Cylindrical secondary battery

The cylindrical secondary battery design addresses peeling issues by ensuring the tacking strength of the first positive electrode mixture layer is greater than the second, and the peel strength is higher, effectively preventing peeling and maintaining capacity through strategic layer alignment and heat treatment.

WO2024225021A1PCT designated stage expired Publication Date: 2024-10-31PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/014368
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2024-04-09
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Cylindrical secondary batteries face peeling issues of the positive electrode mixture layer due to repeated charging and discharging cycles, particularly when the exposed portion is not formed over the entire width, leading to stress concentration and peeling from sides parallel to the protective member.

Method used

The battery design includes a positive electrode exposed portion contacting only one end of the positive electrode, with a first positive electrode mixture layer aligned in the longitudinal direction and a second layer in the width direction, where the tacking strength of the first layer is greater than the second, ensuring T1>T2, and the peel strength P1>P2, to prevent peeling and maintain capacity.

Benefits of technology

This configuration effectively suppresses peeling of the positive electrode mixture layer and maintains battery capacity by distributing stress and improving adhesion, as demonstrated through specific tacking and peel strength ratios and heat treatment adjustments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024014368_31102024_PF_FP_ABST
    Figure JP2024014368_31102024_PF_FP_ABST
Patent Text Reader

Abstract

Provided is a cylindrical secondary battery in which peeling of a positive electrode mixture layer and a reduction in battery capacity due to repeated charging and discharging are suppressed. In this cylindrical secondary battery, a positive electrode has a positive electrode current collector and a positive electrode mixture layer disposed on the surface of the positive electrode current collector. A positive electrode exposed part in which the positive electrode current collector is exposed is disposed on the surface of the positive electrode, and the positive electrode exposed part is in contact with only one end among both ends in the width direction of the positive electrode. A positive electrode tab is connected to the positive electrode exposed part and is led out from one end. A protective member covers the positive electrode exposed part, the tab, and a portion, of the positive electrode mixture layer, adjacent to the positive electrode exposed part. When the positive electrode mixture layer is divided into a first positive electrode mixture layer aligned with the positive electrode exposed part in the longitudinal direction of the positive electrode, and a second positive electrode mixture layer adjacent to the positive electrode exposed part and the first positive electrode mixture layer in the width direction of the positive electrode, the tacking strength T1 of the first positive electrode mixture layer and the tacking strength T2 of the second positive electrode mixture layer satisfy the relationship T1>T2.
Need to check novelty before this filing date? Find Prior Art

Description

Cylindrical secondary battery

[0001] The present disclosure relates to a cylindrical secondary battery.

[0002] A cylindrical secondary battery is a battery in which an electrode assembly, in which a positive electrode and a negative electrode are wound with a separator interposed therebetween, is housed in a cylindrical outer can. The positive electrode and the negative electrode each have a current collector and a mixture layer disposed on the surface of the current collector. The mixture layer contains an active material capable of reversibly absorbing and releasing Li ions. An exposed portion of the current collector is formed on the surface of the electrode, and a tab is connected to the exposed portion for connecting the electrode to a battery terminal. Patent Document 1 discloses a technique for forming multiple exposed portions on an electrode and connecting a tab to each of the exposed portions in order to suppress heat generation at the tab connection portion and improve current collection performance. The electrode disclosed in Patent Document 1 has an exposed portion formed across the entire width. A commonly known technique involves covering the exposed portions and their surroundings with a protective member, such as insulating tape, to ensure battery safety even if the separator is damaged.

[0003] Japanese Patent Application Publication No. 10-261439

[0004] Recently, batteries have been required to have ever higher capacities. From the viewpoint of achieving higher capacity, it is preferable that the area of ​​the exposed portion where the mixture layer is not formed is small. The inventors of the present invention have formed the positive electrode exposed portion only near the portion where the tab is connected, rather than forming the positive electrode exposed portion over the entire width of the positive electrode. After further intensive research, the inventors have found that repeated charge and discharge cycles can cause peeling of the positive electrode mixture layer, starting from the side parallel to the width of the protective member. The technology disclosed in Patent Document 1 does not anticipate the case where the positive electrode exposed portion is formed only at one end, and therefore does not consider peeling of the positive electrode mixture layer after charge and discharge cycles, leaving room for improvement.

[0005] An object of the present disclosure is to provide a cylindrical secondary battery that has a high capacity and is capable of suppressing peeling of the positive electrode mixture layer due to repeated charge and discharge.

[0006] A cylindrical secondary battery according to one aspect of the present disclosure includes an electrode assembly in which a positive electrode and a negative electrode are wound with a separator interposed therebetween, a non-aqueous electrolyte, and a cylindrical outer can that houses the electrode assembly and the non-aqueous electrolyte. The positive electrode has a positive electrode current collector and a positive electrode mixture layer disposed on the surface of the positive electrode current collector. A positive electrode exposed portion, where the positive electrode current collector is exposed, is disposed on the surface of the positive electrode. The positive electrode exposed portion is in contact with only one of both widthwise ends of the positive electrode. A positive electrode tab is connected to the positive electrode exposed portion. and is led out from one end, the protective member covers the positive electrode exposed portion, the tab, and a portion of the positive electrode mixture layer adjacent to the positive electrode exposed portion, and when the positive electrode mixture layer is divided into a first positive electrode mixture layer aligned with the positive electrode exposed portion in the longitudinal direction of the positive electrode and a second positive electrode mixture layer adjacent to the positive electrode exposed portion and the first positive electrode mixture layer in the width direction of the positive electrode, a tacking strength T1 of the first positive electrode mixture layer and a tacking strength T2 of the second positive electrode mixture layer satisfy the relationship T1 > T2.

[0007] According to the cylindrical secondary battery according to the present disclosure, peeling of the positive electrode mixture layer after charge / discharge cycles can be suppressed.

[0008] 1 is a longitudinal cross-sectional view of a cylindrical secondary battery according to an embodiment of the present invention; FIG. 2 is a front view showing a positive electrode and a negative electrode constituting an electrode body of the cylindrical secondary battery of FIG.

[0009] From the viewpoint of achieving high capacity, it is preferable that the area of ​​the positive electrode exposed portion for connecting the positive electrode tab be as small as possible. Therefore, a possible embodiment is one in which the positive electrode exposed portion is not formed over the entire width of the positive electrode, but is formed only near the portion where the positive electrode tab is connected. Furthermore, from the viewpoint of improving battery reliability, the positive electrode exposed portion and its surroundings are covered with a protective member such as insulating tape. However, it has been found that when a positive electrode having such an embodiment is used, peeling of the positive electrode mixture layer is likely to occur starting from the side of the protective member parallel to the width direction during charge / discharge cycles. It is believed that when the electrode body expands and contracts in the longitudinal direction due to charge / discharge, stress concentrates on a portion of the side of the protective member parallel to the width direction, causing the positive electrode mixture layer to peel. After extensive research, the inventors discovered that peeling of the positive electrode mixture layer and a decrease in battery capacity can be suppressed by setting the tacking strength T1 of the first positive electrode mixture layer aligned with the positive electrode exposed portion in the longitudinal direction of the positive electrode greater than the tacking strength T2 of the second positive electrode mixture layer adjacent to the positive electrode exposed portion and the first positive electrode mixture layer in the width direction of the positive electrode.

[0010] An example of an embodiment of a cylindrical secondary battery according to the present disclosure will be described in detail below with reference to FIGS. 1 and 2. In the following description, specific shapes, materials, numerical values, directions, etc. are merely examples for facilitating understanding of the present invention and can be appropriately changed according to the specifications of the cylindrical secondary battery. Furthermore, when multiple embodiments and variations are included in the following description, it is assumed from the outset that their characteristic features will be appropriately combined and used. Furthermore, when the term "approximately" is used in this specification, it is used in the same sense as the term "roughly," and the requirement of "approximately" is met if the two or more embodiments are substantially the same.

[0011] Fig. 1 is a longitudinal cross-sectional view of a cylindrical secondary battery 10 (hereinafter referred to as secondary battery 10) according to an embodiment. In the secondary battery 10 shown in Fig. 1, an electrode assembly 14 and a non-aqueous electrolyte (not shown) are housed in an outer can 15. For ease of explanation, the following description will be given with the sealing body 16 side referred to as "top" and the bottom side of the outer can 15 referred to as "bottom."

[0012] The electrode assembly 14 has a wound structure in which the positive electrode 11 and the negative electrode 12 are wound with a separator 13 interposed therebetween. The positive electrode 11, the negative electrode 12, and the separator 13 are all long strips, and are spirally wound so as to be alternately stacked in the radial direction of the electrode assembly 14. The separator 13 is formed to be slightly larger than the positive electrode 11 and the negative electrode 12, and two separators 13 are arranged to sandwich the positive electrode 11.

[0013] The separator 13 may be, for example, a porous sheet having ion permeability and insulating properties. Specific examples of porous sheets include a microporous thin film, a woven fabric, and a nonwoven fabric. Suitable materials for the separator include olefin-based resins such as polyethylene and polypropylene, and cellulose. The separator 13 may be a laminate having a cellulose fiber layer and a thermoplastic resin fiber layer such as an olefin-based resin. Alternatively, the separator 13 may be a multilayer separator including a polyethylene layer and a polypropylene layer, and the surface of the separator 13 may be coated with a material such as an aramid-based resin or ceramic.

[0014] The non-aqueous electrolyte has lithium ion conductivity and may be a liquid electrolyte (electrolytic solution) or a solid electrolyte.

[0015] The liquid electrolyte (electrolytic solution) contains a non-aqueous solvent and an electrolyte salt dissolved in the non-aqueous solvent. Examples of the non-aqueous solvent include esters, ethers, nitriles, amides, and mixed solvents of two or more of these. Examples of the non-aqueous solvent include ethylene carbonate (EC), ethyl methyl carbonate (EMC), dimethyl carbonate (DMC), diethyl carbonate (DEC), and mixed solvents of these. The non-aqueous solvent may contain a halogen-substituted compound (e.g., fluoroethylene carbonate) in which at least a portion of the hydrogen atoms of these solvents are substituted with halogen atoms such as fluorine. Examples of the electrolyte salt include LiPF 6 Lithium salts such as

[0016] As the solid electrolyte, for example, a solid or gel-like polymer electrolyte, an inorganic solid electrolyte, etc. can be used. As the inorganic solid electrolyte, a material known in all-solid-state lithium ion secondary batteries, etc. (for example, an oxide-based solid electrolyte, a sulfide-based solid electrolyte, a halogen-based solid electrolyte, etc.) can be used. The polymer electrolyte includes, for example, a lithium salt and a matrix polymer, or a non-aqueous solvent, a lithium salt, and a matrix polymer. As the matrix polymer, for example, a polymer material that absorbs the non-aqueous solvent and gels is used. As the polymer material, for example, a fluororesin, an acrylic resin, a polyether resin, etc. can be used.

[0017] The sealing body 16 seals the opening at the top end of the outer can 15, sealing the interior of the secondary battery 10. Insulating plates 17 and 18 are provided above and below the electrode assembly 14. The positive electrode tab 19 extends vertically through a through-hole in the insulating plate 17 and connects the filter 22, which is the bottom plate of the sealing body 16, to the positive electrode 11 included in the electrode assembly 14. This connects the positive electrode 11 to the sealing body 16, and in the secondary battery 10, the cap 26, which is the top plate of the sealing body 16 electrically connected to the filter 22, serves as the positive electrode terminal. The positive electrode tab 19 is, for example, an aluminum tab. On the other hand, the negative electrode tab 20 extends through a through-hole in the insulating plate 18 to the bottom side of the outer can 15 and is welded to the inner bottom surface of the outer can 15. This connects the negative electrode 12 to the outer can 15, and in the secondary battery 10, the outer can 15 serves as the negative electrode terminal. The negative electrode tab 20 is, for example, a nickel tab.

[0018] In the example shown in FIG. 1 , four positive electrode tabs 19 are welded to the electrode assembly 14 in the cross-sectional view. The number of positive electrode tabs 19 extending from the electrode assembly 14 is not particularly limited. Using multiple positive electrode tabs 19 improves the current collection ability of the positive electrode 11, thereby improving the output characteristics of the secondary battery 10. The greater the number of positive electrode tabs 19, the better the current collection ability of the positive electrode 11, but the higher the cost of the secondary battery 10. From the perspective of achieving both the above-mentioned effect and cost, the number of positive electrode tabs 19 is preferably 1 to 20, more preferably 1 to 10, and particularly preferably 3 to 8. The three or more positive electrode tabs 19 extending from the electrode assembly 14 may be connected directly to the sealing member 16 or may be connected to the sealing member 16 via a known current collecting member.

[0019] 1 , the negative electrode tab 20 is led out from near the inner end of the negative electrode 12 and connected to the outer can 15. The position of the negative electrode tab 20 is not limited to the example shown in FIG. 1 , and the negative electrode tab 20 may be provided only near the outer end of the negative electrode 12, or may be provided near both the inner end and the outer end of the negative electrode 12. Alternatively, a negative electrode exposed portion 44 may be formed at the outer end of the negative electrode 12 and brought into contact with the inner circumferential surface of the outer can 15, thereby electrically connecting the vicinity of the outer end of the negative electrode 12 to the outer can 15 without using the negative electrode tab 20.

[0020] The outer can 15 is a cylindrical metal container with a bottom and an opening on one axial side. A gasket 27 is provided between the outer can 15 and the sealing body 16 to ensure the sealing of the interior of the secondary battery 10. The outer can 15 has a groove 21 that supports the sealing body 16 and is formed, for example, by pressing the side surface from the outside. The groove 21 is preferably formed in an annular shape along the circumferential direction of the outer can 15, and supports the sealing body 16 on its upper surface.

[0021] The sealing body 16 includes a filter 22, a lower valve body 23, an insulating member 24, an upper valve body 25, and a cap 26, which are stacked in this order from the electrode body 14 side. Each component of the sealing body 16 has, for example, a disk or ring shape, and all components except for the insulating member 24 are electrically connected to each other. The lower valve body 23 and the upper valve body 25 are connected to each other at their respective centers, with the insulating member 24 interposed between their respective peripheral edges. If the internal pressure of the battery increases due to abnormal heat generation, for example, the lower valve body 23 may rupture, causing the upper valve body 25 to bulge toward the cap 26 and separate from the lower valve body 25, thereby cutting off the electrical connection between them. If the internal pressure continues to increase, the upper valve body 25 may rupture, allowing gas to be released from the opening 26a of the cap 26.

[0022] Next, the positive electrode 11 and the negative electrode 12 will be described with reference to Fig. 2. Fig. 2 is a front view showing the positive electrode 11 and the negative electrode 12 constituting the electrode body 14 provided in the secondary battery 10 of Fig. 1 in a developed state. As shown in Fig. 2, the negative electrode 12 is generally formed to have dimensions slightly larger than the positive electrode 11 in order to prevent lithium precipitation. That is, the negative electrode 12 is formed to be longer than the positive electrode 11 in the longitudinal and width directions.

[0023] The positive electrode 11 has a positive electrode current collector 30 and a positive electrode mixture layer 32 disposed on the surface of the positive electrode current collector 30. A positive electrode exposed portion 34, where the positive electrode current collector 30 is exposed, is disposed on the surface of the positive electrode 11, and the positive electrode exposed portion 34 contacts only one end 11a of both widthwise ends of the positive electrode 11. In other words, the positive electrode exposed portion 34 does not extend to the other widthwise end 11b of the positive electrode 11. As a result, the positive electrode mixture layer 32 is present between the positive electrode exposed portions 34, which increases the area of ​​the positive electrode mixture layer 32 and improves the battery capacity of the secondary battery 10.

[0024] A plurality of positive electrode exposed portions 34 are preferably arranged on the surface of the positive electrode 11. Since one of the positive electrode tabs 19 is connected to each of the positive electrode exposed portions 34, the current collection ability of the positive electrode 11 is improved, and the output characteristics of the secondary battery 10 are improved. Furthermore, the effect of the technology disclosed in the present application, which will be described later, becomes more pronounced as the number of positive electrode exposed portions 34 increases. The number of positive electrode exposed portions 34 is preferably 1 to 20, more preferably 1 to 10, and particularly preferably 3 to 8.

[0025] The positive electrode exposed portion 34, the positive electrode tab 19, and a portion of the positive electrode mixture layer 32 adjacent to the positive electrode exposed portion 34 are covered with the protective member 36. In other words, the protective member 36 covers the positive electrode tab 19, the positive electrode exposed portion 34, and part of the positive electrode mixture layer 32. The protective member 36 is an insulating member that prevents an internal short circuit between the positive electrode tab 19 and the positive electrode exposed portion 34 and the opposing negative electrode mixture layer when the separator 13 is torn.

[0026] The protective member 36 is, for example, an adhesive tape having a substrate and an adhesive portion formed on one surface of the substrate. A heat-resistant layer containing inorganic particles such as metal oxide can be provided between the substrate and the adhesive portion. The substrate can be made of any insulating resin, such as PPS (polyphenylene sulfide), PEEK (polyether ether ketone), PI (polyimide), PP (polypropylene), PET (polyethylene terephthalate), or PBT (polybutylene terephthalate). The thickness of the substrate is, for example, 5 μm or more and 50 μm or less.

[0027] The adhesive portion is a portion for adhering the protective member 36 to the surface of the positive electrode 11. The thickness of the adhesive portion is, for example, 1 μm or more and 30 μm or less. The adhesive portion may contain at least one of a rubber-based polymer and an acrylic-based polymer. The rubber-based polymer and the acrylic-based polymer have adhesive properties, and therefore can adhere the protective member 36 to the surface of the positive electrode 11. The adhesive portion may further contain, for example, a silicone-based polymer.

[0028] A foil of a metal such as aluminum that is stable in the potential range of the positive electrode, a film having such a metal disposed on the surface layer, or the like can be used for the positive electrode current collector 30. The thickness of the positive electrode current collector 30 is, for example, 10 μm or more and 30 μm or less.

[0029] The positive electrode mixture layer 32 is preferably formed on both sides of the positive electrode current collector 30. The thickness of the positive electrode mixture layer 32 is, for example, 10 μm or more and 150 μm or less on one side of the positive electrode current collector 30. The positive electrode mixture layer 32 includes, for example, a positive electrode active material, a conductive agent, and a binder. The positive electrode can be produced, for example, by applying a positive electrode mixture slurry including a positive electrode active material, a conductive agent, a binder, etc. to both sides of the positive electrode current collector 30, drying the coating, and then rolling the coating using a roller or the like.

[0030] The positive electrode active material contained in the positive electrode mixture layer 32 can be, for example, a lithium transition metal composite oxide containing a transition metal element such as Co, Mn, or Ni. x CoO 2 , Li x NiO 2 , Li x MnO 2 , Li x Co y Ni 1-y O 2 , Li x Co y M 1-y O z , Li x Ni 1-y M y O z , Li x Mn 2 O 4 , Li x Mn 2-y M y O 4 , LiMPO 4 , Li 2 MPO 4 F (M is at least one of Na, Mg, Sc, Y, Mn, Fe, Co, Ni, Cu, Zn, Al, Cr, Pb, Sb, and B, and 0<x≦1.2, 0<y≦0.9, and 2.0≦z≦2.3). These may be used alone or in combination.

[0031] The positive electrode active material preferably contains a lithium nickel composite oxide, since this can increase the capacity of the secondary battery 10. The lithium nickel composite oxide is preferably Li x NiO 2 , Li x Coy Ni 1-y O 2 , Li x Ni 1-y M y O z (M is at least one of Na, Mg, Sc, Y, Mn, Fe, Co, Ni, Cu, Zn, Al, Cr, Pb, Sb, and B; 0<x≦1.2, 0<y≦0.9, 2.0≦z≦2.3) The higher the Ni content of the lithium nickel composite oxide, the higher the capacity.

[0032] Examples of the conductive agent contained in the positive electrode mixture layer 32 include carbon-based particles such as carbon black (CB), acetylene black (AB), ketjen black, carbon nanotubes (CNT), graphene, and graphite. These may be used alone or in combination of two or more.

[0033] Examples of the binder contained in the positive electrode mixture layer 32 include fluorine-based resins such as polytetrafluoroethylene (PTFE) and polyvinylidene fluoride (PVDF), polyacrylonitrile (PAN), polyimide-based resins, acrylic-based resins, polyolefin-based resins, etc. These may be used alone or in combination of two or more.

[0034] The positive electrode mixture layer 32 can be divided into a first positive electrode mixture layer 38 aligned with the positive electrode exposed portion 34 in the longitudinal direction of the positive electrode 11, and a second positive electrode mixture layer 39 adjacent to the positive electrode exposed portion 34 and the first positive electrode mixture layer 38 in the width direction of the positive electrode 11. The length t1 in the width direction of the first positive electrode mixture layer 38 and the length t2 in the width direction of the second positive electrode mixture layer 39 preferably satisfy the relationship 1 / 10≦t1 / t2≦1, and more preferably satisfy the relationship 1 / 8≦t1 / t2≦1 / 2.

[0035] The tacking strength T1 of the first positive electrode mixture layer 38 and the tacking strength T2 of the second positive electrode mixture layer 39 satisfy the relationship T1 > T2. This makes it possible to suppress peeling of the positive electrode mixture layer 32 and a decrease in battery capacity. Because peeling of the first positive electrode mixture layer 38 is likely to occur starting from the side 36a parallel to the width direction of the protective member 36 due to charge / discharge cycles, it is preferable that the first positive electrode mixture layer 38 have a relatively high tacking strength. On the other hand, because peeling of the second positive electrode mixture layer 39 is less likely to occur than that of the first positive electrode mixture layer 38, it is preferable that the second positive electrode mixture layer 39 have a lower tacking strength than the first positive electrode mixture layer 38 from the viewpoint of improving battery capacity.

[0036] T1 and T2 preferably satisfy the relationship 1.03≦T1 / T2≦1.68, and more preferably 1.10≦T1 / T2≦1.42. T1 is preferably 320 N or more and 520 N or less, and more preferably 340 N or more and 440 N or less. T2 is, for example, 250 N or more and 400 N or less.

[0037] The tacking strength of the first positive electrode mixture layer 38 and the second positive electrode mixture layer 39 can be measured using a commercially available tacking tester (e.g., a TAC-II manufactured by Rhesca Corporation). Specific measurement conditions are as follows. [Test Sample] The first positive electrode mixture layer 38 and the second positive electrode mixture layer 39 are each cut to a predetermined size from the positive electrode 11 to prepare a test sample. If the positive electrode 11 is incorporated into a battery, the battery is disassembled to remove the positive electrode 11, and the positive electrode 11 is vacuum-dried for one hour and then cut to prepare a test sample. [Measurement Conditions] Nitto Denko double-sided tape #515 is attached to the tip of a metal rod with an adhesive area of ​​2 mmφ. The test sample is pressed with a preload of 400 gf for 10 seconds, and then peeled off at a speed of 600 mm / min. The stress required for peeling is measured. Measurements are performed on five samples of each of the first positive electrode mixture layer 38 and the second positive electrode mixture layer 39, and the average of the measured values ​​is taken as the tacking strength (N).

[0038] The tacking strength of the positive electrode mixture layer 32 can be adjusted, for example, by subjecting the positive electrode mixture layer 32 to a heat treatment. More specifically, by subjecting only the first positive electrode mixture layer 38 to a heat treatment and not subjecting the second positive electrode mixture layer 39 to a heat treatment, T1, T2, and T1 / T2 can be adjusted to fall within the above ranges. Increasing the heat treatment temperature increases the tacking strength. Furthermore, extending the heat treatment time also increases the tacking strength. The heat treatment temperature can be, for example, 100°C or higher and 250°C or lower. The heat treatment time can be, for example, 3 seconds or higher and 60 seconds or lower.

[0039] The heat treatment of the positive electrode mixture layer 32 can be performed, for example, by bringing a high-temperature roller into contact with only the first positive electrode mixture layer 38. For example, the heat treatment temperature and heat treatment time can be adjusted by adjusting the temperature and rotation speed of the roller. Although the heat treatment increases the tacking strength as described above, it may decrease the battery capacity. This is thought to be because, among the components contained in the positive electrode mixture layer 32, the binder in particular forms a film on the surface of the active material.

[0040] The peel strength P1 of the first positive electrode mixture layer and the peel strength P2 of the second positive electrode mixture layer preferably satisfy the relationship P1 > P2. It is more preferable that P1 and P2 satisfy the relationship 1.13 ≦ P1 / P2 ≦ 1.63, and particularly preferable that they satisfy the relationship 1.19 ≦ P1 / P2 ≦ 1.38. P1 is preferably 9 N / m or more and 13 N / m or less, more preferably 9.5 N / m or more and 11 N / m or less. P2 is, for example, 6 N / m or more and 10 N / m or less.

[0041] The peel strength of the first positive electrode mixture layer 38 and the second positive electrode mixture layer 39 can be measured, for example, as follows. [Test Sample] The first positive electrode mixture layer 38 and the second positive electrode mixture layer 39 are each cut to a predetermined size from the positive electrode 11 to prepare a test sample. If the positive electrode 11 is incorporated into a battery, the battery is disassembled, the positive electrode 11 is removed, and the cathode 11 is vacuum-dried for one hour before being cut to prepare a test sample. [Measurement Conditions] Nitto Denko double-sided tape #515 is attached to the positive electrode mixture layer 32 on one side of the test piece and fixed to a stainless steel substrate with a smooth surface. The stainless steel substrate with the test sample fixed is placed horizontally. One end of the positive electrode current collector 30 in the longitudinal direction of the test sample is fixed to a movable jig of a tensile tester (e.g., a Tensilon universal testing machine RTC1210 manufactured by A&D Corporation), and the test sample is set so that the positive electrode current collector 30 is peeled in a direction 90° relative to the substrate surface of the stainless steel substrate. The movable jig is then moved to peel the positive electrode mixture layer 32 of the test piece from the positive electrode current collector 30 at a rate of 20 mm / min. The tensile direction is always maintained at 90° relative to the substrate surface of the stainless steel substrate to which the test piece is fixed. A stable tensile strength value is read when 30 mm or more of the test sample has been peeled off. Five samples of each of the first positive electrode mixture layer 38 and the second positive electrode mixture layer 39 are measured, and the average of the measured values ​​is taken as the peel strength (N / m).

[0042] The negative electrode 12 has a negative electrode current collector 40 and a negative electrode mixture layer 42 disposed on the surface of the negative electrode current collector 40. The negative electrode 12 has a negative electrode exposed portion 44 where the negative electrode current collector 40 is exposed, for example, at an end portion within the winding in the longitudinal direction, and a negative electrode tab 20 is connected to the negative electrode exposed portion 44.

[0043] The negative electrode current collector can be a foil of a metal such as copper that is stable in the potential range of the negative electrode, a film having such a metal disposed on the surface layer, etc. The thickness of the negative electrode current collector is, for example, 5 μm or more and 30 μm or less.

[0044] The negative electrode mixture layer is preferably formed on both sides of the negative electrode current collector. The thickness of the negative electrode mixture layer is, for example, 10 μm or more and 150 μm or less on one side of the negative electrode current collector. The negative electrode mixture layer contains, for example, a negative electrode active material and a binder. The negative electrode can be produced, for example, by applying a negative electrode mixture slurry containing a negative electrode active material, a binder, etc. to both sides of the negative electrode current collector, drying the coating, and then rolling the coating using a roller or the like.

[0045] The negative electrode active material contained in the negative electrode mixture layer is not particularly limited as long as it can reversibly absorb and release lithium ions, and generally, a carbon material such as graphite is used. The graphite may be any of natural graphite such as flake graphite, lump graphite, and amorphous graphite, and artificial graphite such as lump artificial graphite and graphitized mesophase carbon microbeads.

[0046] As the negative electrode active material, metals that can be alloyed with Li, such as Si and Sn, metal compounds containing Si, Sn, etc., and lithium-titanium composite oxides may be used. For example, SiO x Si-containing compounds represented by (0.5≦x≦1.6), Li 2y SiO (2+y) A Si-containing compound in which fine particles of Si are dispersed in a lithium silicate phase represented by (0<y<2), or a Si-containing compound in which Si is dispersed in a carbon material, may be used in combination with graphite.

[0047] Examples of binders contained in the negative electrode mixture layer include styrene butadiene rubber (SBR), nitrile butadiene rubber (NBR), carboxymethyl cellulose (CMC) or a salt thereof, polyacrylic acid (PAA) or a salt thereof (PAA-Na, PAA-K, etc., or a partially neutralized salt), polyvinyl alcohol (PVA), etc. These may be used alone or in combination of two or more.

[0048] The present disclosure will be further described below with reference to examples, but the present disclosure is not limited to these examples.

[0049] Example 1-1 [Preparation of Positive Electrode] As the positive electrode active material, LiNi 0.88 Co 0.09 Al 0.03 O2 Aluminum-containing lithium nickel cobalt oxide represented by the formula (I) was used. 100 parts by mass of the positive electrode active material, 1 part by mass of acetylene black (AB), and 1 part by mass of polyvinylidene fluoride (PVDF) were mixed, and an appropriate amount of N-methyl-2-pyrrolidone (NMP) was added to prepare a positive electrode mixture slurry. Next, the positive electrode mixture slurry was applied to both sides of a strip-shaped positive electrode current collector made of aluminum foil with a thickness of 15 μm, so that eight positive electrode exposed portions were formed. As shown in the example in FIG. 2, the positive electrode exposed portions were arranged to contact only one end of the positive electrode in the width direction. The ratio t1 / t2 calculated from the widthwise length t1 of the first positive electrode mixture layer and the widthwise length t2 of the second positive electrode mixture layer was 1 / 5.

[0050] After drying and rolling the coating, the area corresponding to the first positive electrode mixture layer was heat-treated by contacting it with a roller at 180 ° C for 10 seconds. Next, the electrode was cut to a predetermined plate size to produce a positive electrode having a positive electrode mixture layer formed on both sides of the positive electrode current collector. Then, aluminum positive electrode tabs were welded to each of the eight positive electrode exposed portions, and insulating tape was applied to cover the positive electrode exposed portions, the positive electrode tabs, and a portion of the positive electrode mixture layer adjacent to the positive electrode mixture layer. For the first positive electrode mixture layer, the tacking strength T1 was 370 N and the peel strength P1 was 10 N / m. For the second positive electrode mixture layer, the tacking strength T1 was 310 N and the peel strength P1 was 8 N / m.

[0051] [Preparation of Negative Electrode] 95 parts by mass of graphite, 5 parts by mass of Si oxide (SiO), 1 part by mass of sodium carboxymethyl cellulose (CMC-Na), and 1 part by mass of styrene butadiene rubber (SBR) were mixed, and an appropriate amount of water was added to prepare a negative electrode mixture slurry. Next, the negative electrode mixture slurry was applied to both sides of a strip-shaped negative electrode current collector made of copper foil with a thickness of 8 μm, dried, rolled, and cut to a predetermined electrode plate size to prepare a negative electrode in which a negative electrode mixture layer was formed on both sides of the negative electrode current collector. A negative electrode exposed portion in which no mixture layer was present and the current collector surface was exposed was provided at the inner end of the winding of the negative electrode, and a nickel negative electrode tab was welded to the negative electrode exposed portion.

[0052] [Preparation of non-aqueous electrolyte] 5 parts by mass of vinylene carbonate (VC) was added to 100 parts by mass of a mixed solvent in which ethylene carbonate (EC) and dimethyl carbonate (DMC) were mixed at a volume ratio of 3:7, and lithium hexafluorophosphate (LiPF 6 A non-aqueous electrolyte was prepared by dissolving 1.5 mol / L of ammonium hydroxide in water.

[0053] [Preparation of Test Cell] A wound electrode assembly was prepared by spirally winding a positive electrode and a negative electrode with a polyethylene microporous membrane separator interposed therebetween. This electrode assembly was housed in a cylindrical outer can with a bottom, and the negative electrode tab was welded to the bottom of the cylindrical outer can with a bottom, and the positive electrode tab was welded to a sealing member. After pouring a nonaqueous electrolyte into the outer can, the opening of the outer can was sealed with a sealing member via a gasket to prepare a cylindrical test cell.

[0054] [Evaluation of Capacity Retention Rate] One hundred test cells were prepared, and each test cell was subjected to 500 charge-discharge cycles as follows. The capacity retention rate of each test cell was calculated using the following formula, and the obtained data for the capacity retention rates of the 100 test cells was averaged to determine the capacity retention rate of the test cell of Example 1-1. Capacity retention rate = (discharge capacity at 500th cycle / discharge capacity at 1st cycle) × 100 [Charge-Discharge Cycle] At an ambient temperature of 25°C, the test cell was charged at a constant current of 0.3 C to a battery voltage of 4.2 V, and then charged at a constant voltage of 4.2 V until the current value reached 0.01 C. Thereafter, the test cell was discharged at a constant current of 0.5 C to 2.5 V, and this charge-discharge cycle was defined as one cycle.

[0055] [Number of Peelings of Positive Electrode Mixture Layer] After the above charge-discharge cycles, 100 test cells were disassembled to count the number of test cells in which peeling of the positive electrode mixture layer occurred. As will be described later, in Examples 1-2 and 1-3 and Comparative Examples 1-1, 2, and 3, there were test cells in which peeling of the positive electrode mixture layer occurred, and in all cases, peeling occurred near the sides parallel to the width direction of the protective member.

[0056] Example 1-2 A test cell was prepared and evaluated in the same manner as in Example 1-1, except that the roller temperature was changed to 130° C. in the preparation of the positive electrode.

[0057] Example 1-3 A test cell was prepared and evaluated in the same manner as in Example 1-1, except that the roller temperature was changed to 140° C. in the preparation of the positive electrode.

[0058] Example 1-4 A test cell was prepared and evaluated in the same manner as in Example 1-1, except that in the preparation of the positive electrode, the roller contact time was changed to 20 seconds.

[0059] Example 1-5 A test cell was prepared and evaluated in the same manner as in Example 1-1, except that in preparing the positive electrode, the roller contact time was changed to 30 seconds.

[0060] Comparative Example 1-1 A test cell was produced and evaluated in the same manner as in Example 1-1, except that no heat treatment was performed in the production of the positive electrode.

[0061] <Comparative Example 1-2> A test cell was produced and evaluated in the same manner as in Example 1-1, except that in the production of the positive electrode, the portion corresponding to the second positive electrode mixture layer was also subjected to heat treatment in the same manner as in the first positive electrode mixture layer.

[0062] Example 2 A test cell was produced and evaluated in the same manner as in Example 1-1, except that in the production of the positive electrode, the number of positive electrode exposed portions was changed to three, and an aluminum positive electrode tab was welded to each of the three positive electrode exposed portions.

[0063] Comparative Example 2 A test cell was prepared and evaluated in the same manner as in Example 2, except that no heat treatment was performed in the preparation of the positive electrode.

[0064] Example 3 A test cell was produced and evaluated in the same manner as in Example 1-1, except that in the production of the positive electrode, the number of positive electrode exposed portions was changed to one and an aluminum positive electrode tab was welded to this positive electrode exposed portion.

[0065] Comparative Example 3 A test cell was prepared and evaluated in the same manner as in Example 3, except that no heat treatment was performed in the preparation of the positive electrode.

[0066] The evaluation results of the test cells according to the examples and comparative examples are shown in Tables 1 and 2. In Table 2, the results of Example 1-1 and Comparative Example 1-1 shown in Table 1 are listed again to show the relationship between the effect of suppressing peeling of the positive electrode mixture layer and the number of exposed positive electrode portions. In addition, in the column for the number of peeled positive electrode mixture layers of the test cells of Examples 1-1, 2, and 1-3, the difference in the number of peeled positive electrode mixture layers from the corresponding test cells of Comparative Examples 1-1, 2, and 1-3 is shown in parentheses.

[0067]

[0068]

[0069] As shown in Table 1, the test cells of Examples 1-1 to 1-5 were able to obtain a high capacity retention rate while suppressing peeling of the positive electrode mixture layer. On the other hand, the test cells of Comparative Examples 1-1 and 1-2 were unable to simultaneously suppress peeling of the positive electrode mixture layer after charge / discharge cycling and suppress a decrease in battery capacity. Furthermore, the results shown in Table 2 show that the test cells with a larger number of exposed positive electrode portions were more effective in suppressing peeling of the positive electrode mixture layer.

[0070] The present disclosure is further illustrated by the following embodiments. Configuration: 1 A cylindrical secondary battery comprising an electrode assembly in which a positive electrode and a negative electrode are wound with a separator interposed therebetween, a non-aqueous electrolyte, and a cylindrical outer can accommodating the electrode assembly and the non-aqueous electrolyte, wherein the positive electrode has a positive electrode current collector and a positive electrode mixture layer disposed on the surface of the positive electrode current collector, a positive electrode exposed portion where the positive electrode current collector is exposed is disposed on the surface of the positive electrode, the positive electrode exposed portion is in contact with only one of both end portions in the width direction of the positive electrode, a positive electrode tab is connected to the positive electrode exposed portion and extends from the one end, a protective member covers the positive electrode exposed portion, the positive electrode tab, and a portion of the positive electrode mixture layer adjacent to the positive electrode exposed portion, and when the positive electrode mixture layer is divided into a first positive electrode mixture layer aligned with the positive electrode exposed portion in the longitudinal direction of the positive electrode and a second positive electrode mixture layer adjacent to the positive electrode exposed portion and the first positive electrode mixture layer in the width direction of the positive electrode, A cylindrical secondary battery in which a tacking strength T1 of the first positive electrode mixture layer and a tacking strength T2 of the second positive electrode mixture layer satisfy the relationship T1 > T2. Configuration 2: The cylindrical secondary battery according to Configuration 1, in which T1 and T2 satisfy the relationship 1.03 ≦ T1 / T2 ≦ 1.68. Configuration 3: The cylindrical secondary battery according to Configuration 1, in which T1 and T2 satisfy the relationship 1.10 ≦ T1 / T2 ≦ 1.42. Configuration 4: The cylindrical secondary battery according to any one of Configurations 1 to 3, in which T1 is 320 N or more and 520 N or less. Configuration 5: The cylindrical secondary battery according to any one of Configurations 1 to 4, in which a plurality of the positive electrode exposed portions are arranged on the surface of the positive electrode. Configuration 6: The cylindrical secondary battery according to any one of Configurations 1 to 5, in which a peel strength P1 of the first positive electrode mixture layer and a peel strength P2 of the second positive electrode mixture layer satisfy the relationship P1 > P2. Configuration 7: The cylindrical secondary battery of Configuration 6, wherein P1 and P2 satisfy the relationship 1.13≦P1 / P2≦1.63. Configuration 8: The cylindrical secondary battery of Configuration 6, wherein P1 and P2 satisfy the relationship 1.19≦P1 / P2≦1.38. Configuration 9: The cylindrical secondary battery of any one of Configurations 6 to 8, wherein P1 is 9 N / m or more and 13 N / m or less.

[0071] REFERENCE SIGNS LIST 10 (cylindrical) secondary battery, 11 positive electrode, 12 negative electrode, 13 separator, 14 electrode body, 15 outer can, 16 sealing body, 17, 18 insulating plate, 19 positive electrode tab, 20 negative electrode tab, 21 grooved portion, 22 filter, 23 lower valve body, 24 insulating member, 25 upper valve body, 26 cap, 26a opening, 27 gasket, 30 positive electrode current collector, 32 positive electrode mixture layer, 34 positive electrode exposed portion, 36 protective member, 38 first positive electrode mixture layer, 39 second positive electrode mixture layer

Claims

1. A cylindrical secondary battery comprising an electrode assembly in which a positive electrode and a negative electrode are wound with a separator interposed therebetween, a non-aqueous electrolyte, and a cylindrical exterior can accommodating the electrode assembly and the non-aqueous electrolyte, wherein the positive electrode has a positive electrode current collector and a positive electrode mixture layer disposed on a surface of the positive electrode current collector, a positive electrode exposed portion in which the positive electrode current collector is exposed is disposed on the surface of the positive electrode, the positive electrode exposed portion is in contact with only one of both ends in the width direction of the positive electrode, a positive electrode tab is connected to the positive electrode exposed portion and is led out from the one end, a protective member covers the positive electrode exposed portion, the positive electrode tab, and a portion of the positive electrode mixture layer adjacent to the positive electrode exposed portion, and when the positive electrode mixture layer is divided into a first positive electrode mixture layer aligned with the positive electrode exposed portion in the longitudinal direction of the positive electrode, and a second positive electrode mixture layer adjacent to the positive electrode exposed portion and the first positive electrode mixture layer in the width direction of the positive electrode, a tacking strength T1 of the first positive electrode mixture layer and a tacking strength T2 of the second positive electrode mixture layer satisfying the relationship T1>T2.

2. The cylindrical secondary battery according to claim 1, wherein T1 and T2 satisfy the relationship: 1.03≦T1 / T2≦1.

68.

3. The cylindrical secondary battery according to claim 1, wherein T1 and T2 satisfy the relationship: 1.10≦T1 / T2≦1.

42.

4. The cylindrical secondary battery according to claim 1, wherein T1 is 320N or more and 520N or less.

5. The cylindrical secondary battery according to claim 1, wherein a plurality of the positive electrode exposed portions are arranged on the surface of the positive electrode.

6. The cylindrical secondary battery according to claim 1, wherein a peel strength P1 of the first positive electrode mixture layer and a peel strength P2 of the second positive electrode mixture layer satisfy the relationship P1>P2.

7. The cylindrical secondary battery according to claim 6, wherein P1 and P2 satisfy the relationship 1.13≦P1 / P2≦1.

63.

8. The cylindrical secondary battery according to claim 6, wherein P1 and P2 satisfy the relationship 1.19≦P1 / P2≦1.

38.

9. The cylindrical secondary battery according to claim 6, wherein P1 is equal to or greater than 9 N / m and equal to or less than 13 N / m.

Citation Information

Patent Citations

  • Electrode plate, electrochemical apparatus, and electronic apparatus

    EP3961750A1

  • Lithium-ion secondary battery, and vehicle and apparatus with the lithium-ion secondary battery thereon

    JP2011134564A

  • Method of manufacturing electrode for lithium ion battery

    JP2016115568A

  • Method of manufacturing electrode for lithium ion battery

    JP2016115603A

  • Secondary battery electrode, secondary battery, and method for producing secondary battery electrode

    WO2022209112A1