insulation layer 260 , the third insulation layer 260 can have a higher degree of heat resistance, thereby increasing the service life of the graphitization furnace.
[0241] The present application also provides a battery production system, comprising the graphitization furnace 200 in any of the above embodiments, wherein the graphitization furnace 200 is used to produce negative electrode graphite materials for batteries.
[0242] It is understandable that the battery production system may include, in addition to the graphitization furnace 200 for producing the negative electrode graphite material of the battery, related equipment for producing other battery materials.
[0243] The battery production system may be a battery production line, and a plurality of devices in the battery production line may be arranged in the same centralized location, or may be arranged in separate locations.
[0244] Although the present application has been described with reference to preferred embodiments, various modifications may be made thereto and components may be substituted with equivalents without departing from the scope of the present application. In particular, the various technical features described in the various embodiments may be combined in any manner as long as there are no structural conflicts. The present application is not limited to the specific embodiments disclosed herein, but encompasses all technical solutions within the scope of the claims.
Claims
1. A graphitization furnace, It is characterized in that include: A furnace body (210), wherein a material channel (211) is provided in the furnace body (210); a first electrode (220), at least a portion of the first electrode (220) being located in the material channel (211); a second electrode (230) having a polarity opposite to that of the first electrode, comprising an annular electrode portion (231), the annular electrode portion (231) being protrudingly disposed on an inner wall (2111) of the material channel (211) along a radial direction of the material channel (211) and surrounding a partial channel section of the material channel (211); Along the extension direction of the material channel (211), the distance between the end surface (221) of the first electrode (220) facing the second electrode (230) and the first plane is H1, the inner diameter of the annular electrode portion (231) is D1, and H1 and D1 satisfy: 0.5≤H1 / D1≤5; The first plane is the plane where the surface (2311) of the annular electrode portion (231) facing the first electrode (220) is located.
2. The graphitization furnace according to claim 1, It is characterized in that H1 and D1 satisfy: 0.8≤H1 / D1≤1.
5.
3. The graphitization furnace according to claim 1 or 2, It is characterized in that The value range of H1 is 350~3000mm.
4. The graphitization furnace according to any one of claims 1 to 3, It is characterized in that The value range of D1 is 430~2400mm.
5. The graphitization furnace according to any one of claims 1 to 4, It is characterized in that The outer diameter of the annular electrode portion (231) is D2, and D1 and D2 satisfy: 1.17≤D2 / D1≤3.
6. The graphitization furnace according to claim 5, It is characterized in that D1 and D2 satisfy: 1.24≤D2 / D1≤2.
51.
7. The graphitization furnace according to claim 5 or 6, It is characterized in that The value range of D2 is 580~2750mm.
8. The graphitization furnace according to any one of claims 1 to 7, It is characterized in that Along the radial direction of the material channel (211), the thickness dimension of the annular electrode portion (231) is T, and H1 and T satisfy: 0.6≤H1 / T≤7.
4.
9. The graphitization furnace according to claim 8, It is characterized in that H1 and T satisfy: 0.81≤H1 / T≤5.
10. The graphitization furnace according to claim 8 or 9, It is characterized in that The value range of T is 130~1500mm.
11. The graphitization furnace according to any one of claims 1 to 10, It is characterized in that The first electrode (220) is a cylindrical electrode, the diameter of the first electrode (220) is D3, and D3 and D1 satisfy: 1≤D1 / D3≤3.
4.
12. The graphitization furnace according to claim 11, It is characterized in that D3 and D1 satisfy: 1≤D1 / D3≤2.
13. The graphitization furnace according to claim 11 or 12, It is characterized in that The value range of D3 is 350~1200mm.
14. The graphitization furnace according to any one of claims 1 to 13, It is characterized in that The first electrode (220) is a cylindrical electrode, the diameter of the first electrode (220) is D3, and D3 and H1 satisfy: 0.7≤H1 / D3≤4.
7.
15. The graphitization furnace according to claim 14, It is characterized in that D3 and H1 satisfy: 0.7≤H1 / D3≤2.
16. The graphitization furnace according to any one of claims 1 to 15, It is characterized in that Along the radial direction of the material channel (211), the cross-sectional area of the first electrode (220) is S1, the cross-sectional area of the annular electrode portion (231) is S2, and S1 and S2 satisfy: 0.8≤S2 / S1≤18.
17. The graphitization furnace according to claim 16, It is characterized in that S1 and S2 satisfy: 1.2≤S2 / S1≤12.
18. The graphitization furnace according to claim 16 or 17, It is characterized in that The value range of S1 is 0.12~1.2m 2 .
19. The graphitization furnace according to any one of claims 16 to 18, It is characterized in that The value range of S2 is 0.15~2.5m 2 .
20. The graphitization furnace according to any one of claims 1 to 19, It is characterized in that The second electrode (230) further includes a current-conducting electrode portion (232); One end of the current-conducting electrode portion (232) is connected to the annular electrode portion (231), and the other end of the current-conducting electrode portion (232) is connected to a power source; The contact surface area between the guide electrode portion (232) and the annular electrode portion (231) is S3, the outer surface area of the annular electrode portion (231) is S4, and S3 and S4 satisfy: 1.5≤S4 / S3≤8.
21. The graphitization furnace according to claim 20, It is characterized in that S3 and S4 satisfy: 3≤S4 / S3≤5.
22. The graphitization furnace according to claim 20 or 21, It is characterized in that The value range of S3 is 0.15~1.1m 2 .
23. The graphitization furnace according to any one of claims 20 to 22, It is characterized in that The value range of S4 is 0.5~7m 2 .
24. The graphitization furnace according to any one of claims 20 to 23, It is characterized in that Along the radial direction of the material channel (211), the bottom surface of the guide electrode portion (232) is flush with the bottom surface of the annular electrode portion (231); Along the extension direction of the material channel (211), the height dimension of the annular electrode portion (231) is H2, and the height dimension of the guide electrode portion (232) is H3, and H2 and H3 satisfy: 1≤H2 / H3≤4.
25. The graphitization furnace according to claim 24, It is characterized in that H2 and H3 satisfy: 1≤H2 / H3≤1.
8.
26. The graphitization furnace according to claim 24 or 25, It is characterized in that The value range of H2 is 400~2000mm.
27. The graphitization furnace according to any one of claims 24 to 26, It is characterized in that The value range of H3 is: 350~1200mm.
28. The graphitization furnace according to any one of claims 1 to 27, It is characterized in that The graphitization furnace further comprises a first heat-insulating layer (240), which is arranged at the innermost side of the furnace body (210) and forms a partial channel section of the material channel (211).
29. The graphitization furnace according to claim 28, It is characterized in that The thermal conductivity of the first thermal insulation layer (240) is 0.05-5w / mk; or The compressive strength of the first thermal insulation layer (240) is 0.1-40 MPa; or The first thermal insulation layer (240) has a temperature resistance of 1800 to 3200°C.
30. The graphitization furnace according to claim 28 or 29, It is characterized in that The graphitization furnace further comprises a second thermal insulation layer (250) disposed on a side of the first thermal insulation layer (240) facing the outside of the furnace body (210).
31. The graphitization furnace according to claim 30, It is characterized in that The thermal conductivity of the second thermal insulation layer (250) is 0.1-20w / mk; or The compressive strength of the second thermal insulation layer (250) is 20-60 MPa; or The second thermal insulation layer (250) has a temperature resistance of 1500-3200° C.; or The ash content of the second thermal insulation layer (250) is 0.1% to 10%.
32. The graphitization furnace according to claim 30 or 31, It is characterized in that The graphitization furnace further comprises a third thermal insulation layer (260) disposed on a side of the second thermal insulation layer (250) facing the outside of the furnace body (210).
33. The graphitization furnace according to claim 32, It is characterized in that The third thermal insulation layer (260) contains more than 30% alumina; or The compressive strength of the third thermal insulation layer (260) is 5 to 60 MPa; or The third thermal insulation layer (260) has a temperature resistance of 1000-2000°C.
34. A battery production system, It is characterized in that include: The graphitization furnace according to any one of claims 1 to 33, wherein the graphitization furnace is used to produce negative electrode graphite material for a battery.
Citation Information
Patent Citations
Novel graphitizing furnace
CN105967180A
Electro-calcining high temperature graphitization furnace
CN109081336A
Positive and negative electrode structure of vertical graphitization furnace
CN114166035A
Vertical continuous for graphitizing furnace electrode assembly
CN208022707U
Two-stage heating type vertical graphitization furnace and method for producing graphite
JP2015189645A
Cited By
Negative electrode material graphitized flue gas multi-pollutant efficient treatment and resource utilization method based on waste heat gradient utilization
CN121498412A