Secondary battery

The secondary battery incorporates a recessed design on the electrode body's surface to mitigate stress concentration and tape edge damage, ensuring the structural integrity and performance of the battery during charging and discharging.

WO2024225089A1PCT designated stage expired Publication Date: 2024-10-31PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/014919
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-26
Filing Date
2024-04-15
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Secondary batteries with wound-type electrode bodies face damage due to stress concentration at the edge of the winding tape as the electrode body expands and contracts during charging and discharging, leading to potential wrinkles and structural issues.

Method used

A secondary battery design featuring a wound electrode body with a tape attached to its outer surface, where a recess is formed on the electrode body's surface to alleviate stress concentration, and the tape is strategically positioned to fix the winding end, reducing the likelihood of damage.

Benefits of technology

The recessed design effectively reduces stress on the tape edges and minimizes damage to the electrode body, preventing wrinkles and maintaining the structural integrity of the battery during charge and discharge cycles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024014919_31102024_PF_FP_ABST
    Figure JP2024014919_31102024_PF_FP_ABST
Patent Text Reader

Abstract

A cylindrical battery, which is an example of the embodiment of the present invention, is provided with an electrode body in which a positive electrode (11) that comprises a positive electrode mixture layer (31) and a negative electrode (12) that comprises a negative electrode mixture layer (41) are wound together with a separator being interposed therebetween. A tape (50) for affixing a winding termination end (14x) is adhered to an outer peripheral surface (14s) of the electrode body. An outer peripheral surface (31s) of the positive electrode mixture layer (31) is provided with a recess (35) in a region that overlaps with the tape (50) in the radial direction of the electrode body.
Need to check novelty before this filing date? Find Prior Art

Description

secondary battery

[0001] The present disclosure relates to a secondary battery, and more particularly to a secondary battery including an electrode assembly having a wound structure.

[0002] Conventionally, secondary batteries including a wound electrode assembly in which a positive electrode and a negative electrode are spirally wound with a separator interposed therebetween have been widely known. Generally, a stop tape is attached to the outer periphery of the wound electrode assembly to maintain the wound structure (see, for example, Patent Document 1).

[0003] JP 2009-199974 A

[0004] In secondary batteries such as lithium-ion batteries, a wound electrode body expands and contracts with charge and discharge, but if a stop tape is attached to the outer peripheral surface of the electrode body, stress caused by the expansion of the electrode body may concentrate at the edge of the tape, causing damage to the electrode body. For example, when the volume of the electrode body changes with charge and discharge of the battery, stress may concentrate at the edge of the tape, causing wrinkles in the electrodes that make up the outer peripheral surface of the electrode body.

[0005] The secondary battery according to the present disclosure is a secondary battery comprising an electrode body in which an electrode including a composite layer is wound via a separator, and is characterized in that tape is attached to the outer surface of the electrode body to fix the end of the winding, and a recess is formed on the outer surface of the composite layer in an area where the tape and the electrode body overlap radially.

[0006] According to the secondary battery according to the present disclosure, it is possible to reduce stress concentrated on the edge portion of the winding stop tape, and to suppress damage to the electrode body.

[0007] Fig. 3 is an axial cross-sectional view of a cylindrical battery that is an example of an embodiment; Fig. 4 is a perspective view of an electrode body that is an example of an embodiment; Fig. 5 is a diagram showing a positive electrode and a negative electrode that are an example of an embodiment; Fig. 6 is a cross-sectional view taken along line AA in Fig. 3; Fig. 7 is a diagram showing a modified example of a positive electrode; Fig. 8 is a diagram showing a modified example of a positive electrode.

[0008] Hereinafter, an example of an embodiment of a secondary battery according to the present disclosure will be described in detail with reference to the drawings. The embodiment described below is merely an example, and the present disclosure is not limited to the following embodiment. Furthermore, the present disclosure also includes embodiments obtained by selectively combining the components of the embodiments described below.

[0009] In the following, a cylindrical battery 10 having a cylindrical outer can 16 with a bottom is illustrated as an example of an embodiment of a secondary battery according to the present disclosure, but the battery exterior body is not limited to a cylindrical outer can. The secondary battery according to the present disclosure may be, for example, a prismatic battery having a prismatic outer can, or a pouch-type battery having an exterior body made of a laminate sheet including a metal layer and a resin layer.

[0010] FIG. 1 is a schematic diagram illustrating an axial cross section of a cylindrical battery 10 according to an embodiment. Note that the tape 50 is not shown in FIG. 1 . As shown in FIG. 1 , the cylindrical battery 10 includes a wound electrode assembly 14, an electrolyte, and a bottomed cylindrical outer can 16 that accommodates the electrode assembly 14 and the electrolyte. The electrode assembly 14 includes a positive electrode 11, a negative electrode 12, and a separator 13, and is configured such that the positive electrode 11 and the negative electrode 12 are spirally wound with the separator 13 interposed therebetween. The outer can 16 is a bottomed cylindrical metal container that is open on one axial side, and the opening of the outer can 16 is closed by a sealing member 17. Hereinafter, for convenience of explanation, the sealing member 17 side of the cylindrical battery 10 is referred to as the top, and the bottom side of the outer can 16 is referred to as the bottom.

[0011] The electrolyte may be an aqueous electrolyte, but in this embodiment, a non-aqueous electrolyte is used. The non-aqueous electrolyte has lithium ion conductivity. The non-aqueous electrolyte may be a liquid electrolyte (electrolytic solution) or a solid electrolyte. The cylindrical battery 10 is, for example, a non-aqueous electrolyte secondary battery, and preferably a lithium ion battery.

[0012] The liquid electrolyte (electrolytic solution) contains a non-aqueous solvent and an electrolyte salt dissolved in the non-aqueous solvent. Examples of the non-aqueous solvent include esters, ethers, nitriles, amides, and mixed solvents of two or more of these. Examples of the non-aqueous solvent include ethylene carbonate (EC), ethyl methyl carbonate (EMC), dimethyl carbonate (DMC), diethyl carbonate (DEC), and mixed solvents of these. The non-aqueous solvent may contain a halogen-substituted compound (e.g., fluoroethylene carbonate) in which at least a portion of the hydrogen atoms of these solvents are substituted with halogen atoms such as fluorine. Examples of the electrolyte salt include LiPF 6 Lithium salts such as

[0013] As the solid electrolyte, for example, a solid or gel-like polymer electrolyte, an inorganic solid electrolyte, etc. can be used. As the inorganic solid electrolyte, a material known in all-solid-state lithium ion secondary batteries, etc. (for example, an oxide-based solid electrolyte, a sulfide-based solid electrolyte, a halogen-based solid electrolyte, etc.) can be used. The polymer electrolyte includes, for example, a lithium salt and a matrix polymer, or a non-aqueous solvent, a lithium salt, and a matrix polymer. As the matrix polymer, for example, a polymer material that absorbs a non-aqueous solvent and gels is used. As the polymer material, for example, a fluororesin, an acrylic resin, a polyether resin, etc. can be used.

[0014] The positive electrode 11, negative electrode 12, and separator 13 that make up the electrode assembly 14 are all long, strip-like bodies that are spirally wound and alternately stacked in the radial direction of the electrode assembly 14. The negative electrode 12 is formed to be slightly larger than the positive electrode 11 to prevent lithium deposition. That is, the negative electrode 12 is formed to be longer in the length direction and width direction (short direction) than the positive electrode 11. The separator 13 is formed to be at least slightly larger than the positive electrode 11, and two separators 13 are arranged to sandwich the positive electrode 11. The cylindrical battery 10 includes insulating plates 18 and 19 arranged above and below the electrode assembly 14, respectively.

[0015] The electrode body 14 has a positive electrode lead 20 connected to the positive electrode 11 by welding or the like, and a negative electrode lead 21 connected to the negative electrode 12 by welding or the like. In this embodiment, the positive electrode lead 20 is connected to the center of the positive electrode 11 in the longitudinal direction, and the negative electrode lead 21 is connected to the end of the negative electrode 12 in the longitudinal direction that is located on the winding core side of the electrode body 14.

[0016] The positive electrode 11 includes a positive electrode core 30 and a positive electrode mixture layer 31 formed on the positive electrode core 30. The positive electrode core 30 can be a foil of a metal, such as aluminum or an aluminum alloy, that is stable within the potential range of the positive electrode 11, or a film having such a metal disposed on its surface. The positive electrode mixture layer 31 contains a positive electrode active material, a conductive agent, and a binder, and is preferably formed on both sides of the positive electrode core 30 except for the portion to which the positive electrode lead 20 is welded. The positive electrode 11 can be produced, for example, by applying a positive electrode mixture slurry containing a positive electrode active material, a conductive agent, a binder, etc. to the positive electrode core 30, drying the coating, and then compressing it to form the positive electrode mixture layer 31 on both sides of the positive electrode core 30. An example thickness of the positive electrode mixture layer 31 is 60 μm to 100 μm on one side of the positive electrode core 30.

[0017] The positive electrode mixture layer 31 generally contains particulate lithium metal composite oxide as the positive electrode active material. The lithium metal composite oxide is a composite oxide containing metal elements such as Co, Mn, Ni, and Al in addition to Li. The metal element constituting the lithium metal composite oxide is, for example, at least one selected from Mg, Al, Ca, Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Ge, Y, Zr, Sn, Sb, W, Pb, and Bi. Among these, it is preferable to contain at least one selected from Co, Ni, and Mn. Examples of suitable composite oxides include lithium metal composite oxides containing Ni, Co, and Mn, and lithium metal composite oxides containing Ni, Co, and Al.

[0018] The negative electrode 12 includes a negative electrode core 40 and a negative electrode mixture layer 41 formed on the negative electrode core 40. The negative electrode core 40 can be a foil of a metal, such as copper or a copper alloy, that is stable within the potential range of the negative electrode 12, or a film having such a metal disposed on its surface. The negative electrode mixture layer 41 contains a negative electrode active material, a binder, and, if necessary, a conductive agent, and is preferably formed on both sides of the negative electrode core 40, excluding the exposed portion 42 (described below) and the portion to which the negative electrode lead 21 is welded. The negative electrode 12 can be produced by applying a negative electrode mixture slurry containing a negative electrode active material and a binder to the surface of the negative electrode core 40, drying the coating, and then compressing it to form the negative electrode mixture layer 41 on both sides of the negative electrode core 40. The thickness of the negative electrode mixture layer 41 is, for example, 60 μm to 100 μm on one side of the negative electrode core 40.

[0019] The negative electrode mixture layer 41 generally contains, as the negative electrode active material, a carbon material that reversibly absorbs and releases lithium ions. A suitable example of the carbon material is graphite, such as natural graphite or artificial graphite. Alternatively, the negative electrode active material may be a material containing at least one of an element that alloys with Li, such as Si or Sn, and a material containing such an element. Among these, a composite material containing Si is preferred. A suitable Si-containing composite material is a composite particle containing an ion-conducting phase and a Si phase dispersed in the ion-conducting phase. A carbon material and a Si-containing composite material may be used together as the negative electrode active material, which is preferable from the viewpoint of achieving both high capacity and high durability of the battery.

[0020] A porous sheet having ion permeability and insulating properties is used for the separator 13. Specific examples of the porous sheet include a microporous thin film, a woven fabric, and a nonwoven fabric. Suitable materials for the separator 13 include polyolefins such as polyethylene and polypropylene, and cellulose. The separator 13 may have a single-layer structure or a multi-layer structure. A highly heat-resistant resin layer such as an aramid resin may be formed on the surface of the separator 13. A filler layer containing an inorganic filler may be formed at the interface between the separator 13 and at least one of the positive electrode 11 and the negative electrode 12.

[0021] The negative electrode 12 is disposed on the outer peripheral surface of the electrode body 14, and an exposed portion 42 is formed in which the surface of the negative electrode core 40 is exposed. The exposed portion 42 may be formed on a portion of the outer peripheral surface of the electrode body 14, but is preferably formed on the entire outer peripheral surface. The exposed portion 42 may be formed on only one side (outer surface) of the negative electrode core 40 facing outward from the electrode body 14, or may be formed on both sides of the negative electrode core 40. The exposed portion 42 is formed, for example, within a range of a length equivalent to one to two revolutions around the circumference of the electrode body 14 from the longitudinal end of the negative electrode 12 located on the outer peripheral surface of the electrode body 14.

[0022] In the cylindrical battery 10, the exposed portion 42 of the negative electrode 12 contacts the inner surface of the exterior can 16, and the negative electrode lead 21 is connected by welding or the like to the inner bottom surface of the exterior can 16. For example, the exposed portion 42 contacts the inner surface of the exterior can 16 along the entire outer periphery of the electrode body 14. The positive electrode lead 20 passes through the through hole in the insulating plate 18 and extends toward the sealing body 17, and is connected by welding or the like to the underside of the internal terminal plate 23, which is the bottom plate of the sealing body 17. Therefore, in this embodiment, the sealing body 17 serves as a positive electrode external terminal, and the exterior can 16 serves as a negative electrode external terminal.

[0023] As described above, the outer can 16 is a cylindrical metal container with a bottom and an opening on one axial side. A gasket 28 is provided between the outer can 16 and the sealing body 17 to ensure sealing of the battery interior and insulation between the outer can 16 and the sealing body 17. The outer can 16 has a groove 22 formed by a portion of the side surface protruding inward. The groove 22 is preferably formed in an annular shape along the circumferential direction of the outer can 16, and supports the sealing body 17 on its top surface. The sealing body 17 is fixed to the top of the outer can 16 by the groove 22 and the open end of the outer can 16, which is crimped to the sealing body 17.

[0024] The sealing body 17 has a structure in which, in order from the electrode body 14 side, an internal terminal plate 23, a lower valve body 24, an insulating member 25, an upper valve body 26, and a cap 27 are stacked. Each member constituting the sealing body 17 has, for example, a disk or ring shape, and each member except for the insulating member 25 is electrically connected to one another. The lower valve body 24 and the upper valve body 26 are connected at their respective centers, and the insulating member 25 is interposed between their respective peripheral edges. If an abnormality occurs in the battery and the internal pressure increases, the lower valve body 24 deforms and breaks, pushing the upper valve body 26 toward the cap 27, thereby interrupting the current path between the lower valve body 24 and the upper valve body 26. If the internal pressure further increases, the upper valve body 26 breaks, and gas is discharged from the opening of the cap 27.

[0025] FIG. 2 is a perspective view of the electrode assembly 14. As shown in FIG. 2, tape 50 is attached to the outer peripheral surface 14s of the electrode assembly 14. The tape 50 is a stop tape that secures the winding end 14x of the electrode assembly 14 and maintains the wound structure of the electrode assembly 14. In this embodiment, the outer peripheral surface 14s of the electrode assembly 14 is formed by the exposed portion 42 of the negative electrode 12, and the winding end side end 12x of the negative electrode 12 forms the winding end 14x of the electrode assembly 14. The tape 50 is attached to the outer peripheral surface 14s (exposed portion 42) of the electrode assembly 14 so as to straddle the winding end 14x, and secures the winding end 14x of the outer peripheral surface 14s to a portion located inside the winding.

[0026] Two strip-shaped tapes 50 are attached to the outer peripheral surface 14s of the electrode body 14. The two tapes 50 are preferably arranged so that their respective length directions are aligned with the circumferential direction of the electrode body 14 and are spaced apart from each other in the axial direction of the electrode body 14. One tape 50 is attached to the upper end (one axial end) of the electrode body 14, and the other tape 50 is attached to the lower end (the other axial end) of the electrode body 14. In this case, the wound structure of the electrode body 14 is stably maintained. Furthermore, the axial end of the electrode body 14 is prevented from hitting the edge of the outer can 16 and being turned over, making it easier to fit the electrode body 14 into the outer can 16.

[0027] The tape 50 has a length that is, for example, 50% or more of the circumferential length of the outer peripheral surface 14s of the electrode body 14, and is attached across the winding end 14x. Note that if the length of the tape 50 exceeds 100% of the circumferential length of the outer peripheral surface 14s, the tapes 50 will overlap, so the length is preferably 100% or less of the circumferential length of the outer peripheral surface 14s. The lengths of the two tapes 50 may be different from each other, but in this embodiment they are substantially the same.

[0028] The tape 50 has a width equivalent to, for example, 5% to 25% of the axial length of the electrode body 14. The widths of the two tapes 50 may be different from each other, but in this embodiment they are substantially the same. The tape 50 is attached to the outer peripheral surface 14s with a predetermined gap (for example, 1 mm or less) between the upper and lower ends to allow for attachment error. The width of the tape 50 is, for example, substantially constant over the entire length.

[0029] The tape 50 includes a tape substrate and an adhesive layer provided on one side of the tape substrate. The tape 50 is, for example, an insulating tape that is substantially non-conductive. The tape substrate is composed of a single-layer or multi-layer resin substrate. The tape 50 may contain an inorganic filler such as titania, alumina, silica, or zirconia, and may have a layer containing an inorganic filler provided in addition to the tape substrate and the adhesive layer.

[0030] Examples of resins constituting the tape substrate include polyesters such as polyethylene terephthalate (PET), polypropylene (PP), polyimide (PI), polyphenylene sulfide (PPS), polyetherimide (PEI), polyamide, etc. The adhesive layer is formed, for example, by applying an adhesive to one surface of the tape substrate.

[0031] The adhesive constituting the adhesive layer may be a hot-melt type that exhibits adhesiveness when heated or a thermosetting type that hardens when heated, but is preferably one that has adhesiveness at room temperature from the viewpoint of productivity, etc. Examples of adhesives constituting the adhesive layer include acrylic adhesives and synthetic rubber adhesives.

[0032] The thickness of the tape 50 is, for example, 15 μm to 90 μm, preferably 25 μm to 70 μm. The thickness of the tape substrate is greater than the thickness of the adhesive layer, for example, 20 μm to 65 μm. The thickness of the adhesive layer is, for example, 10 μm to 30 μm.

[0033] Fig. 3 is a diagram showing the positive electrode 11 and the negative electrode 12 in a developed state, and mainly shows the outer winding surfaces 31a, 41a of each electrode facing radially outward from the electrode assembly 14. Fig. 4 is a cross-sectional view taken along line AA in Fig. 3. As shown in Figs. 3 and 4, a recess 35 is formed on the outer peripheral surface 31s of the positive electrode mixture layer 31 in a region where the tape 50 and the electrode assembly 14 overlap in the radial direction. Similarly, a recess 45 is formed on the outer peripheral surface 41s of the negative electrode mixture layer 41 in a region where the tape 50 and the electrode assembly 14 overlap in the radial direction. Here, the outer peripheral surfaces 31s, 41s of each mixture layer refer to the surfaces located radially outward of the outer winding surfaces 31a, 41a facing outward from the electrode assembly 14.

[0034] In this embodiment, the exposed portion 42 of the negative electrode 12 is formed to be slightly longer than the circumferential length of the outer peripheral surface 14s of the electrode body 14. Therefore, the winding end 41x of the outer winding surface 41a of the negative electrode mixture layer 41 is located two turns from the winding end 12x of the negative electrode 12. On the other hand, the winding end 41x of the inner winding surface 41b is located closer to the winding end 12x of the negative electrode 12 than the winding end 41x of the outer winding surface 41a. The winding end of the positive electrode 11 and the winding end 31x of the positive electrode mixture layer 31 are aligned.

[0035] As described above, the tape 50 is attached to the outer peripheral surface 14s of the electrode assembly 14 across the winding end 14x of the electrode assembly 14, and therefore, when the negative electrode 12 is unfolded, it extends in the longitudinal direction from the winding end 12x of the negative electrode 12. In Figure 3, the region of the outer peripheral surface 14s where the portion of the tape 50 extending from the winding end 12x is attached is shown by a virtual line. In the example shown in Figure 3, the length of the tape 50 is slightly shorter than the perimeter of the outer peripheral surface 14s, so there is a gap between both ends of the tape 50 in the longitudinal direction.

[0036] The recesses 35, 45 are depressions formed in each mixture layer, and the thickness of the mixture layer is thinner in the areas where the recesses 35, 45 are formed. The recesses 35, 45 absorb the thickness of the tape 50 and reduce the volume change that occurs with charging and discharging in the area that radially overlaps with the tape 50. This is thought to alleviate stress acting on the edge portion of the tape 50 and effectively suppress damage to the electrode body 14. As will be described in more detail below, the recesses 35, 45 are preferably slightly larger than the area that radially overlaps with the tape 50 and the electrode body 14.

[0037] The recesses 35, 45 may also be formed in regions of the outer winding surfaces 31a, 41a of each mixture layer other than the outer peripheral surfaces 31s, 41s, or may be formed on the inner winding surfaces 31b, 41b. In this embodiment, the recesses 35 are slightly longer than the circumferential length of the outer peripheral surface 31s and are formed from the winding end 31x beyond the outer peripheral surface 31s to the second turn. Similarly, the recesses 45 are slightly longer than the circumferential length of the outer peripheral surface 41s and are formed from the winding end 41x beyond the outer peripheral surface 41s to the second turn. In addition, recesses 35 are also formed on the inner winding surface 31b of the positive electrode mixture layer 31.

[0038] When a recess 45 is formed on the outer winding surface 41a of the negative electrode mixture layer 41, it is preferable to also form a recess 35 on the inner winding surface 31b of the positive electrode mixture layer 31 that faces the recess 45 with the separator 13 interposed therebetween. The recess 35 on the inner winding surface 31b is formed from the perspective of suppressing lithium precipitation rather than suppressing damage to the electrode body 14. In the example shown in Figures 3 and 4, recesses 35 are formed on both the outer winding surface 31a and the inner winding surface 31b of the positive electrode mixture layer 31. The recesses 35 on each surface are formed so as to overlap in the thickness direction of the positive electrode 11.

[0039] The recess 35 has a depth D that is equal to or greater than the thickness of the tape 50. 35 In this case, it is easy to absorb the thickness of the tape 50, and the effect of suppressing damage to the electrode body 14 is improved. In this embodiment, the depth, width, length, etc. of the recess 45 are the same as those of the recess 35, so the following description will be given taking the recess 35 as an example regarding the contents common to the recesses 35 and 45. Depth D of the recess 35 35 is equal to or greater than the thickness of the tape 50, and the thickness D of the positive electrode mixture layer 31 31The depth D is preferably 1.0 to 1.2 times the thickness of the tape 50. 35 A suitable example of the thickness is 30 μm or more and 80 μm or less.

[0040] The thickness of the positive electrode mixture layer 31 at the bottom of the recess 35 is thinner than that of other regions of the positive electrode mixture layer 31 where the recess 35 is not formed (hereinafter referred to as "first regions"). Hereinafter, the thin-walled regions formed at the bottom of the recess 35 are referred to as "second regions" of the positive electrode mixture layer 31. In this embodiment, the second regions are formed only on the outer peripheral surface 31s (first turn) of the positive electrode mixture layer 31 and on a part of the second turn of the positive electrode mixture layer 31 adjacent to the outer peripheral surface 31s, and the other regions are the first regions. In addition, the second regions formed at the bottom of the recess 35 have substantially the same density as the first region.

[0041] The density of the positive electrode mixture layer 31 is substantially the same throughout its entire region, and is, for example, 3.3 g / cc or more and 4.0 g / cc or less. The adhesion strength of the second region to the positive electrode core 30 is also substantially the same as the adhesion strength of the first region. The adhesion strength of the positive electrode mixture layer 31 to the positive electrode core 30 can be evaluated by peel strength. Therefore, it can be said that the peel strength of the positive electrode mixture layer 31 is substantially the same throughout its entire region.

[0042] The recesses 35 are formed closer to both widthwise ends of the positive electrode mixture layer 31 than the widthwise center. That is, the recesses 35 are formed in two locations spaced apart in the widthwise direction of the positive electrode mixture layer 31. In other words, a first region of the positive electrode mixture layer 31 is formed between the two recesses 35. The tape 50 is attached to both axial end portions of the electrode body 14, and the widthwise center portion of the positive electrode mixture layer 31 is a region that does not overlap with the tape 50. Therefore, by designating this region as the first region, it is possible to minimize capacity reduction. In this embodiment, first regions are also formed between each recess 35 and both widthwise ends of the positive electrode mixture layer 31.

[0043] The recess 35 is preferably formed in a groove shape extending in the longitudinal direction of the positive electrode 11. The two recesses 35 are arranged parallel to each other and have substantially the same length L 35 , the same width W 35 , the same depth D 35In this embodiment, since there is an area in the circumferential center of the outer peripheral surface 14s of the electrode body 14 where the tape 50 is not attached, the recess 35 may be divided in the longitudinal direction of the positive electrode 11, but considering misalignment with the tape 50, it is preferable that the recess 35 is formed continuously. The recess 35 is formed continuously from the winding end side end 31x across the range of the outer peripheral surface 31s to the end in the longitudinal direction on the winding start side. The length L of the recess 35 35 is longer than the length of the tape 50 , and a suitable example is 1.1 times or more and 1.5 times or less the length of the tape 50 .

[0044] Width W of the recess 35 35 is the width W of the tape 50 50 The width W of the recess 35 is preferably larger than 35 is, for example, the width W of the tape 50, taking into consideration the positional deviation with respect to the tape 50. 50 The width W of the recess 35 is set to be 1.1 times or more. 35 An example of the upper limit of the width W of the tape 50 50 By forming the recess 35 in the minimum necessary range, it is possible to ensure high capacity while efficiently suppressing damage to the electrode body 14. The recess 35 has a constant width and depth over its entire length.

[0045] The method for forming the recesses 35 is not particularly limited, but one example is a method in which a positive electrode mixture slurry is applied to the positive electrode core 30 to form a positive electrode mixture layer 31 with a certain thickness, and then a portion of the positive electrode mixture layer 31 is removed. The positive electrode mixture layer 31 can be removed, for example, by laser ablation. Laser ablation is a processing method in which a target object is irradiated with high-power laser light to melt and sublimate the constituent materials, thereby removing them. The recesses 35 can be formed by irradiating a desired location on the surface of the positive electrode mixture layer 31 with high-power laser light to remove a portion of the positive electrode mixture layer 31.

[0046] 5 and 6 are cross-sectional views showing modified examples of the positive electrode 11. As shown in FIG. 5, the recesses 35 may be formed only on the outer winding surface 31 a of the positive electrode mixture layer 31. When the recesses 35 are formed on the outer winding surface 31 a, particularly on the outer peripheral surface 31 s, the effect of suppressing damage to the electrode body 14 becomes more pronounced. If the recesses 35 are formed over an excessively wide range, the capacity decreases. Therefore, forming the recesses 35 only on the outer winding surface 31 a is preferable from the perspective of efficiently suppressing damage to the electrode body 14 while ensuring high capacity. The recesses 35 may be formed only on the outer peripheral surface 31 s of the positive electrode mixture layer 31.

[0047] When the recesses 35 are formed only on the outer winding surface 31a of the positive electrode mixture layer 31, it is preferable not to form recesses 45 in the negative electrode mixture layer 41, from the viewpoint of suppressing lithium precipitation. As described above, the recesses 45 are formed in pairs with the recesses 35 on the inner winding surface 31b of the positive electrode mixture layer 31. Furthermore, when the electrode body 14 has both the recesses 35 and 45, the recesses 45 may be formed shallower than the recesses 35. In this case, the depth of the recesses 35 may differ between the outer winding surface 31a and the inner winding surface 31b, or the depth of the recesses 35 on the outer winding surface 31a may be greater than the depth of the recesses 35 on the inner winding surface 31b.

[0048] As shown in Fig. 6 , the recess 35 may be formed in a tapered shape with the groove width gradually narrowing toward the bottom (groove bottom) of the recess 35. In the examples shown in Figs. 4 and 5 , the groove wall along the length direction of the recess 35 is formed substantially perpendicular to the surface of the positive electrode core 30. However, in the example shown in Fig. 6 , the groove wall forms an inclined surface 36 that is inclined at a predetermined angle with respect to the normal direction of the surface of the positive electrode core 30. The predetermined angle is, for example, 30° or more and 70° or less. By forming the recess 35 in a tapered shape, the tape 50 can be easily introduced into the recess 35, facilitating alignment and improving the effect of suppressing damage to the electrode body 14.

[0049] The slope 36 of the recess 35 may be formed on only one side in the width direction of the recess 35, but is preferably formed on both sides in the width direction. The groove bottom of the recess 35 is formed flat so as to fit along the surface of the positive electrode substrate 30, and the interval between the slopes 36 along the width direction of the positive electrode mixture layer 31 is set to be equal to or larger than the width W of the tape 50. 50 It is set to the above.

[0050] As described above, the cylindrical battery 10 with the above configuration is believed to be able to alleviate stress concentration at the edge of the winding tape 50, effectively suppressing damage to the electrode body 14. When the tape 50 is attached to the outer peripheral surface 14s of the electrode body 14, stress tends to concentrate at the edge of the tape 50 when the volume of the electrode body 14 changes as the battery is charged and discharged. In conventional secondary batteries, for example, wrinkles may occur in the electrodes that make up the outer peripheral surface 14s. In the cylindrical battery 10, wrinkles are less likely to occur in the electrodes, and damage to the electrode body 14 is sufficiently suppressed.

[0051] For example, in the above embodiment, the outer peripheral surface 14 s of the electrode body 14 is the exposed portion 42 of the negative electrode 12, but the outer peripheral surface 14 s may be the separator 13.

[0052] The present disclosure will be further described by the following embodiments. Aspect 1: A secondary battery including an electrode assembly in which an electrode including a mixture layer is wound with a separator interposed therebetween, wherein a tape is attached to the outer peripheral surface of the electrode assembly to secure the winding end, and a recess is formed on the outer peripheral surface of the mixture layer in a region where the tape overlaps the electrode assembly in the radial direction. Aspect 2: A secondary battery according to Aspect 1, wherein the recess is formed to a depth equal to or greater than the thickness of the tape. Aspect 3: A secondary battery according to Aspect 1 or Aspect 2, wherein the recess is a groove extending in the length direction of the electrode and formed in a tapered shape with a groove width gradually narrowing toward the groove bottom. Aspect 4: A secondary battery according to any one of Aspects 1 to 3, wherein the mixture layer formed at the bottom of the recess has substantially the same density as the mixture layer formed in a region other than the recess. Aspect 5: A secondary battery according to any one of Aspects 1 to 4, wherein the electrode includes a positive electrode including a positive electrode mixture layer and a negative electrode including a negative electrode mixture layer, and the recess is formed in at least the positive electrode mixture layer.

[0053] 10 Cylindrical battery, 11 Positive electrode, 12 Negative electrode, 12x Winding end side end, 13 Separator, 14 Electrode body, 14s Outer circumferential surface, 14x Winding end side end, 16 Outer can, 17 Sealing body, 18, 19 Insulating plate, 20 Positive electrode lead, 21 Negative electrode lead, 22 Grooved portion, 23 Internal terminal plate, 24 Lower valve body, 25 Insulating member, 26 Upper valve body, 27 Cap, 28 Gasket, 30 Positive electrode core, 31 Positive electrode mixture layer, 31a Winding outer surface, 31b Winding inner surface, 31s Outer circumferential surface, 31x Winding end side end, 35 Recess, 36 Slope, 40 Negative electrode core, 41 Negative electrode mixture layer, 41a Winding outer surface, 41b Winding inner surface, 41s Outer circumferential surface, 41x Winding end side end, 42 Exposed portion, 45 Recessed portion, 50 Tape

Claims

1. A secondary battery comprising an electrode body in which an electrode including a composite layer is wound with a separator interposed therebetween, wherein a tape is attached to the outer peripheral surface of the electrode body to fix the end of the winding, and a recess is formed in the outer peripheral surface of the composite layer in an area where the tape and the electrode body overlap in the radial direction.

2. The secondary battery according to claim 1, wherein the recess is formed to a depth equal to or greater than the thickness of the tape.

3. The secondary battery according to claim 1, wherein the recess is a groove extending in the longitudinal direction of the electrode and formed in a tapered shape with the groove width gradually narrowing toward the bottom of the groove.

4. The secondary battery according to claim 1, wherein the mixture layer formed on the bottom of the recess has substantially the same density as the mixture layer formed in other areas other than the recess.

5. The secondary battery according to any one of claims 1 to 4, wherein the electrodes include a positive electrode including a positive electrode mixture layer and a negative electrode including a negative electrode mixture layer, and the recess is formed in at least the positive electrode mixture layer.

Citation Information

Patent Citations

  • Electrode group for nonaqueous secondary battery, and secondary battery using the same

    JP2009199974A

  • Wound type nonaqueous electrolyte secondary battery and method for manufacturing the same

    JP2014053241A

  • Non-aqueous electrolyte secondary battery and method for manufacturing non-aqueous electrolyte rechargeable battery

    JP2022079876A

  • Cylindrical battery

    JP2022152423A

  • Non-aqueous electrolyte secondary battery

    WO2021049471A1