Display substrate and preparation method therefor, and display device

By setting isolation grooves and barrier layers in the transition area of ​​the display substrate to prevent water vapor and oxygen from penetrating, the problem of reduced reliability of OLED display packaging is solved and the stability and long life of the packaging are improved.

WO2024222318A1PCT designated stage expired Publication Date: 2024-10-31BOE TECHNOLOGY GROUP CO LTD +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/082377
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2024-03-19
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

During the thin film packaging process of OLED displays, the packaging reliability is affected by the penetration of water vapor and oxygen into the organic evaporated film layer after cutting, resulting in a decrease in packaging reliability. It is especially difficult to ensure the stability of the packaging at the opening position.

Method used

A display substrate is designed, including a hole area, a transition area surrounding the hole area, and a display area. The transition area is provided with an isolation structure, including an isolation groove and a barrier layer. By forming grooves and filling layers in the transition area, water vapor and oxygen are prevented. penetration to improve package reliability.

Benefits of technology

It effectively cuts off the luminescent functional film layer in the transition area, prevents water vapor and oxygen from penetrating into the display area, improves the packaging reliability of the OLED display, and ensures the stability and long life of the packaging.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024082377_31102024_PF_FP_ABST
    Figure CN2024082377_31102024_PF_FP_ABST
Patent Text Reader

Abstract

A display substrate and a preparation method therefor, and a display device. The display substrate comprises a hole region, a transition region surrounding the hole region, and a display region surrounding the transition region, wherein the transition region is provided with an isolation structure surrounding the hole region, and the isolation structure comprises at least one isolation groove; the display substrate comprises a base, and the isolation groove comprises a groove and a blocking edge arranged on the side of the groove away from the base; and in a direction perpendicular to the base, the transition region comprises a first structure layer and a second structure layer which are sequentially stacked in the direction away from the base, the first structure layer comprises a blocking layer, the groove extends through the second structure layer and exposes at least part of the surface of the blocking layer, the blocking edge is arranged on the surface of the second structure layer away from the base, and part of the blocking edge extends in a direction parallel to the base and protrudes from a side wall of the groove.
Need to check novelty before this filing date? Find Prior Art

Description

Display substrate and manufacturing method thereof, and display device

[0001] This application claims priority to the Chinese patent application filed with the China Patent Office on April 28, 2023, with application number 202310486035.X and invention name “A display substrate, its preparation method, and display device”, the contents of which should be understood as incorporated into this application by reference. Technical Field

[0002] The present disclosure relates to, but is not limited to, the field of display technology, and specifically to a display substrate and a preparation method thereof, and a display device. Background Art

[0003] As smartphones rapidly develop towards full-screen displays, the screen-to-body ratio requirements are becoming increasingly higher, and the market demand for perforated screens is increasing. Semiconductor packaging technologies to meet this demand are also constantly developing. Currently, thin film encapsulation (TFE) is a commonly used packaging technology for organic light-emitting diode (OLED) displays. Due to the packaging reliability requirements of TFE, no evaporated light-emitting functional film layer is allowed below the edge of the TFE layer. Otherwise, after cutting, water vapor, oxygen, etc. will penetrate into the interior of the OLED display through the organic evaporated film layer on the cut section, affecting the reliability of the OLED display packaging. Therefore, how to improve the packaging reliability of thin film encapsulation at the opening position in the OLED display has become an urgent problem to be solved.

[0004] Summary of the Invention

[0005] The following is a summary of the subject matter described in detail herein. This summary is not intended to limit the scope of the claims.

[0006] An embodiment of the present disclosure provides a display substrate, comprising a hole area, a transition area surrounding the hole area, and a display area surrounding the transition area; the transition area is provided with an isolation structure surrounding the hole area, the isolation structure comprising at least one isolation groove;

[0007] The display substrate includes a base, the isolation groove includes a groove and a blocking edge provided on the side of the groove away from the base; in a direction perpendicular to the base, the transition zone includes a first structural layer and a second structural layer stacked in sequence in a direction away from the base, the first structural layer includes a blocking layer, the groove penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer, the blocking edge is provided on the surface of the second structural layer away from the base, and a portion of the blocking edge extends in a direction parallel to the base and protrudes from the sidewall of the groove.

[0008] An embodiment of the present disclosure further provides a display device, comprising the display substrate.

[0009] The present disclosure also provides a method for preparing the display substrate, including:

[0010] forming a first structural layer and a second structural layer in sequence on the substrate of the transition region, wherein the first structural layer includes a barrier layer, and the second structural layer is provided with a groove, wherein the groove penetrates the second structural layer and exposes at least a portion of the surface of the barrier layer;

[0011] forming a filling layer in the groove, wherein the filling layer fills the groove;

[0012] forming a retaining edge on a surface of the second structural layer away from the substrate, wherein a portion of the retaining edge extends in a direction parallel to the substrate to a surface of the filling layer away from the substrate;

[0013] The filling layer is removed.

[0014] Still other aspects will become apparent upon reading and understanding the accompanying drawings and detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] The accompanying drawings are intended to provide a further understanding of the technical solutions of the present disclosure and constitute a part of the specification. Together with the embodiments of the present disclosure, they are used to explain the technical solutions of the present disclosure and do not constitute a limitation of the technical solutions of the present disclosure. The shapes and sizes of the components in the accompanying drawings do not reflect the actual scale and are intended only to illustrate the contents of the present disclosure.

[0016] FIG1 is a schematic diagram of a planar structure of a display substrate according to some exemplary embodiments;

[0017] FIG2 a is a schematic diagram of the AA cross-sectional structure in FIG1 in some exemplary embodiments;

[0018] FIG2 b is a schematic diagram of the AA cross-sectional structure in FIG1 in some other exemplary embodiments;

[0019] FIG2 c is a schematic diagram of the AA cross-sectional structure in FIG1 in some further exemplary embodiments;

[0020] FIG3 is a schematic diagram of the AA cross-sectional structure in FIG1 in some further exemplary embodiments;

[0021] FIG4 is a schematic diagram of the AA cross-sectional structure in FIG1 in some further exemplary embodiments;

[0022] FIG5 is a schematic diagram of the AA cross-sectional structure in FIG1 in some further exemplary embodiments;

[0023] FIG6 is a schematic diagram of the AA cross-sectional structure in FIG1 in some further exemplary embodiments;

[0024] FIG7 a is a schematic structural diagram of a display substrate after forming a second interlayer insulating layer according to some exemplary embodiments;

[0025] FIG7 b is a schematic structural diagram of a display substrate after forming a first source / drain metal layer according to some exemplary embodiments;

[0026] FIG7 c is a schematic structural diagram of a display substrate after forming a first planarization layer according to some exemplary embodiments;

[0027] FIG7 d is a schematic structural diagram of a display substrate after forming a second source / drain metal layer according to some exemplary embodiments;

[0028] FIG7e is a schematic structural diagram of a display substrate after forming a pixel defining layer according to some exemplary embodiments;

[0029] FIG7 f is a schematic structural diagram of a display substrate after the filling layer is removed according to some exemplary embodiments;

[0030] FIG8 a is a schematic structural diagram of a display substrate after forming a third gate insulating layer according to some exemplary embodiments;

[0031] FIG8 b is a schematic structural diagram of a display substrate after forming a third gate metal layer according to some exemplary embodiments;

[0032] FIG8 c is a schematic structural diagram of a display substrate after forming a second interlayer insulating layer according to some exemplary embodiments;

[0033] FIG8 d is a schematic structural diagram of a display substrate after forming a first source / drain metal layer according to some exemplary embodiments;

[0034] FIG8e is a schematic structural diagram of a display substrate after forming a first planarization layer according to some exemplary embodiments;

[0035] FIG8 f is a schematic structural diagram of a display substrate after forming a second source / drain metal layer according to some exemplary embodiments;

[0036] FIG8g is a schematic structural diagram of a display substrate after forming a first electrode according to some exemplary embodiments;

[0037] FIG8h is a schematic structural diagram of a display substrate after forming a pixel defining layer according to some exemplary embodiments;

[0038] FIG8i is a schematic structural diagram of a display substrate after a filling layer is removed according to some exemplary embodiments;

[0039] FIG9 a is a schematic structural diagram of a display substrate after forming a second interlayer insulating layer according to some exemplary embodiments;

[0040] FIG9 b is a schematic structural diagram of a display substrate after forming a first source / drain metal layer according to some exemplary embodiments;

[0041] FIG9 c is a schematic structural diagram of a display substrate after forming a first planarization layer according to some exemplary embodiments;

[0042] FIG9 d is a schematic structural diagram of a display substrate after forming a second source / drain metal layer according to some exemplary embodiments;

[0043] FIG9e is a schematic structural diagram of a display substrate after forming a first electrode according to some exemplary embodiments;

[0044] FIG9 f is a schematic structural diagram of a display substrate after forming a pixel defining layer according to some exemplary embodiments;

[0045] FIG. 9 g is a schematic structural diagram of a display substrate after the filling layer is removed according to some exemplary embodiments.

[0046] Figure numerals: 10, substrate, 20, driving structure layer, 21, first buffer layer, 22, first gate insulating layer, 23, second gate insulating layer, 24, first interlayer insulating layer, 25, third gate insulating layer, 26, second interlayer insulating layer, 27, first flat layer, 28, second flat layer, 30, light-emitting structure layer, 31, first electrode, 32, pixel defining layer, 33, light-emitting function layer, 34, second electrode layer, 40, packaging structure layer, 41, first packaging layer, 42, second packaging layer, 43, third packaging layer, 50, isolation structure, 51, isolation groove, 52, isolation column, 60, isolation dam, 71, first isolation layer, 72, retaining wall, 73, second isolation layer, 81, first groove, 82, second groove, 83, third groove, 84, first metal ring, 85, second metal ring, 86, first A blocking edge, 87, a second blocking edge, 91, a first convex ring, 92, a second convex ring, 100, a display area, 200, a hole area, 201, a first transistor, 202, a second transistor, 203, a storage capacitor, 204, a connecting electrode, 261, a first sublayer, 262, a second sublayer, 271, a filling layer, 300, a transition region, 511, a groove, 512, a blocking edge, 513, a blocking layer, 514, a convex ring, 521, a first isolation portion, 522, a second isolation portion, 523, a column base, 2011, a first active layer, 2012, a first gate electrode, 2013, a first source electrode, 2014, a first drain electrode, 2021, a second active layer, 2022, a second gate electrode, 2023, a second source electrode, 2024, a second drain electrode, 2031, a first plate, 2032, a second plate. DETAILED DESCRIPTION

[0047] Those skilled in the art should understand that the technical solutions of the embodiments of the present disclosure may be modified or replaced by equivalents without departing from the spirit and scope of the technical solutions of the embodiments of the present disclosure, and all should be included in the scope of the claims of the present disclosure.

[0048] As shown in Figures 1, 2a and 2b, Figure 1 is a schematic diagram of the planar structure of a display substrate of some exemplary embodiments, Figure 2a is a schematic diagram of the AA cross-sectional structure in Figure 1 in some exemplary embodiments, and Figure 2b is a schematic diagram of the AA cross-sectional structure in Figure 1 in other exemplary embodiments. The display substrate includes a hole area 200, a transition area 300 surrounding the hole area 200, and a display area 100 surrounding the transition area 300.

[0049] Exemplarily, the display area 100 includes a driving structure layer 20 , a light emitting structure layer 30 and an encapsulation structure layer 40 sequentially stacked on a substrate 10 .

[0050] The driving structure layer 20 includes multiple pixel driving circuits, each of which includes multiple transistors (T) and storage capacitors 203 (C). FIG2 a illustrates a first transistor 201. The pixel driving circuit may adopt a 3T1C, 4T1C, 5T1C, 5T2C, 6T1C, or 7T1C structure, which is not limited in this disclosure.

[0051] The light-emitting structure layer 30 includes a plurality of light-emitting elements, and the light-emitting element can be an OLED (organic light-emitting diode) or a QLED (quantum dot light-emitting diode) device. The light-emitting element includes a first electrode 31, a light-emitting functional layer 33, and a second electrode layer 34 stacked in sequence in a direction away from the substrate 10. The light-emitting functional layer 33 includes an organic light-emitting layer, and may also include any one or more film layers of a hole injection layer, a hole transport layer, and an electron blocking layer located between the first electrode 31 and the organic light-emitting layer, and any one or more film layers of an electron injection layer, an electron transport layer, and a hole blocking layer located between the second electrode layer 34 and the organic light-emitting layer. The first electrode 31 of the light-emitting element is connected to the pixel driving circuit, and the light-emitting element emits light under the drive of the pixel driving circuit. In a direction perpendicular to the substrate 10, the light-emitting structure layer 30 includes a first electrode layer, a pixel defining layer 32, a light-emitting functional layer 33 and a second electrode layer 34 arranged in sequence; the first electrode layer includes a plurality of first electrodes 31, the pixel defining layer 32 is arranged on the side of the plurality of first electrodes 31 away from the substrate 10 and is provided with a plurality of pixel openings, the pixel openings expose the first electrodes 31, and the light-emitting functional layer 33 and the second electrode layer 34 are stacked in sequence on the side of the first electrode 31 away from the substrate 10.

[0052] The encapsulation structure layer 40 may include a first encapsulation layer 41, a second encapsulation layer 42, and a third encapsulation layer 43 stacked in sequence in a direction away from the substrate 10. The main materials (the material with the largest component in the film layer) of the first encapsulation layer 41 and the third encapsulation layer 43 are inorganic materials, which may include silicon oxide (SiOx), silicon nitride (SiNx), and silicon oxynitride (SiO X N Y), the primary material of the second encapsulation layer 42 can be an organic material, such as epoxy resin, which facilitates encapsulation and prevents moisture erosion. The first encapsulation layer 41 and the third encapsulation layer 43 can be formed using a chemical vapor deposition (CVD) process, and the second encapsulation layer 42 can be formed using an inkjet printing (IJP) process.

[0053] Exemplarily, the transition region 300 is provided with an isolation structure 50 surrounding the hole region 200. The isolation structure 50 is configured to isolate the light-emitting functional layer 33 and the second electrode layer 34 of the transition region 300, thereby preventing water and oxygen from corroding from the hole region 200 along the light-emitting functional layer 33 and the second electrode layer 34 toward the display region 100, thereby protecting the light-emitting functional layer 33 and the second electrode layer 34 of the display region 100 from water and oxygen corrosion. The isolation structure 50 may include at least one isolation trench 51 (shown in FIG. 2 b ) and / or at least one isolation pillar 52 (shown in FIG. 2 a ), and both the isolation pillar 52 and the isolation trench 51 are provided around the hole region 200. The number of the isolation structures 50 may be one or more, and the embodiment of the present disclosure does not limit the number of isolation structures 50.

[0054] The transition region 300 may also be provided with an isolation dam 60, which is provided around the hole region 200. During the process of forming the second encapsulation layer 42 of the encapsulation structure layer 40 using an inkjet printing process, the inkjet printing material may overflow, and the isolation dam 60 may prevent the inkjet printing material from overflowing. The surface of the isolation dam 60 away from the substrate 10 is higher than the surface of the isolation column 52 away from the substrate 10. The number of isolation dams 60 may be one or more, and the embodiment of the present disclosure does not limit the number of isolation dams 60. At least one isolation structure 50 may be located on the side of the isolation dam 60 facing the display region 100 or / and on the side of the isolation dam 60 facing the hole region 200.

[0055] In some exemplary embodiments, as shown in Figures 2a and 2b, in a direction perpendicular to the substrate 10, the driving structure layer 20 may include a first buffer layer 21, a first semiconductor layer, a first gate insulating layer 22, a first gate metal layer, a second gate insulating layer 23, a second gate metal layer, a first interlayer insulating layer 24, a first source-drain metal layer, a first planarizing layer 27, a second source-drain metal layer, and a second planarizing layer 28, which are arranged in sequence along a direction away from the substrate 10; the first semiconductor layer may include a first active layer 2011 of the first transistor 201, the first gate metal layer may include a first gate electrode 2012 of the first transistor 201 and one plate of the storage capacitor 203, the second gate metal layer may include another plate of the storage capacitor 203, the first source-drain metal layer includes a first source electrode 2013 and a first drain electrode 2014 of the first transistor 201, and the second source-drain metal layer includes a connecting electrode 204 connected to the first source electrode 2013 or the first drain electrode 2014 of the first transistor 201, and the connecting electrode 204 is also connected to the first electrode 31.

[0056] In some examples of this embodiment, as shown in Figure 2a, the isolation structure 50 may include at least one isolation column 52, which is arranged around the hole area. The isolation column 52 may include a first isolation portion 521 and a second isolation portion 522 arranged in sequence along a direction away from the substrate 10. On the side of the isolation column 52 facing the display area 100 and / or the hole area 200, the second isolation portion 522 is protruding from the first isolation portion 521.

[0057] The material of the first isolation portion 521 can be an inorganic insulating material. The first isolation portion 521 can be provided in the same layer as the first interlayer insulating layer 24. The first interlayer insulating layer 24 can have a single-layer structure or a multi-layer structure. For example, the first interlayer insulating layer 24 can include a silicon oxide film layer and a silicon nitride film layer stacked in sequence in a direction away from the substrate 10. The first isolation portion 521 includes a silicon oxide film layer and a silicon nitride film layer stacked in sequence in a direction away from the substrate 10. The thickness of the silicon nitride film layer can be 0.5 μm to 1 μm (micrometer), for example, 0.8 μm.

[0058] The second isolation portion 522 may be made of a metal material. The second isolation portion 522 may be provided on the same layer as the first source electrode 2013 and the first drain electrode 2014 of the first transistor 201; or, the second isolation portion 522 may be provided on the same layer as the connecting electrode 204; or, the second isolation portion 522 may include a first sub-isolation portion and a second sub-isolation portion stacked sequentially in a direction away from the substrate 10, wherein the first sub-isolation portion may be provided on the same layer as the first source electrode 2013 and the first drain electrode 2014 of the first transistor 201, and the second sub-isolation portion may be provided on the same layer as the connecting electrode 204.

[0059] In this embodiment, the thickness of the first interlayer insulating layer 24 can be designed to be thicker (for example, in some examples, the thickness of the silicon nitride film layer in the first interlayer insulating layer 24 can be designed to be thicker). Accordingly, the thickness of the first isolation portion 521 is thicker, which is beneficial to improving the isolation effect of the isolation column 52 on the light-emitting functional layer 33 and the second electrode layer 34, and avoiding the light-emitting functional layer 33 located on both sides of the isolation column 52 after being isolated by the isolation column 52 to be connected into a conductive path through the second isolation portion 522 with conductive function of the isolation column 52, thereby avoiding the resulting poor display.

[0060] Herein, "A and B are provided in the same layer" means that the film layers of A and B are derived from the same thin film, which can be a single-layer structure or a multi-layer composite structure, and the film layers of A and B can be the same or different. "A and B are provided in the same layer" can be understood as simultaneously forming A and B from the same thin film through the same patterning process, or simultaneously forming A' and B' from the same thin film through the same patterning process, and then further processing (such as etching) of A' to obtain A, and further processing (such as etching) of B' to obtain B.

[0061] In some examples of this embodiment, as shown in Figure 2b, the isolation structure 50 may include at least one isolation groove 51, which is arranged around the hole area, and the isolation groove 51 includes a groove 511 and a blocking edge 512 arranged on the side of the groove 511 away from the substrate 10. In the direction perpendicular to the substrate 10, the transition zone 300 includes a first structural layer and a second structural layer stacked in sequence along the direction away from the substrate 10, the first structural layer includes a blocking layer 513, the groove 511 penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer 513 (the surface away from the substrate 10), the blocking edge 512 is arranged on the surface of the second structural layer away from the substrate 10, and a portion of the blocking edge 512 extends in a direction parallel to the substrate 10 and protrudes from the sidewall of the groove 511.

[0062] The blocking layer 513 may be provided in the same layer as the first active layer 2011 (first semiconductor layer) of the first transistor 201. The second structural layer may include a plurality of stacked inorganic insulating layers, for example, a first inorganic insulating layer, a second inorganic insulating layer, and a third inorganic insulating layer stacked in sequence in a direction away from the substrate 10, wherein the first inorganic insulating layer is provided in the same layer as the first gate insulating layer 22, the second inorganic insulating layer is provided in the same layer as the second gate insulating layer 23, and the third inorganic insulating layer is provided in the same layer as the first interlayer insulating layer 24.

[0063] The dam 512 may be provided at the same layer as the connection electrode 204 . Alternatively, the dam 512 may be provided at the same layer as the first source electrode 2013 and the first drain electrode 2014 .

[0064] The orthographic projection of the retaining edge 512 on the substrate 10 may include the orthographic projection of the edge of the barrier layer 513 away from the groove 511 on the substrate 10. Alternatively, the orthographic projection of the retaining edge 512 on the substrate 10 may fall within the orthographic projection of the barrier layer 513 on the substrate 10. This is not limited in this embodiment.

[0065] In this embodiment, by providing an isolation trench 51 surrounding the aperture region 200 in the transition region 300, the organic light-emitting functional film layer deposited in the transition region 300 can be isolated, thereby preventing external moisture and oxygen from invading the display region 100 through the aperture region 200 and the organic light-emitting functional film layer, thereby ensuring packaging reliability. In addition, the barrier layer 513 can help control the structural morphology of the groove 511 during the etching process. For example, the sidewalls of the groove 511 near the barrier layer 513 can be further recessed away from the center of the groove 511, thereby improving the isolation effect of the isolation trench 511.

[0066] In some exemplary embodiments, as shown in FIG. 2c , which is a schematic diagram of the AA cross-sectional structure in FIG. 1 in yet other exemplary embodiments, the isolation structure 50 may include multiple isolation trenches 51 (three isolation trenches 51 are shown in FIG. 2c ). The isolation trenches 51 are disposed around the aperture region and include a groove 511 and a retaining edge 512 disposed on the side of the groove 511 away from the substrate 10. In a direction perpendicular to the substrate 10, the transition region 300 includes a first structural layer and a second structural layer stacked sequentially in a direction away from the substrate 10. The first structural layer includes a barrier layer 513. The groove 511 penetrates the second structural layer and exposes at least a portion of the surface of the barrier layer 513 (the surface away from the substrate 10). The retaining edge 512 is disposed on the surface of the second structural layer away from the substrate 10, with a portion of the retaining edge 512 extending parallel to the substrate 10 and protruding beyond the sidewalls of the groove 511. Each isolation trench 51 may include two retaining edges 512, one located on either side of the groove 511.

[0067] The isolation structure 50 may further include at least one isolation column 52; the isolation column 52 includes a first isolation portion 521 and a second isolation portion 522 arranged in sequence along a direction away from the substrate 10, and on the side of the isolation column 52 facing the display area 100 and / or the hole area 200, the second isolation portion 522 is protruding from the first isolation portion 521.

[0068] An isolation column 52 may be formed between two adjacent isolation trenches 51. The retaining edge 512 and the second isolation portion 522 may be provided on the same layer and made of the same material. The second structural layer between two adjacent grooves 511 serves as the first isolation portion 521. The second isolation portion 522 of an isolation column 52 may serve as one of the retaining edges 512 of two adjacent isolation trenches 51.

[0069] The two adjacent barrier layers 513 may not be connected, and at least a portion of the orthographic projection of the second isolation portion 522 on the substrate 10 may not overlap with the orthographic projections of the two adjacent barrier layers 513 on the substrate 10 .

[0070] In other embodiments, at least two adjacent barrier layers 513 may be connected as one, and the orthographic projection of the at least two adjacent barrier layers 513 connected as one on the substrate 10 may include the orthographic projection of at least one isolation column 52 on the substrate 10. In this embodiment, multiple barrier layers 513 in FIG. 2 c may be connected as one.

[0071] In some exemplary embodiments, as shown in Figures 3 and 4, Figure 3 is a schematic diagram of the AA cross-sectional structure in Figure 1 in some further exemplary embodiments, and Figure 4 is a schematic diagram of the AA cross-sectional structure in Figure 1 in some further exemplary embodiments. In a direction perpendicular to the substrate 10, the driving structure layer 20 may include a first buffer layer 21, a first semiconductor layer, a first gate insulating layer 22, a first gate metal layer, a second gate insulating layer 23, a second gate metal layer, a first interlayer insulating layer 24, a second semiconductor layer, a third gate insulating layer 25, a third gate metal layer, a second interlayer insulating layer 26, a first source-drain metal layer, a first planar layer 27, a second source-drain metal layer, and a second planar layer 28, which are sequentially arranged in a direction away from the substrate 10; the first semiconductor layer may include a first active layer 2011 of the first transistor 201, the first gate metal layer The layer may include a first gate electrode 2012 of the first transistor 201 and one plate of the storage capacitor 203, the second gate metal layer may include another plate of the storage capacitor 203, the second semiconductor layer may include a second active layer 2021 of the second transistor 202, the third gate metal layer may include a second gate electrode 2022 of the second transistor 202, the first source-drain metal layer includes a first source electrode 2013 and a first drain electrode 2014 of the first transistor 201, and a second source electrode 2023 and a second drain electrode 2024 of the second transistor 202, the second source-drain metal layer includes a connecting electrode 204 connected to the first source electrode 2013 or the first drain electrode 2014 of the first transistor 201, and the connecting electrode 204 is also connected to the first electrode 31.

[0072] In some examples of this embodiment, the display substrate may be a low-temperature polycrystalline oxide (LTPO) display substrate, and the multiple transistors of the pixel driving circuit may include low-temperature polycrystalline silicon (LTPS) thin-film transistors and oxide thin-film transistors. The oxide thin-film transistors may be indium gallium zinc oxide (IGZO) thin-film transistors. The first transistor 201 may be a low-temperature polycrystalline silicon thin-film transistor, and the material of the first active layer 2011 is low-temperature polycrystalline silicon. The second transistor 202 may be an indium gallium zinc oxide thin-film transistor, and the material of the second active layer 2021 is indium gallium zinc oxide. In other embodiments, the display substrate may be a low-temperature polycrystalline silicon display substrate, and the transistors of the display substrate are low-temperature polycrystalline silicon thin-film transistors. The embodiments of the present disclosure do not limit the type of display substrate and the type of transistors.

[0073] In some exemplary embodiments, the first buffer layer 21, the first gate insulating layer 22, the second gate insulating layer 23, the first interlayer insulating layer 24, the third gate insulating layer 25 and the second interlayer insulating layer 26 may be inorganic insulating layers, and may be made of silicon oxide (SiOx), silicon nitride (SiNx) and silicon oxynitride (SiOX N Y ), and may be a single-layer structure or a multi-layer composite structure. The first flat layer 27 and the second flat layer 28 may be organic insulating layers, and may be made of resin material. The materials of the first gate metal layer, the second gate metal layer, the third gate metal layer, the first source-drain metal layer and the second source-drain metal layer may be any one or more of silver (Ag), copper (Cu), aluminum (Al), titanium (Ti) and molybdenum (Mo), or alloy materials of the above metals, such as aluminum-neodymium alloy (AlNd) or molybdenum-niobium alloy (MoNb), and may be a single-layer structure or a multi-layer composite structure, such as Mo / Cu / Mo, Ti / Al / Ti, etc. The first semiconductor layer and the second semiconductor layer may be made of amorphous indium gallium zinc oxide material (a-IGZO), zinc oxynitride (ZnON), indium zinc tin oxide (IZTO), amorphous silicon (a-Si), polycrystalline silicon (p-Si), sexithiophene or polythiophene, etc.

[0074] In some exemplary embodiments, the substrate 10 may be a flexible substrate or a rigid substrate. The rigid substrate may be glass, quartz, etc., and the flexible substrate may include one or more of polyethylene terephthalate, polyethylene terephthalate, polyetheretherketone, polystyrene, polycarbonate, polyarylate, polyarylate, polyimide, polyvinyl chloride, polyethylene, and textile fibers.

[0075] In some exemplary embodiments, the first source-drain metal layer may include a first metal layer, a second metal layer, and a third metal layer sequentially arranged in a direction away from the substrate. The first and third metal layers may be titanium layers, and the second metal layer may be an aluminum layer. The second source-drain metal layer may include a fourth metal layer, a fifth metal layer, and a sixth metal layer sequentially arranged in a direction away from the substrate. The fourth and sixth metal layers may be titanium layers, and the fifth metal layer may be an aluminum layer. In other embodiments, the first source-drain metal layer and the second source-drain metal layer may have a single-layer structure.

[0076] In some examples of this embodiment, as shown in Figures 3 and 4, the isolation structure 50 may include at least one isolation groove 51, which is arranged around the hole area, and the isolation groove 51 includes a groove 511 and a blocking edge 512 arranged on the side of the groove 511 away from the substrate 10. In a direction perpendicular to the substrate 10, the transition zone 300 includes a first structural layer and a second structural layer stacked in sequence along a direction away from the substrate 10, the first structural layer includes a blocking layer 513, the groove 511 penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer 513, the blocking edge 512 is arranged on the surface of the second structural layer away from the substrate 10, and a portion of the blocking edge 512 extends in a direction parallel to the substrate 10 and protrudes from the sidewall of the groove 511.

[0077] For example, as shown in FIG3 , the blocking layer 513 can be provided in the same layer as the second active layer 2021 (second semiconductor layer) of the second transistor 202. The second structural layer can include multiple stacked inorganic insulating layers, such as a first inorganic insulating layer and a second inorganic insulating layer stacked sequentially away from the substrate 10. The first inorganic insulating layer is provided in the same layer as the third gate insulating layer 25, and the second inorganic insulating layer is provided in the same layer as the second interlayer insulating layer 26. The barrier rib 512 can be provided in the same layer as the connecting electrode 204.

[0078] Alternatively, as shown in FIG4 , the blocking layer 513 may be provided in the same layer as the first active layer 2011 (first semiconductor layer) of the first transistor 201. The second structural layer may include a plurality of stacked inorganic insulating layers, such as a first inorganic insulating layer, a second inorganic insulating layer, a third inorganic insulating layer, a fourth inorganic insulating layer, and a fifth inorganic insulating layer stacked sequentially in a direction away from the substrate 10. The first inorganic insulating layer is provided in the same layer as the first gate insulating layer 22, the second inorganic insulating layer is provided in the same layer as the second gate insulating layer 23, the third inorganic insulating layer is provided in the same layer as the first interlayer insulating layer 24, the fourth inorganic insulating layer is provided in the same layer as the third gate insulating layer 25, and the fifth inorganic insulating layer is provided in the same layer as the second interlayer insulating layer 26. The blocking edge 512 may be provided in the same layer as the connecting electrode 204.

[0079] In other embodiments, the barrier layer 513 may be provided in the same layer as the first gate metal layer, the second gate metal layer, or the third gate metal layer; or the barrier layer 513 may be an inorganic insulating layer, such as a SiOx layer. The second structural layer may include multiple stacked inorganic insulating layers; and the barrier edge 512 may be provided in the same layer as the connecting electrode 204.

[0080] In some exemplary embodiments, as shown in Figure 5, Figure 5 is a schematic diagram of the AA cross-sectional structure in Figure 1 in some further exemplary embodiments, the isolation structure 50 may include at least one isolation groove 51, the isolation groove 51 is arranged around the hole area, the isolation groove 51 includes a groove 511 and a blocking edge 512 arranged on the side of the groove 511 away from the substrate 10, in a direction perpendicular to the substrate 10, the transition zone 300 includes a first structural layer and a second structural layer stacked in sequence along a direction away from the substrate 10, the first structural layer includes a blocking layer 513, the groove 511 penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer 513, the blocking edge 512 is arranged on the surface of the second structural layer away from the substrate 10, and a portion of the blocking edge 512 extends in a direction parallel to the substrate 10 and protrudes from the sidewall of the groove 511.

[0081] For example, as shown in FIG5 , one or more raised rings 514 are provided on the sidewall of the groove 511. The multiple raised rings 514 are sequentially arranged in a direction perpendicular to the substrate 10. The groove 511 forms a groove between adjacent raised rings 514, and a groove is formed between the retaining edge 512 and the raised ring 514. For example, a first raised ring 91 and a second raised ring 92 are sequentially arranged on the sidewall of the groove 511 in a direction perpendicular to the substrate 10. In this example, by providing one or more raised rings 514 on the sidewall of the groove 511, the light-emitting functional layer 33 can be disconnected at the position of at least one raised ring 514, thereby improving the isolation effect of the isolation groove 51. In addition, when the encapsulation layer of inorganic material is subsequently deposited, the encapsulation material can have a better slope on the sidewall of the groove 511, making the encapsulation more dense and improving the encapsulation effect.

[0082] For example, as shown in FIG5 , the retaining edge 512 can be provided in the same layer as the connecting electrode 204 (second source-drain metal layer). The film layer of the retaining edge 512 can be the same as the film layer of the connecting electrode 204. The second source-drain metal layer can be a single-layer structure or a multi-layer structure, then the retaining edge 512 and the connecting electrode 204 can be a single-layer structure or a multi-layer structure. For example, the second source-drain metal layer can include a fourth metal layer, a fifth metal layer, and a sixth metal layer arranged in sequence in a direction away from the substrate 10, the fourth metal layer and the sixth metal layer can be a titanium layer, and the fifth metal layer can be an aluminum layer. Then, the retaining edge 512 and the connecting electrode 204 both include a fourth metal layer, a fifth metal layer, and a sixth metal layer arranged in sequence in a direction away from the substrate 10. On the side of the retaining edge 512 close to the groove 511, the fifth metal layer can be set inward compared to the fourth metal layer and the sixth metal layer (that is, the fourth metal layer and the sixth metal layer are set protruding compared to the fifth metal layer).

[0083] For example, as shown in FIG5 , the second interlayer insulating layer 26 may include a first sublayer 261 and a second sublayer 262 sequentially disposed in a direction away from the substrate 10 . The first sublayer 261 may be made of silicon oxide, and the second sublayer 262 may be made of silicon nitride. The at least one raised ring 514 may be disposed in the same layer and material as the first sublayer 261 .

[0084] 5 , the barrier layer 513 may be disposed in the same layer as the second active layer 2021 of the second transistor 202. In other embodiments, the barrier layer 513 may be disposed in the same layer as the first active layer 2011, the first gate metal layer, the second gate metal layer, or the third gate metal layer of the first transistor 201.

[0085] For example, as shown in FIG5 , the second structural layer may include at least one inorganic insulating layer and at least one metal layer, and the metal layer in the second structural layer may be provided in the same layer as the third gate metal layer. The raised ring 514 may be formed by the inorganic insulating layer in the second structural layer. In other embodiments, any metal layer in the second structural layer may be provided in the same layer as the third gate metal layer, the second gate metal layer, or the first gate metal layer.

[0086] In some exemplary embodiments, as shown in Figure 6, Figure 6 is a schematic diagram of the AA cross-sectional structure in Figure 1 in some further exemplary embodiments. The isolation structure 50 may include at least one isolation column 52, and the isolation column 52 is arranged around the hole area. The isolation column 52 may include a first isolation portion 521 and a second isolation portion 522 arranged in sequence along a direction away from the substrate 10. On the side of the isolation column 52 facing the display area 100 and / or the hole area 200, the second isolation portion 522 is protruding from the first isolation portion 521.

[0087] For example, as shown in FIG6 , the materials of the first isolation portion 521 and the second isolation portion 522 can both be metal materials. The first isolation portion 521 can include a first metal layer, a second metal layer, and a third metal layer sequentially arranged in a direction away from the substrate 10, and on the side of the isolation column 52 facing the display area 100 or / and the hole area 200, the second metal layer is set back relative to the first metal layer and the third metal layer; or / and, the second isolation portion 522 can include a fourth metal layer, a fifth metal layer, and a sixth metal layer sequentially arranged in a direction away from the substrate 10, and on the side of the isolation column 52 facing the display area 100 or / and the hole area 200, the fifth metal layer is set back relative to the fourth metal layer and the sixth metal layer. Compared with some technologies in which the isolation column 52 only includes the first isolation part 521 or the second isolation part 522, the isolation column 52 in this example can improve the isolation effect of the isolation column 52 and enhance the strength of the isolation column 52 by setting the first isolation part 521 and the second isolation part 522.

[0088] The fourth metal layer may be disposed on a surface of the third metal layer away from the substrate 10 , and on a side of the isolation column 52 facing the display area 100 and / or the hole area 200 , the fourth metal layer may be protruded more than the third metal layer.

[0089] The first isolation portion 521 may be provided in the same layer as the first source electrode and the first drain electrode (in the same layer as the first source-drain metal layer), and the second isolation portion 522 may be provided in the same layer as the connection electrode 204 (in the second source-drain metal layer). The first and third metal layers of the first isolation portion 521 may be titanium layers, and the second metal layer may be an aluminum layer. The fourth and sixth metal layers of the second isolation portion 522 may be titanium layers, and the fifth metal layer may be an aluminum layer.

[0090] For example, as shown in FIG6 , the isolation column 52 may further include a column base 523 disposed on the side of the first isolation portion 521 facing the substrate 10. The column base 523 may include at least one inorganic insulating layer. For example, the column base 523 may include multiple stacked inorganic insulating layers, or the column base 523 may include at least one inorganic insulating layer and at least one metal layer, and the metal layer in the column base 523 may be covered by the inorganic insulating layer in the column base 523.

[0091] 6 , the transition region 300 is further provided with a barrier layer 513, and the isolation pillar 52 is provided on a surface of the barrier layer 513 away from the substrate 10. The barrier layer 513 can be provided in the same layer as the first active layer 2011, the first gate electrode 2012, any one plate of the storage capacitor 203, the second active layer 2021, or the second gate electrode 2022.

[0092] 6 , the isolation structure 50 may include a plurality of isolation pillars 52, with one isolation trench 51 formed between two adjacent isolation pillars 52. Similarly, the isolation structure 50 may include a plurality of isolation trenches 51, with one isolation pillar 52 formed between two adjacent isolation trenches 51.

[0093] The structure of the display substrate is exemplified below by the preparation process of the display substrate. The "patterning process" mentioned in this disclosure includes processes such as coating photoresist, mask exposure, development, etching, and stripping photoresist for metal materials, inorganic materials, or transparent conductive materials, and includes processes such as coating organic materials, mask exposure, and development for organic materials. Deposition can be carried out by any one or more of sputtering, evaporation, and chemical vapor deposition, coating can be carried out by any one or more of spraying, spin coating, and inkjet printing, and etching can be carried out by any one or more of dry etching and wet etching, which are not limited in this disclosure. "Thin film" refers to a layer of thin film made by deposition, coating, or other processes on a substrate of a certain material. If the "thin film" does not require a patterning process during the entire production process, the "thin film" can also be called a "layer". If the "thin film" requires a patterning process during the entire production process, it is called a "thin film" before the patterning process and a "layer" after the patterning process. The "layer" after the patterning process contains at least one "pattern". The "thickness" of the film layer is the size of the film layer in the direction perpendicular to the display substrate. In the exemplary embodiments of the present disclosure, "the orthographic projection of B is within the range of the orthographic projection of A" or "the orthographic projection of A contains the orthographic projection of B" means that the boundary of the orthographic projection of B falls within the boundary range of the orthographic projection of A, or the boundary of the orthographic projection of A overlaps with the boundary of the orthographic projection of B.

[0094] In some exemplary embodiments, taking the display substrate shown in FIG. 3 as an example, the preparation process of the display substrate may include the following operations:

[0095] (1) The driving structure layer 20 and the film layer of the isolation groove 51 are formed.

[0096] A first buffer film and a first semiconductor film are sequentially deposited on the substrate 10. The first semiconductor film is patterned through a patterning process to form a first buffer layer 21 covering the substrate 10 and a first semiconductor layer pattern disposed on the first buffer layer 21. The first semiconductor layer pattern includes a plurality of first active layers 2011 located in the display area 100. After this patterning process, the transition region 300 includes the first buffer layer 21 disposed on the substrate 10, as shown in Figure 7a.

[0097] Subsequently, a first gate insulating film and a first gate metal film are sequentially deposited. The first gate metal film is patterned through a patterning process to form a first gate insulating layer 22 covering the first semiconductor layer pattern, and a first gate metal layer pattern disposed on the first gate insulating layer 22. The first gate metal layer pattern includes a plurality of first gate electrodes 2012 and a plurality of first electrode plates 2031 located in the display area 100. After this patterning process, the transition region 300 includes a first buffer layer 21 and a first gate insulating layer 22 sequentially stacked on the substrate 10, as shown in Figure 7a.

[0098] Subsequently, a second gate insulating film and a second gate metal film are sequentially deposited and patterned through a patterning process to form a second gate insulating layer 23 covering the first gate metal layer, and a second gate metal layer pattern disposed on the second gate insulating layer 23. The second gate metal layer pattern includes a plurality of second electrodes 2032 located in the display area 100. The plurality of second electrodes 2032 are disposed opposite the plurality of first electrodes 2031 and form a plurality of storage capacitors 203. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, and a second gate insulating layer 23 sequentially stacked on the substrate 10, as shown in Figure 7a.

[0099] Subsequently, a first interlayer insulating film and a second semiconductor film are deposited, and the second semiconductor film is patterned through a patterning process to form a first interlayer insulating layer 24 covering the second gate metal layer pattern, and a second semiconductor layer pattern disposed on the first interlayer insulating layer 24. The second semiconductor layer pattern includes multiple second active layers 2021 located in the display area 100 and a barrier layer 513 located in the transition region 300. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, and a barrier layer 513 disposed on the first interlayer insulating layer 24, which are sequentially stacked on the substrate 10, as shown in Figure 7a.

[0100] Subsequently, a third gate insulating film and a third gate metal film are sequentially deposited and patterned through a patterning process to form a third gate insulating layer 25 covering the second semiconductor layer pattern and a third gate metal layer pattern disposed on the third gate insulating layer 25. The third gate metal layer pattern includes a plurality of second gate electrodes 2022 located in the display area 100. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, a barrier layer 513, and a third gate insulating layer 25 covering the barrier layer 513, stacked sequentially on the substrate 10, as shown in Figure 7a.

[0101] Subsequently, a second interlayer insulating film is deposited and patterned through a patterning process to form a second interlayer insulating layer 26 pattern covering the third gate metal layer pattern. The second interlayer insulating layer 26 in the display area 100 is provided with a plurality of first via holes V1, a plurality of second via holes V2, a plurality of third via holes V3, and a plurality of fourth via holes V4. The plurality of first via holes V1 expose one end of the plurality of first active layers 2011, the plurality of second via holes V2 expose the other end of the plurality of first active layers 2011, the plurality of third via holes V3 expose one end of the plurality of second active layers 2021, and the plurality of fourth via holes V4 expose the other end of the plurality of second active layers 2021. The second interlayer insulating layer 26 in the transition area 300 is provided with a groove 511 that penetrates the third gate insulating layer 25 and exposes the barrier layer 513. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, a barrier layer 513, a third gate insulating layer 25 covering the barrier layer 513, and a second interlayer insulating layer 26 disposed on the third gate insulating layer 25, which are sequentially stacked on the substrate 10. The second interlayer insulating layer 26 in the transition region 300 has a recess 511 that penetrates the third gate insulating layer 25 and exposes the barrier layer 513, as shown in FIG. 7a .

[0102] Subsequently, a first source-drain metal film is deposited and patterned through a patterning process to form a first source-drain metal layer pattern on the second interlayer insulating layer 26. The first source-drain metal layer pattern includes a plurality of first source electrodes 2013, a plurality of first drain electrodes 2014, a plurality of second source electrodes 2023 and a plurality of second drain electrodes 2024 located in the display area 100. The first source electrode 2013 is connected to one end of the first active layer 2011 through a first via hole V1, the first drain electrode 2014 is connected to the other end of the first active layer 2011 through a second via hole V2, the second source electrode 2023 is connected to one end of the second active layer 2021 through a third via hole V3, and the second drain electrode 2024 is connected to the other end of the second active layer 2021 through a fourth via hole V4. The plurality of first active layers 2011, the plurality of first gate electrodes 2012, the plurality of first source electrodes 2013, and the plurality of first drain electrodes 2014 of the display area 100 form a plurality of first transistors 201, and the plurality of second active layers 2021, the plurality of second gate electrodes 2022, the plurality of second source electrodes 2023, and the plurality of second drain electrodes 2024 form a plurality of second transistors 202. As shown in FIG. 7B , FIG. 7B illustrates one first transistor 201 and one second transistor 202.

[0103] The first source-drain metal layer may include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10. For example, the first metal layer and the third metal layer may be titanium layers, and the second metal layer may be an aluminum layer. The first source electrode 2013, the first drain electrode 2014, the second source electrode 2023, and the second drain electrode 2024 each include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10.

[0104] Subsequently, a first planarizing film is applied and patterned through a patterning process to form a first planarizing layer 27 pattern covering the first source / drain metal layer pattern. The first planarizing layer 27 has a fifth via hole V5 defined in the display area 100. The first planarizing layer 27 within the fifth via hole V5 is removed, exposing the surface of the first source electrode 2013 or the first drain electrode 2014. The first planarizing layer 27 pattern includes a filling layer 271 located in the transition region 300 and filling the groove 511. The filling layer 271 can fill the groove 511, as shown in FIG. 7c .

[0105] Subsequently, a second source / drain metal film is deposited and patterned using a patterning process to form a second source / drain metal layer pattern on the first planar layer 27. The second source / drain metal layer pattern includes multiple anode connection electrodes 204 located in the display area 100 and multiple ridges 512 located in the transition area 300. The anode connection electrode 204 is connected to the first source electrode 2013 or the first drain electrode 2014 through a fifth via V5. The multiple ridges 512 include a first ridge 86 and a second ridge 87. The first ridge 86 is located on the second interlayer insulating layer 26 on the side of the groove 511 facing the display area 100, with a portion of the first ridge 86 located on the filling layer 271. The second ridge 87 is located on the second interlayer insulating layer 26 on the side of the groove 511 facing the hole region, with a portion of the second ridge 87 located on the filling layer 271. The distance between the first ridge 86 and the second ridge 87 in a direction parallel to the substrate 10 is less than the width of the notch of the groove 511, as shown in FIG. 7d.

[0106] Among them, the film layer structure and material of the second source-drain metal layer can be the same as the film layer structure and material of the first source-drain metal layer. For example, the second source-drain metal layer can include a fourth metal layer, a fifth metal layer and a sixth metal layer stacked in sequence in a direction away from the substrate 10. For example, the fourth metal layer and the sixth metal layer can be titanium layers, and the fifth metal layer can be an aluminum layer.

[0107] Subsequently, a second planar film is applied and patterned using a patterning process to form a second planar layer 28 pattern covering the second source / drain metal layer pattern in the display area 100. The second planar layer 28 exposes the multiple ridges 512 in the transition area 300 and the filling layer 271 in the groove 511. The second planar layer 28 is formed with multiple sixth via holes in the display area 100. The second planar layer 28 in the sixth via holes is removed, exposing the surface of the anode connection electrode 204, as shown in FIG. 7e.

[0108] At this point, the driving structure layer 20 and the film layer of the isolation trench 51 are completed.

[0109] (2) Forming the light emitting structure layer 30. In an exemplary embodiment, forming the light emitting structure layer 30 may include:

[0110] A first electrode 31 thin film is deposited on the substrate 10 having the aforementioned pattern formed thereon. The first electrode 31 thin film is patterned through a patterning process to form a first electrode layer pattern. The first electrode layer pattern includes a plurality of first electrodes 31 (anodes) located in the display area 100. The first electrodes 31 are connected to the anode connection electrode 204 through the sixth via hole in the second planar layer 28. Thus, the first electrodes 31 are connected to the first source electrode 2013 or the first drain electrode 2014 through the anode connection electrode 204, as shown in FIG. 7e.

[0111] Subsequently, a pixel defining film is coated on the substrate 10 having the aforementioned pattern formed thereon. The pixel defining film is patterned through a patterning process to form a pixel defining layer 32. The pixel defining layer 32 is provided with a plurality of pixel openings, which expose the surface of the first electrode 31 of the display area 100, as shown in FIG7e.

[0112] Subsequently, an etching process is used to remove the filling layer 271 in the groove 511. For example, oxygen etching can be used, as shown in FIG7f.

[0113] Subsequently, on the substrate 10 formed with the aforementioned pattern, multiple film layers of the light-emitting functional layer 33 can be sequentially formed through an evaporation process. The light-emitting functional layer 33 can include a hole injection layer, a hole transport layer, an electron blocking layer, an organic light-emitting layer, a hole blocking layer, an electron transport layer, and an electron injection layer, which are sequentially arranged in a direction away from the substrate 10. Except for the organic light-emitting layer, the remaining film layers of the light-emitting functional layer 33 can all be an integrated, full-surface structure. That is, the remaining film layers of the light-emitting functional layer 33 can be common layers for sub-pixels of different colors. These common layers can be formed in the display area 100 and the transition area 300 during evaporation. Since the isolation groove 51 is provided in the transition area 300, these common layers will be disconnected at the isolation groove 51, blocking the path for water and oxygen to be transmitted from the hole area 200 through the light-emitting functional layer 33 to the display area 100, thereby preventing water and oxygen from corroding the light-emitting functional layer 33 in the display area 100. As shown in Figure 3.

[0114] Subsequently, a second electrode (cathode) layer is formed on the patterned substrate 10 through an evaporation process. The second electrode layer 34 of the sub-pixels of different colors is a common layer connected into an integrated structure. The second electrode layer 34 can be formed in the display area 100 and the transition area 300. The second electrode layer 34 can be disconnected at the isolation trench 51, blocking the path for water and oxygen to transmit from the hole area 200 through the second electrode layer 34 to the display area 100, thereby preventing water and oxygen from corroding the second electrode layer 34 in the display area 100. This is shown in Figure 3.

[0115] At this point, the light emitting structure layer 30 is completed.

[0116] (3) Forming the encapsulation structure layer 40. In an exemplary embodiment, forming the encapsulation structure layer 40 may include:

[0117] On the substrate 10 with the aforementioned pattern, a first encapsulation film is first deposited using an open reticle to form a first encapsulation layer 41 located in the display area 100 and transition area 300. Subsequently, a second encapsulation material is printed using an open reticle using an inkjet printing process to form a second encapsulation layer 42 located in the display area 100 and transition area 300. Isolation dams 60 in the transition area 300 prevent ink overflow during the inkjet printing process. Subsequently, a third encapsulation film is deposited using an open reticle to form a third encapsulation layer 43 located in the display area 100 and transition area 300. The materials for the first and third encapsulation layers 41 and 43 can be inorganic materials, while the material for the second encapsulation layer 42 can be organic materials, as shown in Figure 3.

[0118] Subsequently, film layers such as a touch structure layer and a color filter layer may be formed in sequence on the side of the encapsulation structure layer 40 away from the substrate 10 .

[0119] In some other exemplary embodiments, taking the display substrate shown in FIG. 5 as an example, the preparation process of the display substrate may include the following operations:

[0120] (1) The driving structure layer 20 and the film layer of the isolation groove 51 are formed.

[0121] A first buffer film and a first semiconductor film are sequentially deposited on the substrate 10. The first semiconductor film is patterned through a patterning process to form a first buffer layer 21 covering the substrate 10 and a first semiconductor layer pattern disposed on the first buffer layer 21. The first semiconductor layer pattern includes multiple first active layers 2011 located in the display area 100. After this patterning process, the transition region 300 includes the first buffer layer 21 disposed on the substrate 10, as shown in Figure 8a.

[0122] Subsequently, a first gate insulating film and a first gate metal film are sequentially deposited. The first gate metal film is patterned through a patterning process to form a first gate insulating layer 22 covering the first semiconductor layer pattern, and a first gate metal layer pattern disposed on the first gate insulating layer 22. The first gate metal layer pattern includes a plurality of first gate electrodes 2012 and a plurality of first electrode plates 2031 located in the display area 100. After this patterning process, the transition region 300 includes a first buffer layer 21 and a first gate insulating layer 22 sequentially stacked on the substrate 10, as shown in Figure 8a.

[0123] Subsequently, a second gate insulating film and a second gate metal film are sequentially deposited and patterned through a patterning process to form a second gate insulating layer 23 covering the first gate metal layer, and a second gate metal layer pattern disposed on the second gate insulating layer 23. The second gate metal layer pattern includes a plurality of second electrodes 2032 located in the display area 100. The plurality of second electrodes 2032 are disposed opposite the plurality of first electrodes 2031 and form a plurality of storage capacitors 203. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, and a second gate insulating layer 23 sequentially stacked on the substrate 10, as shown in FIG8a.

[0124] Subsequently, a first interlayer insulating film and a second semiconductor film are deposited, and the second semiconductor film is patterned through a patterning process to form a first interlayer insulating layer 24 covering the second gate metal layer pattern, and a second semiconductor layer pattern disposed on the first interlayer insulating layer 24. The second semiconductor layer pattern includes multiple second active layers 2021 located in the display area 100 and a barrier layer 513 located in the transition region 300. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, and a barrier layer 513 disposed on the first interlayer insulating layer 24, which are sequentially stacked on the substrate 10, as shown in Figure 8a.

[0125] Subsequently, a third gate insulating film is sequentially deposited and patterned through a patterning process to form a third gate insulating layer 25 pattern covering the second semiconductor layer pattern. The third gate insulating layer 25 in the transition region 300 is provided with a first groove 81 surrounding the hole region 200. The first groove 81 at least partially exposes the barrier layer 513, as shown in FIG8 a.

[0126] Subsequently, a third gate metal film is deposited and patterned through a patterning process to form a third gate metal layer pattern located on the third gate insulating layer 25. The third gate metal layer pattern includes a plurality of second gate electrodes 2022 located in the display area 100, and a first metal ring 84 and a second metal ring 85 located in the transition area 300. The first metal ring 84 and the second metal ring 85 are located on the side of the first groove 81 near the display area 100 and the side near the hole area 200, respectively. The edges of the first metal ring 84 and the second metal ring 85 near the first groove 81 are recessed relative to the sidewalls of the first groove 81. The portion of the third gate insulating layer 25 protruding from the edge of the first metal ring 84 near the first groove 81 forms a first raised ring 91, and the portion of the third gate insulating layer 25 protruding from the edge of the second metal ring 85 near the first groove 81 forms another first raised ring 91. A second groove 82 is formed between the first metal ring 84 and the second metal ring 85, as shown in FIG. 8b .

[0127] Subsequently, a second interlayer insulating film is deposited and patterned by a patterning process to form a second interlayer insulating layer 26 pattern covering the third gate metal layer pattern. The second interlayer insulating layer 26 may include a first sublayer 261 and a second sublayer 262 stacked in sequence in a direction away from the substrate 10. The material of the first sublayer 261 may be silicon oxide, and the material of the second sublayer 262 may be silicon nitride. The second interlayer insulating layer 26 of the display area 100 is provided with a plurality of first vias V1, a plurality of second vias V2, a plurality of third vias V3 and a plurality of fourth vias V4. The plurality of first vias V1 expose one end of the plurality of first active layers 2011, the plurality of second vias V2 expose the other end of the plurality of first active layers 2011, the plurality of third vias V3 expose one end of the plurality of second active layers 2021, and the plurality of fourth vias V4 expose the other end of the plurality of second active layers 2021; the second interlayer insulating layer 26 of the transition area 300 is provided with a first via hole 81 exposing the first groove 81 and the second groove 82. Three grooves 83 are formed. On the sidewalls of the third groove 83, the first sublayer 261 protrudes from the second sublayer 262. (During the etching process, the etching solution or etching gas has different selectivity ratios for the first sublayer 261 and the second sublayer 262, thereby forming a stepped sidewall of the third groove 83.) A second raised ring 92 is formed on the sidewall of the third groove 83 near the display area 100, where the first sublayer 261 protrudes from the second sublayer 262. Another second raised ring 92 is formed on the sidewall of the third groove 83 near the hole area 200, where the first sublayer 261 protrudes from the second sublayer 262. The two second raised rings 92 also protrude from the first metal ring 84 and the second metal ring 85, respectively, as shown in FIG8c.

[0128] Subsequently, a first source-drain metal film is deposited and patterned through a patterning process to form a first source-drain metal layer pattern on the second interlayer insulating layer 26. The first source-drain metal layer pattern includes a plurality of first source electrodes 2013, a plurality of first drain electrodes 2014, a plurality of second source electrodes 2023 and a plurality of second drain electrodes 2024 located in the display area 100. The first source electrode 2013 is connected to one end of the first active layer 2011 through a first via hole V1, the first drain electrode 2014 is connected to the other end of the first active layer 2011 through a second via hole V2, the second source electrode 2023 is connected to one end of the second active layer 2021 through a third via hole V3, and the second drain electrode 2024 is connected to the other end of the second active layer 2021 through a fourth via hole V4. The plurality of first active layers 2011, the plurality of first gate electrodes 2012, the plurality of first source electrodes 2013, and the plurality of first drain electrodes 2014 of the display area 100 form a plurality of first transistors 201, and the plurality of second active layers 2021, the plurality of second gate electrodes 2022, the plurality of second source electrodes 2023, and the plurality of second drain electrodes 2024 form a plurality of second transistors 202. As shown in FIG8 d , FIG8 d illustrates one first transistor 201 and one second transistor 202.

[0129] The first source-drain metal layer may include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10. For example, the first metal layer and the third metal layer may be titanium layers, and the second metal layer may be an aluminum layer. The first source electrode 2013, the first drain electrode 2014, the second source electrode 2023, and the second drain electrode 2024 each include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10.

[0130] Subsequently, a first planarizing film is applied and patterned through a patterning process to form a first planarizing layer 27 pattern covering the first source / drain metal layer pattern. The first planarizing layer 27 has a fifth via hole V5 defined in the display area 100. The first planarizing layer 27 within the fifth via hole V5 is removed, exposing the surface of the first source electrode 2013 or the first drain electrode 2014. The pattern of the first planarizing layer 27 includes a filling layer 271 located in the transition region 300 and filling the third groove 83, the second groove 82, and the first groove 81. The filling layer 271 can fill the third groove 83, as shown in FIG8e.

[0131] Subsequently, a second source / drain metal film is deposited and patterned using a patterning process to form a second source / drain metal layer pattern on the first planar layer 27. The second source / drain metal layer pattern includes multiple anode connection electrodes 204 located in the display area 100 and a first lip 86 and a second lip 87 located in the transition area 300. The anode connection electrode 204 is connected to the first source electrode 2013 or the first drain electrode 2014 via a fifth via V5. The first lip 86 and the second lip 87 are located on the side of the third groove 83 near the display area 100 and the side near the hole area 200, respectively. Each of the first lip 86 and the second lip 87 is partially located on the second interlayer insulating layer 26 and partially located on the filling layer 271. The third groove 83, the second groove 82, and the first groove 81 form the groove 511 of the isolation trench 51. The first lip 86 and the second lip 87 are both partially located above the groove 511 (i.e., on the side of the groove 511 away from the substrate 10), as shown in FIG. 8f.

[0132] The film structure and material of the second source / drain metal layer can be the same as those of the first source / drain metal layer. For example, the second source / drain metal layer can include a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked sequentially in a direction away from the substrate 10. For example, the fourth and sixth metal layers can be titanium layers, and the fifth metal layer can be aluminum layers. Consequently, the connecting electrode 204, the first stop edge 86, and the second stop edge 87 all include a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked sequentially in a direction away from the substrate 10, as shown in FIG. 8f.

[0133] Subsequently, a second planar film is applied and patterned using a patterning process to form a second planar layer 28 pattern covering the second source / drain metal layer pattern in the display area 100. A plurality of sixth via holes are formed in the second planar layer 28 and located in the display area 100. The second planar layer 28 within the sixth via holes is removed, exposing the surface of the anode connection electrode 204, as shown in FIG. 8g .

[0134] At this point, the driving structure layer 20 and the film layer of the isolation trench 51 are completed.

[0135] (2) Forming the light emitting structure layer 30. In an exemplary embodiment, forming the light emitting structure layer 30 may include:

[0136] A first electrode 31 thin film is deposited on the substrate 10 having the aforementioned pattern formed thereon. The first electrode 31 thin film is patterned through a patterning process to form a first electrode layer pattern. The first electrode layer pattern includes a plurality of first electrodes 31 (anodes) located in the display area 100. The first electrodes 31 are connected to the anode connection electrode 204 through the sixth via hole in the second planar layer 28. Thus, the first electrodes 31 are connected to the first source electrode 2013 or the first drain electrode 2014 through the anode connection electrode 204, as shown in FIG. 8g .

[0137] During the patterning process (e.g., wet etching) of the first electrode 31 film, the fifth metal layer of the first and second stop edges 86 and 87 can be simultaneously laterally etched, causing the fifth metal layer of the first and second stop edges 86 and 87 to be partially indented relative to the fourth and sixth metal layers (i.e., the fourth and sixth metal layers protrude relative to the fifth metal layer) on the side of the first and second stop edges 86 and 87 near the groove 511 of the isolation trench 51, as shown in FIG8g. In other embodiments, during the aforementioned patterning process (e.g., developing process) of the second flat film, the fifth metal layer of the first and second stop edges 86 and 87 can be simultaneously laterally etched, causing the fifth metal layer of the first and second stop edges 86 and 87 to be partially indented relative to the fourth and sixth metal layers on the side of the first and second stop edges 86 and 87 near the groove 511 of the isolation trench 51.

[0138] Subsequently, a pixel defining film is coated on the substrate 10 having the aforementioned pattern formed thereon. The pixel defining film is patterned through a patterning process to form a pixel defining layer 32. The pixel defining layer 32 is provided with a plurality of pixel openings, which expose the surface of the first electrode 31 of the display area 100, as shown in FIG8h.

[0139] Subsequently, an etching process (dry etching or wet etching, such as etching with oxygen) is used to remove the filling layer 271 in the groove 511 of the isolation trench 51, as shown in FIG8i. Thus, the isolation trench 51 structure is formed.

[0140] Subsequently, on the substrate 10 formed with the aforementioned pattern, multiple film layers of the light-emitting functional layer 33 can be sequentially formed through an evaporation process. The light-emitting functional layer 33 can include a hole injection layer, a hole transport layer, an electron blocking layer, an organic light-emitting layer, a hole blocking layer, an electron transport layer, and an electron injection layer, which are sequentially arranged in a direction away from the substrate 10. Except for the organic light-emitting layer, the remaining film layers of the light-emitting functional layer 33 can all be an integrated, full-surface structure. That is, the remaining film layers of the light-emitting functional layer 33 can be common layers for sub-pixels of different colors. These common layers can be formed in the display area 100 and the transition area 300 during evaporation. Since the isolation groove 51 is provided in the transition area 300, these common layers will be disconnected at the isolation groove 51, blocking the path for water and oxygen to be transmitted from the hole area 200 through the light-emitting functional layer 33 to the display area 100, thereby preventing water and oxygen from corroding the light-emitting functional layer 33 in the display area 100. As shown in Figure 5.

[0141] Subsequently, a second electrode (cathode) layer is formed on the patterned substrate 10 through an evaporation process. The second electrode layer 34 of the sub-pixels of different colors is a common layer connected into an integrated structure. The second electrode layer 34 can be formed in the display area 100 and the transition area 300. The second electrode layer 34 can be disconnected at the isolation trench 51, blocking the path for water and oxygen to be transmitted from the hole area 200 through the second electrode layer 34 to the display area 100, thereby preventing water and oxygen from corroding the second electrode layer 34 in the display area 100. This is shown in Figure 5.

[0142] At this point, the light emitting structure layer 30 is completed.

[0143] (3) Forming the encapsulation structure layer 40. In an exemplary embodiment, forming the encapsulation structure layer 40 may include:

[0144] On the substrate 10 with the aforementioned pattern, a first encapsulation film is first deposited using an open reticle to form a first encapsulation layer 41 located in the display area 100 and transition area 300. Subsequently, a second encapsulation material is printed using an open reticle using an inkjet printing process to form a second encapsulation layer 42 located in the display area 100 and transition area 300. Isolation dams 60 in the transition area 300 prevent ink overflow during the inkjet printing process. Subsequently, a third encapsulation film is deposited using an open reticle to form a third encapsulation layer 43 located in the display area 100 and transition area 300. The materials for the first and third encapsulation layers 41 and 43 can be inorganic materials, while the material for the second encapsulation layer 42 can be organic materials, as shown in Figure 5.

[0145] Subsequently, film layers such as a touch structure layer and a color filter layer may be formed in sequence on the side of the encapsulation structure layer 40 away from the substrate 10 .

[0146] Based on the method for preparing the display substrate illustrated in FIG3 and FIG5 , the embodiment of the present disclosure further provides a method for preparing the display substrate illustrated in FIG3 and FIG5 , comprising:

[0147] forming a first structural layer and a second structural layer in sequence on the substrate of the transition region, wherein the first structural layer includes a barrier layer, and the second structural layer is provided with a groove, wherein the groove penetrates the second structural layer and exposes at least a portion of the surface of the barrier layer;

[0148] forming a filling layer in the groove, wherein the filling layer fills the groove;

[0149] forming a retaining edge on a surface of the second structural layer away from the substrate, wherein a portion of the retaining edge extends in a direction parallel to the substrate to a surface of the filling layer away from the substrate;

[0150] The filling layer is removed.

[0151] In some exemplary embodiments, the guard edge includes a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked in sequence in a direction away from the substrate. The method also includes etching the fifth metal layer of the guard edge so that the fifth metal layer is retracted compared to the fourth metal layer and the sixth metal layer on the side of the guard edge close to the groove.

[0152] In some further exemplary embodiments, taking the display substrate shown in FIG. 6 as an example, the preparation process of the display substrate may include the following operations:

[0153] (1) The driving structure layer 20 and the film layer of the isolation column 52 are formed.

[0154] A first buffer film and a first semiconductor film are sequentially deposited on a substrate 10. The first semiconductor film is patterned through a patterning process to form a first buffer layer 21 covering the substrate 10 and a first semiconductor layer pattern disposed on the first buffer layer 21. The first semiconductor layer pattern includes a plurality of first active layers 2011 located in the display area 100. After this patterning process, the transition region 300 includes the first buffer layer 21 disposed on the substrate 10, as shown in Figure 9a.

[0155] Subsequently, a first gate insulating film and a first gate metal film are sequentially deposited. The first gate metal film is patterned through a patterning process to form a first gate insulating layer 22 covering the first semiconductor layer pattern, and a first gate metal layer pattern disposed on the first gate insulating layer 22. The first gate metal layer pattern includes a plurality of first gate electrodes 2012 and a plurality of first electrode plates 2031 located in the display area 100. After this patterning process, the transition region 300 includes a first buffer layer 21 and a first gate insulating layer 22 sequentially stacked on the substrate 10, as shown in Figure 9a.

[0156] Subsequently, a second gate insulating film and a second gate metal film are sequentially deposited and patterned through a patterning process to form a second gate insulating layer 23 covering the first gate metal layer, and a second gate metal layer pattern disposed on the second gate insulating layer 23. The second gate metal layer pattern includes a plurality of second electrodes 2032 located in the display area 100. The plurality of second electrodes 2032 are disposed opposite the plurality of first electrodes 2031 and form a plurality of storage capacitors 203. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, and a second gate insulating layer 23 sequentially stacked on the substrate 10, as shown in FIG9a.

[0157] Subsequently, a first interlayer insulating film and a second semiconductor film are deposited, and the second semiconductor film is patterned through a patterning process to form a first interlayer insulating layer 24 covering the second gate metal layer pattern, and a second semiconductor layer pattern disposed on the first interlayer insulating layer 24. The second semiconductor layer pattern includes multiple second active layers 2021 located in the display area 100 and a barrier layer 513 located in the transition region 300. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, and a barrier layer 513 disposed on the first interlayer insulating layer 24, which are sequentially stacked on the substrate 10, as shown in Figure 9a.

[0158] Subsequently, a third gate insulating film and a third gate metal film are sequentially deposited and patterned through a patterning process to form a third gate insulating layer 25 covering the second semiconductor layer pattern and a third gate metal layer pattern disposed on the third gate insulating layer 25. The third gate metal layer pattern includes a plurality of second gate electrodes 2022 located in the display area 100. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, a barrier layer 513, and a third gate insulating layer 25 covering the barrier layer 513, stacked sequentially on the substrate 10, as shown in FIG9a.

[0159] Subsequently, a second interlayer insulating film is deposited and patterned through a patterning process to form a second interlayer insulating layer 26 pattern covering the third gate metal layer pattern. The second interlayer insulating layer 26 in the display area 100 is provided with a plurality of first via holes V1, a plurality of second via holes V2, a plurality of third via holes V3, and a plurality of fourth via holes V4. The plurality of first via holes V1 expose one end of the plurality of first active layers 2011, the plurality of second via holes V2 expose the other end of the plurality of first active layers 2011, the plurality of third via holes V3 expose one end of the plurality of second active layers 2021, and the plurality of fourth via holes V4 expose the other end of the plurality of second active layers 2021. The second interlayer insulating layer 26 in the transition area 300 is provided with a plurality of grooves that penetrate the third gate insulating layer 25 and expose the barrier layer 513. Adjacent grooves form the bases 523 of the isolation columns 52 located on the barrier layer 513. The bases 523 include the stacked third gate insulating layer 25 and the second interlayer insulating layer 26, as shown in FIG. 9a.

[0160] Subsequently, a first source / drain metal film is deposited and patterned through a patterning process to form a first source / drain metal layer pattern on the second interlayer insulating layer 26. The first source / drain metal layer pattern includes a plurality of first source electrodes 2013, a plurality of first drain electrodes 2014, a plurality of second source electrodes 2023, and a plurality of second drain electrodes 2024 located in the display area 100, as well as a first isolation layer 71 located on the column base 523 in the transition area 300 and a retaining wall 72 located on the second interlayer insulating layer 26. The side of the retaining wall 72 adjacent to the groove can be flush with the side of the groove. The first source electrode 2013 is connected to one end of the first active layer 2011 through a first via V1, the first drain electrode 2014 is connected to the other end of the first active layer 2011 through a second via V2, the second source electrode 2023 is connected to one end of the second active layer 2021 through a third via V3, and the second drain electrode 2024 is connected to the other end of the second active layer 2021 through a fourth via V4. The plurality of first active layers 2011, the plurality of first gate electrodes 2012, the plurality of first source electrodes 2013, and the plurality of first drain electrodes 2014 of the display area 100 form a plurality of first transistors 201, and the plurality of second active layers 2021, the plurality of second gate electrodes 2022, the plurality of second source electrodes 2023, and the plurality of second drain electrodes 2024 form a plurality of second transistors 202. As shown in FIG. 9 b , FIG. 9 b illustrates one first transistor 201 and one second transistor 202.

[0161] The first source / drain metal layer may include a first metal layer, a second metal layer, and a third metal layer stacked sequentially in a direction away from the substrate 10. For example, the first metal layer and the third metal layer may be titanium layers, and the second metal layer may be an aluminum layer. The first source electrode 2013, the first drain electrode 2014, the second source electrode 2023, the second drain electrode 2024, the first isolation layer 71, and the retaining wall 72 each include a first metal layer, a second metal layer, and a third metal layer stacked sequentially in a direction away from the substrate 10.

[0162] Subsequently, a first planarizing film is applied and patterned through a patterning process to form a first planarizing layer 27 pattern covering the first source / drain metal layer pattern in the display area 100. The first planarizing layer 27 is provided with a fifth via hole V5 in the display area 100. The first planarizing layer 27 within the fifth via hole V5 is removed, exposing the surface of the first source electrode 2013 or the first drain electrode 2014. The pattern of the first planarizing layer 27 includes a filling layer 271 located in the transition region 300 and filling the groove. The filling layer 271 can fill the groove, and the surface of the filling layer 271 facing away from the substrate 10 can be flush with the surfaces of the first isolation layer 71 and the retaining wall 72 facing away from the substrate 10, as shown in FIG. 9c.

[0163] Subsequently, a second source / drain metal film is deposited and patterned using a patterning process to form a second source / drain metal layer pattern on the first planar layer 27. The second source / drain metal layer pattern includes multiple anode connection electrodes 204 located in the display area 100 and a second isolation layer 73 located on the first isolation layer 71 in the transition area 300. The anode connection electrodes 204 are connected to the first source electrode 2013 or the first drain electrode 2014 through fifth vias V5. The second isolation layer 73 is also partially located on the filling layer 271. The side of the second isolation layer 73 facing the display area 100 and / or the hole area 200 protrudes from the corresponding side of the first isolation layer 71, as shown in Figure 9d.

[0164] The film structure and material of the second source / drain metal layer can be the same as those of the first source / drain metal layer. For example, the second source / drain metal layer can include a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked sequentially in a direction away from the substrate 10. For example, the fourth metal layer and the sixth metal layer can be titanium layers, and the fifth metal layer can be an aluminum layer. Therefore, both the anode connection electrode 204 and the second isolation layer 73 include a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked sequentially in a direction away from the substrate 10.

[0165] Subsequently, a second planar film is applied and patterned using a patterning process to form a second planar layer 28 pattern covering the second source / drain metal layer pattern in the display area 100. A plurality of sixth via holes are formed in the second planar layer 28 and located in the display area 100. The second planar layer 28 within the sixth via holes is removed, exposing the surface of the anode connection electrode 204, as shown in FIG. 9e.

[0166] At this point, the driving structure layer 20 and the film layer of the isolation column 52 are completed.

[0167] (2) Forming the light emitting structure layer 30. In an exemplary embodiment, forming the light emitting structure layer 30 may include:

[0168] A first electrode 31 thin film is deposited on the substrate 10 on which the aforementioned pattern is formed, and the first electrode 31 thin film is patterned through a patterning process to form a first electrode layer pattern. The first electrode layer pattern includes a plurality of first electrodes 31 (anodes) located in the display area 100. The first electrode 31 is connected to the anode connecting electrode 204 through the sixth via hole on the second flat layer 28, so that the first electrode 31 is connected to the first source electrode 2013 or the first drain electrode 2014 through the anode connecting electrode 204.

[0169] In the patterning process (e.g., wet etching process) of the first electrode 31 film, the fifth metal layer of the second isolation layer 73 can be simultaneously laterally etched, so that on the side of the second isolation layer 73 facing the display area 100 and the hole area 200, the fifth metal layer of the second isolation layer 73 is partially indented relative to the fourth metal layer and the sixth metal layer, as shown in FIG9e . In other embodiments, during the aforementioned patterning process (e.g., developing process) of the second flat film, the fifth metal layer of the second isolation layer 73 can be simultaneously laterally etched, so that on the side of the second isolation layer 73 facing the display area 100 and the hole area 200, the fifth metal layer of the second isolation layer 73 is partially indented relative to the fourth metal layer and the sixth metal layer.

[0170] Subsequently, a pixel defining film is coated on the substrate 10 having the aforementioned pattern formed thereon. The pixel defining film is patterned through a patterning process to form a pixel defining layer 32. The pixel defining layer 32 is provided with a plurality of pixel openings, which expose the surface of the first electrode 31 of the display area 100, as shown in FIG9f.

[0171] Subsequently, an etching process (dry or wet etching, for example, using oxygen as the etching gas) is used to etch away the filling layer 271 within the groove. Simultaneously, a portion of the fifth metal layer of the second isolation layer 73 and the second metal layer of the first isolation layer 71 are laterally etched. This causes the fifth metal layer of the second isolation layer 73 to be partially inward relative to the fourth and sixth metal layers on the sides of the second isolation layer 73 and the first isolation layer 71 facing the display area 100 and the hole area 200, and the second metal layer of the first isolation layer 71 to be partially inward relative to the first and third metal layers. This results in the first isolation layer 71 becoming the first isolation portion 521 of the isolation column 52, and the second isolation layer 73 becoming the second isolation portion 522 of the isolation column 52. The column base 523, the first isolation portion 521, and the second isolation portion 522 form the isolation column 52, as shown in FIG. 9g.

[0172] Subsequently, on the substrate 10 formed with the aforementioned pattern, multiple film layers of the light-emitting functional layer 33 can be sequentially formed through an evaporation process. The light-emitting functional layer 33 can include a hole injection layer, a hole transport layer, an electron blocking layer, an organic light-emitting layer, a hole blocking layer, an electron transport layer, and an electron injection layer, which are sequentially arranged in a direction away from the substrate 10. Except for the organic light-emitting layer, the remaining film layers of the light-emitting functional layer 33 can all be an integrated, full-surface structure. That is, the remaining film layers of the light-emitting functional layer 33 can be common layers for sub-pixels of different colors. These common layers can be formed in the display area 100 and the transition area 300 during evaporation. Because isolation columns 52 are provided in the transition area 300, these common layers will be disconnected at the isolation columns 52, blocking the path for water and oxygen to be transmitted from the hole area 200 through the light-emitting functional layer 33 to the display area 100, thereby preventing water and oxygen from corroding the light-emitting functional layer 33 in the display area 100. As shown in Figure 6.

[0173] Subsequently, a second electrode (cathode) layer is formed on the patterned substrate 10 through an evaporation process. The second electrode layer 34 of the sub-pixels of different colors is a common layer connected into an integrated structure. The second electrode layer 34 can be formed in the display area 100 and the transition area 300. The second electrode layer 34 can be disconnected at the isolation column 52, blocking the path for water and oxygen to be transmitted from the aperture area 200 through the second electrode layer 34 to the display area 100, thereby preventing water and oxygen from corroding the second electrode layer 34 in the display area 100. This is shown in Figure 6.

[0174] At this point, the light emitting structure layer 30 is completed.

[0175] (3) Forming the encapsulation structure layer 40. In an exemplary embodiment, forming the encapsulation structure layer 40 may include:

[0176] On the substrate 10 with the aforementioned pattern, a first encapsulation film is first deposited using an open reticle to form a first encapsulation layer 41 located in the display area 100 and transition area 300. Subsequently, a second encapsulation material is printed using an open reticle using an inkjet printing process to form a second encapsulation layer 42 located in the display area 100 and transition area 300. Isolation dams 60 in the transition area 300 prevent ink overflow during the inkjet printing process. Subsequently, a third encapsulation film is deposited using an open reticle to form a third encapsulation layer 43 located in the display area 100 and transition area 300. The materials for the first and third encapsulation layers 41 and 43 can be inorganic materials, while the material for the second encapsulation layer 42 can be organic materials, as shown in Figure 6.

[0177] Subsequently, film layers such as a touch structure layer and a color filter layer may be formed in sequence on the side of the encapsulation structure layer 40 away from the substrate 10 .

[0178] The present disclosure also provides a display device comprising the display substrate described in any of the above embodiments. The display device can be any product or component with a display function, such as a mobile phone, tablet computer, television, monitor, laptop computer, digital photo frame, or navigation system.

[0179] In the drawings, the sizes of components, layer thicknesses, or regions are sometimes exaggerated for clarity. Therefore, the embodiments of the present disclosure are not necessarily limited to these dimensions, and the shapes and sizes of each component in the drawings do not reflect true proportions. Furthermore, the drawings schematically illustrate some examples, and the embodiments of the present disclosure are not limited to the shapes or values ​​shown in the drawings.

[0180] In this description, "parallel" refers to a state where the angle formed by two straight lines is greater than -10° and less than 10°, and thus includes a state where the angle is greater than -5° and less than 5°. Furthermore, "perpendicular" refers to a state where the angle formed by two straight lines is greater than 80° and less than 100°, and thus includes a state where the angle is greater than 85° and less than 95°.

[0181] In the description herein, the terms "upper", "lower", "left", "right", "top", "inner", "outer", "axial", "four corners", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings. They are merely simplified descriptions for the convenience of describing the embodiments of the present disclosure, and do not indicate or imply that the structure referred to has a specific orientation, is constructed and operated in a specific orientation. Therefore, they should not be understood as limitations on the present disclosure.

[0182] In the description herein, unless otherwise expressly specified or limited, the terms "connect," "fixed connection," "installation," and "assembly" should be understood in a broad sense, for example, to mean a fixed connection, a detachable connection, or an integral connection; the terms "installation," "connection," and "fixed connection" can mean a direct connection, an indirect connection through an intermediate medium, or internal communication between two components. A person of ordinary skill in the art can understand the meaning of the above terms in the embodiments of the present disclosure according to the circumstances.

Claims

1. A display substrate, comprising a hole area, a transition area surrounding the hole area, and a display area surrounding the transition area; the transition area is provided with an isolation structure surrounding the hole area, the isolation structure comprising at least one isolation groove; The display substrate includes a base, the isolation groove includes a groove and a blocking edge arranged on a side of the groove away from the base; in a direction perpendicular to the base, the transition zone includes a first structural layer and a second structural layer stacked in sequence in a direction away from the base, the first structural layer includes a blocking layer, the groove penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer, the blocking edge is arranged on a surface of the second structural layer away from the base, and a portion of the blocking edge extends in a direction parallel to the base and protrudes from the side wall of the groove.

2. The display substrate according to claim 1, in, The retaining edge includes a fourth metal layer, a fifth metal layer and a sixth metal layer arranged in sequence in a direction away from the base. On a side of the retaining edge close to the groove, the fifth metal layer is set back compared to the fourth metal layer and the sixth metal layer.

3. The display substrate according to claim 1, in, The display area includes a driving structure layer and a light-emitting structure layer sequentially stacked on the substrate, the driving structure layer includes a pixel driving circuit, the pixel driving circuit includes a plurality of transistors and a storage capacitor, the light-emitting structure layer includes a plurality of light-emitting elements, and the light-emitting elements include a first electrode, a light-emitting function layer, and a second electrode layer sequentially stacked in a direction away from the substrate; In a direction perpendicular to the substrate, the driving structure layer includes a first source-drain metal layer, a first flat layer, a second source-drain metal layer, and a second flat layer, which are sequentially arranged in a direction away from the substrate; the first source-drain metal layer includes a first source electrode and a first drain electrode of the first transistor, and the second source-drain metal layer includes a connecting electrode connected to the first source electrode or the first drain electrode, and the connecting electrode is also connected to the first electrode; The blocking edge is disposed in the same layer as the connecting electrode, or the blocking edge is disposed in the same layer as the first source electrode and the first drain electrode.

4. The display substrate according to claim 3, in, In a direction perpendicular to the substrate, the driving structure layer further includes a first semiconductor layer, a first gate metal layer, and a second gate metal layer, which are arranged on a side of the first source-drain metal layer close to the substrate; the first semiconductor layer includes a first active layer of the first transistor, the first gate metal layer includes a first gate electrode of the first transistor and one plate of the storage capacitor, and the second gate metal layer includes another plate of the storage capacitor; The barrier layer is disposed in the same layer as the first active layer, the first gate metal layer or the second gate metal layer.

5. The display substrate according to claim 3, in, In a direction perpendicular to the substrate, the driving structure layer further includes a first semiconductor layer, a first gate metal layer, a second gate metal layer, a second semiconductor layer and a third gate metal layer, which are arranged on a side of the first source-drain metal layer close to the substrate; the first semiconductor layer includes a first active layer of the first transistor, the first gate metal layer includes a first gate electrode of the first transistor and one plate of the storage capacitor, the second gate metal layer includes another plate of the storage capacitor, the second semiconductor layer includes a second active layer of the second transistor, and the third gate metal layer includes a second gate electrode of the second transistor; the first source-drain metal layer also includes a second source electrode and a second drain electrode of the second transistor; The barrier layer is disposed in the same layer as any one of the first active layer, the first gate metal layer, the second gate metal layer, the second active layer and the third gate metal layer.

6. The display substrate according to claim 1, in, The second structure layer includes a plurality of stacked inorganic insulating layers, or the second structure layer includes at least one inorganic insulating layer and at least one metal layer.

7. The display substrate according to claim 6, in, One or more convex rings are arranged on the side wall of the groove, and the plurality of convex rings are arranged in sequence along a direction perpendicular to the substrate, and the convex rings are formed by the inorganic insulating layer.

8. The display substrate according to claim 3, in, The isolation structure further comprises at least one isolation column; the isolation column comprises a first isolation portion and a second isolation portion sequentially arranged in a direction away from the substrate, and on a side of the isolation column facing the display area and / or the hole area, the second isolation portion is arranged to protrude from the first isolation portion; The material of the first isolation part is an inorganic insulating material, and the material of the second isolation part is a metal material; the second isolation part is arranged on the same layer as the first source electrode and the first drain electrode; or, the second isolation part is arranged on the same layer as the connecting electrode; or, the second isolation part includes a first sub-isolation part and a second sub-isolation part stacked in sequence along a direction away from the substrate, the first sub-isolation part is arranged on the same layer as the first source electrode and the first drain electrode, and the second sub-isolation part is arranged on the same layer as the connecting electrode.

9. The display substrate according to claim 8, in, An isolation column is formed between two adjacent isolation grooves, the blocking edge is arranged in the same layer and made of the same material as the second isolation portion, and the second structural layer between two adjacent grooves is the first isolation portion.

10. The display substrate according to claim 9, in, The two adjacent barrier layers are not connected, and at least a portion of an orthographic projection of the second isolation portion on the substrate does not overlap with an orthographic projection of the two adjacent barrier layers on the substrate.

11. The display substrate according to claim 9, in, At least two adjacent barrier layers are connected as a whole, and the orthographic projection of the at least two adjacent barrier layers connected as a whole on the substrate includes the orthographic projection of at least one isolation column on the substrate.

12. The display substrate according to claim 3, in, The isolation structure further comprises at least one isolation column; the isolation column comprises a first isolation portion and a second isolation portion sequentially arranged in a direction away from the substrate, and on a side of the isolation column facing the display area and / or the hole area, the second isolation portion is arranged to protrude from the first isolation portion; The materials of the first isolation part and the second isolation part are both metal materials, the first isolation part is arranged in the same layer as the first source electrode and the first drain electrode, and the second isolation part is arranged in the same layer as the connection electrode; The isolation column further includes a column base disposed on a side of the first isolation portion facing the substrate, and the column base includes at least one inorganic insulating layer.

13. The display substrate according to claim 12, in, The first isolation portion includes a first metal layer, a second metal layer and a third metal layer arranged in sequence in a direction away from the substrate, and on a side of the isolation column facing the display area or / and the hole area, the second metal layer is arranged inwardly compared with the first metal layer and the third metal layer; Or / and, the second isolation portion includes a fourth metal layer, a fifth metal layer and a sixth metal layer arranged in sequence along a direction away from the substrate, and on the side of the isolation column facing the display area and / or the hole area, the fifth metal layer is retracted compared to the fourth metal layer and the sixth metal layer.

14. The display substrate according to claim 8, in, The first isolation portion includes a silicon oxide film layer and a silicon nitride film layer stacked in sequence in a direction away from the substrate, and the thickness of the silicon nitride film layer is 0.5um to 1um.

15. A display device comprising the display substrate according to any one of claims 1 to 14.

16. A method for preparing the display substrate according to claim 1, include: forming a first structural layer and a second structural layer on the substrate of the transition zone in sequence, wherein the first structural layer comprises a barrier layer, and the second structural layer is provided with a groove, wherein the groove penetrates the second structural layer and exposes at least a portion of the surface of the barrier layer; forming a filling layer in the groove, wherein the filling layer fills the groove; forming a stop edge on a surface of the second structural layer away from the substrate, wherein a portion of the stop edge extends in a direction parallel to the substrate to a surface of the filling layer away from the substrate; The filling layer is removed.

Citation Information

Patent Citations

  • Display substrate, manufacturing method thereof and display panel

    CN111653595A

  • Display substrate, preparation method thereof and display device

    CN112186023A

  • Display substrate, manufacturing method thereof and display device

    CN114144886A

  • Display substrate and display device

    CN220023504U

  • Display panel and manufacturing method thereof, display device

    US20220190285A1