Coolant and method for producing coolant

The coolant, comprising solids that undergo an endothermic reaction and are formed into specific-sized lumps, addresses the issue of rapid cooling by facilitating a gradual cooling process, ensuring comfort and effective temperature management.

WO2024225079A1PCT designated stage expired Publication Date: 2024-10-31MITSUBISHI GAS CHEM CO INC
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/014817
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-24
Filing Date
2024-04-12
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Coolants often cool too rapidly, causing discomfort due to excessive cooling immediately after the cooling reaction, which is not effectively addressed by existing technologies.

Method used

A coolant comprising two solids that undergo an endothermic reaction, where at least one solid is formed into a lump of specific dimensions, allowing for controlled cooling by facilitating a gradual reaction, and optionally including a moisture absorbent to manage moisture generated during the reaction.

Benefits of technology

The coolant provides a controlled cooling effect that prevents excessive cooling immediately after use, maintaining a suitable temperature and ensuring comfort while effectively managing the cooling reaction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024014817_31102024_PF_FP_ABST
    Figure JP2024014817_31102024_PF_FP_ABST
Patent Text Reader

Abstract

Provided are a coolant and a method for producing a coolant. This coolant contains a solid A and a solid B, wherein: the solid A and the solid B respectively contain compounds that undergo an endothermic reaction upon coming into contact with each other; at least one of the solid A and the solid B is in the form of lumps; and if the lumps are thrown onto a horizontal plane and observed, from a direction that is perpendicular to the horizontal plane, in a state where each of the lumps remains stationary in the most stable manner, the average (bx) of the lengths of minor axes (b) excluding the top 10% and the bottom 10% thereof is 1 mm to 100 mm, each of the lengths of the minor axes (b) being the minimum distance between two parallel lines that are in contact with the outline (projected image) of each lump.
Need to check novelty before this filing date? Find Prior Art

Description

Coolant and method for producing the same

[0001] The present invention relates to a coolant and a method for producing the coolant.

[0002] In recent years, the need for cooling has increased in many fields, including sports, leisure, and distribution. Patent Document 1 discloses a portable ice pack that contains a cryogen consisting of ammonium nitrate and urea, and a solvent selected from the group consisting of an aqueous solution of a water-soluble polymeric substance, its gel, and water, sealed in an inner synthetic polymer bag strong enough to easily burst under external force during use. The outer synthetic polymer bag is resistant to external forces that easily burst the inner bag, and the cryogen and solvent are brought into contact with each other by applying external force to the outer bag to rupture the inner bag. Patent Document 2 also describes a cryogen consisting of a molded ammonium nitrate product containing 0.1 to 1.5% by weight of water, obtained by solidifying and molding molten ammonium nitrate.

[0003] JP-A-59-155486 JP-A-8-295508

[0004] However, the colder the coolant, the better, and in particular, if it becomes too cold immediately after the cooling reaction, it can cause problems such as pain and discomfort due to excessive cooling. The present invention aims to solve such problems and provides a coolant that does not become too cold immediately after cooling, and a method for producing the coolant.

[0005] In light of the above-mentioned problems, the present inventors have conducted research and found that the above-mentioned problems can be solved by bringing two types of solids into contact with each other to cause an endothermic reaction, and by forming at least one of the solids into a lump of a predetermined size. Specifically, the above-mentioned problems have been solved by the following means: <1> A substance comprising solid A and solid B, wherein solid A and solid B contain compounds that undergo an endothermic reaction when in contact with each other, and at least one of solid A and solid B is a lump, and when the lump is thrown onto a horizontal plane and each lump is observed in its most stable state at rest from a direction perpendicular to the horizontal plane, the smallest distance between two parallel lines tangent to the outline (projected image) of the lump is defined as the minor axis diameter (b), and the average value (b) of the lengths of (b) excluding the top 10% and bottom 10% of the lengths is obtained. x ) is 1 mm to 100 mm. <2> The coolant according to <1>, wherein the solid A contains a hydrate, and the solid B contains a hydrate dissociator. <3> The coolant according to <1> or <2>, wherein the solid A contains a hydrate of an inorganic substance, and the solid B contains at least one selected from the group consisting of a polybasic acid, a metal salt of a polybasic acid, and an inorganic ammonium salt. <4> The coolant according to <1> or <2>, wherein the solid A contains a hydrate of an inorganic substance, and the solid B contains at least one selected from the group consisting of adipic acid, oxalic acid, succinic acid, malic acid, acetic acid, tartaric acid, fumaric acid, citric acid, and metal salts thereof. <5> The coolant according to any one of <1> to <4>, wherein the solid B is a block. <6> The coolant according to <5>, wherein the solid B contains a moisture absorbent. <7> The cooling agent according to any one of <1> to <6>, further comprising a moisture absorbent. <8> The cooling agent according to <6> or <7>, wherein the moisture absorbent is at least one selected from the group consisting of starch, lactose, and cellulose. <9> The cooling agent according to any one of <1> to <8>, wherein solid A and solid B are in a non-contact state until use. <10> The cooling agent according to any one of <1> to <8>, wherein the distance between the blocks measured in a direction perpendicular to the minor axis diameter (b) is defined as the major axis diameter (l), and the average value (l) of the values ​​excluding the top 10% and bottom 10% of the lengths of (l) is obtained. x ) and the average value (b x) is the ratio of (l x ) / (b x ) is 1 to 50. <11> A method for producing a coolant, comprising solid A and solid B, wherein solid A and solid B contain compounds that undergo an endothermic reaction when in contact with each other, and the method comprises molding at least one of solid A and solid B into a block. <12> A method for producing a coolant according to <11>, wherein the coolant is the coolant according to any one of <1> to <10>.

[0006] The present invention makes it possible to provide a coolant that does not become too cold immediately after cooling, and a method for producing the coolant.

[0007] FIG. 1 is a schematic diagram for explaining the minor axis diameter (b) and major axis diameter (l) of a lump of the present invention, and the length of the highest part (t) of the height from the horizontal plane.

[0008] Hereinafter, a mode for carrying out the present invention (hereinafter simply referred to as "the present embodiment") will be described in detail. Note that the following present embodiment is an example for explaining the present invention, and the present invention is not limited to only this embodiment. Note that in this specification, "to" is used to mean that the numerical values ​​written before and after it are included as lower and upper limits. In this specification, various physical property values ​​and characteristic values ​​are at 23°C unless otherwise specified. If the measurement methods etc. described in the standards shown in this specification vary depending on the fiscal year, they are based on the standards as of January 1, 2023, unless otherwise specified. In Figure 1, the scale may not be consistent with reality.

[0009] The coolant of this embodiment includes a solid A and a solid B, and the solid A and the solid B contain compounds that undergo an endothermic reaction when in contact with each other, and at least one of the solids A and B is a mass, and when the mass is thrown onto a horizontal plane and the state in which each mass is most stable is observed from a direction perpendicular to the horizontal plane, the smallest distance between two parallel lines tangent to the outline (projected image) of the mass is defined as the minor axis diameter (b), and the average value (b) of the values ​​excluding the top 10% and bottom 10% of the length of (b) is obtained. x) is 1 mm to 100 mm. By adopting such a configuration, the endothermic reaction proceeds gradually, and it is possible to provide a coolant that does not become too cold immediately after cooling.

[0010] In this embodiment, the coolant includes solid A and solid B, at least one of which is a lump. The lump is intended to include granules, tablets, etc. It also includes granules formed by the aggregation of two or more particles due to heat, pressure, water, adhesive components, etc. In this embodiment, it is sufficient that one of solid A and solid B is a lump, but both may be a lump.

[0011] In this embodiment, when a lump is thrown onto a horizontal plane and observed in a direction perpendicular to the horizontal plane while the lump is at its most stable state, the shortest distance between two parallel lines tangent to the outline (projected image) of the lump is defined as the minor axis diameter (b). The average value (b) of the shortest distance between the two parallel lines tangent to the outline (projected image) of the lump is calculated by excluding the top 10% and bottom 10% of the lengths of (b). x ) is 1 mm to 100 mm. FIG. 1 shows a schematic diagram of an example of a single lump of this embodiment, with FIG. 1(X) being an external view of a single lump in a stably stationary state, and FIG. 1(Y) being a view of the lump of FIG. 1(X) viewed from another direction. When a lump such as that shown in FIG. 1(X) is thrown onto a horizontal plane, it will most stably rest in a state where one of the disk faces is resting on the surface of the horizontal plane, as shown in FIG. 1(X). In this state, the direction perpendicular to the horizontal plane is the upper view of FIG. 1(Y). When observed from a direction perpendicular to the horizontal plane, the smallest distance b between two parallel lines tangent to the outline (projected image) of the lump is the minor axis diameter. In this embodiment, the average value (b) of the minor axis diameter (b) excluding the top 10% and bottom 10% of the lengths of (b) is used. x ) is 1 mm to 100 mm. x ) is set to the lower limit or more, the rapid cooling reaction tends to be more effectively suppressed. xBy making the length (b) equal to or less than the upper limit, the productivity is excellent, the cooling reaction is not excessively suppressed, the contact between solid A and solid B is facilitated, and the feeling of a foreign body when the solid A comes into contact with the cooled object such as the body during use tends to be effectively suppressed. In addition, when the number of lumps is three or less, the average value of the minor axis diameter (b) of all lumps is calculated as the average value (b) without excluding the top 10% and bottom 10% of the length of (b). x ) The average value (l x The same applies to the average value (b x ) is preferably 2 mm or more, and is preferably 90 mm or less, more preferably 70 mm or less, even more preferably 50 mm or less, even more preferably 40 mm or less, and even more preferably 30 mm or less, and may further be 24 mm or less, 19 mm or less, or 9 mm or less depending on the application, etc.

[0012] In this embodiment, when the distance measured in the direction perpendicular to the minor axis diameter (b) of the block is defined as the major axis diameter (l), the average value (l) of the major axis diameter (l) is calculated by excluding the top 10% and bottom 10% of the major axis diameter (l). x ) and the average value (b x ) is the ratio of (l x ) / (b x ) is preferably 1 to 50. x By making the average value (l) equal to or greater than the lower limit, productivity tends to be further improved. x By making the diameter (l) equal to or less than the upper limit, the shape can be maintained against impact and the ease of transport tends to be improved. Here, the major axis diameter (l) corresponds to (l) in Figure 1 (Y) and means the distance measured in the direction perpendicular to the minor axis diameter (b). The measurement method of the major axis diameter (l) and the average value (l x ) calculation method, measurement method of minor axis diameter (b) and average value (b x ) is calculated in the same manner as the above (l x ) / (b x) is preferably 1 or more, and is preferably 40 or less, more preferably 30 or less, even more preferably 20 or less, still more preferably 10 or less, and even more preferably 5 or less.

[0013] In this embodiment, when a lump is thrown onto a horizontal plane and the state in which each lump is most stably stationary is observed from a direction perpendicular to the horizontal plane, the average value (t) of the length of the highest part (t) of the height from the horizontal plane of the outline (projected image) of the lump is calculated by excluding the top 10% and bottom 10% of the length of (t). x ) is preferably 1 mm or more, more preferably 2 mm or more, even more preferably 3 mm or more, even more preferably 4 mm or more, and may be 5 mm or more. By making it equal to or greater than the lower limit, the effect of suppressing a rapid cooling reaction tends to be further improved. In addition, the average value t x ) is preferably 100 mm or less, more preferably 80 mm or less, even more preferably 50 mm or less, even more preferably 25 mm or less, and even more preferably 10 mm or less. By making it equal to or less than the upper limit, excellent manufacturability is achieved, the cooling reaction is not excessively suppressed, contact between solid A and solid B is facilitated, and a foreign body sensation or the like when contacting an object to be cooled such as the body during use tends to be effectively suppressed.

[0014] In this embodiment, the average value (V) of the volume (V) of the aggregates excluding the top 10% and bottom 10% is further calculated. x ) is 1 mm 3 It is preferable that the thickness is 8 mm or more. 3 More preferably, it is 27 mm or more. 3 More preferably, it is 64 mm or more. 3 More preferably, it is 125 mm or more. 3 It is more preferable that the volume is equal to or greater than the lower limit. By making the volume equal to or greater than the lower limit, the effect of suppressing a rapid cooling reaction tends to be further improved. In addition, the average value (V x ) is 1,000,000 mm 3Preferably, the length is 512,000 mm or less. 3 More preferably, it is 216,000 mm or less. 3 More preferably, it is 64,000 mm or less. 3 More preferably, it is 8,000 mm or less. 3 By setting the temperature to the upper limit or less, excellent productivity is achieved, the cooling reaction is not excessively suppressed, contact between solid A and solid B is facilitated, and there is a tendency to effectively suppress a foreign body sensation or the like when solid A comes into contact with an object to be cooled, such as the body, during use.

[0015] In this embodiment, as described above, it is sufficient that one of solid A and solid B is a lump, but it is preferable that one is a lump and the other is a powder.

[0016] In this embodiment, solid A and solid B contain compounds that undergo an endothermic reaction when they come into contact with each other. That is, when component a contained in solid A and component b contained in solid B come into contact, an endothermic reaction proceeds. By proceeding with the endothermic reaction in this manner, a cooling effect can be exerted. In particular, in this embodiment, by precisely adjusting the size of the aggregates, excessive cooling immediately after the start of the endothermic reaction can be effectively suppressed.

[0017] In this embodiment, the mass ratio of component a contained in solid A to component b contained in solid B is not particularly limited as long as the endothermic reaction proceeds, but is preferably 1:9 to 9:1, more preferably 2:8 to 8:2, and may further be 3:7 to 8:2, 4:6 to 8:2, 5:5 to 8:2, or 6:4 to 8:2. The coolant in this embodiment may contain only one type of component a contained in solid A, or may contain two or more types. When two or more types are contained, it is preferable that the total amount of component a falls within the above range. The coolant in this embodiment may contain only one type of component b contained in solid B, or may contain two or more types. When two or more types are contained, it is preferable that the total amount of component b falls within the above range.

[0018] In the coolant of this embodiment, it is preferable that solid A contains a hydrate and solid B contains a hydrate dissociator. That is, in this embodiment, it is preferable that component a contained in solid A is a hydrate and component b contained in solid B is a hydrate dissociator. By making the endothermic reaction a hydrate dissociation reaction, it is possible to obtain a coolant that is highly safe.

[0019] As described above, component a contained in solid A is preferably a hydrate, more preferably an inorganic hydrate. Furthermore, the inorganic hydrate is preferably a pentahydrate or more, more preferably an octahydrate or more, and preferably a 20-hydrate or less, more preferably an 18-hydrate or less, and even more preferably a 15-hydrate or less. Component a is more preferably a hydrate of a metal salt of citric acid, sulfate, or phosphoric acid, and even more preferably a hydrate of a metal phosphate. Examples of component a include magnesium citrate nonahydrate, sodium sulfate decahydrate, sodium hexacyanoferrate(II) decahydrate, ammonium aluminum sulfate dodecahydrate, disodium hydrogen phosphate dodecahydrate, trisodium phosphate dodecahydrate, ammonium iron(III) sulfate dodecahydrate, potassium aluminum sulfate dodecahydrate, and aluminum sulfate dodecahydrates from 14 to 18.

[0020] The solid A preferably contains a moisture absorbent. By containing the moisture absorbent, moisture generated in the endothermic reaction can be effectively absorbed, and a long cooling time can be achieved. The type of moisture absorbent is not particularly limited, and a wide variety of compounds that absorb moisture generated in the endothermic reaction can be used. The moisture absorbent is preferably at least one selected from the group consisting of starch, lactose, and cellulose, more preferably cellulose, and even more preferably crystalline cellulose.

[0021] The amount of component a contained in the solid A is preferably 80% by mass or more, more preferably 90% by mass or more, even more preferably 95% by mass or more, and even more preferably 99% by mass or more, when the solid A is taken as 100% by mass. The upper limit of the amount of component a contained in the solid A may be 100% by mass when the solid A is taken as 100% by mass. Furthermore, when the solid A contains a moisture absorbent, the total amount of component a and the moisture absorbent is preferably 75% by mass or more, more preferably 85% by mass or more, even more preferably 90% by mass or more, and even more preferably 93% by mass or more, when the solid A is taken as 100% by mass. Depending on the application, it may be 95% by mass or more, 97% by mass or more, or 99% by mass or more. The upper limit of the total amount of component a and the moisture absorbent contained in the solid A may be 100% by mass when the solid A is taken as 100% by mass. On the other hand, the amount of the moisture absorbent contained in the solid A is preferably 0.1% by mass or more, more preferably 0.5% by mass or more, and even more preferably 1.5% by mass or more, and is preferably 10% by mass or less, and more preferably 7% by mass or less, when the solid A is taken as 100% by mass. The solid A may contain only one type of moisture absorbent, or may contain two or more types. When two or more types of moisture absorbents are contained, it is preferable that the total amount is in the above range.

[0022] As described above, component b contained in solid B in the coolant of this embodiment is preferably a hydrate dissociator. The hydrate dissociator is not particularly limited as long as it is a substance that causes an endothermic reaction when it comes into contact with the hydrate (component a). However, it is more preferably at least one selected from polybasic acids, metal salts of polybasic acids, and inorganic ammonium salts, more preferably polybasic acids and / or inorganic ammonium salts, and even more preferably polybasic acids. The polybasic acids and metal salts of polybasic acids preferably include at least one selected from the group consisting of adipic acid, oxalic acid, succinic acid, malic acid, acetic acid, tartaric acid, fumaric acid, and citric acid, and metal salts thereof. Examples of salts constituting the metal salt include sodium salts, potassium salts, calcium salts, and magnesium salts, with sodium salts and potassium salts being preferred, and sodium salts being more preferred. Examples of inorganic ammonium salts include ammonium dihydrogen phosphate, potassium dihydrogen phosphate, sodium dihydrogen phosphate, ammonium nitrate, ammonium chloride, ammonium sulfate, ammonium carbonate, ammonium hydrogen carbonate, ammonium aluminum sulfate dodecahydrate, ammonium bromide, ammonium borate, ammonium borate octahydrate, and ammonium hydrogen phosphate, of which ammonium sulfate, ammonium carbonate, ammonium hydrogen carbonate, ammonium aluminum sulfate dodecahydrate, ammonium bromide, ammonium borate octahydrate, and ammonium hydrogen phosphate are preferred, and ammonium hydrogen carbonate and ammonium borate octahydrate are more preferred.

[0023] The solid B preferably contains a moisture absorbent. By containing the moisture absorbent, the moisture generated in the endothermic reaction can be effectively absorbed, and a long cooling time can be achieved. The type of moisture absorbent is not particularly limited, and a wide variety of compounds that absorb moisture generated in the endothermic reaction can be used. The moisture absorbent is preferably at least one selected from the group consisting of starch, lactose, and cellulose, more preferably cellulose, and even more preferably crystalline cellulose.

[0024] The amount of component b contained in solid B is preferably 75% by mass or more, more preferably 85% by mass or more, even more preferably 90% by mass or more, and even more preferably 93% by mass or more, when solid B is taken as 100% by mass. Depending on the intended use, etc., it may be 95% by mass or more, 97% by mass or more, or 99% by mass or more. The upper limit of the amount of component b contained in solid B may be 100% by mass, when solid B is taken as 100% by mass. Furthermore, when solid B contains a moisture absorbent, the total amount of component b and the moisture absorbent is preferably 75% by mass or more, more preferably 85% by mass or more, even more preferably 90% by mass or more, and even more preferably 93% by mass or more, when solid B is taken as 100% by mass. Depending on the intended use, it may be 95% by mass or more, 97% by mass or more, or 99% by mass or more. The upper limit of the total amount of component b and the moisture absorbent contained in solid B may be 100% by mass, when solid B is taken as 100% by mass. On the other hand, the amount of the moisture absorbent contained in Solid B is preferably 0.1% by mass or more, more preferably 0.5% by mass or more, and even more preferably 1.5% by mass or more, and is preferably 10% by mass or less, and more preferably 7% by mass or less, when Solid B is taken as 100% by mass. Solid B may contain only one type of moisture absorbent, or may contain two or more types. When two or more types of moisture absorbents are contained, it is preferable that the total amount is in the above range.

[0025] The coolant of this embodiment may contain components other than solid A and solid B. Examples of components other than solid A and solid B include a moisture absorbent, an excipient, a lubricant, and a surface coating agent. By containing a moisture absorbent, moisture generated in the endothermic reaction can be effectively absorbed, and acceleration of the endothermic reaction can be more effectively suppressed. More specifically, when the moisture absorbent absorbs moisture, the polybasic acid dissolves in water, effectively suppressing acceleration of the reaction. The details of the moisture absorbent are the same as those of the moisture absorbent that may be contained in solid B described above, and the preferred range is also the same.

[0026] When the coolant of this embodiment contains a moisture absorbent, the content of the moisture absorbent in 100% by mass of the coolant is preferably 0.01% by mass or more, more preferably 0.05% by mass or more, even more preferably 0.1% by mass or more, and even more preferably 0.5% by mass or more. Depending on the application, the content may be 1% by mass or more, and preferably 5% by mass or less, more preferably 3% by mass or less, and may be 2% by mass or less. Other components such as a moisture absorbent contained in the coolant refer to components other than solid A and / or solid B. The coolant of this embodiment may contain only one other component (preferably a moisture absorbent) or two or more other components. When two or more components are contained, the total amount is preferably within the above range.

[0027] In a first embodiment of the coolant of this embodiment, solid A is a powder, solid B is a lump, component a is a hydrate of an inorganic substance, and component B is at least one selected from a polybasic acid, a metal salt of a polybasic acid, and an inorganic ammonium salt. Furthermore, solid B may contain a moisture absorbent. In a second embodiment of the coolant of this embodiment, solid A is a lump, solid B is a powder, component a is a hydrate of an inorganic substance, and component B is at least one selected from a polybasic acid, a metal salt of a polybasic acid, and an inorganic ammonium salt. Furthermore, the coolant may contain a moisture absorbent as another component.

[0028] In this embodiment, it is preferable that solid A and solid B are kept out of contact with each other until use. By keeping solid A and solid B out of contact with each other until use, it is possible to prevent the endothermic reaction between solid A and solid B from progressing until use. Examples of methods for keeping solid A and solid B out of contact include storing them in different packaging containers and mixing them when used, and coating the surface of at least one of solid A and / or solid B with a surface coating agent.

[0029] The method for producing the coolant of this embodiment is not particularly limited, but includes forming at least one of solid A and solid B into a mass, where solid A and solid B contain compounds that undergo an endothermic reaction when in contact with each other. By forming at least one of solid A and solid B into a mass, excessive progress of the endothermic reaction can be suppressed, and initial overcooling can be effectively suppressed. Furthermore, when forming at least one of solid A and solid B into a mass, a lubricant may be blended into the raw material. The addition of a lubricant tends to improve slipperiness, making it easier to produce the mass.

[0030] In the coolant of this embodiment, when a total amount of 10 g of the coolant is brought into contact with solid A and solid B at 23°C, after the cooling temperature falls below 18°C, the time until the cooling temperature returns to 18°C ​​is preferably within 60 minutes, more preferably within 50 minutes, even more preferably within 40 minutes, even more preferably within 30 minutes, even more preferably within 30 minutes, and even more preferably within 20 minutes. The lower limit of the time until the temperature returns to 18°C ​​may be greater than 0 minutes, and may be 1 minute or more. Furthermore, depending on the application, the minimum cooling temperature of the coolant of this embodiment may be such that it does not fall below 18°C. The coolant of this embodiment is very beneficial because it can prevent excessive cooling immediately after contact between solid A and solid B. The coolant of this embodiment preferably cools moderately. Specifically, the minimum cooling temperature is preferably 5°C or higher, more preferably 8°C or higher, and even more preferably 10°C or higher. Furthermore, the minimum cooling temperature of this embodiment is preferably 25°C or lower, and more preferably 20°C or lower.

[0031] The coolant of this embodiment can be widely used for purposes requiring cooling, and can be preferably used as a body coolant, food coolant, equipment coolant, animal coolant, fresh flower coolant, etc.

[0032] The present invention will be explained in more detail below with reference to examples. The materials, amounts used, ratios, treatment contents, treatment procedures, etc. shown in the following examples can be changed as appropriate without departing from the spirit of the present invention. Therefore, the scope of the present invention is not limited to the specific examples shown below. If the measuring instruments used in the examples are difficult to obtain due to discontinuation or the like, measurements can be made using other instruments with equivalent performance.

[0033] Disodium hydrogen phosphate dodecahydrate: Manufacturer: Fujifilm Wako Pure Chemical Corporation Trisodium phosphate dodecahydrate: Manufacturer: Fujifilm Wako Pure Chemical Corporation Citric acid: Manufacturer: Fujifilm Wako Pure Chemical Corporation DL-Malic acid: Manufacturer: Fujifilm Wako Pure Chemical Corporation KC Floc-W50: Crystalline cellulose, Manufacturer: Nippon Paper Industries Co., Ltd. KC Floc-W200: Crystalline cellulose, Manufacturer: Nippon Paper Industries Co., Ltd.

[0034] Example 1 Component b shown in Table 1 was compressed in a molding machine at 415 kgf / cm 2 Each of the obtained blocks was thrown onto a horizontal plane and allowed to rest stably. As described above, the minor axis diameter (b), the major axis diameter (l) measured in a direction perpendicular to the minor axis diameter (b), and the maximum height (t) of the block's outline (projected image) from the horizontal plane were measured for the projection of the block's outline, as shown in FIG. 1. x is 25 mm, b x is 25 mm, t x The volume of the lump was 2454 mm 3 The projection was performed visually. Component a (powder) shown in Table 1 was blended with the obtained block in the proportion (parts by mass) shown in Table 1, and the minimum cooling temperature (°C) was measured. In addition, the time (minutes) required for the temperature to return to 18°C ​​after blending component a and dropping below 18°C ​​was measured. The cooling temperature was measured as follows. An aluminum cup measuring upper diameter x lower diameter x height H (mm) Φ65 x Φ54 x 23 with a thermocouple attached to the underside was placed on a heat insulating material with a thickness of 3 cm or more, and measurements were performed using a data logger.

[0035] Examples 2 to 4 Component b and a moisture absorbent shown in Table 1 were mixed in the ratio (parts by mass) shown in Table 1, homogenized, and then treated in the same manner as in Example 1 to obtain lumps. x is 25 mm, b x is 25 mm, t x The volume of the lump was 2454 mm 3 The component a (powder) shown in Table 1 was added to the obtained block in the proportion shown in Table 1, and the minimum temperature (°C) and the time (minutes) required for the temperature to return to 18°C ​​were measured in the same manner as in Example 1. The difference Δ (°C) in the minimum temperature compared to Example 1 was also calculated.

[0036] Comparative Examples 1 to 4 Component a (powder) and component b (powder) shown in Table 1 were mixed, and if necessary, a moisture absorbent (powder) in the proportions (parts by mass) shown in Table 1. The minimum cooling temperature (°C) after homogenization and the time (minutes) required to return to 18°C ​​were measured in the same manner as in Example 1. For Comparative Examples 2 to 4, the difference Δ (°C) in the minimum temperature compared to Comparative Example 1 was calculated.

[0037]

[0038] Examples 5 to 7 Component b and a moisture absorbent shown in Table 2 were mixed in the ratio (parts by mass) shown in Table 2, and then lumps were obtained in the same manner as in Example 1. The lumps obtained were 1 x is 25 mm, b x is 25 mm, t x The average volume of the aggregates was 2454 mm 3 As in Example 1, the minimum temperature (°C) and the time (minutes) required for the temperature to return to 18°C ​​were measured. In addition, the difference Δ (°C) in the minimum temperature compared to Example 1 was calculated.

[0039] Comparative Examples 5 to 7 Component a (powder) and component b (powder) shown in Table 2 were mixed, and if necessary, a moisture absorbent (powder) in the proportions (parts by mass) shown in Table 2. The minimum temperature (°C) and the time (minutes) required to return to 18°C ​​were measured in the same manner as in Example 1. The difference Δ (°C) in the minimum temperature compared to Comparative Example 1 was also calculated.

[0040]

[0041] Examples 8 to 11 Component b and a moisture absorbent shown in Table 3 were mixed in the ratio (parts by mass) shown in Table 3, homogenized, and then treated in the same manner as in Example 1 to obtain lumps. x is 25 mm, b x is 25 mm, t x The average volume of the aggregates was 2454 mm 3 As in Example 1, the minimum temperature (°C) and the time (minutes) until the temperature returned to 18°C ​​were measured. For Examples 9 to 11, the difference Δ (°C) in the minimum temperature compared to Example 8 was calculated. Note that #N / A indicates that the minimum temperature did not fall below 18°C.

[0042] Comparative Examples 8 to 11 Component a (powder) and component b (powder) shown in Table 3, and optionally a moisture absorbent (powder), were mixed in the proportions (parts by mass) shown in Table 3 and homogenized. As in Example 1, the minimum temperature (°C) and the time (minutes) required to return to 18°C ​​were measured. For Comparative Examples 9 to 11, the difference Δ (°C) in the minimum temperature compared to Comparative Example 8 was calculated.

[0043]

[0044] Examples 12 to 15 Component b and a moisture absorbent shown in Table 4 were mixed in the ratio (parts by mass) shown in Table 4, homogenized, and then treated in the same manner as in Example 1 to obtain lumps. x is 25 mm, b x is 25 mm, t x The average volume of the aggregates was 2454 mm 3 The minimum temperature (°C) and the time (minutes) required to return to 18°C ​​were measured in the same manner as in Example 1. For Examples 13 to 15, the difference Δ (°C) in the minimum temperature compared to Example 12 was calculated.

[0045] Comparative Examples 12 to 15 Component a (powder) and component b (powder) shown in Table 4, and optionally a moisture absorbent (powder), were mixed in the proportions (parts by mass) shown in Table 4 and homogenized. The minimum temperature (°C) and the time (minutes) required to return to 18°C ​​were measured in the same manner as in Example 1. Furthermore, for Comparative Examples 13 to 15, the difference Δ (°C) in the minimum temperature compared to Comparative Example 12 was calculated.

[0046]

[0047] Examples 16 to 19 The lumps obtained in Example 3 (lumps of component b and moisture absorbent) were crushed to the sizes (l) shown in Table 5. x , b x , t x As in Example 1, the minimum temperature (°C) and the time (minutes) required for the temperature to return to 18°C ​​were measured. In addition, the difference Δ (°C) in the minimum temperature for Examples 16 to 19 and Example 3 compared to Comparative Example 3 was calculated.

[0048]

[0049] Examples 20 to 22 and Comparative Examples 16 to 18 The same procedures as in Example 1 were carried out except that the amounts of component a, component b, and moisture absorbent, and the size of the aggregates were changed as shown in Table 6. As in Example 1, the minimum temperature (°C) and the time (minutes) required to return to 18°C ​​were measured.

[0050]

[0051] Examples 23 and 24 Component a shown in Table 7 was mixed in a molding machine at 415 kgf / cm 2 The pressure is 1 x is 25 mm, b x is 25 mm, t x The average volume of the aggregates was 4909 mm. 3 The component b (powder) and moisture absorbent shown in Table 7 were blended with the obtained lump in the proportions shown in Table 7, and the minimum cooling temperature (°C) was measured in the same manner as in Example 1. The time (minutes) required for the temperature to return to 18°C ​​after blending component b and the moisture absorbent and dropping to below 18°C ​​was also measured in the same manner as in Example 1. The difference Δ (°C) in the minimum temperature compared to Comparative Example 1 was also calculated.

[0052]

[0053] As is clear from the above results, the coolant of the present invention was able to cool moderately without being too cold by forming at least one of solid A and solid B into a mass of a predetermined size. Furthermore, when a moisture absorbent was added, the moisture absorbent absorbed water and was able to suppress the acceleration of the endothermic reaction. It was presumed that this was because the moisture absorbent absorbed the moisture generated in the endothermic reaction, thereby suppressing the acceleration of the reaction. Another advantage of the coolant of the present invention is that it can be produced using only highly safe compounds.

Claims

1. A substance comprising solid A and solid B, wherein said solid A and said solid B contain compounds which undergo an endothermic reaction when in contact with each other, and at least one of said solids A and B is a lump, and when said lump is thrown onto a horizontal plane and each lump is observed in the most stable stationary state from a direction perpendicular to the horizontal plane, the outline (projected image) of the lump is sandwiched between two parallel lines tangent to the same and the smallest gap between them is defined as the minor axis diameter (b), and the average value (b) of the values ​​excluding the top 10% and bottom 10% of the lengths of (b) is obtained. x ) is 1 mm to 100 mm.

2. The coolant of claim 1, wherein said solid A comprises a hydrate and said solid B comprises a hydrate dissociator.

3. The coolant according to claim 1 or 2, wherein said solid A comprises a hydrate of an inorganic substance, and said solid B comprises at least one selected from a polybasic acid, a metal salt of a polybasic acid, and an inorganic ammonium salt.

4. The coolant according to claim 1 or 2, wherein said solid A includes an inorganic hydrate, and said solid B includes at least one selected from the group consisting of adipic acid, oxalic acid, succinic acid, malic acid, acetic acid, tartaric acid, fumaric acid, and citric acid, and metal salts thereof.

5. The coolant according to any one of claims 1 to 4, wherein said solid B is a lump.

6. The coolant of claim 5, wherein said solid B comprises a moisture absorbent.

7. The coolant of any one of claims 1 to 6, further comprising a moisture absorbing agent.

8. The cooling agent according to claim 6 or 7, wherein the moisture absorbent is at least one selected from the group consisting of starch, lactose, and cellulose.

9. The coolant according to any one of claims 1 to 8, wherein said solid A and said solid B are in a non-contact state until use.

10. The average value (l) of the major axis diameter (l) of the length of the agglomerate excluding the top 10% and bottom 10% of the length (l) when the distance between the agglomerates measured in the direction perpendicular to the minor axis diameter (b) is the major axis diameter (l) of the agglomerate x ) and the average value (b x ) is the ratio of (l x) / (b x 10. The coolant according to claim 1, wherein Mn is 1 to 50.

11. A method for producing a coolant comprising: solid A and solid B, said solid A and solid B containing compounds which undergo an endothermic reaction when in contact with each other; and forming at least one of said solid A and solid B into a block.

12. A method for producing a coolant according to claim 11, wherein the coolant is a coolant according to any one of claims 1 to 10.

Citation Information

Patent Citations

  • Ammonium nitrate molding and coolant

    JP1996295508A

  • Xanthene-based compound, resin composition, and color filter

    JP2025155486A

  • Portable ice bag with immediate effect

    JP1984155486A

  • cooling bag

    JP1995026671U

  • Powder mixture for coolant, and coolant

    JP2013116947A