Method for producing wiring structure

The method addresses the issue of excessive overburden in electrolytic plating by using a substrate with recesses of different widths and controlled metal plating layer deposition, reducing the need for excess material removal and improving the planarity of wiring structures.

WO2024228238A1PCT designated stage expired Publication Date: 2024-11-07RESONAC CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/017048
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-01
Publication Date
2024-11-07

AI Technical Summary

Technical Problem

The growth rate of metal plating layers by electrolytic plating tends to be higher in narrower openings, leading to excessive metal plating in wider openings and increased overburden that requires significant removal during planarization in multi-opening structures with varying widths.

Method used

A method involving a substrate with recesses of different widths, forming a temporary protective layer, and sequentially depositing metal plating layers to fill both wide and narrow openings while minimizing overburden, using electrolytic plating to form a conductor layer with controlled thickness and depression on the surface, allowing for efficient removal of excess material.

Benefits of technology

This method effectively reduces the amount of overburden that needs to be removed, resulting in a more efficient and planarized metal plating layer, enhancing the manufacturing process for wiring structures with varying opening widths.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023017048_07112024_PF_FP_ABST
    Figure JP2023017048_07112024_PF_FP_ABST
Patent Text Reader

Abstract

This method for producing a novel wiring structure includes forming a conductor layer by two-stage electrolytic plating on a substrate that has a main surface forming a first recess and a second recess and in which the minimum width of a first bottom surface is larger than the minimum width of a second bottom surface. The method additionally includes: forming a temporary protective layer that has a pattern including an opening in which at least part of the first bottom surface is exposed; forming a first metal plating layer on the first bottom surface; removing the temporary protective layer and exposing the second recess; and forming a conductor layer including the first metal plating layer and a second metal plating layer by forming a second metal plating layer that includes a portion filling the second recess and a portion provided on the first metal plating layer.
Need to check novelty before this filing date? Find Prior Art

Description

Method for manufacturing a wiring structure

[0001] The present disclosure relates to a method for manufacturing an interconnect structure.

[0002] In electronic component devices including semiconductor elements, a wiring structure including fine wiring such as a redistribution layer connected to the semiconductor elements is sometimes provided. The wiring structure may be formed by a damascene method including forming an electrolytic plating layer in an opening in an insulating layer (see, for example, Patent Document 1).

[0003] International Publication No. 2018 / 056466

[0004] The growth rate of a metal plating layer by electroplating tends to be faster in narrower openings. Therefore, when a metal plating layer is formed simultaneously in multiple openings of different widths by electroplating, if the metal plating layer is formed so as to fully fill the larger openings, the amount of excess metal plating layer (overburden) that protrudes from the narrower openings tends to be large. As a result, after the metal plating layer is formed, the amount of overburden that needs to be removed for purposes such as planarization of the metal plating layer may become large.

[0005] The present disclosure relates to a method for forming a metal plating layer while suppressing the amount of overburden that needs to be removed when forming a wiring structure by a method that includes forming a metal plating layer by electrolytic plating in multiple openings of different widths.

[0006] The present disclosure includes the following: [1] A method for manufacturing a substrate comprising: preparing a substrate having a main surface forming a first recess and a second recess, the first recess having a first bottom surface and a first wall surface, the second recess having a second bottom surface and a second wall surface, and a minimum width of the first bottom surface being greater than a minimum width of the second bottom surface; forming a temporary protective layer on the main surface of the substrate, the temporary protective layer having a pattern including an opening through which at least a portion of the first bottom surface is exposed, and including a portion that closes the second recess; forming a first metal plating layer on the first bottom surface exposed in the opening; removing the temporary protective layer to expose the second recess; forming a second metal plating layer including a portion that fills the second recess and a portion that is provided on the first metal plating layer, thereby forming a conductor layer that includes the first metal plating layer and the second metal plating layer; and removing a portion of the conductor layer, thereby forming a first conductor portion that is provided in the first recess and includes the first metal plating layer and the second metal plating layer, and a second conductor portion that is provided in the second recess and includes the second metal plating layer. A method for manufacturing a wiring structure, wherein the substrate comprises a seed layer having a surface including the first bottom surface and the second bottom surface, and the first metal plating layer and the second metal plating layer are formed by electrolytic plating. [2] The method according to [1], wherein the substrate further comprises an insulating layer having a pattern including an opening along the first wall surface and an opening along the second wall surface. [3] The method according to [1] or [2], wherein the first metal plating layer is formed so that a recess is formed in the surface of the first metal plating layer opposite the first bottom surface. [4] The method according to any one of [1] to [3], wherein forming the temporary protective layer comprises: providing a photosensitive resist layer on the main surface of the substrate; and patterning the photosensitive resist layer by exposure and development to form the temporary protective layer having the pattern. [5] The method according to [4], wherein the photosensitive resist layer comprises a binder polymer, a photopolymerizable compound having an ethylenically unsaturated bond, and a photopolymerization initiator.

[0007] When forming a wiring structure by a method that includes forming a metal plating layer by electrolytic plating in multiple openings of different widths, the metal plating layer can be formed while suppressing the amount of overburden that needs to be removed.

[0008] 1A and 1B are process diagrams showing an example of a method for manufacturing a wiring structure, respectively; FIG. 1C are process diagrams showing an example of a method for manufacturing a wiring structure, respectively; FIG. 1D are process diagrams showing an example of a method for manufacturing a wiring structure;

[0009] The present invention is not limited to the following examples.

[0010] 1, 2 and 3 are process diagrams showing an example of a method for manufacturing a wiring structure. The method shown in Figures 1 to 3 includes preparing a substrate 1 having a main surface S1 forming a first recess 11 having a first bottom surface 11a and a second recess 12 having a second bottom surface 12a; forming a temporary protective layer 7 on the main surface S1 of the substrate 1, the temporary protective layer 7 having a pattern including an opening 7a through which at least a portion of the first bottom surface 11a is exposed and including a portion that fills the second recess 12; forming a first metal plating layer 51 on the first bottom surface 11a exposed in the opening 7a; removing the temporary protective layer 7 to expose the second recess 12; forming a second metal plating layer 52 including a portion that fills the second recess 12 and a portion provided on the first metal plating layer 51, thereby forming a conductor layer 5 including the first metal plating layer 51 and the second metal plating layer 52; and removing a portion of the conductor layer 5, thereby forming a first conductor portion 5A provided in the first recess 11 and a second conductor portion 5B provided in the second recess 12. By this method, it is possible to form a wiring structure 50 including a circuit configured from the first conductor portion 5A and the second conductor portion 5B.

[0011] The first recess 11 formed by the main surface S1 of the substrate 1 has a first bottom surface 11a and a first wall surface 11b surrounding the first bottom surface 11a. The second recess 12 formed by the main surface S1 of the substrate 1 has a second bottom surface 12a and a second wall surface 12b surrounding the second bottom surface 12a. The minimum width W1 of the first bottom surface 11a is greater than the minimum width W2 of the second bottom surface 12a. The minimum width of a bottom surface having a longitudinal direction can be the minimum value of the width in a direction perpendicular to the longitudinal direction. The minimum width of a rectangular or approximately rectangular bottom surface is considered to be the length of its short side.

[0012] The ratio W1 / W2 of the minimum width of the first bottom surface 11a to the minimum width W2 of the second bottom surface 12a may be 3 to 100, 5 to 500, or 20 to 1000. The minimum width W1 of the first bottom surface 11a may be 10 μm to 200 μm, 50 μm to 500 μm, or 20 μm to 2000 μm. The minimum width W2 of the second bottom surface 12a may be 1 μm to 3 μm, 0.5 μm to 5 μm, or 0.3 μm to 10 μm.

[0013] The main surface S1 of the substrate 1 may have three or more recesses formed thereon, each having a different minimum width. In this case, the recesses may be classified into a plurality of recesses, each having a bottom surface with a minimum width equal to or greater than the reference value, and a second recess may be classified into a plurality of recesses, each having a minimum width less than the reference value. The reference minimum width may be set, for example, in the range of 0.3 μm to 10 μm. In this case, the ratio W1 / W2 of the average value of the minimum width W1 to the average value of the minimum width W2 may be 3 to 100, 5 to 500, or 20 to 1000.

[0014] The substrate 1 has a substrate body 2 and a seed layer 3 provided on the main surface S1 side of the substrate body 2 .

[0015] The substrate main body 2 has a base 2A located inside the positions of the first bottom surface 11a and the second bottom surface 12a, and a plurality of substrate protrusions 2B provided on the base 2A. A first recess 11 and a second recess 12 are formed between adjacent substrate protrusions 2B. The substrate protrusions 2B may be formed integrally with part or all of the base 2A, or the substrate protrusions 2B may be provided separately from the base 2A.

[0016] The substrate main body 2 or the base 2A may be a temporary support for forming a wiring structure, or may be a component including a circuit to which the wiring in the wiring structure is connected. The substrate main body 2 or the substrate protrusion 2B may be an insulating layer that constitutes the wiring structure. For example, the substrate 1 may be a component including a semiconductor element, and the wiring structure may be a rewiring layer that is a wiring structure connected to the semiconductor element. In this case, the method according to the present disclosure can be used, for example, to manufacture a fan-out type semiconductor package having a semiconductor element and a rewiring layer. The method according to the present disclosure can also be used to manufacture an interposer, which is a wiring structure that connects semiconductor elements to each other in so-called 2.5D, 2.3D, 2.1D, or other semiconductor packages.

[0017] The surface of the seed layer 3 opposite the substrate main body portion 2 includes a first bottom surface 11a and a second bottom surface 12a. In the example of FIG. 1 , the surface of the seed layer 3 further includes a first wall surface 11b and a second wall surface 12b. In other words, the seed layer 3 forms the entire main surface S1. The seed layer 3 is used to form the first metal plating layer 51 or the second metal plating layer 52 by electrolytic plating. The seed layer 3 can be a layer containing a metal such as copper. The thickness of the seed layer 3 may be, for example, 50 nm or more and 500 nm or less. The seed layer 3 can be formed by, for example, a sputtering method. The seed layer 3 may also be formed by electroless plating.

[0018] 1B, a temporary protective layer 7 including a portion that fills the second recess 12 is formed on the main surface S1 of the substrate 1. The temporary protective layer 7 has a pattern including an opening 7a that exposes at least a portion of the first bottom surface 11a. The temporary protective layer 7 may be provided so as to extend over the edge of the first recess 11. Although the temporary protective layer 7 illustrated in FIG. 1 fills the second recess 12, it is not necessary for the temporary protective layer to completely fill the second recess, and a cavity may be formed between the temporary protective layer 7 and the seed layer 3 within the second recess.

[0019] The temporary protective layer 7 can be formed by a method including, for example, providing a photosensitive resist layer on the main surface 1S of the substrate 1 and patterning the photosensitive resist layer by exposure and development to form the temporary protective layer 7 having a pattern including the openings 7a. Examples of resist materials (photosensitive resin compositions) for forming the photosensitive resist layer in this case will be described later.

[0020] As shown in FIG. 2C , a first metal plating layer 51 is formed by electrolytic plating on the first bottom surface 11a exposed in the opening 7a. The first metal plating layer 51 may be a layer containing copper. The first metal plating layer 51 is formed so as not to completely fill the first recess 11. For example, the ratio of the minimum thickness of the first metal plating layer 51 to the depth of the first recess 11 may be 0.2 or more and 0.9 or less. The thickness here refers to the thickness in a direction perpendicular to the first bottom surface 11a. A depression may be formed on the surface of the first metal plating layer 51 opposite the first bottom surface 11a. This depression typically has a shape such that the thickness of the first metal plating layer 51 is minimum at a position above the center of the first bottom surface 11a.

[0021] After the first metal plating layer 51 is formed, the temporary protective layer 7 is removed as shown in Fig. 2(d) . Removal of the temporary protective layer 7 exposes the second recess 12. The temporary protective layer 7 can be removed by, for example, dissolving it in a stripping solution.

[0022] Next, as shown in FIG. 3E, a second metal plating layer 52 is formed by electrolytic plating. The first metal plating layer 51 can also be a layer containing copper. The second metal plating layer 52 includes a portion filling the second recess 12, a portion within the first recess 11 provided on the first metal plating layer, and a portion (overburden) extending beyond the first recess 11 and the second recess 12. The conductor layer 5 is composed of the first metal plating layer 51 and the second metal plating layer 52. Because the first metal plating layer 51 is provided in advance, the conductor layer 5 filling the first recess 11 and the second recess 12 can be formed while avoiding the formation of an excessive amount of overburden near the second recess 12. As a result, the amount of conductor layer 5 that needs to be removed to form the wiring structure 50 having the first conductor portion 5A and the second conductor portion 5B as shown in FIG. 3F can be reduced. Furthermore, even if the amount of overburden is relatively small, the surface S2 of the conductor layer 5 (second metal plating layer 52) opposite the substrate 1 is likely to be flat. Having a flat surface for the conductor layer 5 is advantageous for efficient removal of the conductor layer 5 by a method such as chemical mechanical polishing.

[0023] In the wiring structure 50 formed by removing a portion of the conductor layer 5, the first conductor portion 5A includes a first metal plating layer 51 and a second metal plating layer 52, and the second conductor portion 5B includes the second metal plating layer 52. In the example of FIG. 3 , a portion of the seed layer 3 is also removed, and a flat main surface S3 is formed by the first conductor portion 5A, the second conductor portion 5B, and the substrate 1 (or the substrate main body portion 2). The first conductor portion 5A having a wide width can be, for example, a land or a via. The second conductor portion 5B having a narrow width can be, for example, a wiring having a linearly extending portion. A wiring structure having a multilayer structure may be formed by forming an additional wiring layer on the wiring layer including the first conductor portion 5A and the second conductor portion 5B.

[0024] The method of the present disclosure is not limited to the above examples and can be modified as necessary. For example, the substrate 1 may have a base having a flat surface along a plane including the first bottom surface 11a and the second bottom surface 12a, and a substrate convex portion provided on the flat surface side of the base, and the substrate convex portion may be a resist layer. In this case, the resist layer (substrate convex portion 2B) has a pattern including an opening along the first wall surface 11b and an opening along the second wall surface 12b. After the first conductor portion 5A and the second conductor portion 5B are formed, the resist layer (substrate convex portion 2B) may be removed.

[0025] The photosensitive resist layer for forming the temporary protective layer 7 having a predetermined pattern can be, for example, a layer formed from a photosensitive resin composition containing a binder polymer, a photopolymerizable compound having an ethylenically unsaturated bond, and a photopolymerization initiator.

[0026] The binder polymer may be, for example, a copolymer containing benzyl (meth)acrylate or a derivative thereof, styrene or a styrene derivative, a (meth)acrylic acid alkyl ester, and (meth)acrylic acid as monomer units.

[0027] Specific examples of the benzyl (meth)acrylate derivative constituting the binder polymer include 4-methylbenzyl (meth)acrylate, 4-ethylbenzyl (meth)acrylate, 4-tert-butylbenzyl (meth)acrylate, 4-methoxybenzyl (meth)acrylate, 4-ethoxybenzyl (meth)acrylate, 4-hydroxybenzyl (meth)acrylate, and 4-chlorobenzyl (meth)acrylate.

[0028] Specific examples of the styrene derivative that constitutes the binder polymer include vinyltoluene, p-methylstyrene, and p-chlorostyrene.

[0029] The (meth)acrylic acid alkyl ester constituting the binder polymer may be an ester compound formed from (meth)acrylic acid and a linear or branched aliphatic alcohol having 1 to 12 carbon atoms. The aliphatic alcohol may have 1 to 8 or 1 to 4 carbon atoms. Specific examples of the (meth)acrylic acid alkyl ester include methyl (meth)acrylate, ethyl (meth)acrylate, propyl (meth)acrylate, isopropyl (meth)acrylate, butyl (meth)acrylate, tert-butyl (meth)acrylate, pentyl (meth)acrylate, hexyl (meth)acrylate, heptyl (meth)acrylate, octyl (meth)acrylate, and 2-ethylhexyl (meth)acrylate.

[0030] The proportion of monomer units derived from benzyl (meth)acrylate or a derivative thereof in the binder polymer may be 50 to 80% by mass, 50 to 75% by mass, 50 to 70% by mass, or 50 to 65% by mass, based on the mass of the binder polymer. The proportion of monomer units derived from styrene or a styrene derivative in the binder polymer may be 5 to 40% by mass, or 5 to 35% by mass, based on the mass of the binder polymer. The proportion of monomer units derived from (meth)acrylic acid alkyl ester in the binder polymer may be 1 to 20% by mass, 1 to 15% by mass, 1 to 10% by mass, or 1 to 5% by mass, based on the mass of the binder polymer. The proportion of monomer units derived from (meth)acrylic acid in the binder polymer may be 5 to 30% by mass, 5 to 25% by mass, or 10 to 25% by mass, based on the mass of the binder polymer.

[0031] The weight average molecular weight (Mw) of the binder polymer may be 20,000 to 150,000, 30,000 to 100,000, 40,000 to 80,000, or 40,000 to 60,000. The weight average molecular weight here refers to a value calculated in terms of standard polystyrene determined by gel permeation chromatography (GPC).

[0032] The acid value (mg KOH / g) of the binder polymer may be 13 to 78, 39 to 65, or 52 to 62. The acid value here means the amount (mg) of potassium hydroxide required to neutralize 1 g of the binder polymer.

[0033] Specific examples of photopolymerizable compounds having an ethylenically unsaturated bond include bisphenol A (meth)acrylate compounds, hydrogenated bisphenol A (meth)acrylate compounds, polyalkylene glycol (meth)acrylates, urethane monomers, pentaerythritol (meth)acrylate, and trimethylolpropane (meth)acrylate. These may be used alone or in combination of two or more. The bisphenol A di(meth)acrylate compound may be, for example, a compound represented by the following general formula (1):

[0034]

[0035] In formula (1), each R independently represents a hydrogen atom or a methyl group. EO and PO represent an oxyethylene group and an oxypropylene group, respectively. 1 , m 2 , n 1 , n 2 each independently represents 0 to 40, m 1 +m 2 is 1 to 40, and n 1 +n 2 is 0 to 20. Either EO or PO may be on the phenolic hydroxyl group side. 1 , m 2 , n 1 and n 2 indicates the number of EO or PO, respectively. 1 +m 2 a compound having an average of 5 or less, and m 1 +m 2 It may be combined with a compound having an average of 6 to 40.

[0036] The polyalkylene glycol (meth)acrylate may be a compound represented by the following formula (2): As the photopolymerizable compound having an ethylenically unsaturated bond, a bisphenol A-based di(meth)acrylate compound may be combined with a compound represented by the following formula (2):

[0037]

[0038] In formula (2), R 14 and R 15 each independently represents a hydrogen atom or a methyl group, EO and PO are as defined above, s 1 indicates 1 to 30, and r 1 and r 2 indicates 0 to 30, and r 1 +r 2 is 1 to 30. Examples of commercially available compounds represented by formula (2) include 14 and R 15 is a methyl group, r 1 +r 2 = 4 (average value), s 1 = 12 (average value) (manufactured by Hitachi Chemical Co., Ltd., trade name: FA-023M).

[0039] Specific examples of the photopolymerization initiator include aromatic ketones such as benzophenone, N,N'-tetramethyl-4,4'-diaminobenzophenone (Michler's ketone), N,N'-tetraethyl-4,4'-diaminobenzophenone, 4-methoxy-4'-dimethylaminobenzophenone, 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-butanone-1, and 2-methyl-1-[4-(methylthio)phenyl]-2-morpholino-propanone-1. ton; 2-ethylanthraquinone, phenanthrenequinone, 2-tert-butylanthraquinone, octamethylanthraquinone, 1,2-benzanthraquinone, 2,3-benzanthraquinone, 2-phenylanthraquinone, 2,3-diphenylanthraquinone, 1-chloroanthraquinone, 2-methylanthraquinone, 1,4-naphthoquinone, 9,10-phenanthranequinone, 2-methyl-1,4-naphthoquinone, 2,3-dimethylanthraquinone quinones such as benzoinone; benzoin ether compounds such as benzoin methyl ether, benzoin ethyl ether, and benzoin phenyl ether; benzoin compounds such as benzoin, methylbenzoin, and ethylbenzoin; benzyl derivatives such as benzil dimethyl ketal; 2,4,5-triarylimidazole dimers such as 2-(o-chlorophenyl)-4,5-diphenylimidazole dimer, 2-(o-chlorophenyl)-4,5-di(methoxyphenyl)imidazole dimer, 2-(o-fluorophenyl)-4,5-diphenylimidazole dimer, 2-(o-methoxyphenyl)-4,5-diphenylimidazole dimer, and 2-(p-methoxyphenyl)-4,5-diphenylimidazole dimer; acridine derivatives such as 9-phenylacridine and 1,7-bis(9,9'-acridinyl)heptane; N-phenylglycine, N-phenylglycine derivatives, and coumarin compounds. These may be used alone or in combination of two or more. The photoinitiator may comprise a 2,4,5-triarylimidazole dimer, particularly a 2-(O-chlorophenyl)-4,5-diphenylimidazole dimer.

[0040] The content of the binder polymer in the photosensitive resin composition may be 40 to 80 parts by mass, 45 to 75 parts by mass, or 50 to 70 parts by mass, relative to 100 parts by mass of the total amount of the binder polymer and the photopolymerizable compound. The content of the photopolymerization initiator in the photosensitive resin composition may be 0.01 to 5 parts by mass, 0.1 to 4.5 parts by mass, or 1 to 4 parts by mass, relative to 100 parts by mass of the total amount of the binder polymer and the photopolymerizable compound.

[0041] The photosensitive resin composition may contain other components as needed. Examples of other components include a photopolymerizable compound having a cationically polymerizable cyclic ether group, a cationic polymerization initiator, a sensitizer, a dye such as malachite green, a photocoloring agent such as tribromomethylphenyl sulfone or leucocrystal violet, a thermal color-developing inhibitor, a plasticizer such as p-toluenesulfonamide, a pigment, a filler, an antifoaming agent, a flame retardant, a stabilizer, an adhesion promoter, a leveling agent, a release accelerator, an antioxidant, a fragrance, an imaging agent, and a thermal crosslinking agent. The content of each of the other components may be about 0.01 to 20 parts by mass per 100 parts by mass of the combined amount of the binder polymer and the photopolymerizable compound.

[0042] The total content of the binder polymer, the photopolymerizable compound, and the photopolymerization initiator in the photosensitive resin composition may be 90 to 100% by mass, or 95 to 100% by mass, based on the total mass of the components other than the solvent in the photosensitive resin composition.

[0043] To form the photosensitive resist layer, a resist film containing a photosensitive resin composition may be laminated on the main surface S1 of the substrate 1, or a photosensitive resin composition containing a solvent may be applied to the main surface S1 of the substrate 1 and the solvent may be removed from the coating.

[0044] 1...substrate, 2...substrate main body, 3...seed layer, 5...conductor layer, 5A...first conductor portion, 5B...second conductor portion, 7...temporary protective layer, 7a...opening, 11...first recess, 11a...first bottom surface, 11b...first wall surface, 12...second recess, 12a...second bottom surface, 12b...second wall surface, 50...wiring structure, 51...first metal plating layer, 52...second metal plating layer, W1...minimum width of first bottom surface, W2...minimum width of second bottom surface.

Claims

1. A method for manufacturing a semiconductor device comprising: preparing a substrate having a main surface forming a first recess and a second recess, the first recess having a first bottom surface and a first wall surface, the second recess having a second bottom surface and a second wall surface, the first bottom surface having a minimum width greater than the minimum width of the second bottom surface; forming a temporary protective layer on the main surface of the substrate, the temporary protective layer having a pattern including an opening through which at least a portion of the first bottom surface is exposed, the temporary protective layer including a portion covering the second recess; forming a first metal plating layer on the first bottom surface exposed in the opening; removing the temporary protective layer to expose the second recess; forming a second metal plating layer including a portion filling the second recess and a portion provided on the first metal plating layer, thereby forming a conductor layer including the first metal plating layer and the second metal plating layer; removing a portion of the conductor layer, thereby forming a first conductor portion provided in the first recess and including the first metal plating layer and the second metal plating layer, and a second conductor portion provided in the second recess and including the second metal plating layer. The method for manufacturing a wiring structure, wherein the substrate comprises a seed layer having a surface including the first bottom surface and the second bottom surface, and the first metal plating layer and the second metal plating layer are formed by electrolytic plating.

2. The method of claim 1, wherein said substrate further comprises an insulating layer having a pattern including an opening along said first wall and an opening along said second wall.

3. The method of claim 1, wherein the first metal plating layer is formed such that a depression is formed in a surface of the first metal plating layer opposite the first bottom surface.

4. The method of claim 1, wherein forming the temporary protective layer comprises: providing a photosensitive resist layer on the main surface of the substrate; and patterning the photosensitive resist layer by exposure and development to form the temporary protective layer having the pattern.

5. The method according to claim 4, wherein the photosensitive resist layer comprises a binder polymer, a photopolymerizable compound having an ethylenically unsaturated bond, and a photopolymerization initiator.

Citation Information

Patent Citations

  • Method for forming copper wiring layer

    JP2006041036A

  • Method for manufacturing semiconductor device

    JP2007189068A

  • Method of forming wiring structure and wiring structure

    JP2011258839A

  • Method for forming resist pattern, method for manufacturing printed wiring board, photosensitive resin composition for projection exposure, and photosensitive element

    JP2019109543A

  • Method of plating a semiconductor structure

    US20040188260A1