Device and method for producing device
By employing a method that forms controlled conductive films within through holes using masks, the method addresses the issue of resist film thickness variations and defects in conductive patterns, enhancing the manufacturing process for devices with through electrodes.
Patent Information
- Application Number
- PCT/JP2023/017613
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-10
- Publication Date
- 2024-11-14
AI Technical Summary
The existing methods for forming conductive films on the inner walls of through holes in substrates result in variations in resist film thickness, leading to defects during etching processes due to the thick conductive films on the substrate surfaces, causing unintended etching of protected areas.
A method involving the formation of a first opening that penetrates the substrate, followed by a second opening etched halfway through, with conductive films deposited using masks to control the film thickness and prevent protrusion, ensuring uniform resist film application and reducing defects.
This approach reduces variations in resist film thickness and suppresses defects in conductive patterns, ensuring accurate etching and reliable device manufacturing with through electrodes.
Smart Images

Figure JP2023017613_14112024_PF_FP_ABST
Abstract
Description
Device and method for manufacturing the same
[0001] The present invention relates to a device and a method for manufacturing the device.
[0002] A configuration is known in which wiring on the front and back surfaces of a substrate is electrically connected by a through electrode provided in a through hole penetrating the substrate (e.g., Patent Documents 1 and 2).A configuration is known in which a metal film is formed on the inner wall of a through hole in a substrate or a dielectric film by depositing the metal film from a direction tilted relative to the surface of the substrate or the dielectric film (e.g., Patent Documents 3 and 4).
[0003] Japanese Patent Application Publication No. 2016-213253 U.S. Patent Application Publication No. 2020 / 0152540 International Publication No. 2020 / 059607 Japanese Patent Application Publication No. 2004-311545
[0004] When a second conductive film is formed on the inner wall of a through hole in a substrate having a first conductive film on its surface, the second conductive film may become thick on the surface of the substrate. In this case, when a resist film is applied to the surface of the substrate after the second conductive film is formed, the thick second conductive film may cause variations in the thickness of the resist film. If variations in the thickness of the resist film occur, when the first conductive film is etched using the resist film as a mask, the first conductive film may be etched in areas that should be protected by the resist film.
[0005] In one aspect, an object is to reduce variations in the film thickness of a resist film.
[0006] In one aspect, a method for manufacturing a device includes the steps of: forming a first opening in a substrate, the first opening penetrating the substrate; forming a first mask that includes the first opening in a plan view and has an opening area wider than the first opening; etching the substrate halfway through the substrate using the first mask as a mask to form a second opening; forming a first conductive film on at least a surface of the substrate after the step of forming the second opening; forming a second mask on the substrate after the step of forming the first conductive film so as to expose the first opening and cover an edge of the second opening; depositing a second conductive film using the second mask as a mask; removing the second mask; applying a resist film to the first conductive film after the step of removing the second mask; forming a third mask using the resist film; and etching the first conductive film using the third mask as a mask.
[0007] In one aspect, the device is characterized by comprising: a substrate having a through hole extending from the front surface to the back surface, the through hole having a first opening and a second opening located closer to the front surface than the first opening and wider than the first opening in a planar view; a conductive pattern provided on at least the front surface of the substrate; and a through electrode provided in the through hole away from the end of the second opening.
[0008] As one aspect, it is possible to reduce variations in the thickness of the resist film.
[0009] FIGS. 1( a ) to 1 ( d ) are cross-sectional views (part 1 ) illustrating a method for manufacturing a device according to a comparative example. FIGS. 2( a ) to 2 ( c ) are cross-sectional views (part 2 ) illustrating a method for manufacturing a device according to a comparative example. FIGS. 3( a ) to 3 ( c ) are cross-sectional views (part 3 ) illustrating a method for manufacturing a device according to a comparative example. FIGS. 4( a ) and 4 ( b ) are cross-sectional views (part 4 ) illustrating a method for manufacturing a device according to a comparative example. FIGS. 5( a ) to 5 ( c ) are cross-sectional views (part 1 ) illustrating a method for manufacturing a device according to Example 1. FIGS. 6( a ) to 6 ( c ) are cross-sectional views (part 2 ) illustrating a method for manufacturing a device according to Example 1. FIGS. 7( a ) to 7 ( c ) are cross-sectional views (part 3 ) illustrating a method for manufacturing a device according to Example 1. FIGS. 8( a ) to 8 ( c ) are cross-sectional views (part 4 ) illustrating a method for manufacturing a device according to Example 1. FIGS. 9( a ) to 9 ( c ) are cross-sectional views (part 5 ) illustrating a method for manufacturing a device according to Example 1. FIG. 10 is a plan view of the vicinity of the first opening in FIG. 5(c). FIG. 11 is a plan view of the vicinity of the second opening in FIG. 7(a). FIG. 12 is a plan view of a device according to Example 2. FIGS. 13(a) to 13(d) are cross-sectional views (part 1) showing a method for manufacturing a device according to Example 2. FIGS. 14(a) to 14(d) are cross-sectional views (part 2) showing a method for manufacturing a device according to Example 2. FIGS. 15(a) to 15(d) are cross-sectional views (part 3) showing a method for manufacturing a device according to Example 2. FIG. 16 is a plan view of a device according to a modified example of Example 2.
[0010] Hereinafter, embodiments of the present invention will be described with reference to the drawings.
[0011] First, in order to clarify the problem to be solved by the present invention, a method for manufacturing a device according to a comparative example will be described.
[0012] 1A to 4B are cross-sectional views showing a method for manufacturing a device according to a comparative example. As shown in Fig. 1A, a resist film is applied to a substrate 110, and then the resist film is exposed to light, developed, and patterned to form a mask layer 111 having an opening region 112. The substrate 110 is then attached to a silicon substrate 113.
[0013] As shown in FIG. 1B, the substrate 110 is dry-etched using the mask layer 111 as a mask to form a through-hole 120 penetrating the substrate 110 .
[0014] As shown in FIG. 1C, after removing the mask layer 111 and the silicon substrate 113, a conductive film 130 is formed on the front surface of the substrate 110 and a conductive film 140 is formed on the rear surface thereof by, for example, sputtering.
[0015] 1D, a conductive film 132 is formed on the surface of the substrate 110 using oblique vacuum deposition. By using oblique vacuum deposition, the conductive film 132 is also formed on part of the inner wall of the through hole 120. The conductive film 132 formed on the inner wall of the through hole 120 becomes thinner the deeper it is in the through hole 120. Therefore, when attempting to form a conductive film 132 of a desired thickness on the inner wall of the through hole 120, the conductive film 132 on the surface of the substrate 110 becomes thicker than necessary.
[0016] As shown in FIG. 2A, after a resist film, for example, is attached onto the conductive film 132, the resist film is exposed to light, developed and patterned to form a mask layer 150 having an opening region 151.
[0017] 2B, the conductive film 132 is etched using the mask layer 150 as a mask to form a conductive pattern 133 made of the conductive film 132. Thereafter, the mask layer 150 is removed. The conductive pattern 133 is formed on a part of the inner wall of the through hole 120, and is also formed around the through hole 120 on the conductive film 130. The conductive pattern 133 formed on the conductive film 130 around the through hole 120 is formed as a thick film.
[0018] 2( c), a conductive pattern 143 is also formed on the back surface of the substrate 110 by the same method as in FIGS. 1( d) to 2( b), extending from a part of the inner wall of the through hole 120 onto the conductive film 140. The conductive pattern 133 and the conductive pattern 143 are formed so as to be in contact with each other on the inner wall of the through hole 120, and function as a through electrode 160 that penetrates the substrate 110.
[0019] 3A, a resist film 152 is applied onto the surface of the substrate 110 by spin coating. Because a thick conductive pattern 133 is formed on the surface of the substrate 110, the flow of the resist is blocked by the conductive pattern 133. This can cause, for example, a Karman vortex street to occur behind the conductive pattern 133 in the resist flow, making the resist flow uneven and resulting in the generation of thin portions of the resist film 152.
[0020] As shown in FIG. 3B, the resist film 152 is exposed to light, developed, and patterned to form a mask layer 153 having an opening region 154 .
[0021] 3C, the conductive film 130 is dry-etched using the mask layer 153 as a mask, forming a conductive pattern 131 made of the conductive film 130. When the conductive film 130 is etched, the mask layer 153 is also etched. If there are thin portions of the mask layer 153 due to variations in the film thickness of the resist film 152, the mask layer 153 in the thin portions may be removed during etching of the conductive film 130, and portions of the conductive film 130 that would not normally be etched may also be etched. This may result in defects 134 in the conductive pattern 131.
[0022] 4A, the mask layer 153 is removed. Then, a resist film is applied, exposed, and developed on the rear surface of the substrate 110 to form a mask layer 155 having an opening region 156. The conductive film 140 is dry-etched using the mask layer 155 as a mask to form a conductive pattern 141 made of the conductive film 140. Defects 144 may also occur in the conductive pattern 141 for the same reasons as in the conductive pattern 131.
[0023] 4B, the mask layer 155 is removed, and thus the device according to the comparative example is formed.
[0024] 3(a) to 3(c), variations in the film thickness of the resist film 152 may cause etching of the conductive film 130 in areas that should be protected by the mask layer 153, resulting in defects 134 in the conductive pattern 131. Similarly, defects 144 may also occur in the conductive pattern 141, as shown in FIG.
[0025] Therefore, a first embodiment will be described below, which can reduce the variation in the thickness of the resist film and suppress the occurrence of defects in the conductive pattern.
[0026] 5A to 9C are cross-sectional views showing a method for manufacturing a device according to Example 1. The method for manufacturing a device according to Example 1 can be applied to various devices having through electrodes penetrating a substrate, such as interposers. As shown in FIG. 5A, a resist film is applied to the surface of a substrate 10, which is, for example, a silicon substrate, and then the resist film is exposed and developed to form a mask layer 11 having an opening region 12 on the surface of the substrate 10. The substrate 10 is then attached to a silicon substrate 13, which is a support substrate, using an adhesive.
[0027] 5B, the substrate 10 is dry-etched using the mask layer 11 as a mask to form a first opening 21, which is a through-hole penetrating the substrate 10. The first opening 21 is formed by reactive ion etching using, for example, the Bosch process. For example, SF is used as a fluorine-based gas. 6 The substrate 10 is etched using a gas, and O is used as the oxygen-based gas. 2 The first opening 21 is formed by alternately repeating the steps of forming a protective film on the inner wall of the hole etched with a gas. 6 The gas flow rate is 200 sccm, O 2 The gas flow rate may be set to 40 sccm, and the RF power may be set to 2500 W. By forming the first opening 21 using this method, a deep first opening 21 can be formed. The inner walls of the first opening 21 are formed to be almost vertical. The first opening 21 has a diameter of, for example, about 100 μm to 150 μm, and a depth of about 250 μm to 350 μm.
[0028] As shown in FIG. 5( c), the mask layer 11 is removed. Thereafter, a resist film is applied to the surface of the substrate 10, and the resist film is exposed and developed to pattern it, thereby forming a mask layer 14 having an opening region 15 on the surface of the substrate 10. FIG. 10 is a plan view of the vicinity of the first opening 21 in FIG. 5( c). In FIG. 10, the mask layer 14 is hatched for clarity. As shown in FIGS. 5( c) and 10, the opening region 15 of the mask layer 14 is formed to overlap the first opening 21 and has a shape larger than the first opening 21. In other words, the opening region 15 encompasses the first opening 21 in a plan view and has a shape wider than the first opening 21.
[0029] 6A, the substrate 10 is dry-etched partway through using the mask layer 14 as a mask, and a second opening 22 larger than the first opening 21 is formed in the surface of the substrate 10. The second opening 22 is formed by reactive ion etching using, for example, a fluorine-based gas. For example, the fluorine-based gas is SF 6 Gas and C 4 F 8 The substrate 10 is etched using a gas mixture containing SF 2 and SF 5 to form the second opening 22. 6 The gas flow rate is 400 sccm, C 4 F 8 The gas flow rate may be set to 400 sccm, and the RF power may be set to 1000 W. By forming the second opening 22 in this manner, the inner wall of the second opening 22 is formed to have a tapered shape. The second opening 22 has a diameter of about 200 μm to 250 μm and a depth of about 80 μm to 120 μm, for example.
[0030] As shown in FIG. 6( b), the mask layer 14 and the silicon substrate 13 are removed. Then, a third opening 23, which is larger than the first opening 21 in plan view, is formed on the rear surface of the substrate 10 by the same method as in FIGS. 5( c) and 6( a). Because the third opening 23 is formed by the same method as the second opening 22, the inner wall of the third opening 23 is tapered. The third opening 23 has a diameter and depth similar to those of the second opening 22, e.g., a diameter of approximately 200 μm to 250 μm and a depth of approximately 80 μm to 120 μm. The first opening 21, the second opening 22, and the third opening 23 form a through-hole 20 penetrating the substrate 10.
[0031] As shown in FIG. 6C , a conductive film 30 is formed on the front surface of the substrate 10, and a conductive film 40 is formed on the rear surface thereof, using, for example, sputtering. Because the inner wall of the second opening 22 formed on the front surface of the substrate 10 is tapered, the conductive film 30 is formed from the front surface of the substrate 10 to the inner wall and bottom surface of the second opening 22. Similarly, because the inner wall of the third opening 23 formed on the rear surface of the substrate 10 is tapered, the conductive film 40 is formed from the rear surface of the substrate 10 to the inner wall and bottom surface of the third opening 23. The conductive films 30 and 40 are formed of a superconducting material, such as aluminum (Al), titanium nitride (TiN), or niobium (Nb). The thickness of the conductive films 30 and 40 is, for example, approximately 100 nm to 500 nm.
[0032] As shown in FIG. 7( a), a mask layer 16 having an opening region 17 is formed on the surface of the substrate 10. The mask layer 16 may be a stencil mask made of metal, or may be made of resist. FIG. 11 is a plan view of the vicinity of the second opening 22 in FIG. 7( a). In FIG. 11, the mask layer 16 is hatched for clarity. As shown in FIGS. 7( a) and 11, the opening region 17 of the mask layer 16 is formed to overlap the first opening 21 and the second opening 22, but is larger than the first opening 21 and smaller than the second opening 22. That is, the mask layer 16 is formed to expose the first opening 21 and cover the end 24 of the second opening 22 that connects to the surface of the substrate 10.
[0033] As shown in FIG. 7B , the conductive film 32 is formed by, for example, oblique vacuum deposition using the mask layer 16 as a mask. Because the mask layer 16 is formed to cover the edge 24 of the second opening 22, the conductive film 32 formed in the second opening 22 is formed away from the edge 24 of the second opening 22. By forming the conductive film 32 using oblique vacuum deposition, the conductive film 32 is formed from the second opening 22 to at least a portion of the inner wall of the first opening 21. By forming the conductive film 32 in the second opening 22, even if the conductive film 32 on the inner wall of the first opening 21 is thickened, the conductive film 32 is prevented from protruding from the upper surface of the conductive film 30. The conductive film 32 is formed of a superconducting material, for example, aluminum (Al), titanium nitride (TiN), or niobium (Nb). The thickness of the conductive film 32 is, for example, approximately 300 nm to 1000 nm.
[0034] As shown in FIG. 7C , the mask layer 16 and the conductive film 32 thereon are removed. This forms a conductive pattern 33 made of the conductive film 32 in the second opening 22. A mask layer 18 having an opening region 19 is then formed on the back surface of the substrate 10. The mask layer 18 may be a stencil mask made of metal, or may be made of resist. The opening region 19 of the mask layer 18, like the opening region 17 of the mask layer 16, is formed to overlap the first opening 21 and the third opening 23, but is larger than the first opening 21 and smaller than the third opening 23. That is, the mask layer 18 is formed to expose the first opening 21 and cover the end 25 of the third opening 23 that connects to the back surface of the substrate 10. A conductive film 42 is then formed by, for example, oblique vacuum deposition using the mask layer 18 as a mask. The conductive film 42 is formed away from the edge 25 of the third opening 23 and extends from the third opening 23 to at least a portion of the inner wall of the first opening 21. The conductive film 42 is formed on the inner wall of the first opening 21 in contact with the conductive pattern 33. The conductive film 42 is made of a superconducting material, such as aluminum (Al), titanium nitride (TiN), or niobium (Nb). The thickness of the conductive film 42 is, for example, about 300 nm to 1000 nm.
[0035] 8A, the mask layer 18 and the conductive film 42 thereon are removed. As a result, a conductive pattern 43 made of the conductive film 42 is formed in the third opening 23. The conductive pattern 33 and the conductive pattern 43 function as a through electrode 60 that penetrates the substrate 10. Thereafter, a resist film 50 is applied onto the surface of the substrate 10. The resist film 50 is applied using, for example, a spin coating method. Since the protrusion of the conductive pattern 33 from the surface of the conductive film 30 is suppressed, variations in the film thickness of the resist film 50 are suppressed.
[0036] 8B, the resist film 50 is exposed to light, developed, and patterned to form a mask layer 51 having an opening region 52. Since the variation in the thickness of the resist film 50 is suppressed, the variation in the thickness of the mask layer 51 is also suppressed.
[0037] 8C, the conductive film 30 is dry-etched using the mask layer 51 as a mask to form the conductive pattern 31. The conductive film 30 is etched by reactive ion etching using a fluorine-based gas, for example. Since the variation in the film thickness of the mask layer 51 is suppressed, the occurrence of defects in the conductive pattern 31 is suppressed.
[0038] 9A, the mask layer 51 is removed. Then, a resist film 53 is applied to the rear surface of the substrate 10. The resist film 53 is applied by, for example, spin coating. Since the conductive pattern 43 is prevented from protruding from the surface of the conductive film 40, variations in the thickness of the resist film 53 are suppressed.
[0039] 9B, the resist film 53 is exposed and developed to pattern it, thereby forming a mask layer 54 having an opening region 55. The conductive film 40 is dry-etched using the mask layer 54 as a mask to form the conductive pattern 41. The conductive film 40 is etched by reactive ion etching using a fluorine-based gas, for example. Since the variation in the film thickness of the resist film 53 is suppressed, the occurrence of defects in the conductive pattern 41 is suppressed.
[0040] 9C, the mask layer 54 is removed, and thus the device 100 according to the first embodiment is formed.
[0041] As described above, according to the first embodiment, as shown in FIG. 5B, a first opening 21 penetrating the substrate 10 is formed. As shown in FIGS. 5C and 10, a mask layer 14 (first mask) is formed, which includes the first opening 21 in a plan view and has an opening region 15 wider than the first opening 21. As shown in FIG. 6A, the substrate 10 is etched partway through using the mask layer 14 as a mask to form a second opening 22. As shown in FIG. 6C, after the second opening 22 is formed, a conductive film 30 (first conductive film) is formed on at least the surface of the substrate 10. As shown in FIGS. 7A and 11, after the conductive film 30 is formed, a mask layer 16 (second mask) is formed on the substrate 10 so as to expose the first opening 21 and cover the end 24 of the second opening 22. As shown in FIG. 7B, a conductive film 32 (second conductive film) is deposited using the mask layer 16 as a mask. As shown in FIG. 7( c), the mask layer 16 is removed. As shown in FIG. 8( a), after removing the mask layer 16, a resist film 50 is applied to the conductive film 30. As shown in FIG. 8( b), a mask layer 51 (third mask) is formed using the resist film 50. As shown in FIG. 8( c), the conductive film 32 is etched using the mask layer 51 as a mask. By using this manufacturing method, a device 100 is obtained, as shown in FIG. 9( c), having a through electrode 60 provided in the through hole 20 away from the end 24 of the second opening 22. As shown in FIG. 8( a), the conductive pattern 33 is formed in the second opening 22, thereby suppressing the protrusion of the conductive pattern 33 from the surface of the conductive film 30. This reduces the variation in the film thickness of the resist film 50 formed by application on the conductive film 30. Therefore, when the conductive film 30 is etched using the mask layer 51 formed from the resist film 50 to form a conductive pattern 31 made of the conductive film 30, as shown in FIG. 8( c), defects in the conductive pattern 31 can be suppressed.
[0042] 7B, the conductive film 30 and the conductive film 32 are formed so as to be electrically connected to each other. This allows the conductive pattern 31 made of the conductive film 30 to be electrically connected to the through electrode 60 formed including the conductive pattern 33 made of the conductive film 32. Therefore, a configuration is obtained in which the conductive pattern 31 on the front surface of the substrate 10 and the conductive pattern 41 on the back surface of the substrate 10 are electrically connected to each other via the through electrode 60.
[0043] 7B, the conductive film 32 is formed so as to cover at least a part of the inner wall of the first opening 21. This makes it easier to form the through electrode 60 including the conductive pattern 33 made of the conductive film 32.
[0044] 6C, the conductive film 30 is formed from the surface of the substrate 10 to the inner wall of the second opening 22. Since the inner wall of the second opening 22 is inclined, the conductive film 30 can be prevented from having poor conductivity at the end 24.
[0045] 8B and 8C, in Example 1, the step of patterning the conductive film 30 to form the conductive pattern 31 is performed after the through electrode 60 is created. For example, if the step of patterning the conductive film 30 to form the conductive pattern 31 is performed before the through electrode 60 is created, resist residue may be generated on the conductive pattern 31 when the resist formed on the conductive film 30 is removed. If the through electrode 60 is formed on the resist residue generated on the conductive pattern 31, poor connection between the conductive pattern 31 and the through electrode 60 may occur. Therefore, in this example, the step of patterning the conductive film 30 to form the conductive pattern 31 is performed after the through electrode 60 is created.
[0046] FIG. 12 is a plan view of a device according to a second embodiment. A device 200 according to the second embodiment is a quantum bit device. In FIG. 12, a conductive film provided on a substrate 10 is hatched for clarity. As shown in FIG. 12, a quantum bit 70, a resonator 71, and a filter 72 are provided on the substrate 10. The quantum bit 70 includes a Josephson junction element 75 connected between a first electrode 73 and a second electrode 74. The Josephson junction element 75 is connected between the first electrode 73 and the second electrode 74 by a superconducting film 77 (described later) connected to the second electrode 74 and a superconducting film 78 (described later) connected to the first electrode 73. Thus, the quantum bit 70 includes a transmon including the Josephson junction element 75 and a capacitor connected in parallel to the Josephson junction element 75 and consisting of the first electrode 73 and the second electrode 74. The resonator 71 includes a coplanar line with a meander structure, and one end is electrostatically coupled to the quantum bit 70. The other end of the resonator 71 is connected to a readout unit 79 via a filter 72. The readout unit 79 includes a through hole 20 that penetrates the substrate 10 and a through electrode 60 that is provided on the inner wall of the through hole 20 and includes conductive patterns 33, 43 (not shown in FIG. 12 ).
[0047] FIGS. 13( a ) to 15( d ) are cross-sectional views showing a method for manufacturing a device according to Example 2. First, the same method as that shown in FIGS. 5( a ) to 7( c ) of Example 1 is performed, followed by removing the mask layer 18, resulting in the device shown in FIG. 13( a ). In FIG. 13( a ), the conductive film 30, the conductive film 40, the conductive pattern 33, and the conductive pattern 43 are superconducting films formed of a superconducting material. The material of the conductive film 30 and the conductive film 40 is, for example, titanium nitride (TiN), aluminum (Al), tantalum (Ta), niobium (Nb), or niobium nitride (NbN). The material of the conductive pattern 33 and the conductive pattern 43 is, for example, a superconducting material such as aluminum (Al).
[0048] As shown in FIG. 13(b), after forming a mask layer 51 by the same method as in FIGS. 8(a) and 8(b) of Example 1, the conductive film 30 is dry-etched using the mask layer 51 as a mask, thereby forming a conductive pattern 31 made of the conductive film 30.
[0049] 13(c), the mask layer 51 is removed. Thereafter, a mask layer 54 is formed by the same method as in FIGS. 9(a) and 9(b) of Example 1, and then the conductive film 40 is dry-etched using the mask layer 54 as a mask to form a conductive pattern 41 made of the conductive film 40.
[0050] 13D, the mask layer 54 is removed. As a result, a resonator 71 including a coplanar line and a filter 72 are formed from the conductive patterns 31 and 41. Although not shown, a first electrode 73 and a second electrode 74 are also formed from the conductive patterns 31 and 41.
[0051] 14(a) and 15(a), a mask layer 80 including a lower layer 81 and an upper layer 82 that is thicker than the lower layer 81 is formed on the surface of the substrate 10. An opening region 83 is formed in the mask layer 80.
[0052] As shown in Figures 14(b) and 15(b), a superconducting film 77 is formed on the surface of the substrate 10 by oblique vacuum deposition using a mask layer 80 as a mask. Thereafter, while maintaining the vacuum state in which the superconducting film 77 was formed, oxygen is introduced into the chamber to oxidize the surface of the superconducting film 77, thereby forming an insulating film 84 on the surface of the superconducting film 77. Because the diameter of the through-hole 20 is small, the superconducting film 77 is not formed on the side wall of the through-hole 20. The material of the superconducting film 77 is, for example, aluminum (Al). The material of the insulating film 84 is, for example, aluminum oxide (Al 2 O 3 )
[0053] 14(c) and 15(c), using the mask layer 80 as a mask, a superconducting film 78 is formed on the surface of the substrate 10 by oblique vacuum deposition from a direction perpendicular to the direction of deposition of the superconducting film 77. Because the diameter of the through-hole 20 is small, the superconducting film 78 is not formed on the sidewall of the through-hole 20. The material of the superconducting film 78 is, for example, aluminum (Al).
[0054] 14(d) and 15(d), the mask layer 80 is removed. A Josephson junction element 75 is formed on the surface of the substrate 10, in which a superconducting film 77 and a superconducting film 78 overlap with an insulating film 84 interposed therebetween. Since a first electrode 73 and a second electrode 74 are also formed, a quantum bit 70 including the Josephson junction element 75 and a capacitor is formed, as shown in FIG.
[0055] [Modification] Fig. 16 is a plan view of a device according to a modification of Example 2. In Fig. 16, for clarity of the drawing, the conductive film provided on the substrate 10 is hatched. As shown in Fig. 16, in a device 210 according to a modification of Example 2, a plurality of through holes 20a are provided in the substrate 10. A through electrode 60a including conductive patterns 33, 43 (not shown in Fig. 16) is provided on the inner wall of the through hole 20a. The through electrode 60a is provided to electrically connect the conductive patterns 31, 41 on the front and back surfaces of the substrate 10. The other configurations are the same as those of Example 2, and therefore description thereof will be omitted.
[0056] In a modified example of the second embodiment, the plurality of through holes 20a and the through electrodes 60a provided in the through holes 20a are formed simultaneously by the same method as the through holes 20 and the through electrodes 60 provided in the through holes 20 of the second embodiment.
[0057] 13(b) to 15(d), the conductive films 30 and 40 are etched using the mask layers 51 and 54, and then the quantum bit 70 including the Josephson junction element 75 is formed on the substrate 10. For example, if the through-hole 20 is formed and the conductive films 30 and 40 are deposited and processed after the quantum bit 70 is formed, there is a risk of damaging the quantum bit 70. However, by forming the quantum bit 70 after etching the conductive films 30 and 40, damage to the quantum bit 70 can be reduced.
[0058] In addition, in Example 2 and its modified example, as shown in FIG. 13D, the conductive film 30 is etched to form a resonator 71 and a filter 72 using the conductive film 30. This makes it possible to easily form a quantum bit device. When forming a quantum bit device, the conductive film 30 and the conductive film 32 are made of a superconducting material. Note that the conductive film 30 is not limited to being used to form both the resonator 71 and the filter 72, and only one of them may be formed.
[0059] Although the embodiments of the present invention have been described in detail above, the present invention is not limited to such specific embodiments, and various modifications and changes are possible within the scope of the gist of the present invention described in the claims.
[0060] 10...substrate, 11...mask layer, 12...opening region, 13...silicon substrate, 14...mask layer, 15...opening region, 16...mask layer, 17...opening region, 18...mask layer, 19...opening region, 20, 20a...through hole, 21...first opening, 22...second opening, 23...third opening, 24...end, 25...end, 30...conductive film, 31...conductive pattern, 32...conductive film, 33...conductive pattern, 40...conductive film, 41...conductive pattern, 42...conductive film, 43...conductive pattern, 50...resist film, 51...mask layer, 52...opening region, 53...resist film, 54...mask layer, 55...opening region, 60, 60a...through electrode, 70...quantum bit, 71...resonator, 72...filter, 73...first electrode, 7 4...second electrode, 75...Josephson junction element, 77, 78...superconducting film, 79...readout section, 80...mask layer, 81...lower layer, 82...upper layer, 83...opening region, 84...insulating film, 100...device, 110...substrate, 111...mask layer, 112...opening region, 113...silicon substrate, 120...through hole, 130...conductive film, 131...conductive pattern, 132...conductive film, 133...conductive pattern, 134...defect, 140...conductive film, 141...conductive pattern, 143...conductive pattern, 144...defect, 150...mask layer, 151...opening region, 152...resist film, 153...mask layer, 154...opening region, 155...mask layer, 156...opening region, 160...through electrode, 200, 210...device
Claims
1. A method for manufacturing a device, comprising the steps of: forming a first opening in a substrate, the first opening penetrating the substrate; forming a first mask having an opening area that includes the first opening in a plan view and is wider than the first opening; etching the substrate halfway through the substrate using the first mask as a mask to form a second opening; forming a first conductive film on at least a surface of the substrate after the step of forming the second opening; forming a second mask on the substrate after the step of forming the first conductive film, exposing the first opening and covering an end of the second opening; depositing a second conductive film using the second mask as a mask; removing the second mask; applying a resist film on the first conductive film after the step of removing the second mask; forming a third mask using the resist film; and etching the first conductive film using the third mask as a mask.
2. A method for manufacturing a device according to claim 1, further comprising the step of forming quantum bits on the substrate after the step of etching the first conductive film.
3. The method for manufacturing a device according to claim 1 or 2, characterized in that the first conductive film and the second conductive film are electrically connected to each other.
4. The method for manufacturing a device according to claim 1 or 2, characterized in that at least one of a resonator and a filter using the first conductive film is formed by the step of etching the first conductive film.
5. A method for manufacturing a device according to claim 1 or 2, characterized in that the first conductive film and the second conductive film are made of a superconducting material.
6. The method for manufacturing a device according to claim 1 or 2, wherein at least a portion of the inner wall of the first opening is covered with the second conductive film.
7. A method for manufacturing a device according to claim 1 or 2, wherein the inner wall of the second opening is inclined.
8. A device comprising: a substrate having a through hole extending from a front surface to a back surface, the through hole having a first opening and a second opening located on the front surface side of the first opening and wider than the first opening in a planar view; a conductive pattern provided on at least the front surface of the substrate; and a through electrode provided in the through hole away from an end of the second opening.
Citation Information
Patent Citations
Semiconductor device
JP1992170051A
Semiconductor device and method of manufacturing semiconductor device
JP2009302453A
Semiconductor device and method for manufacturing the same
JP2017224690A
Low-loss architecture for superconducting qubit circuits
JP2021504964A
Fabrication of through-silicon vias in planar quantum devices
JP2022530310A