Optical element, variable focus element, and head-mounted display

The optical element configuration with liquid crystal cells and quarter wavelength films, combined with a Pancharatnam Berry lens, addresses the challenge of switching polarization states efficiently in head-mounted displays, achieving broad band and viewing angle coverage for improved display performance.

WO2024224472A1PCT designated stage expired Publication Date: 2024-10-31SHARP DISPLAY TECHNOLOGY CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/016243
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-25
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Existing variable focus optical systems for head-mounted displays face challenges in efficiently switching between polarization modulation and non-polarization modulation over a wide band and wide viewing angle, as previous solutions either fail to achieve broadband polarization conversion or compromise on viewing angle.

Method used

A novel optical element configuration incorporating a first and second liquid crystal cell with quarter wavelength films and positive C plates, where the liquid crystal molecules can switch between vertically aligned and twisted states, enabling efficient polarization modulation and non-modulation across a broad spectrum and angle, combined with a Pancharatnam Berry lens for variable focus.

Benefits of technology

The solution allows for high-efficiency switching between polarization modulation and non-modulation over a wide band and wide viewing angle, enhancing the performance of head-mounted displays by maintaining optical performance across various wavelengths and angles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023016243_31102024_PF_FP_ABST
    Figure JP2023016243_31102024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention provides an optical element capable of highly efficiently switching between polarization modulation and polarization non-modulation over a wide band and at a wide viewing angle, a variable focus element provided with the optical element, and a head-mounted display provided with the variable focus element. An optical element according to the present invention comprises: a first liquid crystal cell having first liquid crystal molecules and a first electrode; a second liquid crystal cell having second liquid crystal molecules and a second electrode, and can switch between a first state and a second state. The azimuth angles in the orientation direction of the second liquid crystal molecules on a third substrate side and a fourth substrate side in the first state are respectively angles obtained by turning the azimuth angles in the orientation direction of the first liquid crystal molecules on a first substrate side and a second substrate side in the second state one quarter of a turn in the same direction. The optical element comprises a first quarter wavelength film and a second quarter wavelength film that are disposed on the opposite side of the first liquid crystal cell from the second liquid crystal cell or on the opposite side of the second liquid crystal cell from the first liquid crystal cell.
Need to check novelty before this filing date? Find Prior Art

Description

Optical element, variable focus element and head-mounted display

[0001] The following disclosure relates to an optical element, a variable-focus element including the optical element, and a head-mounted display including the variable-focus element.

[0002] In recent years, variable-focus optical systems that combine Pancharatnam Berry (PB) lenses with optical elements such as switchable half-wave plates (sHWPs) have been proposed for head-mounted displays, etc. An sHWP is a device that can switch the polarization state of left-handed or right-handed circularly polarized light, and is realized using liquid crystal.

[0003] As a technology relating to a variable-focus optical system, for example, Patent Document 1 discloses a display device including a waveguide and a broadband adaptive lens assembly, wherein the waveguide is configured to guide light in a lateral direction parallel to an output surface of the waveguide and is further configured to externally couple the guided light through the output surface, and the broadband adaptive lens assembly is configured to internally couple and diffract the externally coupled light from the waveguide through the broadband adaptive lens assembly.

[0004] Patent Document 2 discloses a variable focus block including an sHWP and a plurality of liquid crystal lenses.

[0005] Patent document 3 discloses an achromatic polarization switch that converts linearly polarized light of an initial polarization orientation, the achromatic polarization switch comprising a first liquid crystal (LC) cell having a first alignment axis relative to the initial polarization orientation, and a second LC cell having a second alignment axis relative to the first alignment axis.

[0006] Patent Document 4 discloses an optical element comprising a first laminated birefringent layer and a second laminated birefringent layer, the respective local optical axes of which are rotated at respective twist angles through the respective thicknesses of the first layer and the second layer and aligned along the interface between the first layer and the second layer.

[0007] Patent Document 5 proposes an optical element having a laminated liquid crystal structure for use in a head-mounted display, which rotates the polarization of incident circularly polarized light over a wide range of wavelengths and angles of incidence.

[0008] JP 2021-501361 A U.S. Patent No. 10,379,419 Specification JP 2009-524106 A U.S. Patent No. 2014-528597 A U.S. Patent No. 10,678,057 Specification

[0009] The above Patent Documents 1 to 5 have a problem in that it is difficult to realize a device structure that can switch between polarization modulation, which converts the polarization state of left- and right-handed circularly polarized light, and polarization non-modulation, which does not convert the polarization state of left- and right-handed circularly polarized light, with high efficiency over a wide bandwidth and a wide viewing angle.

[0010] The present invention has been made in consideration of the above-mentioned current situation, and aims to provide an optical element that can switch between polarization modulation and polarization non-modulation with high efficiency over a wide bandwidth and a wide viewing angle, a variable-focus element that includes the optical element, and a head-mounted display that includes the variable-focus element.

[0011] (1) One embodiment of the present invention is a liquid crystal display device comprising, in this order, a first substrate, a first liquid crystal layer containing first liquid crystal molecules, a second substrate, a third substrate, a second liquid crystal layer containing second liquid crystal molecules, and a fourth substrate, wherein the first substrate, the first liquid crystal layer, and the second substrate constitute a first liquid crystal cell, and the third substrate, the second liquid crystal layer, and the fourth substrate constitute a second liquid crystal cell, wherein the first liquid crystal cell has, on at least one of the first substrate and the second substrate, a first electrode for applying a voltage to the first liquid crystal layer, and the second liquid crystal cell has, on at least one of the third substrate and the fourth substrate, a second electrode for applying a voltage to the second liquid crystal layer, and the first electrode and the second electrode are arranged to provide a first state in which the second liquid crystal molecules are twistedly aligned and the first liquid crystal molecules are vertically aligned, and a second state in which the first liquid crystal molecules are twistedly aligned and a first state in which the second liquid crystal molecules are vertically aligned, and a second state in which the second liquid crystal molecules are vertically aligned, wherein an azimuth angle of the alignment direction of the second liquid crystal molecules on the third substrate side in the first state and an azimuth angle of the alignment direction of the second liquid crystal molecules on the fourth substrate side in the first state are angles obtained by rotating the azimuth angle of the alignment direction of the first liquid crystal molecules on the first substrate side in the second state and the azimuth angle of the alignment direction of the first liquid crystal molecules on the second substrate side in the second state in the same direction by a quarter of a second, respectively; and further comprising a first quarter-wave film and a second quarter-wave film arranged on the side of the first liquid crystal cell opposite to the second liquid crystal cell, or on the side of the second liquid crystal cell opposite to the first liquid crystal cell, wherein the first quarter-wave film is arranged between the second quarter-wave film and the first liquid crystal cell and the second liquid crystal cell.

[0012] (2) In addition to the configuration of (1), another embodiment of the present invention is an optical element in which the retardation Re of the first quarter-wave film at a wavelength of 550 nm is 72 nm or more and 210 nm or less.

[0013] (3) In addition to the configuration of (1) or (2), an embodiment of the present invention is an optical element, wherein the azimuth angle of the slow axis of the first quarter-wave film is 52° or more and 66° or less.

[0014] (4) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), or (3), the retardation Re of the second quarter-wave film at a wavelength of 550 nm is 112 nm or more and 162 nm or less.

[0015] (5) In addition to the configuration of (1), (2), (3), or (4), an embodiment of the present invention is an optical element, wherein the azimuth angle of the slow axis of the second quarter-wave film is 4° or more and 23° or less.

[0016] (6) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4), or (5), at least one of the first quarter-wave film and the second quarter-wave film has a reverse wavelength dispersion characteristic.

[0017] (7) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4), (5), or (6), at least one of the first quarter-wave film and the second quarter-wave film has flat wavelength dispersion characteristics.

[0018] (8) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4), (5), (6), or (7), the retardation Re of the first liquid crystal layer in the second state at a wavelength of 550 nm is 196 nm or more and 280 nm or less.

[0019] (9) Also, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4), (5), (6), (7), or (8), the retardation Re of the second liquid crystal layer in the first state at a wavelength of 550 nm is 200 nm or more and 280 nm or less.

[0020] (10) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4), (5), (6), (7), (8), or (9), the first liquid crystal molecules in the second state are twisted and aligned at a twist angle of 58° or more and 78° or less.

[0021] (11) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4), (5), (6), (7), (8), (9), or (10), the second liquid crystal molecules in the first state are twist-oriented at a twist angle of 57° or more and 76° or less.

[0022] (12) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4), (5), (6), (7), (8), (9), (10), or (11), an optical element in which the azimuth angle of the alignment direction of the first liquid crystal molecules on the first substrate side in the second state is not less than −12° and not more than 10°.

[0023] (13) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4), (5), (6), (7), (8), (9), (10), (11), or (12), an optical element in which the azimuth angle of the alignment direction of the second liquid crystal molecules on the third substrate side in the first state is 79° or more and 98° or less.

[0024] (14) Furthermore, in addition to the configuration of (1), (2), (3), (4), (5), (6), (7), (8), (9), (10), (11), (12), or (13), an embodiment of the present invention provides an optical element further comprising: a first positive C plate disposed between the first quarter-wave film and the second quarter-wave film; a second positive C plate disposed on the second liquid crystal cell on the opposite side to the first liquid crystal cell; and a third positive C plate disposed on the first liquid crystal cell on the opposite side to the second liquid crystal cell.

[0025] (15) Furthermore, in addition to the configuration of (14), an embodiment of the present invention is an optical element, in which the retardation Rth in the thickness direction of the first positive C plate is 0 nm or more and 320 nm or less.

[0026] (16) Furthermore, in addition to the configuration of (14) or (15), an embodiment of the present invention is an optical element, wherein the retardation Rth in the thickness direction of the second positive C plate is 0 nm or more and 252 nm or less.

[0027] (17) Furthermore, in addition to the configuration of (14), (15), or (16), an embodiment of the present invention is an optical element, wherein the retardation Rth in the thickness direction of the third positive C plate is 0 nm or more and 290 nm or less.

[0028] (18) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4), (5), (6), (7), (8), (9), (10), (11), (12), (13), (14), (15), (16), or (17), the optical element further comprises a negative C plate between the first liquid crystal cell and the second liquid crystal cell.

[0029] (19) Furthermore, in addition to the configuration of (18), an embodiment of the present invention is an optical element, in which the retardation Rth in the thickness direction of the negative C plate is −410 nm or more and 0 nm or less.

[0030] (20) Another embodiment of the present invention is a variable focus element comprising the optical element described in (1), (2), (3), (4), (5), (6), (7), (8), (9), (10), (11), (12), (13), (14), (15), (16), (17), (18) or (19) above, and a Pancharatnam Berry lens.

[0031] (21) Furthermore, in addition to the configuration of (20), one embodiment of the present invention is a variable-focus element, in which the Pancharatnam Berry lens is disposed within the optical element.

[0032] (22) Another embodiment of the present invention is a head-mounted display including the variable focus element described in (20) or (21) above.

[0033] According to the present invention, it is possible to provide an optical element that can switch between polarization modulation and polarization non-modulation with high efficiency over a wide bandwidth and a wide viewing angle, a variable-focus element that includes the optical element, and a head-mounted display that includes the variable-focus element.

[0034] FIG. 1 is a cross-sectional view of an optical element according to Embodiment 1. FIG. 1 is a cross-sectional view of a first liquid crystal cell and a second liquid crystal cell included in the optical element according to Embodiment 1. FIG. 2 is a cross-sectional view of an optical element according to Comparative Embodiment 1. FIG. 3 is a cross-sectional view of an optical element according to Comparative Embodiment 2. FIG. 4 is a graph showing the relationship between the Stokes parameter S3 during modulation and the wavelength of emitted light for optical elements according to Comparative Embodiments 1 and 2. FIG. 5 is a cross-sectional view of an optical element according to a first embodiment. FIG. 6 is a cross-sectional view of an optical element according to Embodiment 2. FIG. 7 is a cross-sectional view of an optical element according to Modification 1 of Embodiment 1. FIG. 8 is a cross-sectional view of an optical element according to Embodiment 2. FIG. 9 is a cross-sectional view of an optical element according to Embodiment 3. FIG. 10 is a cross-sectional view of an optical element according to Embodiment 3. FIG. 1 is a cross-sectional view illustrating a second state of the optical element according to Embodiment 3. FIG. 1 is a cross-sectional view illustrating a first liquid crystal cell and a second liquid crystal cell included in the optical element according to Embodiment 4. FIG. 1 is a cross-sectional view illustrating a first state of the optical element according to Embodiment 4. FIG. 1 is a cross-sectional view illustrating a second state of the optical element according to Embodiment 4. FIG. 1 is a cross-sectional view illustrating a variable-focus element according to Embodiment 5. FIG. 1 is an example of a cross-sectional view of a PB lens included in the variable-focus element according to Embodiment 5. FIG. 1 is a cross-sectional view of a variable-focus element according to Modification 1 of Embodiment 5. FIG. 2 is an enlarged cross-sectional view of a variable-focus element according to Modification 1 of Embodiment 5. FIG. 2 is a cross-sectional view illustrating the alignment of liquid crystal molecules in the first state and the second state of the optical element according to Modification 1 of Embodiment 5. FIG. 3 is a plan view illustrating the orientation pattern of the PB lens included in the variable-focus element according to Modification 1 of Embodiment 5. FIG. 4 is a cross-sectional view illustrating a detailed configuration of the variable-focus element according to Modification 1 of Embodiment 5. 13A and 13B are diagrams illustrating the polarization state of a variable-focus element according to Modification 1 of Embodiment 5 in the F-2.5 mode.1 is a cross-sectional schematic diagram of a head-mounted display according to embodiment 6. FIG. 2 is a perspective schematic diagram showing an example of the appearance of the head-mounted display according to embodiment 6. FIG. 3 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to example 1 is not modulated, when the incident angle is set to 30°. FIG. 4 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to example 1 is modulated, when the incident angle is set to 30°. FIG. 5 is a graph showing the Stokes parameter (worst S3) versus the retardation Re of the second quarter-wave film included in the optical element of example 1. FIG. 6 is a graph showing the Stokes parameter (worst S3) versus the azimuth angle of the slow axis of the second quarter-wave film included in the optical element of example 1. FIG. 7 is a graph showing the Stokes parameter (worst S3) versus the retardation Rth in the thickness direction of the first positive C-plate included in the optical element of example 1. FIG. 8 is a graph showing the Stokes parameter (worst S3) versus the retardation Re of the first quarter-wave film included in the optical element of example 1. 1 is a graph showing the Stokes parameter (worst S3) versus the azimuth angle of the slow axis of the first quarter-wave film included in the optical element of Example 1. FIG. 2 is a graph showing the Stokes parameter (worst S3) versus the retardation Rth in the thickness direction of the second positive C-plate included in the optical element of Example 1. FIG. 3 is a graph showing the Stokes parameter (worst S3) versus the retardation Re in the first state at a wavelength of 550 nm of the second liquid crystal layer included in the optical element of Example 1. FIG. 4 is a graph showing the Stokes parameter (worst S3) versus the twist angle in the first state of the second liquid crystal molecules included in the optical element of Example 1. FIG. 5 is a graph showing the Stokes parameter (worst S3) versus the azimuth angle of the alignment direction of the second liquid crystal molecules on the third substrate side in the first state of the optical element of Example 1. FIG. 6 is a graph showing the Stokes parameter (worst S3) versus the retardation Rth in the thickness direction of the negative C-plate included in the optical element of Example 1. 10 is a graph showing the Stokes parameter (worst S3) versus retardation Re in the second state at a wavelength of 550 nm of the first liquid crystal layer included in the optical element of Example 1.1 is a graph showing the Stokes parameter (worst S3) versus the azimuth angle of the alignment direction of the first liquid crystal molecules on the first substrate side in the second state of the optical element of Example 1. FIG. 2 is a graph showing the Stokes parameter (worst S3) versus the twist angle in the second state of the first liquid crystal molecules of the optical element of Example 1. FIG. 3 is a graph showing the Stokes parameter (worst S3) versus the retardation Rth in the thickness direction of the third positive C-plate included in the optical element of Example 1. FIG. 4 is a schematic cross-sectional view of an optical element according to Comparative Example 1. FIG. 5 is a schematic cross-sectional view of an optical element according to Comparative Example 2. FIG. 6 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle of the optical element according to Comparative Example 1 in the non-modulated state when the incident angle is set to 30°. FIG. 7 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle of the optical element according to Comparative Example 1 in the modulated state when the incident angle is set to 30°. FIG. 8 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle of the optical element according to Comparative Example 2 in the non-modulated state when the incident angle is set to 30°. 1 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Comparative Example 2 is modulated when the incident angle is set to 30°. FIG. 2 is a schematic cross-sectional view of the optical element according to Example 2. FIG. 3 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Example 2 is not modulated when the incident angle is set to 30°. FIG. 4 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Example 2 is modulated when the incident angle is set to 30°.

[0035] Hereinafter, embodiments of the present invention will be described. The present invention is not limited to the contents described in the following embodiments, and appropriate design changes can be made within the scope of the configuration of the present invention. In the following description, the same reference numerals will be used in different drawings as appropriate for the same parts or parts having similar functions, and repeated explanations will be omitted as appropriate. Each aspect of the present invention may be combined as appropriate within the scope of the gist of the present invention.

[0036] (Definition of Terms) In this specification, the term "azimuth" refers to the direction of interest when projected onto the substrate surface on the emission side of the optical element, and is expressed as the angle (azimuth angle) between the direction and a reference direction. Here, the reference direction (0°) is set to the horizontal right direction of the screen of the liquid crystal panel when the optical element is viewed from the emission side. The azimuth angle is defined as a positive angle counterclockwise and a negative angle clockwise. Both counterclockwise and clockwise represent the rotation directions when the optical element is viewed from the emission side. The azimuth angle represents a value measured when the optical element is viewed in plan from the emission side.

[0037] In this specification, "two straight lines (including axes, directions, and orientations) perpendicular to each other" means that they are perpendicular to each other when the optical element is viewed in plan from the light-emitting side. "One of the two straight lines is oblique to the other" means that one of the two straight lines is oblique to the other when the optical element is viewed in plan from the light-emitting side. "The angle between the two straight lines" means the angle between one straight line and the other when the optical element is viewed in plan from the light-emitting side.

[0038] In this specification, when two straight lines (including axes, directions, and orientations) are perpendicular to each other, the angle between them is 90°±5°, preferably 90°±3°, more preferably 90°±1°, and particularly preferably 90° (completely perpendicular). When two straight lines are parallel to each other, the angle between them is 0°±5°, preferably 0°±3°, more preferably 0°±1°, and particularly preferably 0° (completely parallel).

[0039] In this specification, the retardation in the in-plane direction (in-plane phase difference, in-plane retardation) Re is defined as Re = (ns - nf) d. Furthermore, the retardation in the thickness direction Rth is defined as Rth = (nz - (nx + ny) / 2) d. ns indicates the larger of nx and ny, and nf indicates the smaller. Furthermore, nx and ny indicate the principal refractive index in the in-plane direction of the birefringent layer (including the retardation film and the liquid crystal layer), nz indicates the principal refractive index in the out-of-plane direction, i.e., the direction perpendicular to the surface of the birefringent layer, and d indicates the thickness of the birefringent layer.

[0040] In this specification, the wavelength for measuring optical parameters such as the principal refractive index and phase difference is 550 nm unless otherwise specified. The retardation Re in the in-plane direction is also simply referred to as "retardation Re."

[0041] The following describes embodiments of the present invention. The present invention is not limited to the contents described in the following embodiments, and appropriate design changes can be made within the scope of the configuration of the present invention.

[0042] (Embodiment 1) Fig. 1 is a cross-sectional schematic diagram of an optical element according to embodiment 1. Fig. 2 is a cross-sectional schematic diagram of a first liquid crystal cell and a second liquid crystal cell included in the optical element according to embodiment 1. Fig. 3 is a schematic diagram illustrating the orientation of liquid crystal molecules in a first state and a second state of the optical element according to embodiment 1.

[0043] 1 to 3, the optical element 10 of this embodiment includes, in this order, a first substrate 100, a first liquid crystal layer 500 containing first liquid crystal molecules 510, a second substrate 200, a third substrate 300, a second liquid crystal layer 600 containing second liquid crystal molecules 610, and a fourth substrate 400. The first substrate 100, the first liquid crystal layer 500, and the second substrate 200 constitute a first liquid crystal cell 11A, and the third substrate 300, the second liquid crystal layer 600, and the fourth substrate 400 constitute a second liquid crystal cell 11B. The first liquid crystal cell 11A has, on at least one of the first substrate 100 and the second substrate 200, a first solid electrode 120 and a second solid electrode 220 as the first electrodes for applying a voltage to the first liquid crystal layer 500. The second liquid crystal cell 11B has, on at least one of the third substrate 300 and the fourth substrate 400, a third solid electrode 320 and a fourth solid electrode 420 as the second electrodes for applying a voltage to the second liquid crystal layer 600. The first electrode and the second electrode are arranged so as to be switchable between a first state in which the second liquid crystal molecules 610 are twistedly aligned and the first liquid crystal molecules 510 are vertically aligned, and a second state in which the first liquid crystal molecules 510 are twistedly aligned and the second liquid crystal molecules 610 are vertically aligned. The azimuth angle of the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side in the first state and the azimuth angle of the alignment direction 612A of the second liquid crystal molecules 612 on the fourth substrate 400 side in the first state are angles obtained by rotating the azimuth angle of the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side in the second state and the azimuth angle of the alignment direction 512A of the first liquid crystal molecules 512 on the second substrate 200 side in the second state in the same direction, respectively. By adopting such an embodiment, it is possible to drive the first state and the second state in the same way except that the entire system is rotated by a quarter, and it is possible to achieve polarization modulation in one of the first state and the second state and polarization non-modulation in the other state over a wide bandwidth and a wide viewing angle. That is, it is possible to realize an optical element that can switch between polarization modulation and polarization non-modulation over a wide band and a wide viewing angle, more specifically, a switchable half wave plate (sHWP) element.

[0044] Furthermore, the optical element 10 of this embodiment includes a first quarter-wave film 13 and a second quarter-wave film 14, which are arranged on the side of the first liquid crystal cell 11A opposite to the second liquid crystal cell 11B, or on the side of the second liquid crystal cell 11B opposite to the first liquid crystal cell 11A, and the first quarter-wave film 13 is arranged between the second quarter-wave film 14 and the first liquid crystal cell 11A and the second liquid crystal cell 11B. By adopting such an embodiment, it is possible to switch between polarization modulation and polarization non-modulation with high efficiency.

[0045] To achieve sHWP with a single liquid crystal layer, a possible configuration is an optical element 10R1 according to Comparative Example 1, which uses a liquid crystal cell 11R1 having a 90°-twisted TN liquid crystal layer 500R1, as shown in Fig. 4. More specifically, the optical element 10R1 according to Comparative Example 1 includes, in order, a quarter-wave film 15R having a slow-axis azimuth angle of 75°, a half-wave film 16R having a slow-axis azimuth angle of 15°, a liquid crystal cell 11R1, a half-wave film 17R having a slow-axis azimuth angle of -75°, and a quarter-wave film 18R having a slow-axis azimuth angle of -15°. Fig. 4 is a cross-sectional schematic diagram of the optical element according to Comparative Example 1.

[0046] Furthermore, when attempting to realize sHWP with two liquid crystal layers, a possible configuration is an optical element 10R2 of Comparative Example 2 in which a TN liquid crystal layer 500R2 twisted at 70° and a TN liquid crystal layer 500R3 twisted at −70° are stacked, as shown in Fig. 5. Fig. 5 is a cross-sectional schematic diagram of the optical element of Comparative Example 2.

[0047] Fig. 6 is a graph showing the relationship between the Stokes parameter S3 during modulation and the wavelength of the emitted light for the optical elements according to Comparative Example 1 and Comparative Example 2. Fig. 6 shows the wavelength dependency of the polarization state of the emitted light when right-handed circularly polarized light (Stokes parameter S3 = +1) is incident. The closer S3 is to -1, the more the light is converted to left-handed circularly polarized light. The closer it is to -1 across a wide wavelength range, the wider the bandwidth during modulation.

[0048] The optical element 10R1 of Comparative Example 1 is easy to design, but due to the influence of wavelength dispersion and the like of the 90° twisted TN liquid crystal layer 500R1, it is difficult to achieve a wide bandwidth, as shown in Figure 6. Furthermore, the optical element 10R2 of Comparative Example 2 can achieve a wide bandwidth by stacking a liquid crystal layer twisted by about 70 degrees, but it is difficult to achieve a wide viewing angle. On the other hand, the optical element 10 of this embodiment can switch between polarization modulation and polarization non-modulation over a wide bandwidth and a wide viewing angle.

[0049] The above-mentioned Patent Document 1 does not disclose any polarization modulation characteristics. Patent Document 1 discloses the configuration of a single TN liquid crystal layer, but with this configuration, during polarization modulation (inactive state, voltage OFF state in Patent Document 1), appropriate polarization conversion is only possible at specific wavelengths, and polarization conversion over a wide band cannot be achieved.

[0050] More specifically, in the single-layer configuration disclosed in Patent Document 1, the liquid crystal molecules are twisted 90° during polarization modulation, and are vertically aligned when a vertical electric field is applied during polarization non-modulation. Because the liquid crystal molecules are twisted 90° during polarization modulation, there is wavelength dependence, making it impossible to achieve polarization modulation over a wide bandwidth. Even if polarization modulation over a wide bandwidth can be achieved by adjusting the twist angle of the liquid crystal molecules or the cell thickness of the liquid crystal layer, polarization non-modulation over a wide bandwidth cannot be achieved during polarization non-modulation due to the influence of residual retardation by liquid crystal molecules near the substrate. In other words, it is impossible to achieve both polarization modulation and polarization non-modulation over a wide bandwidth.

[0051] The above-mentioned Patent Document 5 does not disclose any modulation characteristics. Furthermore, it does not describe specific physical properties of the retardation film, etc. Furthermore, since one of the stacked liquid crystal cells in Patent Document 5 is used as a backup, it is considered to have the same cell design as the other liquid crystal cell.

[0052] This embodiment will be described in detail below.

[0053] The alignment direction of the first liquid crystal molecules on the first substrate side refers to the alignment direction of the first liquid crystal molecules that are horizontally aligned near the first substrate. More specifically, when the alignment film provided on the first substrate on the first liquid crystal layer side is a horizontal alignment film, the alignment direction of the first liquid crystal molecules on the first substrate side refers to the alignment direction of the first liquid crystal molecules located at the interface of the first liquid crystal layer on the first substrate side. When the alignment film provided on the first substrate on the first liquid crystal layer side is a vertical alignment film, the liquid crystal molecules located at the interface of the first liquid crystal layer on the first substrate side are vertically aligned, and therefore the alignment direction of the first liquid crystal molecules on the first substrate side refers to the alignment direction of the first liquid crystal molecules that are horizontally aligned and located inside the first liquid crystal layer from the interface on the first substrate side.

[0054] Similarly, the alignment direction of the first liquid crystal molecules on the second substrate side refers to the alignment direction of the first liquid crystal molecules that are horizontally aligned near the second substrate. More specifically, when the alignment film provided on the first liquid crystal layer side of the second substrate is a horizontal alignment film, the alignment direction of the first liquid crystal molecules on the second substrate side refers to the alignment direction of the first liquid crystal molecules located at the interface of the first liquid crystal layer on the second substrate side. When the alignment film provided on the first liquid crystal layer side of the second substrate is a vertical alignment film, the liquid crystal molecules located at the interface of the first liquid crystal layer on the second substrate side are vertically aligned, so the alignment direction of the first liquid crystal molecules on the second substrate side refers to the alignment direction of the first liquid crystal molecules that are horizontally aligned and located inside the first liquid crystal layer from the interface on the second substrate side.

[0055] Similarly, the alignment direction of the second liquid crystal molecules on the third substrate side refers to the alignment direction of the second liquid crystal molecules that are horizontally aligned near the third substrate. More specifically, when the alignment film provided on the second liquid crystal layer side of the third substrate is a horizontal alignment film, the alignment direction of the second liquid crystal molecules on the third substrate side refers to the alignment direction of the second liquid crystal molecules located at the interface of the second liquid crystal layer on the third substrate side. When the alignment film provided on the second liquid crystal layer side of the third substrate is a vertical alignment film, the liquid crystal molecules located at the interface of the second liquid crystal layer on the third substrate side are vertically aligned, so the alignment direction of the second liquid crystal molecules on the third substrate side refers to the alignment direction of the second liquid crystal molecules that are horizontally aligned and located inside the second liquid crystal layer from the interface on the third substrate side.

[0056] Similarly, the alignment direction of the second liquid crystal molecules on the fourth substrate side refers to the alignment direction of the second liquid crystal molecules that are horizontally aligned near the fourth substrate. More specifically, when the alignment film provided on the second liquid crystal layer side of the fourth substrate is a horizontal alignment film, the alignment direction of the second liquid crystal molecules on the fourth substrate side refers to the alignment direction of the second liquid crystal molecules located at the interface of the second liquid crystal layer on the fourth substrate side. When the alignment film provided on the second liquid crystal layer side of the fourth substrate is a vertical alignment film, the liquid crystal molecules located at the interface of the second liquid crystal layer on the fourth substrate side are vertically aligned, and therefore the alignment direction of the second liquid crystal molecules on the fourth substrate side refers to the alignment direction of the second liquid crystal molecules that are horizontally aligned and located inside the second liquid crystal layer from the interface on the fourth substrate side.

[0057] The azimuth angle of the alignment direction of the second liquid crystal molecules on the third substrate side in the first state and the azimuth angle of the alignment direction of the second liquid crystal molecules on the fourth substrate side in the first state are respectively an angle obtained by rotating the azimuth angle of the alignment direction of the first liquid crystal molecules on the first substrate side in the second state and the azimuth angle of the alignment direction of the first liquid crystal molecules on the second substrate side in the second state by 1 / 4 in the same direction means that the azimuth angle of the alignment direction of the second liquid crystal molecules on the third substrate side in the first state and the azimuth angle of the alignment direction of the second liquid crystal molecules on the fourth substrate side in the first state are respectively an angle obtained by rotating the azimuth angle of the alignment direction of the second liquid crystal molecules on the third substrate side in the first state by 1 / 4 in the same direction. The azimuth angle of the alignment direction of the first liquid crystal molecules on the first substrate side in the second state and the azimuth angle of the alignment direction of the first liquid crystal molecules on the second substrate side in the second state are respectively a quarter-rotation angle in the positive direction of the azimuth angle of the alignment direction of the first liquid crystal molecules on the third substrate side in the first state and the azimuth angle of the alignment direction of the second liquid crystal molecules on the fourth substrate side in the first state.

[0058] Here, a quarter turn means 80° or more and 100° or less, preferably 85° or more and 95° or less, and more preferably 87° or more and 93° or less.

[0059] The first liquid crystal cell 11A includes, in order from the incident side to the exit side, a first substrate 100, a first liquid crystal layer 500 containing first liquid crystal molecules 510, and a second substrate 200. The first substrate 100 includes a first support substrate 110 and a first solid electrode 120, and the second substrate 200 includes a second support substrate 210 and a second solid electrode 220.

[0060] The second liquid crystal cell 11B includes, in order from the incident side to the exit side, a third substrate 300, a second liquid crystal layer 600 containing second liquid crystal molecules 610, and a fourth substrate 400. The third substrate 300 includes a third support substrate 310 and a third solid electrode 320, and the fourth substrate 400 includes a fourth support substrate 410 and a fourth solid electrode 420.

[0061] Examples of the first support substrate 110, the second support substrate 210, the third support substrate 310, and the fourth support substrate 410 include insulating substrates such as glass substrates and plastic substrates. Examples of materials for glass substrates include glass such as float glass and soda glass. Examples of materials for plastic substrates include plastics such as polyethylene terephthalate, polybutylene terephthalate, polyethersulfone, polycarbonate, polyimide, and alicyclic polyolefin.

[0062] The first solid electrode 120, the second solid electrode 220, the third solid electrode 320, and the fourth solid electrode 420 can be formed by forming a single layer or multiple layers of a transparent conductive material such as indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO), or tin oxide (SnO), or an alloy thereof, by sputtering or the like, and then patterning the layer using photolithography. In this specification, a solid electrode refers to an electrode that does not have a slit or opening at least in an area that overlaps with the optical opening of a pixel in a plan view.

[0063] One of the first solid electrode 120 and the second solid electrode 220 is a pixel electrode, and the other is a common electrode. One of the third solid electrode 320 and the fourth solid electrode 420 is a pixel electrode, and the other is a common electrode.

[0064] The first liquid crystal layer 500 contains a liquid crystal material, and by applying a voltage to the first liquid crystal layer 500 and changing the orientation state of the first liquid crystal molecules 510 in the liquid crystal material in accordance with the applied voltage, the polarization state of light passing through the first liquid crystal layer 500 can be changed.

[0065] The second liquid crystal layer 600 contains a liquid crystal material, and by applying a voltage to the second liquid crystal layer 600 and changing the orientation state of the second liquid crystal molecules 610 in the liquid crystal material in accordance with the applied voltage, the polarization state of light passing through the second liquid crystal layer 600 can be changed.

[0066] The first liquid crystal molecules 510 and the second liquid crystal molecules 610 may be positive-type liquid crystal molecules having a positive dielectric anisotropy (Δε) defined by the following formula (L), or may be negative-type liquid crystal molecules having a negative dielectric anisotropy. Alternatively, one of the first liquid crystal molecules 510 and the second liquid crystal molecules 610 may be a positive-type liquid crystal molecule, and the other may be a negative-type liquid crystal molecule. In this embodiment, a case where the first liquid crystal molecules 510 and the second liquid crystal molecules 610 are positive-type liquid crystal molecules will be described as an example. The long axis direction of the liquid crystal molecules is the direction of the slow axis. Δε = (dielectric constant in the long axis direction of the liquid crystal molecules) - (dielectric constant in the short axis direction of the liquid crystal molecules) (L)

[0067] The first liquid crystal layer 500 contains first liquid crystal molecules 510 that are twistedly aligned between the first substrate 100 and the second substrate 200. In the second state, the first liquid crystal molecules 510 are twistedly aligned from the first substrate 100 side to the second substrate 200 side.

[0068] The second liquid crystal layer 600 contains second liquid crystal molecules 610 that are twistedly aligned between the third substrate 300 and the fourth substrate 400. In the first state, the second liquid crystal molecules 610 are twistedly aligned from the third substrate 300 side to the fourth substrate 400 side.

[0069] The twisted alignment of the first liquid crystal molecules 510 and the second liquid crystal molecules 610 can be achieved, for example, by adding a chiral agent to the liquid crystal material. There are no particular limitations on the chiral agent, and any conventionally known agent can be used. For example, S-811 (manufactured by Merck) can be used as the chiral agent.

[0070] In this embodiment, the first liquid crystal molecules 510 and the second liquid crystal molecules 610 are twistedly aligned positive liquid crystal molecules. Therefore, when the first liquid crystal layer 500 is in a voltage-applied state and the second liquid crystal layer 600 is in a voltage-unapplied state, a first state can be achieved in which the first liquid crystal molecules 510 are vertically aligned and the second liquid crystal molecules 610 are twistedly aligned. Furthermore, when the first liquid crystal layer 500 is in a voltage-unapplied state and the second liquid crystal layer 600 is in a voltage-applied state, a second state can be achieved in which the first liquid crystal molecules 510 are twistedly aligned and the second liquid crystal molecules 610 are vertically aligned. In this embodiment, polarization non-modulation can be achieved in the first state, and polarization modulation can be achieved in the second state.

[0071] The retardation Re of the first liquid crystal layer 500 in the second state at a wavelength of 550 nm is preferably 196 nm or more and 280 nm or less, and more preferably 210 nm or more and 265 nm or less. This configuration allows for more efficient switching between polarization modulation and polarization non-modulation. In this specification, the voltage-applied state in which a voltage equal to or greater than a threshold value is applied to the liquid crystal layer is also referred to simply as the "voltage-applied state" or "when a voltage is applied," and the voltage-free state in which a voltage below the threshold value (including when no voltage is applied) is applied to the liquid crystal layer is also referred to simply as the "voltage-free state" or "when no voltage is applied."

[0072] The retardation Re of the second liquid crystal layer 600 in the first state at a wavelength of 550 nm is preferably 200 nm or more and 280 nm or less, and more preferably 220 nm or more and 264 nm or less. By adopting such an embodiment, it is possible to switch between polarization modulation and polarization non-modulation with higher efficiency.

[0073] The first liquid crystal molecules 510 in the second state are preferably twisted at a twist angle of 58° or more and 78° or less, and more preferably at a twist angle of 62° or more and 75° or less. This configuration allows for more efficient switching between polarization modulation and polarization non-modulation. The twist angle of the liquid crystal molecules can be determined by measuring the Mueller matrix after light is emitted from the liquid crystal layer using an Axoscan (manufactured by OptoScience).

[0074] The second liquid crystal molecules 610 in the first state are preferably twisted at a twist angle of 57° or more and 76° or less, and more preferably at a twist angle of 62° or more and 73° or less. By adopting such an embodiment, it is possible to more efficiently switch between polarization modulation and polarization non-modulation.

[0075] The twist angle of the first liquid crystal molecules 510 in the second state refers to the angle between the azimuth angle of the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side in the second state and the azimuth angle of the alignment direction 512A of the first liquid crystal molecules 512 on the second substrate 200 side. The twist angle of the second liquid crystal molecules 610 in the first state refers to the angle between the azimuth angle of the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side in the first state and the azimuth angle of the alignment direction 612A of the second liquid crystal molecules 612 on the fourth substrate 400 side.

[0076] In the second state, the azimuth angle of the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side is preferably −12° or more and 10° or less, and more preferably −7.5° or more and 7.2° or less. By adopting such an embodiment, it is possible to switch between polarization modulation and polarization non-modulation with higher efficiency.

[0077] In the first state, the azimuth angle of the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side is preferably 79° or more and 98° or less, and more preferably 83° or more and 95° or less. By adopting such an embodiment, it is possible to switch between polarization modulation and polarization non-modulation with higher efficiency.

[0078] For example, the azimuth angle of the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side in the second state can be set to 0°, and the azimuth angle of the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side in the first state can be set to 90°.

[0079] The first liquid crystal cell 11A preferably includes a first alignment film 41 on the first liquid crystal layer 500 side of the first substrate 100, and a second alignment film 42 on the first liquid crystal layer 500 side of the second substrate 200. The second liquid crystal cell 11B preferably includes a third alignment film 43 on the second liquid crystal layer 600 side of the third substrate 300, and a fourth alignment film 44 on the second liquid crystal layer 600 side of the fourth substrate 400.

[0080] The first alignment film 41 and the second alignment film 42 have the function of controlling the alignment of the first liquid crystal molecules 510 in the first liquid crystal layer 500, and when no voltage is applied to the first liquid crystal layer 500, the alignment of the first liquid crystal molecules 510 in the first liquid crystal layer 500 is controlled mainly by the action of the first alignment film 41 and the second alignment film 42.

[0081] The third alignment film 43 and the fourth alignment film 44 have a function of controlling the alignment of the second liquid crystal molecules 610 in the second liquid crystal layer 600, and when no voltage is applied to the second liquid crystal layer 600, the alignment of the second liquid crystal molecules 610 in the second liquid crystal layer 600 is controlled mainly by the action of the third alignment film 43 and the fourth alignment film 44. Hereinafter, the first alignment film 41, the second alignment film 42, the third alignment film 43, and the fourth alignment film 44 will also be simply referred to as alignment films.

[0082] As the material for the alignment film, a material commonly used in the field of liquid crystal display panels can be used, such as a polymer having polyimide in the main chain, a polymer having polyamic acid in the main chain, a polymer having polysiloxane in the main chain, etc. The alignment film can be formed by applying an alignment film material, and the application method is not particularly limited, and for example, flexographic printing, inkjet application, etc. can be used.

[0083] The alignment film may be a horizontal alignment film that aligns liquid crystal molecules approximately horizontally with respect to the film surface, or a vertical alignment film that aligns liquid crystal molecules approximately perpendicularly with respect to the film surface. In this embodiment, the first alignment film 41, the second alignment film 42, the third alignment film 43, and the fourth alignment film 44 are horizontal alignment films.

[0084] The horizontal alignment film has the function of aligning the liquid crystal molecules in the liquid crystal layer in the pixel region in a direction horizontal to the surface of the horizontal alignment film when no voltage is applied to the liquid crystal layer. Here, "the liquid crystal molecules are aligned in a direction horizontal to the surface of the horizontal alignment film" means that the pretilt angle of the liquid crystal molecules is 0° to 5°, preferably 0° to 2°, and more preferably 0° to 1°, with respect to the surface of the horizontal alignment film. The pretilt angle of the liquid crystal molecules means the angle at which the major axes of the liquid crystal molecules are inclined with respect to the main surfaces of the substrates when no voltage is applied to the liquid crystal layer.

[0085] The vertical alignment film has the function of aligning the liquid crystal molecules in the liquid crystal layer in the pixel region in a direction perpendicular to the surface of the vertical alignment film when no voltage is applied to the liquid crystal layer. Here, the liquid crystal molecules being aligned in a direction perpendicular to the surface of the vertical alignment film means that the pretilt angle of the liquid crystal molecules with respect to the surface of the vertical alignment film is 86° to 90°, preferably 87° to 89°, and more preferably 87.5° to 89°.

[0086] The alignment film may be a photo-alignment film having a photofunctional group and having been subjected to a photo-alignment treatment as an alignment treatment, or may be a rubbed alignment film having been subjected to a rubbing treatment as an alignment treatment. By performing the alignment treatment, a pretilt can be imparted to the liquid crystal molecules.

[0087] Since the alignment direction of the liquid crystal molecules is the direction of the alignment main axis (the direction in which the molecular long axes are aligned on average in nematic liquid crystal), the azimuth angle of the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side coincides with the azimuth angle of the alignment treatment direction of the alignment film (first alignment film 41) provided on the first liquid crystal layer 500 side of the first substrate 100. The azimuth angle of the alignment direction 512A of the first liquid crystal molecules 512 on the second substrate 200 side coincides with the azimuth angle of the alignment treatment direction of the alignment film (second alignment film 42) provided on the first liquid crystal layer 500 side of the second substrate 200. The azimuth angle of the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side coincides with the azimuth angle of the alignment treatment direction of the alignment film (third alignment film 43) provided on the second liquid crystal layer 600 side of the third substrate 300. The azimuth angle of the alignment direction 612A of the second liquid crystal molecules 612 on the fourth substrate 400 side coincides with the azimuth angle of the alignment treatment direction of the alignment film (fourth alignment film 44) provided on the second liquid crystal layer 600 side of the fourth substrate 400.

[0088] FIG. 7 is a cross-sectional view illustrating a first state of the optical element according to embodiment 1. FIG. 8 is a cross-sectional view illustrating a second state of the optical element according to embodiment 1. The optical element 10 of this embodiment preferably includes a negative C plate 12 between the first liquid crystal cell 11A and the second liquid crystal cell 11B. By adopting this configuration, as shown in FIG. 7 , in the first state, the phase difference of the first liquid crystal cell 11A at oblique incidence can be canceled by the negative C plate 12. Furthermore, as shown in FIG. 8 , in the second state, the phase difference of the second liquid crystal cell 11B at oblique incidence can be canceled by the negative C plate 12. As a result, it is possible to activate only the liquid crystal layer that is not being driven, and switching between polarization modulation and polarization non-modulation can be performed in a wider bandwidth and at a wider viewing angle.

[0089] The negative C plate 12 may be, for example, a stretched cycloolefin polymer film.

[0090] The retardation Rth in the thickness direction of the negative C plate 12 is preferably −410 nm or more and 0 nm or less, and more preferably −339 nm or more and −115 nm or less. By adopting such an embodiment, it is possible to switch between polarization modulation and polarization non-modulation with higher efficiency. Due to production reasons, the negative C plate 12 may have a retardation Re of about several nanometers, so the retardation Re of the negative C plate 12 is, for example, 0 nm or more and 5 nm or less.

[0091] 1 and other figures, the optical element 10 of this embodiment includes a first quarter-wave film 13 and a second quarter-wave film 14 on the side of the first liquid crystal cell 11A opposite to the second liquid crystal cell 11B, or on the side of the second liquid crystal cell 11B opposite to the first liquid crystal cell 11A, and the first quarter-wave film 13 is disposed between the second quarter-wave film 14 and the first and second liquid crystal cells 11A and 11B. By adopting such an embodiment, it is possible to switch between polarization modulation and polarization non-modulation with high efficiency over a wide band.

[0092] The quarter-wave films (specifically, the first quarter-wave film 13 and the second quarter-wave film 14) may be any films that impart a retardation Re of 20 nm or more and 240 nm or less to light with a wavelength of at least 550 nm.

[0093] Examples of materials for the quarter wavelength film include photopolymerizable liquid crystal materials, etc. Examples of the structure of the photopolymerizable liquid crystal material include a structure having a photopolymerizable group such as an acrylate group or a methacrylate group at the end of the skeleton of the liquid crystal molecule.

[0094] The quarter-wave film can be formed, for example, by the following method. First, a photopolymerizable liquid crystal material is dissolved in an organic solvent such as propylene glycol monomethyl ether acetate (PGMEA). Next, the resulting solution is applied to the surface of a substrate (e.g., a polyethylene terephthalate (PET) film) to form a coating film of the solution. The coating film of the solution is then pre-baked, irradiated with light (e.g., ultraviolet light), and then baked in this order to form the quarter-wave film.

[0095] Furthermore, a chiral agent may be added to the photopolymerizable liquid crystal material, and the liquid crystal polymer may be polymerized in a state twisted by 68° and used as the quarter-wave film.

[0096] The quarter-wave film may be, for example, a stretched polymer film, and examples of materials for the polymer film include cycloolefin polymer, polycarbonate, polysulfone, polyethersulfone, polyethylene terephthalate, polyethylene, polyvinyl alcohol, norbornene, triacetyl cellulose, and diacetyl cellulose.

[0097] The retardation Re of the first quarter-wave film 13 at a wavelength of 550 nm is preferably 72 nm or more and 210 nm or less, and more preferably 110 nm or more and 175 nm or less, so that polarization modulation and polarization non-modulation can be switched with higher efficiency.

[0098] The azimuth angle of the slow axis of the first quarter-wave film 13 is preferably 52° or more and 66° or less, and more preferably 55° or more and 64° or less, which allows for more efficient switching between polarization modulation and polarization non-modulation.

[0099] The retardation Re of the second quarter-wave film 14 at a wavelength of 550 nm is preferably 112 nm or more and 162 nm or less, and more preferably 121 nm or more and 152 nm or less, in this embodiment, it is possible to switch between polarization modulation and polarization non-modulation with higher efficiency.

[0100] The azimuth angle of the slow axis of the second quarter-wave film 14 is preferably 4° to 23°, more preferably 8° to 19°, inclusive, such that polarization modulation and non-modulation can be switched with higher efficiency.

[0101] At least one of the first quarter-wave film 13 and the second quarter-wave film 14 preferably has reverse wavelength dispersion characteristics, which allows for more efficient switching between polarization modulation and polarization non-modulation.

[0102] At least one of the first quarter-wave film 13 and the second quarter-wave film 14 preferably has flat wavelength dispersion characteristics. Since quarter-wave films with flat wavelength dispersion characteristics are cheaper than quarter-wave films with reverse wavelength dispersion characteristics, costs can be reduced by having at least one of the first quarter-wave film 13 and the second quarter-wave film 14 have flat wavelength dispersion characteristics.

[0103] It is preferable that one of the first quarter-wave film 13 and the second quarter-wave film 14 has flat wavelength dispersion characteristics and the other has reverse wavelength dispersion characteristics, which makes it possible to switch between polarization modulation and polarization non-modulation with high efficiency while suppressing costs.

[0104] It is also preferable that the first quarter-wave film 13 and the second quarter-wave film 14 have flat wavelength dispersion characteristics, which can further reduce costs.

[0105] In this specification, the term "wavelength dispersion of a retardation film" refers to the correlation between the absolute value of the retardation imparted by the retardation film and the wavelength of incident light. In the visible light region, the property in which the absolute value of the retardation imparted by the retardation film does not change even when the wavelength of incident light changes is called "flat wavelength dispersion characteristic." In addition, in the visible light region, the property in which the absolute value of the retardation imparted by the retardation film decreases as the wavelength of incident light increases is called "positive wavelength dispersion characteristic," and in the visible light region, the property in which the absolute value of the retardation imparted by the retardation film increases as the wavelength of incident light increases is called "reverse wavelength dispersion characteristic."

[0106] Having flat wavelength dispersion characteristics means that the retardation Re at a wavelength of 450 nm is 0.96 times or more and 1.06 times or less relative to the retardation Re at a wavelength of 550 nm, and that the retardation Re at a wavelength of 650 nm is 0.94 times or more and 1.04 times or less relative to the retardation Re at a wavelength of 550 nm.

[0107] Having inverse wavelength dispersion characteristics means that the retardation Re at a wavelength of 450 nm is 0.84 times or more and 1.00 times or less relative to the retardation Re at a wavelength of 550 nm, and that the retardation Re at a wavelength of 650 nm is 0.99 times or more and 1.09 times or less relative to the retardation Re at a wavelength of 550 nm.

[0108] It is preferable that the light incident on the optical element 10 is circularly polarized light. By adopting such an embodiment, it is possible to realize the optical element 10 that can switch the polarization state of circularly polarized light.

[0109] 9 is a diagram illustrating the polarization state. The principle of polarization modulation by the optical element 10 of this embodiment will be explained using the Poincaré sphere in FIG. 9. First, right-handed circularly polarized light (S3=+1) is incident on the first liquid crystal cell 11A (plot indicated by X1 in FIG. 9).

[0110] Next, after passing through the first liquid crystal layer 500 with a 68-degree twist, the right-handed circularly polarized light is converted once into the polarization state shown by the plot X2 in Figure 9. The multiple plots shown by X2 correspond to different wavelengths within the wavelength range of 380 nm to 780 nm. Light with a wavelength of around 550 nm is linearly polarized (on the equator on the Poincaré sphere), but light with other wavelengths is plotted in the northern hemisphere of the Poincaré sphere and is elliptically polarized.

[0111] 9 passes through the first quarter-wave film 13 and is converted to the polarization state plotted as X3 in Fig. 9. Light with a wavelength of around 550 nm is linearly polarized (on the equator on the Poincaré sphere), but light with other wavelengths is elliptically polarized.

[0112] Furthermore, when the polarized light in the state indicated by X3 in Fig. 9 passes through the second quarter-wave film 14, almost all wavelengths are converted into left-handed circularly polarized light (south pole position on the Poincaré sphere) and emitted (converted into the polarization state indicated by X4 in Fig. 9). In other words, it can be seen that modulation from right-handed circularly polarized light to left-handed circularly polarized light has occurred.

[0113] Similarly, during non-modulation, right-handed circularly polarized light becomes linearly polarized once after passing through the second liquid crystal layer 600, which has a 68-degree twist. However, because the entire orientation of the liquid crystal is rotated by 90 degrees, the linear polarization is approximately 90 degrees different from that during modulation. Then, after the polarized light passes through the first quarter-wave film 13 and the second quarter-wave film 14, all wavelengths become right-handed circularly polarized light. In other words, right-handed circularly polarized light can be emitted as right-handed circularly polarized light, resulting in non-modulation.

[0114] (Variation 1 of Embodiment 1) In this variation, an aspect will be described in which the optical element 10 of the above-described Embodiment 1 further includes three positive C plates. FIG. 10 is a schematic cross-sectional view of an optical element according to Variation 1 of Embodiment 1. As shown in FIG. 10, the optical element 10 of this variation further includes a first positive C plate 19X disposed between the first quarter-wave film 13 and the second quarter-wave film 14. By adopting such an aspect, it is possible to more efficiently switch between polarization modulation and polarization non-modulation.

[0115] 10, the optical element 10 of this modification further includes, in addition to the first positive C plate 19X, a second positive C plate 19A arranged on the side of the second liquid crystal cell 11B opposite to the first liquid crystal cell 11A, and a third positive C plate 19B arranged on the side of the first liquid crystal cell 11A opposite to the second liquid crystal cell 11B. By adopting such an embodiment, it is possible to switch between polarization modulation and polarization non-modulation with even higher efficiency.

[0116] As the first positive C plate 19X, the second positive C plate 19A, and the third positive C plate 19B, for example, a film containing a material with negative intrinsic birefringence as a component and biaxially stretched in both the longitudinal and transverse directions, or a film coated with a liquid crystalline material such as a nematic liquid crystal, can be appropriately used.

[0117] The retardation Rth of the first positive C plate 19X in the thickness direction is preferably 0 nm or more and 320 nm or less, and more preferably 0 nm or more and 230 nm or less, so that polarization modulation and polarization non-modulation can be switched with higher efficiency.

[0118] 10, the second positive C plate 19A is preferably disposed between the second liquid crystal cell 11B and the first quarter-wave film 13. By adopting such an embodiment, it is possible to more efficiently switch between polarization modulation and polarization non-modulation.

[0119] The retardation Rth of the second positive C plate 19A in the thickness direction is preferably 0 nm or more and 252 nm or less, and more preferably 0 nm or more and 174 nm or less, so that polarization modulation and polarization non-modulation can be switched with higher efficiency.

[0120] The retardation Rth of the third positive C plate 19B in the thickness direction is preferably 0 nm or more and 290 nm or less, and more preferably 0 nm or more and 213 nm or less, which makes it possible to switch between polarization modulation and polarization non-modulation with higher efficiency.

[0121] The retardations Rth in the thickness direction of the first positive C plate 19X, the second positive C plate 19A, and the third positive C plate 19B may be the same or different from one another. The retardations Re of the first positive C plate 19X, the second positive C plate 19A, and the third positive C plate 19B may be the same or different from one another.

[0122] For production reasons, the first positive C plate 19X, the second positive C plate 19A, and the third positive C plate 19B may have a retardation Re of several nanometers, so the retardation Re of the first positive C plate 19X is, for example, 0 nm or more and 5 nm or less.

[0123] (Embodiment 2) In this embodiment, the features unique to this embodiment will be mainly described, and descriptions of the contents overlapping with those of the above-described Embodiment 1 and its modifications will be omitted. This embodiment is substantially the same as Embodiment 1 except that it does not include a negative C plate 12.

[0124] Fig. 11 is a cross-sectional schematic diagram of an optical element according to embodiment 2. In the above embodiment 1, the optical element 10 is described as including a negative C plate 12, but as shown in Fig. 11, the optical element 10 does not have to include a negative C plate 12. By adopting such an embodiment, the optical element 10 can be manufactured thin and at low cost.

[0125] (Embodiment 3) In this embodiment, the features unique to this embodiment will be mainly described, and descriptions of the same content as in the above-described Embodiment 1 and its modifications, and Embodiment 2 will be omitted. This embodiment is substantially the same as Embodiment 1, except that the configurations of the first liquid crystal cell 11A and the second liquid crystal cell 11B are different.

[0126] Fig. 12 is a cross-sectional schematic view of a first liquid crystal cell and a second liquid crystal cell included in an optical element according to embodiment 3. Fig. 13 is a schematic view illustrating the orientation of liquid crystal molecules in a first state and a second state of an optical element according to embodiment 3. Fig. 14 is a cross-sectional schematic view illustrating the first state of an optical element according to embodiment 3. Fig. 15 is a cross-sectional schematic view illustrating the second state of an optical element according to embodiment 3.

[0127] The first liquid crystal molecules 510 and the second liquid crystal molecules 610 of the optical element 10 of this embodiment shown in FIGS. 12 to 15 are twisted, negative-type liquid crystal molecules. Therefore, as shown in FIG. 14 , when the first liquid crystal layer 500 is in a voltage-unapplied state and the second liquid crystal layer 600 is in a voltage-applied state, a first state can be achieved in which the first liquid crystal molecules 510 are vertically aligned and the second liquid crystal molecules 610 are twistedly aligned. In the first state, the retardation of the first liquid crystal cell 11A can be canceled by the negative C-plate 12. Furthermore, as shown in FIG. 15 , when the first liquid crystal layer 500 is in a voltage-applied state and the second liquid crystal layer 600 is in a voltage-unapplied state, a second state can be achieved in which the first liquid crystal molecules 510 are twistedly aligned and the second liquid crystal molecules 610 are vertically aligned. In the second state, the retardation of the second liquid crystal cell 11B can be canceled by the negative C-plate 12.

[0128] The first alignment film 41, the second alignment film 42, the third alignment film 43 and the fourth alignment film 44 are preferably vertical alignment films.

[0129] (Embodiment 4) In this embodiment, the features unique to this embodiment will be mainly described, and descriptions of the contents overlapping with those of the above-described Embodiment 1 and its modifications, and Embodiments 2 and 3 will be omitted. This embodiment is substantially the same as Embodiment 1, except that the configuration of the second liquid crystal cell 11B is different.

[0130] Fig. 16 is a cross-sectional schematic view of a first liquid crystal cell and a second liquid crystal cell included in an optical element according to embodiment 4. Fig. 17 is a schematic view illustrating the orientation of liquid crystal molecules in a first state and a second state of an optical element according to embodiment 4. Fig. 18 is a cross-sectional schematic view illustrating a first state of an optical element according to embodiment 4. Fig. 19 is a cross-sectional schematic view illustrating a second state of an optical element according to embodiment 4.

[0131] The first liquid crystal molecules 510 of the optical element 10 of this embodiment shown in Figures 16 to 19 are twistedly aligned positive liquid crystal molecules, and the second liquid crystal molecules 610 are twistedly aligned negative liquid crystal molecules. Therefore, as shown in Figure 18, when a voltage is applied to both the first liquid crystal layer 500 and the second liquid crystal layer 600, a first state can be achieved in which the first liquid crystal molecules 510 are vertically aligned and the second liquid crystal molecules 610 are twistedly aligned. In the first state, the retardation of the first liquid crystal cell 11A can be canceled by the negative C plate 12. Furthermore, as shown in Figure 19, when a voltage is not applied to both the first liquid crystal layer 500 and the second liquid crystal layer 600, a second state can be achieved in which the first liquid crystal molecules 510 are twistedly aligned and the second liquid crystal molecules 610 are vertically aligned. In the second state, the retardation of the second liquid crystal cell 11B can be canceled by the negative C plate 12.

[0132] It is preferable that the first alignment film 41 and the second alignment film 42 are horizontal alignment films, and the third alignment film 43 and the fourth alignment film 44 are vertical alignment films.

[0133] (Embodiment 5) In this embodiment, features unique to this embodiment will be mainly described, and descriptions of content that overlaps with the above-described Embodiment 1 and its modifications, and Embodiments 2 to 4 will be omitted. In this embodiment, a variable-focus element including the optical element (sHWP) of Embodiments 1 to 4 will be described. FIG. 20 is a cross-sectional schematic diagram of a variable-focus element according to Embodiment 5. The variable-focus element 30 of this embodiment shown in FIG. 20 includes an optical element 10 and a Pancharatnam Berry (PB) lens 20.

[0134] As described above, the optical element 10 of Embodiments 1 to 4 can modulate circularly polarized light. Furthermore, since the PB lens 20 has different focal lengths for right-handed and left-handed circularly polarized light, a variable-focus element 30 can be realized by combining the optical element 10 and the PB lens 20.

[0135] The PB lens 20 has a function of condensing and diverging circularly polarized light. The PB lens 20 can be produced by, for example, the method described in WO 2019 / 189818.

[0136] Fig. 21 is an example of a cross-sectional schematic diagram of a PB lens included in a variable-focus element according to embodiment 5. As shown in Fig. 21 , the PB lens 20 includes an optically anisotropic layer 700. As an example, the PB lens 20 refracts and transmits circularly polarized light incident thereon in a predetermined direction. Note that in Fig. 21 , the incident light is assumed to be left-handed circularly polarized light.

[0137] In the portion shown in Figure 21, the optically anisotropic layer 700 has three regions R0, R1, and R2 from the left in Figure 21, and the length Λ of one period is different in each region. Specifically, the length Λ of one period becomes shorter in the order of regions R0, R1, and R2. Furthermore, regions R1 and R2 have a structure in which the optical axis is twisted and rotated in the thickness direction of the optically anisotropic layer (hereinafter also referred to as a twisted structure). The twist angle in the thickness direction of region R1 is smaller than the twist angle in the thickness direction of region R2. Note that region R0 is a region that does not have a twisted structure (i.e., the twist angle is 0°). Note that the twist angle is the twist angle in the entire thickness direction.

[0138] In the optical element 10, when left-handed circularly polarized light LC1 enters region R1 in the plane of the optically anisotropic layer 700, it is refracted at a predetermined angle in the direction of arrow X with respect to the direction of incidence, i.e., in one direction in which the orientation of the optical axes of the liquid crystal molecules 710 changes while continuously rotating, and then transmitted. Similarly, when left-handed circularly polarized light LC2 enters region R2 in the plane of the optically anisotropic layer 700, it is refracted at a predetermined angle in the direction of arrow X with respect to the direction of incidence and then transmitted. Similarly, when left-handed circularly polarized light LC0 enters region R0 in the plane of the optically anisotropic layer 700, it is refracted at a predetermined angle in the direction of arrow X with respect to the direction of incidence and then transmitted.

[0139] Here, the angle of refraction by the optically anisotropic layer 700 is one period Λ of the liquid crystal alignment pattern in the region R1. R1 than one period Λ of the liquid crystal alignment pattern in region R2 R2 Since the angle of refraction of the incident light is short, as shown in FIG. 21, the angle θ R2 The angle θ of the transmitted light in the region R1 isR1 In addition, one period Λ of the liquid crystal alignment pattern in the region R1 is larger than R1 than one period Λ of the liquid crystal alignment pattern in the region R0 R0 Since the angle of refraction of the incident light is long, as shown in FIG. 21, the angle θ of the transmitted light in the region R0 is R0 The angle θ of the transmitted light in the region R1 is R1 will be smaller than

[0140] Here, in the diffraction of light by an optically anisotropic layer having a liquid crystal orientation pattern in which the orientation of the optical axes of the liquid crystal molecules changes while continuously rotating within the plane, there is a problem that the diffraction efficiency decreases as the diffraction angle increases, that is, the intensity of the diffracted light weakens. Therefore, if the optically anisotropic layer is configured to have regions where the length of one period in which the orientation of the optical axes of the liquid crystal molecules rotates 180° within the plane varies, the diffraction angle varies depending on the position of incidence of light, resulting in a difference in the amount of diffracted light depending on the position of incidence within the plane. In other words, depending on the position of incidence within the plane, there will be regions where the transmitted and diffracted light becomes dark.

[0141] In contrast, the PB lens 20 of this embodiment has a region where the optically anisotropic layer twists and rotates in the thickness direction, and has regions with different twist angles in the thickness direction. In the example shown in Figure 21, the twist angle φ in the thickness direction of region R2 of the optically anisotropic layer 700 is R2 is the twist angle φ in the thickness direction of region R1 R1 Furthermore, the region R0 does not have a twisted structure in the thickness direction, which makes it possible to suppress a decrease in the diffraction efficiency of refracted light.

[0142] 21 , by providing a twisted structure to regions R1 and R2, which have a larger diffraction angle than region R0, it is possible to suppress a decrease in the amount of light refracted in regions R1 and R2. Furthermore, by making the twisted angle of the twisted structure in region R2, which has a larger diffraction angle than region R1, larger than that of region R1, it is possible to suppress a decrease in the amount of light refracted in region R2. This makes it possible to make the amount of transmitted light uniform depending on the incident position within the plane.

[0143] As described above, in the PB lens 20 of this embodiment, in in-plane regions where the refraction by the optically anisotropic layer is large, incident light passes through and is refracted in layers with a large twist angle in the thickness direction. In contrast, in in-plane regions where the refraction by the optically anisotropic layer is small, incident light passes through and is refracted in layers with a small twist angle in the thickness direction. That is, in the PB lens 20, by setting the in-plane twist angle in the thickness direction according to the magnitude of refraction by the optically anisotropic layer, it is possible to brighten the transmitted light relative to the incident light. Therefore, the PB lens 20 can reduce the refraction angle dependence of the amount of transmitted light in the plane.

[0144] The angle of light refraction in the plane of the optically anisotropic layer 700 increases as the period Λ of the liquid crystal orientation pattern decreases. Furthermore, the twist angle in the thickness direction in the plane of the optically anisotropic layer 700 is larger in a region with a short period Λ, where the optical axis rotates 180° along the direction of the arrow X in the liquid crystal orientation pattern, than in a region with a long period Λ. In the PB lens 20, as shown in FIG. 21 , for example, the period Λ of the liquid crystal orientation pattern in region R2 of the optically anisotropic layer 700 is R2 is one period Λ of the liquid crystal alignment pattern in the region R1. R1 shorter than the twist angle φ in the thickness direction R2 That is, the region R2 of the optically anisotropic layer 700 on the light incident side refracts light more.

[0145] Therefore, by setting the in-plane twist angle φ in the thickness direction for one period Λ of the target liquid crystal orientation pattern, it is possible to suitably brighten the transmitted light that is refracted at different angles in different regions in the plane.

[0146] As described above, in the PB lens 20, the shorter the period Λ of the liquid crystal orientation pattern, the larger the angle of refraction, and therefore, the brighter the transmitted light can be made by increasing the twist angle in the thickness direction in regions where the period Λ of the liquid crystal orientation pattern is shorter. Therefore, in the PB lens 20, it is preferable to have regions where the permutation of the length of one period and the permutation of the magnitude of the twist angle in the thickness direction are different in regions where the length of one period of the liquid crystal orientation pattern is different.

[0147] As described above, the PB lens 20 has an optically anisotropic layer 700 formed using a liquid crystal composition containing liquid crystal molecules 710, and the optically anisotropic layer 700 has a liquid crystal orientation pattern in which the direction of the optical axis derived from the liquid crystal molecules changes while continuously rotating along at least one direction in the plane, and has a region in which the optical axis twists and rotates in the thickness direction of the optically anisotropic layer 700, and preferably has regions with different magnitudes of twist angles in the thickness direction.

[0148] It is preferable that the PB lens 20 has regions in which the length of one period in the liquid crystal orientation pattern is different, when the length of one period is defined as the length of the optical axis direction originating from the liquid crystal molecule 710 rotating 180° in the plane.

[0149] In the optically anisotropic layer 700, it is preferable that a plurality of regions having different lengths of one period in the liquid crystal orientation pattern are arranged in the order of the lengths of one period, and a plurality of regions having different magnitudes of twist angles in the thickness direction are arranged in the order of the magnitudes of the twist angles in the thickness direction, and that the direction of the permutation of the lengths of one period is different from the direction of the permutation of the magnitudes of the twist angles in the thickness direction.

[0150] The optically anisotropic layer 700 preferably has a region where the twist angle in the thickness direction is 10° to 360°.

[0151] In the optically anisotropic layer 700, it is preferable that one period of the liquid crystal orientation pattern gradually becomes shorter toward the one direction in which the direction of the optical axis derived from the liquid crystal molecules 710 in the liquid crystal orientation pattern changes while continuously rotating.

[0152] The liquid crystal orientation pattern of the optically anisotropic layer 700 is preferably a concentric pattern extending from the inside to the outside in the one direction in which the orientation of the optical axis derived from the liquid crystal molecules 710 changes while continuously rotating.

[0153] 21 is a PB lens whose twist angle varies in-plane and is an element that has high diffraction efficiency even when the diffraction angle is large, but the PB lens 20 may also be a PB lens whose twist angle does not vary in-plane. Specifically, the PB lens 20 may be a PB lens that has no twist in the thickness direction or has a constant twist angle in-plane, and for example, the polarization diffraction grating described in JP-A-2008-532085 can be used.

[0154] The PB lens 20 is a PB lens having a plurality of optically anisotropic layers 700, and preferably has optically anisotropic layers 700 whose twist angles in the thickness direction of the optically anisotropic layers 700 are different from each other.

[0155] The PB lens 20 is a PB lens having a plurality of optically anisotropic layers 700, and preferably has optically anisotropic layers 700 with different twist angles in the thickness direction of the optically anisotropic layers 700.

[0156] The PB lens 20 is a PB lens having multiple optically anisotropic layers 700, and it is preferable that the optically anisotropic layers 700 have a liquid crystal orientation pattern in which the directions in which the optical axes derived from the liquid crystal molecules 710 continuously rotate along at least one direction in the plane are the same.

[0157] The length of one period in the liquid crystal alignment pattern is preferably 50 μm or less.

[0158] The variable-focus element 30 may be a binary variable-focus element 30A having one laminated body made up of the optical element 10 and the PB lens 20, or may be a multi-stage variable-focus element 30B having two or more sets of laminated bodies made up of the optical element 10 and the PB lens 20. In this way, by combining multiple sets of the optical element 10 and the PB lens 20, it is possible to realize a variable-focus element 30B that is endowed with multi-stage tunability.

[0159] The variable-focus element 30 can be produced, for example, by attaching a PB lens 20 produced by the method described in International Publication No. 2019 / 189818 to the optical element 10.

[0160] (Variation 1 of Embodiment 5) In this variation, a variable-focus element 30 will be described in which the PB lens 20 of the above-described Embodiment 5 is disposed within the optical element 10 and is in-cell. Fig. 22 is a cross-sectional schematic diagram of a variable-focus element according to Variation 1 of Embodiment 5. Fig. 23 is an enlarged cross-sectional schematic diagram of a variable-focus element according to Variation 1 of Embodiment 5. Fig. 24 is a schematic diagram illustrating the orientation of liquid crystal molecules in the first state and the second state of the optical element according to Variation 1 of Embodiment 5.

[0161] The variable-focus element 30 of this modified example is a multi-stage variable-focus element 30B that includes two or more sets of laminated bodies each made up of an optical element 10 and a PB lens 20, as shown in FIG.

[0162] The PB lens 20 included in the variable-focus element 30 of this modified example is disposed within the optical element 10, as shown in Fig. 23. By incorporating the PB lens 20 in this manner, it is not necessary to attach the PB lens 20 externally, which allows for a significant reduction in manufacturing costs. It also makes it possible to reduce the thickness of the variable-focus element 30. Note that, for convenience, the optical element 10 and the PB lens 20 are shown separately in Fig. 22.

[0163] As shown in Figure 23, the variable focus element 30 of this modified example more specifically comprises, in order from the incident side to the exit side, a second quarter-wave film 14, a first quarter-wave film 13, a first substrate 100, a first liquid crystal layer 500, a second substrate 200, a third substrate 300, a second liquid crystal layer 600, a PB lens 20, and a fourth substrate 400.

[0164] The variable-focus element 30 may include a first alignment film 41 between the first substrate 100 and the first liquid crystal layer 500. The variable-focus element 30 may also include a second alignment film 42 between the second substrate 200 and the first liquid crystal layer 500. The variable-focus element 30 may also include a third alignment film 43 between the third substrate 300 and the second liquid crystal layer 600. The variable-focus element 30 may also include a fourth alignment film 44 between the PB lens 20 and the second liquid crystal layer 600.

[0165] In this modified example, the first liquid crystal cell 11A and the second liquid crystal cell 11B have the same configuration as in embodiment 1, and the first alignment film 41, the second alignment film 42, the third alignment film 43 and the fourth alignment film 44 are horizontal alignment films.

[0166] 24 , in this modification, the azimuth angle of the alignment direction 512A of the first liquid crystal molecules 512 on the second substrate 200 side in the second state is preferably −12° or more and 10° or less, and more preferably −7.5° or more and 7.2° or less. By adopting such an embodiment, it is possible to switch more efficiently between polarization modulation and polarization non-modulation. Furthermore, the azimuth angle of the alignment direction 612A of the second liquid crystal molecules 612 on the fourth substrate 400 side in the first state is preferably 79° or more and 98° or less, and more preferably 83° or more and 95° or less. By adopting such an embodiment, it is possible to switch more efficiently between polarization modulation and polarization non-modulation.

[0167] In this modified example, a negative C plate 12 is not disposed between the first liquid crystal cell 11A and the second liquid crystal cell 11B, but a negative C plate 12 may be disposed between the first liquid crystal cell 11A and the second liquid crystal cell 11B.

[0168] In other words, the in-cell PB lens 20 (PB lens layer) is an in-cell retardation layer patterned so that the slow axis direction rotates in-plane.

[0169] The PB lens can be in-cell formed, for example, as follows: A photosensitive material for forming an in-cell PB lens, which contains a polymer represented by the following general formula (PB-1), is applied to the fourth substrate 400 to form a PB lens forming film, and then an orientation treatment is performed on the PB lens forming film, thereby forming the PB lens 20 in-cell.

[0170] (In the above formula, V represents a spacer group, W represents a divalent organic group having a photofunctional group, and R 5 represents a monovalent group, and p represents an integer of 1 or more.

[0171] In the general formula (PB-1), V represents a spacer group.2 ) n It is preferable that the compound has an alkylene group having two or more carbon atoms, represented by - (where n is an integer of two or more). By adopting such an embodiment, it is possible to exhibit good retardation. The alkylene group is preferably linear.

[0172] In the above general formula (PB-1), W represents a divalent organic group having a photofunctional group. Examples of divalent organic groups having a photofunctional group include divalent organic groups containing a photofunctional group (photoreactive site) that undergoes reactions such as photodimerization, photoisomerization, photo-Fries rearrangement, and photodecomposition. Examples of photofunctional groups capable of photodimerization and photoisomerization include a cinnamate group, a chalcone group, a coumarin group, and a stilbene group. Examples of photofunctional groups capable of photoisomerization include an azobenzene group. Examples of photofunctional groups capable of photo-Fries rearrangement include a phenol ester group. Examples of photofunctional groups capable of photodecomposition include a cyclobutane ring.

[0173] R in the above general formula (PB-1) 5 represents a monovalent group. 5 is preferably a hydrogen atom or a monovalent hydrocarbon group, more preferably a hydrogen atom, a methyl group, or an ethyl group.

[0174] The orientation treatment on the PB lens formation film is performed by a plurality of orientation treatments, and the directions of the polarized light irradiated in the plurality of orientation treatments are different from one another. The orientation treatment on the PB lens formation film includes, for example, a first orientation treatment in which the PB lens formation film is oriented with polarized light at an azimuth angle of 0°, a second orientation treatment in which the PB lens formation film is oriented with polarized light at an azimuth angle of 45°, a third orientation treatment in which the PB lens formation film is oriented with polarized light at an azimuth angle of 90°, and a fourth orientation treatment in which the PB lens formation film is oriented with polarized light at an azimuth angle of 135°.

[0175] Fig. 25 is a plan view schematic diagram showing the orientation pattern of the PB lens provided in the variable-focus element according to Modification 1 of Embodiment 5. As shown in Fig. 25, the orientation pattern of the PB lens 20 has, for example, a continuously rotating orientation direction from the center to the periphery. In addition, in plan view, the orientation direction of the liquid crystal molecules 710 at the position of radius R is all the same. In other words, there is a predetermined angular distribution according to the distance from the center. The period P of the orientation pattern 1 and the diffraction angle θ is 1 = 2 × λ / sinθ, and the shorter the period of the orientation pattern, the greater the light diffraction angle. Therefore, if you want to obtain a lens effect that focuses light, you can achieve this by making the pitch wider (smaller diffraction angle) toward the center of the optical element and shorter (larger diffraction angle) toward the periphery.

[0176] The PB lens 20 having a different diopter D, which will be described later, can be manufactured by changing the design of this orientation pattern period. The orientation pattern can also be set based on WO 2020 / 186123, JP 2008-532085 A, etc.

[0177] In this modified example, the alignment process is performed using four exposures, but the more divided exposures there are, the more diffraction efficiency of the variable-focus element 30 can be obtained. Fabrication using a multi-light alignment process that applies a light alignment device is compatible with existing liquid crystal factories and allows for highly productive manufacturing. In this embodiment, the fabrication of the PB lens 20 using a multi-light alignment process is described, but alignment patterns can also be fabricated using existing methods such as optical interference and laser direct writing.

[0178] The phase difference of the in-cell PB lens 20 (PB lens layer) is preferably 100 nm or more and 500 nm or less, more preferably 200 nm or more and 350 nm or less, and particularly preferably λ / 2 (i.e., 275 nm). The diffraction efficiency is expressed by the following (Equation 1), and reaches its maximum value when Δnd = λ / 2.

[0179]

[0180] The variable focus element 30 of this modified example, i.e., a multi-stage variable focus element 30 that combines multiple laminates of optical elements 10 and PB lenses 20 in-cell in the optical elements 10, has, for example, the following characteristics.

[0181] Fig. 26 is a cross-sectional schematic diagram illustrating a detailed configuration of a variable-focus element according to Modification 1 of Embodiment 5. As shown in Fig. 26, variable-focus element 30 includes, in order from the incident side to the output side, optical element 10, a first PB lens 20A1, optical element 10, the first PB lens 20A1, optical element 10, a second PB lens 20A2, optical element 10, the second PB lens 20A2, optical element 10, a third PB lens 20A3, optical element 10, and the third PB lens 20A3.

[0182] The first PB lens 20A1 has a diopter D of ±0.25, the second PB lens 20A2 has a diopter D of ±0.5, and the third PB lens 20A3 has a diopter D of ±1. They have a characteristic of converging (+) when right-handed circularly polarized light is incident, and diverging (-) when left-handed circularly polarized light is incident.

[0183] Table 1 below explains the state of the optical element 10 and PB lenses 20A1, 20A2, and 20A3 in each mode of the variable-focus element 30 according to the first modification of the fifth embodiment.

[0184]

[0185] The F0 mode will be explained using Table 1 above. In this mode, all optical elements 10 are in the first state (non-modulation). Right-handed circularly polarized light enters the first optical element 10 without being modulated, and enters the first PB lens 20A1 as is. There, it is focused by 0.25D. The exiting light then becomes left-handed circularly polarized. Here, the change in direction of circular polarization even after passing through the PB lens 20 is a characteristic of the PB lens 20. Because the optical element 10 is non-modulated, the light passes through the second optical element 10 as left-handed circularly polarized light. The second PB lens 20A1 generates a divergence of -0.25D. As a result, the incident light passes unchanged through the first four lenses from the entrance side (optical element 10, first PB lens 20A1, optical element 10, and first PB lens 20A1). Subsequently, it similarly passes through the second PB lens 20A2 and PB lens 20A3, and the exiting light is emitted unchanged at 0D, just like the incident light.

[0186] The F1 mode will be explained using Table 1 above. In this mode, only the fourth optical element 10 from the incident side is in the second state. In this state, after passing through the first second PB lens 20A2, the light is left-handed circularly polarized with 0.5D added, just like in the F0 mode. It is then converted to right-handed circularly polarized light by the optical element in the second state. Next, the second second PB lens 20A2 adds +0.5D, giving the light a total of 1D, and it emerges as left-handed circularly polarized light. Thereafter, it emerges as 1D left-handed circularly polarized light. Because it has become left-handed circularly polarized light after passing through the second second PB lens 20A2, the sign at the third PB lens 20A3 is opposite to that at F0.

[0187] The F-2.5 mode will be described using Table 1 above and FIG. 27. FIG. 27 is a diagram illustrating the polarization state in the F-2.5 mode of the variable-focus element according to Modification 1 of Embodiment 5. As shown in Table 1 and FIG. 27, in the F-2.5 mode, the first four lenses from the incident side (optical element 10, first PB lens 20A1, optical element 10, and first PB lens 20A1) impart a bias of −0.5D to the right-handed circularly polarized light, and the last four lenses on the exit side (optical element 10, third PB lens 20A3, optical element 10, and third PB lens 20A3) impart a bias of −2D to the light, and the light is emitted as right-handed circularly polarized light with a total bias of −2.5D.

[0188] In addition, by using the same principle, it is possible to realize multiple focal lengths depending on which optical element 10 is set to the second modulation state. In this modified example, only three conditions are shown.

[0189] (Variation 2 of Embodiment 5) In the above-described Embodiment 5 and Variation 1 of Embodiment 5, the PB lens is provided in a film form (in-cell polymer form), but the PB lens may be a liquid crystal layer with fluidity, that is, a liquid crystal layer that can be driven by voltage. In this variation, a case where the PB lens is a liquid crystal layer that can be driven by voltage will be described.

[0190] A polymer-like PB lens, such as in the fifth embodiment and the first modification of the fifth embodiment, is called a passive PB lens because it cannot be changed by voltage. On the other hand, a PB lens formed from a liquid crystal layer with fluidity is called an active PB lens because it can be driven by voltage.

[0191] An active PB lens can be fabricated by the following procedure. First, an alignment treatment of a PB lens pattern is performed on the alignment film of one of a pair of substrates. The alignment film of the other substrate is a weak anchoring alignment film (slippery interface). Both substrates are provided with transparent electrodes. When this pair of substrates is bonded together with a liquid crystal layer sandwiched between them, the liquid crystal molecules are oriented along the pattern of the alignment treatment, and the liquid crystal layer also adopts the orientation of the PB lens pattern. This achieves an active PB lens. More preferably, a PSA (Polymer Sustained Alignment) treatment is then performed to stabilize the alignment of the liquid crystal molecules at the interface, thereby achieving an active PB lens with greater alignment stability and reliability.

[0192] When the voltage is off, the active PB lens has a PB lens pattern, which causes the lens to focus or diverge depending on the polarization state of the incident light.When the voltage is on, the liquid crystal molecules are vertically aligned, so the light passes through as is without focusing or diverging.

[0193] While a variable-focus element that combines an sHWP and a passive PB lens, such as in the fifth embodiment and the first modification of the fifth embodiment, can switch between two values, focusing and diverging, a variable-focus element that combines an sHWP and an active PB lens, such as in this modification, can switch between three values, focusing, diverging, and transmitting. As a result, smoother focus control is possible. Alternatively, the number of stacked voltage-driven elements can be reduced to achieve the same number of focal lengths.

[0194] (Embodiment 6) In this embodiment, features unique to this embodiment will be mainly described, and descriptions of content that overlaps with the above-described Embodiment 1 and its modifications, and Embodiments 2 to 5 and their modifications will be omitted. In this embodiment, a head-mounted display including a variable-focus element 30 will be described. Fig. 28 is a cross-sectional schematic diagram of a head-mounted display according to Embodiment 6. Fig. 29 is a perspective schematic diagram showing an example of the appearance of the head-mounted display according to Embodiment 6.

[0195] 28 and 29 , the head mounted display 1 of this embodiment includes a display panel 1P that displays an image, a retardation plate 40, and a variable-focus element 30. By using the head mounted display 1, light emitted from the display panel 1P, such as a liquid crystal display device or an organic electroluminescence display device, passes through the retardation plate 40 to become circularly polarized light, which then passes through the variable-focus element 30 and is visually perceived by the user U.

[0196] The effects of the present invention will be explained below with reference to examples and comparative examples, but the present invention is not limited to these examples.

[0197] Example 1 A simulation was performed on an optical element 10 of Example 1 having a configuration similar to that of Modification 1 of Embodiment 1 above, to evaluate the performance of switching between polarization modulation and polarization non-modulation. The optical element 10 of this example had a first liquid crystal cell 11A and a second liquid crystal cell 11B, and a negative C plate 12 having a thickness direction retardation Rth of -213 nm was disposed therebetween. The first liquid crystal molecules 510 and the second liquid crystal molecules 610 were positive-type liquid crystal molecules, and had a refractive index anisotropy Δn = 0.07. The first alignment film 41, the second alignment film 42, the third alignment film 43, and the fourth alignment film 44 were horizontal alignment films.

[0198] In the second state, the azimuth angle of the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side was 0°, and the azimuth angle of the alignment direction 512A of the first liquid crystal molecules 512 on the second substrate 200 side in the second state was 68°. In addition, the azimuth angle of the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side in the first state was 90°, and the azimuth angle of the alignment direction 612A of the second liquid crystal molecules 612 on the fourth substrate 400 side in the first state was 158°. In addition, the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side in the second state, the alignment direction 512A of the first liquid crystal molecules 512 on the second substrate 200 side in the second state, the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side in the first state, and the alignment direction 612A of the second liquid crystal molecules 612 on the fourth substrate 400 side in the first state correspond to the alignment treatment directions of the first alignment film 41, the second alignment film 42, the third alignment film 43, and the fourth alignment film 44, respectively, and therefore the alignment directions 511A, 512A, 611A, and 612A can be determined from the alignment treatment directions of the first alignment film 41, the second alignment film 42, the third alignment film 43, and the fourth alignment film 44, respectively.

[0199] The first quarter-wave film 13 had a reverse wavelength dispersion characteristic, and the second quarter-wave film 14 had a flat wavelength dispersion characteristic. Specifically, the quarter-wave film with a reverse wavelength dispersion characteristic used in the examples and comparative examples had a retardation Re at a wavelength of 450 nm that was 1.01 times the retardation Re at a wavelength of 550 nm, and a retardation Re at a wavelength of 650 nm that was 0.99 times the retardation Re at a wavelength of 550 nm. Specifically, the quarter-wave film with a flat wavelength dispersion characteristic used in the examples and comparative examples had a retardation Re at a wavelength of 450 nm that was 0.89 times the retardation Re at a wavelength of 550 nm, and a retardation Re at a wavelength of 650 nm that was 1.04 times the retardation Re at a wavelength of 550 nm.

[0200] The retardation Re of both the first quarter-wave film 13 and the second quarter-wave film 14 for light with a wavelength of 550 nm was 140 nm. The azimuth angle of the slow axis 13A of the first quarter-wave film 13 was 58.3°, and the azimuth angle of the slow axis 14A of the second quarter-wave film 14 was 13.9°. The azimuth angles of the slow axis 13A of the first quarter-wave film 13 and the slow axis 14A of the second quarter-wave film 14 were set so as to optimize the worst value of S3 emitted from the front surface of the optical element of Example 1.

[0201] The optical element 10 of this example further included a first positive C plate 19X between the first quarter-wave film 13 and the second quarter-wave film 14. The retardation Rth in the thickness direction of the first positive C plate 19X was 108 nm.

[0202] The optical element 10 of this example further included a second positive C plate 19A on the side of the second liquid crystal cell 11B opposite to the first liquid crystal cell 11A, and a third positive C plate 19B on the side of the first liquid crystal cell 11A opposite to the second liquid crystal cell 11B. The retardation Rth in the thickness direction of the second positive C plate 19A was 79 nm. The retardation Rth in the thickness direction of the third positive C plate 19B was 98 nm.

[0203] In this example, in order to achieve a wide viewing angle, three positive C plates are arranged: a first positive C plate 19X, a second positive C plate 19A, and a third positive C plate 19B. Note that although ideal C plates are assumed in the example, these C plates may have retardation Re due to manufacturing variations and the like.

[0204] The first state is driven by applying a voltage to the first liquid crystal layer 500. In the first state, it is preferable to apply as high a voltage as possible to the first liquid crystal layer 500, and in this embodiment, 20 V was applied. Because the negative C plate 12 is designed so that the phase difference between the driven liquid crystal layer (first liquid crystal layer 500) and the negative C plate 12 is canceled, only the undriven liquid crystal layer (second liquid crystal layer 600) is effective. This makes it possible to achieve a wide viewing angle and a wide bandwidth sHWP.

[0205] In the second state, which is the opposite of the first state, a voltage is applied to the second liquid crystal layer 600 to drive it, and a liquid crystal layer (first liquid crystal layer 500) that is rotated 90 degrees from the liquid crystal layer (second liquid crystal layer 600) that was active in the first state becomes active, and the light that has passed through the two quarter-wave films (first quarter-wave film 13 and second quarter-wave film 14) becomes circularly polarized light having a polarization state opposite to that of the light that entered the optical element 10.

[0206] (Evaluation of Example 1) The Stokes parameter S3 of the emitted light was evaluated when right-handed circularly polarized light (S3=+1) and left-handed circularly polarized light (S3=-1) were incident on the optical element (sHWP) of Example 1. The evaluation of the Stokes parameter S3 was performed by optical calculation using an LCD-MASTER 1D manufactured by Shintech Co., Ltd.

[0207] Fig. 30 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Example 1 is not modulated, when the incident angle is set to 30°. Fig. 31 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Example 1 is modulated, when the incident angle is set to 30°. Figs. 30 and 31 show evaluation results at wavelengths of 450 nm, 550 nm, and 650 nm.

[0208] In Example 1, in the case of incident right-handed circularly polarized light (S3=+1) and incident left-handed circularly polarized light (S3=-1) shown in FIGS. 30 and 31 , |S3|≧0.98 was achieved in all directions in the range of 450 nm to 650 nm, both during modulation and non-modulation. That is, the optical element of this example was able to switch between polarization modulation and polarization non-modulation with high efficiency over a wide bandwidth and a wide viewing angle. In this example, the results for incident right-handed circularly polarized light (S3=+1), which produced worse results than incident left-handed circularly polarized light (S3=-1), are shown in FIGS. 30 and 31 .

[0209] In order to study the design of a suitable liquid crystal cell, optical calculations were performed on the optical element 10 of Example 1 using an LCD-MASTER 1D manufactured by Shintech Co., Ltd. Specifically, similar to the above, the Stokes parameter S3 of the emitted light was evaluated when right-handed circularly polarized light (S3=+1) and left-handed circularly polarized light (S3=-1) were incident. In this example, simulations were performed under the following conditions. <Conditions> Wavelength: 450 nm, 550 nm, 650 nm (3 wavelengths) Orientation: Omnidirectional 0° to 360° Polar angle: 30° (fixed) State: modulated, unmodulated (2 states) Incident polarization: right-handed circularly polarized light (S3=+1), left-handed circularly polarized light (S3=-1) (2 states)

[0210] In the following, based on the results obtained by simulation, the range in which 90% or more modulation and non-modulation can be achieved at an incident angle of 30° and a wavelength range of 450 nm to 650 nm was determined to be the preferable range. In this example, simulations were performed for all combinations of the above <conditions>, but for simplicity, only the results for the worst S3 (worst S3) are shown below.

[0211] In the simulation of this example, the modulated and unmodulated states were simulated for each of the two incident polarization states (S3 = +1 and S3 = -1). That is, a total of four states were simulated to obtain the optimal design. Here, the incident polarization state or the output polarization state may be fixed by installing a circular polarizer on the incident side or the output side. In that case, only that polarization state needs to be considered, that is, the optimal design needs to be performed for the two states.

[0212] First, in order to consider a suitable range for the retardation Re of the second quarter-wave film 14, the Stokes parameter S3 relative to the retardation Re of the second quarter-wave film 14 included in the optical element 10 of Example 1 was determined by simulation. Fig. 32 is a graph showing the Stokes parameter (worst S3) relative to the retardation Re of the second quarter-wave film included in the optical element of Example 1. In Fig. 32, the region surrounded by the dashed line is a preferred range in which 90% or more modulation and non-modulation can be achieved, and the region surrounded by the dashed line is a more preferred range in which 95% or more modulation and non-modulation can be achieved.

[0213] From FIG. 32, it can be seen that the retardation Re of the second quarter-wave film 14 at a wavelength of 550 nm is preferably 112 nm or more and 162 nm or less, and more preferably 121 nm or more and 152 nm or less.

[0214] In order to consider a preferred range of the azimuth angle of the slow axis 14A of the second quarter-wave film 14, the Stokes parameter S3 relative to the azimuth angle of the slow axis 14A of the second quarter-wave film 14 included in the optical element 10 of Example 1 was determined by simulation. Fig. 33 is a graph showing the Stokes parameter (worst S3) relative to the azimuth angle of the slow axis of the second quarter-wave film included in the optical element of Example 1. In Fig. 33, the region surrounded by the dashed line is a preferred range in which 90% or more modulation and non-modulation can be achieved, and the region surrounded by the dashed line is a more preferred range in which 95% or more modulation and non-modulation can be achieved.

[0215] From FIG. 33, it is found that the azimuth angle of the slow axis 14A of the second quarter-wave film 14 is preferably 4° or more and 23° or less, and more preferably 8° or more and 19° or less.

[0216] In order to consider a suitable range for the retardation Rth in the thickness direction of the first positive C plate 19X, the Stokes parameter S3 for the retardation Rth in the thickness direction of the first positive C plate 19X included in the optical element 10 of Example 1 was determined by simulation. Fig. 34 is a graph showing the Stokes parameter (worst S3) for the retardation Rth in the thickness direction of the first positive C plate included in the optical element of Example 1. In Fig. 34, the region surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the region surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0217] It is clear from FIG. 34 that the retardation Rth in the thickness direction of the first positive C plate 19X is preferably 0 nm or more and 320 nm or less, and more preferably 0 nm or more and 230 nm or less.

[0218] In order to consider a suitable range for the retardation Re of the first quarter-wave film 13, the Stokes parameter S3 relative to the retardation Re of the first quarter-wave film 13 included in the optical element 10 of Example 1 was determined by simulation. Fig. 35 is a graph showing the Stokes parameter (worst S3) relative to the retardation Re of the first quarter-wave film included in the optical element of Example 1. In Fig. 35, the area surrounded by the dashed line is a preferred range in which 90% or more modulation and non-modulation can be achieved, and the area surrounded by the dashed line is a more preferred range in which 95% or more modulation and non-modulation can be achieved.

[0219] From FIG. 35, it is found that the retardation Re of the first quarter-wave film 13 at a wavelength of 550 nm is preferably 72 nm or more and 210 nm or less, and more preferably 110 nm or more and 175 nm or less.

[0220] In order to consider a preferred range of the azimuth angle of the slow axis 13A of the first quarter-wave film 13, the Stokes parameter S3 relative to the azimuth angle of the slow axis 13A of the first quarter-wave film 13 included in the optical element 10 of Example 1 was determined by simulation. Fig. 36 is a graph showing the Stokes parameter (worst S3) relative to the azimuth angle of the slow axis of the first quarter-wave film included in the optical element of Example 1. In Fig. 36, the region surrounded by the dashed line is a preferred range in which 90% or more modulation and non-modulation can be achieved, and the region surrounded by the dashed line is a more preferred range in which 95% or more modulation and non-modulation can be achieved.

[0221] From FIG. 36, it is found that the azimuth angle of the slow axis 13A of the first quarter-wave film 13 is preferably 52° or more and 66° or less, and more preferably 55° or more and 64° or less.

[0222] In order to consider a suitable range for the retardation Rth in the thickness direction of the second positive C plate 19A, the Stokes parameter S3 for the retardation Rth in the thickness direction of the second positive C plate 19A included in the optical element 10 of Example 1 was determined by simulation. Fig. 37 is a graph showing the Stokes parameter (worst S3) for the retardation Rth in the thickness direction of the second positive C plate included in the optical element of Example 1. In Fig. 37, the region surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the region surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0223] It is clear from FIG. 37 that the retardation Rth in the thickness direction of the second positive C plate 19A is preferably 0 nm or more and 252 nm or less, and more preferably 0 nm or more and 174 nm or less.

[0224] In order to examine the preferred range of the retardation Re of the second liquid crystal layer 600 in the first state at a wavelength of 550 nm, the Stokes parameter S3 for the retardation Re of the second liquid crystal layer 600 included in the optical element 10 of Example 1 in the first state at a wavelength of 550 nm was determined by simulation. Figure 38 is a graph showing the Stokes parameter (worst S3) for the retardation Re of the second liquid crystal layer included in the optical element of Example 1 in the first state at a wavelength of 550 nm. In Figure 38, the region surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the region surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0225] From Figure 38, it can be seen that the retardation Re of the second liquid crystal layer 600 in the first state at a wavelength of 550 nm is preferably 200 nm or more and 280 nm or less, and more preferably 220 nm or more and 264 nm or less.

[0226] In order to consider a suitable range of the twist angle of the second liquid crystal molecules 610 in the first state, the Stokes parameter S3 for the twist angle in the first state of the second liquid crystal molecules 610 in the optical element 10 of Example 1 was determined by simulation. Fig. 39 is a graph showing the Stokes parameter (worst S3) for the twist angle in the first state of the second liquid crystal molecules in the optical element of Example 1. In Fig. 39, the region surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the region surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0227] From Figure 39, it can be seen that the second liquid crystal molecules 610 in the first state are preferably twisted at a twist angle of 57° or more and 76° or less, and more preferably twisted at a twist angle of 62° or more and 73° or less.

[0228] In order to consider a suitable range of the azimuth angle of the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side in the first state, the Stokes parameter S3 for the azimuth angle of the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side in the first state of the optical element 10 of Example 1 was obtained by simulation. Fig. 40 is a graph showing the Stokes parameter (worst S3) for the azimuth angle of the alignment direction of the second liquid crystal molecules on the third substrate side in the first state of the optical element of Example 1. In Fig. 40, the region surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the region surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0229] From Figure 40, it can be seen that the azimuth angle of the alignment direction 611A of the second liquid crystal molecules 611 on the third substrate 300 side in the first state is preferably 79° or more and 98° or less, and more preferably 83° or more and 95° or less.

[0230] In order to consider a suitable range for the retardation Rth in the thickness direction of the negative C plate 12, the Stokes parameter S3 relative to the retardation Rth in the thickness direction of the negative C plate 12 included in the optical element 10 of Example 1 was determined by simulation. Fig. 41 is a graph showing the Stokes parameter (worst S3) relative to the retardation Rth in the thickness direction of the negative C plate included in the optical element of Example 1. In Fig. 41, the region surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the region surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0231] It is clear from FIG. 41 that the retardation Rth in the thickness direction of the negative C plate 12 is preferably −410 nm or more and 0 nm or less, and more preferably −339 nm or more and −115 nm or less.

[0232] In order to consider a suitable range of the retardation Re of the first liquid crystal layer 500 in the second state at a wavelength of 550 nm, the Stokes parameter S3 for the retardation Re of the first liquid crystal layer 500 included in the optical element 10 of Example 1 in the second state at a wavelength of 550 nm was obtained by simulation. Figure 42 is a graph showing the Stokes parameter (worst S3) for the retardation Re of the first liquid crystal layer included in the optical element of Example 1 in the second state at a wavelength of 550 nm. In Figure 42, the area surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the area surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0233] From Figure 42, it can be seen that the retardation Re of the first liquid crystal layer 500 in the second state at a wavelength of 550 nm is preferably 196 nm or more and 280 nm or less, and more preferably 210 nm or more and 265 nm or less.

[0234] In order to consider a suitable range of the azimuth angle of the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side in the second state, the Stokes parameter S3 for the azimuth angle of the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side in the second state of the optical element 10 of Example 1 was obtained by simulation. Fig. 43 is a graph showing the Stokes parameter (worst S3) for the azimuth angle of the alignment direction of the first liquid crystal molecules on the first substrate side in the second state of the optical element of Example 1. In Fig. 43, the region surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the region surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0235] From Figure 43, it can be seen that the azimuth angle of the alignment direction 511A of the first liquid crystal molecules 511 on the first substrate 100 side in the second state is preferably -12° or more and 10° or less, and more preferably -7.5° or more and 7.2° or less.

[0236] In order to consider a suitable range of the twist angle of the first liquid crystal molecules 510 in the second state, the Stokes parameter S3 for the twist angle in the second state of the first liquid crystal molecules 510 in the optical element 10 of Example 1 was determined by simulation. Fig. 44 is a graph showing the Stokes parameter (worst S3) for the twist angle in the second state of the first liquid crystal molecules in the optical element of Example 1. In Fig. 44, the region surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the region surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0237] From Figure 44, it can be seen that the first liquid crystal molecules 510 in the second state are preferably twisted at a twist angle of 58° or more and 78° or less, and more preferably twisted at a twist angle of 62° or more and 75° or less.

[0238] In order to consider a suitable range for the retardation Rth in the thickness direction of the third positive C plate 19B, the Stokes parameter S3 for the retardation Rth in the thickness direction of the third positive C plate 19B included in the optical element 10 of Example 1 was determined by simulation. Fig. 45 is a graph showing the Stokes parameter (worst S3) for the retardation Rth in the thickness direction of the third positive C plate included in the optical element of Example 1. In Fig. 45, the region surrounded by the dashed line is a preferred range in which modulation and non-modulation of 90% or more can be achieved, and the region surrounded by the dashed line is a more preferred range in which modulation and non-modulation of 95% or more can be achieved.

[0239] It is clear from FIG. 45 that the retardation Rth in the thickness direction of the third positive C plate 19B is preferably 0 nm or more and 290 nm or less, and more preferably 0 nm or more and 213 nm or less.

[0240] Comparative Example 1 Fig. 46 is a cross-sectional schematic diagram of an optical element according to Comparative Example 1. A simulation was performed on the optical element 10R1 of Comparative Example 1 shown in Fig. 46 in the same manner as in Example 1 to evaluate the switching performance between polarization modulation and polarization non-modulation. The optical element 10R1 of Comparative Example 1 was an optical element corresponding to the optical element of Comparative Example 1. The optical element 10R1 of Comparative Example 1 included, in order from the incident side to the output side, a quarter-wave film 15R having a slow axis azimuth angle of 75°, a half-wave film 16R having a slow axis azimuth angle of 15°, a liquid crystal cell 11R1 including a TN liquid crystal layer 500R1 twisted by 90°, a half-wave film 17R having a slow axis azimuth angle of -75°, and a quarter-wave film 18R having a slow axis azimuth angle of -15°.

[0241] Comparative Example 2 Fig. 47 is a cross-sectional schematic diagram of an optical element according to Comparative Example 2. A simulation was performed on the optical element 10R2 of Comparative Example 2 shown in Fig. 47 in the same manner as in Example 1, and the performance for switching between polarization modulation and polarization non-modulation was evaluated. The optical element 10R2 of Comparative Example 2 was an optical element corresponding to the optical element of Comparative Example 2 described above. The optical element 10R2 of Comparative Example 2 had a structure in which, from the incident side to the output side, a TN liquid crystal layer 500R2 twisted at 70° and a TN liquid crystal layer 500R3 twisted at -70° were stacked.

[0242] (Evaluation of Comparative Examples 1 and 2) Fig. 48 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Comparative Example 1 is not modulated when the incident angle is set to 30°. Fig. 49 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Comparative Example 1 is modulated when the incident angle is set to 30°. Fig. 50 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Comparative Example 2 is not modulated when the incident angle is set to 30°. Fig. 51 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Comparative Example 2 is modulated when the incident angle is set to 30°. Figs. 48 to 51 show evaluation results at wavelengths of 450 nm, 550 nm, and 650 nm.

[0243] 48 and 49, |S3| ≧ 0.9 could not be achieved in either the modulated or non-modulated state in Comparative Example 1. As shown in Figures 50 and 51, |S3| ≧ 0.9 was generally achieved in Comparative Example 2 in the modulated state, but was not achieved in the non-modulated state.

[0244] Example 2 Figure 52 is a cross-sectional schematic diagram of an optical element according to Example 2. A simulation was performed on the optical element 10 of Example 2 shown in Figure 52 in the same manner as in Example 1 to evaluate the switching performance between polarization modulation and polarization non-modulation. The optical element 10 of Example 2 had the same configuration as Example 1, except that it did not include a first positive C plate 19X, the refractive index anisotropy Δn of the first liquid crystal molecules 510 and the second liquid crystal molecules 610 was 0.066, the thickness direction retardation Rth of the second positive C plate 19A and the third positive C plate 19B was 70 nm, the thickness direction retardation Rth of the negative C plate 12 was -140 nm, the azimuth angle of the slow axis 13A of the first quarter-wave film 13 was 57.2°, and the azimuth angle of the slow axis 14A of the second quarter-wave film 14 was 12.2°. The azimuth angles of the slow axis 13A of the first quarter-wave film 13 and the slow axis 14A of the second quarter-wave film 14 were set so as to optimize the worst value of S3 emitted from the front surface of the optical element of Example 2.

[0245] Fig. 53 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Example 2 is not modulated, when the incident angle is set to 30°. Fig. 54 is a graph showing the relationship between the Stokes parameter S3 and the azimuth angle when the optical element according to Example 2 is modulated, when the incident angle is set to 30°. Figs. 53 and 54 show evaluation results at wavelengths of 450 nm, 550 nm, and 650 nm.

[0246] 53 and 54, Example 2 exhibited S3 characteristics in the range of 450 nm to 650 nm both during modulation and non-modulation, which were superior to those of Comparative Examples 1 and 2. On the other hand, it was found that Example 1 was able to switch between the modulated state and the non-modulated state more efficiently than Example 2.

[0247] Example 3 In Example 3, the first quarter-wave film 13 of Example 1, which had a reverse wavelength dispersion characteristic, was replaced with a quarter-wave film having a flat wavelength dispersion characteristic, and the resulting configuration was examined. A simulation was performed on the optical element of Example 3, in which the first quarter-wave film 13 had a flat wavelength dispersion characteristic, and optimal values ​​for the azimuth angle of the slow axis 13A of the first quarter-wave film 13 and the azimuth angle of the slow axis 14A of the second quarter-wave film 14 were determined so as to optimize the worst value of S3 emitted from the front surface of the optical element of Example 3. The results are shown in Table 2 below, along with those of Examples 1 and 2.

[0248]

[0249] The results of Example 3 in the table above show that when both the first quarter-wave film 13 and the second quarter-wave film 14 have flat wavelength dispersion characteristics, it is preferable to set the azimuth angle of the slow axis 13A of the first quarter-wave film 13 to 57.9° and the azimuth angle of the slow axis 14A of the second quarter-wave film 14 to 14.3°. As with Example 1, the optical element of this example can switch between polarization modulation and polarization non-modulation with high efficiency over a wide bandwidth and a wide viewing angle.

[0250] 1: Head-mounted display 1P: Display panel 10, 10R1, 10R2: Optical elements 11A, 11B, 11R1: Liquid crystal cell 12: Negative C-plate 13, 14, 15R, 18R: 1 / 4 wavelength film 13A, 14A: Slow axis 16R, 17R: 1 / 2 wavelength film 19A, 19B, 19X: Positive C-plate 20, 20A1, 20A2, 20A3: Pancharatnam Berry (PB) lens 30, 30A, 30B: Variable focus element 40: Retardation plate 41, 42, 43, 44: Alignment film 100, 200, 300, 400: Substrate 110, 210, 310, 410: Support substrate 120, 220, 320, 420: Solid electrode 500, 600: Liquid crystal layer 500R1, 500R2, 500R3: TN liquid crystal layer 510, 511, 512, 610, 611, 612, 710: Liquid crystal molecules 511A, 512A, 611A, 612A: Alignment direction 700: Optically anisotropic layer LC0, LC1, LC2: Left-handed circularly polarized light R0, R1, R2: Region U: User

Claims

1. A liquid crystal display device comprising, in this order, a first substrate, a first liquid crystal layer containing first liquid crystal molecules, a second substrate, a third substrate, a second liquid crystal layer containing second liquid crystal molecules, and a fourth substrate, wherein the first substrate, the first liquid crystal layer, and the second substrate constitute a first liquid crystal cell, and the third substrate, the second liquid crystal layer, and the fourth substrate constitute a second liquid crystal cell, wherein the first liquid crystal cell has, on at least one of the first substrate and the second substrate, a first electrode for applying a voltage to the first liquid crystal layer, and the second liquid crystal cell has, on at least one of the third substrate and the fourth substrate, a second electrode for applying a voltage to the second liquid crystal layer, and the first electrode and the second electrode are arranged to be switchable between a first state in which the second liquid crystal molecules are twistedly aligned and the first liquid crystal molecules are vertically aligned, and a second state in which the first liquid crystal molecules are twistedly aligned and the second liquid crystal molecules are vertically aligned, an azimuth angle of the alignment direction of the second liquid crystal molecules on the third substrate side in the first state and an azimuth angle of the alignment direction of the second liquid crystal molecules on the fourth substrate side in the first state are angles obtained by rotating the azimuth angle of the alignment direction of the first liquid crystal molecules on the first substrate side in the second state and the azimuth angle of the alignment direction of the first liquid crystal molecules on the second substrate side in the second state by ¼ in the same direction, respectively; and further comprising a first ¼ wavelength film and a second ¼ wavelength film arranged on the opposite side of the first liquid crystal cell to the second liquid crystal cell or the opposite side of the second liquid crystal cell to the first liquid crystal cell, and the first ¼ wavelength film is arranged between the second ¼ wavelength film and the first liquid crystal cell and the second liquid crystal cell.

2. The optical element according to claim 1, wherein the retardation Re of the first quarter-wave film at a wavelength of 550 nm is 72 nm or more and 210 nm or less.

3. The optical element according to claim 1, wherein the azimuth angle of the slow axis of the first quarter-wave film is 52° or more and 66° or less.

4. The optical element according to claim 1, wherein the retardation Re of the second quarter-wave film at a wavelength of 550 nm is 112 nm or more and 162 nm or less.

5. The optical element according to claim 1, wherein the azimuth angle of the slow axis of said second quarter-wave film is 4° or more and 23° or less.

6. The optical element according to claim 1, wherein at least one of said first quarter-wave film and said second quarter-wave film has a reverse wavelength dispersion characteristic.

7. The optical element according to claim 1, wherein at least one of said first quarter-wave film and said second quarter-wave film has a flat wavelength dispersion characteristic.

8. The optical element according to claim 1, wherein the retardation Re of said first liquid crystal layer in said second state at a wavelength of 550 nm is 196 nm or more and 280 nm or less.

9. The optical element according to claim 1, wherein the retardation Re of said second liquid crystal layer in said first state at a wavelength of 550 nm is not less than 200 nm and not more than 280 nm.

10. The optical element according to claim 1, wherein the first liquid crystal molecules in the second state are twisted and aligned with a twist angle of 58° or more and 78° or less.

11. The optical element according to claim 1, wherein the second liquid crystal molecules in the first state are twisted at a twist angle of 57° or more and 76° or less.

12. The optical element according to claim 1, wherein the azimuth angle of the alignment direction of the first liquid crystal molecules on the first substrate side in the second state is not less than −12° and not more than 10°.

13. The optical element according to claim 1, wherein the azimuth angle of the alignment direction of the second liquid crystal molecules on the third substrate side in the first state is 79° or more and 98° or less.

14. The optical element of claim 1, further comprising: a first positive C plate disposed between the first quarter-wave film and the second quarter-wave film; a second positive C plate disposed on the side of the second liquid crystal cell opposite the first liquid crystal cell; and a third positive C plate disposed on the side of the first liquid crystal cell opposite the second liquid crystal cell.

15. The optical element according to claim 14, wherein the retardation Rth in the thickness direction of the first positive C plate is 0 nm or more and 320 nm or less.

16. The optical element according to claim 14, wherein the retardation Rth in the thickness direction of the second positive C plate is 0 nm or more and 252 nm or less.

17. The optical element according to claim 14, wherein the retardation Rth in the thickness direction of the third positive C plate is 0 nm or more and 290 nm or less.

18. The optical element according to claim 1, further comprising a negative C plate between the first liquid crystal cell and the second liquid crystal cell.

19. The optical element according to claim 18, wherein the retardation Rth in the thickness direction of the negative C plate is −410 nm or more and 0 nm or less.

20. A variable focus element comprising an optical element according to any one of claims 1 to 19 and a Pancharatnam Berry lens.

21. The variable focus element of claim 20, wherein the Pancharatnam Berry lens is disposed within the optical element.

22. A head mounted display comprising the variable focus element according to claim 20.

Citation Information

Patent Citations

  • Layered liquid crystal structure

    JP2022547645A

  • Liquid crystal cells for polarization rotation

    US20180335630A1

  • Transmissive liquid crystal diffractive element

    WO2021235416A1